Elapsed Time, Volts/Count, Torch On, Arc Good, Voltage Control, THC Up, THC Down, Set Point, Current Voltage
14605, V, 0, 0, 0, 0, 0, 700, 52
14605, V, 0, 0, 0, 0, 0, 700, 52
14862, V, 0, 0, 0, 0, 0, 700, 52
14862, V, 0, 0, 0, 0, 0, 700, 52
15119, V, 0, 0, 0, 0, 0, 700, 52
15119, V, 0, 0, 0, 0, 0, 700, 52
15376, V, 0, 0, 0, 0, 0, 700, 52
15376, V, 0, 0, 0, 0, 0, 700, 52
15633, V, 0, 0, 0, 0, 0, 700, 52
15633, V, 0, 0, 0, 0, 0, 700, 52
15890, V, 0, 0, 0, 0, 0, 700, 52
15890, V, 0, 0, 0, 0, 0, 700, 52
16147, V, 0, 0, 0, 0, 0, 700, 52
16147, V, 0, 0, 0, 0, 0, 700, 52
16404, V, 0, 0, 0, 0, 0, 700, 52
16404, V, 0, 0, 0, 0, 0, 700, 52
16661, V, 0, 0, 0, 0, 0, 700, 52
16661, V, 0, 0, 0, 0, 0, 700, 52
16918, V, 0, 0, 0, 0, 0, 700, 52
16918, V, 0, 0, 0, 0, 0, 700, 52
17175, V, 0, 0, 0, 0, 0, 700, 52
17175, V, 0, 0, 0, 0, 0, 700, 52
17432, V, 0, 0, 0, 0, 0, 700, 52
17432, V, 0, 0, 0, 0, 0, 700, 52
17689, V, 0, 0, 0, 0, 0, 700, 52
17689, V, 0, 0, 0, 0, 0, 700, 52
17946, V, 0, 0, 0, 0, 0, 700, 52
17946, V, 0, 0, 0, 0, 0, 700, 52
18203, V, 0, 0, 0, 0, 0, 700, 52
18203, V, 0, 0, 0, 0, 0, 700, 52
18460, V, 0, 0, 0, 0, 0, 700, 52
18460, V, 0, 0, 0, 0, 0, 700, 52
18717, V, 0, 0, 0, 0, 0, 700, 52
18717, V, 0, 0, 0, 0, 0, 700, 52
18974, V, 0, 0, 0, 0, 0, 700, 52
18974, V, 0, 0, 0, 0, 0, 700, 52
19231, V, 0, 0, 0, 0, 0, 700, 52
19231, V, 0, 0, 0, 0, 0, 700, 52
19488, V, 0, 0, 0, 0, 0, 700, 52
19488, V, 0, 0, 0, 0, 0, 700, 52
19745, V, 0, 0, 0, 0, 0, 700, 52
19745, V, 0, 0, 0, 0, 0, 700, 52
20002, V, 0, 0, 0, 0, 0, 700, 52
20002, V, 0, 0, 0, 0, 0, 700, 52
20259, V, 0, 0, 0, 0, 0, 700, 52
20259, V, 0, 0, 0, 0, 0, 700, 52
20516, V, 0, 0, 0, 0, 0, 700, 52
20516, V, 0, 0, 0, 0, 0, 700, 52
20773, V, 0, 0, 0, 0, 0, 700, 52
20773, V, 0, 0, 0, 0, 0, 700, 52
21030, V, 0, 0, 0, 0, 0, 700, 52
21030, V, 0, 0, 0, 0, 0, 700, 52
21287, V, 0, 0, 0, 0, 0, 700, 52
21287, V, 0, 0, 0, 0, 0, 700, 52
21544, V, 0, 0, 0, 0, 0, 700, 52
21544, V, 0, 0, 0, 0, 0, 700, 52
21801, V, 0, 0, 0, 0, 0, 700, 52
21801, V, 0, 0, 0, 0, 0, 700, 52
22059, V, 0, 0, 0, 0, 0, 700, 52
22059, V, 0, 0, 0, 0, 0, 700, 52
22316, V, 0, 0, 0, 0, 0, 700, 52
22316, V, 0, 0, 0, 0, 0, 700, 52
22573, V, 0, 0, 0, 0, 0, 700, 52
22573, V, 0, 0, 0, 0, 0, 700, 52
22830, V, 0, 0, 0, 0, 0, 700, 52
22830, V, 0, 0, 0, 0, 0, 700, 52
23087, V, 0, 0, 0, 0, 0, 700, 52
23087, V, 0, 0, 0, 0, 0, 700, 52
23344, V, 0, 0, 0, 0, 0, 700, 52
23344, V, 0, 0, 0, 0, 0, 700, 52
23601, V, 0, 0, 0, 0, 0, 700, 52
23601, V, 0, 0, 0, 0, 0, 700, 52
23858, V, 0, 0, 0, 0, 0, 700, 52
23858, V, 0, 0, 0, 0, 0, 700, 52
24115, V, 0, 0, 0, 0, 0, 700, 52
24115, V, 0, 0, 0, 0, 0, 700, 52
24372, V, 0, 0, 0, 0, 0, 700, 52
24372, V, 0, 0, 0, 0, 0, 700, 52
24629, V, 0, 0, 0, 0, 0, 700, 52
24629, V, 0, 0, 0, 0, 0, 700, 52
24886, V, 0, 0, 0, 0, 0, 700, 52
24886, V, 0, 0, 0, 0, 0, 700, 52
25143, V, 0, 0, 0, 0, 0, 700, 52
25143, V, 0, 0, 0, 0, 0, 700, 52
25400, V, 0, 0, 0, 0, 0, 700, 52
25400, V, 0, 0, 0, 0, 0, 700, 52
25657, V, 0, 0, 0, 0, 0, 700, 52
25657, V, 0, 0, 0, 0, 0, 700, 52
25914, V, 0, 0, 0, 0, 0, 700, 52
25914, V, 0, 0, 0, 0, 0, 700, 52
26171, V, 0, 0, 0, 0, 0, 700, 52
26171, V, 0, 0, 0, 0, 0, 700, 52
26428, V, 0, 0, 0, 0, 0, 700, 52
26428, V, 0, 0, 0, 0, 0, 700, 52
26685, V, 0, 0, 0, 0, 0, 700, 52
26685, V, 0, 0, 0, 0, 0, 700, 52
26942, V, 0, 0, 0, 0, 0, 700, 52
26942, V, 0, 0, 0, 0, 0, 700, 52
27199, V, 0, 0, 0, 0, 0, 700, 52
27199, V, 0, 0, 0, 0, 0, 700, 52
27456, V, 0, 0, 0, 0, 0, 700, 52
27456, V, 0, 0, 0, 0, 0, 700, 52
27713, V, 0, 0, 0, 0, 0, 700, 52
27713, V, 0, 0, 0, 0, 0, 700, 52
27970, V, 0, 0, 0, 0, 0, 700, 52
27970, V, 0, 0, 0, 0, 0, 700, 52
28227, V, 0, 0, 0, 0, 0, 700, 52
28227, V, 0, 0, 0, 0, 0, 700, 52
28484, V, 0, 0, 0, 0, 0, 700, 52
28484, V, 0, 0, 0, 0, 0, 700, 52
28741, V, 0, 0, 0, 0, 0, 700, 52
28741, V, 0, 0, 0, 0, 0, 700, 52
28998, V, 0, 0, 0, 0, 0, 700, 52
28998, V, 0, 0, 0, 0, 0, 700, 52
29255, V, 0, 0, 0, 0, 0, 700, 52
29255, V, 0, 0, 0, 0, 0, 700, 52
29512, V, 0, 0, 0, 0, 0, 700, 52
29512, V, 0, 0, 0, 0, 0, 700, 52
29769, V, 0, 0, 0, 0, 0, 700, 52
29769, V, 0, 0, 0, 0, 0, 700, 52
30026, V, 0, 0, 0, 0, 0, 700, 52
30026, V, 0, 0, 0, 0, 0, 700, 52
30283, V, 0, 0, 0, 0, 0, 700, 52
30283, V, 0, 0, 0, 0, 0, 700, 52
30540, V, 0, 0, 0, 0, 0, 700, 52
30540, V, 0, 0, 0, 0, 0, 700, 52
30797, V, 0, 0, 0, 0, 0, 700, 52
30797, V, 0, 0, 0, 0, 0, 700, 52
31054, V, 0, 0, 0, 0, 0, 700, 52
31054, V, 0, 0, 0, 0, 0, 700, 52
31311, V, 0, 0, 0, 0, 0, 700, 52
31311, V, 0, 0, 0, 0, 0, 700, 52
31568, V, 0, 0, 0, 0, 0, 700, 52
31568, V, 0, 0, 0, 0, 0, 700, 52
31825, V, 0, 0, 0, 0, 0, 700, 52
31825, V, 0, 0, 0, 0, 0, 700, 52
32082, V, 0, 0, 0, 0, 0, 700, 52
32082, V, 0, 0, 0, 0, 0, 700, 52
32339, V, 0, 0, 0, 0, 0, 700, 52
32339, V, 0, 0, 0, 0, 0, 700, 52
32596, V, 0, 0, 0, 0, 0, 700, 52
32596, V, 0, 0, 0, 0, 0, 700, 52
32854, V, 0, 0, 0, 0, 0, 700, 52
32854, V, 0, 0, 0, 0, 0, 700, 52
33111, V, 0, 0, 0, 0, 0, 700, 52
33111, V, 0, 0, 0, 0, 0, 700, 52
33368, V, 0, 0, 0, 0, 0, 700, 52
33368, V, 0, 0, 0, 0, 0, 700, 52
33625, V, 0, 0, 0, 0, 0, 700, 52
33625, V, 0, 0, 0, 0, 0, 700, 52
33882, V, 0, 0, 0, 0, 0, 700, 52
33882, V, 0, 0, 0, 0, 0, 700, 52
34139, V, 0, 0, 0, 0, 0, 700, 52
34139, V, 0, 0, 0, 0, 0, 700, 52
34396, V, 0, 0, 0, 0, 0, 700, 52
34396, V, 0, 0, 0, 0, 0, 700, 52
34653, V, 0, 0, 0, 0, 0, 700, 52
34653, V, 0, 0, 0, 0, 0, 700, 52
34910, V, 0, 0, 0, 0, 0, 700, 52
34910, V, 0, 0, 0, 0, 0, 700, 52
35167, V, 0, 0, 0, 0, 0, 700, 52
35167, V, 0, 0, 0, 0, 0, 700, 52
35424, V, 0, 0, 0, 0, 0, 700, 52
35424, V, 0, 0, 0, 0, 0, 700, 52
35681, V, 0, 0, 0, 0, 0, 700, 52
35681, V, 0, 0, 0, 0, 0, 700, 52
35938, V, 0, 0, 0, 0, 0, 700, 52
35938, V, 0, 0, 0, 0, 0, 700, 52
36195, V, 0, 0, 0, 0, 0, 700, 52
36195, V, 0, 0, 0, 0, 0, 700, 52
36452, V, 0, 0, 0, 0, 0, 700, 52
36452, V, 0, 0, 0, 0, 0, 700, 52
36709, V, 0, 0, 0, 0, 0, 700, 52
36709, V, 0, 0, 0, 0, 0, 700, 52
36966, V, 0, 0, 0, 0, 0, 700, 52
36966, V, 0, 0, 0, 0, 0, 700, 52
37223, V, 0, 0, 0, 0, 0, 700, 52
37223, V, 0, 0, 0, 0, 0, 700, 52
37480, V, 0, 0, 0, 0, 0, 700, 52
37480, V, 0, 0, 0, 0, 0, 700, 52
37737, V, 0, 0, 0, 0, 0, 700, 52
37737, V, 0, 0, 0, 0, 0, 700, 52
37994, V, 0, 0, 0, 0, 0, 700, 52
37994, V, 0, 0, 0, 0, 0, 700, 52
38251, V, 0, 0, 0, 0, 0, 700, 52
38251, V, 0, 0, 0, 0, 0, 700, 52
38508, V, 0, 0, 0, 0, 0, 700, 52
38508, V, 0, 0, 0, 0, 0, 700, 52
38765, V, 0, 0, 0, 0, 0, 700, 52
38765, V, 0, 0, 0, 0, 0, 700, 52
39022, V, 0, 0, 0, 0, 0, 700, 52
39022, V, 0, 0, 0, 0, 0, 700, 52
39279, V, 0, 0, 0, 0, 0, 700, 52
39279, V, 0, 0, 0, 0, 0, 700, 52
39536, V, 0, 0, 0, 0, 0, 700, 52
39536, V, 0, 0, 0, 0, 0, 700, 52
39793, V, 0, 0, 0, 0, 0, 700, 52
39793, V, 0, 0, 0, 0, 0, 700, 52
40050, V, 0, 0, 0, 0, 0, 700, 52
40050, V, 0, 0, 0, 0, 0, 700, 52
40307, V, 0, 0, 0, 0, 0, 700, 52
40307, V, 0, 0, 0, 0, 0, 700, 52
40564, V, 0, 0, 0, 0, 0, 700, 52
40564, V, 0, 0, 0, 0, 0, 700, 52
40821, V, 0, 0, 0, 0, 0, 700, 52
40821, V, 0, 0, 0, 0, 0, 700, 52
41078, V, 0, 0, 0, 0, 0, 700, 52
41078, V, 0, 0, 0, 0, 0, 700, 52
41335, V, 0, 0, 0, 0, 0, 700, 52
41335, V, 0, 0, 0, 0, 0, 700, 52
41592, V, 0, 0, 0, 0, 0, 700, 52
41592, V, 0, 0, 0, 0, 0, 700, 52
41849, V, 0, 0, 0, 0, 0, 700, 52
41849, V, 0, 0, 0, 0, 0, 700, 52
42106, V, 0, 0, 0, 0, 0, 700, 52
42106, V, 0, 0, 0, 0, 0, 700, 52
42363, V, 0, 0, 0, 0, 0, 700, 52
42363, V, 0, 0, 0, 0, 0, 700, 52
42620, V, 0, 0, 0, 0, 0, 700, 52
42620, V, 0, 0, 0, 0, 0, 700, 52
42877, V, 0, 0, 0, 0, 0, 700, 52
42877, V, 0, 0, 0, 0, 0, 700, 52
43134, V, 0, 0, 0, 0, 0, 700, 52
43134, V, 0, 0, 0, 0, 0, 700, 52
43392, V, 0, 0, 0, 0, 0, 700, 52
43392, V, 0, 0, 0, 0, 0, 700, 52
43649, V, 0, 0, 0, 0, 0, 700, 52
43649, V, 0, 0, 0, 0, 0, 700, 52
43906, V, 0, 0, 0, 0, 0, 700, 52
43906, V, 0, 0, 0, 0, 0, 700, 52
44163, V, 0, 0, 0, 0, 0, 700, 52
44163, V, 0, 0, 0, 0, 0, 700, 52
44420, V, 0, 0, 0, 0, 0, 700, 52
44420, V, 0, 0, 0, 0, 0, 700, 52
44677, V, 0, 0, 0, 0, 0, 700, 52
44677, V, 0, 0, 0, 0, 0, 700, 52
44934, V, 0, 0, 0, 0, 0, 700, 52
44934, V, 0, 0, 0, 0, 0, 700, 52
45191, V, 0, 0, 0, 0, 0, 700, 52
45191, V, 0, 0, 0, 0, 0, 700, 52
45448, V, 0, 0, 0, 0, 0, 700, 52
45448, V, 0, 0, 0, 0, 0, 700, 52
45705, V, 0, 0, 0, 0, 0, 700, 52
45705, V, 0, 0, 0, 0, 0, 700, 52
45962, V, 0, 0, 0, 0, 0, 700, 52
45962, V, 0, 0, 0, 0, 0, 700, 52
46219, V, 0, 0, 0, 0, 0, 700, 52
46219, V, 0, 0, 0, 0, 0, 700, 52
46476, V, 0, 0, 0, 0, 0, 700, 52
46476, V, 0, 0, 0, 0, 0, 700, 52
46733, V, 0, 0, 0, 0, 0, 700, 52
46733, V, 0, 0, 0, 0, 0, 700, 52
46990, V, 0, 0, 0, 0, 0, 700, 52
46990, V, 0, 0, 0, 0, 0, 700, 52
47247, V, 0, 0, 0, 0, 0, 700, 52
47247, V, 0, 0, 0, 0, 0, 700, 52
47504, V, 0, 0, 0, 0, 0, 700, 52
47504, V, 0, 0, 0, 0, 0, 700, 52
47761, V, 0, 0, 0, 0, 0, 700, 52
47761, V, 0, 0, 0, 0, 0, 700, 52
48018, V, 0, 0, 0, 0, 0, 700, 52
48018, V, 0, 0, 0, 0, 0, 700, 52
48275, V, 0, 0, 0, 0, 0, 700, 52
48275, V, 0, 0, 0, 0, 0, 700, 52
48532, V, 0, 0, 0, 0, 0, 700, 52
48532, V, 0, 0, 0, 0, 0, 700, 52
48789, V, 0, 0, 0, 0, 0, 700, 52
48789, V, 0, 0, 0, 0, 0, 700, 52
49046, V, 0, 0, 0, 0, 0, 700, 52
49046, V, 0, 0, 0, 0, 0, 700, 52
49303, V, 0, 0, 0, 0, 0, 700, 52
49303, V, 0, 0, 0, 0, 0, 700, 52
49560, V, 0, 0, 0, 0, 0, 700, 52
49560, V, 0, 0, 0, 0, 0, 700, 52
49817, V, 0, 0, 0, 0, 0, 700, 52
49817, V, 0, 0, 0, 0, 0, 700, 52
50074, V, 0, 0, 0, 0, 0, 700, 52
50074, V, 0, 0, 0, 0, 0, 700, 52
50331, V, 0, 0, 0, 0, 0, 700, 52
50331, V, 0, 0, 0, 0, 0, 700, 52
50588, V, 0, 0, 0, 0, 0, 700, 52
50588, V, 0, 0, 0, 0, 0, 700, 52
50845, V, 0, 0, 0, 0, 0, 700, 52
50845, V, 0, 0, 0, 0, 0, 700, 52
51102, V, 0, 0, 0, 0, 0, 700, 52
51102, V, 0, 0, 0, 0, 0, 700, 52
51359, V, 0, 0, 0, 0, 0, 700, 52
51359, V, 0, 0, 0, 0, 0, 700, 52
51616, V, 0, 0, 0, 0, 0, 700, 52
51616, V, 0, 0, 0, 0, 0, 700, 52
51873, V, 0, 0, 0, 0, 0, 700, 52
51873, V, 0, 0, 0, 0, 0, 700, 52
52130, V, 0, 0, 0, 0, 0, 700, 52
52130, V, 0, 0, 0, 0, 0, 700, 52
52387, V, 0, 0, 0, 0, 0, 700, 52
52387, V, 0, 0, 0, 0, 0, 700, 52
52644, V, 0, 0, 0, 0, 0, 700, 52
52644, V, 0, 0, 0, 0, 0, 700, 52
52901, V, 0, 0, 0, 0, 0, 700, 52
52901, V, 0, 0, 0, 0, 0, 700, 52
53158, V, 0, 0, 0, 0, 0, 700, 52
53158, V, 0, 0, 0, 0, 0, 700, 52
53415, V, 0, 0, 0, 0, 0, 700, 52
53415, V, 0, 0, 0, 0, 0, 700, 52
53672, V, 0, 0, 0, 0, 0, 700, 52
53672, V, 0, 0, 0, 0, 0, 700, 52
53929, V, 0, 0, 0, 0, 0, 700, 52
53929, V, 0, 0, 0, 0, 0, 700, 52
54187, V, 0, 0, 0, 0, 0, 700, 52
54187, V, 0, 0, 0, 0, 0, 700, 52
54444, V, 0, 0, 0, 0, 0, 700, 52
54444, V, 0, 0, 0, 0, 0, 700, 52
54701, V, 0, 0, 0, 0, 0, 700, 52
54701, V, 0, 0, 0, 0, 0, 700, 52
54958, V, 0, 0, 0, 0, 0, 700, 52
54958, V, 0, 0, 0, 0, 0, 700, 52
55215, V, 0, 0, 0, 0, 0, 700, 52
55215, V, 0, 0, 0, 0, 0, 700, 52
55472, V, 0, 0, 0, 0, 0, 700, 52
55472, V, 0, 0, 0, 0, 0, 700, 52
55729, V, 0, 0, 0, 0, 0, 700, 52
55729, V, 0, 0, 0, 0, 0, 700, 52
55986, V, 0, 0, 0, 0, 0, 700, 52
55986, V, 0, 0, 0, 0, 0, 700, 52
56243, V, 0, 0, 0, 0, 0, 700, 52
56243, V, 0, 0, 0, 0, 0, 700, 52
56500, V, 0, 0, 0, 0, 0, 700, 52
56500, V, 0, 0, 0, 0, 0, 700, 52
56757, V, 0, 0, 0, 0, 0, 700, 52
56757, V, 0, 0, 0, 0, 0, 700, 52
57014, V, 0, 0, 0, 0, 0, 700, 52
57014, V, 0, 0, 0, 0, 0, 700, 52
57271, V, 0, 0, 0, 0, 0, 700, 52
57271, V, 0, 0, 0, 0, 0, 700, 52
57528, V, 0, 0, 0, 0, 0, 700, 52
57528, V, 0, 0, 0, 0, 0, 700, 52
57785, V, 0, 0, 0, 0, 0, 700, 52
57785, V, 0, 0, 0, 0, 0, 700, 52
58042, V, 0, 0, 0, 0, 0, 700, 52
58042, V, 0, 0, 0, 0, 0, 700, 52
58299, V, 0, 0, 0, 0, 0, 700, 52
58299, V, 0, 0, 0, 0, 0, 700, 52
58556, V, 0, 0, 0, 0, 0, 700, 52
58556, V, 0, 0, 0, 0, 0, 700, 52
58813, V, 0, 0, 0, 0, 0, 700, 52
58813, V, 0, 0, 0, 0, 0, 700, 52
59070, V, 0, 0, 0, 0, 0, 700, 52
59070, V, 0, 0, 0, 0, 0, 700, 52
59327, V, 0, 0, 0, 0, 0, 700, 52
59327, V, 0, 0, 0, 0, 0, 700, 52
59584, V, 0, 0, 0, 0, 0, 700, 52
59584, V, 0, 0, 0, 0, 0, 700, 52
59841, V, 0, 0, 0, 0, 0, 700, 52
59841, V, 0, 0, 0, 0, 0, 700, 52
60098, V, 0, 0, 0, 0, 0, 700, 52
60098, V, 0, 0, 0, 0, 0, 700, 52
60355, V, 0, 0, 0, 0, 0, 700, 52
60355, V, 0, 0, 0, 0, 0, 700, 52
60612, V, 0, 0, 0, 0, 0, 700, 52
60612, V, 0, 0, 0, 0, 0, 700, 52
60869, V, 0, 0, 0, 0, 0, 700, 52
60869, V, 0, 0, 0, 0, 0, 700, 52
61126, V, 0, 0, 0, 0, 0, 700, 52
61126, V, 0, 0, 0, 0, 0, 700, 52
61383, V, 0, 0, 0, 0, 0, 700, 52
61383, V, 0, 0, 0, 0, 0, 700, 52
61640, V, 0, 0, 0, 0, 0, 700, 52
61640, V, 0, 0, 0, 0, 0, 700, 52
61897, V, 0, 0, 0, 0, 0, 700, 52
61897, V, 0, 0, 0, 0, 0, 700, 52
62154, V, 0, 0, 0, 0, 0, 700, 52
62154, V, 0, 0, 0, 0, 0, 700, 52
62411, V, 0, 0, 0, 0, 0, 700, 52
62411, V, 0, 0, 0, 0, 0, 700, 52
62668, V, 0, 0, 0, 0, 0, 700, 52
62668, V, 0, 0, 0, 0, 0, 700, 52
62925, V, 0, 0, 0, 0, 0, 700, 52
62925, V, 0, 0, 0, 0, 0, 700, 52
63182, V, 0, 0, 0, 0, 0, 700, 52
63182, V, 0, 0, 0, 0, 0, 700, 52
63439, V, 0, 0, 0, 0, 0, 700, 52
63439, V, 0, 0, 0, 0, 0, 700, 52
63696, V, 0, 0, 0, 0, 0, 700, 52
63696, V, 0, 0, 0, 0, 0, 700, 52
63953, V, 0, 0, 0, 0, 0, 700, 52
63953, V, 0, 0, 0, 0, 0, 700, 52
64210, V, 0, 0, 0, 0, 0, 700, 52
64210, V, 0, 0, 0, 0, 0, 700, 52
64467, V, 0, 0, 0, 0, 0, 700, 52
64467, V, 0, 0, 0, 0, 0, 700, 52
64724, V, 0, 0, 0, 0, 0, 700, 52
64724, V, 0, 0, 0, 0, 0, 700, 52
64982, V, 0, 0, 0, 0, 0, 700, 52
64982, V, 0, 0, 0, 0, 0, 700, 52
65239, V, 0, 0, 0, 0, 0, 700, 52
65239, V, 0, 0, 0, 0, 0, 700, 52
65496, V, 0, 0, 0, 0, 0, 700, 52
65496, V, 0, 0, 0, 0, 0, 700, 52
217, V, 0, 0, 0, 0, 0, 700, 52
217, V, 0, 0, 0, 0, 0, 700, 52
474, V, 0, 0, 0, 0, 0, 700, 52
474, V, 0, 0, 0, 0, 0, 700, 52
731, V, 0, 0, 0, 0, 0, 700, 52
731, V, 0, 0, 0, 0, 0, 700, 52
988, V, 0, 0, 0, 0, 0, 700, 52
988, V, 0, 0, 0, 0, 0, 700, 52
1245, V, 0, 0, 0, 0, 0, 700, 52
1245, V, 0, 0, 0, 0, 0, 700, 52
1502, V, 0, 0, 0, 0, 0, 700, 52
1502, V, 0, 0, 0, 0, 0, 700, 52
1759, V, 0, 0, 0, 0, 0, 700, 52
1759, V, 0, 0, 0, 0, 0, 700, 52
2016, V, 0, 0, 0, 0, 0, 700, 52
2016, V, 0, 0, 0, 0, 0, 700, 52
2273, V, 0, 0, 0, 0, 0, 700, 52
2273, V, 0, 0, 0, 0, 0, 700, 52
2530, V, 0, 0, 0, 0, 0, 700, 52
2530, V, 0, 0, 0, 0, 0, 700, 52
2787, V, 0, 0, 0, 0, 0, 700, 52
2787, V, 0, 0, 0, 0, 0, 700, 52
3044, V, 0, 0, 0, 0, 0, 700, 52
3044, V, 0, 0, 0, 0, 0, 700, 52
3301, V, 0, 0, 0, 0, 0, 700, 52
3301, V, 0, 0, 0, 0, 0, 700, 52
3558, V, 0, 0, 0, 0, 0, 700, 52
3558, V, 0, 0, 0, 0, 0, 700, 52
3815, V, 0, 0, 0, 0, 0, 700, 52
3815, V, 0, 0, 0, 0, 0, 700, 52
4072, V, 0, 0, 0, 0, 0, 700, 52
4072, V, 0, 0, 0, 0, 0, 700, 52
4329, V, 0, 0, 0, 0, 0, 700, 52
4329, V, 0, 0, 0, 0, 0, 700, 52
4586, V, 0, 0, 0, 0, 0, 700, 52
4586, V, 0, 0, 0, 0, 0, 700, 52
4843, V, 0, 0, 0, 0, 0, 700, 52
4843, V, 0, 0, 0, 0, 0, 700, 52
5100, V, 0, 0, 0, 0, 0, 700, 52
5100, V, 0, 0, 0, 0, 0, 700, 52
5357, V, 0, 0, 0, 0, 0, 700, 52
5357, V, 0, 0, 0, 0, 0, 700, 52
5614, V, 0, 0, 0, 0, 0, 700, 52
5614, V, 0, 0, 0, 0, 0, 700, 52
5871, V, 0, 0, 0, 0, 0, 700, 52
5871, V, 0, 0, 0, 0, 0, 700, 52
6128, V, 0, 0, 0, 0, 0, 700, 52
6128, V, 0, 0, 0, 0, 0, 700, 52
6385, V, 0, 0, 0, 0, 0, 700, 52
6385, V, 0, 0, 0, 0, 0, 700, 52
6642, V, 0, 0, 0, 0, 0, 700, 52
6642, V, 0, 0, 0, 0, 0, 700, 52
6899, V, 0, 0, 0, 0, 0, 700, 52
6899, V, 0, 0, 0, 0, 0, 700, 52
7156, V, 0, 0, 0, 0, 0, 700, 52
7156, V, 0, 0, 0, 0, 0, 700, 52
7413, V, 0, 0, 0, 0, 0, 700, 52
7413, V, 0, 0, 0, 0, 0, 700, 52
7670, V, 0, 0, 0, 0, 0, 700, 52
7670, V, 0, 0, 0, 0, 0, 700, 52
7927, V, 0, 0, 0, 0, 0, 700, 52
7927, V, 0, 0, 0, 0, 0, 700, 52
8184, V, 0, 0, 0, 0, 0, 700, 52
8184, V, 0, 0, 0, 0, 0, 700, 52
8441, V, 0, 0, 0, 0, 0, 700, 52
8441, V, 0, 0, 0, 0, 0, 700, 52
8698, V, 0, 0, 0, 0, 0, 700, 52
8698, V, 0, 0, 0, 0, 0, 700, 52
8955, V, 0, 0, 0, 0, 0, 700, 52
8955, V, 0, 0, 0, 0, 0, 700, 52
9212, V, 0, 0, 0, 0, 0, 700, 52
9212, V, 0, 0, 0, 0, 0, 700, 52
9469, V, 0, 0, 0, 0, 0, 700, 52
9469, V, 0, 0, 0, 0, 0, 700, 52
9726, V, 0, 0, 0, 0, 0, 700, 52
9726, V, 0, 0, 0, 0, 0, 700, 52
9984, V, 0, 0, 0, 0, 0, 700, 52
9984, V, 0, 0, 0, 0, 0, 700, 52
10241, V, 0, 0, 0, 0, 0, 700, 52
10241, V, 0, 0, 0, 0, 0, 700, 52
10498, V, 0, 0, 0, 0, 0, 700, 52
10498, V, 0, 0, 0, 0, 0, 700, 52
10755, V, 0, 0, 0, 0, 0, 700, 52
10755, V, 0, 0, 0, 0, 0, 700, 52
11012, V, 0, 0, 0, 0, 0, 700, 52
11012, V, 0, 0, 0, 0, 0, 700, 52
11269, V, 0, 0, 0, 0, 0, 700, 52
11269, V, 0, 0, 0, 0, 0, 700, 52
11526, V, 0, 0, 0, 0, 0, 700, 52
11526, V, 0, 0, 0, 0, 0, 700, 52
11783, V, 0, 0, 0, 0, 0, 700, 52
11783, V, 0, 0, 0, 0, 0, 700, 52
12040, V, 0, 0, 0, 0, 0, 700, 52
12040, V, 0, 0, 0, 0, 0, 700, 52
12297, V, 0, 0, 0, 0, 0, 700, 52
12297, V, 0, 0, 0, 0, 0, 700, 52
12554, V, 0, 0, 0, 0, 0, 700, 52
12554, V, 0, 0, 0, 0, 0, 700, 52
12811, V, 0, 0, 0, 0, 0, 700, 52
12811, V, 0, 0, 0, 0, 0, 700, 52
13068, V, 0, 0, 0, 0, 0, 700, 52
13068, V, 0, 0, 0, 0, 0, 700, 52
13325, V, 0, 0, 0, 0, 0, 700, 52
13325, V, 0, 0, 0, 0, 0, 700, 52
13582, V, 0, 0, 0, 0, 0, 700, 52
13582, V, 0, 0, 0, 0, 0, 700, 52
13839, V, 0, 0, 0, 0, 0, 700, 52
13839, V, 0, 0, 0, 0, 0, 700, 52
14096, V, 0, 0, 0, 0, 0, 700, 52
14096, V, 0, 0, 0, 0, 0, 700, 52
14353, V, 0, 0, 0, 0, 0, 700, 52
14353, V, 0, 0, 0, 0, 0, 700, 52
14610, V, 0, 0, 0, 0, 0, 700, 52
14610, V, 0, 0, 0, 0, 0, 700, 52
14867, V, 0, 0, 0, 0, 0, 700, 52
14867, V, 0, 0, 0, 0, 0, 700, 52
15124, V, 0, 0, 0, 0, 0, 700, 52
15124, V, 0, 0, 0, 0, 0, 700, 52
15381, V, 0, 0, 0, 0, 0, 700, 52
15381, V, 0, 0, 0, 0, 0, 700, 52
15638, V, 0, 0, 0, 0, 0, 700, 52
15638, V, 0, 0, 0, 0, 0, 700, 52
15895, V, 0, 0, 0, 0, 0, 700, 52
15895, V, 0, 0, 0, 0, 0, 700, 52
16152, V, 0, 0, 0, 0, 0, 700, 52
16152, V, 0, 0, 0, 0, 0, 700, 52
16409, V, 0, 0, 0, 0, 0, 700, 52
16409, V, 0, 0, 0, 0, 0, 700, 52
16666, V, 0, 0, 0, 0, 0, 700, 52
16666, V, 0, 0, 0, 0, 0, 700, 52
16923, V, 0, 0, 0, 0, 0, 700, 52
16923, V, 0, 0, 0, 0, 0, 700, 52
17180, V, 0, 0, 0, 0, 0, 700, 52
17180, V, 0, 0, 0, 0, 0, 700, 52
17437, V, 0, 0, 0, 0, 0, 700, 52
17437, V, 0, 0, 0, 0, 0, 700, 52
17694, V, 0, 0, 0, 0, 0, 700, 52
17694, V, 0, 0, 0, 0, 0, 700, 52
17951, V, 0, 0, 0, 0, 0, 700, 52
17951, V, 0, 0, 0, 0, 0, 700, 52
18208, V, 0, 0, 0, 0, 0, 700, 52
18208, V, 0, 0, 0, 0, 0, 700, 52
18465, V, 0, 0, 0, 0, 0, 700, 52
18465, V, 0, 0, 0, 0, 0, 700, 52
18722, V, 0, 0, 0, 0, 0, 700, 52
18722, V, 0, 0, 0, 0, 0, 700, 52
18979, V, 0, 0, 0, 0, 0, 700, 52
18979, V, 0, 0, 0, 0, 0, 700, 52
19236, V, 0, 0, 0, 0, 0, 700, 52
19236, V, 0, 0, 0, 0, 0, 700, 52
19493, V, 0, 0, 0, 0, 0, 700, 52
19493, V, 0, 0, 0, 0, 0, 700, 52
19750, V, 0, 0, 0, 0, 0, 700, 52
19750, V, 0, 0, 0, 0, 0, 700, 52
20007, V, 0, 0, 0, 0, 0, 700, 52
20007, V, 0, 0, 0, 0, 0, 700, 52
20264, V, 0, 0, 0, 0, 0, 700, 52
20264, V, 0, 0, 0, 0, 0, 700, 52
20521, V, 0, 0, 0, 0, 0, 700, 52
20521, V, 0, 0, 0, 0, 0, 700, 52
20779, V, 0, 0, 0, 0, 0, 700, 52
20779, V, 0, 0, 0, 0, 0, 700, 52
21036, V, 0, 0, 0, 0, 0, 700, 52
21036, V, 0, 0, 0, 0, 0, 700, 52
21293, V, 0, 0, 0, 0, 0, 700, 52
21293, V, 0, 0, 0, 0, 0, 700, 52
21550, V, 0, 0, 0, 0, 0, 700, 52
21550, V, 0, 0, 0, 0, 0, 700, 52
21807, V, 0, 0, 0, 0, 0, 700, 52
21807, V, 0, 0, 0, 0, 0, 700, 52
22064, V, 0, 0, 0, 0, 0, 700, 52
22064, V, 0, 0, 0, 0, 0, 700, 52
22321, V, 0, 0, 0, 0, 0, 700, 52
22321, V, 0, 0, 0, 0, 0, 700, 52
22578, V, 0, 0, 0, 0, 0, 700, 52
22578, V, 0, 0, 0, 0, 0, 700, 52
22835, V, 0, 0, 0, 0, 0, 700, 52
22835, V, 0, 0, 0, 0, 0, 700, 52
23092, V, 0, 0, 0, 0, 0, 700, 52
23092, V, 0, 0, 0, 0, 0, 700, 52
23349, V, 0, 0, 0, 0, 0, 700, 52
23349, V, 0, 0, 0, 0, 0, 700, 52
23606, V, 0, 0, 0, 0, 0, 700, 52
23606, V, 0, 0, 0, 0, 0, 700, 52
23863, V, 0, 0, 0, 0, 0, 700, 52
23863, V, 0, 0, 0, 0, 0, 700, 52
24120, V, 0, 0, 0, 0, 0, 700, 52
24120, V, 0, 0, 0, 0, 0, 700, 52
24377, V, 0, 0, 0, 0, 0, 700, 52
24377, V, 0, 0, 0, 0, 0, 700, 52
24634, V, 0, 0, 0, 0, 0, 700, 52
24634, V, 0, 0, 0, 0, 0, 700, 52
24891, V, 0, 0, 0, 0, 0, 700, 52
24891, V, 0, 0, 0, 0, 0, 700, 52
25148, V, 0, 0, 0, 0, 0, 700, 52
25148, V, 0, 0, 0, 0, 0, 700, 52
25405, V, 0, 0, 0, 0, 0, 700, 52
25405, V, 0, 0, 0, 0, 0, 700, 52
25662, V, 0, 0, 0, 0, 0, 700, 52
25662, V, 0, 0, 0, 0, 0, 700, 52
25919, V, 0, 0, 0, 0, 0, 700, 52
25919, V, 0, 0, 0, 0, 0, 700, 52
26176, V, 0, 0, 0, 0, 0, 700, 52
26176, V, 0, 0, 0, 0, 0, 700, 52
26433, V, 0, 0, 0, 0, 0, 700, 52
26433, V, 0, 0, 0, 0, 0, 700, 52
26690, V, 0, 0, 0, 0, 0, 700, 52
26690, V, 0, 0, 0, 0, 0, 700, 52
26947, V, 0, 0, 0, 0, 0, 700, 52
26947, V, 0, 0, 0, 0, 0, 700, 52
27204, V, 0, 0, 0, 0, 0, 700, 52
27204, V, 0, 0, 0, 0, 0, 700, 52
27461, V, 0, 0, 0, 0, 0, 700, 52
27461, V, 0, 0, 0, 0, 0, 700, 52
27718, V, 0, 0, 0, 0, 0, 700, 52
27718, V, 0, 0, 0, 0, 0, 700, 52
27975, V, 0, 0, 0, 0, 0, 700, 52
27975, V, 0, 0, 0, 0, 0, 700, 52
28232, V, 0, 0, 0, 0, 0, 700, 52
28232, V, 0, 0, 0, 0, 0, 700, 52
28489, V, 0, 0, 0, 0, 0, 700, 52
28489, V, 0, 0, 0, 0, 0, 700, 52
28746, V, 0, 0, 0, 0, 0, 700, 52
28746, V, 0, 0, 0, 0, 0, 700, 52
29003, V, 0, 0, 0, 0, 0, 700, 52
29003, V, 0, 0, 0, 0, 0, 700, 52
29260, V, 0, 0, 0, 0, 0, 700, 52
29260, V, 0, 0, 0, 0, 0, 700, 52
29517, V, 0, 0, 0, 0, 0, 700, 52
29517, V, 0, 0, 0, 0, 0, 700, 52
29774, V, 0, 0, 0, 0, 0, 700, 52
29774, V, 0, 0, 0, 0, 0, 700, 52
30031, V, 0, 0, 0, 0, 0, 700, 52
30031, V, 0, 0, 0, 0, 0, 700, 52
30288, V, 0, 0, 0, 0, 0, 700, 52
30288, V, 0, 0, 0, 0, 0, 700, 52
30545, V, 0, 0, 0, 0, 0, 700, 52
30545, V, 0, 0, 0, 0, 0, 700, 52
30802, V, 0, 0, 0, 0, 0, 700, 52
30802, V, 0, 0, 0, 0, 0, 700, 52
31059, V, 0, 0, 0, 0, 0, 700, 52
31059, V, 0, 0, 0, 0, 0, 700, 52
31316, V, 0, 0, 0, 0, 0, 700, 52
31316, V, 0, 0, 0, 0, 0, 700, 52
31574, V, 0, 0, 0, 0, 0, 700, 52
31574, V, 0, 0, 0, 0, 0, 700, 52
31831, V, 0, 0, 0, 0, 0, 700, 52
31831, V, 0, 0, 0, 0, 0, 700, 52
32088, V, 0, 0, 0, 0, 0, 700, 52
32088, V, 0, 0, 0, 0, 0, 700, 52
32345, V, 0, 0, 0, 0, 0, 700, 52
32345, V, 0, 0, 0, 0, 0, 700, 52
32602, V, 0, 0, 0, 0, 0, 700, 52
32602, V, 0, 0, 0, 0, 0, 700, 52
32859, V, 0, 0, 0, 0, 0, 700, 52
32859, V, 0, 0, 0, 0, 0, 700, 52
33116, V, 0, 0, 0, 0, 0, 700, 52
33116, V, 0, 0, 0, 0, 0, 700, 52
33373, V, 0, 0, 0, 0, 0, 700, 52
33373, V, 0, 0, 0, 0, 0, 700, 52
33630, V, 0, 0, 0, 0, 0, 700, 52
33630, V, 0, 0, 0, 0, 0, 700, 52
33887, V, 0, 0, 0, 0, 0, 700, 52
33887, V, 0, 0, 0, 0, 0, 700, 52
34144, V, 0, 0, 0, 0, 0, 700, 52
34144, V, 0, 0, 0, 0, 0, 700, 52
34401, V, 0, 0, 0, 0, 0, 700, 52
34401, V, 0, 0, 0, 0, 0, 700, 52
34658, V, 0, 0, 0, 0, 0, 700, 52
34658, V, 0, 0, 0, 0, 0, 700, 52
34915, V, 0, 0, 0, 0, 0, 700, 52
34915, V, 0, 0, 0, 0, 0, 700, 52
35172, V, 0, 0, 0, 0, 0, 700, 52
35172, V, 0, 0, 0, 0, 0, 700, 52
35429, V, 0, 0, 0, 0, 0, 700, 52
35429, V, 0, 0, 0, 0, 0, 700, 52
35686, V, 0, 0, 0, 0, 0, 700, 52
35686, V, 0, 0, 0, 0, 0, 700, 52
35943, V, 0, 0, 0, 0, 0, 700, 52
35943, V, 0, 0, 0, 0, 0, 700, 52
36200, V, 0, 0, 0, 0, 0, 700, 52
36200, V, 0, 0, 0, 0, 0, 700, 52
36457, V, 0, 0, 0, 0, 0, 700, 52
36457, V, 0, 0, 0, 0, 0, 700, 52
36714, V, 0, 0, 0, 0, 0, 700, 52
36714, V, 0, 0, 0, 0, 0, 700, 52
36971, V, 0, 0, 0, 0, 0, 700, 52
36971, V, 0, 0, 0, 0, 0, 700, 52
37228, V, 0, 0, 0, 0, 0, 700, 52
37228, V, 0, 0, 0, 0, 0, 700, 52
37485, V, 0, 0, 0, 0, 0, 700, 52
37485, V, 0, 0, 0, 0, 0, 700, 52
37742, V, 0, 0, 0, 0, 0, 700, 52
37742, V, 0, 0, 0, 0, 0, 700, 52
37999, V, 0, 0, 0, 0, 0, 700, 52
37999, V, 0, 0, 0, 0, 0, 700, 52
38256, V, 0, 0, 0, 0, 0, 700, 52
38256, V, 0, 0, 0, 0, 0, 700, 52
38513, V, 0, 0, 0, 0, 0, 700, 52
38513, V, 0, 0, 0, 0, 0, 700, 52
38770, V, 0, 0, 0, 0, 0, 700, 52
38770, V, 0, 0, 0, 0, 0, 700, 52
39027, V, 0, 0, 0, 0, 0, 700, 52
39027, V, 0, 0, 0, 0, 0, 700, 52
39284, V, 0, 0, 0, 0, 0, 700, 52
39284, V, 0, 0, 0, 0, 0, 700, 52
39541, V, 0, 0, 0, 0, 0, 700, 52
39541, V, 0, 0, 0, 0, 0, 700, 52
39798, V, 0, 0, 0, 0, 0, 700, 52
39798, V, 0, 0, 0, 0, 0, 700, 52
40055, V, 0, 0, 0, 0, 0, 700, 52
40055, V, 0, 0, 0, 0, 0, 700, 52
40312, V, 0, 0, 0, 0, 0, 700, 52
40312, V, 0, 0, 0, 0, 0, 700, 52
40569, V, 0, 0, 0, 0, 0, 700, 52
40569, V, 0, 0, 0, 0, 0, 700, 52
40826, V, 0, 0, 0, 0, 0, 700, 52
40826, V, 0, 0, 0, 0, 0, 700, 52
41083, V, 0, 0, 0, 0, 0, 700, 52
41083, V, 0, 0, 0, 0, 0, 700, 52
41340, V, 0, 0, 0, 0, 0, 700, 52
41340, V, 0, 0, 0, 0, 0, 700, 52
41597, V, 0, 0, 0, 0, 0, 700, 52
41597, V, 0, 0, 0, 0, 0, 700, 52
41854, V, 0, 0, 0, 0, 0, 700, 52
41854, V, 0, 0, 0, 0, 0, 700, 52
42112, V, 0, 0, 0, 0, 0, 700, 52
42112, V, 0, 0, 0, 0, 0, 700, 52
42369, V, 0, 0, 0, 0, 0, 700, 52
42369, V, 0, 0, 0, 0, 0, 700, 52
42626, V, 0, 0, 0, 0, 0, 700, 52
42626, V, 0, 0, 0, 0, 0, 700, 52
42883, V, 0, 0, 0, 0, 0, 700, 52
42883, V, 0, 0, 0, 0, 0, 700, 52
43140, V, 0, 0, 0, 0, 0, 700, 52
43140, V, 0, 0, 0, 0, 0, 700, 52
43397, V, 0, 0, 0, 0, 0, 700, 52
43397, V, 0, 0, 0, 0, 0, 700, 52
43654, V, 0, 0, 0, 0, 0, 700, 52
43654, V, 0, 0, 0, 0, 0, 700, 52
43911, V, 0, 0, 0, 0, 0, 700, 52
43911, V, 0, 0, 0, 0, 0, 700, 52
44168, V, 0, 0, 0, 0, 0, 700, 52
44168, V, 0, 0, 0, 0, 0, 700, 52
44425, V, 0, 0, 0, 0, 0, 700, 52
44425, V, 0, 0, 0, 0, 0, 700, 52
44682, V, 0, 0, 0, 0, 0, 700, 52
44682, V, 0, 0, 0, 0, 0, 700, 52
44939, V, 0, 0, 0, 0, 0, 700, 52
44939, V, 0, 0, 0, 0, 0, 700, 52
45196, V, 0, 0, 0, 0, 0, 700, 52
45196, V, 0, 0, 0, 0, 0, 700, 52
45453, V, 0, 0, 0, 0, 0, 700, 52
45453, V, 0, 0, 0, 0, 0, 700, 52
45710, V, 0, 0, 0, 0, 0, 700, 52
45710, V, 0, 0, 0, 0, 0, 700, 52
45967, V, 0, 0, 0, 0, 0, 700, 52
45967, V, 0, 0, 0, 0, 0, 700, 52
46224, V, 0, 0, 0, 0, 0, 700, 52
46224, V, 0, 0, 0, 0, 0, 700, 52
46481, V, 0, 0, 0, 0, 0, 700, 52
46481, V, 0, 0, 0, 0, 0, 700, 52
46738, V, 0, 0, 0, 0, 0, 700, 52
46738, V, 0, 0, 0, 0, 0, 700, 52
46995, V, 0, 0, 0, 0, 0, 700, 52
46995, V, 0, 0, 0, 0, 0, 700, 52
47252, V, 0, 0, 0, 0, 0, 700, 52
47252, V, 0, 0, 0, 0, 0, 700, 52
47509, V, 0, 0, 0, 0, 0, 700, 52
47509, V, 0, 0, 0, 0, 0, 700, 52
47766, V, 0, 0, 0, 0, 0, 700, 52
47766, V, 0, 0, 0, 0, 0, 700, 52
48023, V, 0, 0, 0, 0, 0, 700, 52
48023, V, 0, 0, 0, 0, 0, 700, 52
48280, V, 0, 0, 0, 0, 0, 700, 52
48280, V, 0, 0, 0, 0, 0, 700, 52
48537, V, 0, 0, 0, 0, 0, 700, 52
48537, V, 0, 0, 0, 0, 0, 700, 52
48794, V, 0, 0, 0, 0, 0, 700, 52
48794, V, 0, 0, 0, 0, 0, 700, 52
49051, V, 0, 0, 0, 0, 0, 700, 52
49051, V, 0, 0, 0, 0, 0, 700, 52
49308, V, 0, 0, 0, 0, 0, 700, 52
49308, V, 0, 0, 0, 0, 0, 700, 52
49565, V, 0, 0, 0, 0, 0, 700, 52
49565, V, 0, 0, 0, 0, 0, 700, 52
49822, V, 0, 0, 0, 0, 0, 700, 52
49822, V, 0, 0, 0, 0, 0, 700, 52
50079, V, 0, 0, 0, 0, 0, 700, 52
50079, V, 0, 0, 0, 0, 0, 700, 52
50336, V, 0, 0, 0, 0, 0, 700, 52
50336, V, 0, 0, 0, 0, 0, 700, 52
50593, V, 0, 0, 0, 0, 0, 700, 52
50593, V, 0, 0, 0, 0, 0, 700, 52
50850, V, 0, 0, 0, 0, 0, 700, 52
50850, V, 0, 0, 0, 0, 0, 700, 52
51107, V, 0, 0, 0, 0, 0, 700, 52
51107, V, 0, 0, 0, 0, 0, 700, 52
51364, V, 0, 0, 0, 0, 0, 700, 52
51364, V, 0, 0, 0, 0, 0, 700, 52
51621, V, 0, 0, 0, 0, 0, 700, 52
51621, V, 0, 0, 0, 0, 0, 700, 52
51878, V, 0, 0, 0, 0, 0, 700, 52
51878, V, 0, 0, 0, 0, 0, 700, 52
52135, V, 0, 0, 0, 0, 0, 700, 52
52135, V, 0, 0, 0, 0, 0, 700, 52
52392, V, 0, 0, 0, 0, 0, 700, 52
52392, V, 0, 0, 0, 0, 0, 700, 52
52649, V, 0, 0, 0, 0, 0, 700, 52
52649, V, 0, 0, 0, 0, 0, 700, 52
52907, V, 0, 0, 0, 0, 0, 700, 52
52907, V, 0, 0, 0, 0, 0, 700, 52
53164, V, 0, 0, 0, 0, 0, 700, 52
53164, V, 0, 0, 0, 0, 0, 700, 52
53421, V, 0, 0, 0, 0, 0, 700, 52
53421, V, 0, 0, 0, 0, 0, 700, 52
53678, V, 0, 0, 0, 0, 0, 700, 52
53678, V, 0, 0, 0, 0, 0, 700, 52
53935, V, 0, 0, 0, 0, 0, 700, 52
53935, V, 0, 0, 0, 0, 0, 700, 52
54192, V, 0, 0, 0, 0, 0, 700, 52
54192, V, 0, 0, 0, 0, 0, 700, 52
54449, V, 0, 0, 0, 0, 0, 700, 52
54449, V, 0, 0, 0, 0, 0, 700, 52
54706, V, 0, 0, 0, 0, 0, 700, 52
54706, V, 0, 0, 0, 0, 0, 700, 52
54963, V, 0, 0, 0, 0, 0, 700, 52
54963, V, 0, 0, 0, 0, 0, 700, 52
55220, V, 0, 0, 0, 0, 0, 700, 52
55220, V, 0, 0, 0, 0, 0, 700, 52
55477, V, 0, 0, 0, 0, 0, 700, 52
55477, V, 0, 0, 0, 0, 0, 700, 52
55734, V, 0, 0, 0, 0, 0, 700, 52
55734, V, 0, 0, 0, 0, 0, 700, 52
55991, V, 0, 0, 0, 0, 0, 700, 52
55991, V, 0, 0, 0, 0, 0, 700, 52
56248, V, 0, 0, 0, 0, 0, 700, 52
56248, V, 0, 0, 0, 0, 0, 700, 52
56505, V, 0, 0, 0, 0, 0, 700, 52
56505, V, 0, 0, 0, 0, 0, 700, 52
56762, V, 0, 0, 0, 0, 0, 700, 52
56762, V, 0, 0, 0, 0, 0, 700, 52
57019, V, 0, 0, 0, 0, 0, 700, 52
57019, V, 0, 0, 0, 0, 0, 700, 52
57276, V, 0, 0, 0, 0, 0, 700, 52
57276, V, 0, 0, 0, 0, 0, 700, 52
57533, V, 0, 0, 0, 0, 0, 700, 52
57533, V, 0, 0, 0, 0, 0, 700, 52
57790, V, 0, 0, 0, 0, 0, 700, 52
57790, V, 0, 0, 0, 0, 0, 700, 52
58047, V, 0, 0, 0, 0, 0, 700, 52
58047, V, 0, 0, 0, 0, 0, 700, 52
58304, V, 0, 0, 0, 0, 0, 700, 52
58304, V, 0, 0, 0, 0, 0, 700, 52
58561, V, 0, 0, 0, 0, 0, 700, 52
58561, V, 0, 0, 0, 0, 0, 700, 52
58818, V, 0, 0, 0, 0, 0, 700, 52
58818, V, 0, 0, 0, 0, 0, 700, 52
59075, V, 0, 0, 0, 0, 0, 700, 52
59075, V, 0, 0, 0, 0, 0, 700, 52
59332, V, 0, 0, 0, 0, 0, 700, 52
59332, V, 0, 0, 0, 0, 0, 700, 52
59589, V, 0, 0, 0, 0, 0, 700, 52
59589, V, 0, 0, 0, 0, 0, 700, 52
59846, V, 0, 0, 0, 0, 0, 700, 52
59846, V, 0, 0, 0, 0, 0, 700, 52
60103, V, 0, 0, 0, 0, 0, 700, 52
60103, V, 0, 0, 0, 0, 0, 700, 52
60360, V, 0, 0, 0, 0, 0, 700, 52
60360, V, 0, 0, 0, 0, 0, 700, 52
60617, V, 0, 0, 0, 0, 0, 700, 52
60617, V, 0, 0, 0, 0, 0, 700, 52
60874, V, 0, 0, 0, 0, 0, 700, 52
60874, V, 0, 0, 0, 0, 0, 700, 52
61131, V, 0, 0, 0, 0, 0, 700, 52
61131, V, 0, 0, 0, 0, 0, 700, 52
61388, V, 0, 0, 0, 0, 0, 700, 52
61388, V, 0, 0, 0, 0, 0, 700, 52
61645, V, 0, 0, 0, 0, 0, 700, 52
61645, V, 0, 0, 0, 0, 0, 700, 52
61902, V, 0, 0, 0, 0, 0, 700, 52
61902, V, 0, 0, 0, 0, 0, 700, 52
62159, V, 0, 0, 0, 0, 0, 700, 52
62159, V, 0, 0, 0, 0, 0, 700, 52
62416, V, 0, 0, 0, 0, 0, 700, 52
62416, V, 0, 0, 0, 0, 0, 700, 52
62673, V, 0, 0, 0, 0, 0, 700, 52
62673, V, 0, 0, 0, 0, 0, 700, 52
62930, V, 0, 0, 0, 0, 0, 700, 52
62930, V, 0, 0, 0, 0, 0, 700, 52
63187, V, 0, 0, 0, 0, 0, 700, 52
63187, V, 0, 0, 0, 0, 0, 700, 52
63444, V, 0, 0, 0, 0, 0, 700, 52
63444, V, 0, 0, 0, 0, 0, 700, 52
63702, V, 0, 0, 0, 0, 0, 700, 52
63702, V, 0, 0, 0, 0, 0, 700, 52
63959, V, 0, 0, 0, 0, 0, 700, 52
63959, V, 0, 0, 0, 0, 0, 700, 52
64216, V, 0, 0, 0, 0, 0, 700, 52
64216, V, 0, 0, 0, 0, 0, 700, 52
64473, V, 0, 0, 0, 0, 0, 700, 52
64473, V, 0, 0, 0, 0, 0, 700, 52
64730, V, 0, 0, 0, 0, 0, 700, 52
64730, V, 0, 0, 0, 0, 0, 700, 52
64987, V, 0, 0, 0, 0, 0, 700, 52
64987, V, 0, 0, 0, 0, 0, 700, 52
65244, V, 0, 0, 0, 0, 0, 700, 52
65244, V, 0, 0, 0, 0, 0, 700, 52
65501, V, 0, 0, 0, 0, 0, 700, 52
65501, V, 0, 0, 0, 0, 0, 700, 52
222, V, 0, 0, 0, 0, 0, 700, 52
222, V, 0, 0, 0, 0, 0, 700, 52
479, V, 0, 0, 0, 0, 0, 700, 52
479, V, 0, 0, 0, 0, 0, 700, 52
736, V, 0, 0, 0, 0, 0, 700, 52
736, V, 0, 0, 0, 0, 0, 700, 52
993, V, 0, 0, 0, 0, 0, 700, 52
993, V, 0, 0, 0, 0, 0, 700, 52
1250, V, 0, 0, 0, 0, 0, 700, 52
1250, V, 0, 0, 0, 0, 0, 700, 52
1507, V, 0, 0, 0, 0, 0, 700, 52
1507, V, 0, 0, 0, 0, 0, 700, 52
1764, V, 0, 0, 0, 0, 0, 700, 52
1764, V, 0, 0, 0, 0, 0, 700, 52
2021, V, 0, 0, 0, 0, 0, 700, 52
2021, V, 0, 0, 0, 0, 0, 700, 52
2278, V, 0, 0, 0, 0, 0, 700, 52
2278, V, 0, 0, 0, 0, 0, 700, 52
2535, V, 0, 0, 0, 0, 0, 700, 52
2535, V, 0, 0, 0, 0, 0, 700, 52
2792, V, 0, 0, 0, 0, 0, 700, 52
2792, V, 0, 0, 0, 0, 0, 700, 52
3049, V, 0, 0, 0, 0, 0, 700, 52
3049, V, 0, 0, 0, 0, 0, 700, 52
3306, V, 0, 0, 0, 0, 0, 700, 52
3306, V, 0, 0, 0, 0, 0, 700, 52
3563, V, 0, 0, 0, 0, 0, 700, 52
3563, V, 0, 0, 0, 0, 0, 700, 52
3820, V, 0, 0, 0, 0, 0, 700, 52
3820, V, 0, 0, 0, 0, 0, 700, 52
4077, V, 0, 0, 0, 0, 0, 700, 52
4077, V, 0, 0, 0, 0, 0, 700, 52
4334, V, 0, 0, 0, 0, 0, 700, 52
4334, V, 0, 0, 0, 0, 0, 700, 52
4591, V, 0, 0, 0, 0, 0, 700, 52
4591, V, 0, 0, 0, 0, 0, 700, 52
4848, V, 0, 0, 0, 0, 0, 700, 52
4848, V, 0, 0, 0, 0, 0, 700, 52
5105, V, 0, 0, 0, 0, 0, 700, 52
5105, V, 0, 0, 0, 0, 0, 700, 52
5362, V, 0, 0, 0, 0, 0, 700, 52
5362, V, 0, 0, 0, 0, 0, 700, 52
5619, V, 0, 0, 0, 0, 0, 700, 52
5619, V, 0, 0, 0, 0, 0, 700, 52
5876, V, 0, 0, 0, 0, 0, 700, 52
5876, V, 0, 0, 0, 0, 0, 700, 52
6133, V, 0, 0, 0, 0, 0, 700, 52
6133, V, 0, 0, 0, 0, 0, 700, 52
6390, V, 0, 0, 0, 0, 0, 700, 52
6390, V, 0, 0, 0, 0, 0, 700, 52
6647, V, 0, 0, 0, 0, 0, 700, 52
6647, V, 0, 0, 0, 0, 0, 700, 52
6904, V, 0, 0, 0, 0, 0, 700, 52
6904, V, 0, 0, 0, 0, 0, 700, 52
7161, V, 0, 0, 0, 0, 0, 700, 52
7161, V, 0, 0, 0, 0, 0, 700, 52
7418, V, 0, 0, 0, 0, 0, 700, 52
7418, V, 0, 0, 0, 0, 0, 700, 52
7675, V, 0, 0, 0, 0, 0, 700, 52
7675, V, 0, 0, 0, 0, 0, 700, 52
7932, V, 0, 0, 0, 0, 0, 700, 52
7932, V, 0, 0, 0, 0, 0, 700, 52
8189, V, 0, 0, 0, 0, 0, 700, 52
8189, V, 0, 0, 0, 0, 0, 700, 52
8446, V, 0, 0, 0, 0, 0, 700, 52
8446, V, 0, 0, 0, 0, 0, 700, 52
8704, V, 0, 0, 0, 0, 0, 700, 52
8704, V, 0, 0, 0, 0, 0, 700, 52
8961, V, 0, 0, 0, 0, 0, 700, 52
8961, V, 0, 0, 0, 0, 0, 700, 52
9218, V, 0, 0, 0, 0, 0, 700, 52
9218, V, 0, 0, 0, 0, 0, 700, 52
9475, V, 0, 0, 0, 0, 0, 700, 52
9475, V, 0, 0, 0, 0, 0, 700, 52
9732, V, 0, 0, 0, 0, 0, 700, 52
9732, V, 0, 0, 0, 0, 0, 700, 52
9989, V, 0, 0, 0, 0, 0, 700, 52
9989, V, 0, 0, 0, 0, 0, 700, 52
10246, V, 0, 0, 0, 0, 0, 700, 52
10246, V, 0, 0, 0, 0, 0, 700, 52
10503, V, 0, 0, 0, 0, 0, 700, 52
10503, V, 0, 0, 0, 0, 0, 700, 52
10760, V, 0, 0, 0, 0, 0, 700, 52
10760, V, 0, 0, 0, 0, 0, 700, 52
11017, V, 0, 0, 0, 0, 0, 700, 52
11017, V, 0, 0, 0, 0, 0, 700, 52
11274, V, 0, 0, 0, 0, 0, 700, 52
11274, V, 0, 0, 0, 0, 0, 700, 52
11531, V, 0, 0, 0, 0, 0, 700, 52
11531, V, 0, 0, 0, 0, 0, 700, 52
11788, V, 0, 0, 0, 0, 0, 700, 52
11788, V, 0, 0, 0, 0, 0, 700, 52
12045, V, 0, 0, 0, 0, 0, 700, 52
12045, V, 0, 0, 0, 0, 0, 700, 52
12302, V, 0, 0, 0, 0, 0, 700, 52
12302, V, 0, 0, 0, 0, 0, 700, 52
12559, V, 0, 0, 0, 0, 0, 700, 52
12559, V, 0, 0, 0, 0, 0, 700, 52
12816, V, 0, 0, 0, 0, 0, 700, 52
12816, V, 0, 0, 0, 0, 0, 700, 52
13073, V, 0, 0, 0, 0, 0, 700, 52
13073, V, 0, 0, 0, 0, 0, 700, 52
13330, V, 0, 0, 0, 0, 0, 700, 52
13330, V, 0, 0, 0, 0, 0, 700, 52
13587, V, 0, 0, 0, 0, 0, 700, 52
13587, V, 0, 0, 0, 0, 0, 700, 52
13844, V, 0, 0, 0, 0, 0, 700, 52
13844, V, 0, 0, 0, 0, 0, 700, 52
14101, V, 0, 0, 0, 0, 0, 700, 52
14101, V, 0, 0, 0, 0, 0, 700, 52
14358, V, 0, 0, 0, 0, 0, 700, 52
14358, V, 0, 0, 0, 0, 0, 700, 52
14615, V, 0, 0, 0, 0, 0, 700, 52
14615, V, 0, 0, 0, 0, 0, 700, 52
14872, V, 0, 0, 0, 0, 0, 700, 52
14872, V, 0, 0, 0, 0, 0, 700, 52
15129, V, 0, 0, 0, 0, 0, 700, 52
15129, V, 0, 0, 0, 0, 0, 700, 52
15386, V, 0, 0, 0, 0, 0, 700, 52
15386, V, 0, 0, 0, 0, 0, 700, 52
15643, V, 0, 0, 0, 0, 0, 700, 52
15643, V, 0, 0, 0, 0, 0, 700, 52
15900, V, 0, 0, 0, 0, 0, 700, 52
15900, V, 0, 0, 0, 0, 0, 700, 52
16157, V, 0, 0, 0, 0, 0, 700, 52
16157, V, 0, 0, 0, 0, 0, 700, 52
16414, V, 0, 0, 0, 0, 0, 700, 52
16414, V, 0, 0, 0, 0, 0, 700, 52
16671, V, 0, 0, 0, 0, 0, 700, 52
16671, V, 0, 0, 0, 0, 0, 700, 52
16928, V, 0, 0, 0, 0, 0, 700, 52
16928, V, 0, 0, 0, 0, 0, 700, 52
17185, V, 0, 0, 0, 0, 0, 700, 52
17185, V, 0, 0, 0, 0, 0, 700, 52
17442, V, 0, 0, 0, 0, 0, 700, 52
17442, V, 0, 0, 0, 0, 0, 700, 52
17699, V, 0, 0, 0, 0, 0, 700, 51
17699, V, 0, 0, 0, 0, 0, 700, 51
17956, V, 0, 0, 0, 0, 0, 700, 51
17956, V, 0, 0, 0, 0, 0, 700, 51
18213, V, 0, 0, 0, 0, 0, 700, 51
18213, V, 0, 0, 0, 0, 0, 700, 51
18470, V, 0, 0, 0, 0, 0, 700, 51
18470, V, 0, 0, 0, 0, 0, 700, 51
18727, V, 0, 0, 0, 0, 0, 700, 51
18727, V, 0, 0, 0, 0, 0, 700, 51
18984, V, 0, 0, 0, 0, 0, 700, 51
18984, V, 0, 0, 0, 0, 0, 700, 51
19241, V, 0, 0, 0, 0, 0, 700, 22
19241, V, 0, 0, 0, 0, 0, 700, 22
19499, V, 0, 0, 0, 0, 0, 700, 12
19499, V, 0, 0, 0, 0, 0, 700, 12
19756, V, 0, 0, 0, 0, 0, 700, 52
19756, V, 0, 0, 0, 0, 0, 700, 52
20013, V, 0, 0, 0, 0, 0, 700, 51
20013, V, 0, 0, 0, 0, 0, 700, 51
20075, V, 1, 0, 0, 0, 0, 700, 52
20076, V, 1, 0, 0, 0, 0, 700, 52
20077, V, 1, 0, 0, 0, 0, 700, 52
20078, V, 1, 0, 0, 0, 0, 700, 52
20079, V, 1, 0, 0, 0, 0, 700, 52
20080, V, 1, 0, 0, 0, 0, 700, 52
20081, V, 1, 0, 0, 0, 0, 700, 52
20082, V, 1, 0, 0, 0, 0, 700, 52
20083, V, 1, 0, 0, 0, 0, 700, 52
20084, V, 1, 0, 0, 0, 0, 700, 52
20085, V, 1, 0, 0, 0, 0, 700, 52
20086, V, 1, 0, 0, 0, 0, 700, 52
20087, V, 1, 0, 0, 0, 0, 700, 52
20088, V, 1, 0, 0, 0, 0, 700, 52
20089, V, 1, 0, 0, 0, 0, 700, 52
20090, V, 1, 0, 0, 0, 0, 700, 52
20091, V, 1, 0, 0, 0, 0, 700, 52
20092, V, 1, 0, 0, 0, 0, 700, 52
20093, V, 1, 0, 0, 0, 0, 700, 52
20094, V, 1, 0, 0, 0, 0, 700, 52
20096, V, 1, 0, 0, 0, 0, 700, 52
20097, V, 1, 0, 0, 0, 0, 700, 52
20098, V, 1, 0, 0, 0, 0, 700, 52
20099, V, 1, 0, 0, 0, 0, 700, 52
20100, V, 1, 0, 0, 0, 0, 700, 52
20101, V, 1, 0, 0, 0, 0, 700, 52
20102, V, 1, 0, 0, 0, 0, 700, 52
20103, V, 1, 0, 0, 0, 0, 700, 52
20104, V, 1, 0, 0, 0, 0, 700, 52
20105, V, 1, 0, 0, 0, 0, 700, 52
20106, V, 1, 0, 0, 0, 0, 700, 52
20107, V, 1, 0, 0, 0, 0, 700, 52
20108, V, 1, 0, 0, 0, 0, 700, 52
20109, V, 1, 0, 0, 0, 0, 700, 52
20110, V, 1, 0, 0, 0, 0, 700, 52
20111, V, 1, 0, 0, 0, 0, 700, 52
20112, V, 1, 0, 0, 0, 0, 700, 52
20113, V, 1, 0, 0, 0, 0, 700, 52
20114, V, 1, 0, 0, 0, 0, 700, 52
20115, V, 1, 0, 0, 0, 0, 700, 52
20116, V, 1, 0, 0, 0, 0, 700, 52
20117, V, 1, 0, 0, 0, 0, 700, 52
20118, V, 1, 0, 0, 0, 0, 700, 52
20119, V, 1, 0, 0, 0, 0, 700, 52
20120, V, 1, 0, 0, 0, 0, 700, 52
20121, V, 1, 0, 0, 0, 0, 700, 52
20122, V, 1, 0, 0, 0, 0, 700, 52
20123, V, 1, 0, 0, 0, 0, 700, 52
20124, V, 1, 0, 0, 0, 0, 700, 52
20125, V, 1, 0, 0, 0, 0, 700, 52
20126, V, 1, 0, 0, 0, 0, 700, 52
20127, V, 1, 0, 0, 0, 0, 700, 52
20128, V, 1, 0, 0, 0, 0, 700, 52
20129, V, 1, 0, 0, 0, 0, 700, 52
20130, V, 1, 0, 0, 0, 0, 700, 52
20131, V, 1, 0, 0, 0, 0, 700, 52
20132, V, 1, 0, 0, 0, 0, 700, 52
20133, V, 1, 0, 0, 0, 0, 700, 52
20134, V, 1, 0, 0, 0, 0, 700, 52
20135, V, 1, 0, 0, 0, 0, 700, 52
20136, V, 1, 0, 0, 0, 0, 700, 52
20137, V, 1, 0, 0, 0, 0, 700, 53
20139, V, 1, 0, 0, 0, 0, 700, 52
20140, V, 1, 0, 0, 0, 0, 700, 52
20141, V, 1, 0, 0, 0, 0, 700, 53
20142, V, 1, 0, 0, 0, 0, 700, 53
20143, V, 1, 0, 0, 0, 0, 700, 53
20144, V, 1, 0, 0, 0, 0, 700, 53
20145, V, 1, 0, 0, 0, 0, 700, 53
20146, V, 1, 0, 0, 0, 0, 700, 53
20147, V, 1, 0, 0, 0, 0, 700, 52
20148, V, 1, 0, 0, 0, 0, 700, 52
20149, V, 1, 0, 0, 0, 0, 700, 53
20150, V, 1, 0, 0, 0, 0, 700, 53
20151, V, 1, 0, 0, 0, 0, 700, 52
20152, V, 1, 0, 0, 0, 0, 700, 53
20153, V, 1, 0, 0, 0, 0, 700, 53
20154, V, 1, 0, 0, 0, 0, 700, 53
20155, V, 1, 0, 0, 0, 0, 700, 53
20156, V, 1, 0, 0, 0, 0, 700, 53
20157, V, 1, 0, 0, 0, 0, 700, 53
20158, V, 1, 0, 0, 0, 0, 700, 53
20159, V, 1, 0, 0, 0, 0, 700, 53
20160, V, 1, 0, 0, 0, 0, 700, 53
20161, V, 1, 0, 0, 0, 0, 700, 53
20162, V, 1, 0, 0, 0, 0, 700, 53
20163, V, 1, 0, 0, 0, 0, 700, 53
20164, V, 1, 0, 0, 0, 0, 700, 53
20165, V, 1, 0, 0, 0, 0, 700, 53
20166, V, 1, 0, 0, 0, 0, 700, 53
20167, V, 1, 0, 0, 0, 0, 700, 52
20168, V, 1, 0, 0, 0, 0, 700, 53
20169, V, 1, 0, 0, 0, 0, 700, 53
20170, V, 1, 0, 0, 0, 0, 700, 53
20171, V, 1, 0, 0, 0, 0, 700, 53
20172, V, 1, 0, 0, 0, 0, 700, 53
20173, V, 1, 0, 0, 0, 0, 700, 53
20174, V, 1, 0, 0, 0, 0, 700, 53
20175, V, 1, 0, 0, 0, 0, 700, 53
20176, V, 1, 0, 0, 0, 0, 700, 53
20177, V, 1, 0, 0, 0, 0, 700, 53
20178, V, 1, 0, 0, 0, 0, 700, 53
20179, V, 1, 0, 0, 0, 0, 700, 53
20180, V, 1, 0, 0, 0, 0, 700, 53
20182, V, 1, 0, 0, 0, 0, 700, 53
20183, V, 1, 0, 0, 0, 0, 700, 53
20184, V, 1, 0, 0, 0, 0, 700, 53
20185, V, 1, 0, 0, 0, 0, 700, 53
20186, V, 1, 0, 0, 0, 0, 700, 53
20187, V, 1, 0, 0, 0, 0, 700, 53
20188, V, 1, 0, 0, 0, 0, 700, 53
20189, V, 1, 0, 0, 0, 0, 700, 53
20190, V, 1, 0, 0, 0, 0, 700, 53
20191, V, 1, 0, 0, 0, 0, 700, 53
20192, V, 1, 0, 0, 0, 0, 700, 53
20193, V, 1, 0, 0, 0, 0, 700, 53
20194, V, 1, 0, 0, 0, 0, 700, 53
20195, V, 1, 0, 0, 0, 0, 700, 53
20196, V, 1, 0, 0, 0, 0, 700, 53
20197, V, 1, 0, 0, 0, 0, 700, 53
20198, V, 1, 0, 0, 0, 0, 700, 53
20199, V, 1, 0, 0, 0, 0, 700, 53
20200, V, 1, 0, 0, 0, 0, 700, 53
20201, V, 1, 0, 0, 0, 0, 700, 53
20202, V, 1, 0, 0, 0, 0, 700, 53
20203, V, 1, 0, 0, 0, 0, 700, 53
20204, V, 1, 0, 0, 0, 0, 700, 53
20205, V, 1, 0, 0, 0, 0, 700, 53
20206, V, 1, 0, 0, 0, 0, 700, 53
20207, V, 1, 0, 0, 0, 0, 700, 53
20208, V, 1, 0, 0, 0, 0, 700, 53
20209, V, 1, 0, 0, 0, 0, 700, 53
20210, V, 1, 0, 0, 0, 0, 700, 53
20211, V, 1, 0, 0, 0, 0, 700, 53
20212, V, 1, 0, 0, 0, 0, 700, 53
20213, V, 1, 0, 0, 0, 0, 700, 53
20214, V, 1, 0, 0, 0, 0, 700, 53
20215, V, 1, 0, 0, 0, 0, 700, 53
20216, V, 1, 0, 0, 0, 0, 700, 53
20217, V, 1, 0, 0, 0, 0, 700, 53
20218, V, 1, 0, 0, 0, 0, 700, 53
20219, V, 1, 0, 0, 0, 0, 700, 53
20220, V, 1, 0, 0, 0, 0, 700, 53
20221, V, 1, 0, 0, 0, 0, 700, 53
20222, V, 1, 0, 0, 0, 0, 700, 53
20224, V, 1, 0, 0, 0, 0, 700, 53
20225, V, 1, 0, 0, 0, 0, 700, 53
20226, V, 1, 0, 0, 0, 0, 700, 53
20227, V, 1, 0, 0, 0, 0, 700, 53
20228, V, 1, 0, 0, 0, 0, 700, 53
20229, V, 1, 0, 0, 0, 0, 700, 53
20230, V, 1, 0, 0, 0, 0, 700, 53
20231, V, 1, 0, 0, 0, 0, 700, 53
20232, V, 1, 0, 0, 0, 0, 700, 53
20233, V, 1, 0, 0, 0, 0, 700, 53
20234, V, 1, 0, 0, 0, 0, 700, 53
20235, V, 1, 0, 0, 0, 0, 700, 53
20236, V, 1, 0, 0, 0, 0, 700, 53
20237, V, 1, 0, 0, 0, 0, 700, 53
20238, V, 1, 0, 0, 0, 0, 700, 53
20239, V, 1, 0, 0, 0, 0, 700, 53
20240, V, 1, 0, 0, 0, 0, 700, 53
20241, V, 1, 0, 0, 0, 0, 700, 53
20242, V, 1, 0, 0, 0, 0, 700, 53
20243, V, 1, 0, 0, 0, 0, 700, 53
20244, V, 1, 0, 0, 0, 0, 700, 53
20245, V, 1, 0, 0, 0, 0, 700, 53
20246, V, 1, 0, 0, 0, 0, 700, 53
20247, V, 1, 0, 0, 0, 0, 700, 53
20248, V, 1, 0, 0, 0, 0, 700, 53
20249, V, 1, 0, 0, 0, 0, 700, 53
20250, V, 1, 0, 0, 0, 0, 700, 53
20251, V, 1, 0, 0, 0, 0, 700, 53
20252, V, 1, 0, 0, 0, 0, 700, 53
20253, V, 1, 0, 0, 0, 0, 700, 53
20254, V, 1, 0, 0, 0, 0, 700, 53
20255, V, 1, 0, 0, 0, 0, 700, 53
20256, V, 1, 0, 0, 0, 0, 700, 53
20257, V, 1, 0, 0, 0, 0, 700, 53
20258, V, 1, 0, 0, 0, 0, 700, 53
20259, V, 1, 0, 0, 0, 0, 700, 53
20260, V, 1, 0, 0, 0, 0, 700, 53
20261, V, 1, 0, 0, 0, 0, 700, 53
20262, V, 1, 0, 0, 0, 0, 700, 53
20263, V, 1, 0, 0, 0, 0, 700, 53
20264, V, 1, 0, 0, 0, 0, 700, 53
20265, V, 1, 0, 0, 0, 0, 700, 53
20267, V, 1, 0, 0, 0, 0, 700, 53
20268, V, 1, 0, 0, 0, 0, 700, 53
20269, V, 1, 0, 0, 0, 0, 700, 53
20270, V, 1, 0, 0, 0, 0, 700, 53
20271, V, 1, 0, 0, 0, 0, 700, 53
20272, V, 1, 0, 0, 0, 0, 700, 53
20273, V, 1, 0, 0, 0, 0, 700, 53
20274, V, 1, 0, 0, 0, 0, 700, 53
20275, V, 1, 0, 0, 0, 0, 700, 53
20276, V, 1, 0, 0, 0, 0, 700, 53
20277, V, 1, 0, 0, 0, 0, 700, 53
20278, V, 1, 0, 0, 0, 0, 700, 53
20279, V, 1, 0, 0, 0, 0, 700, 53
20280, V, 1, 0, 0, 0, 0, 700, 53
20281, V, 1, 0, 0, 0, 0, 700, 53
20282, V, 1, 0, 0, 0, 0, 700, 53
20283, V, 1, 0, 0, 0, 0, 700, 53
20284, V, 1, 0, 0, 0, 0, 700, 53
20285, V, 1, 0, 0, 0, 0, 700, 53
20286, V, 1, 0, 0, 0, 0, 700, 53
20287, V, 1, 0, 0, 0, 0, 700, 53
20288, V, 1, 0, 0, 0, 0, 700, 53
20289, V, 1, 0, 0, 0, 0, 700, 53
20290, V, 1, 0, 0, 0, 0, 700, 53
20291, V, 1, 0, 0, 0, 0, 700, 53
20292, V, 1, 0, 0, 0, 0, 700, 53
20293, V, 1, 0, 0, 0, 0, 700, 53
20294, V, 1, 0, 0, 0, 0, 700, 53
20295, V, 1, 0, 0, 0, 0, 700, 53
20296, V, 1, 0, 0, 0, 0, 700, 53
20297, V, 1, 0, 0, 0, 0, 700, 53
20298, V, 1, 0, 0, 0, 0, 700, 53
20299, V, 1, 0, 0, 0, 0, 700, 53
20300, V, 1, 0, 0, 0, 0, 700, 53
20301, V, 1, 0, 0, 0, 0, 700, 53
20302, V, 1, 0, 0, 0, 0, 700, 53
20303, V, 1, 0, 0, 0, 0, 700, 53
20304, V, 1, 0, 0, 0, 0, 700, 53
20305, V, 1, 0, 0, 0, 0, 700, 53
20306, V, 1, 0, 0, 0, 0, 700, 53
20307, V, 1, 0, 0, 0, 0, 700, 53
20308, V, 1, 0, 0, 0, 0, 700, 53
20310, V, 1, 0, 0, 0, 0, 700, 53
20311, V, 1, 0, 0, 0, 0, 700, 53
20312, V, 1, 0, 0, 0, 0, 700, 53
20313, V, 1, 0, 0, 0, 0, 700, 53
20314, V, 1, 0, 0, 0, 0, 700, 53
20315, V, 1, 0, 0, 0, 0, 700, 53
20316, V, 1, 0, 0, 0, 0, 700, 53
20317, V, 1, 0, 0, 0, 0, 700, 53
20318, V, 1, 0, 0, 0, 0, 700, 53
20319, V, 1, 0, 0, 0, 0, 700, 53
20320, V, 1, 0, 0, 0, 0, 700, 53
20321, V, 1, 0, 0, 0, 0, 700, 53
20322, V, 1, 0, 0, 0, 0, 700, 53
20323, V, 1, 0, 0, 0, 0, 700, 53
20324, V, 1, 0, 0, 0, 0, 700, 53
20325, V, 1, 0, 0, 0, 0, 700, 53
20326, V, 1, 0, 0, 0, 0, 700, 53
20327, V, 1, 0, 0, 0, 0, 700, 53
20328, V, 1, 0, 0, 0, 0, 700, 53
20329, V, 1, 0, 0, 0, 0, 700, 53
20330, V, 1, 0, 0, 0, 0, 700, 53
20331, V, 1, 0, 0, 0, 0, 700, 53
20332, V, 1, 0, 0, 0, 0, 700, 53
20333, V, 1, 0, 0, 0, 0, 700, 53
20334, V, 1, 0, 0, 0, 0, 700, 53
20335, V, 1, 0, 0, 0, 0, 700, 53
20336, V, 1, 0, 0, 0, 0, 700, 53
20337, V, 1, 0, 0, 0, 0, 700, 53
20338, V, 1, 0, 0, 0, 0, 700, 53
20339, V, 1, 0, 0, 0, 0, 700, 53
20340, V, 1, 0, 0, 0, 0, 700, 53
20341, V, 1, 0, 0, 0, 0, 700, 53
20342, V, 1, 0, 0, 0, 0, 700, 53
20343, V, 1, 0, 0, 0, 0, 700, 53
20344, V, 1, 0, 0, 0, 0, 700, 53
20345, V, 1, 0, 0, 0, 0, 700, 53
20346, V, 1, 0, 0, 0, 0, 700, 53
20347, V, 1, 0, 0, 0, 0, 700, 53
20348, V, 1, 0, 0, 0, 0, 700, 53
20349, V, 1, 0, 0, 0, 0, 700, 53
20350, V, 1, 0, 0, 0, 0, 700, 53
20352, V, 1, 0, 0, 0, 0, 700, 53
20353, V, 1, 0, 0, 0, 0, 700, 53
20354, V, 1, 0, 0, 0, 0, 700, 53
20355, V, 1, 0, 0, 0, 0, 700, 53
20356, V, 1, 0, 0, 0, 0, 700, 53
20357, V, 1, 0, 0, 0, 0, 700, 53
20358, V, 1, 0, 0, 0, 0, 700, 53
20359, V, 1, 0, 0, 0, 0, 700, 53
20360, V, 1, 0, 0, 0, 0, 700, 53
20361, V, 1, 0, 0, 0, 0, 700, 53
20362, V, 1, 0, 0, 0, 0, 700, 53
20363, V, 1, 0, 0, 0, 0, 700, 53
20364, V, 1, 0, 0, 0, 0, 700, 53
20365, V, 1, 0, 0, 0, 0, 700, 53
20366, V, 1, 0, 0, 0, 0, 700, 53
20367, V, 1, 0, 0, 0, 0, 700, 53
20368, V, 1, 0, 0, 0, 0, 700, 53
20369, V, 1, 0, 0, 0, 0, 700, 53
20370, V, 1, 0, 0, 0, 0, 700, 53
20371, V, 1, 0, 0, 0, 0, 700, 53
20372, V, 1, 0, 0, 0, 0, 700, 53
20373, V, 1, 0, 0, 0, 0, 700, 53
20374, V, 1, 0, 0, 0, 0, 700, 53
20375, V, 1, 0, 0, 0, 0, 700, 53
20376, V, 1, 0, 0, 0, 0, 700, 53
20377, V, 1, 0, 0, 0, 0, 700, 53
20378, V, 1, 0, 0, 0, 0, 700, 53
20379, V, 1, 0, 0, 0, 0, 700, 53
20380, V, 1, 0, 0, 0, 0, 700, 53
20381, V, 1, 0, 0, 0, 0, 700, 53
20382, V, 1, 0, 0, 0, 0, 700, 53
20383, V, 1, 0, 0, 0, 0, 700, 53
20384, V, 1, 0, 0, 0, 0, 700, 53
20385, V, 1, 0, 0, 0, 0, 700, 53
20386, V, 1, 0, 0, 0, 0, 700, 53
20387, V, 1, 0, 0, 0, 0, 700, 53
20388, V, 1, 0, 0, 0, 0, 700, 53
20389, V, 1, 0, 0, 0, 0, 700, 53
20390, V, 1, 0, 0, 0, 0, 700, 53
20391, V, 1, 0, 0, 0, 0, 700, 53
20392, V, 1, 0, 0, 0, 0, 700, 53
20393, V, 1, 0, 0, 0, 0, 700, 53
20395, V, 1, 0, 0, 0, 0, 700, 53
20396, V, 1, 0, 0, 0, 0, 700, 53
20397, V, 1, 0, 0, 0, 0, 700, 53
20398, V, 1, 0, 0, 0, 0, 700, 53
20399, V, 1, 0, 0, 0, 0, 700, 53
20400, V, 1, 0, 0, 0, 0, 700, 53
20401, V, 1, 0, 0, 0, 0, 700, 53
20402, V, 1, 0, 0, 0, 0, 700, 53
20403, V, 1, 0, 0, 0, 0, 700, 53
20404, V, 1, 0, 0, 0, 0, 700, 53
20405, V, 1, 0, 0, 0, 0, 700, 53
20406, V, 1, 0, 0, 0, 0, 700, 53
20407, V, 1, 0, 0, 0, 0, 700, 53
20408, V, 1, 0, 0, 0, 0, 700, 53
20409, V, 1, 0, 0, 0, 0, 700, 53
20410, V, 1, 0, 0, 0, 0, 700, 53
20411, V, 1, 0, 0, 0, 0, 700, 53
20412, V, 1, 0, 0, 0, 0, 700, 53
20413, V, 1, 0, 0, 0, 0, 700, 53
20414, V, 1, 0, 0, 0, 0, 700, 53
20415, V, 1, 0, 0, 0, 0, 700, 53
20416, V, 1, 0, 0, 0, 0, 700, 53
20417, V, 1, 0, 0, 0, 0, 700, 53
20418, V, 1, 0, 0, 0, 0, 700, 53
20419, V, 1, 0, 0, 0, 0, 700, 53
20420, V, 1, 0, 0, 0, 0, 700, 53
20421, V, 1, 0, 0, 0, 0, 700, 53
20422, V, 1, 0, 0, 0, 0, 700, 53
20423, V, 1, 0, 0, 0, 0, 700, 53
20424, V, 1, 0, 0, 0, 0, 700, 53
20425, V, 1, 0, 0, 0, 0, 700, 53
20426, V, 1, 0, 0, 0, 0, 700, 53
20427, V, 1, 0, 0, 0, 0, 700, 53
20428, V, 1, 0, 0, 0, 0, 700, 53
20429, V, 1, 0, 0, 0, 0, 700, 53
20430, V, 1, 0, 0, 0, 0, 700, 53
20431, V, 1, 0, 0, 0, 0, 700, 53
20432, V, 1, 0, 0, 0, 0, 700, 53
20433, V, 1, 0, 0, 0, 0, 700, 53
20434, V, 1, 0, 0, 0, 0, 700, 53
20435, V, 1, 0, 0, 0, 0, 700, 53
20436, V, 1, 0, 0, 0, 0, 700, 53
20438, V, 1, 0, 0, 0, 0, 700, 53
20439, V, 1, 0, 0, 0, 0, 700, 53
20440, V, 1, 0, 0, 0, 0, 700, 53
20441, V, 1, 0, 0, 0, 0, 700, 53
20442, V, 1, 0, 0, 0, 0, 700, 53
20443, V, 1, 0, 0, 0, 0, 700, 53
20444, V, 1, 0, 0, 0, 0, 700, 53
20445, V, 1, 0, 0, 0, 0, 700, 53
20446, V, 1, 0, 0, 0, 0, 700, 53
20447, V, 1, 0, 0, 0, 0, 700, 53
20448, V, 1, 0, 0, 0, 0, 700, 53
20449, V, 1, 0, 0, 0, 0, 700, 53
20450, V, 1, 0, 0, 0, 0, 700, 53
20451, V, 1, 0, 0, 0, 0, 700, 53
20452, V, 1, 0, 0, 0, 0, 700, 53
20453, V, 1, 0, 0, 0, 0, 700, 53
20454, V, 1, 0, 0, 0, 0, 700, 53
20455, V, 1, 0, 0, 0, 0, 700, 53
20456, V, 1, 0, 0, 0, 0, 700, 53
20457, V, 1, 0, 0, 0, 0, 700, 53
20458, V, 1, 0, 0, 0, 0, 700, 53
20459, V, 1, 0, 0, 0, 0, 700, 53
20460, V, 1, 0, 0, 0, 0, 700, 53
20461, V, 1, 0, 0, 0, 0, 700, 53
20462, V, 1, 0, 0, 0, 0, 700, 53
20463, V, 1, 0, 0, 0, 0, 700, 53
20464, V, 1, 0, 0, 0, 0, 700, 53
20465, V, 1, 0, 0, 0, 0, 700, 53
20466, V, 1, 0, 0, 0, 0, 700, 53
20467, V, 1, 0, 0, 0, 0, 700, 53
20468, V, 1, 0, 0, 0, 0, 700, 53
20469, V, 1, 0, 0, 0, 0, 700, 53
20470, V, 1, 0, 0, 0, 0, 700, 53
20471, V, 1, 0, 0, 0, 0, 700, 53
20472, V, 1, 0, 0, 0, 0, 700, 53
20473, V, 1, 0, 0, 0, 0, 700, 53
20474, V, 1, 0, 0, 0, 0, 700, 53
20475, V, 1, 0, 0, 0, 0, 700, 53
20476, V, 1, 0, 0, 0, 0, 700, 53
20477, V, 1, 0, 0, 0, 0, 700, 53
20478, V, 1, 0, 0, 0, 0, 700, 53
20480, V, 1, 0, 0, 0, 0, 700, 53
20481, V, 1, 0, 0, 0, 0, 700, 53
20482, V, 1, 0, 0, 0, 0, 700, 53
20483, V, 1, 0, 0, 0, 0, 700, 53
20484, V, 1, 0, 0, 0, 0, 700, 53
20485, V, 1, 0, 0, 0, 0, 700, 53
20486, V, 1, 0, 0, 0, 0, 700, 53
20487, V, 1, 0, 0, 0, 0, 700, 53
20488, V, 1, 0, 0, 0, 0, 700, 53
20489, V, 1, 0, 0, 0, 0, 700, 53
20490, V, 1, 0, 0, 0, 0, 700, 53
20491, V, 1, 0, 0, 0, 0, 700, 53
20492, V, 1, 0, 0, 0, 0, 700, 53
20493, V, 1, 0, 0, 0, 0, 700, 53
20494, V, 1, 0, 0, 0, 0, 700, 53
20495, V, 1, 0, 0, 0, 0, 700, 53
20496, V, 1, 0, 0, 0, 0, 700, 53
20497, V, 1, 0, 0, 0, 0, 700, 53
20498, V, 1, 0, 0, 0, 0, 700, 53
20499, V, 1, 0, 0, 0, 0, 700, 53
20500, V, 1, 0, 0, 0, 0, 700, 53
20501, V, 1, 0, 0, 0, 0, 700, 53
20502, V, 1, 0, 0, 0, 0, 700, 53
20503, V, 1, 0, 0, 0, 0, 700, 53
20504, V, 1, 0, 0, 0, 0, 700, 53
20505, V, 1, 0, 0, 0, 0, 700, 53
20506, V, 1, 0, 0, 0, 0, 700, 53
20507, V, 1, 0, 0, 0, 0, 700, 53
20508, V, 1, 0, 0, 0, 0, 700, 53
20509, V, 1, 0, 0, 0, 0, 700, 53
20510, V, 1, 0, 0, 0, 0, 700, 53
20511, V, 1, 0, 0, 0, 0, 700, 53
20512, V, 1, 0, 0, 0, 0, 700, 53
20513, V, 1, 0, 0, 0, 0, 700, 53
20514, V, 1, 0, 0, 0, 0, 700, 53
20515, V, 1, 0, 0, 0, 0, 700, 53
20516, V, 1, 0, 0, 0, 0, 700, 53
20517, V, 1, 0, 0, 0, 0, 700, 53
20518, V, 1, 0, 0, 0, 0, 700, 53
20519, V, 1, 0, 0, 0, 0, 700, 53
20520, V, 1, 0, 0, 0, 0, 700, 53
20521, V, 1, 0, 0, 0, 0, 700, 53
20523, V, 1, 0, 0, 0, 0, 700, 53
20524, V, 1, 0, 0, 0, 0, 700, 53
20525, V, 1, 0, 0, 0, 0, 700, 53
20526, V, 1, 0, 0, 0, 0, 700, 53
20527, V, 1, 0, 0, 0, 0, 700, 53
20528, V, 1, 0, 0, 0, 0, 700, 53
20529, V, 1, 0, 0, 0, 0, 700, 53
20530, V, 1, 0, 0, 0, 0, 700, 53
20531, V, 1, 0, 0, 0, 0, 700, 53
20532, V, 1, 0, 0, 0, 0, 700, 53
20533, V, 1, 0, 0, 0, 0, 700, 53
20534, V, 1, 0, 0, 0, 0, 700, 53
20535, V, 1, 0, 0, 0, 0, 700, 53
20536, V, 1, 0, 0, 0, 0, 700, 53
20537, V, 1, 0, 0, 0, 0, 700, 53
20538, V, 1, 0, 0, 0, 0, 700, 53
20539, V, 1, 0, 0, 0, 0, 700, 53
20540, V, 1, 0, 0, 0, 0, 700, 53
20541, V, 1, 0, 0, 0, 0, 700, 53
20542, V, 1, 0, 0, 0, 0, 700, 53
20543, V, 1, 0, 0, 0, 0, 700, 53
20544, V, 1, 0, 0, 0, 0, 700, 53
20545, V, 1, 0, 0, 0, 0, 700, 53
20546, V, 1, 0, 0, 0, 0, 700, 53
20547, V, 1, 0, 0, 0, 0, 700, 53
20548, V, 1, 0, 0, 0, 0, 700, 53
20549, V, 1, 0, 0, 0, 0, 700, 53
20550, V, 1, 0, 0, 0, 0, 700, 53
20551, V, 1, 0, 0, 0, 0, 700, 53
20552, V, 1, 0, 0, 0, 0, 700, 53
20553, V, 1, 0, 0, 0, 0, 700, 53
20554, V, 1, 0, 0, 0, 0, 700, 53
20555, V, 1, 0, 0, 0, 0, 700, 53
20556, V, 1, 0, 0, 0, 0, 700, 53
20557, V, 1, 0, 0, 0, 0, 700, 53
20558, V, 1, 0, 0, 0, 0, 700, 53
20559, V, 1, 0, 0, 0, 0, 700, 53
20560, V, 1, 0, 0, 0, 0, 700, 53
20561, V, 1, 0, 0, 0, 0, 700, 53
20562, V, 1, 0, 0, 0, 0, 700, 53
20563, V, 1, 0, 0, 0, 0, 700, 53
20564, V, 1, 0, 0, 0, 0, 700, 53
20566, V, 1, 0, 0, 0, 0, 700, 53
20567, V, 1, 0, 0, 0, 0, 700, 53
20568, V, 1, 0, 0, 0, 0, 700, 53
20569, V, 1, 0, 0, 0, 0, 700, 53
20570, V, 1, 0, 0, 0, 0, 700, 53
20571, V, 1, 0, 0, 0, 0, 700, 53
20572, V, 1, 0, 0, 0, 0, 700, 53
20573, V, 1, 0, 0, 0, 0, 700, 53
20574, V, 1, 0, 0, 0, 0, 700, 53
20575, V, 1, 0, 0, 0, 0, 700, 53
20576, V, 1, 0, 0, 0, 0, 700, 53
20577, V, 1, 0, 0, 0, 0, 700, 53
20578, V, 1, 0, 0, 0, 0, 700, 53
20579, V, 1, 0, 0, 0, 0, 700, 53
20580, V, 1, 0, 0, 0, 0, 700, 53
20581, V, 1, 0, 0, 0, 0, 700, 53
20582, V, 1, 0, 0, 0, 0, 700, 53
20583, V, 1, 0, 0, 0, 0, 700, 53
20584, V, 1, 0, 0, 0, 0, 700, 53
20585, V, 1, 0, 0, 0, 0, 700, 53
20586, V, 1, 0, 0, 0, 0, 700, 53
20587, V, 1, 0, 0, 0, 0, 700, 53
20588, V, 1, 0, 0, 0, 0, 700, 53
20589, V, 1, 0, 0, 0, 0, 700, 53
20590, V, 1, 0, 0, 0, 0, 700, 53
20591, V, 1, 0, 0, 0, 0, 700, 53
20592, V, 1, 0, 0, 0, 0, 700, 53
20593, V, 1, 0, 0, 0, 0, 700, 53
20594, V, 1, 0, 0, 0, 0, 700, 53
20595, V, 1, 0, 0, 0, 0, 700, 53
20596, V, 1, 0, 0, 0, 0, 700, 53
20597, V, 1, 0, 0, 0, 0, 700, 53
20598, V, 1, 0, 0, 0, 0, 700, 53
20599, V, 1, 0, 0, 0, 0, 700, 53
20600, V, 1, 0, 0, 0, 0, 700, 53
20601, V, 1, 0, 0, 0, 0, 700, 53
20602, V, 1, 0, 0, 0, 0, 700, 53
20603, V, 1, 0, 0, 0, 0, 700, 53
20604, V, 1, 0, 0, 0, 0, 700, 53
20605, V, 1, 0, 0, 0, 0, 700, 53
20606, V, 1, 0, 0, 0, 0, 700, 53
20608, V, 1, 0, 0, 0, 0, 700, 53
20609, V, 1, 0, 0, 0, 0, 700, 53
20610, V, 1, 0, 0, 0, 0, 700, 53
20611, V, 1, 0, 0, 0, 0, 700, 53
20612, V, 1, 0, 0, 0, 0, 700, 53
20613, V, 1, 0, 0, 0, 0, 700, 53
20614, V, 1, 0, 0, 0, 0, 700, 53
20615, V, 1, 0, 0, 0, 0, 700, 53
20616, V, 1, 0, 0, 0, 0, 700, 53
20617, V, 1, 0, 0, 0, 0, 700, 53
20618, V, 1, 0, 0, 0, 0, 700, 53
20619, V, 1, 0, 0, 0, 0, 700, 53
20620, V, 1, 0, 0, 0, 0, 700, 53
20621, V, 1, 0, 0, 0, 0, 700, 53
20622, V, 1, 0, 0, 0, 0, 700, 53
20623, V, 1, 0, 0, 0, 0, 700, 53
20624, V, 1, 0, 0, 0, 0, 700, 53
20625, V, 1, 0, 0, 0, 0, 700, 53
20626, V, 1, 0, 0, 0, 0, 700, 53
20627, V, 1, 0, 0, 0, 0, 700, 53
20628, V, 1, 0, 0, 0, 0, 700, 53
20629, V, 1, 0, 0, 0, 0, 700, 53
20630, V, 1, 0, 0, 0, 0, 700, 53
20631, V, 1, 0, 0, 0, 0, 700, 53
20632, V, 1, 0, 0, 0, 0, 700, 53
20633, V, 1, 0, 0, 0, 0, 700, 53
20634, V, 1, 0, 0, 0, 0, 700, 53
20635, V, 1, 0, 0, 0, 0, 700, 53
20636, V, 1, 0, 0, 0, 0, 700, 53
20637, V, 1, 0, 0, 0, 0, 700, 53
20638, V, 1, 0, 0, 0, 0, 700, 53
20639, V, 1, 0, 0, 0, 0, 700, 53
20640, V, 1, 0, 0, 0, 0, 700, 53
20641, V, 1, 0, 0, 0, 0, 700, 53
20642, V, 1, 0, 0, 0, 0, 700, 53
20643, V, 1, 0, 0, 0, 0, 700, 53
20644, V, 1, 0, 0, 0, 0, 700, 53
20645, V, 1, 0, 0, 0, 0, 700, 53
20646, V, 1, 0, 0, 0, 0, 700, 53
20647, V, 1, 0, 0, 0, 0, 700, 53
20648, V, 1, 0, 0, 0, 0, 700, 53
20649, V, 1, 0, 0, 0, 0, 700, 53
20651, V, 1, 0, 0, 0, 0, 700, 53
20652, V, 1, 0, 0, 0, 0, 700, 53
20653, V, 1, 0, 0, 0, 0, 700, 53
20654, V, 1, 0, 0, 0, 0, 700, 53
20655, V, 1, 0, 0, 0, 0, 700, 53
20656, V, 1, 0, 0, 0, 0, 700, 53
20657, V, 1, 0, 0, 0, 0, 700, 53
20658, V, 1, 0, 0, 0, 0, 700, 53
20659, V, 1, 0, 0, 0, 0, 700, 53
20660, V, 1, 0, 0, 0, 0, 700, 53
20661, V, 1, 0, 0, 0, 0, 700, 53
20662, V, 1, 0, 0, 0, 0, 700, 53
20663, V, 1, 0, 0, 0, 0, 700, 53
20664, V, 1, 0, 0, 0, 0, 700, 53
20665, V, 1, 0, 0, 0, 0, 700, 53
20666, V, 1, 0, 0, 0, 0, 700, 53
20667, V, 1, 0, 0, 0, 0, 700, 53
20668, V, 1, 0, 0, 0, 0, 700, 53
20669, V, 1, 0, 0, 0, 0, 700, 53
20670, V, 1, 0, 0, 0, 0, 700, 53
20671, V, 1, 0, 0, 0, 0, 700, 53
20672, V, 1, 0, 0, 0, 0, 700, 53
20673, V, 1, 0, 0, 0, 0, 700, 53
20674, V, 1, 0, 0, 0, 0, 700, 53
20675, V, 1, 0, 0, 0, 0, 700, 53
20676, V, 1, 0, 0, 0, 0, 700, 53
20677, V, 1, 0, 0, 0, 0, 700, 53
20678, V, 1, 0, 0, 0, 0, 700, 53
20679, V, 1, 0, 0, 0, 0, 700, 53
20680, V, 1, 0, 0, 0, 0, 700, 53
20681, V, 1, 0, 0, 0, 0, 700, 53
20682, V, 1, 0, 0, 0, 0, 700, 53
20683, V, 1, 0, 0, 0, 0, 700, 53
20684, V, 1, 0, 0, 0, 0, 700, 53
20685, V, 1, 0, 0, 0, 0, 700, 53
20686, V, 1, 0, 0, 0, 0, 700, 53
20687, V, 1, 0, 0, 0, 0, 700, 53
20688, V, 1, 0, 0, 0, 0, 700, 53
20689, V, 1, 0, 0, 0, 0, 700, 53
20690, V, 1, 0, 0, 0, 0, 700, 53
20691, V, 1, 0, 0, 0, 0, 700, 53
20692, V, 1, 0, 0, 0, 0, 700, 53
20694, V, 1, 0, 0, 0, 0, 700, 53
20695, V, 1, 0, 0, 0, 0, 700, 53
20696, V, 1, 0, 0, 0, 0, 700, 53
20697, V, 1, 0, 0, 0, 0, 700, 53
20698, V, 1, 0, 0, 0, 0, 700, 53
20699, V, 1, 0, 0, 0, 0, 700, 53
20700, V, 1, 0, 0, 0, 0, 700, 53
20701, V, 1, 0, 0, 0, 0, 700, 53
20702, V, 1, 0, 0, 0, 0, 700, 53
20703, V, 1, 0, 0, 0, 0, 700, 53
20704, V, 1, 0, 0, 0, 0, 700, 53
20705, V, 1, 0, 0, 0, 0, 700, 53
20706, V, 1, 0, 0, 0, 0, 700, 53
20707, V, 1, 0, 0, 0, 0, 700, 53
20708, V, 1, 0, 0, 0, 0, 700, 53
20709, V, 1, 0, 0, 0, 0, 700, 53
20710, V, 1, 0, 0, 0, 0, 700, 53
20711, V, 1, 0, 0, 0, 0, 700, 53
20712, V, 1, 0, 0, 0, 0, 700, 53
20713, V, 1, 0, 0, 0, 0, 700, 53
20714, V, 1, 0, 0, 0, 0, 700, 53
20715, V, 1, 0, 0, 0, 0, 700, 53
20716, V, 1, 0, 0, 0, 0, 700, 53
20717, V, 1, 0, 0, 0, 0, 700, 53
20718, V, 1, 0, 0, 0, 0, 700, 53
20719, V, 1, 0, 0, 0, 0, 700, 53
20720, V, 1, 0, 0, 0, 0, 700, 53
20721, V, 1, 0, 0, 0, 0, 700, 53
20722, V, 1, 0, 0, 0, 0, 700, 53
20723, V, 1, 0, 0, 0, 0, 700, 53
20724, V, 1, 0, 0, 0, 0, 700, 53
20725, V, 1, 0, 0, 0, 0, 700, 53
20726, V, 1, 0, 0, 0, 0, 700, 53
20727, V, 1, 0, 0, 0, 0, 700, 53
20728, V, 1, 0, 0, 0, 0, 700, 53
20729, V, 1, 0, 0, 0, 0, 700, 53
20730, V, 1, 0, 0, 0, 0, 700, 53
20731, V, 1, 0, 0, 0, 0, 700, 53
20732, V, 1, 0, 0, 0, 0, 700, 53
20733, V, 1, 0, 0, 0, 0, 700, 53
20734, V, 1, 0, 0, 0, 0, 700, 53
20736, V, 1, 0, 0, 0, 0, 700, 53
20737, V, 1, 0, 0, 0, 0, 700, 53
20738, V, 1, 0, 0, 0, 0, 700, 53
20739, V, 1, 0, 0, 0, 0, 700, 53
20740, V, 1, 0, 0, 0, 0, 700, 53
20741, V, 1, 0, 0, 0, 0, 700, 53
20742, V, 1, 0, 0, 0, 0, 700, 53
20743, V, 1, 0, 0, 0, 0, 700, 53
20744, V, 1, 0, 0, 0, 0, 700, 53
20745, V, 1, 0, 0, 0, 0, 700, 53
20746, V, 1, 0, 0, 0, 0, 700, 53
20747, V, 1, 0, 0, 0, 0, 700, 53
20748, V, 1, 0, 0, 0, 0, 700, 53
20749, V, 1, 0, 0, 0, 0, 700, 53
20750, V, 1, 0, 0, 0, 0, 700, 53
20751, V, 1, 0, 0, 0, 0, 700, 53
20752, V, 1, 0, 0, 0, 0, 700, 53
20753, V, 1, 0, 0, 0, 0, 700, 53
20754, V, 1, 0, 0, 0, 0, 700, 53
20755, V, 1, 0, 0, 0, 0, 700, 53
20756, V, 1, 0, 0, 0, 0, 700, 53
20757, V, 1, 0, 0, 0, 0, 700, 53
20758, V, 1, 0, 0, 0, 0, 700, 53
20759, V, 1, 0, 0, 0, 0, 700, 53
20760, V, 1, 0, 0, 0, 0, 700, 53
20761, V, 1, 0, 0, 0, 0, 700, 53
20762, V, 1, 0, 0, 0, 0, 700, 53
20763, V, 1, 0, 0, 0, 0, 700, 53
20764, V, 1, 0, 0, 0, 0, 700, 53
20765, V, 1, 0, 0, 0, 0, 700, 53
20766, V, 1, 0, 0, 0, 0, 700, 53
20767, V, 1, 0, 0, 0, 0, 700, 53
20768, V, 1, 0, 0, 0, 0, 700, 53
20769, V, 1, 0, 0, 0, 0, 700, 53
20770, V, 1, 0, 0, 0, 0, 700, 53
20771, V, 1, 0, 0, 0, 0, 700, 53
20772, V, 1, 0, 0, 0, 0, 700, 53
20773, V, 1, 0, 0, 0, 0, 700, 53
20774, V, 1, 0, 0, 0, 0, 700, 53
20775, V, 1, 0, 0, 0, 0, 700, 53
20776, V, 1, 0, 0, 0, 0, 700, 53
20777, V, 1, 0, 0, 0, 0, 700, 53
20779, V, 1, 0, 0, 0, 0, 700, 53
20780, V, 1, 0, 0, 0, 0, 700, 53
20781, V, 1, 0, 0, 0, 0, 700, 53
20782, V, 1, 0, 0, 0, 0, 700, 53
20783, V, 1, 0, 0, 0, 0, 700, 53
20784, V, 1, 0, 0, 0, 0, 700, 53
20785, V, 1, 0, 0, 0, 0, 700, 53
20786, V, 1, 0, 0, 0, 0, 700, 53
20787, V, 1, 0, 0, 0, 0, 700, 53
20788, V, 1, 0, 0, 0, 0, 700, 53
20789, V, 1, 0, 0, 0, 0, 700, 53
20790, V, 1, 0, 0, 0, 0, 700, 53
20791, V, 1, 0, 0, 0, 0, 700, 53
20792, V, 1, 0, 0, 0, 0, 700, 53
20793, V, 1, 0, 0, 0, 0, 700, 53
20794, V, 1, 0, 0, 0, 0, 700, 53
20795, V, 1, 0, 0, 0, 0, 700, 53
20796, V, 1, 0, 0, 0, 0, 700, 53
20797, V, 1, 0, 0, 0, 0, 700, 53
20798, V, 1, 0, 0, 0, 0, 700, 53
20799, V, 1, 0, 0, 0, 0, 700, 53
20800, V, 1, 0, 0, 0, 0, 700, 53
20801, V, 1, 0, 0, 0, 0, 700, 53
20802, V, 1, 0, 0, 0, 0, 700, 53
20803, V, 1, 0, 0, 0, 0, 700, 53
20804, V, 1, 0, 0, 0, 0, 700, 53
20805, V, 1, 0, 0, 0, 0, 700, 53
20806, V, 1, 0, 0, 0, 0, 700, 53
20807, V, 1, 0, 0, 0, 0, 700, 53
20808, V, 1, 0, 0, 0, 0, 700, 53
20809, V, 1, 0, 0, 0, 0, 700, 53
20810, V, 1, 0, 0, 0, 0, 700, 53
20811, V, 1, 0, 0, 0, 0, 700, 53
20812, V, 1, 0, 0, 0, 0, 700, 53
20813, V, 1, 0, 0, 0, 0, 700, 53
20814, V, 1, 0, 0, 0, 0, 700, 53
20815, V, 1, 0, 0, 0, 0, 700, 53
20816, V, 1, 0, 0, 0, 0, 700, 53
20817, V, 1, 0, 0, 0, 0, 700, 53
20818, V, 1, 0, 0, 0, 0, 700, 53
20819, V, 1, 0, 0, 0, 0, 700, 53
20820, V, 1, 0, 0, 0, 0, 700, 53
20822, V, 1, 0, 0, 0, 0, 700, 53
20823, V, 1, 0, 0, 0, 0, 700, 53
20824, V, 1, 0, 0, 0, 0, 700, 53
20825, V, 1, 0, 0, 0, 0, 700, 53
20826, V, 1, 0, 0, 0, 0, 700, 53
20827, V, 1, 0, 0, 0, 0, 700, 54
20828, V, 1, 0, 0, 0, 0, 700, 54
20829, V, 1, 0, 0, 0, 0, 700, 54
20830, V, 1, 0, 0, 0, 0, 700, 54
20831, V, 1, 0, 0, 0, 0, 700, 54
20832, V, 1, 0, 0, 0, 0, 700, 54
20833, V, 1, 0, 0, 0, 0, 700, 54
20834, V, 1, 0, 0, 0, 0, 700, 54
20835, V, 1, 0, 0, 0, 0, 700, 54
20836, V, 1, 0, 0, 0, 0, 700, 54
20837, V, 1, 0, 0, 0, 0, 700, 54
20838, V, 1, 0, 0, 0, 0, 700, 54
20839, V, 1, 0, 0, 0, 0, 700, 54
20840, V, 1, 0, 0, 0, 0, 700, 54
20841, V, 1, 0, 0, 0, 0, 700, 54
20842, V, 1, 0, 0, 0, 0, 700, 55
20843, V, 1, 0, 0, 0, 0, 700, 55
20844, V, 1, 0, 0, 0, 0, 700, 55
20845, V, 1, 0, 0, 0, 0, 700, 55
20846, V, 1, 0, 0, 0, 0, 700, 55
20847, V, 1, 0, 0, 0, 0, 700, 55
20848, V, 1, 0, 0, 0, 0, 700, 55
20849, V, 1, 0, 0, 0, 0, 700, 55
20850, V, 1, 0, 0, 0, 0, 700, 55
20851, V, 1, 0, 0, 0, 0, 700, 55
20852, V, 1, 0, 0, 0, 0, 700, 55
20853, V, 1, 0, 0, 0, 0, 700, 55
20854, V, 1, 0, 0, 0, 0, 700, 55
20855, V, 1, 0, 0, 0, 0, 700, 55
20856, V, 1, 0, 0, 0, 0, 700, 55
20857, V, 1, 0, 0, 0, 0, 700, 55
20858, V, 1, 0, 0, 0, 0, 700, 55
20859, V, 1, 0, 0, 0, 0, 700, 55
20860, V, 1, 0, 0, 0, 0, 700, 55
20861, V, 1, 0, 0, 0, 0, 700, 55
20862, V, 1, 0, 0, 0, 0, 700, 56
20864, V, 1, 0, 0, 0, 0, 700, 56
20865, V, 1, 0, 0, 0, 0, 700, 56
20866, V, 1, 0, 0, 0, 0, 700, 56
20867, V, 1, 0, 0, 0, 0, 700, 56
20868, V, 1, 0, 0, 0, 0, 700, 56
20869, V, 1, 0, 0, 0, 0, 700, 56
20870, V, 1, 0, 0, 0, 0, 700, 56
20871, V, 1, 0, 0, 0, 0, 700, 56
20872, V, 1, 0, 0, 0, 0, 700, 56
20873, V, 1, 0, 0, 0, 0, 700, 56
20874, V, 1, 0, 0, 0, 0, 700, 56
20875, V, 1, 0, 0, 0, 0, 700, 56
20876, V, 1, 0, 0, 0, 0, 700, 56
20877, V, 1, 0, 0, 0, 0, 700, 56
20878, V, 1, 0, 0, 0, 0, 700, 56
20879, V, 1, 0, 0, 0, 0, 700, 56
20880, V, 1, 0, 0, 0, 0, 700, 56
20881, V, 1, 0, 0, 0, 0, 700, 56
20882, V, 1, 0, 0, 0, 0, 700, 56
20883, V, 1, 0, 0, 0, 0, 700, 56
20884, V, 1, 0, 0, 0, 0, 700, 56
20885, V, 1, 0, 0, 0, 0, 700, 56
20886, V, 1, 0, 0, 0, 0, 700, 56
20887, V, 1, 0, 0, 0, 0, 700, 56
20888, V, 1, 0, 0, 0, 0, 700, 56
20889, V, 1, 0, 0, 0, 0, 700, 56
20890, V, 1, 0, 0, 0, 0, 700, 56
20891, V, 1, 0, 0, 0, 0, 700, 56
20892, V, 1, 0, 0, 0, 0, 700, 56
20893, V, 1, 0, 0, 0, 0, 700, 56
20894, V, 1, 0, 0, 0, 0, 700, 56
20895, V, 1, 0, 0, 0, 0, 700, 56
20896, V, 1, 0, 0, 0, 0, 700, 56
20897, V, 1, 0, 0, 0, 0, 700, 56
20898, V, 1, 0, 0, 0, 0, 700, 56
20899, V, 1, 0, 0, 0, 0, 700, 56
20900, V, 1, 0, 0, 0, 0, 700, 56
20901, V, 1, 0, 0, 0, 0, 700, 57
20902, V, 1, 0, 0, 0, 0, 700, 57
20903, V, 1, 0, 0, 0, 0, 700, 57
20904, V, 1, 0, 0, 0, 0, 700, 57
20905, V, 1, 0, 0, 0, 0, 700, 57
20907, V, 1, 0, 0, 0, 0, 700, 58
20908, V, 1, 0, 0, 0, 0, 700, 58
20909, V, 1, 0, 0, 0, 0, 700, 58
20910, V, 1, 0, 0, 0, 0, 700, 59
20911, V, 1, 0, 0, 0, 0, 700, 59
20912, V, 1, 0, 0, 0, 0, 700, 59
20913, V, 1, 0, 0, 0, 0, 700, 59
20914, V, 1, 0, 0, 0, 0, 700, 60
20915, V, 1, 0, 0, 0, 0, 700, 60
20916, V, 1, 0, 0, 0, 0, 700, 60
20917, V, 1, 0, 0, 0, 0, 700, 60
20918, V, 1, 0, 0, 0, 0, 700, 60
20919, V, 1, 0, 0, 0, 0, 700, 61
20920, V, 1, 0, 0, 0, 0, 700, 61
20921, V, 1, 0, 0, 0, 0, 700, 61
20922, V, 1, 0, 0, 0, 0, 700, 61
20923, V, 1, 0, 0, 0, 0, 700, 61
20924, V, 1, 0, 0, 0, 0, 700, 62
20925, V, 1, 0, 0, 0, 0, 700, 62
20926, V, 1, 0, 0, 0, 0, 700, 62
20927, V, 1, 0, 0, 0, 0, 700, 62
20928, V, 1, 0, 0, 0, 0, 700, 62
20929, V, 1, 0, 0, 0, 0, 700, 62
20930, V, 1, 0, 0, 0, 0, 700, 63
20931, V, 1, 0, 0, 0, 0, 700, 63
20932, V, 1, 0, 0, 0, 0, 700, 63
20933, V, 1, 0, 0, 0, 0, 700, 63
20934, V, 1, 0, 0, 0, 0, 700, 63
20935, V, 1, 0, 0, 0, 0, 700, 63
20936, V, 1, 0, 0, 0, 0, 700, 64
20937, V, 1, 0, 0, 0, 0, 700, 64
20938, V, 1, 0, 0, 0, 0, 700, 64
20939, V, 1, 0, 0, 0, 0, 700, 64
20940, V, 1, 0, 0, 0, 0, 700, 64
20941, V, 1, 0, 0, 0, 0, 700, 64
20942, V, 1, 0, 0, 0, 0, 700, 64
20943, V, 1, 0, 0, 0, 0, 700, 64
20944, V, 1, 0, 0, 0, 0, 700, 65
20945, V, 1, 0, 0, 0, 0, 700, 65
20946, V, 1, 0, 0, 0, 0, 700, 65
20947, V, 1, 0, 0, 0, 0, 700, 65
20948, V, 1, 0, 0, 0, 0, 700, 65
20950, V, 1, 0, 0, 0, 0, 700, 65
20951, V, 1, 0, 0, 0, 0, 700, 65
20952, V, 1, 0, 0, 0, 0, 700, 65
20953, V, 1, 0, 0, 0, 0, 700, 65
20954, V, 1, 0, 0, 0, 0, 700, 65
20955, V, 1, 0, 0, 0, 0, 700, 66
20956, V, 1, 0, 0, 0, 0, 700, 66
20957, V, 1, 0, 0, 0, 0, 700, 66
20958, V, 1, 0, 0, 0, 0, 700, 66
20959, V, 1, 0, 0, 0, 0, 700, 66
20960, V, 1, 0, 0, 0, 0, 700, 66
20961, V, 1, 0, 0, 0, 0, 700, 66
20962, V, 1, 0, 0, 0, 0, 700, 66
20963, V, 1, 0, 0, 0, 0, 700, 66
20964, V, 1, 0, 0, 0, 0, 700, 66
20965, V, 1, 0, 0, 0, 0, 700, 67
20966, V, 1, 0, 0, 0, 0, 700, 67
20967, V, 1, 0, 0, 0, 0, 700, 67
20968, V, 1, 0, 0, 0, 0, 700, 67
20969, V, 1, 0, 0, 0, 0, 700, 67
20970, V, 1, 0, 0, 0, 0, 700, 67
20971, V, 1, 0, 0, 0, 0, 700, 67
20972, V, 1, 0, 0, 0, 0, 700, 67
20973, V, 1, 0, 0, 0, 0, 700, 67
20974, V, 1, 0, 0, 0, 0, 700, 67
20975, V, 1, 0, 0, 0, 0, 700, 67
20976, V, 1, 0, 0, 0, 0, 700, 67
20977, V, 1, 0, 0, 0, 0, 700, 67
20978, V, 1, 0, 0, 0, 0, 700, 68
20979, V, 1, 1, 0, 0, 0, 700, 68
20979, V, 1, 1, 0, 0, 0, 700, 68
20980, V, 1, 0, 0, 0, 0, 700, 68
20980, V, 1, 0, 0, 0, 0, 700, 68
20981, V, 1, 0, 0, 0, 0, 700, 68
20982, V, 1, 0, 0, 0, 0, 700, 68
20983, V, 1, 0, 0, 0, 0, 700, 68
20984, V, 1, 0, 0, 0, 0, 700, 68
20985, V, 1, 0, 0, 0, 0, 700, 68
20986, V, 1, 0, 0, 0, 0, 700, 68
20987, V, 1, 0, 0, 0, 0, 700, 69
20988, V, 1, 0, 0, 0, 0, 700, 69
20989, V, 1, 0, 0, 0, 0, 700, 69
20990, V, 1, 0, 0, 0, 0, 700, 69
20992, V, 1, 0, 0, 0, 0, 700, 69
20993, V, 1, 0, 0, 0, 0, 700, 69
20994, V, 1, 0, 0, 0, 0, 700, 69
20995, V, 1, 0, 0, 0, 0, 700, 69
20996, V, 1, 0, 0, 0, 0, 700, 69
20997, V, 1, 0, 0, 0, 0, 700, 69
20998, V, 1, 0, 0, 0, 0, 700, 69
20999, V, 1, 0, 0, 0, 0, 700, 69
21000, V, 1, 0, 0, 0, 0, 700, 69
21001, V, 1, 0, 0, 0, 0, 700, 69
21002, V, 1, 0, 0, 0, 0, 700, 69
21003, V, 1, 0, 0, 0, 0, 700, 69
21004, V, 1, 0, 0, 0, 0, 700, 69
21005, V, 1, 0, 0, 0, 0, 700, 69
21006, V, 1, 0, 0, 0, 0, 700, 69
21007, V, 1, 0, 0, 0, 0, 700, 69
21008, V, 1, 0, 0, 0, 0, 700, 69
21009, V, 1, 0, 0, 0, 0, 700, 69
21010, V, 1, 0, 0, 0, 0, 700, 69
21011, V, 1, 0, 0, 0, 0, 700, 69
21012, V, 1, 0, 0, 0, 0, 700, 69
21013, V, 1, 0, 0, 0, 0, 700, 69
21014, V, 1, 0, 0, 0, 0, 700, 69
21015, V, 1, 0, 0, 0, 0, 700, 69
21016, V, 1, 0, 0, 0, 0, 700, 70
21017, V, 1, 0, 0, 0, 0, 700, 70
21018, V, 1, 0, 0, 0, 0, 700, 70
21019, V, 1, 0, 0, 0, 0, 700, 70
21020, V, 1, 0, 0, 0, 0, 700, 70
21021, V, 1, 0, 0, 0, 0, 700, 70
21022, V, 1, 0, 0, 0, 0, 700, 70
21023, V, 1, 0, 0, 0, 0, 700, 70
21024, V, 1, 0, 0, 0, 0, 700, 70
21025, V, 1, 0, 0, 0, 0, 700, 70
21026, V, 1, 0, 0, 0, 0, 700, 70
21027, V, 1, 0, 0, 0, 0, 700, 70
21028, V, 1, 0, 0, 0, 0, 700, 70
21029, V, 1, 0, 0, 0, 0, 700, 70
21030, V, 1, 0, 0, 0, 0, 700, 70
21031, V, 1, 0, 0, 0, 0, 700, 70
21032, V, 1, 0, 0, 0, 0, 700, 70
21033, V, 1, 0, 0, 0, 0, 700, 70
21035, V, 1, 0, 0, 0, 0, 700, 70
21036, V, 1, 0, 0, 0, 0, 700, 70
21037, V, 1, 0, 0, 0, 0, 700, 70
21038, V, 1, 0, 0, 0, 0, 700, 70
21039, V, 1, 0, 0, 0, 0, 700, 70
21040, V, 1, 0, 0, 0, 0, 700, 70
21041, V, 1, 0, 0, 0, 0, 700, 70
21042, V, 1, 0, 0, 0, 0, 700, 70
21043, V, 1, 0, 0, 0, 0, 700, 70
21044, V, 1, 0, 0, 0, 0, 700, 70
21045, V, 1, 0, 0, 0, 0, 700, 70
21046, V, 1, 0, 0, 0, 0, 700, 70
21047, V, 1, 0, 0, 0, 0, 700, 70
21048, V, 1, 0, 0, 0, 0, 700, 70
21049, V, 1, 0, 0, 0, 0, 700, 70
21050, V, 1, 0, 0, 0, 0, 700, 70
21051, V, 1, 0, 0, 0, 0, 700, 70
21052, V, 1, 0, 0, 0, 0, 700, 70
21053, V, 1, 0, 0, 0, 0, 700, 70
21054, V, 1, 0, 0, 0, 0, 700, 70
21055, V, 1, 0, 0, 0, 0, 700, 70
21056, V, 1, 0, 0, 0, 0, 700, 70
21057, V, 1, 0, 0, 0, 0, 700, 70
21058, V, 1, 0, 0, 0, 0, 700, 70
21059, V, 1, 0, 0, 0, 0, 700, 70
21060, V, 1, 0, 0, 0, 0, 700, 70
21061, V, 1, 0, 0, 0, 0, 700, 71
21062, V, 1, 0, 0, 0, 0, 700, 71
21063, V, 1, 0, 0, 0, 0, 700, 71
21064, V, 1, 0, 0, 0, 0, 700, 71
21065, V, 1, 0, 0, 0, 0, 700, 71
21066, V, 1, 0, 0, 0, 0, 700, 71
21067, V, 1, 0, 0, 0, 0, 700, 71
21068, V, 1, 0, 0, 0, 0, 700, 71
21069, V, 1, 0, 0, 0, 0, 700, 71
21070, V, 1, 0, 0, 0, 0, 700, 71
21071, V, 1, 0, 0, 0, 0, 700, 71
21072, V, 1, 0, 0, 0, 0, 700, 71
21073, V, 1, 0, 0, 0, 0, 700, 71
21074, V, 1, 0, 0, 0, 0, 700, 71
21075, V, 1, 0, 0, 0, 0, 700, 71
21076, V, 1, 0, 0, 0, 0, 700, 71
21078, V, 1, 0, 0, 0, 0, 700, 71
21079, V, 1, 0, 0, 0, 0, 700, 71
21080, V, 1, 0, 0, 0, 0, 700, 71
21081, V, 1, 0, 0, 0, 0, 700, 71
21082, V, 1, 0, 0, 0, 0, 700, 71
21083, V, 1, 0, 0, 0, 0, 700, 71
21084, V, 1, 0, 0, 0, 0, 700, 71
21085, V, 1, 0, 0, 0, 0, 700, 71
21086, V, 1, 0, 0, 0, 0, 700, 71
21087, V, 1, 0, 0, 0, 0, 700, 71
21088, V, 1, 0, 0, 0, 0, 700, 71
21089, V, 1, 0, 0, 0, 0, 700, 71
21090, V, 1, 0, 0, 0, 0, 700, 71
21091, V, 1, 0, 0, 0, 0, 700, 71
21092, V, 1, 0, 0, 0, 0, 700, 71
21093, V, 1, 0, 0, 0, 0, 700, 71
21094, V, 1, 0, 0, 0, 0, 700, 71
21095, V, 1, 0, 0, 0, 0, 700, 71
21096, V, 1, 0, 0, 0, 0, 700, 71
21097, V, 1, 0, 0, 0, 0, 700, 71
21098, V, 1, 0, 0, 0, 0, 700, 71
21099, V, 1, 0, 0, 0, 0, 700, 71
21100, V, 1, 0, 0, 0, 0, 700, 71
21101, V, 1, 0, 0, 0, 0, 700, 71
21102, V, 1, 0, 0, 0, 0, 700, 71
21103, V, 1, 0, 0, 0, 0, 700, 71
21104, V, 1, 0, 0, 0, 0, 700, 71
21105, V, 1, 0, 0, 0, 0, 700, 71
21106, V, 1, 0, 0, 0, 0, 700, 71
21107, V, 1, 0, 0, 0, 0, 700, 71
21108, V, 1, 0, 0, 0, 0, 700, 71
21109, V, 1, 0, 0, 0, 0, 700, 71
21110, V, 1, 0, 0, 0, 0, 700, 71
21111, V, 1, 0, 0, 0, 0, 700, 71
21112, V, 1, 0, 0, 0, 0, 700, 71
21113, V, 1, 0, 0, 0, 0, 700, 71
21114, V, 1, 0, 0, 0, 0, 700, 71
21115, V, 1, 0, 0, 0, 0, 700, 71
21116, V, 1, 0, 0, 0, 0, 700, 71
21117, V, 1, 0, 0, 0, 0, 700, 71
21118, V, 1, 0, 0, 0, 0, 700, 71
21120, V, 1, 0, 0, 0, 0, 700, 71
21121, V, 1, 0, 0, 0, 0, 700, 72
21122, V, 1, 0, 0, 0, 0, 700, 71
21123, V, 1, 0, 0, 0, 0, 700, 72
21124, V, 1, 0, 0, 0, 0, 700, 72
21125, V, 1, 0, 0, 0, 0, 700, 72
21126, V, 1, 0, 0, 0, 0, 700, 72
21127, V, 1, 0, 0, 0, 0, 700, 71
21128, V, 1, 0, 0, 0, 0, 700, 72
21129, V, 1, 0, 0, 0, 0, 700, 72
21130, V, 1, 0, 0, 0, 0, 700, 72
21131, V, 1, 0, 0, 0, 0, 700, 72
21132, V, 1, 0, 0, 0, 0, 700, 71
21133, V, 1, 0, 0, 0, 0, 700, 72
21134, V, 1, 0, 0, 0, 0, 700, 72
21135, V, 1, 0, 0, 0, 0, 700, 72
21136, V, 1, 0, 0, 0, 0, 700, 72
21137, V, 1, 0, 0, 0, 0, 700, 72
21138, V, 1, 0, 0, 0, 0, 700, 72
21139, V, 1, 0, 0, 0, 0, 700, 72
21140, V, 1, 0, 0, 0, 0, 700, 72
21141, V, 1, 0, 0, 0, 0, 700, 72
21142, V, 1, 0, 0, 0, 0, 700, 72
21143, V, 1, 0, 0, 0, 0, 700, 72
21144, V, 1, 0, 0, 0, 0, 700, 72
21145, V, 1, 0, 0, 0, 0, 700, 72
21146, V, 1, 0, 0, 0, 0, 700, 72
21147, V, 1, 0, 0, 0, 0, 700, 72
21148, V, 1, 0, 0, 0, 0, 700, 72
21149, V, 1, 0, 0, 0, 0, 700, 72
21150, V, 1, 0, 0, 0, 0, 700, 72
21151, V, 1, 0, 0, 0, 0, 700, 72
21152, V, 1, 0, 0, 0, 0, 700, 72
21153, V, 1, 0, 0, 0, 0, 700, 72
21154, V, 1, 0, 0, 0, 0, 700, 72
21155, V, 1, 0, 0, 0, 0, 700, 72
21156, V, 1, 0, 0, 0, 0, 700, 72
21157, V, 1, 0, 0, 0, 0, 700, 72
21158, V, 1, 0, 0, 0, 0, 700, 72
21159, V, 1, 0, 0, 0, 0, 700, 72
21160, V, 1, 0, 0, 0, 0, 700, 72
21161, V, 1, 0, 0, 0, 0, 700, 72
21163, V, 1, 0, 0, 0, 0, 700, 72
21164, V, 1, 0, 0, 0, 0, 700, 72
21165, V, 1, 0, 0, 0, 0, 700, 72
21166, V, 1, 0, 0, 0, 0, 700, 72
21167, V, 1, 0, 0, 0, 0, 700, 72
21168, V, 1, 0, 0, 0, 0, 700, 72
21169, V, 1, 0, 0, 0, 0, 700, 72
21170, V, 1, 0, 0, 0, 0, 700, 72
21171, V, 1, 0, 0, 0, 0, 700, 72
21172, V, 1, 0, 0, 0, 0, 700, 72
21173, V, 1, 1, 0, 0, 0, 700, 72
21173, V, 1, 1, 0, 0, 0, 700, 72
21174, V, 1, 0, 0, 0, 0, 700, 72
21174, V, 1, 0, 0, 0, 0, 700, 72
21175, V, 1, 0, 0, 0, 0, 700, 72
21176, V, 1, 0, 0, 0, 0, 700, 72
21177, V, 1, 0, 0, 0, 0, 700, 72
21178, V, 1, 0, 0, 0, 0, 700, 72
21179, V, 1, 1, 0, 0, 0, 700, 72
21179, V, 1, 1, 0, 0, 0, 700, 72
21180, V, 1, 0, 0, 0, 0, 700, 72
21180, V, 1, 0, 0, 0, 0, 700, 72
21181, V, 1, 0, 0, 0, 0, 700, 72
21182, V, 1, 0, 0, 0, 0, 700, 72
21183, V, 1, 0, 0, 0, 0, 700, 72
21184, V, 1, 0, 0, 0, 0, 700, 72
21185, V, 1, 0, 0, 0, 0, 700, 72
21186, V, 1, 0, 0, 0, 0, 700, 73
21187, V, 1, 0, 0, 0, 0, 700, 73
21188, V, 1, 0, 0, 0, 0, 700, 73
21189, V, 1, 0, 0, 0, 0, 700, 73
21190, V, 1, 0, 0, 0, 0, 700, 73
21191, V, 1, 0, 0, 0, 0, 700, 73
21192, V, 1, 0, 0, 0, 0, 700, 72
21193, V, 1, 0, 0, 0, 0, 700, 72
21194, V, 1, 0, 0, 0, 0, 700, 72
21195, V, 1, 0, 0, 0, 0, 700, 72
21196, V, 1, 0, 0, 0, 0, 700, 72
21197, V, 1, 0, 0, 0, 0, 700, 72
21198, V, 1, 0, 0, 0, 0, 700, 72
21199, V, 1, 0, 0, 0, 0, 700, 72
21200, V, 1, 0, 0, 0, 0, 700, 72
21201, V, 1, 0, 0, 0, 0, 700, 72
21202, V, 1, 0, 0, 0, 0, 700, 72
21203, V, 1, 0, 0, 0, 0, 700, 72
21204, V, 1, 0, 0, 0, 0, 700, 72
21206, V, 1, 0, 0, 0, 0, 700, 72
21207, V, 1, 0, 0, 0, 0, 700, 72
21208, V, 1, 0, 0, 0, 0, 700, 72
21209, V, 1, 0, 0, 0, 0, 700, 72
21210, V, 1, 0, 0, 0, 0, 700, 72
21211, V, 1, 0, 0, 0, 0, 700, 72
21212, V, 1, 0, 0, 0, 0, 700, 72
21213, V, 1, 0, 0, 0, 0, 700, 72
21214, V, 1, 0, 0, 0, 0, 700, 72
21215, V, 1, 0, 0, 0, 0, 700, 72
21216, V, 1, 0, 0, 0, 0, 700, 72
21217, V, 1, 0, 0, 0, 0, 700, 72
21218, V, 1, 0, 0, 0, 0, 700, 72
21219, V, 1, 0, 0, 0, 0, 700, 72
21220, V, 1, 0, 0, 0, 0, 700, 72
21221, V, 1, 0, 0, 0, 0, 700, 72
21222, V, 1, 0, 0, 0, 0, 700, 72
21223, V, 1, 0, 0, 0, 0, 700, 72
21224, V, 1, 0, 0, 0, 0, 700, 72
21225, V, 1, 0, 0, 0, 0, 700, 72
21226, V, 1, 0, 0, 0, 0, 700, 72
21227, V, 1, 0, 0, 0, 0, 700, 72
21228, V, 1, 0, 0, 0, 0, 700, 72
21229, V, 1, 0, 0, 0, 0, 700, 72
21230, V, 1, 0, 0, 0, 0, 700, 72
21231, V, 1, 0, 0, 0, 0, 700, 72
21232, V, 1, 0, 0, 0, 0, 700, 72
21233, V, 1, 0, 0, 0, 0, 700, 72
21234, V, 1, 0, 0, 0, 0, 700, 72
21235, V, 1, 0, 0, 0, 0, 700, 72
21236, V, 1, 0, 0, 0, 0, 700, 72
21237, V, 1, 0, 0, 0, 0, 700, 72
21238, V, 1, 0, 0, 0, 0, 700, 72
21239, V, 1, 0, 0, 0, 0, 700, 72
21240, V, 1, 0, 0, 0, 0, 700, 72
21241, V, 1, 0, 0, 0, 0, 700, 72
21242, V, 1, 0, 0, 0, 0, 700, 72
21243, V, 1, 0, 0, 0, 0, 700, 72
21244, V, 1, 0, 0, 0, 0, 700, 72
21245, V, 1, 0, 0, 0, 0, 700, 72
21246, V, 1, 0, 0, 0, 0, 700, 72
21248, V, 1, 0, 0, 0, 0, 700, 72
21249, V, 1, 0, 0, 0, 0, 700, 72
21250, V, 1, 0, 0, 0, 0, 700, 72
21251, V, 1, 0, 0, 0, 0, 700, 72
21252, V, 1, 0, 0, 0, 0, 700, 72
21253, V, 1, 0, 0, 0, 0, 700, 72
21254, V, 1, 0, 0, 0, 0, 700, 72
21255, V, 1, 0, 0, 0, 0, 700, 72
21256, V, 1, 0, 0, 0, 0, 700, 72
21257, V, 1, 0, 0, 0, 0, 700, 72
21258, V, 1, 1, 0, 0, 0, 700, 72
21258, V, 1, 1, 0, 0, 0, 700, 72
21259, V, 1, 0, 0, 0, 0, 700, 72
21259, V, 1, 0, 0, 0, 0, 700, 72
21260, V, 1, 0, 0, 0, 0, 700, 72
21261, V, 1, 0, 0, 0, 0, 700, 72
21262, V, 1, 0, 0, 0, 0, 700, 72
21263, V, 1, 0, 0, 0, 0, 700, 72
21264, V, 1, 0, 0, 0, 0, 700, 72
21265, V, 1, 0, 0, 0, 0, 700, 72
21266, V, 1, 0, 0, 0, 0, 700, 72
21267, V, 1, 0, 0, 0, 0, 700, 72
21268, V, 1, 0, 0, 0, 0, 700, 72
21269, V, 1, 0, 0, 0, 0, 700, 72
21270, V, 1, 0, 0, 0, 0, 700, 72
21271, V, 1, 0, 0, 0, 0, 700, 72
21272, V, 1, 0, 0, 0, 0, 700, 72
21273, V, 1, 0, 0, 0, 0, 700, 72
21274, V, 1, 0, 0, 0, 0, 700, 72
21275, V, 1, 0, 0, 0, 0, 700, 72
21276, V, 1, 0, 0, 0, 0, 700, 72
21277, V, 1, 0, 0, 0, 0, 700, 72
21278, V, 1, 0, 0, 0, 0, 700, 72
21279, V, 1, 0, 0, 0, 0, 700, 72
21280, V, 1, 0, 0, 0, 0, 700, 72
21281, V, 1, 0, 0, 0, 0, 700, 72
21282, V, 1, 0, 0, 0, 0, 700, 72
21283, V, 1, 0, 0, 0, 0, 700, 72
21284, V, 1, 0, 0, 0, 0, 700, 72
21285, V, 1, 0, 0, 0, 0, 700, 72
21286, V, 1, 0, 0, 0, 0, 700, 72
21287, V, 1, 0, 0, 0, 0, 700, 72
21288, V, 1, 0, 0, 0, 0, 700, 71
21289, V, 1, 0, 0, 0, 0, 700, 71
21291, V, 1, 0, 0, 0, 0, 700, 71
21292, V, 1, 0, 0, 0, 0, 700, 71
21293, V, 1, 0, 0, 0, 0, 700, 71
21294, V, 1, 0, 0, 0, 0, 700, 71
21295, V, 1, 0, 0, 0, 0, 700, 71
21296, V, 1, 0, 0, 0, 0, 700, 71
21297, V, 1, 0, 0, 0, 0, 700, 71
21298, V, 1, 0, 0, 0, 0, 700, 71
21299, V, 1, 0, 0, 0, 0, 700, 71
21300, V, 1, 0, 0, 0, 0, 700, 71
21301, V, 1, 0, 0, 0, 0, 700, 71
21302, V, 1, 1, 0, 0, 0, 700, 71
21302, V, 1, 1, 0, 0, 0, 700, 71
21303, V, 1, 0, 0, 0, 0, 700, 71
21303, V, 1, 0, 0, 0, 0, 700, 71
21304, V, 1, 0, 0, 0, 0, 700, 71
21305, V, 1, 0, 0, 0, 0, 700, 71
21306, V, 1, 0, 0, 0, 0, 700, 71
21307, V, 1, 0, 0, 0, 0, 700, 71
21308, V, 1, 0, 0, 0, 0, 700, 71
21309, V, 1, 0, 0, 0, 0, 700, 71
21310, V, 1, 0, 0, 0, 0, 700, 71
21311, V, 1, 0, 0, 0, 0, 700, 71
21312, V, 1, 0, 0, 0, 0, 700, 71
21313, V, 1, 0, 0, 0, 0, 700, 71
21314, V, 1, 0, 0, 0, 0, 700, 70
21315, V, 1, 0, 0, 0, 0, 700, 70
21316, V, 1, 0, 0, 0, 0, 700, 70
21317, V, 1, 0, 0, 0, 0, 700, 70
21318, V, 1, 0, 0, 0, 0, 700, 70
21319, V, 1, 0, 0, 0, 0, 700, 70
21320, V, 1, 0, 0, 0, 0, 700, 70
21321, V, 1, 0, 0, 0, 0, 700, 70
21322, V, 1, 0, 0, 0, 0, 700, 70
21323, V, 1, 0, 0, 0, 0, 700, 70
21324, V, 1, 0, 0, 0, 0, 700, 70
21325, V, 1, 0, 0, 0, 0, 700, 70
21326, V, 1, 0, 0, 0, 0, 700, 70
21327, V, 1, 0, 0, 0, 0, 700, 70
21328, V, 1, 0, 0, 0, 0, 700, 70
21329, V, 1, 0, 0, 0, 0, 700, 70
21330, V, 1, 0, 0, 0, 0, 700, 70
21331, V, 1, 0, 0, 0, 0, 700, 69
21332, V, 1, 0, 0, 0, 0, 700, 69
21334, V, 1, 0, 0, 0, 0, 700, 69
21335, V, 1, 0, 0, 0, 0, 700, 69
21336, V, 1, 0, 0, 0, 0, 700, 69
21337, V, 1, 0, 0, 0, 0, 700, 69
21338, V, 1, 0, 0, 0, 0, 700, 69
21339, V, 1, 0, 0, 0, 0, 700, 69
21340, V, 1, 1, 0, 0, 0, 700, 69
21340, V, 1, 1, 0, 0, 0, 700, 69
21341, V, 1, 0, 0, 0, 0, 700, 69
21341, V, 1, 0, 0, 0, 0, 700, 69
21342, V, 1, 0, 0, 0, 0, 700, 69
21343, V, 1, 0, 0, 0, 0, 700, 69
21344, V, 1, 0, 0, 0, 0, 700, 69
21345, V, 1, 0, 0, 0, 0, 700, 69
21346, V, 1, 0, 0, 0, 0, 700, 69
21347, V, 1, 0, 0, 0, 0, 700, 69
21348, V, 1, 0, 0, 0, 0, 700, 69
21349, V, 1, 0, 0, 0, 0, 700, 69
21350, V, 1, 0, 0, 0, 0, 700, 69
21351, V, 1, 0, 0, 0, 0, 700, 69
21352, V, 1, 0, 0, 0, 0, 700, 69
21353, V, 1, 0, 0, 0, 0, 700, 69
21354, V, 1, 0, 0, 0, 0, 700, 69
21355, V, 1, 0, 0, 0, 0, 700, 69
21356, V, 1, 0, 0, 0, 0, 700, 69
21357, V, 1, 0, 0, 0, 0, 700, 69
21358, V, 1, 0, 0, 0, 0, 700, 69
21359, V, 1, 0, 0, 0, 0, 700, 69
21360, V, 1, 0, 0, 0, 0, 700, 69
21361, V, 1, 0, 0, 0, 0, 700, 69
21362, V, 1, 0, 0, 0, 0, 700, 69
21363, V, 1, 0, 0, 0, 0, 700, 69
21364, V, 1, 0, 0, 0, 0, 700, 69
21365, V, 1, 0, 0, 0, 0, 700, 69
21366, V, 1, 0, 0, 0, 0, 700, 69
21367, V, 1, 0, 0, 0, 0, 700, 69
21368, V, 1, 0, 0, 0, 0, 700, 69
21369, V, 1, 0, 0, 0, 0, 700, 69
21370, V, 1, 0, 0, 0, 0, 700, 69
21371, V, 1, 0, 0, 0, 0, 700, 69
21372, V, 1, 0, 0, 0, 0, 700, 69
21373, V, 1, 0, 0, 0, 0, 700, 69
21374, V, 1, 0, 0, 0, 0, 700, 68
21376, V, 1, 0, 0, 0, 0, 700, 68
21377, V, 1, 0, 0, 0, 0, 700, 69
21378, V, 1, 0, 0, 0, 0, 700, 69
21379, V, 1, 0, 0, 0, 0, 700, 68
21380, V, 1, 0, 0, 0, 0, 700, 68
21381, V, 1, 0, 0, 0, 0, 700, 68
21382, V, 1, 0, 0, 0, 0, 700, 68
21383, V, 1, 0, 0, 0, 0, 700, 68
21384, V, 1, 0, 0, 0, 0, 700, 68
21385, V, 1, 0, 0, 0, 0, 700, 68
21386, V, 1, 0, 0, 0, 0, 700, 68
21387, V, 1, 0, 0, 0, 0, 700, 68
21388, V, 1, 0, 0, 0, 0, 700, 68
21389, V, 1, 0, 0, 0, 0, 700, 68
21390, V, 1, 0, 0, 0, 0, 700, 68
21391, V, 1, 0, 0, 0, 0, 700, 68
21392, V, 1, 0, 0, 0, 0, 700, 68
21393, V, 1, 0, 0, 0, 0, 700, 68
21394, V, 1, 0, 0, 0, 0, 700, 68
21395, V, 1, 0, 0, 0, 0, 700, 68
21396, V, 1, 0, 0, 0, 0, 700, 68
21397, V, 1, 0, 0, 0, 0, 700, 68
21398, V, 1, 0, 0, 0, 0, 700, 68
21399, V, 1, 0, 0, 0, 0, 700, 68
21400, V, 1, 0, 0, 0, 0, 700, 68
21401, V, 1, 0, 0, 0, 0, 700, 68
21402, V, 1, 0, 0, 0, 0, 700, 68
21403, V, 1, 0, 0, 0, 0, 700, 68
21404, V, 1, 0, 0, 0, 0, 700, 68
21405, V, 1, 0, 0, 0, 0, 700, 68
21406, V, 1, 0, 0, 0, 0, 700, 68
21407, V, 1, 0, 0, 0, 0, 700, 68
21408, V, 1, 0, 0, 0, 0, 700, 68
21409, V, 1, 0, 0, 0, 0, 700, 68
21410, V, 1, 0, 0, 0, 0, 700, 68
21411, V, 1, 0, 0, 0, 0, 700, 68
21412, V, 1, 0, 0, 0, 0, 700, 68
21413, V, 1, 0, 0, 0, 0, 700, 68
21414, V, 1, 0, 0, 0, 0, 700, 68
21415, V, 1, 0, 0, 0, 0, 700, 68
21416, V, 1, 0, 0, 0, 0, 700, 68
21417, V, 1, 0, 0, 0, 0, 700, 68
21419, V, 1, 0, 0, 0, 0, 700, 68
21420, V, 1, 0, 0, 0, 0, 700, 68
21421, V, 1, 0, 0, 0, 0, 700, 68
21422, V, 1, 0, 0, 0, 0, 700, 68
21423, V, 1, 0, 0, 0, 0, 700, 68
21424, V, 1, 0, 0, 0, 0, 700, 68
21425, V, 1, 0, 0, 0, 0, 700, 68
21426, V, 1, 0, 0, 0, 0, 700, 68
21427, V, 1, 0, 0, 0, 0, 700, 68
21428, V, 1, 0, 0, 0, 0, 700, 68
21429, V, 1, 0, 0, 0, 0, 700, 68
21430, V, 1, 0, 0, 0, 0, 700, 68
21431, V, 1, 0, 0, 0, 0, 700, 68
21432, V, 1, 1, 0, 0, 0, 700, 68
21432, V, 1, 1, 0, 0, 0, 700, 68
21433, V, 1, 0, 0, 0, 0, 700, 68
21433, V, 1, 0, 0, 0, 0, 700, 68
21434, V, 1, 0, 0, 0, 0, 700, 68
21435, V, 1, 0, 0, 0, 0, 700, 68
21436, V, 1, 0, 0, 0, 0, 700, 68
21437, V, 1, 0, 0, 0, 0, 700, 68
21438, V, 1, 0, 0, 0, 0, 700, 68
21439, V, 1, 0, 0, 0, 0, 700, 68
21440, V, 1, 0, 0, 0, 0, 700, 68
21441, V, 1, 0, 0, 0, 0, 700, 68
21442, V, 1, 0, 0, 0, 0, 700, 68
21443, V, 1, 0, 0, 0, 0, 700, 68
21444, V, 1, 0, 0, 0, 0, 700, 68
21445, V, 1, 0, 0, 0, 0, 700, 68
21446, V, 1, 0, 0, 0, 0, 700, 68
21447, V, 1, 0, 0, 0, 0, 700, 68
21448, V, 1, 0, 0, 0, 0, 700, 68
21449, V, 1, 0, 0, 0, 0, 700, 68
21450, V, 1, 0, 0, 0, 0, 700, 68
21451, V, 1, 0, 0, 0, 0, 700, 68
21452, V, 1, 0, 0, 0, 0, 700, 68
21453, V, 1, 0, 0, 0, 0, 700, 68
21454, V, 1, 0, 0, 0, 0, 700, 68
21455, V, 1, 1, 0, 0, 0, 700, 68
21455, V, 1, 1, 0, 0, 0, 700, 68
21456, V, 1, 0, 0, 0, 0, 700, 68
21456, V, 1, 0, 0, 0, 0, 700, 68
21457, V, 1, 0, 0, 0, 0, 700, 68
21458, V, 1, 0, 0, 0, 0, 700, 68
21459, V, 1, 0, 0, 0, 0, 700, 68
21460, V, 1, 0, 0, 0, 0, 700, 68
21462, V, 1, 0, 0, 0, 0, 700, 68
21463, V, 1, 0, 0, 0, 0, 700, 68
21464, V, 1, 0, 0, 0, 0, 700, 68
21465, V, 1, 0, 0, 0, 0, 700, 68
21466, V, 1, 0, 0, 0, 0, 700, 68
21467, V, 1, 0, 0, 0, 0, 700, 68
21468, V, 1, 0, 0, 0, 0, 700, 68
21469, V, 1, 0, 0, 0, 0, 700, 68
21470, V, 1, 0, 0, 0, 0, 700, 68
21471, V, 1, 0, 0, 0, 0, 700, 68
21472, V, 1, 0, 0, 0, 0, 700, 68
21473, V, 1, 0, 0, 0, 0, 700, 68
21474, V, 1, 0, 0, 0, 0, 700, 68
21475, V, 1, 0, 0, 0, 0, 700, 68
21476, V, 1, 0, 0, 0, 0, 700, 68
21477, V, 1, 0, 0, 0, 0, 700, 68
21478, V, 1, 0, 0, 0, 0, 700, 68
21479, V, 1, 0, 0, 0, 0, 700, 68
21480, V, 1, 0, 0, 0, 0, 700, 68
21481, V, 1, 0, 0, 0, 0, 700, 68
21482, V, 1, 0, 0, 0, 0, 700, 68
21483, V, 1, 0, 0, 0, 0, 700, 68
21484, V, 1, 0, 0, 0, 0, 700, 68
21485, V, 1, 0, 0, 0, 0, 700, 68
21486, V, 1, 0, 0, 0, 0, 700, 68
21487, V, 1, 0, 0, 0, 0, 700, 68
21488, V, 1, 0, 0, 0, 0, 700, 68
21489, V, 1, 0, 0, 0, 0, 700, 68
21490, V, 1, 0, 0, 0, 0, 700, 68
21491, V, 1, 0, 0, 0, 0, 700, 68
21492, V, 1, 0, 0, 0, 0, 700, 68
21493, V, 1, 0, 0, 0, 0, 700, 68
21494, V, 1, 0, 0, 0, 0, 700, 68
21495, V, 1, 0, 0, 0, 0, 700, 68
21496, V, 1, 0, 0, 0, 0, 700, 68
21497, V, 1, 0, 0, 0, 0, 700, 68
21498, V, 1, 0, 0, 0, 0, 700, 68
21499, V, 1, 0, 0, 0, 0, 700, 68
21500, V, 1, 0, 0, 0, 0, 700, 68
21501, V, 1, 0, 0, 0, 0, 700, 68
21502, V, 1, 0, 0, 0, 0, 700, 68
21504, V, 1, 0, 0, 0, 0, 700, 68
21505, V, 1, 0, 0, 0, 0, 700, 68
21506, V, 1, 0, 0, 0, 0, 700, 68
21507, V, 1, 0, 0, 0, 0, 700, 68
21508, V, 1, 1, 0, 0, 0, 700, 69
21508, V, 1, 1, 0, 0, 0, 700, 69
21509, V, 1, 0, 0, 0, 0, 700, 68
21509, V, 1, 0, 0, 0, 0, 700, 68
21510, V, 1, 0, 0, 0, 0, 700, 69
21511, V, 1, 0, 0, 0, 0, 700, 69
21512, V, 1, 0, 0, 0, 0, 700, 69
21513, V, 1, 0, 0, 0, 0, 700, 69
21514, V, 1, 0, 0, 0, 0, 700, 69
21515, V, 1, 0, 0, 0, 0, 700, 69
21516, V, 1, 0, 0, 0, 0, 700, 69
21517, V, 1, 0, 0, 0, 0, 700, 69
21518, V, 1, 0, 0, 0, 0, 700, 69
21519, V, 1, 0, 0, 0, 0, 700, 69
21520, V, 1, 0, 0, 0, 0, 700, 69
21521, V, 1, 0, 0, 0, 0, 700, 69
21522, V, 1, 0, 0, 0, 0, 700, 69
21523, V, 1, 0, 0, 0, 0, 700, 70
21524, V, 1, 0, 0, 0, 0, 700, 70
21525, V, 1, 0, 0, 0, 0, 700, 70
21526, V, 1, 0, 0, 0, 0, 700, 70
21527, V, 1, 0, 0, 0, 0, 700, 70
21528, V, 1, 0, 0, 0, 0, 700, 70
21529, V, 1, 0, 0, 0, 0, 700, 70
21530, V, 1, 0, 0, 0, 0, 700, 70
21531, V, 1, 0, 0, 0, 0, 700, 70
21532, V, 1, 0, 0, 0, 0, 700, 70
21533, V, 1, 0, 0, 0, 0, 700, 70
21534, V, 1, 0, 0, 0, 0, 700, 70
21535, V, 1, 0, 0, 0, 0, 700, 70
21536, V, 1, 0, 0, 0, 0, 700, 70
21537, V, 1, 0, 0, 0, 0, 700, 70
21538, V, 1, 0, 0, 0, 0, 700, 70
21539, V, 1, 0, 0, 0, 0, 700, 70
21540, V, 1, 0, 0, 0, 0, 700, 70
21541, V, 1, 0, 0, 0, 0, 700, 70
21542, V, 1, 0, 0, 0, 0, 700, 70
21543, V, 1, 0, 0, 0, 0, 700, 70
21544, V, 1, 0, 0, 0, 0, 700, 70
21545, V, 1, 0, 0, 0, 0, 700, 70
21547, V, 1, 0, 0, 0, 0, 700, 70
21548, V, 1, 0, 0, 0, 0, 700, 70
21549, V, 1, 0, 0, 0, 0, 700, 70
21550, V, 1, 0, 0, 0, 0, 700, 70
21551, V, 1, 0, 0, 0, 0, 700, 70
21552, V, 1, 0, 0, 0, 0, 700, 70
21553, V, 1, 0, 0, 0, 0, 700, 70
21554, V, 1, 0, 0, 0, 0, 700, 70
21555, V, 1, 0, 0, 0, 0, 700, 70
21556, V, 1, 0, 0, 0, 0, 700, 70
21557, V, 1, 1, 0, 0, 0, 700, 70
21557, V, 1, 1, 0, 0, 0, 700, 70
21558, V, 1, 0, 0, 0, 0, 700, 70
21558, V, 1, 0, 0, 0, 0, 700, 70
21559, V, 1, 0, 0, 0, 0, 700, 70
21560, V, 1, 0, 0, 0, 0, 700, 71
21561, V, 1, 0, 0, 0, 0, 700, 71
21562, V, 1, 0, 0, 0, 0, 700, 71
21563, V, 1, 0, 0, 0, 0, 700, 71
21564, V, 1, 0, 0, 0, 0, 700, 71
21565, V, 1, 0, 0, 0, 0, 700, 71
21566, V, 1, 0, 0, 0, 0, 700, 71
21567, V, 1, 1, 0, 0, 0, 700, 71
21567, V, 1, 1, 0, 0, 0, 700, 71
21568, V, 1, 0, 0, 0, 0, 700, 71
21568, V, 1, 0, 0, 0, 0, 700, 71
21569, V, 1, 0, 0, 0, 0, 700, 71
21570, V, 1, 0, 0, 0, 0, 700, 71
21571, V, 1, 0, 0, 0, 0, 700, 71
21572, V, 1, 0, 0, 0, 0, 700, 71
21573, V, 1, 0, 0, 0, 0, 700, 71
21574, V, 1, 1, 0, 0, 0, 700, 71
21574, V, 1, 1, 0, 0, 0, 700, 71
21575, V, 1, 0, 0, 0, 0, 700, 72
21575, V, 1, 0, 0, 0, 0, 700, 72
21576, V, 1, 0, 0, 0, 0, 700, 72
21577, V, 1, 0, 0, 0, 0, 700, 72
21578, V, 1, 0, 0, 0, 0, 700, 72
21579, V, 1, 0, 0, 0, 0, 700, 72
21580, V, 1, 0, 0, 0, 0, 700, 72
21581, V, 1, 0, 0, 0, 0, 700, 72
21582, V, 1, 0, 0, 0, 0, 700, 72
21583, V, 1, 0, 0, 0, 0, 700, 72
21584, V, 1, 0, 0, 0, 0, 700, 72
21585, V, 1, 0, 0, 0, 0, 700, 72
21586, V, 1, 0, 0, 0, 0, 700, 72
21587, V, 1, 0, 0, 0, 0, 700, 72
21588, V, 1, 0, 0, 0, 0, 700, 72
21590, V, 1, 1, 0, 0, 0, 700, 72
21590, V, 1, 1, 0, 0, 0, 700, 72
21591, V, 1, 0, 0, 0, 0, 700, 72
21591, V, 1, 0, 0, 0, 0, 700, 72
21592, V, 1, 0, 0, 0, 0, 700, 72
21593, V, 1, 0, 0, 0, 0, 700, 72
21594, V, 1, 0, 0, 0, 0, 700, 72
21595, V, 1, 0, 0, 0, 0, 700, 72
21596, V, 1, 0, 0, 0, 0, 700, 72
21597, V, 1, 0, 0, 0, 0, 700, 72
21598, V, 1, 0, 0, 0, 0, 700, 72
21599, V, 1, 0, 0, 0, 0, 700, 72
21600, V, 1, 0, 0, 0, 0, 700, 72
21601, V, 1, 0, 0, 0, 0, 700, 72
21602, V, 1, 0, 0, 0, 0, 700, 72
21603, V, 1, 0, 0, 0, 0, 700, 72
21604, V, 1, 0, 0, 0, 0, 700, 72
21605, V, 1, 0, 0, 0, 0, 700, 72
21606, V, 1, 0, 0, 0, 0, 700, 72
21607, V, 1, 0, 0, 0, 0, 700, 72
21608, V, 1, 0, 0, 0, 0, 700, 72
21609, V, 1, 0, 0, 0, 0, 700, 72
21610, V, 1, 0, 0, 0, 0, 700, 72
21611, V, 1, 0, 0, 0, 0, 700, 72
21612, V, 1, 0, 0, 0, 0, 700, 72
21613, V, 1, 0, 0, 0, 0, 700, 72
21614, V, 1, 1, 0, 0, 0, 700, 72
21614, V, 1, 1, 0, 0, 0, 700, 72
21615, V, 1, 0, 0, 0, 0, 700, 72
21615, V, 1, 0, 0, 0, 0, 700, 72
21616, V, 1, 1, 0, 0, 0, 700, 72
21616, V, 1, 1, 0, 0, 0, 700, 72
21617, V, 1, 0, 0, 0, 0, 700, 72
21617, V, 1, 0, 0, 0, 0, 700, 72
21618, V, 1, 0, 0, 0, 0, 700, 72
21619, V, 1, 0, 0, 0, 0, 700, 72
21620, V, 1, 0, 0, 0, 0, 700, 72
21621, V, 1, 0, 0, 0, 0, 700, 73
21622, V, 1, 0, 0, 0, 0, 700, 73
21623, V, 1, 0, 0, 0, 0, 700, 73
21624, V, 1, 0, 0, 0, 0, 700, 73
21625, V, 1, 0, 0, 0, 0, 700, 73
21626, V, 1, 0, 0, 0, 0, 700, 73
21627, V, 1, 0, 0, 0, 0, 700, 73
21628, V, 1, 0, 0, 0, 0, 700, 73
21629, V, 1, 0, 0, 0, 0, 700, 73
21630, V, 1, 0, 0, 0, 0, 700, 73
21632, V, 1, 0, 0, 0, 0, 700, 73
21633, V, 1, 0, 0, 0, 0, 700, 72
21634, V, 1, 0, 0, 0, 0, 700, 72
21635, V, 1, 0, 0, 0, 0, 700, 72
21636, V, 1, 1, 0, 0, 0, 700, 72
21636, V, 1, 1, 0, 0, 0, 700, 72
21637, V, 1, 0, 0, 0, 0, 700, 72
21637, V, 1, 0, 0, 0, 0, 700, 72
21638, V, 1, 0, 0, 0, 0, 700, 72
21639, V, 1, 0, 0, 0, 0, 700, 73
21640, V, 1, 0, 0, 0, 0, 700, 72
21641, V, 1, 0, 0, 0, 0, 700, 73
21642, V, 1, 0, 0, 0, 0, 700, 73
21643, V, 1, 0, 0, 0, 0, 700, 73
21644, V, 1, 0, 0, 0, 0, 700, 73
21645, V, 1, 0, 0, 0, 0, 700, 73
21646, V, 1, 0, 0, 0, 0, 700, 73
21647, V, 1, 0, 0, 0, 0, 700, 73
21648, V, 1, 0, 0, 0, 0, 700, 73
21649, V, 1, 1, 0, 0, 0, 700, 73
21649, V, 1, 1, 0, 0, 0, 700, 73
21650, V, 1, 0, 0, 0, 0, 700, 72
21650, V, 1, 0, 0, 0, 0, 700, 72
21651, V, 1, 0, 0, 0, 0, 700, 73
21652, V, 1, 0, 0, 0, 0, 700, 73
21653, V, 1, 0, 0, 0, 0, 700, 73
21654, V, 1, 1, 0, 0, 0, 700, 73
21654, V, 1, 1, 0, 0, 0, 700, 73
21655, V, 1, 1, 1, 1, 0, 700, 73
21656, V, 1, 1, 1, 1, 0, 700, 73
21657, V, 1, 1, 1, 1, 0, 700, 74
21658, V, 1, 1, 1, 1, 0, 700, 74
21659, V, 1, 1, 1, 1, 0, 700, 74
21660, V, 1, 1, 1, 1, 0, 700, 75
21661, V, 1, 1, 1, 1, 0, 700, 75
21662, V, 1, 1, 1, 1, 0, 700, 76
21663, V, 1, 1, 1, 1, 0, 700, 77
21664, V, 1, 1, 1, 1, 0, 700, 77
21665, V, 1, 1, 1, 1, 0, 700, 78
21666, V, 1, 1, 1, 1, 0, 700, 79
21667, V, 1, 1, 1, 1, 0, 700, 79
21668, V, 1, 1, 1, 1, 0, 700, 80
21669, V, 1, 1, 1, 1, 0, 700, 80
21670, V, 1, 1, 1, 1, 0, 700, 81
21671, V, 1, 1, 1, 1, 0, 700, 82
21672, V, 1, 1, 1, 1, 0, 700, 82
21673, V, 1, 1, 1, 1, 0, 700, 83
21675, V, 1, 1, 1, 1, 0, 700, 83
21676, V, 1, 1, 1, 1, 0, 700, 84
21677, V, 1, 1, 1, 1, 0, 700, 84
21678, V, 1, 1, 1, 1, 0, 700, 85
21679, V, 1, 1, 1, 1, 0, 700, 85
21680, V, 1, 1, 1, 1, 0, 700, 86
21681, V, 1, 1, 1, 1, 0, 700, 86
21682, V, 1, 1, 1, 1, 0, 700, 86
21683, V, 1, 1, 1, 1, 0, 700, 87
21684, V, 1, 1, 1, 1, 0, 700, 87
21685, V, 1, 1, 1, 1, 0, 700, 88
21686, V, 1, 1, 1, 1, 0, 700, 88
21687, V, 1, 1, 1, 1, 0, 700, 88
21688, V, 1, 1, 1, 1, 0, 700, 89
21689, V, 1, 1, 1, 1, 0, 700, 89
21690, V, 1, 1, 1, 1, 0, 700, 89
21691, V, 1, 1, 1, 1, 0, 700, 89
21692, V, 1, 1, 1, 1, 0, 700, 90
21693, V, 1, 1, 1, 1, 0, 700, 90
21694, V, 1, 1, 1, 1, 0, 700, 90
21695, V, 1, 1, 1, 1, 0, 700, 91
21696, V, 1, 1, 1, 1, 0, 700, 91
21697, V, 1, 1, 1, 1, 0, 700, 91
21698, V, 1, 1, 1, 1, 0, 700, 91
21699, V, 1, 1, 1, 1, 0, 700, 92
21700, V, 1, 1, 1, 1, 0, 700, 92
21701, V, 1, 1, 1, 1, 0, 700, 92
21702, V, 1, 1, 1, 1, 0, 700, 92
21703, V, 1, 1, 1, 1, 0, 700, 93
21704, V, 1, 1, 1, 1, 0, 700, 93
21705, V, 1, 1, 1, 1, 0, 700, 93
21706, V, 1, 1, 1, 1, 0, 700, 93
21707, V, 1, 1, 1, 1, 0, 700, 93
21708, V, 1, 1, 1, 1, 0, 700, 94
21709, V, 1, 1, 1, 1, 0, 700, 94
21710, V, 1, 1, 1, 1, 0, 700, 94
21711, V, 1, 1, 1, 1, 0, 700, 94
21712, V, 1, 1, 1, 1, 0, 700, 94
21713, V, 1, 1, 1, 1, 0, 700, 94
21714, V, 1, 1, 1, 1, 0, 700, 95
21715, V, 1, 1, 1, 1, 0, 700, 95
21716, V, 1, 1, 1, 1, 0, 700, 95
21718, V, 1, 1, 1, 1, 0, 700, 95
21719, V, 1, 1, 1, 1, 0, 700, 95
21720, V, 1, 1, 1, 1, 0, 700, 95
21721, V, 1, 1, 1, 1, 0, 700, 96
21722, V, 1, 1, 1, 1, 0, 700, 96
21723, V, 1, 1, 1, 1, 0, 700, 96
21724, V, 1, 1, 1, 1, 0, 700, 96
21725, V, 1, 1, 1, 1, 0, 700, 96
21726, V, 1, 1, 1, 1, 0, 700, 96
21727, V, 1, 1, 1, 1, 0, 700, 96
21728, V, 1, 1, 1, 1, 0, 700, 96
21729, V, 1, 1, 1, 1, 0, 700, 96
21730, V, 1, 1, 1, 1, 0, 700, 96
21731, V, 1, 1, 1, 1, 0, 700, 97
21732, V, 1, 1, 1, 1, 0, 700, 97
21733, V, 1, 1, 1, 1, 0, 700, 97
21734, V, 1, 1, 1, 1, 0, 700, 97
21735, V, 1, 1, 1, 1, 0, 700, 97
21736, V, 1, 1, 1, 1, 0, 700, 97
21737, V, 1, 1, 1, 1, 0, 700, 97
21738, V, 1, 1, 1, 1, 0, 700, 97
21739, V, 1, 1, 1, 1, 0, 700, 97
21740, V, 1, 1, 1, 1, 0, 700, 97
21741, V, 1, 1, 1, 1, 0, 700, 97
21742, V, 1, 1, 1, 1, 0, 700, 97
21743, V, 1, 1, 1, 1, 0, 700, 97
21744, V, 1, 1, 1, 1, 0, 700, 98
21745, V, 1, 1, 1, 1, 0, 700, 98
21746, V, 1, 1, 1, 1, 0, 700, 98
21747, V, 1, 1, 1, 1, 0, 700, 98
21748, V, 1, 1, 1, 1, 0, 700, 98
21749, V, 1, 1, 1, 1, 0, 700, 98
21750, V, 1, 1, 1, 1, 0, 700, 98
21751, V, 1, 1, 1, 1, 0, 700, 98
21752, V, 1, 1, 1, 1, 0, 700, 98
21753, V, 1, 1, 1, 1, 0, 700, 98
21754, V, 1, 1, 1, 1, 0, 700, 98
21755, V, 1, 1, 1, 1, 0, 700, 98
21756, V, 1, 1, 1, 1, 0, 700, 98
21757, V, 1, 1, 1, 1, 0, 700, 98
21758, V, 1, 1, 1, 1, 0, 700, 98
21760, V, 1, 1, 1, 1, 0, 700, 98
21761, V, 1, 1, 1, 1, 0, 700, 98
21762, V, 1, 1, 1, 1, 0, 700, 98
21763, V, 1, 1, 1, 1, 0, 700, 98
21764, V, 1, 1, 1, 1, 0, 700, 98
21765, V, 1, 1, 1, 1, 0, 700, 98
21766, V, 1, 1, 1, 1, 0, 700, 98
21767, V, 1, 1, 1, 1, 0, 700, 99
21768, V, 1, 1, 1, 1, 0, 700, 99
21769, V, 1, 1, 1, 1, 0, 700, 99
21770, V, 1, 1, 1, 1, 0, 700, 99
21771, V, 1, 1, 1, 1, 0, 700, 99
21772, V, 1, 1, 1, 1, 0, 700, 99
21773, V, 1, 1, 1, 1, 0, 700, 99
21774, V, 1, 1, 1, 1, 0, 700, 99
21775, V, 1, 1, 1, 1, 0, 700, 99
21776, V, 1, 1, 1, 1, 0, 700, 99
21777, V, 1, 1, 1, 1, 0, 700, 99
21778, V, 1, 1, 1, 1, 0, 700, 99
21779, V, 1, 1, 1, 1, 0, 700, 99
21780, V, 1, 1, 1, 1, 0, 700, 99
21781, V, 1, 1, 1, 1, 0, 700, 99
21782, V, 1, 1, 1, 1, 0, 700, 99
21783, V, 1, 1, 1, 1, 0, 700, 99
21784, V, 1, 1, 1, 1, 0, 700, 99
21785, V, 1, 1, 1, 1, 0, 700, 99
21786, V, 1, 1, 1, 1, 0, 700, 99
21787, V, 1, 1, 1, 1, 0, 700, 99
21788, V, 1, 1, 1, 1, 0, 700, 99
21789, V, 1, 1, 1, 1, 0, 700, 99
21790, V, 1, 1, 1, 1, 0, 700, 99
21791, V, 1, 1, 1, 1, 0, 700, 99
21792, V, 1, 1, 1, 1, 0, 700, 99
21793, V, 1, 1, 1, 1, 0, 700, 99
21794, V, 1, 1, 1, 1, 0, 700, 99
21795, V, 1, 1, 1, 1, 0, 700, 99
21796, V, 1, 1, 1, 1, 0, 700, 99
21797, V, 1, 1, 1, 1, 0, 700, 99
21798, V, 1, 1, 1, 1, 0, 700, 99
21799, V, 1, 1, 1, 1, 0, 700, 99
21800, V, 1, 1, 1, 1, 0, 700, 99
21801, V, 1, 1, 1, 1, 0, 700, 99
21803, V, 1, 1, 1, 1, 0, 700, 99
21804, V, 1, 1, 1, 1, 0, 700, 99
21805, V, 1, 1, 1, 1, 0, 700, 99
21806, V, 1, 1, 1, 1, 0, 700, 99
21807, V, 1, 1, 1, 1, 0, 700, 99
21808, V, 1, 1, 1, 1, 0, 700, 99
21809, V, 1, 1, 1, 1, 0, 700, 99
21810, V, 1, 1, 1, 1, 0, 700, 99
21811, V, 1, 1, 1, 1, 0, 700, 99
21812, V, 1, 1, 1, 1, 0, 700, 99
21813, V, 1, 1, 1, 1, 0, 700, 99
21814, V, 1, 1, 1, 1, 0, 700, 99
21815, V, 1, 1, 1, 1, 0, 700, 99
21816, V, 1, 1, 1, 1, 0, 700, 99
21817, V, 1, 1, 1, 1, 0, 700, 99
21818, V, 1, 1, 1, 1, 0, 700, 99
21819, V, 1, 1, 1, 1, 0, 700, 99
21820, V, 1, 1, 1, 1, 0, 700, 99
21821, V, 1, 1, 1, 1, 0, 700, 99
21822, V, 1, 1, 1, 1, 0, 700, 99
21823, V, 1, 1, 1, 1, 0, 700, 99
21824, V, 1, 1, 1, 1, 0, 700, 99
21825, V, 1, 1, 1, 1, 0, 700, 99
21826, V, 1, 1, 1, 1, 0, 700, 99
21827, V, 1, 1, 1, 1, 0, 700, 99
21828, V, 1, 1, 1, 1, 0, 700, 99
21829, V, 1, 1, 1, 1, 0, 700, 99
21830, V, 1, 1, 1, 1, 0, 700, 99
21831, V, 1, 1, 1, 1, 0, 700, 99
21832, V, 1, 1, 1, 1, 0, 700, 99
21833, V, 1, 1, 1, 1, 0, 700, 99
21834, V, 1, 1, 1, 1, 0, 700, 99
21835, V, 1, 1, 1, 1, 0, 700, 99
21836, V, 1, 1, 1, 1, 0, 700, 99
21837, V, 1, 1, 1, 1, 0, 700, 99
21838, V, 1, 1, 1, 1, 0, 700, 99
21839, V, 1, 1, 1, 1, 0, 700, 99
21840, V, 1, 1, 1, 1, 0, 700, 99
21841, V, 1, 1, 1, 1, 0, 700, 99
21842, V, 1, 1, 1, 1, 0, 700, 99
21843, V, 1, 1, 1, 1, 0, 700, 99
21844, V, 1, 1, 1, 1, 0, 700, 100
21846, V, 1, 1, 1, 1, 0, 700, 99
21847, V, 1, 1, 1, 1, 0, 700, 100
21848, V, 1, 1, 1, 1, 0, 700, 100
21849, V, 1, 1, 1, 1, 0, 700, 99
21850, V, 1, 1, 1, 1, 0, 700, 100
21851, V, 1, 1, 1, 1, 0, 700, 99
21852, V, 1, 1, 1, 1, 0, 700, 100
21853, V, 1, 1, 1, 1, 0, 700, 99
21854, V, 1, 1, 1, 1, 0, 700, 100
21855, V, 1, 1, 1, 1, 0, 700, 100
21856, V, 1, 1, 1, 1, 0, 700, 100
21857, V, 1, 1, 1, 1, 0, 700, 100
21858, V, 1, 1, 1, 1, 0, 700, 100
21859, V, 1, 1, 1, 1, 0, 700, 100
21860, V, 1, 1, 1, 1, 0, 700, 100
21861, V, 1, 1, 1, 1, 0, 700, 100
21862, V, 1, 1, 1, 1, 0, 700, 100
21863, V, 1, 1, 1, 1, 0, 700, 100
21864, V, 1, 1, 1, 1, 0, 700, 100
21865, V, 1, 1, 1, 1, 0, 700, 100
21866, V, 1, 1, 1, 1, 0, 700, 100
21867, V, 1, 1, 1, 1, 0, 700, 100
21868, V, 1, 1, 1, 1, 0, 700, 100
21869, V, 1, 1, 1, 1, 0, 700, 100
21870, V, 1, 1, 1, 1, 0, 700, 100
21871, V, 1, 1, 1, 1, 0, 700, 100
21872, V, 1, 1, 1, 1, 0, 700, 100
21873, V, 1, 1, 1, 1, 0, 700, 100
21874, V, 1, 1, 1, 1, 0, 700, 100
21875, V, 1, 1, 1, 1, 0, 700, 100
21876, V, 1, 1, 1, 1, 0, 700, 100
21877, V, 1, 1, 1, 1, 0, 700, 100
21878, V, 1, 1, 1, 1, 0, 700, 100
21879, V, 1, 1, 1, 1, 0, 700, 100
21880, V, 1, 1, 1, 1, 0, 700, 100
21881, V, 1, 1, 1, 1, 0, 700, 100
21882, V, 1, 1, 1, 1, 0, 700, 100
21883, V, 1, 1, 1, 1, 0, 700, 100
21884, V, 1, 1, 1, 1, 0, 700, 100
21885, V, 1, 1, 1, 1, 0, 700, 100
21886, V, 1, 1, 1, 1, 0, 700, 100
21888, V, 1, 1, 1, 1, 0, 700, 100
21889, V, 1, 1, 1, 1, 0, 700, 100
21890, V, 1, 1, 1, 1, 0, 700, 100
21891, V, 1, 1, 1, 1, 0, 700, 100
21892, V, 1, 1, 1, 1, 0, 700, 100
21893, V, 1, 1, 1, 1, 0, 700, 100
21894, V, 1, 1, 1, 1, 0, 700, 100
21895, V, 1, 1, 1, 1, 0, 700, 100
21896, V, 1, 1, 1, 1, 0, 700, 100
21897, V, 1, 1, 1, 1, 0, 700, 100
21898, V, 1, 1, 1, 1, 0, 700, 100
21899, V, 1, 1, 1, 1, 0, 700, 100
21900, V, 1, 1, 1, 1, 0, 700, 100
21901, V, 1, 1, 1, 1, 0, 700, 100
21902, V, 1, 1, 1, 1, 0, 700, 100
21903, V, 1, 1, 1, 1, 0, 700, 100
21904, V, 1, 1, 1, 1, 0, 700, 100
21905, V, 1, 1, 1, 1, 0, 700, 100
21906, V, 1, 1, 1, 1, 0, 700, 100
21907, V, 1, 1, 1, 1, 0, 700, 100
21908, V, 1, 1, 1, 1, 0, 700, 100
21909, V, 1, 1, 1, 1, 0, 700, 99
21910, V, 1, 1, 1, 1, 0, 700, 100
21911, V, 1, 1, 1, 1, 0, 700, 99
21912, V, 1, 1, 1, 1, 0, 700, 100
21913, V, 1, 1, 1, 1, 0, 700, 99
21914, V, 1, 1, 1, 1, 0, 700, 99
21915, V, 1, 1, 1, 1, 0, 700, 99
21916, V, 1, 1, 1, 1, 0, 700, 99
21917, V, 1, 1, 1, 1, 0, 700, 99
21918, V, 1, 1, 1, 1, 0, 700, 99
21919, V, 1, 1, 1, 1, 0, 700, 99
21920, V, 1, 1, 1, 1, 0, 700, 100
21921, V, 1, 1, 1, 1, 0, 700, 99
21922, V, 1, 1, 1, 1, 0, 700, 99
21923, V, 1, 1, 1, 1, 0, 700, 100
21924, V, 1, 1, 1, 1, 0, 700, 100
21925, V, 1, 1, 1, 1, 0, 700, 100
21926, V, 1, 1, 1, 1, 0, 700, 100
21927, V, 1, 1, 1, 1, 0, 700, 100
21928, V, 1, 1, 1, 1, 0, 700, 100
21929, V, 1, 1, 1, 1, 0, 700, 99
21931, V, 1, 1, 1, 1, 0, 700, 100
21932, V, 1, 1, 1, 1, 0, 700, 100
21933, V, 1, 1, 1, 1, 0, 700, 100
21934, V, 1, 1, 1, 1, 0, 700, 100
21935, V, 1, 1, 1, 1, 0, 700, 100
21936, V, 1, 1, 1, 1, 0, 700, 100
21937, V, 1, 1, 1, 1, 0, 700, 100
21938, V, 1, 1, 1, 1, 0, 700, 100
21939, V, 1, 1, 1, 1, 0, 700, 100
21940, V, 1, 1, 1, 1, 0, 700, 100
21941, V, 1, 1, 1, 1, 0, 700, 100
21942, V, 1, 1, 1, 1, 0, 700, 100
21943, V, 1, 1, 1, 1, 0, 700, 100
21944, V, 1, 1, 1, 1, 0, 700, 100
21945, V, 1, 1, 1, 1, 0, 700, 100
21946, V, 1, 1, 1, 1, 0, 700, 100
21947, V, 1, 1, 1, 1, 0, 700, 100
21948, V, 1, 1, 1, 1, 0, 700, 100
21949, V, 1, 1, 1, 1, 0, 700, 100
21950, V, 1, 1, 1, 1, 0, 700, 100
21951, V, 1, 1, 1, 1, 0, 700, 100
21952, V, 1, 1, 1, 1, 0, 700, 100
21953, V, 1, 1, 1, 1, 0, 700, 100
21954, V, 1, 1, 1, 1, 0, 700, 100
21955, V, 1, 1, 1, 1, 0, 700, 100
21956, V, 1, 1, 1, 1, 0, 700, 100
21957, V, 1, 1, 1, 1, 0, 700, 100
21958, V, 1, 1, 1, 1, 0, 700, 100
21959, V, 1, 1, 1, 1, 0, 700, 100
21960, V, 1, 1, 1, 1, 0, 700, 100
21961, V, 1, 1, 1, 1, 0, 700, 100
21962, V, 1, 1, 1, 1, 0, 700, 100
21963, V, 1, 1, 1, 1, 0, 700, 100
21964, V, 1, 1, 1, 1, 0, 700, 100
21965, V, 1, 1, 1, 1, 0, 700, 100
21966, V, 1, 1, 1, 1, 0, 700, 100
21967, V, 1, 1, 1, 1, 0, 700, 100
21968, V, 1, 1, 1, 1, 0, 700, 100
21969, V, 1, 1, 1, 1, 0, 700, 99
21970, V, 1, 1, 1, 1, 0, 700, 100
21971, V, 1, 1, 1, 1, 0, 700, 100
21972, V, 1, 1, 1, 1, 0, 700, 100
21974, V, 1, 1, 1, 1, 0, 700, 100
21975, V, 1, 1, 1, 1, 0, 700, 99
21976, V, 1, 1, 1, 1, 0, 700, 100
21977, V, 1, 1, 1, 1, 0, 700, 99
21978, V, 1, 1, 1, 1, 0, 700, 99
21979, V, 1, 1, 1, 1, 0, 700, 100
21980, V, 1, 1, 1, 1, 0, 700, 99
21981, V, 1, 1, 1, 1, 0, 700, 100
21982, V, 1, 1, 1, 1, 0, 700, 99
21983, V, 1, 1, 1, 1, 0, 700, 99
21984, V, 1, 1, 1, 1, 0, 700, 100
21985, V, 1, 1, 1, 1, 0, 700, 100
21986, V, 1, 1, 1, 1, 0, 700, 99
21987, V, 1, 1, 1, 1, 0, 700, 99
21988, V, 1, 1, 1, 1, 0, 700, 99
21989, V, 1, 1, 1, 1, 0, 700, 99
21990, V, 1, 1, 1, 1, 0, 700, 99
21991, V, 1, 1, 1, 1, 0, 700, 99
21992, V, 1, 1, 1, 1, 0, 700, 99
21993, V, 1, 1, 1, 1, 0, 700, 100
21994, V, 1, 1, 1, 1, 0, 700, 100
21995, V, 1, 1, 1, 1, 0, 700, 99
21996, V, 1, 1, 1, 1, 0, 700, 99
21997, V, 1, 1, 1, 1, 0, 700, 99
21998, V, 1, 1, 1, 1, 0, 700, 99
21999, V, 1, 1, 1, 1, 0, 700, 99
22000, V, 1, 1, 1, 1, 0, 700, 100
22001, V, 1, 1, 1, 1, 0, 700, 100
22002, V, 1, 1, 1, 1, 0, 700, 99
22003, V, 1, 1, 1, 1, 0, 700, 100
22004, V, 1, 1, 1, 1, 0, 700, 100
22005, V, 1, 1, 1, 1, 0, 700, 99
22006, V, 1, 1, 1, 1, 0, 700, 100
22007, V, 1, 1, 1, 1, 0, 700, 100
22008, V, 1, 1, 1, 1, 0, 700, 100
22009, V, 1, 1, 1, 1, 0, 700, 100
22010, V, 1, 1, 1, 1, 0, 700, 99
22011, V, 1, 1, 1, 1, 0, 700, 100
22012, V, 1, 1, 1, 1, 0, 700, 100
22013, V, 1, 1, 1, 1, 0, 700, 100
22014, V, 1, 1, 1, 1, 0, 700, 100
22016, V, 1, 1, 1, 1, 0, 700, 100
22017, V, 1, 1, 1, 1, 0, 700, 100
22018, V, 1, 1, 1, 1, 0, 700, 100
22019, V, 1, 1, 1, 1, 0, 700, 100
22020, V, 1, 1, 1, 1, 0, 700, 100
22021, V, 1, 1, 1, 1, 0, 700, 100
22022, V, 1, 1, 1, 1, 0, 700, 100
22023, V, 1, 1, 1, 1, 0, 700, 100
22024, V, 1, 1, 1, 1, 0, 700, 100
22025, V, 1, 1, 1, 1, 0, 700, 100
22026, V, 1, 1, 1, 1, 0, 700, 100
22027, V, 1, 1, 1, 1, 0, 700, 100
22028, V, 1, 1, 1, 1, 0, 700, 100
22029, V, 1, 1, 1, 1, 0, 700, 100
22030, V, 1, 1, 1, 1, 0, 700, 100
22031, V, 1, 1, 1, 1, 0, 700, 100
22032, V, 1, 1, 1, 1, 0, 700, 99
22033, V, 1, 1, 1, 1, 0, 700, 100
22034, V, 1, 1, 1, 1, 0, 700, 100
22035, V, 1, 1, 1, 1, 0, 700, 100
22036, V, 1, 1, 1, 1, 0, 700, 100
22037, V, 1, 1, 1, 1, 0, 700, 100
22038, V, 1, 1, 1, 1, 0, 700, 100
22039, V, 1, 1, 1, 1, 0, 700, 100
22040, V, 1, 1, 1, 1, 0, 700, 100
22041, V, 1, 1, 1, 1, 0, 700, 100
22042, V, 1, 1, 1, 1, 0, 700, 100
22043, V, 1, 1, 1, 1, 0, 700, 99
22044, V, 1, 1, 1, 1, 0, 700, 99
22045, V, 1, 1, 1, 1, 0, 700, 99
22046, V, 1, 1, 1, 1, 0, 700, 100
22047, V, 1, 1, 1, 1, 0, 700, 99
22048, V, 1, 1, 1, 1, 0, 700, 99
22049, V, 1, 1, 1, 1, 0, 700, 99
22050, V, 1, 1, 1, 1, 0, 700, 99
22051, V, 1, 1, 1, 1, 0, 700, 99
22052, V, 1, 1, 1, 1, 0, 700, 99
22053, V, 1, 1, 1, 1, 0, 700, 99
22054, V, 1, 1, 1, 1, 0, 700, 99
22055, V, 1, 1, 1, 1, 0, 700, 99
22056, V, 1, 1, 1, 1, 0, 700, 99
22057, V, 1, 1, 1, 1, 0, 700, 99
22059, V, 1, 1, 1, 1, 0, 700, 99
22060, V, 1, 1, 1, 1, 0, 700, 99
22061, V, 1, 1, 1, 1, 0, 700, 99
22062, V, 1, 1, 1, 1, 0, 700, 99
22063, V, 1, 1, 1, 1, 0, 700, 99
22064, V, 1, 1, 1, 1, 0, 700, 99
22065, V, 1, 1, 1, 1, 0, 700, 99
22066, V, 1, 1, 1, 1, 0, 700, 99
22067, V, 1, 1, 1, 1, 0, 700, 99
22068, V, 1, 1, 1, 1, 0, 700, 99
22069, V, 1, 1, 1, 1, 0, 700, 99
22070, V, 1, 1, 1, 1, 0, 700, 99
22071, V, 1, 1, 1, 1, 0, 700, 99
22072, V, 1, 1, 1, 1, 0, 700, 99
22073, V, 1, 1, 1, 1, 0, 700, 99
22074, V, 1, 1, 1, 1, 0, 700, 99
22075, V, 1, 1, 1, 1, 0, 700, 99
22076, V, 1, 1, 1, 1, 0, 700, 99
22077, V, 1, 1, 1, 1, 0, 700, 99
22078, V, 1, 1, 1, 1, 0, 700, 99
22079, V, 1, 1, 1, 1, 0, 700, 99
22080, V, 1, 1, 1, 1, 0, 700, 99
22081, V, 1, 1, 1, 1, 0, 700, 99
22082, V, 1, 1, 1, 1, 0, 700, 99
22083, V, 1, 1, 1, 1, 0, 700, 99
22084, V, 1, 1, 1, 1, 0, 700, 100
22085, V, 1, 1, 1, 1, 0, 700, 100
22086, V, 1, 1, 1, 1, 0, 700, 100
22087, V, 1, 1, 1, 1, 0, 700, 99
22088, V, 1, 1, 1, 1, 0, 700, 100
22089, V, 1, 1, 1, 1, 0, 700, 99
22090, V, 1, 1, 1, 1, 0, 700, 100
22091, V, 1, 1, 1, 1, 0, 700, 100
22092, V, 1, 1, 1, 1, 0, 700, 99
22093, V, 1, 1, 1, 1, 0, 700, 100
22094, V, 1, 1, 1, 1, 0, 700, 100
22095, V, 1, 1, 1, 1, 0, 700, 100
22096, V, 1, 1, 1, 1, 0, 700, 100
22097, V, 1, 1, 1, 1, 0, 700, 100
22098, V, 1, 1, 1, 1, 0, 700, 100
22099, V, 1, 1, 1, 1, 0, 700, 100
22100, V, 1, 1, 1, 1, 0, 700, 100
22102, V, 1, 1, 1, 1, 0, 700, 100
22103, V, 1, 1, 1, 1, 0, 700, 100
22104, V, 1, 1, 1, 1, 0, 700, 100
22105, V, 1, 1, 1, 1, 0, 700, 100
22106, V, 1, 1, 1, 1, 0, 700, 100
22107, V, 1, 1, 1, 1, 0, 700, 100
22108, V, 1, 1, 1, 1, 0, 700, 99
22109, V, 1, 1, 1, 1, 0, 700, 99
22110, V, 1, 1, 1, 1, 0, 700, 100
22111, V, 1, 1, 1, 1, 0, 700, 99
22112, V, 1, 1, 1, 1, 0, 700, 99
22113, V, 1, 1, 1, 1, 0, 700, 100
22114, V, 1, 1, 1, 1, 0, 700, 99
22115, V, 1, 1, 1, 1, 0, 700, 100
22116, V, 1, 1, 1, 1, 0, 700, 99
22117, V, 1, 1, 1, 1, 0, 700, 99
22118, V, 1, 1, 1, 1, 0, 700, 99
22119, V, 1, 1, 1, 1, 0, 700, 99
22120, V, 1, 1, 1, 1, 0, 700, 99
22121, V, 1, 1, 1, 1, 0, 700, 99
22122, V, 1, 1, 1, 1, 0, 700, 99
22123, V, 1, 1, 1, 1, 0, 700, 99
22124, V, 1, 1, 1, 1, 0, 700, 99
22125, V, 1, 1, 1, 1, 0, 700, 99
22126, V, 1, 1, 1, 1, 0, 700, 99
22127, V, 1, 1, 1, 1, 0, 700, 99
22128, V, 1, 1, 1, 1, 0, 700, 99
22129, V, 1, 1, 1, 1, 0, 700, 99
22130, V, 1, 1, 1, 1, 0, 700, 99
22131, V, 1, 1, 1, 1, 0, 700, 99
22132, V, 1, 1, 1, 1, 0, 700, 99
22133, V, 1, 1, 1, 1, 0, 700, 99
22134, V, 1, 1, 1, 1, 0, 700, 99
22135, V, 1, 1, 1, 1, 0, 700, 99
22136, V, 1, 1, 1, 1, 0, 700, 99
22137, V, 1, 1, 1, 1, 0, 700, 99
22138, V, 1, 1, 1, 1, 0, 700, 99
22139, V, 1, 1, 1, 1, 0, 700, 99
22140, V, 1, 1, 1, 1, 0, 700, 99
22141, V, 1, 1, 1, 1, 0, 700, 99
22142, V, 1, 1, 1, 1, 0, 700, 99
22144, V, 1, 1, 1, 1, 0, 700, 99
22145, V, 1, 1, 1, 1, 0, 700, 99
22146, V, 1, 1, 1, 1, 0, 700, 99
22147, V, 1, 1, 1, 1, 0, 700, 99
22148, V, 1, 1, 1, 1, 0, 700, 100
22149, V, 1, 1, 1, 1, 0, 700, 99
22150, V, 1, 1, 1, 1, 0, 700, 99
22151, V, 1, 1, 1, 1, 0, 700, 99
22152, V, 1, 1, 1, 1, 0, 700, 99
22153, V, 1, 1, 1, 1, 0, 700, 99
22154, V, 1, 1, 1, 1, 0, 700, 99
22155, V, 1, 1, 1, 1, 0, 700, 99
22156, V, 1, 1, 1, 1, 0, 700, 99
22157, V, 1, 1, 1, 1, 0, 700, 99
22158, V, 1, 1, 1, 1, 0, 700, 99
22159, V, 1, 1, 1, 1, 0, 700, 99
22160, V, 1, 0, 0, 1, 0, 700, 99
22160, V, 1, 0, 0, 0, 0, 700, 99
22161, V, 1, 1, 0, 0, 0, 700, 99
22161, V, 1, 1, 0, 0, 0, 700, 99
22162, V, 1, 1, 1, 1, 0, 700, 99
22163, V, 1, 1, 1, 1, 0, 700, 99
22164, V, 1, 1, 1, 1, 0, 700, 99
22165, V, 1, 1, 1, 1, 0, 700, 99
22166, V, 1, 1, 1, 1, 0, 700, 99
22167, V, 1, 1, 1, 1, 0, 700, 99
22168, V, 1, 1, 1, 1, 0, 700, 99
22169, V, 1, 1, 1, 1, 0, 700, 99
22170, V, 1, 1, 1, 1, 0, 700, 99
22171, V, 1, 1, 1, 1, 0, 700, 99
22172, V, 1, 1, 1, 1, 0, 700, 99
22173, V, 1, 1, 1, 1, 0, 700, 99
22174, V, 1, 1, 1, 1, 0, 700, 99
22175, V, 1, 1, 1, 1, 0, 700, 99
22176, V, 1, 1, 1, 1, 0, 700, 99
22177, V, 1, 1, 1, 1, 0, 700, 99
22178, V, 1, 1, 1, 1, 0, 700, 99
22179, V, 1, 1, 1, 1, 0, 700, 99
22180, V, 1, 1, 1, 1, 0, 700, 99
22181, V, 1, 1, 1, 1, 0, 700, 99
22182, V, 1, 1, 1, 1, 0, 700, 99
22183, V, 1, 1, 1, 1, 0, 700, 99
22184, V, 1, 1, 1, 1, 0, 700, 99
22185, V, 1, 1, 1, 1, 0, 700, 99
22187, V, 1, 1, 1, 1, 0, 700, 99
22188, V, 1, 1, 1, 1, 0, 700, 99
22189, V, 1, 1, 1, 1, 0, 700, 99
22190, V, 1, 1, 1, 1, 0, 700, 99
22191, V, 1, 1, 1, 1, 0, 700, 99
22192, V, 1, 1, 1, 1, 0, 700, 99
22193, V, 1, 1, 1, 1, 0, 700, 99
22194, V, 1, 1, 1, 1, 0, 700, 99
22195, V, 1, 1, 1, 1, 0, 700, 99
22196, V, 1, 1, 1, 1, 0, 700, 99
22197, V, 1, 1, 1, 1, 0, 700, 99
22198, V, 1, 1, 1, 1, 0, 700, 99
22199, V, 1, 1, 1, 1, 0, 700, 99
22200, V, 1, 1, 1, 1, 0, 700, 99
22201, V, 1, 1, 1, 1, 0, 700, 99
22202, V, 1, 1, 1, 1, 0, 700, 99
22203, V, 1, 1, 1, 1, 0, 700, 99
22204, V, 1, 1, 1, 1, 0, 700, 99
22205, V, 1, 1, 1, 1, 0, 700, 99
22206, V, 1, 1, 1, 1, 0, 700, 99
22207, V, 1, 1, 1, 1, 0, 700, 99
22208, V, 1, 1, 1, 1, 0, 700, 99
22209, V, 1, 1, 1, 1, 0, 700, 99
22210, V, 1, 1, 1, 1, 0, 700, 99
22211, V, 1, 1, 1, 1, 0, 700, 99
22212, V, 1, 1, 1, 1, 0, 700, 99
22213, V, 1, 1, 1, 1, 0, 700, 99
22214, V, 1, 1, 1, 1, 0, 700, 99
22215, V, 1, 1, 1, 1, 0, 700, 99
22216, V, 1, 1, 1, 1, 0, 700, 99
22217, V, 1, 1, 1, 1, 0, 700, 99
22218, V, 1, 1, 1, 1, 0, 700, 99
22219, V, 1, 1, 1, 1, 0, 700, 99
22220, V, 1, 1, 1, 1, 0, 700, 99
22221, V, 1, 1, 1, 1, 0, 700, 99
22222, V, 1, 1, 1, 1, 0, 700, 99
22223, V, 1, 1, 1, 1, 0, 700, 99
22224, V, 1, 1, 1, 1, 0, 700, 99
22225, V, 1, 1, 1, 1, 0, 700, 99
22226, V, 1, 1, 1, 1, 0, 700, 99
22227, V, 1, 1, 1, 1, 0, 700, 99
22228, V, 1, 1, 1, 1, 0, 700, 99
22230, V, 1, 1, 1, 1, 0, 700, 99
22231, V, 1, 1, 1, 1, 0, 700, 99
22232, V, 1, 1, 1, 1, 0, 700, 99
22233, V, 1, 1, 1, 1, 0, 700, 99
22234, V, 1, 1, 1, 1, 0, 700, 99
22235, V, 1, 1, 1, 1, 0, 700, 99
22236, V, 1, 1, 1, 1, 0, 700, 99
22237, V, 1, 1, 1, 1, 0, 700, 99
22238, V, 1, 1, 1, 1, 0, 700, 99
22239, V, 1, 1, 1, 1, 0, 700, 99
22240, V, 1, 1, 1, 1, 0, 700, 99
22241, V, 1, 1, 1, 1, 0, 700, 99
22242, V, 1, 1, 1, 1, 0, 700, 99
22243, V, 1, 1, 1, 1, 0, 700, 99
22244, V, 1, 1, 1, 1, 0, 700, 99
22245, V, 1, 1, 1, 1, 0, 700, 99
22246, V, 1, 1, 1, 1, 0, 700, 99
22247, V, 1, 1, 1, 1, 0, 700, 99
22248, V, 1, 1, 1, 1, 0, 700, 99
22249, V, 1, 1, 1, 1, 0, 700, 99
22250, V, 1, 1, 1, 1, 0, 700, 99
22251, V, 1, 1, 1, 1, 0, 700, 99
22252, V, 1, 1, 1, 1, 0, 700, 99
22253, V, 1, 1, 1, 1, 0, 700, 99
22254, V, 1, 1, 1, 1, 0, 700, 99
22255, V, 1, 1, 1, 1, 0, 700, 99
22256, V, 1, 1, 1, 1, 0, 700, 99
22257, V, 1, 1, 1, 1, 0, 700, 100
22258, V, 1, 1, 1, 1, 0, 700, 99
22259, V, 1, 1, 1, 1, 0, 700, 99
22260, V, 1, 1, 1, 1, 0, 700, 99
22261, V, 1, 1, 1, 1, 0, 700, 99
22262, V, 1, 1, 1, 1, 0, 700, 99
22263, V, 1, 1, 1, 1, 0, 700, 99
22264, V, 1, 1, 1, 1, 0, 700, 99
22265, V, 1, 1, 1, 1, 0, 700, 99
22266, V, 1, 1, 1, 1, 0, 700, 99
22267, V, 1, 1, 1, 1, 0, 700, 99
22268, V, 1, 1, 1, 1, 0, 700, 99
22269, V, 1, 1, 1, 1, 0, 700, 99
22270, V, 1, 1, 1, 1, 0, 700, 99
22272, V, 1, 1, 1, 1, 0, 700, 99
22273, V, 1, 1, 1, 1, 0, 700, 99
22274, V, 1, 1, 1, 1, 0, 700, 99
22275, V, 1, 1, 1, 1, 0, 700, 99
22276, V, 1, 1, 1, 1, 0, 700, 99
22277, V, 1, 1, 1, 1, 0, 700, 99
22278, V, 1, 1, 1, 1, 0, 700, 99
22279, V, 1, 1, 1, 1, 0, 700, 99
22280, V, 1, 1, 1, 1, 0, 700, 99
22281, V, 1, 1, 1, 1, 0, 700, 99
22282, V, 1, 1, 1, 1, 0, 700, 99
22283, V, 1, 1, 1, 1, 0, 700, 99
22284, V, 1, 1, 1, 1, 0, 700, 99
22285, V, 1, 1, 1, 1, 0, 700, 99
22286, V, 1, 1, 1, 1, 0, 700, 99
22287, V, 1, 1, 1, 1, 0, 700, 99
22288, V, 1, 1, 1, 1, 0, 700, 99
22289, V, 1, 1, 1, 1, 0, 700, 99
22290, V, 1, 1, 1, 1, 0, 700, 99
22291, V, 1, 1, 1, 1, 0, 700, 99
22292, V, 1, 1, 1, 1, 0, 700, 99
22293, V, 1, 1, 1, 1, 0, 700, 99
22294, V, 1, 1, 1, 1, 0, 700, 99
22295, V, 1, 1, 1, 1, 0, 700, 99
22296, V, 1, 1, 1, 1, 0, 700, 99
22297, V, 1, 1, 1, 1, 0, 700, 99
22298, V, 1, 1, 1, 1, 0, 700, 99
22299, V, 1, 1, 1, 1, 0, 700, 99
22300, V, 1, 1, 1, 1, 0, 700, 99
22301, V, 1, 1, 1, 1, 0, 700, 99
22302, V, 1, 1, 1, 1, 0, 700, 99
22303, V, 1, 1, 1, 1, 0, 700, 99
22304, V, 1, 1, 1, 1, 0, 700, 99
22305, V, 1, 1, 1, 1, 0, 700, 99
22306, V, 1, 1, 1, 1, 0, 700, 99
22307, V, 1, 1, 1, 1, 0, 700, 99
22308, V, 1, 1, 1, 1, 0, 700, 99
22309, V, 1, 1, 1, 1, 0, 700, 99
22310, V, 1, 1, 1, 1, 0, 700, 99
22311, V, 1, 1, 1, 1, 0, 700, 99
22312, V, 1, 1, 1, 1, 0, 700, 99
22313, V, 1, 1, 1, 1, 0, 700, 99
22315, V, 1, 1, 1, 1, 0, 700, 99
22316, V, 1, 1, 1, 1, 0, 700, 99
22317, V, 1, 1, 1, 1, 0, 700, 99
22318, V, 1, 1, 1, 1, 0, 700, 99
22319, V, 1, 1, 1, 1, 0, 700, 99
22320, V, 1, 1, 1, 1, 0, 700, 99
22321, V, 1, 1, 1, 1, 0, 700, 99
22322, V, 1, 1, 1, 1, 0, 700, 99
22323, V, 1, 1, 1, 1, 0, 700, 99
22324, V, 1, 1, 1, 1, 0, 700, 99
22325, V, 1, 1, 1, 1, 0, 700, 99
22326, V, 1, 1, 1, 1, 0, 700, 99
22327, V, 1, 1, 1, 1, 0, 700, 99
22328, V, 1, 1, 1, 1, 0, 700, 99
22329, V, 1, 1, 1, 1, 0, 700, 99
22330, V, 1, 1, 1, 1, 0, 700, 99
22331, V, 1, 1, 1, 1, 0, 700, 99
22332, V, 1, 1, 1, 1, 0, 700, 99
22333, V, 1, 1, 1, 1, 0, 700, 100
22334, V, 1, 1, 1, 1, 0, 700, 99
22335, V, 1, 1, 1, 1, 0, 700, 99
22336, V, 1, 1, 1, 1, 0, 700, 99
22337, V, 1, 1, 1, 1, 0, 700, 99
22338, V, 1, 1, 1, 1, 0, 700, 99
22339, V, 1, 1, 1, 1, 0, 700, 99
22340, V, 1, 1, 1, 1, 0, 700, 99
22341, V, 1, 1, 1, 1, 0, 700, 99
22342, V, 1, 1, 1, 1, 0, 700, 99
22343, V, 1, 1, 1, 1, 0, 700, 99
22344, V, 1, 1, 1, 1, 0, 700, 99
22345, V, 1, 1, 1, 1, 0, 700, 99
22346, V, 1, 1, 1, 1, 0, 700, 99
22347, V, 1, 1, 1, 1, 0, 700, 99
22348, V, 1, 1, 1, 1, 0, 700, 99
22349, V, 1, 1, 1, 1, 0, 700, 99
22350, V, 1, 1, 1, 1, 0, 700, 99
22351, V, 1, 1, 1, 1, 0, 700, 99
22352, V, 1, 1, 1, 1, 0, 700, 99
22353, V, 1, 1, 1, 1, 0, 700, 99
22354, V, 1, 1, 1, 1, 0, 700, 99
22355, V, 1, 1, 1, 1, 0, 700, 99
22356, V, 1, 1, 1, 1, 0, 700, 99
22358, V, 1, 1, 1, 1, 0, 700, 99
22359, V, 1, 1, 1, 1, 0, 700, 99
22360, V, 1, 1, 1, 1, 0, 700, 99
22361, V, 1, 1, 1, 1, 0, 700, 99
22362, V, 1, 1, 1, 1, 0, 700, 99
22363, V, 1, 1, 1, 1, 0, 700, 99
22364, V, 1, 1, 1, 1, 0, 700, 99
22365, V, 1, 1, 1, 1, 0, 700, 99
22366, V, 1, 1, 1, 1, 0, 700, 99
22367, V, 1, 1, 1, 1, 0, 700, 99
22368, V, 1, 1, 1, 1, 0, 700, 99
22369, V, 1, 1, 1, 1, 0, 700, 99
22370, V, 1, 1, 1, 1, 0, 700, 99
22371, V, 1, 1, 1, 1, 0, 700, 99
22372, V, 1, 1, 1, 1, 0, 700, 99
22373, V, 1, 1, 1, 1, 0, 700, 99
22374, V, 1, 1, 1, 1, 0, 700, 99
22375, V, 1, 1, 1, 1, 0, 700, 99
22376, V, 1, 1, 1, 1, 0, 700, 99
22377, V, 1, 1, 1, 1, 0, 700, 99
22378, V, 1, 1, 1, 1, 0, 700, 99
22379, V, 1, 1, 1, 1, 0, 700, 99
22380, V, 1, 1, 1, 1, 0, 700, 99
22381, V, 1, 1, 1, 1, 0, 700, 99
22382, V, 1, 1, 1, 1, 0, 700, 99
22383, V, 1, 1, 1, 1, 0, 700, 99
22384, V, 1, 1, 1, 1, 0, 700, 99
22385, V, 1, 1, 1, 1, 0, 700, 99
22386, V, 1, 1, 1, 1, 0, 700, 99
22387, V, 1, 1, 1, 1, 0, 700, 99
22388, V, 1, 0, 0, 1, 0, 700, 99
22388, V, 1, 0, 0, 0, 0, 700, 99
22389, V, 1, 1, 0, 0, 0, 700, 99
22389, V, 1, 1, 0, 0, 0, 700, 99
22390, V, 1, 1, 1, 1, 0, 700, 99
22391, V, 1, 1, 1, 1, 0, 700, 99
22392, V, 1, 1, 1, 1, 0, 700, 99
22393, V, 1, 1, 1, 1, 0, 700, 99
22394, V, 1, 1, 1, 1, 0, 700, 99
22395, V, 1, 1, 1, 1, 0, 700, 99
22396, V, 1, 1, 1, 1, 0, 700, 99
22397, V, 1, 1, 1, 1, 0, 700, 99
22398, V, 1, 1, 1, 1, 0, 700, 99
22400, V, 1, 1, 1, 1, 0, 700, 99
22401, V, 1, 1, 1, 1, 0, 700, 99
22402, V, 1, 1, 1, 1, 0, 700, 99
22403, V, 1, 1, 1, 1, 0, 700, 99
22404, V, 1, 1, 1, 1, 0, 700, 99
22405, V, 1, 1, 1, 1, 0, 700, 99
22406, V, 1, 1, 1, 1, 0, 700, 99
22407, V, 1, 1, 1, 1, 0, 700, 99
22408, V, 1, 1, 1, 1, 0, 700, 99
22409, V, 1, 1, 1, 1, 0, 700, 99
22410, V, 1, 1, 1, 1, 0, 700, 99
22411, V, 1, 1, 1, 1, 0, 700, 99
22412, V, 1, 1, 1, 1, 0, 700, 99
22413, V, 1, 1, 1, 1, 0, 700, 99
22414, V, 1, 1, 1, 1, 0, 700, 99
22415, V, 1, 1, 1, 1, 0, 700, 99
22416, V, 1, 1, 1, 1, 0, 700, 99
22417, V, 1, 1, 1, 1, 0, 700, 99
22418, V, 1, 1, 1, 1, 0, 700, 99
22419, V, 1, 1, 1, 1, 0, 700, 99
22420, V, 1, 1, 1, 1, 0, 700, 99
22421, V, 1, 1, 1, 1, 0, 700, 99
22422, V, 1, 1, 1, 1, 0, 700, 99
22423, V, 1, 1, 1, 1, 0, 700, 99
22424, V, 1, 1, 1, 1, 0, 700, 99
22425, V, 1, 1, 1, 1, 0, 700, 99
22426, V, 1, 1, 1, 1, 0, 700, 99
22427, V, 1, 1, 1, 1, 0, 700, 99
22428, V, 1, 1, 1, 1, 0, 700, 99
22429, V, 1, 1, 1, 1, 0, 700, 99
22430, V, 1, 1, 1, 1, 0, 700, 99
22431, V, 1, 1, 1, 1, 0, 700, 99
22432, V, 1, 1, 1, 1, 0, 700, 99
22433, V, 1, 1, 1, 1, 0, 700, 99
22434, V, 1, 1, 1, 1, 0, 700, 99
22435, V, 1, 1, 1, 1, 0, 700, 99
22436, V, 1, 1, 1, 1, 0, 700, 99
22437, V, 1, 1, 1, 1, 0, 700, 99
22438, V, 1, 1, 1, 1, 0, 700, 99
22439, V, 1, 1, 1, 1, 0, 700, 99
22440, V, 1, 1, 1, 1, 0, 700, 99
22441, V, 1, 1, 1, 1, 0, 700, 99
22443, V, 1, 1, 1, 1, 0, 700, 99
22444, V, 1, 1, 1, 1, 0, 700, 99
22445, V, 1, 1, 1, 1, 0, 700, 99
22446, V, 1, 1, 1, 1, 0, 700, 99
22447, V, 1, 1, 1, 1, 0, 700, 99
22448, V, 1, 1, 1, 1, 0, 700, 99
22449, V, 1, 1, 1, 1, 0, 700, 99
22450, V, 1, 1, 1, 1, 0, 700, 99
22451, V, 1, 1, 1, 1, 0, 700, 99
22452, V, 1, 1, 1, 1, 0, 700, 99
22453, V, 1, 1, 1, 1, 0, 700, 99
22454, V, 1, 1, 1, 1, 0, 700, 99
22455, V, 1, 1, 1, 1, 0, 700, 99
22456, V, 1, 1, 1, 1, 0, 700, 99
22457, V, 1, 1, 1, 1, 0, 700, 99
22458, V, 1, 1, 1, 1, 0, 700, 99
22459, V, 1, 1, 1, 1, 0, 700, 99
22460, V, 1, 1, 1, 1, 0, 700, 99
22461, V, 1, 1, 1, 1, 0, 700, 99
22462, V, 1, 1, 1, 1, 0, 700, 99
22463, V, 1, 1, 1, 1, 0, 700, 99
22464, V, 1, 1, 1, 1, 0, 700, 99
22465, V, 1, 1, 1, 1, 0, 700, 99
22466, V, 1, 1, 1, 1, 0, 700, 99
22467, V, 1, 1, 1, 1, 0, 700, 99
22468, V, 1, 1, 1, 1, 0, 700, 99
22469, V, 1, 1, 1, 1, 0, 700, 99
22470, V, 1, 1, 1, 1, 0, 700, 99
22471, V, 1, 1, 1, 1, 0, 700, 99
22472, V, 1, 1, 1, 1, 0, 700, 99
22473, V, 1, 1, 1, 1, 0, 700, 99
22474, V, 1, 1, 1, 1, 0, 700, 99
22475, V, 1, 1, 1, 1, 0, 700, 99
22476, V, 1, 1, 1, 1, 0, 700, 99
22477, V, 1, 1, 1, 1, 0, 700, 99
22478, V, 1, 1, 1, 1, 0, 700, 99
22479, V, 1, 1, 1, 1, 0, 700, 99
22480, V, 1, 1, 1, 1, 0, 700, 99
22481, V, 1, 1, 1, 1, 0, 700, 99
22482, V, 1, 1, 1, 1, 0, 700, 99
22483, V, 1, 1, 1, 1, 0, 700, 99
22484, V, 1, 1, 1, 1, 0, 700, 99
22486, V, 1, 1, 1, 1, 0, 700, 100
22487, V, 1, 1, 1, 1, 0, 700, 99
22488, V, 1, 1, 1, 1, 0, 700, 99
22489, V, 1, 1, 1, 1, 0, 700, 99
22490, V, 1, 1, 1, 1, 0, 700, 99
22491, V, 1, 1, 1, 1, 0, 700, 99
22492, V, 1, 1, 1, 1, 0, 700, 99
22493, V, 1, 1, 1, 1, 0, 700, 99
22494, V, 1, 1, 1, 1, 0, 700, 99
22495, V, 1, 1, 1, 1, 0, 700, 99
22496, V, 1, 1, 1, 1, 0, 700, 99
22497, V, 1, 1, 1, 1, 0, 700, 99
22498, V, 1, 1, 1, 1, 0, 700, 99
22499, V, 1, 1, 1, 1, 0, 700, 99
22500, V, 1, 1, 1, 1, 0, 700, 99
22501, V, 1, 1, 1, 1, 0, 700, 99
22502, V, 1, 1, 1, 1, 0, 700, 99
22503, V, 1, 1, 1, 1, 0, 700, 99
22504, V, 1, 1, 1, 1, 0, 700, 99
22505, V, 1, 1, 1, 1, 0, 700, 99
22506, V, 1, 1, 1, 1, 0, 700, 99
22507, V, 1, 1, 1, 1, 0, 700, 99
22508, V, 1, 1, 1, 1, 0, 700, 99
22509, V, 1, 1, 1, 1, 0, 700, 99
22510, V, 1, 1, 1, 1, 0, 700, 99
22511, V, 1, 1, 1, 1, 0, 700, 99
22512, V, 1, 1, 1, 1, 0, 700, 99
22513, V, 1, 1, 1, 1, 0, 700, 99
22514, V, 1, 1, 1, 1, 0, 700, 99
22515, V, 1, 1, 1, 1, 0, 700, 99
22516, V, 1, 1, 1, 1, 0, 700, 99
22517, V, 1, 1, 1, 1, 0, 700, 99
22518, V, 1, 1, 1, 1, 0, 700, 99
22519, V, 1, 1, 1, 1, 0, 700, 99
22520, V, 1, 1, 1, 1, 0, 700, 99
22521, V, 1, 1, 1, 1, 0, 700, 99
22522, V, 1, 1, 1, 1, 0, 700, 99
22523, V, 1, 1, 1, 1, 0, 700, 99
22524, V, 1, 1, 1, 1, 0, 700, 99
22525, V, 1, 1, 1, 1, 0, 700, 99
22526, V, 1, 1, 1, 1, 0, 700, 99
22528, V, 1, 1, 1, 1, 0, 700, 99
22529, V, 1, 1, 1, 1, 0, 700, 99
22530, V, 1, 1, 1, 1, 0, 700, 99
22531, V, 1, 1, 1, 1, 0, 700, 99
22532, V, 1, 1, 1, 1, 0, 700, 99
22533, V, 1, 1, 1, 1, 0, 700, 99
22534, V, 1, 1, 1, 1, 0, 700, 99
22535, V, 1, 1, 1, 1, 0, 700, 99
22536, V, 1, 1, 1, 1, 0, 700, 99
22537, V, 1, 1, 1, 1, 0, 700, 99
22538, V, 1, 1, 1, 1, 0, 700, 99
22539, V, 1, 1, 1, 1, 0, 700, 99
22540, V, 1, 1, 1, 1, 0, 700, 99
22541, V, 1, 1, 1, 1, 0, 700, 99
22542, V, 1, 1, 1, 1, 0, 700, 99
22543, V, 1, 1, 1, 1, 0, 700, 99
22544, V, 1, 1, 1, 1, 0, 700, 99
22545, V, 1, 1, 1, 1, 0, 700, 99
22546, V, 1, 1, 1, 1, 0, 700, 99
22547, V, 1, 1, 1, 1, 0, 700, 99
22548, V, 1, 1, 1, 1, 0, 700, 99
22549, V, 1, 1, 1, 1, 0, 700, 99
22550, V, 1, 1, 1, 1, 0, 700, 99
22551, V, 1, 1, 1, 1, 0, 700, 99
22552, V, 1, 1, 1, 1, 0, 700, 99
22553, V, 1, 1, 1, 1, 0, 700, 99
22554, V, 1, 1, 1, 1, 0, 700, 99
22555, V, 1, 1, 1, 1, 0, 700, 99
22556, V, 1, 1, 1, 1, 0, 700, 99
22557, V, 1, 1, 1, 1, 0, 700, 99
22558, V, 1, 1, 1, 1, 0, 700, 99
22559, V, 1, 1, 1, 1, 0, 700, 99
22560, V, 1, 1, 1, 1, 0, 700, 99
22561, V, 1, 1, 1, 1, 0, 700, 99
22562, V, 1, 1, 1, 1, 0, 700, 99
22563, V, 1, 1, 1, 1, 0, 700, 99
22564, V, 1, 1, 1, 1, 0, 700, 99
22565, V, 1, 1, 1, 1, 0, 700, 99
22566, V, 1, 1, 1, 1, 0, 700, 99
22567, V, 1, 1, 1, 1, 0, 700, 99
22568, V, 1, 1, 1, 1, 0, 700, 99
22569, V, 1, 1, 1, 1, 0, 700, 99
22571, V, 1, 1, 1, 1, 0, 700, 99
22572, V, 1, 1, 1, 1, 0, 700, 99
22573, V, 1, 1, 1, 1, 0, 700, 99
22574, V, 1, 1, 1, 1, 0, 700, 99
22575, V, 1, 1, 1, 1, 0, 700, 99
22576, V, 1, 1, 1, 1, 0, 700, 99
22577, V, 1, 1, 1, 1, 0, 700, 99
22578, V, 1, 1, 1, 1, 0, 700, 99
22579, V, 1, 1, 1, 1, 0, 700, 99
22580, V, 1, 1, 1, 1, 0, 700, 99
22581, V, 1, 1, 1, 1, 0, 700, 99
22582, V, 1, 1, 1, 1, 0, 700, 99
22583, V, 1, 1, 1, 1, 0, 700, 99
22584, V, 1, 1, 1, 1, 0, 700, 99
22585, V, 1, 1, 1, 1, 0, 700, 99
22586, V, 1, 1, 1, 1, 0, 700, 99
22587, V, 1, 1, 1, 1, 0, 700, 99
22588, V, 1, 1, 1, 1, 0, 700, 99
22589, V, 1, 1, 1, 1, 0, 700, 99
22590, V, 1, 1, 1, 1, 0, 700, 99
22591, V, 1, 1, 1, 1, 0, 700, 99
22592, V, 1, 1, 1, 1, 0, 700, 99
22593, V, 1, 1, 1, 1, 0, 700, 99
22594, V, 1, 1, 1, 1, 0, 700, 99
22595, V, 1, 1, 1, 1, 0, 700, 99
22596, V, 1, 1, 1, 1, 0, 700, 99
22597, V, 1, 1, 1, 1, 0, 700, 99
22598, V, 1, 1, 1, 1, 0, 700, 99
22599, V, 1, 1, 1, 1, 0, 700, 99
22600, V, 1, 1, 1, 1, 0, 700, 99
22601, V, 1, 1, 1, 1, 0, 700, 99
22602, V, 1, 1, 1, 1, 0, 700, 99
22603, V, 1, 1, 1, 1, 0, 700, 99
22604, V, 1, 1, 1, 1, 0, 700, 99
22605, V, 1, 1, 1, 1, 0, 700, 99
22606, V, 1, 1, 1, 1, 0, 700, 99
22607, V, 1, 1, 1, 1, 0, 700, 99
22608, V, 1, 1, 1, 1, 0, 700, 99
22609, V, 1, 1, 1, 1, 0, 700, 99
22610, V, 1, 1, 1, 1, 0, 700, 99
22611, V, 1, 1, 1, 1, 0, 700, 99
22612, V, 1, 1, 1, 1, 0, 700, 99
22614, V, 1, 1, 1, 1, 0, 700, 99
22615, V, 1, 1, 1, 1, 0, 700, 99
22616, V, 1, 1, 1, 1, 0, 700, 99
22617, V, 1, 1, 1, 1, 0, 700, 99
22618, V, 1, 1, 1, 1, 0, 700, 99
22619, V, 1, 1, 1, 1, 0, 700, 99
22620, V, 1, 1, 1, 1, 0, 700, 99
22621, V, 1, 1, 1, 1, 0, 700, 99
22622, V, 1, 1, 1, 1, 0, 700, 99
22623, V, 1, 1, 1, 1, 0, 700, 99
22624, V, 1, 1, 1, 1, 0, 700, 99
22625, V, 1, 1, 1, 1, 0, 700, 99
22626, V, 1, 1, 1, 1, 0, 700, 99
22627, V, 1, 1, 1, 1, 0, 700, 99
22628, V, 1, 1, 1, 1, 0, 700, 99
22629, V, 1, 1, 1, 1, 0, 700, 99
22630, V, 1, 1, 1, 1, 0, 700, 99
22631, V, 1, 1, 1, 1, 0, 700, 99
22632, V, 1, 1, 1, 1, 0, 700, 99
22633, V, 1, 1, 1, 1, 0, 700, 99
22634, V, 1, 1, 1, 1, 0, 700, 99
22635, V, 1, 1, 1, 1, 0, 700, 99
22636, V, 1, 1, 1, 1, 0, 700, 99
22637, V, 1, 1, 1, 1, 0, 700, 99
22638, V, 1, 1, 1, 1, 0, 700, 99
22639, V, 1, 1, 1, 1, 0, 700, 99
22640, V, 1, 1, 1, 1, 0, 700, 99
22641, V, 1, 1, 1, 1, 0, 700, 99
22642, V, 1, 1, 1, 1, 0, 700, 99
22643, V, 1, 1, 1, 1, 0, 700, 99
22644, V, 1, 1, 1, 1, 0, 700, 99
22645, V, 1, 1, 1, 1, 0, 700, 99
22646, V, 1, 1, 1, 1, 0, 700, 99
22647, V, 1, 1, 1, 1, 0, 700, 99
22648, V, 1, 1, 1, 1, 0, 700, 99
22649, V, 1, 1, 1, 1, 0, 700, 99
22650, V, 1, 1, 1, 1, 0, 700, 99
22651, V, 1, 1, 1, 1, 0, 700, 99
22652, V, 1, 1, 1, 1, 0, 700, 99
22653, V, 1, 1, 1, 1, 0, 700, 99
22654, V, 1, 1, 1, 1, 0, 700, 99
22656, V, 1, 1, 1, 1, 0, 700, 99
22657, V, 1, 1, 1, 1, 0, 700, 99
22658, V, 1, 1, 1, 1, 0, 700, 99
22659, V, 1, 1, 1, 1, 0, 700, 99
22660, V, 1, 1, 1, 1, 0, 700, 99
22661, V, 1, 1, 1, 1, 0, 700, 99
22662, V, 1, 1, 1, 1, 0, 700, 99
22663, V, 1, 1, 1, 1, 0, 700, 99
22664, V, 1, 1, 1, 1, 0, 700, 99
22665, V, 1, 1, 1, 1, 0, 700, 99
22666, V, 1, 1, 1, 1, 0, 700, 99
22667, V, 1, 1, 1, 1, 0, 700, 99
22668, V, 1, 1, 1, 1, 0, 700, 99
22669, V, 1, 1, 1, 1, 0, 700, 99
22670, V, 1, 1, 1, 1, 0, 700, 99
22671, V, 1, 1, 1, 1, 0, 700, 99
22672, V, 1, 1, 1, 1, 0, 700, 99
22673, V, 1, 1, 1, 1, 0, 700, 99
22674, V, 1, 1, 1, 1, 0, 700, 99
22675, V, 1, 1, 1, 1, 0, 700, 99
22676, V, 1, 1, 1, 1, 0, 700, 99
22677, V, 1, 1, 1, 1, 0, 700, 99
22678, V, 1, 1, 1, 1, 0, 700, 99
22679, V, 1, 1, 1, 1, 0, 700, 99
22680, V, 1, 1, 1, 1, 0, 700, 99
22681, V, 1, 1, 1, 1, 0, 700, 99
22682, V, 1, 1, 1, 1, 0, 700, 99
22683, V, 1, 1, 1, 1, 0, 700, 99
22684, V, 1, 1, 1, 1, 0, 700, 99
22685, V, 1, 1, 1, 1, 0, 700, 99
22686, V, 1, 1, 1, 1, 0, 700, 99
22687, V, 1, 1, 1, 1, 0, 700, 99
22688, V, 1, 1, 1, 1, 0, 700, 99
22689, V, 1, 1, 1, 1, 0, 700, 99
22690, V, 1, 1, 1, 1, 0, 700, 99
22691, V, 1, 1, 1, 1, 0, 700, 99
22692, V, 1, 1, 1, 1, 0, 700, 99
22693, V, 1, 1, 1, 1, 0, 700, 99
22694, V, 1, 1, 1, 1, 0, 700, 99
22695, V, 1, 1, 1, 1, 0, 700, 99
22696, V, 1, 1, 1, 1, 0, 700, 99
22697, V, 1, 1, 1, 1, 0, 700, 99
22699, V, 1, 1, 1, 1, 0, 700, 99
22700, V, 1, 1, 1, 1, 0, 700, 99
22701, V, 1, 1, 1, 1, 0, 700, 99
22702, V, 1, 1, 1, 1, 0, 700, 99
22703, V, 1, 1, 1, 1, 0, 700, 99
22704, V, 1, 1, 1, 1, 0, 700, 99
22705, V, 1, 1, 1, 1, 0, 700, 99
22706, V, 1, 1, 1, 1, 0, 700, 99
22707, V, 1, 1, 1, 1, 0, 700, 99
22708, V, 1, 1, 1, 1, 0, 700, 99
22709, V, 1, 1, 1, 1, 0, 700, 99
22710, V, 1, 1, 1, 1, 0, 700, 99
22711, V, 1, 1, 1, 1, 0, 700, 99
22712, V, 1, 1, 1, 1, 0, 700, 99
22713, V, 1, 1, 1, 1, 0, 700, 99
22714, V, 1, 1, 1, 1, 0, 700, 99
22715, V, 1, 1, 1, 1, 0, 700, 99
22716, V, 1, 1, 1, 1, 0, 700, 99
22717, V, 1, 1, 1, 1, 0, 700, 99
22718, V, 1, 1, 1, 1, 0, 700, 99
22719, V, 1, 1, 1, 1, 0, 700, 99
22720, V, 1, 1, 1, 1, 0, 700, 99
22721, V, 1, 1, 1, 1, 0, 700, 99
22722, V, 1, 1, 1, 1, 0, 700, 99
22723, V, 1, 1, 1, 1, 0, 700, 99
22724, V, 1, 1, 1, 1, 0, 700, 99
22725, V, 1, 1, 1, 1, 0, 700, 99
22726, V, 1, 1, 1, 1, 0, 700, 99
22727, V, 1, 1, 1, 1, 0, 700, 99
22728, V, 1, 1, 1, 1, 0, 700, 99
22729, V, 1, 1, 1, 1, 0, 700, 99
22730, V, 1, 1, 1, 1, 0, 700, 99
22731, V, 1, 1, 1, 1, 0, 700, 99
22732, V, 1, 1, 1, 1, 0, 700, 99
22733, V, 1, 1, 1, 1, 0, 700, 99
22734, V, 1, 1, 1, 1, 0, 700, 99
22735, V, 1, 1, 1, 1, 0, 700, 99
22736, V, 1, 1, 1, 1, 0, 700, 99
22737, V, 1, 1, 1, 1, 0, 700, 99
22738, V, 1, 1, 1, 1, 0, 700, 99
22739, V, 1, 1, 1, 1, 0, 700, 99
22740, V, 1, 1, 1, 1, 0, 700, 99
22742, V, 1, 1, 1, 1, 0, 700, 99
22743, V, 1, 1, 1, 1, 0, 700, 99
22744, V, 1, 1, 1, 1, 0, 700, 99
22745, V, 1, 1, 1, 1, 0, 700, 99
22746, V, 1, 1, 1, 1, 0, 700, 99
22747, V, 1, 1, 1, 1, 0, 700, 99
22748, V, 1, 1, 1, 1, 0, 700, 99
22749, V, 1, 1, 1, 1, 0, 700, 99
22750, V, 1, 1, 1, 1, 0, 700, 99
22751, V, 1, 1, 1, 1, 0, 700, 99
22752, V, 1, 1, 1, 1, 0, 700, 99
22753, V, 1, 1, 1, 1, 0, 700, 99
22754, V, 1, 1, 1, 1, 0, 700, 99
22755, V, 1, 1, 1, 1, 0, 700, 99
22756, V, 1, 1, 1, 1, 0, 700, 99
22757, V, 1, 1, 1, 1, 0, 700, 99
22758, V, 1, 1, 1, 1, 0, 700, 99
22759, V, 1, 1, 1, 1, 0, 700, 99
22760, V, 1, 1, 1, 1, 0, 700, 99
22761, V, 1, 1, 1, 1, 0, 700, 99
22762, V, 1, 1, 1, 1, 0, 700, 99
22763, V, 1, 1, 1, 1, 0, 700, 99
22764, V, 1, 1, 1, 1, 0, 700, 99
22765, V, 1, 1, 1, 1, 0, 700, 99
22766, V, 1, 1, 1, 1, 0, 700, 99
22767, V, 1, 1, 1, 1, 0, 700, 99
22768, V, 1, 1, 1, 1, 0, 700, 99
22769, V, 1, 1, 1, 1, 0, 700, 99
22770, V, 1, 1, 1, 1, 0, 700, 99
22771, V, 1, 1, 1, 1, 0, 700, 99
22772, V, 1, 1, 1, 1, 0, 700, 99
22773, V, 1, 1, 1, 1, 0, 700, 99
22774, V, 1, 1, 1, 1, 0, 700, 99
22775, V, 1, 1, 1, 1, 0, 700, 99
22776, V, 1, 1, 1, 1, 0, 700, 99
22777, V, 1, 1, 1, 1, 0, 700, 99
22778, V, 1, 1, 1, 1, 0, 700, 99
22779, V, 1, 1, 1, 1, 0, 700, 99
22780, V, 1, 1, 1, 1, 0, 700, 99
22781, V, 1, 1, 1, 1, 0, 700, 99
22782, V, 1, 1, 1, 1, 0, 700, 99
22784, V, 1, 1, 1, 1, 0, 700, 99
22785, V, 1, 1, 1, 1, 0, 700, 99
22786, V, 1, 1, 1, 1, 0, 700, 99
22787, V, 1, 1, 1, 1, 0, 700, 99
22788, V, 1, 1, 1, 1, 0, 700, 99
22789, V, 1, 1, 1, 1, 0, 700, 99
22790, V, 1, 1, 1, 1, 0, 700, 99
22791, V, 1, 1, 1, 1, 0, 700, 99
22792, V, 1, 1, 1, 1, 0, 700, 99
22793, V, 1, 1, 1, 1, 0, 700, 99
22794, V, 1, 1, 1, 1, 0, 700, 99
22795, V, 1, 1, 1, 1, 0, 700, 99
22796, V, 1, 1, 1, 1, 0, 700, 99
22797, V, 1, 1, 1, 1, 0, 700, 99
22798, V, 1, 1, 1, 1, 0, 700, 99
22799, V, 1, 1, 1, 1, 0, 700, 99
22800, V, 1, 1, 1, 1, 0, 700, 99
22801, V, 1, 1, 1, 1, 0, 700, 99
22802, V, 1, 1, 1, 1, 0, 700, 99
22803, V, 1, 1, 1, 1, 0, 700, 99
22804, V, 1, 1, 1, 1, 0, 700, 99
22805, V, 1, 1, 1, 1, 0, 700, 99
22806, V, 1, 1, 1, 1, 0, 700, 99
22807, V, 1, 1, 1, 1, 0, 700, 99
22808, V, 1, 1, 1, 1, 0, 700, 99
22809, V, 1, 1, 1, 1, 0, 700, 99
22810, V, 1, 1, 1, 1, 0, 700, 99
22811, V, 1, 1, 1, 1, 0, 700, 99
22812, V, 1, 1, 1, 1, 0, 700, 99
22813, V, 1, 1, 1, 1, 0, 700, 99
22814, V, 1, 1, 1, 1, 0, 700, 99
22815, V, 1, 1, 1, 1, 0, 700, 99
22816, V, 1, 1, 1, 1, 0, 700, 99
22817, V, 1, 1, 1, 1, 0, 700, 99
22818, V, 1, 1, 1, 1, 0, 700, 99
22819, V, 1, 1, 1, 1, 0, 700, 99
22820, V, 1, 1, 1, 1, 0, 700, 99
22821, V, 1, 1, 1, 1, 0, 700, 99
22822, V, 1, 1, 1, 1, 0, 700, 99
22823, V, 1, 1, 1, 1, 0, 700, 99
22824, V, 1, 1, 1, 1, 0, 700, 99
22825, V, 1, 1, 1, 1, 0, 700, 99
22827, V, 1, 1, 1, 1, 0, 700, 99
22828, V, 1, 1, 1, 1, 0, 700, 99
22829, V, 1, 1, 1, 1, 0, 700, 99
22830, V, 1, 1, 1, 1, 0, 700, 99
22831, V, 1, 1, 1, 1, 0, 700, 99
22832, V, 1, 1, 1, 1, 0, 700, 99
22833, V, 1, 1, 1, 1, 0, 700, 99
22834, V, 1, 1, 1, 1, 0, 700, 99
22835, V, 1, 1, 1, 1, 0, 700, 99
22836, V, 1, 1, 1, 1, 0, 700, 99
22837, V, 1, 1, 1, 1, 0, 700, 99
22838, V, 1, 1, 1, 1, 0, 700, 99
22839, V, 1, 1, 1, 1, 0, 700, 99
22840, V, 1, 1, 1, 1, 0, 700, 99
22841, V, 1, 1, 1, 1, 0, 700, 99
22842, V, 1, 1, 1, 1, 0, 700, 99
22843, V, 1, 1, 1, 1, 0, 700, 99
22844, V, 1, 1, 1, 1, 0, 700, 99
22845, V, 1, 1, 1, 1, 0, 700, 99
22846, V, 1, 1, 1, 1, 0, 700, 99
22847, V, 1, 1, 1, 1, 0, 700, 99
22848, V, 1, 1, 1, 1, 0, 700, 99
22849, V, 1, 1, 1, 1, 0, 700, 99
22850, V, 1, 1, 1, 1, 0, 700, 99
22851, V, 1, 1, 1, 1, 0, 700, 99
22852, V, 1, 1, 1, 1, 0, 700, 99
22853, V, 1, 1, 1, 1, 0, 700, 99
22854, V, 1, 1, 1, 1, 0, 700, 99
22855, V, 1, 1, 1, 1, 0, 700, 99
22856, V, 1, 1, 1, 1, 0, 700, 99
22857, V, 1, 1, 1, 1, 0, 700, 99
22858, V, 1, 1, 1, 1, 0, 700, 99
22859, V, 1, 1, 1, 1, 0, 700, 99
22860, V, 1, 1, 1, 1, 0, 700, 99
22861, V, 1, 1, 1, 1, 0, 700, 99
22862, V, 1, 1, 1, 1, 0, 700, 99
22863, V, 1, 1, 1, 1, 0, 700, 99
22864, V, 1, 1, 1, 1, 0, 700, 99
22865, V, 1, 1, 1, 1, 0, 700, 99
22866, V, 1, 1, 1, 1, 0, 700, 99
22867, V, 1, 1, 1, 1, 0, 700, 99
22868, V, 1, 1, 1, 1, 0, 700, 99
22870, V, 1, 1, 1, 1, 0, 700, 99
22871, V, 1, 1, 1, 1, 0, 700, 99
22872, V, 1, 1, 1, 1, 0, 700, 99
22873, V, 1, 1, 1, 1, 0, 700, 99
22874, V, 1, 1, 1, 1, 0, 700, 99
22875, V, 1, 1, 1, 1, 0, 700, 99
22876, V, 1, 1, 1, 1, 0, 700, 99
22877, V, 1, 1, 1, 1, 0, 700, 99
22878, V, 1, 1, 1, 1, 0, 700, 99
22879, V, 1, 1, 1, 1, 0, 700, 99
22880, V, 1, 1, 1, 1, 0, 700, 99
22881, V, 1, 1, 1, 1, 0, 700, 99
22882, V, 1, 1, 1, 1, 0, 700, 99
22883, V, 1, 1, 1, 1, 0, 700, 99
22884, V, 1, 1, 1, 1, 0, 700, 99
22885, V, 1, 1, 1, 1, 0, 700, 99
22886, V, 1, 1, 1, 1, 0, 700, 99
22887, V, 1, 1, 1, 1, 0, 700, 99
22888, V, 1, 1, 1, 1, 0, 700, 99
22889, V, 1, 1, 1, 1, 0, 700, 99
22890, V, 1, 1, 1, 1, 0, 700, 99
22891, V, 1, 1, 1, 1, 0, 700, 99
22892, V, 1, 1, 1, 1, 0, 700, 99
22893, V, 1, 1, 1, 1, 0, 700, 99
22894, V, 1, 1, 1, 1, 0, 700, 99
22895, V, 1, 1, 1, 1, 0, 700, 99
22896, V, 1, 1, 1, 1, 0, 700, 99
22897, V, 1, 1, 1, 1, 0, 700, 99
22898, V, 1, 1, 1, 1, 0, 700, 99
22899, V, 1, 1, 1, 1, 0, 700, 99
22900, V, 1, 1, 1, 1, 0, 700, 99
22901, V, 1, 1, 1, 1, 0, 700, 99
22902, V, 1, 1, 1, 1, 0, 700, 99
22903, V, 1, 1, 1, 1, 0, 700, 99
22904, V, 1, 1, 1, 1, 0, 700, 99
22905, V, 1, 1, 1, 1, 0, 700, 99
22906, V, 1, 1, 1, 1, 0, 700, 99
22907, V, 1, 1, 1, 1, 0, 700, 99
22908, V, 1, 1, 1, 1, 0, 700, 99
22909, V, 1, 1, 1, 1, 0, 700, 99
22910, V, 1, 1, 1, 1, 0, 700, 99
22912, V, 1, 1, 1, 1, 0, 700, 99
22913, V, 1, 1, 1, 1, 0, 700, 99
22914, V, 1, 1, 1, 1, 0, 700, 99
22915, V, 1, 1, 1, 1, 0, 700, 99
22916, V, 1, 1, 1, 1, 0, 700, 99
22917, V, 1, 1, 1, 1, 0, 700, 99
22918, V, 1, 1, 1, 1, 0, 700, 99
22919, V, 1, 1, 1, 1, 0, 700, 99
22920, V, 1, 1, 1, 1, 0, 700, 99
22921, V, 1, 1, 1, 1, 0, 700, 99
22922, V, 1, 1, 1, 1, 0, 700, 99
22923, V, 1, 1, 1, 1, 0, 700, 99
22924, V, 1, 1, 1, 1, 0, 700, 99
22925, V, 1, 1, 1, 1, 0, 700, 99
22926, V, 1, 1, 1, 1, 0, 700, 99
22927, V, 1, 1, 1, 1, 0, 700, 99
22928, V, 1, 1, 1, 1, 0, 700, 99
22929, V, 1, 1, 1, 1, 0, 700, 99
22930, V, 1, 1, 1, 1, 0, 700, 99
22931, V, 1, 1, 1, 1, 0, 700, 99
22932, V, 1, 1, 1, 1, 0, 700, 99
22933, V, 1, 1, 1, 1, 0, 700, 99
22934, V, 1, 1, 1, 1, 0, 700, 99
22935, V, 1, 1, 1, 1, 0, 700, 99
22936, V, 1, 1, 1, 1, 0, 700, 99
22937, V, 1, 1, 1, 1, 0, 700, 99
22938, V, 1, 1, 1, 1, 0, 700, 99
22939, V, 1, 1, 1, 1, 0, 700, 99
22940, V, 1, 1, 1, 1, 0, 700, 99
22941, V, 1, 1, 1, 1, 0, 700, 99
22942, V, 1, 1, 1, 1, 0, 700, 99
22943, V, 1, 1, 1, 1, 0, 700, 99
22944, V, 1, 1, 1, 1, 0, 700, 99
22945, V, 1, 1, 1, 1, 0, 700, 99
22946, V, 1, 1, 1, 1, 0, 700, 99
22947, V, 1, 1, 1, 1, 0, 700, 99
22948, V, 1, 1, 1, 1, 0, 700, 99
22949, V, 1, 1, 1, 1, 0, 700, 99
22950, V, 1, 1, 1, 1, 0, 700, 99
22951, V, 1, 1, 1, 1, 0, 700, 99
22952, V, 1, 1, 1, 1, 0, 700, 99
22953, V, 1, 1, 1, 1, 0, 700, 99
22955, V, 1, 1, 1, 1, 0, 700, 99
22956, V, 1, 1, 1, 1, 0, 700, 99
22957, V, 1, 1, 1, 1, 0, 700, 99
22958, V, 1, 1, 1, 1, 0, 700, 99
22959, V, 1, 1, 1, 1, 0, 700, 99
22960, V, 1, 1, 1, 1, 0, 700, 99
22961, V, 1, 1, 1, 1, 0, 700, 99
22962, V, 1, 1, 1, 1, 0, 700, 99
22963, V, 1, 1, 1, 1, 0, 700, 99
22964, V, 1, 1, 1, 1, 0, 700, 99
22965, V, 1, 1, 1, 1, 0, 700, 99
22966, V, 1, 1, 1, 1, 0, 700, 99
22967, V, 1, 1, 1, 1, 0, 700, 99
22968, V, 1, 1, 1, 1, 0, 700, 99
22969, V, 1, 1, 1, 1, 0, 700, 99
22970, V, 1, 1, 1, 1, 0, 700, 99
22971, V, 1, 1, 1, 1, 0, 700, 99
22972, V, 1, 1, 1, 1, 0, 700, 99
22973, V, 1, 1, 1, 1, 0, 700, 99
22974, V, 1, 1, 1, 1, 0, 700, 99
22975, V, 1, 1, 1, 1, 0, 700, 99
22976, V, 1, 1, 1, 1, 0, 700, 99
22977, V, 1, 1, 1, 1, 0, 700, 99
22978, V, 1, 1, 1, 1, 0, 700, 99
22979, V, 1, 1, 1, 1, 0, 700, 99
22980, V, 1, 1, 1, 1, 0, 700, 99
22981, V, 1, 1, 1, 1, 0, 700, 99
22982, V, 1, 1, 1, 1, 0, 700, 99
22983, V, 1, 1, 1, 1, 0, 700, 99
22984, V, 1, 1, 1, 1, 0, 700, 99
22985, V, 1, 1, 1, 1, 0, 700, 99
22986, V, 1, 1, 1, 1, 0, 700, 99
22987, V, 1, 1, 1, 1, 0, 700, 99
22988, V, 1, 1, 1, 1, 0, 700, 99
22989, V, 1, 1, 1, 1, 0, 700, 99
22990, V, 1, 1, 1, 1, 0, 700, 99
22991, V, 1, 1, 1, 1, 0, 700, 99
22992, V, 1, 1, 1, 1, 0, 700, 99
22993, V, 1, 1, 1, 1, 0, 700, 99
22994, V, 1, 1, 1, 1, 0, 700, 99
22995, V, 1, 1, 1, 1, 0, 700, 99
22996, V, 1, 1, 1, 1, 0, 700, 99
22998, V, 1, 1, 1, 1, 0, 700, 99
22999, V, 1, 1, 1, 1, 0, 700, 99
23000, V, 1, 1, 1, 1, 0, 700, 99
23001, V, 1, 1, 1, 1, 0, 700, 99
23002, V, 1, 1, 1, 1, 0, 700, 99
23003, V, 1, 1, 1, 1, 0, 700, 99
23004, V, 1, 1, 1, 1, 0, 700, 99
23005, V, 1, 1, 1, 1, 0, 700, 99
23006, V, 1, 1, 1, 1, 0, 700, 99
23007, V, 1, 1, 1, 1, 0, 700, 99
23008, V, 1, 1, 1, 1, 0, 700, 99
23009, V, 1, 1, 1, 1, 0, 700, 99
23010, V, 1, 1, 1, 1, 0, 700, 99
23011, V, 1, 1, 1, 1, 0, 700, 99
23012, V, 1, 1, 1, 1, 0, 700, 99
23013, V, 1, 1, 1, 1, 0, 700, 99
23014, V, 1, 1, 1, 1, 0, 700, 99
23015, V, 1, 1, 1, 1, 0, 700, 99
23016, V, 1, 1, 1, 1, 0, 700, 99
23017, V, 1, 1, 1, 1, 0, 700, 99
23018, V, 1, 1, 1, 1, 0, 700, 99
23019, V, 1, 1, 1, 1, 0, 700, 99
23020, V, 1, 1, 1, 1, 0, 700, 99
23021, V, 1, 1, 1, 1, 0, 700, 99
23022, V, 1, 1, 1, 1, 0, 700, 99
23023, V, 1, 1, 1, 1, 0, 700, 99
23024, V, 1, 1, 1, 1, 0, 700, 99
23025, V, 1, 1, 1, 1, 0, 700, 99
23026, V, 1, 1, 1, 1, 0, 700, 99
23027, V, 1, 1, 1, 1, 0, 700, 99
23028, V, 1, 1, 1, 1, 0, 700, 99
23029, V, 1, 1, 1, 1, 0, 700, 99
23030, V, 1, 1, 1, 1, 0, 700, 99
23031, V, 1, 1, 1, 1, 0, 700, 99
23032, V, 1, 1, 1, 1, 0, 700, 99
23033, V, 1, 1, 1, 1, 0, 700, 99
23034, V, 1, 1, 1, 1, 0, 700, 99
23035, V, 1, 1, 1, 1, 0, 700, 99
23036, V, 1, 1, 1, 1, 0, 700, 99
23037, V, 1, 1, 1, 1, 0, 700, 99
23038, V, 1, 0, 0, 1, 0, 700, 99
23038, V, 1, 0, 0, 0, 0, 700, 99
23040, V, 1, 1, 0, 0, 0, 700, 99
23040, V, 1, 1, 0, 0, 0, 700, 99
23041, V, 1, 1, 1, 1, 0, 700, 99
23042, V, 1, 1, 1, 1, 0, 700, 99
23043, V, 1, 1, 1, 1, 0, 700, 99
23044, V, 1, 1, 1, 1, 0, 700, 99
23045, V, 1, 1, 1, 1, 0, 700, 99
23046, V, 1, 1, 1, 1, 0, 700, 99
23047, V, 1, 1, 1, 1, 0, 700, 98
23048, V, 1, 1, 1, 1, 0, 700, 98
23049, V, 1, 1, 1, 1, 0, 700, 98
23050, V, 1, 1, 1, 1, 0, 700, 98
23051, V, 1, 1, 1, 1, 0, 700, 98
23052, V, 1, 1, 1, 1, 0, 700, 98
23053, V, 1, 1, 1, 1, 0, 700, 98
23054, V, 1, 1, 1, 1, 0, 700, 98
23055, V, 1, 1, 1, 1, 0, 700, 99
23056, V, 1, 1, 1, 1, 0, 700, 99
23057, V, 1, 1, 1, 1, 0, 700, 99
23058, V, 1, 1, 1, 1, 0, 700, 99
23059, V, 1, 1, 1, 1, 0, 700, 99
23060, V, 1, 1, 1, 1, 0, 700, 99
23061, V, 1, 1, 1, 1, 0, 700, 99
23062, V, 1, 1, 1, 1, 0, 700, 99
23063, V, 1, 1, 1, 1, 0, 700, 99
23064, V, 1, 1, 1, 1, 0, 700, 99
23065, V, 1, 1, 1, 1, 0, 700, 99
23066, V, 1, 1, 1, 1, 0, 700, 99
23067, V, 1, 1, 1, 1, 0, 700, 99
23068, V, 1, 1, 1, 1, 0, 700, 99
23069, V, 1, 1, 1, 1, 0, 700, 99
23070, V, 1, 1, 1, 1, 0, 700, 99
23071, V, 1, 1, 1, 1, 0, 700, 99
23072, V, 1, 1, 1, 1, 0, 700, 99
23073, V, 1, 1, 1, 1, 0, 700, 99
23074, V, 1, 1, 1, 1, 0, 700, 99
23075, V, 1, 1, 1, 1, 0, 700, 99
23076, V, 1, 1, 1, 1, 0, 700, 99
23077, V, 1, 1, 1, 1, 0, 700, 99
23078, V, 1, 1, 1, 1, 0, 700, 99
23079, V, 1, 1, 1, 1, 0, 700, 99
23080, V, 1, 1, 1, 1, 0, 700, 99
23081, V, 1, 1, 1, 1, 0, 700, 99
23083, V, 1, 1, 1, 1, 0, 700, 99
23084, V, 1, 1, 1, 1, 0, 700, 99
23085, V, 1, 1, 1, 1, 0, 700, 99
23086, V, 1, 1, 1, 1, 0, 700, 99
23087, V, 1, 1, 1, 1, 0, 700, 99
23088, V, 1, 1, 1, 1, 0, 700, 99
23089, V, 1, 1, 1, 1, 0, 700, 99
23090, V, 1, 1, 1, 1, 0, 700, 99
23091, V, 1, 1, 1, 1, 0, 700, 99
23092, V, 1, 1, 1, 1, 0, 700, 99
23093, V, 1, 1, 1, 1, 0, 700, 99
23094, V, 1, 1, 1, 1, 0, 700, 99
23095, V, 1, 1, 1, 1, 0, 700, 99
23096, V, 1, 1, 1, 1, 0, 700, 99
23097, V, 1, 1, 1, 1, 0, 700, 99
23098, V, 1, 1, 1, 1, 0, 700, 99
23099, V, 1, 1, 1, 1, 0, 700, 99
23100, V, 1, 1, 1, 1, 0, 700, 99
23101, V, 1, 1, 1, 1, 0, 700, 99
23102, V, 1, 1, 1, 1, 0, 700, 99
23103, V, 1, 1, 1, 1, 0, 700, 99
23104, V, 1, 1, 1, 1, 0, 700, 99
23105, V, 1, 1, 1, 1, 0, 700, 99
23106, V, 1, 1, 1, 1, 0, 700, 99
23107, V, 1, 1, 1, 1, 0, 700, 99
23108, V, 1, 1, 1, 1, 0, 700, 99
23109, V, 1, 1, 1, 1, 0, 700, 99
23110, V, 1, 1, 1, 1, 0, 700, 99
23111, V, 1, 1, 1, 1, 0, 700, 99
23112, V, 1, 1, 1, 1, 0, 700, 99
23113, V, 1, 1, 1, 1, 0, 700, 99
23114, V, 1, 1, 1, 1, 0, 700, 99
23115, V, 1, 1, 1, 1, 0, 700, 99
23116, V, 1, 1, 1, 1, 0, 700, 99
23117, V, 1, 1, 1, 1, 0, 700, 99
23118, V, 1, 1, 1, 1, 0, 700, 99
23119, V, 1, 1, 1, 1, 0, 700, 99
23120, V, 1, 1, 1, 1, 0, 700, 99
23121, V, 1, 1, 1, 1, 0, 700, 99
23122, V, 1, 1, 1, 1, 0, 700, 99
23123, V, 1, 1, 1, 1, 0, 700, 99
23124, V, 1, 1, 1, 1, 0, 700, 99
23126, V, 1, 1, 1, 1, 0, 700, 99
23127, V, 1, 1, 1, 1, 0, 700, 99
23128, V, 1, 1, 1, 1, 0, 700, 99
23129, V, 1, 1, 1, 1, 0, 700, 99
23130, V, 1, 1, 1, 1, 0, 700, 99
23131, V, 1, 1, 1, 1, 0, 700, 99
23132, V, 1, 1, 1, 1, 0, 700, 99
23133, V, 1, 1, 1, 1, 0, 700, 99
23134, V, 1, 1, 1, 1, 0, 700, 99
23135, V, 1, 1, 1, 1, 0, 700, 99
23136, V, 1, 1, 1, 1, 0, 700, 99
23137, V, 1, 1, 1, 1, 0, 700, 99
23138, V, 1, 1, 1, 1, 0, 700, 99
23139, V, 1, 1, 1, 1, 0, 700, 99
23140, V, 1, 1, 1, 1, 0, 700, 99
23141, V, 1, 1, 1, 1, 0, 700, 99
23142, V, 1, 1, 1, 1, 0, 700, 99
23143, V, 1, 1, 1, 1, 0, 700, 99
23144, V, 1, 1, 1, 1, 0, 700, 99
23145, V, 1, 1, 1, 1, 0, 700, 99
23146, V, 1, 1, 1, 1, 0, 700, 99
23147, V, 1, 1, 1, 1, 0, 700, 99
23148, V, 1, 1, 1, 1, 0, 700, 99
23149, V, 1, 1, 1, 1, 0, 700, 99
23150, V, 1, 1, 1, 1, 0, 700, 99
23151, V, 1, 1, 1, 1, 0, 700, 99
23152, V, 1, 1, 1, 1, 0, 700, 99
23153, V, 1, 1, 1, 1, 0, 700, 99
23154, V, 1, 1, 1, 1, 0, 700, 99
23155, V, 1, 1, 1, 1, 0, 700, 99
23156, V, 1, 1, 1, 1, 0, 700, 99
23157, V, 1, 1, 1, 1, 0, 700, 99
23158, V, 1, 1, 1, 1, 0, 700, 99
23159, V, 1, 1, 1, 1, 0, 700, 99
23160, V, 1, 1, 1, 1, 0, 700, 99
23161, V, 1, 1, 1, 1, 0, 700, 99
23162, V, 1, 1, 1, 1, 0, 700, 99
23163, V, 1, 1, 1, 1, 0, 700, 99
23164, V, 1, 1, 1, 1, 0, 700, 99
23165, V, 1, 1, 1, 1, 0, 700, 99
23166, V, 1, 1, 1, 1, 0, 700, 99
23168, V, 1, 1, 1, 1, 0, 700, 99
23169, V, 1, 1, 1, 1, 0, 700, 99
23170, V, 1, 1, 1, 1, 0, 700, 99
23171, V, 1, 1, 1, 1, 0, 700, 99
23172, V, 1, 1, 1, 1, 0, 700, 99
23173, V, 1, 1, 1, 1, 0, 700, 99
23174, V, 1, 1, 1, 1, 0, 700, 99
23175, V, 1, 1, 1, 1, 0, 700, 99
23176, V, 1, 1, 1, 1, 0, 700, 99
23177, V, 1, 1, 1, 1, 0, 700, 99
23178, V, 1, 1, 1, 1, 0, 700, 99
23179, V, 1, 1, 1, 1, 0, 700, 99
23180, V, 1, 1, 1, 1, 0, 700, 99
23181, V, 1, 1, 1, 1, 0, 700, 99
23182, V, 1, 1, 1, 1, 0, 700, 99
23183, V, 1, 1, 1, 1, 0, 700, 99
23184, V, 1, 1, 1, 1, 0, 700, 99
23185, V, 1, 1, 1, 1, 0, 700, 99
23186, V, 1, 1, 1, 1, 0, 700, 99
23187, V, 1, 1, 1, 1, 0, 700, 99
23188, V, 1, 1, 1, 1, 0, 700, 99
23189, V, 1, 1, 1, 1, 0, 700, 99
23190, V, 1, 1, 1, 1, 0, 700, 99
23191, V, 1, 1, 1, 1, 0, 700, 99
23192, V, 1, 1, 1, 1, 0, 700, 99
23193, V, 1, 1, 1, 1, 0, 700, 99
23194, V, 1, 1, 1, 1, 0, 700, 99
23195, V, 1, 1, 1, 1, 0, 700, 99
23196, V, 1, 1, 1, 1, 0, 700, 99
23197, V, 1, 1, 1, 1, 0, 700, 99
23198, V, 1, 1, 1, 1, 0, 700, 99
23199, V, 1, 1, 1, 1, 0, 700, 99
23200, V, 1, 1, 1, 1, 0, 700, 99
23201, V, 1, 1, 1, 1, 0, 700, 99
23202, V, 1, 1, 1, 1, 0, 700, 99
23203, V, 1, 1, 1, 1, 0, 700, 99
23204, V, 1, 1, 1, 1, 0, 700, 99
23205, V, 1, 1, 1, 1, 0, 700, 99
23206, V, 1, 1, 1, 1, 0, 700, 99
23207, V, 1, 1, 1, 1, 0, 700, 99
23208, V, 1, 1, 1, 1, 0, 700, 99
23209, V, 1, 1, 1, 1, 0, 700, 99
23211, V, 1, 1, 1, 1, 0, 700, 99
23212, V, 1, 1, 1, 1, 0, 700, 99
23213, V, 1, 1, 1, 1, 0, 700, 99
23214, V, 1, 1, 1, 1, 0, 700, 99
23215, V, 1, 1, 1, 1, 0, 700, 99
23216, V, 1, 1, 1, 1, 0, 700, 99
23217, V, 1, 1, 1, 1, 0, 700, 99
23218, V, 1, 1, 1, 1, 0, 700, 99
23219, V, 1, 1, 1, 1, 0, 700, 99
23220, V, 1, 1, 1, 1, 0, 700, 99
23221, V, 1, 1, 1, 1, 0, 700, 99
23222, V, 1, 1, 1, 1, 0, 700, 99
23223, V, 1, 1, 1, 1, 0, 700, 99
23224, V, 1, 1, 1, 1, 0, 700, 99
23225, V, 1, 1, 1, 1, 0, 700, 99
23226, V, 1, 1, 1, 1, 0, 700, 99
23227, V, 1, 1, 1, 1, 0, 700, 99
23228, V, 1, 1, 1, 1, 0, 700, 99
23229, V, 1, 1, 1, 1, 0, 700, 99
23230, V, 1, 1, 1, 1, 0, 700, 99
23231, V, 1, 1, 1, 1, 0, 700, 99
23232, V, 1, 1, 1, 1, 0, 700, 99
23233, V, 1, 1, 1, 1, 0, 700, 99
23234, V, 1, 1, 1, 1, 0, 700, 99
23235, V, 1, 1, 1, 1, 0, 700, 99
23236, V, 1, 1, 1, 1, 0, 700, 99
23237, V, 1, 1, 1, 1, 0, 700, 99
23238, V, 1, 1, 1, 1, 0, 700, 99
23239, V, 1, 1, 1, 1, 0, 700, 99
23240, V, 1, 1, 1, 1, 0, 700, 99
23241, V, 1, 1, 1, 1, 0, 700, 99
23242, V, 1, 1, 1, 1, 0, 700, 99
23243, V, 1, 1, 1, 1, 0, 700, 99
23244, V, 1, 1, 1, 1, 0, 700, 99
23245, V, 1, 1, 1, 1, 0, 700, 99
23246, V, 1, 1, 1, 1, 0, 700, 99
23247, V, 1, 1, 1, 1, 0, 700, 99
23248, V, 1, 1, 1, 1, 0, 700, 99
23249, V, 1, 1, 1, 1, 0, 700, 99
23250, V, 1, 1, 1, 1, 0, 700, 99
23251, V, 1, 1, 1, 1, 0, 700, 99
23252, V, 1, 1, 1, 1, 0, 700, 99
23254, V, 1, 1, 1, 1, 0, 700, 99
23255, V, 1, 1, 1, 1, 0, 700, 99
23256, V, 1, 1, 1, 1, 0, 700, 99
23257, V, 1, 1, 1, 1, 0, 700, 99
23258, V, 1, 1, 1, 1, 0, 700, 99
23259, V, 1, 1, 1, 1, 0, 700, 99
23260, V, 1, 1, 1, 1, 0, 700, 99
23261, V, 1, 1, 1, 1, 0, 700, 99
23262, V, 1, 1, 1, 1, 0, 700, 99
23263, V, 1, 1, 1, 1, 0, 700, 99
23264, V, 1, 1, 1, 1, 0, 700, 99
23265, V, 1, 1, 1, 1, 0, 700, 99
23266, V, 1, 1, 1, 1, 0, 700, 99
23267, V, 1, 1, 1, 1, 0, 700, 99
23268, V, 1, 1, 1, 1, 0, 700, 99
23269, V, 1, 1, 1, 1, 0, 700, 99
23270, V, 1, 1, 1, 1, 0, 700, 99
23271, V, 1, 1, 1, 1, 0, 700, 99
23272, V, 1, 1, 1, 1, 0, 700, 99
23273, V, 1, 1, 1, 1, 0, 700, 99
23274, V, 1, 1, 1, 1, 0, 700, 99
23275, V, 1, 1, 1, 1, 0, 700, 99
23276, V, 1, 1, 1, 1, 0, 700, 99
23277, V, 1, 1, 1, 1, 0, 700, 99
23278, V, 1, 1, 1, 1, 0, 700, 99
23279, V, 1, 1, 1, 1, 0, 700, 99
23280, V, 1, 1, 1, 1, 0, 700, 99
23281, V, 1, 1, 1, 1, 0, 700, 99
23282, V, 1, 1, 1, 1, 0, 700, 99
23283, V, 1, 1, 1, 1, 0, 700, 99
23284, V, 1, 1, 1, 1, 0, 700, 99
23285, V, 1, 1, 1, 1, 0, 700, 99
23286, V, 1, 1, 1, 1, 0, 700, 99
23287, V, 1, 1, 1, 1, 0, 700, 99
23288, V, 1, 1, 1, 1, 0, 700, 99
23289, V, 1, 1, 1, 1, 0, 700, 99
23290, V, 1, 1, 1, 1, 0, 700, 99
23291, V, 1, 1, 1, 1, 0, 700, 99
23292, V, 1, 1, 1, 1, 0, 700, 99
23293, V, 1, 1, 1, 1, 0, 700, 99
23294, V, 1, 1, 1, 1, 0, 700, 99
23296, V, 1, 1, 1, 1, 0, 700, 99
23297, V, 1, 1, 1, 1, 0, 700, 99
23298, V, 1, 1, 1, 1, 0, 700, 99
23299, V, 1, 1, 1, 1, 0, 700, 99
23300, V, 1, 1, 1, 1, 0, 700, 99
23301, V, 1, 1, 1, 1, 0, 700, 99
23302, V, 1, 1, 1, 1, 0, 700, 99
23303, V, 1, 1, 1, 1, 0, 700, 99
23304, V, 1, 1, 1, 1, 0, 700, 99
23305, V, 1, 1, 1, 1, 0, 700, 99
23306, V, 1, 1, 1, 1, 0, 700, 99
23307, V, 1, 1, 1, 1, 0, 700, 99
23308, V, 1, 1, 1, 1, 0, 700, 99
23309, V, 1, 1, 1, 1, 0, 700, 99
23310, V, 1, 1, 1, 1, 0, 700, 99
23311, V, 1, 1, 1, 1, 0, 700, 99
23312, V, 1, 1, 1, 1, 0, 700, 99
23313, V, 1, 1, 1, 1, 0, 700, 99
23314, V, 1, 1, 1, 1, 0, 700, 99
23315, V, 1, 1, 1, 1, 0, 700, 99
23316, V, 1, 1, 1, 1, 0, 700, 99
23317, V, 1, 1, 1, 1, 0, 700, 99
23318, V, 1, 1, 1, 1, 0, 700, 99
23319, V, 1, 1, 1, 1, 0, 700, 99
23320, V, 1, 1, 1, 1, 0, 700, 99
23321, V, 1, 1, 1, 1, 0, 700, 99
23322, V, 1, 1, 1, 1, 0, 700, 99
23323, V, 1, 1, 1, 1, 0, 700, 99
23324, V, 1, 1, 1, 1, 0, 700, 99
23325, V, 1, 1, 1, 1, 0, 700, 99
23326, V, 1, 1, 1, 1, 0, 700, 99
23327, V, 1, 1, 1, 1, 0, 700, 99
23328, V, 1, 1, 1, 1, 0, 700, 99
23329, V, 1, 1, 1, 1, 0, 700, 99
23330, V, 1, 1, 1, 1, 0, 700, 99
23331, V, 1, 1, 1, 1, 0, 700, 99
23332, V, 1, 1, 1, 1, 0, 700, 99
23333, V, 1, 1, 1, 1, 0, 700, 99
23334, V, 1, 1, 1, 1, 0, 700, 99
23335, V, 1, 1, 1, 1, 0, 700, 99
23336, V, 1, 1, 1, 1, 0, 700, 99
23337, V, 1, 1, 1, 1, 0, 700, 99
23339, V, 1, 1, 1, 1, 0, 700, 99
23340, V, 1, 1, 1, 1, 0, 700, 99
23341, V, 1, 1, 1, 1, 0, 700, 99
23342, V, 1, 1, 1, 1, 0, 700, 99
23343, V, 1, 1, 1, 1, 0, 700, 99
23344, V, 1, 1, 1, 1, 0, 700, 99
23345, V, 1, 1, 1, 1, 0, 700, 99
23346, V, 1, 1, 1, 1, 0, 700, 99
23347, V, 1, 1, 1, 1, 0, 700, 99
23348, V, 1, 1, 1, 1, 0, 700, 99
23349, V, 1, 1, 1, 1, 0, 700, 99
23350, V, 1, 1, 1, 1, 0, 700, 99
23351, V, 1, 1, 1, 1, 0, 700, 99
23352, V, 1, 1, 1, 1, 0, 700, 99
23353, V, 1, 1, 1, 1, 0, 700, 99
23354, V, 1, 1, 1, 1, 0, 700, 99
23355, V, 1, 1, 1, 1, 0, 700, 99
23356, V, 1, 1, 1, 1, 0, 700, 99
23357, V, 1, 1, 1, 1, 0, 700, 99
23358, V, 1, 1, 1, 1, 0, 700, 99
23359, V, 1, 1, 1, 1, 0, 700, 99
23360, V, 1, 1, 1, 1, 0, 700, 99
23361, V, 1, 1, 1, 1, 0, 700, 99
23362, V, 1, 1, 1, 1, 0, 700, 99
23363, V, 1, 1, 1, 1, 0, 700, 99
23364, V, 1, 1, 1, 1, 0, 700, 99
23365, V, 1, 1, 1, 1, 0, 700, 99
23366, V, 1, 1, 1, 1, 0, 700, 99
23367, V, 1, 1, 1, 1, 0, 700, 99
23368, V, 1, 1, 1, 1, 0, 700, 99
23369, V, 1, 1, 1, 1, 0, 700, 99
23370, V, 1, 1, 1, 1, 0, 700, 99
23371, V, 1, 1, 1, 1, 0, 700, 99
23372, V, 1, 1, 1, 1, 0, 700, 99
23373, V, 1, 1, 1, 1, 0, 700, 99
23374, V, 1, 1, 1, 1, 0, 700, 99
23375, V, 1, 1, 1, 1, 0, 700, 99
23376, V, 1, 1, 1, 1, 0, 700, 99
23377, V, 1, 1, 1, 1, 0, 700, 99
23378, V, 1, 1, 1, 1, 0, 700, 99
23379, V, 1, 1, 1, 1, 0, 700, 99
23380, V, 1, 1, 1, 1, 0, 700, 99
23382, V, 1, 1, 1, 1, 0, 700, 99
23383, V, 1, 1, 1, 1, 0, 700, 99
23384, V, 1, 1, 1, 1, 0, 700, 99
23385, V, 1, 1, 1, 1, 0, 700, 99
23386, V, 1, 1, 1, 1, 0, 700, 99
23387, V, 1, 1, 1, 1, 0, 700, 99
23388, V, 1, 1, 1, 1, 0, 700, 99
23389, V, 1, 1, 1, 1, 0, 700, 99
23390, V, 1, 1, 1, 1, 0, 700, 99
23391, V, 1, 1, 1, 1, 0, 700, 99
23392, V, 1, 1, 1, 1, 0, 700, 99
23393, V, 1, 1, 1, 1, 0, 700, 99
23394, V, 1, 1, 1, 1, 0, 700, 99
23395, V, 1, 1, 1, 1, 0, 700, 99
23396, V, 1, 1, 1, 1, 0, 700, 99
23397, V, 1, 1, 1, 1, 0, 700, 99
23398, V, 1, 1, 1, 1, 0, 700, 99
23399, V, 1, 1, 1, 1, 0, 700, 99
23400, V, 1, 1, 1, 1, 0, 700, 99
23401, V, 1, 1, 1, 1, 0, 700, 99
23402, V, 1, 1, 1, 1, 0, 700, 99
23403, V, 1, 1, 1, 1, 0, 700, 99
23404, V, 1, 1, 1, 1, 0, 700, 99
23405, V, 1, 1, 1, 1, 0, 700, 99
23406, V, 1, 1, 1, 1, 0, 700, 99
23407, V, 1, 1, 1, 1, 0, 700, 99
23408, V, 1, 1, 1, 1, 0, 700, 99
23409, V, 1, 1, 1, 1, 0, 700, 99
23410, V, 1, 1, 1, 1, 0, 700, 99
23411, V, 1, 1, 1, 1, 0, 700, 99
23412, V, 1, 1, 1, 1, 0, 700, 99
23413, V, 1, 1, 1, 1, 0, 700, 99
23414, V, 1, 1, 1, 1, 0, 700, 99
23415, V, 1, 1, 1, 1, 0, 700, 99
23416, V, 1, 1, 1, 1, 0, 700, 99
23417, V, 1, 1, 1, 1, 0, 700, 99
23418, V, 1, 1, 1, 1, 0, 700, 99
23419, V, 1, 1, 1, 1, 0, 700, 99
23420, V, 1, 1, 1, 1, 0, 700, 99
23421, V, 1, 1, 1, 1, 0, 700, 99
23422, V, 1, 1, 1, 1, 0, 700, 99
23424, V, 1, 1, 1, 1, 0, 700, 99
23425, V, 1, 1, 1, 1, 0, 700, 99
23426, V, 1, 1, 1, 1, 0, 700, 99
23427, V, 1, 1, 1, 1, 0, 700, 99
23428, V, 1, 1, 1, 1, 0, 700, 99
23429, V, 1, 1, 1, 1, 0, 700, 99
23430, V, 1, 1, 1, 1, 0, 700, 99
23431, V, 1, 1, 1, 1, 0, 700, 99
23432, V, 1, 1, 1, 1, 0, 700, 99
23433, V, 1, 1, 1, 1, 0, 700, 99
23434, V, 1, 1, 1, 1, 0, 700, 99
23435, V, 1, 1, 1, 1, 0, 700, 99
23436, V, 1, 1, 1, 1, 0, 700, 99
23437, V, 1, 1, 1, 1, 0, 700, 99
23438, V, 1, 1, 1, 1, 0, 700, 99
23439, V, 1, 1, 1, 1, 0, 700, 99
23440, V, 1, 1, 1, 1, 0, 700, 99
23441, V, 1, 1, 1, 1, 0, 700, 99
23442, V, 1, 1, 1, 1, 0, 700, 99
23443, V, 1, 1, 1, 1, 0, 700, 99
23444, V, 1, 1, 1, 1, 0, 700, 99
23445, V, 1, 1, 1, 1, 0, 700, 99
23446, V, 1, 1, 1, 1, 0, 700, 99
23447, V, 1, 1, 1, 1, 0, 700, 99
23448, V, 1, 1, 1, 1, 0, 700, 99
23449, V, 1, 1, 1, 1, 0, 700, 99
23450, V, 1, 1, 1, 1, 0, 700, 99
23451, V, 1, 1, 1, 1, 0, 700, 99
23452, V, 1, 1, 1, 1, 0, 700, 99
23453, V, 1, 1, 1, 1, 0, 700, 99
23454, V, 1, 1, 1, 1, 0, 700, 99
23455, V, 1, 1, 1, 1, 0, 700, 99
23456, V, 1, 1, 1, 1, 0, 700, 99
23457, V, 1, 1, 1, 1, 0, 700, 99
23458, V, 1, 1, 1, 1, 0, 700, 99
23459, V, 1, 1, 1, 1, 0, 700, 99
23460, V, 1, 1, 1, 1, 0, 700, 99
23461, V, 1, 1, 1, 1, 0, 700, 99
23462, V, 1, 1, 1, 1, 0, 700, 99
23463, V, 1, 1, 1, 1, 0, 700, 99
23464, V, 1, 1, 1, 1, 0, 700, 99
23465, V, 1, 1, 1, 1, 0, 700, 99
23467, V, 1, 1, 1, 1, 0, 700, 99
23468, V, 1, 1, 1, 1, 0, 700, 99
23469, V, 1, 1, 1, 1, 0, 700, 99
23470, V, 1, 1, 1, 1, 0, 700, 99
23471, V, 1, 1, 1, 1, 0, 700, 99
23472, V, 1, 1, 1, 1, 0, 700, 99
23473, V, 1, 1, 1, 1, 0, 700, 99
23474, V, 1, 1, 1, 1, 0, 700, 99
23475, V, 1, 1, 1, 1, 0, 700, 99
23476, V, 1, 1, 1, 1, 0, 700, 99
23477, V, 1, 1, 1, 1, 0, 700, 99
23478, V, 1, 1, 1, 1, 0, 700, 99
23479, V, 1, 1, 1, 1, 0, 700, 99
23480, V, 1, 1, 1, 1, 0, 700, 99
23481, V, 1, 1, 1, 1, 0, 700, 99
23482, V, 1, 1, 1, 1, 0, 700, 99
23483, V, 1, 1, 1, 1, 0, 700, 99
23484, V, 1, 1, 1, 1, 0, 700, 99
23485, V, 1, 1, 1, 1, 0, 700, 99
23486, V, 1, 1, 1, 1, 0, 700, 99
23487, V, 1, 1, 1, 1, 0, 700, 99
23488, V, 1, 1, 1, 1, 0, 700, 99
23489, V, 1, 1, 1, 1, 0, 700, 99
23490, V, 1, 1, 1, 1, 0, 700, 99
23491, V, 1, 1, 1, 1, 0, 700, 99
23492, V, 1, 1, 1, 1, 0, 700, 99
23493, V, 1, 1, 1, 1, 0, 700, 99
23494, V, 1, 1, 1, 1, 0, 700, 99
23495, V, 1, 1, 1, 1, 0, 700, 99
23496, V, 1, 1, 1, 1, 0, 700, 99
23497, V, 1, 1, 1, 1, 0, 700, 99
23498, V, 1, 1, 1, 1, 0, 700, 99
23499, V, 1, 1, 1, 1, 0, 700, 99
23500, V, 1, 1, 1, 1, 0, 700, 99
23501, V, 1, 1, 1, 1, 0, 700, 99
23502, V, 1, 1, 1, 1, 0, 700, 99
23503, V, 1, 1, 1, 1, 0, 700, 99
23504, V, 1, 1, 1, 1, 0, 700, 99
23505, V, 1, 1, 1, 1, 0, 700, 99
23506, V, 1, 1, 1, 1, 0, 700, 99
23507, V, 1, 1, 1, 1, 0, 700, 99
23508, V, 1, 1, 1, 1, 0, 700, 99
23510, V, 1, 1, 1, 1, 0, 700, 99
23511, V, 1, 1, 1, 1, 0, 700, 99
23512, V, 1, 1, 1, 1, 0, 700, 99
23513, V, 1, 1, 1, 1, 0, 700, 99
23514, V, 1, 1, 1, 1, 0, 700, 99
23515, V, 1, 1, 1, 1, 0, 700, 99
23516, V, 1, 1, 1, 1, 0, 700, 99
23517, V, 1, 1, 1, 1, 0, 700, 99
23518, V, 1, 1, 1, 1, 0, 700, 99
23519, V, 1, 1, 1, 1, 0, 700, 99
23520, V, 1, 1, 1, 1, 0, 700, 99
23521, V, 1, 1, 1, 1, 0, 700, 99
23522, V, 1, 1, 1, 1, 0, 700, 99
23523, V, 1, 1, 1, 1, 0, 700, 99
23524, V, 1, 1, 1, 1, 0, 700, 99
23525, V, 1, 1, 1, 1, 0, 700, 99
23526, V, 1, 1, 1, 1, 0, 700, 99
23527, V, 1, 1, 1, 1, 0, 700, 99
23528, V, 1, 1, 1, 1, 0, 700, 99
23529, V, 1, 1, 1, 1, 0, 700, 99
23530, V, 1, 1, 1, 1, 0, 700, 99
23531, V, 1, 1, 1, 1, 0, 700, 99
23532, V, 1, 1, 1, 1, 0, 700, 99
23533, V, 1, 1, 1, 1, 0, 700, 99
23534, V, 1, 1, 1, 1, 0, 700, 99
23535, V, 1, 1, 1, 1, 0, 700, 99
23536, V, 1, 1, 1, 1, 0, 700, 99
23537, V, 1, 1, 1, 1, 0, 700, 99
23538, V, 1, 1, 1, 1, 0, 700, 99
23539, V, 1, 1, 1, 1, 0, 700, 99
23540, V, 1, 1, 1, 1, 0, 700, 99
23541, V, 1, 1, 1, 1, 0, 700, 99
23542, V, 1, 1, 1, 1, 0, 700, 99
23543, V, 1, 1, 1, 1, 0, 700, 99
23544, V, 1, 1, 1, 1, 0, 700, 99
23545, V, 1, 1, 1, 1, 0, 700, 99
23546, V, 1, 1, 1, 1, 0, 700, 99
23547, V, 1, 1, 1, 1, 0, 700, 99
23548, V, 1, 1, 1, 1, 0, 700, 99
23549, V, 1, 1, 1, 1, 0, 700, 99
23550, V, 1, 1, 1, 1, 0, 700, 99
23552, V, 1, 1, 1, 1, 0, 700, 99
23553, V, 1, 1, 1, 1, 0, 700, 99
23554, V, 1, 1, 1, 1, 0, 700, 99
23555, V, 1, 1, 1, 1, 0, 700, 99
23556, V, 1, 1, 1, 1, 0, 700, 99
23557, V, 1, 1, 1, 1, 0, 700, 99
23558, V, 1, 1, 1, 1, 0, 700, 99
23559, V, 1, 1, 1, 1, 0, 700, 99
23560, V, 1, 1, 1, 1, 0, 700, 99
23561, V, 1, 1, 1, 1, 0, 700, 99
23562, V, 1, 1, 1, 1, 0, 700, 99
23563, V, 1, 1, 1, 1, 0, 700, 99
23564, V, 1, 1, 1, 1, 0, 700, 99
23565, V, 1, 1, 1, 1, 0, 700, 99
23566, V, 1, 1, 1, 1, 0, 700, 99
23567, V, 1, 1, 1, 1, 0, 700, 99
23568, V, 1, 1, 1, 1, 0, 700, 99
23569, V, 1, 1, 1, 1, 0, 700, 99
23570, V, 1, 1, 1, 1, 0, 700, 99
23571, V, 1, 1, 1, 1, 0, 700, 99
23572, V, 1, 1, 1, 1, 0, 700, 99
23573, V, 1, 1, 1, 1, 0, 700, 99
23574, V, 1, 1, 1, 1, 0, 700, 99
23575, V, 1, 1, 1, 1, 0, 700, 99
23576, V, 1, 1, 1, 1, 0, 700, 99
23577, V, 1, 1, 1, 1, 0, 700, 99
23578, V, 1, 1, 1, 1, 0, 700, 99
23579, V, 1, 1, 1, 1, 0, 700, 99
23580, V, 1, 1, 1, 1, 0, 700, 99
23581, V, 1, 1, 1, 1, 0, 700, 99
23582, V, 1, 1, 1, 1, 0, 700, 99
23583, V, 1, 1, 1, 1, 0, 700, 99
23584, V, 1, 1, 1, 1, 0, 700, 99
23585, V, 1, 1, 1, 1, 0, 700, 99
23586, V, 1, 1, 1, 1, 0, 700, 99
23587, V, 1, 1, 1, 1, 0, 700, 99
23588, V, 1, 1, 1, 1, 0, 700, 99
23589, V, 1, 1, 1, 1, 0, 700, 99
23590, V, 1, 1, 1, 1, 0, 700, 99
23591, V, 1, 1, 1, 1, 0, 700, 99
23592, V, 1, 1, 1, 1, 0, 700, 99
23593, V, 1, 1, 1, 1, 0, 700, 99
23595, V, 1, 1, 1, 1, 0, 700, 99
23596, V, 1, 1, 1, 1, 0, 700, 99
23597, V, 1, 1, 1, 1, 0, 700, 99
23598, V, 1, 1, 1, 1, 0, 700, 99
23599, V, 1, 1, 1, 1, 0, 700, 99
23600, V, 1, 1, 1, 1, 0, 700, 99
23601, V, 1, 1, 1, 1, 0, 700, 99
23602, V, 1, 1, 1, 1, 0, 700, 99
23603, V, 1, 1, 1, 1, 0, 700, 99
23604, V, 1, 1, 1, 1, 0, 700, 99
23605, V, 1, 1, 1, 1, 0, 700, 99
23606, V, 1, 1, 1, 1, 0, 700, 99
23607, V, 1, 1, 1, 1, 0, 700, 99
23608, V, 1, 1, 1, 1, 0, 700, 99
23609, V, 1, 1, 1, 1, 0, 700, 99
23610, V, 1, 1, 1, 1, 0, 700, 99
23611, V, 1, 1, 1, 1, 0, 700, 99
23612, V, 1, 1, 1, 1, 0, 700, 99
23613, V, 1, 1, 1, 1, 0, 700, 99
23614, V, 1, 1, 1, 1, 0, 700, 99
23615, V, 1, 1, 1, 1, 0, 700, 99
23616, V, 1, 1, 1, 1, 0, 700, 99
23617, V, 1, 1, 1, 1, 0, 700, 99
23618, V, 1, 1, 1, 1, 0, 700, 99
23619, V, 1, 1, 1, 1, 0, 700, 99
23620, V, 1, 1, 1, 1, 0, 700, 99
23621, V, 1, 1, 1, 1, 0, 700, 99
23622, V, 1, 1, 1, 1, 0, 700, 99
23623, V, 1, 1, 1, 1, 0, 700, 99
23624, V, 1, 1, 1, 1, 0, 700, 99
23625, V, 1, 1, 1, 1, 0, 700, 99
23626, V, 1, 1, 1, 1, 0, 700, 99
23627, V, 1, 1, 1, 1, 0, 700, 99
23628, V, 1, 1, 1, 1, 0, 700, 99
23629, V, 1, 1, 1, 1, 0, 700, 99
23630, V, 1, 1, 1, 1, 0, 700, 99
23631, V, 1, 1, 1, 1, 0, 700, 99
23632, V, 1, 1, 1, 1, 0, 700, 99
23633, V, 1, 1, 1, 1, 0, 700, 99
23634, V, 1, 1, 1, 1, 0, 700, 99
23635, V, 1, 1, 1, 1, 0, 700, 99
23636, V, 1, 1, 1, 1, 0, 700, 99
23638, V, 1, 1, 1, 1, 0, 700, 99
23639, V, 1, 1, 1, 1, 0, 700, 99
23640, V, 1, 1, 1, 1, 0, 700, 99
23641, V, 1, 1, 1, 1, 0, 700, 99
23642, V, 1, 1, 1, 1, 0, 700, 99
23643, V, 1, 1, 1, 1, 0, 700, 99
23644, V, 1, 1, 1, 1, 0, 700, 99
23645, V, 1, 1, 1, 1, 0, 700, 99
23646, V, 1, 1, 1, 1, 0, 700, 99
23647, V, 1, 1, 1, 1, 0, 700, 99
23648, V, 1, 1, 1, 1, 0, 700, 99
23649, V, 1, 1, 1, 1, 0, 700, 99
23650, V, 1, 1, 1, 1, 0, 700, 99
23651, V, 1, 1, 1, 1, 0, 700, 99
23652, V, 1, 1, 1, 1, 0, 700, 99
23653, V, 1, 1, 1, 1, 0, 700, 99
23654, V, 1, 1, 1, 1, 0, 700, 99
23655, V, 1, 1, 1, 1, 0, 700, 99
23656, V, 1, 1, 1, 1, 0, 700, 99
23657, V, 1, 1, 1, 1, 0, 700, 99
23658, V, 1, 1, 1, 1, 0, 700, 99
23659, V, 1, 1, 1, 1, 0, 700, 99
23660, V, 1, 1, 1, 1, 0, 700, 99
23661, V, 1, 1, 1, 1, 0, 700, 99
23662, V, 1, 1, 1, 1, 0, 700, 99
23663, V, 1, 1, 1, 1, 0, 700, 99
23664, V, 1, 1, 1, 1, 0, 700, 99
23665, V, 1, 1, 1, 1, 0, 700, 99
23666, V, 1, 1, 1, 1, 0, 700, 99
23667, V, 1, 1, 1, 1, 0, 700, 99
23668, V, 1, 1, 1, 1, 0, 700, 99
23669, V, 1, 1, 1, 1, 0, 700, 99
23670, V, 1, 1, 1, 1, 0, 700, 99
23671, V, 1, 1, 1, 1, 0, 700, 99
23672, V, 1, 1, 1, 1, 0, 700, 99
23673, V, 1, 1, 1, 1, 0, 700, 99
23674, V, 1, 1, 1, 1, 0, 700, 99
23675, V, 1, 1, 1, 1, 0, 700, 99
23676, V, 1, 1, 1, 1, 0, 700, 99
23677, V, 1, 1, 1, 1, 0, 700, 99
23678, V, 1, 1, 1, 1, 0, 700, 99
23680, V, 1, 1, 1, 1, 0, 700, 99
23681, V, 1, 1, 1, 1, 0, 700, 99
23682, V, 1, 1, 1, 1, 0, 700, 99
23683, V, 1, 1, 1, 1, 0, 700, 99
23684, V, 1, 1, 1, 1, 0, 700, 99
23685, V, 1, 1, 1, 1, 0, 700, 99
23686, V, 1, 1, 1, 1, 0, 700, 99
23687, V, 1, 1, 1, 1, 0, 700, 99
23688, V, 1, 1, 1, 1, 0, 700, 99
23689, V, 1, 1, 1, 1, 0, 700, 99
23690, V, 1, 1, 1, 1, 0, 700, 99
23691, V, 1, 1, 1, 1, 0, 700, 99
23692, V, 1, 1, 1, 1, 0, 700, 99
23693, V, 1, 1, 1, 1, 0, 700, 99
23694, V, 1, 1, 1, 1, 0, 700, 99
23695, V, 1, 1, 1, 1, 0, 700, 99
23696, V, 1, 1, 1, 1, 0, 700, 99
23697, V, 1, 1, 1, 1, 0, 700, 99
23698, V, 1, 1, 1, 1, 0, 700, 99
23699, V, 1, 1, 1, 1, 0, 700, 99
23700, V, 1, 1, 1, 1, 0, 700, 99
23701, V, 1, 1, 1, 1, 0, 700, 99
23702, V, 1, 1, 1, 1, 0, 700, 99
23703, V, 1, 1, 1, 1, 0, 700, 99
23704, V, 1, 1, 1, 1, 0, 700, 99
23705, V, 1, 1, 1, 1, 0, 700, 99
23706, V, 1, 1, 1, 1, 0, 700, 99
23707, V, 1, 1, 1, 1, 0, 700, 99
23708, V, 1, 1, 1, 1, 0, 700, 99
23709, V, 1, 1, 1, 1, 0, 700, 99
23710, V, 1, 1, 1, 1, 0, 700, 99
23711, V, 1, 1, 1, 1, 0, 700, 99
23712, V, 1, 1, 1, 1, 0, 700, 99
23713, V, 1, 1, 1, 1, 0, 700, 99
23714, V, 1, 1, 1, 1, 0, 700, 99
23715, V, 1, 1, 1, 1, 0, 700, 99
23716, V, 1, 1, 1, 1, 0, 700, 99
23717, V, 1, 1, 1, 1, 0, 700, 99
23718, V, 1, 1, 1, 1, 0, 700, 99
23719, V, 1, 1, 1, 1, 0, 700, 99
23720, V, 1, 1, 1, 1, 0, 700, 99
23721, V, 1, 1, 1, 1, 0, 700, 99
23723, V, 1, 1, 1, 1, 0, 700, 99
23724, V, 1, 1, 1, 1, 0, 700, 99
23725, V, 1, 1, 1, 1, 0, 700, 99
23726, V, 1, 1, 1, 1, 0, 700, 99
23727, V, 1, 1, 1, 1, 0, 700, 99
23728, V, 1, 1, 1, 1, 0, 700, 99
23729, V, 1, 1, 1, 1, 0, 700, 99
23730, V, 1, 1, 1, 1, 0, 700, 99
23731, V, 1, 1, 1, 1, 0, 700, 99
23732, V, 1, 1, 1, 1, 0, 700, 99
23733, V, 1, 1, 1, 1, 0, 700, 99
23734, V, 1, 1, 1, 1, 0, 700, 99
23735, V, 1, 1, 1, 1, 0, 700, 99
23736, V, 1, 1, 1, 1, 0, 700, 99
23737, V, 1, 1, 1, 1, 0, 700, 99
23738, V, 1, 1, 1, 1, 0, 700, 99
23739, V, 1, 1, 1, 1, 0, 700, 99
23740, V, 1, 1, 1, 1, 0, 700, 99
23741, V, 1, 1, 1, 1, 0, 700, 99
23742, V, 1, 1, 1, 1, 0, 700, 99
23743, V, 1, 1, 1, 1, 0, 700, 99
23744, V, 1, 1, 1, 1, 0, 700, 99
23745, V, 1, 1, 1, 1, 0, 700, 99
23746, V, 1, 1, 1, 1, 0, 700, 99
23747, V, 1, 1, 1, 1, 0, 700, 99
23748, V, 1, 1, 1, 1, 0, 700, 99
23749, V, 1, 1, 1, 1, 0, 700, 99
23750, V, 1, 1, 1, 1, 0, 700, 99
23751, V, 1, 1, 1, 1, 0, 700, 99
23752, V, 1, 1, 1, 1, 0, 700, 99
23753, V, 1, 1, 1, 1, 0, 700, 99
23754, V, 1, 1, 1, 1, 0, 700, 99
23755, V, 1, 1, 1, 1, 0, 700, 99
23756, V, 1, 1, 1, 1, 0, 700, 99
23757, V, 1, 1, 1, 1, 0, 700, 99
23758, V, 1, 1, 1, 1, 0, 700, 99
23759, V, 1, 1, 1, 1, 0, 700, 99
23760, V, 1, 1, 1, 1, 0, 700, 99
23761, V, 1, 1, 1, 1, 0, 700, 99
23762, V, 1, 1, 1, 1, 0, 700, 99
23763, V, 1, 1, 1, 1, 0, 700, 99
23764, V, 1, 1, 1, 1, 0, 700, 99
23766, V, 1, 1, 1, 1, 0, 700, 99
23767, V, 1, 1, 1, 1, 0, 700, 99
23768, V, 1, 1, 1, 1, 0, 700, 99
23769, V, 1, 1, 1, 1, 0, 700, 99
23770, V, 1, 1, 1, 1, 0, 700, 99
23771, V, 1, 1, 1, 1, 0, 700, 99
23772, V, 1, 1, 1, 1, 0, 700, 99
23773, V, 1, 1, 1, 1, 0, 700, 99
23774, V, 1, 1, 1, 1, 0, 700, 99
23775, V, 1, 1, 1, 1, 0, 700, 99
23776, V, 1, 1, 1, 1, 0, 700, 99
23777, V, 1, 1, 1, 1, 0, 700, 99
23778, V, 1, 1, 1, 1, 0, 700, 99
23779, V, 1, 1, 1, 1, 0, 700, 99
23780, V, 1, 1, 1, 1, 0, 700, 99
23781, V, 1, 1, 1, 1, 0, 700, 99
23782, V, 1, 1, 1, 1, 0, 700, 99
23783, V, 1, 1, 1, 1, 0, 700, 99
23784, V, 1, 1, 1, 1, 0, 700, 99
23785, V, 1, 1, 1, 1, 0, 700, 99
23786, V, 1, 1, 1, 1, 0, 700, 99
23787, V, 1, 1, 1, 1, 0, 700, 99
23788, V, 1, 1, 1, 1, 0, 700, 99
23789, V, 1, 1, 1, 1, 0, 700, 99
23790, V, 1, 1, 1, 1, 0, 700, 99
23791, V, 1, 1, 1, 1, 0, 700, 99
23792, V, 1, 1, 1, 1, 0, 700, 99
23793, V, 1, 1, 1, 1, 0, 700, 99
23794, V, 1, 1, 1, 1, 0, 700, 99
23795, V, 1, 1, 1, 1, 0, 700, 99
23796, V, 1, 1, 1, 1, 0, 700, 99
23797, V, 1, 1, 1, 1, 0, 700, 99
23798, V, 1, 1, 1, 1, 0, 700, 99
23799, V, 1, 1, 1, 1, 0, 700, 99
23800, V, 1, 1, 1, 1, 0, 700, 99
23801, V, 1, 1, 1, 1, 0, 700, 99
23802, V, 1, 1, 1, 1, 0, 700, 99
23803, V, 1, 1, 1, 1, 0, 700, 99
23804, V, 1, 1, 1, 1, 0, 700, 99
23805, V, 1, 1, 1, 1, 0, 700, 99
23806, V, 1, 1, 1, 1, 0, 700, 99
23808, V, 1, 1, 1, 1, 0, 700, 99
23809, V, 1, 1, 1, 1, 0, 700, 99
23810, V, 1, 1, 1, 1, 0, 700, 99
23811, V, 1, 1, 1, 1, 0, 700, 99
23812, V, 1, 1, 1, 1, 0, 700, 99
23813, V, 1, 1, 1, 1, 0, 700, 99
23814, V, 1, 1, 1, 1, 0, 700, 99
23815, V, 1, 1, 1, 1, 0, 700, 99
23816, V, 1, 1, 1, 1, 0, 700, 99
23817, V, 1, 1, 1, 1, 0, 700, 99
23818, V, 1, 1, 1, 1, 0, 700, 99
23819, V, 1, 1, 1, 1, 0, 700, 99
23820, V, 1, 1, 1, 1, 0, 700, 99
23821, V, 1, 1, 1, 1, 0, 700, 99
23822, V, 1, 1, 1, 1, 0, 700, 99
23823, V, 1, 1, 1, 1, 0, 700, 99
23824, V, 1, 1, 1, 1, 0, 700, 99
23825, V, 1, 1, 1, 1, 0, 700, 99
23826, V, 1, 1, 1, 1, 0, 700, 99
23827, V, 1, 1, 1, 1, 0, 700, 99
23828, V, 1, 1, 1, 1, 0, 700, 99
23829, V, 1, 1, 1, 1, 0, 700, 99
23830, V, 1, 1, 1, 1, 0, 700, 99
23831, V, 1, 1, 1, 1, 0, 700, 99
23832, V, 1, 1, 1, 1, 0, 700, 99
23833, V, 1, 1, 1, 1, 0, 700, 99
23834, V, 1, 1, 1, 1, 0, 700, 99
23835, V, 1, 1, 1, 1, 0, 700, 99
23836, V, 1, 1, 1, 1, 0, 700, 99
23837, V, 1, 1, 1, 1, 0, 700, 99
23838, V, 1, 1, 1, 1, 0, 700, 99
23839, V, 1, 1, 1, 1, 0, 700, 99
23840, V, 1, 1, 1, 1, 0, 700, 99
23841, V, 1, 1, 1, 1, 0, 700, 99
23842, V, 1, 1, 1, 1, 0, 700, 99
23843, V, 1, 1, 1, 1, 0, 700, 99
23844, V, 1, 1, 1, 1, 0, 700, 99
23845, V, 1, 1, 1, 1, 0, 700, 99
23846, V, 1, 1, 1, 1, 0, 700, 99
23847, V, 1, 1, 1, 1, 0, 700, 99
23848, V, 1, 1, 1, 1, 0, 700, 99
23849, V, 1, 1, 1, 1, 0, 700, 99
23851, V, 1, 1, 1, 1, 0, 700, 99
23852, V, 1, 1, 1, 1, 0, 700, 99
23853, V, 1, 1, 1, 1, 0, 700, 99
23854, V, 1, 1, 1, 1, 0, 700, 99
23855, V, 1, 1, 1, 1, 0, 700, 99
23856, V, 1, 1, 1, 1, 0, 700, 99
23857, V, 1, 1, 1, 1, 0, 700, 99
23858, V, 1, 1, 1, 1, 0, 700, 99
23859, V, 1, 1, 1, 1, 0, 700, 99
23860, V, 1, 1, 1, 1, 0, 700, 99
23861, V, 1, 1, 1, 1, 0, 700, 99
23862, V, 1, 1, 1, 1, 0, 700, 99
23863, V, 1, 1, 1, 1, 0, 700, 99
23864, V, 1, 1, 1, 1, 0, 700, 99
23865, V, 1, 1, 1, 1, 0, 700, 99
23866, V, 1, 1, 1, 1, 0, 700, 99
23867, V, 1, 1, 1, 1, 0, 700, 99
23868, V, 1, 1, 1, 1, 0, 700, 99
23869, V, 1, 1, 1, 1, 0, 700, 99
23870, V, 1, 1, 1, 1, 0, 700, 99
23871, V, 1, 1, 1, 1, 0, 700, 99
23872, V, 1, 1, 1, 1, 0, 700, 99
23873, V, 1, 1, 1, 1, 0, 700, 99
23874, V, 1, 1, 1, 1, 0, 700, 99
23875, V, 1, 1, 1, 1, 0, 700, 99
23876, V, 1, 1, 1, 1, 0, 700, 99
23877, V, 1, 1, 1, 1, 0, 700, 99
23878, V, 1, 1, 1, 1, 0, 700, 99
23879, V, 1, 1, 1, 1, 0, 700, 99
23880, V, 1, 1, 1, 1, 0, 700, 99
23881, V, 1, 1, 1, 1, 0, 700, 99
23882, V, 1, 1, 1, 1, 0, 700, 99
23883, V, 1, 1, 1, 1, 0, 700, 99
23884, V, 1, 1, 1, 1, 0, 700, 99
23885, V, 1, 1, 1, 1, 0, 700, 99
23886, V, 1, 1, 1, 1, 0, 700, 99
23887, V, 1, 1, 1, 1, 0, 700, 99
23888, V, 1, 1, 1, 1, 0, 700, 99
23889, V, 1, 1, 1, 1, 0, 700, 99
23890, V, 1, 1, 1, 1, 0, 700, 99
23891, V, 1, 1, 1, 1, 0, 700, 99
23892, V, 1, 1, 1, 1, 0, 700, 99
23894, V, 1, 1, 1, 1, 0, 700, 99
23895, V, 1, 1, 1, 1, 0, 700, 99
23896, V, 1, 1, 1, 1, 0, 700, 99
23897, V, 1, 1, 1, 1, 0, 700, 99
23898, V, 1, 1, 1, 1, 0, 700, 99
23899, V, 1, 1, 1, 1, 0, 700, 99
23900, V, 1, 1, 1, 1, 0, 700, 99
23901, V, 1, 1, 1, 1, 0, 700, 99
23902, V, 1, 1, 1, 1, 0, 700, 99
23903, V, 1, 1, 1, 1, 0, 700, 99
23904, V, 1, 1, 1, 1, 0, 700, 99
23905, V, 1, 1, 1, 1, 0, 700, 99
23906, V, 1, 1, 1, 1, 0, 700, 99
23907, V, 1, 1, 1, 1, 0, 700, 99
23908, V, 1, 1, 1, 1, 0, 700, 99
23909, V, 1, 1, 1, 1, 0, 700, 99
23910, V, 1, 1, 1, 1, 0, 700, 99
23911, V, 1, 1, 1, 1, 0, 700, 99
23912, V, 1, 1, 1, 1, 0, 700, 99
23913, V, 1, 1, 1, 1, 0, 700, 99
23914, V, 1, 1, 1, 1, 0, 700, 99
23915, V, 1, 1, 1, 1, 0, 700, 99
23916, V, 1, 1, 1, 1, 0, 700, 99
23917, V, 1, 1, 1, 1, 0, 700, 99
23918, V, 1, 1, 1, 1, 0, 700, 99
23919, V, 1, 1, 1, 1, 0, 700, 99
23920, V, 1, 1, 1, 1, 0, 700, 99
23921, V, 1, 1, 1, 1, 0, 700, 99
23922, V, 1, 1, 1, 1, 0, 700, 99
23923, V, 1, 1, 1, 1, 0, 700, 99
23924, V, 1, 1, 1, 1, 0, 700, 99
23925, V, 1, 1, 1, 1, 0, 700, 99
23926, V, 1, 1, 1, 1, 0, 700, 99
23927, V, 1, 1, 1, 1, 0, 700, 99
23928, V, 1, 1, 1, 1, 0, 700, 99
23929, V, 1, 1, 1, 1, 0, 700, 99
23930, V, 1, 1, 1, 1, 0, 700, 99
23931, V, 1, 1, 1, 1, 0, 700, 99
23932, V, 1, 1, 1, 1, 0, 700, 99
23933, V, 1, 1, 1, 1, 0, 700, 99
23934, V, 1, 1, 1, 1, 0, 700, 99
23936, V, 1, 1, 1, 1, 0, 700, 99
23937, V, 1, 1, 1, 1, 0, 700, 99
23938, V, 1, 1, 1, 1, 0, 700, 99
23939, V, 1, 1, 1, 1, 0, 700, 99
23940, V, 1, 1, 1, 1, 0, 700, 99
23941, V, 1, 1, 1, 1, 0, 700, 99
23942, V, 1, 1, 1, 1, 0, 700, 99
23943, V, 1, 1, 1, 1, 0, 700, 99
23944, V, 1, 1, 1, 1, 0, 700, 99
23945, V, 1, 1, 1, 1, 0, 700, 99
23946, V, 1, 1, 1, 1, 0, 700, 99
23947, V, 1, 1, 1, 1, 0, 700, 99
23948, V, 1, 1, 1, 1, 0, 700, 99
23949, V, 1, 1, 1, 1, 0, 700, 99
23950, V, 1, 1, 1, 1, 0, 700, 99
23951, V, 1, 1, 1, 1, 0, 700, 99
23952, V, 1, 1, 1, 1, 0, 700, 99
23953, V, 1, 1, 1, 1, 0, 700, 99
23954, V, 1, 1, 1, 1, 0, 700, 99
23955, V, 1, 1, 1, 1, 0, 700, 99
23956, V, 1, 1, 1, 1, 0, 700, 99
23957, V, 1, 1, 1, 1, 0, 700, 99
23958, V, 1, 1, 1, 1, 0, 700, 99
23959, V, 1, 1, 1, 1, 0, 700, 98
23960, V, 1, 1, 1, 1, 0, 700, 99
23961, V, 1, 1, 1, 1, 0, 700, 99
23962, V, 1, 1, 1, 1, 0, 700, 99
23963, V, 1, 1, 1, 1, 0, 700, 99
23964, V, 1, 1, 1, 1, 0, 700, 98
23965, V, 1, 1, 1, 1, 0, 700, 99
23966, V, 1, 1, 1, 1, 0, 700, 98
23967, V, 1, 1, 1, 1, 0, 700, 98
23968, V, 1, 1, 1, 1, 0, 700, 99
23969, V, 1, 1, 1, 1, 0, 700, 98
23970, V, 1, 1, 1, 1, 0, 700, 98
23971, V, 1, 1, 1, 1, 0, 700, 99
23972, V, 1, 1, 1, 1, 0, 700, 99
23973, V, 1, 1, 1, 1, 0, 700, 98
23974, V, 1, 1, 1, 1, 0, 700, 98
23975, V, 1, 1, 1, 1, 0, 700, 98
23976, V, 1, 1, 1, 1, 0, 700, 98
23977, V, 1, 1, 1, 1, 0, 700, 98
23979, V, 1, 1, 1, 1, 0, 700, 99
23980, V, 1, 1, 1, 1, 0, 700, 98
23981, V, 1, 1, 1, 1, 0, 700, 99
23982, V, 1, 1, 1, 1, 0, 700, 98
23983, V, 1, 1, 1, 1, 0, 700, 98
23984, V, 1, 1, 1, 1, 0, 700, 99
23985, V, 1, 1, 1, 1, 0, 700, 99
23986, V, 1, 1, 1, 1, 0, 700, 99
23987, V, 1, 1, 1, 1, 0, 700, 99
23988, V, 1, 1, 1, 1, 0, 700, 99
23989, V, 1, 1, 1, 1, 0, 700, 99
23990, V, 1, 1, 1, 1, 0, 700, 98
23991, V, 1, 1, 1, 1, 0, 700, 99
23992, V, 1, 1, 1, 1, 0, 700, 99
23993, V, 1, 1, 1, 1, 0, 700, 99
23994, V, 1, 1, 1, 1, 0, 700, 99
23995, V, 1, 1, 1, 1, 0, 700, 99
23996, V, 1, 1, 1, 1, 0, 700, 99
23997, V, 1, 1, 1, 1, 0, 700, 99
23998, V, 1, 1, 1, 1, 0, 700, 98
23999, V, 1, 1, 1, 1, 0, 700, 99
24000, V, 1, 1, 1, 1, 0, 700, 99
24001, V, 1, 1, 1, 1, 0, 700, 99
24002, V, 1, 1, 1, 1, 0, 700, 99
24003, V, 1, 1, 1, 1, 0, 700, 99
24004, V, 1, 1, 1, 1, 0, 700, 99
24005, V, 1, 1, 1, 1, 0, 700, 98
24006, V, 1, 1, 1, 1, 0, 700, 98
24007, V, 1, 1, 1, 1, 0, 700, 98
24008, V, 1, 1, 1, 1, 0, 700, 98
24009, V, 1, 1, 1, 1, 0, 700, 98
24010, V, 1, 1, 1, 1, 0, 700, 98
24011, V, 1, 1, 1, 1, 0, 700, 98
24012, V, 1, 1, 1, 1, 0, 700, 98
24013, V, 1, 1, 1, 1, 0, 700, 98
24014, V, 1, 1, 1, 1, 0, 700, 98
24015, V, 1, 1, 1, 1, 0, 700, 98
24016, V, 1, 1, 1, 1, 0, 700, 98
24017, V, 1, 1, 1, 1, 0, 700, 98
24018, V, 1, 1, 1, 1, 0, 700, 98
24019, V, 1, 1, 1, 1, 0, 700, 98
24020, V, 1, 1, 1, 1, 0, 700, 98
24022, V, 1, 1, 1, 1, 0, 700, 98
24023, V, 1, 1, 1, 1, 0, 700, 98
24024, V, 1, 1, 1, 1, 0, 700, 98
24025, V, 1, 1, 1, 1, 0, 700, 98
24026, V, 1, 1, 1, 1, 0, 700, 98
24027, V, 1, 1, 1, 1, 0, 700, 98
24028, V, 1, 1, 1, 1, 0, 700, 98
24029, V, 1, 1, 1, 1, 0, 700, 98
24030, V, 1, 1, 1, 1, 0, 700, 98
24031, V, 1, 1, 1, 1, 0, 700, 98
24032, V, 1, 1, 1, 1, 0, 700, 98
24033, V, 1, 1, 1, 1, 0, 700, 98
24034, V, 1, 1, 1, 1, 0, 700, 98
24035, V, 1, 1, 1, 1, 0, 700, 98
24036, V, 1, 1, 1, 1, 0, 700, 98
24037, V, 1, 1, 1, 1, 0, 700, 98
24038, V, 1, 1, 1, 1, 0, 700, 98
24039, V, 1, 1, 1, 1, 0, 700, 98
24040, V, 1, 1, 1, 1, 0, 700, 98
24041, V, 1, 1, 1, 1, 0, 700, 98
24042, V, 1, 1, 1, 1, 0, 700, 98
24043, V, 1, 1, 1, 1, 0, 700, 98
24044, V, 1, 1, 1, 1, 0, 700, 98
24045, V, 1, 1, 1, 1, 0, 700, 98
24046, V, 1, 1, 1, 1, 0, 700, 98
24047, V, 1, 1, 1, 1, 0, 700, 98
24048, V, 1, 1, 1, 1, 0, 700, 98
24049, V, 1, 1, 1, 1, 0, 700, 99
24050, V, 1, 1, 1, 1, 0, 700, 99
24051, V, 1, 1, 1, 1, 0, 700, 98
24052, V, 1, 1, 1, 1, 0, 700, 99
24053, V, 1, 1, 1, 1, 0, 700, 98
24054, V, 1, 1, 1, 1, 0, 700, 99
24055, V, 1, 1, 1, 1, 0, 700, 99
24056, V, 1, 1, 1, 1, 0, 700, 99
24057, V, 1, 1, 1, 1, 0, 700, 99
24058, V, 1, 1, 1, 1, 0, 700, 99
24059, V, 1, 1, 1, 1, 0, 700, 99
24060, V, 1, 1, 1, 1, 0, 700, 99
24061, V, 1, 1, 1, 1, 0, 700, 99
24062, V, 1, 1, 1, 1, 0, 700, 99
24064, V, 1, 1, 1, 1, 0, 700, 99
24065, V, 1, 1, 1, 1, 0, 700, 99
24066, V, 1, 1, 1, 1, 0, 700, 99
24067, V, 1, 1, 1, 1, 0, 700, 99
24068, V, 1, 1, 1, 1, 0, 700, 99
24069, V, 1, 1, 1, 1, 0, 700, 99
24070, V, 1, 1, 1, 1, 0, 700, 99
24071, V, 1, 1, 1, 1, 0, 700, 99
24072, V, 1, 1, 1, 1, 0, 700, 99
24073, V, 1, 1, 1, 1, 0, 700, 99
24074, V, 1, 1, 1, 1, 0, 700, 99
24075, V, 1, 1, 1, 1, 0, 700, 99
24076, V, 1, 1, 1, 1, 0, 700, 99
24077, V, 1, 1, 1, 1, 0, 700, 99
24078, V, 1, 1, 1, 1, 0, 700, 99
24079, V, 1, 1, 1, 1, 0, 700, 99
24080, V, 1, 1, 1, 1, 0, 700, 99
24081, V, 1, 1, 1, 1, 0, 700, 99
24082, V, 1, 1, 1, 1, 0, 700, 99
24083, V, 1, 1, 1, 1, 0, 700, 99
24084, V, 1, 1, 1, 1, 0, 700, 99
24085, V, 1, 1, 1, 1, 0, 700, 99
24086, V, 1, 1, 1, 1, 0, 700, 99
24087, V, 1, 1, 1, 1, 0, 700, 99
24088, V, 1, 1, 1, 1, 0, 700, 99
24089, V, 1, 1, 1, 1, 0, 700, 99
24090, V, 1, 1, 1, 1, 0, 700, 99
24091, V, 1, 1, 1, 1, 0, 700, 99
24092, V, 1, 1, 1, 1, 0, 700, 99
24093, V, 1, 1, 1, 1, 0, 700, 99
24094, V, 1, 1, 1, 1, 0, 700, 99
24095, V, 1, 1, 1, 1, 0, 700, 99
24096, V, 1, 1, 1, 1, 0, 700, 99
24097, V, 1, 1, 1, 1, 0, 700, 99
24098, V, 1, 1, 1, 1, 0, 700, 99
24099, V, 1, 1, 1, 1, 0, 700, 99
24100, V, 1, 1, 1, 1, 0, 700, 99
24101, V, 1, 1, 1, 1, 0, 700, 99
24102, V, 1, 1, 1, 1, 0, 700, 99
24103, V, 1, 1, 1, 1, 0, 700, 99
24104, V, 1, 1, 1, 1, 0, 700, 99
24105, V, 1, 1, 1, 1, 0, 700, 99
24107, V, 1, 1, 1, 1, 0, 700, 99
24108, V, 1, 1, 1, 1, 0, 700, 99
24109, V, 1, 1, 1, 1, 0, 700, 99
24110, V, 1, 1, 1, 1, 0, 700, 99
24111, V, 1, 1, 1, 1, 0, 700, 99
24112, V, 1, 1, 1, 1, 0, 700, 99
24113, V, 1, 1, 1, 1, 0, 700, 99
24114, V, 1, 1, 1, 1, 0, 700, 99
24115, V, 1, 1, 1, 1, 0, 700, 99
24116, V, 1, 1, 1, 1, 0, 700, 99
24117, V, 1, 1, 1, 1, 0, 700, 99
24118, V, 1, 1, 1, 1, 0, 700, 99
24119, V, 1, 1, 1, 1, 0, 700, 99
24120, V, 1, 1, 1, 1, 0, 700, 99
24121, V, 1, 1, 1, 1, 0, 700, 99
24122, V, 1, 1, 1, 1, 0, 700, 99
24123, V, 1, 1, 1, 1, 0, 700, 99
24124, V, 1, 1, 1, 1, 0, 700, 99
24125, V, 1, 1, 1, 1, 0, 700, 99
24126, V, 1, 1, 1, 1, 0, 700, 99
24127, V, 1, 1, 1, 1, 0, 700, 99
24128, V, 1, 1, 1, 1, 0, 700, 99
24129, V, 1, 1, 1, 1, 0, 700, 99
24130, V, 1, 1, 1, 1, 0, 700, 99
24131, V, 1, 1, 1, 1, 0, 700, 99
24132, V, 1, 1, 1, 1, 0, 700, 99
24133, V, 1, 1, 1, 1, 0, 700, 99
24134, V, 1, 1, 1, 1, 0, 700, 99
24135, V, 1, 1, 1, 1, 0, 700, 99
24136, V, 1, 1, 1, 1, 0, 700, 99
24137, V, 1, 1, 1, 1, 0, 700, 99
24138, V, 1, 1, 1, 1, 0, 700, 99
24139, V, 1, 1, 1, 1, 0, 700, 99
24140, V, 1, 1, 1, 1, 0, 700, 99
24141, V, 1, 1, 1, 1, 0, 700, 99
24142, V, 1, 1, 1, 1, 0, 700, 99
24143, V, 1, 1, 1, 1, 0, 700, 99
24144, V, 1, 1, 1, 1, 0, 700, 99
24145, V, 1, 1, 1, 1, 0, 700, 99
24146, V, 1, 1, 1, 1, 0, 700, 99
24147, V, 1, 1, 1, 1, 0, 700, 99
24148, V, 1, 1, 1, 1, 0, 700, 99
24150, V, 1, 1, 1, 1, 0, 700, 99
24151, V, 1, 1, 1, 1, 0, 700, 99
24152, V, 1, 1, 1, 1, 0, 700, 99
24153, V, 1, 1, 1, 1, 0, 700, 99
24154, V, 1, 1, 1, 1, 0, 700, 99
24155, V, 1, 1, 1, 1, 0, 700, 99
24156, V, 1, 1, 1, 1, 0, 700, 99
24157, V, 1, 1, 1, 1, 0, 700, 99
24158, V, 1, 1, 1, 1, 0, 700, 99
24159, V, 1, 1, 1, 1, 0, 700, 99
24160, V, 1, 1, 1, 1, 0, 700, 99
24161, V, 1, 1, 1, 1, 0, 700, 99
24162, V, 1, 1, 1, 1, 0, 700, 99
24163, V, 1, 1, 1, 1, 0, 700, 99
24164, V, 1, 1, 1, 1, 0, 700, 99
24165, V, 1, 1, 1, 1, 0, 700, 99
24166, V, 1, 1, 1, 1, 0, 700, 99
24167, V, 1, 1, 1, 1, 0, 700, 99
24168, V, 1, 1, 1, 1, 0, 700, 99
24169, V, 1, 1, 1, 1, 0, 700, 99
24170, V, 1, 1, 1, 1, 0, 700, 99
24171, V, 1, 1, 1, 1, 0, 700, 99
24172, V, 1, 1, 1, 1, 0, 700, 98
24173, V, 1, 1, 1, 1, 0, 700, 98
24174, V, 1, 1, 1, 1, 0, 700, 99
24175, V, 1, 1, 1, 1, 0, 700, 98
24176, V, 1, 1, 1, 1, 0, 700, 99
24177, V, 1, 1, 1, 1, 0, 700, 98
24178, V, 1, 1, 1, 1, 0, 700, 98
24179, V, 1, 1, 1, 1, 0, 700, 98
24180, V, 1, 1, 1, 1, 0, 700, 98
24181, V, 1, 1, 1, 1, 0, 700, 98
24182, V, 1, 1, 1, 1, 0, 700, 98
24183, V, 1, 1, 1, 1, 0, 700, 98
24184, V, 1, 1, 1, 1, 0, 700, 98
24185, V, 1, 1, 1, 1, 0, 700, 98
24186, V, 1, 1, 1, 1, 0, 700, 98
24187, V, 1, 1, 1, 1, 0, 700, 98
24188, V, 1, 1, 1, 1, 0, 700, 98
24189, V, 1, 1, 1, 1, 0, 700, 98
24190, V, 1, 1, 1, 1, 0, 700, 98
24192, V, 1, 1, 1, 1, 0, 700, 98
24193, V, 1, 1, 1, 1, 0, 700, 98
24194, V, 1, 1, 1, 1, 0, 700, 98
24195, V, 1, 1, 1, 1, 0, 700, 98
24196, V, 1, 1, 1, 1, 0, 700, 98
24197, V, 1, 1, 1, 1, 0, 700, 98
24198, V, 1, 1, 1, 1, 0, 700, 98
24199, V, 1, 1, 1, 1, 0, 700, 98
24200, V, 1, 1, 1, 1, 0, 700, 98
24201, V, 1, 1, 1, 1, 0, 700, 98
24202, V, 1, 1, 1, 1, 0, 700, 98
24203, V, 1, 1, 1, 1, 0, 700, 98
24204, V, 1, 1, 1, 1, 0, 700, 98
24205, V, 1, 1, 1, 1, 0, 700, 98
24206, V, 1, 1, 1, 1, 0, 700, 98
24207, V, 1, 1, 1, 1, 0, 700, 98
24208, V, 1, 1, 1, 1, 0, 700, 98
24209, V, 1, 1, 1, 1, 0, 700, 98
24210, V, 1, 1, 1, 1, 0, 700, 98
24211, V, 1, 1, 1, 1, 0, 700, 98
24212, V, 1, 1, 1, 1, 0, 700, 98
24213, V, 1, 1, 1, 1, 0, 700, 98
24214, V, 1, 1, 1, 1, 0, 700, 98
24215, V, 1, 1, 1, 1, 0, 700, 98
24216, V, 1, 1, 1, 1, 0, 700, 98
24217, V, 1, 1, 1, 1, 0, 700, 98
24218, V, 1, 1, 1, 1, 0, 700, 98
24219, V, 1, 1, 1, 1, 0, 700, 99
24220, V, 1, 1, 1, 1, 0, 700, 99
24221, V, 1, 1, 1, 1, 0, 700, 99
24222, V, 1, 1, 1, 1, 0, 700, 98
24223, V, 1, 1, 1, 1, 0, 700, 99
24224, V, 1, 1, 1, 1, 0, 700, 99
24225, V, 1, 1, 1, 1, 0, 700, 98
24226, V, 1, 1, 1, 1, 0, 700, 99
24227, V, 1, 1, 1, 1, 0, 700, 98
24228, V, 1, 1, 1, 1, 0, 700, 98
24229, V, 1, 1, 1, 1, 0, 700, 98
24230, V, 1, 1, 1, 1, 0, 700, 99
24231, V, 1, 1, 1, 1, 0, 700, 99
24232, V, 1, 1, 1, 1, 0, 700, 98
24233, V, 1, 1, 1, 1, 0, 700, 98
24235, V, 1, 1, 1, 1, 0, 700, 98
24236, V, 1, 1, 1, 1, 0, 700, 98
24237, V, 1, 1, 1, 1, 0, 700, 98
24238, V, 1, 1, 1, 1, 0, 700, 98
24239, V, 1, 1, 1, 1, 0, 700, 99
24240, V, 1, 1, 1, 1, 0, 700, 98
24241, V, 1, 1, 1, 1, 0, 700, 98
24242, V, 1, 1, 1, 1, 0, 700, 98
24243, V, 1, 1, 1, 1, 0, 700, 99
24244, V, 1, 1, 1, 1, 0, 700, 98
24245, V, 1, 1, 1, 1, 0, 700, 98
24246, V, 1, 1, 1, 1, 0, 700, 98
24247, V, 1, 1, 1, 1, 0, 700, 98
24248, V, 1, 1, 1, 1, 0, 700, 98
24249, V, 1, 1, 1, 1, 0, 700, 98
24250, V, 1, 1, 1, 1, 0, 700, 98
24251, V, 1, 1, 1, 1, 0, 700, 98
24252, V, 1, 1, 1, 1, 0, 700, 98
24253, V, 1, 1, 1, 1, 0, 700, 98
24254, V, 1, 1, 1, 1, 0, 700, 98
24255, V, 1, 1, 1, 1, 0, 700, 98
24256, V, 1, 1, 1, 1, 0, 700, 98
24257, V, 1, 1, 1, 1, 0, 700, 98
24258, V, 1, 1, 1, 1, 0, 700, 98
24259, V, 1, 1, 1, 1, 0, 700, 98
24260, V, 1, 1, 1, 1, 0, 700, 98
24261, V, 1, 1, 1, 1, 0, 700, 98
24262, V, 1, 1, 1, 1, 0, 700, 98
24263, V, 1, 1, 1, 1, 0, 700, 98
24264, V, 1, 1, 1, 1, 0, 700, 98
24265, V, 1, 1, 1, 1, 0, 700, 98
24266, V, 1, 1, 1, 1, 0, 700, 98
24267, V, 1, 1, 1, 1, 0, 700, 98
24268, V, 1, 1, 1, 1, 0, 700, 98
24269, V, 1, 1, 1, 1, 0, 700, 98
24270, V, 1, 1, 1, 1, 0, 700, 98
24271, V, 1, 1, 1, 1, 0, 700, 98
24272, V, 1, 1, 1, 1, 0, 700, 98
24273, V, 1, 1, 1, 1, 0, 700, 98
24274, V, 1, 1, 1, 1, 0, 700, 98
24275, V, 1, 1, 1, 1, 0, 700, 98
24276, V, 1, 1, 1, 1, 0, 700, 98
24278, V, 1, 1, 1, 1, 0, 700, 98
24279, V, 1, 1, 1, 1, 0, 700, 98
24280, V, 1, 1, 1, 1, 0, 700, 98
24281, V, 1, 1, 1, 1, 0, 700, 98
24282, V, 1, 1, 1, 1, 0, 700, 98
24283, V, 1, 1, 1, 1, 0, 700, 98
24284, V, 1, 1, 1, 1, 0, 700, 98
24285, V, 1, 1, 1, 1, 0, 700, 98
24286, V, 1, 1, 1, 1, 0, 700, 98
24287, V, 1, 1, 1, 1, 0, 700, 98
24288, V, 1, 1, 1, 1, 0, 700, 98
24289, V, 1, 1, 1, 1, 0, 700, 98
24290, V, 1, 1, 1, 1, 0, 700, 98
24291, V, 1, 1, 1, 1, 0, 700, 98
24292, V, 1, 1, 1, 1, 0, 700, 98
24293, V, 1, 1, 1, 1, 0, 700, 98
24294, V, 1, 1, 1, 1, 0, 700, 98
24295, V, 1, 1, 1, 1, 0, 700, 98
24296, V, 1, 1, 1, 1, 0, 700, 98
24297, V, 1, 1, 1, 1, 0, 700, 98
24298, V, 1, 1, 1, 1, 0, 700, 98
24299, V, 1, 1, 1, 1, 0, 700, 98
24300, V, 1, 1, 1, 1, 0, 700, 98
24301, V, 1, 1, 1, 1, 0, 700, 98
24302, V, 1, 1, 1, 1, 0, 700, 98
24303, V, 1, 1, 1, 1, 0, 700, 98
24304, V, 1, 1, 1, 1, 0, 700, 98
24305, V, 1, 1, 1, 1, 0, 700, 98
24306, V, 1, 1, 1, 1, 0, 700, 98
24307, V, 1, 1, 1, 1, 0, 700, 98
24308, V, 1, 1, 1, 1, 0, 700, 98
24309, V, 1, 1, 1, 1, 0, 700, 98
24310, V, 1, 1, 1, 1, 0, 700, 98
24311, V, 1, 1, 1, 1, 0, 700, 98
24312, V, 1, 1, 1, 1, 0, 700, 98
24313, V, 1, 1, 1, 1, 0, 700, 98
24314, V, 1, 1, 1, 1, 0, 700, 98
24315, V, 1, 1, 1, 1, 0, 700, 98
24316, V, 1, 1, 1, 1, 0, 700, 98
24317, V, 1, 1, 1, 1, 0, 700, 98
24318, V, 1, 1, 1, 1, 0, 700, 98
24320, V, 1, 1, 1, 1, 0, 700, 98
24321, V, 1, 1, 1, 1, 0, 700, 98
24322, V, 1, 1, 1, 1, 0, 700, 98
24323, V, 1, 1, 1, 1, 0, 700, 98
24324, V, 1, 1, 1, 1, 0, 700, 98
24325, V, 1, 1, 1, 1, 0, 700, 98
24326, V, 1, 1, 1, 1, 0, 700, 98
24327, V, 1, 1, 1, 1, 0, 700, 98
24328, V, 1, 1, 1, 1, 0, 700, 98
24329, V, 1, 1, 1, 1, 0, 700, 98
24330, V, 1, 1, 1, 1, 0, 700, 98
24331, V, 1, 1, 1, 1, 0, 700, 98
24332, V, 1, 1, 1, 1, 0, 700, 98
24333, V, 1, 1, 1, 1, 0, 700, 98
24334, V, 1, 1, 1, 1, 0, 700, 98
24335, V, 1, 1, 1, 1, 0, 700, 98
24336, V, 1, 1, 1, 1, 0, 700, 98
24337, V, 1, 1, 1, 1, 0, 700, 98
24338, V, 1, 1, 1, 1, 0, 700, 98
24339, V, 1, 1, 1, 1, 0, 700, 98
24340, V, 1, 1, 1, 1, 0, 700, 98
24341, V, 1, 1, 1, 1, 0, 700, 98
24342, V, 1, 1, 1, 1, 0, 700, 98
24343, V, 1, 1, 1, 1, 0, 700, 98
24344, V, 1, 1, 1, 1, 0, 700, 98
24345, V, 1, 1, 1, 1, 0, 700, 98
24346, V, 1, 1, 1, 1, 0, 700, 98
24347, V, 1, 1, 1, 1, 0, 700, 98
24348, V, 1, 1, 1, 1, 0, 700, 98
24349, V, 1, 1, 1, 1, 0, 700, 98
24350, V, 1, 1, 1, 1, 0, 700, 98
24351, V, 1, 1, 1, 1, 0, 700, 98
24352, V, 1, 1, 1, 1, 0, 700, 98
24353, V, 1, 1, 1, 1, 0, 700, 98
24354, V, 1, 1, 1, 1, 0, 700, 98
24355, V, 1, 1, 1, 1, 0, 700, 98
24356, V, 1, 1, 1, 1, 0, 700, 98
24357, V, 1, 1, 1, 1, 0, 700, 98
24358, V, 1, 1, 1, 1, 0, 700, 98
24359, V, 1, 1, 1, 1, 0, 700, 98
24360, V, 1, 1, 1, 1, 0, 700, 98
24361, V, 1, 1, 1, 1, 0, 700, 98
24363, V, 1, 1, 1, 1, 0, 700, 98
24364, V, 1, 1, 1, 1, 0, 700, 98
24365, V, 1, 1, 1, 1, 0, 700, 98
24366, V, 1, 1, 1, 1, 0, 700, 98
24367, V, 1, 1, 1, 1, 0, 700, 98
24368, V, 1, 1, 1, 1, 0, 700, 98
24369, V, 1, 1, 1, 1, 0, 700, 98
24370, V, 1, 1, 1, 1, 0, 700, 98
24371, V, 1, 1, 1, 1, 0, 700, 98
24372, V, 1, 1, 1, 1, 0, 700, 98
24373, V, 1, 1, 1, 1, 0, 700, 98
24374, V, 1, 1, 1, 1, 0, 700, 98
24375, V, 1, 1, 1, 1, 0, 700, 98
24376, V, 1, 1, 1, 1, 0, 700, 98
24377, V, 1, 1, 1, 1, 0, 700, 98
24378, V, 1, 1, 1, 1, 0, 700, 98
24379, V, 1, 1, 1, 1, 0, 700, 98
24380, V, 1, 1, 1, 1, 0, 700, 98
24381, V, 1, 1, 1, 1, 0, 700, 98
24382, V, 1, 1, 1, 1, 0, 700, 98
24383, V, 1, 1, 1, 1, 0, 700, 98
24384, V, 1, 1, 1, 1, 0, 700, 98
24385, V, 1, 1, 1, 1, 0, 700, 98
24386, V, 1, 1, 1, 1, 0, 700, 98
24387, V, 1, 1, 1, 1, 0, 700, 98
24388, V, 1, 1, 1, 1, 0, 700, 98
24389, V, 1, 1, 1, 1, 0, 700, 98
24390, V, 1, 1, 1, 1, 0, 700, 98
24391, V, 1, 1, 1, 1, 0, 700, 98
24392, V, 1, 1, 1, 1, 0, 700, 98
24393, V, 1, 1, 1, 1, 0, 700, 98
24394, V, 1, 1, 1, 1, 0, 700, 98
24395, V, 1, 1, 1, 1, 0, 700, 98
24396, V, 1, 1, 1, 1, 0, 700, 98
24397, V, 1, 1, 1, 1, 0, 700, 98
24398, V, 1, 1, 1, 1, 0, 700, 98
24399, V, 1, 1, 1, 1, 0, 700, 98
24400, V, 1, 1, 1, 1, 0, 700, 98
24401, V, 1, 1, 1, 1, 0, 700, 98
24402, V, 1, 1, 1, 1, 0, 700, 98
24403, V, 1, 1, 1, 1, 0, 700, 98
24404, V, 1, 1, 1, 1, 0, 700, 98
24406, V, 1, 1, 1, 1, 0, 700, 98
24407, V, 1, 1, 1, 1, 0, 700, 98
24408, V, 1, 1, 1, 1, 0, 700, 98
24409, V, 1, 1, 1, 1, 0, 700, 98
24410, V, 1, 1, 1, 1, 0, 700, 98
24411, V, 1, 1, 1, 1, 0, 700, 98
24412, V, 1, 1, 1, 1, 0, 700, 98
24413, V, 1, 1, 1, 1, 0, 700, 98
24414, V, 1, 1, 1, 1, 0, 700, 98
24415, V, 1, 1, 1, 1, 0, 700, 98
24416, V, 1, 1, 1, 1, 0, 700, 98
24417, V, 1, 1, 1, 1, 0, 700, 98
24418, V, 1, 1, 1, 1, 0, 700, 98
24419, V, 1, 1, 1, 1, 0, 700, 98
24420, V, 1, 1, 1, 1, 0, 700, 98
24421, V, 1, 1, 1, 1, 0, 700, 98
24422, V, 1, 1, 1, 1, 0, 700, 98
24423, V, 1, 1, 1, 1, 0, 700, 98
24424, V, 1, 1, 1, 1, 0, 700, 98
24425, V, 1, 1, 1, 1, 0, 700, 98
24426, V, 1, 1, 1, 1, 0, 700, 98
24427, V, 1, 1, 1, 1, 0, 700, 98
24428, V, 1, 1, 1, 1, 0, 700, 98
24429, V, 1, 1, 1, 1, 0, 700, 98
24430, V, 1, 1, 1, 1, 0, 700, 98
24431, V, 1, 1, 1, 1, 0, 700, 99
24432, V, 1, 1, 1, 1, 0, 700, 98
24433, V, 1, 1, 1, 1, 0, 700, 98
24434, V, 1, 1, 1, 1, 0, 700, 98
24435, V, 1, 1, 1, 1, 0, 700, 98
24436, V, 1, 1, 1, 1, 0, 700, 98
24437, V, 1, 1, 1, 1, 0, 700, 98
24438, V, 1, 1, 1, 1, 0, 700, 98
24439, V, 1, 1, 1, 1, 0, 700, 98
24440, V, 1, 1, 1, 1, 0, 700, 98
24441, V, 1, 1, 1, 1, 0, 700, 99
24442, V, 1, 1, 1, 1, 0, 700, 98
24443, V, 1, 1, 1, 1, 0, 700, 98
24444, V, 1, 1, 1, 1, 0, 700, 99
24445, V, 1, 1, 1, 1, 0, 700, 99
24446, V, 1, 1, 1, 1, 0, 700, 99
24448, V, 1, 1, 1, 1, 0, 700, 99
24449, V, 1, 1, 1, 1, 0, 700, 99
24450, V, 1, 1, 1, 1, 0, 700, 99
24451, V, 1, 1, 1, 1, 0, 700, 99
24452, V, 1, 1, 1, 1, 0, 700, 99
24453, V, 1, 1, 1, 1, 0, 700, 99
24454, V, 1, 1, 1, 1, 0, 700, 99
24455, V, 1, 1, 1, 1, 0, 700, 99
24456, V, 1, 1, 1, 1, 0, 700, 99
24457, V, 1, 1, 1, 1, 0, 700, 99
24458, V, 1, 1, 1, 1, 0, 700, 98
24459, V, 1, 1, 1, 1, 0, 700, 99
24460, V, 1, 1, 1, 1, 0, 700, 99
24461, V, 1, 1, 1, 1, 0, 700, 99
24462, V, 1, 1, 1, 1, 0, 700, 99
24463, V, 1, 1, 1, 1, 0, 700, 98
24464, V, 1, 1, 1, 1, 0, 700, 98
24465, V, 1, 1, 1, 1, 0, 700, 98
24466, V, 1, 1, 1, 1, 0, 700, 98
24467, V, 1, 1, 1, 1, 0, 700, 98
24468, V, 1, 1, 1, 1, 0, 700, 98
24469, V, 1, 1, 1, 1, 0, 700, 99
24470, V, 1, 1, 1, 1, 0, 700, 98
24471, V, 1, 1, 1, 1, 0, 700, 98
24472, V, 1, 1, 1, 1, 0, 700, 98
24473, V, 1, 1, 1, 1, 0, 700, 98
24474, V, 1, 1, 1, 1, 0, 700, 98
24475, V, 1, 1, 1, 1, 0, 700, 98
24476, V, 1, 1, 1, 1, 0, 700, 98
24477, V, 1, 1, 1, 1, 0, 700, 99
24478, V, 1, 1, 1, 1, 0, 700, 98
24479, V, 1, 1, 1, 1, 0, 700, 98
24480, V, 1, 1, 1, 1, 0, 700, 98
24481, V, 1, 1, 1, 1, 0, 700, 98
24482, V, 1, 1, 1, 1, 0, 700, 98
24483, V, 1, 1, 1, 1, 0, 700, 98
24484, V, 1, 1, 1, 1, 0, 700, 98
24485, V, 1, 1, 1, 1, 0, 700, 98
24486, V, 1, 1, 1, 1, 0, 700, 98
24487, V, 1, 1, 1, 1, 0, 700, 98
24488, V, 1, 1, 1, 1, 0, 700, 98
24489, V, 1, 1, 1, 1, 0, 700, 98
24491, V, 1, 1, 1, 1, 0, 700, 98
24492, V, 1, 1, 1, 1, 0, 700, 98
24493, V, 1, 1, 1, 1, 0, 700, 98
24494, V, 1, 1, 1, 1, 0, 700, 98
24495, V, 1, 1, 1, 1, 0, 700, 98
24496, V, 1, 1, 1, 1, 0, 700, 98
24497, V, 1, 1, 1, 1, 0, 700, 98
24498, V, 1, 1, 1, 1, 0, 700, 98
24499, V, 1, 1, 1, 1, 0, 700, 98
24500, V, 1, 1, 1, 1, 0, 700, 98
24501, V, 1, 1, 1, 1, 0, 700, 98
24502, V, 1, 1, 1, 1, 0, 700, 98
24503, V, 1, 1, 1, 1, 0, 700, 98
24504, V, 1, 1, 1, 1, 0, 700, 98
24505, V, 1, 1, 1, 1, 0, 700, 98
24506, V, 1, 1, 1, 1, 0, 700, 98
24507, V, 1, 1, 1, 1, 0, 700, 98
24508, V, 1, 1, 1, 1, 0, 700, 98
24509, V, 1, 1, 1, 1, 0, 700, 98
24510, V, 1, 1, 1, 1, 0, 700, 98
24511, V, 1, 1, 1, 1, 0, 700, 98
24512, V, 1, 1, 1, 1, 0, 700, 98
24513, V, 1, 1, 1, 1, 0, 700, 98
24514, V, 1, 1, 1, 1, 0, 700, 98
24515, V, 1, 1, 1, 1, 0, 700, 98
24516, V, 1, 1, 1, 1, 0, 700, 98
24517, V, 1, 1, 1, 1, 0, 700, 98
24518, V, 1, 1, 1, 1, 0, 700, 98
24519, V, 1, 1, 1, 1, 0, 700, 98
24520, V, 1, 1, 1, 1, 0, 700, 98
24521, V, 1, 1, 1, 1, 0, 700, 98
24522, V, 1, 1, 1, 1, 0, 700, 99
24523, V, 1, 1, 1, 1, 0, 700, 99
24524, V, 1, 1, 1, 1, 0, 700, 99
24525, V, 1, 1, 1, 1, 0, 700, 99
24526, V, 1, 1, 1, 1, 0, 700, 99
24527, V, 1, 1, 1, 1, 0, 700, 99
24528, V, 1, 1, 1, 1, 0, 700, 99
24529, V, 1, 1, 1, 1, 0, 700, 99
24530, V, 1, 1, 1, 1, 0, 700, 99
24531, V, 1, 1, 1, 1, 0, 700, 99
24532, V, 1, 1, 1, 1, 0, 700, 99
24534, V, 1, 1, 1, 1, 0, 700, 99
24535, V, 1, 1, 1, 1, 0, 700, 99
24536, V, 1, 1, 1, 1, 0, 700, 99
24537, V, 1, 1, 1, 1, 0, 700, 99
24538, V, 1, 1, 1, 1, 0, 700, 99
24539, V, 1, 1, 1, 1, 0, 700, 99
24540, V, 1, 1, 1, 1, 0, 700, 99
24541, V, 1, 1, 1, 1, 0, 700, 99
24542, V, 1, 1, 1, 1, 0, 700, 99
24543, V, 1, 1, 1, 1, 0, 700, 99
24544, V, 1, 1, 1, 1, 0, 700, 99
24545, V, 1, 1, 1, 1, 0, 700, 99
24546, V, 1, 1, 1, 1, 0, 700, 99
24547, V, 1, 1, 1, 1, 0, 700, 99
24548, V, 1, 1, 1, 1, 0, 700, 99
24549, V, 1, 1, 1, 1, 0, 700, 99
24550, V, 1, 1, 1, 1, 0, 700, 99
24551, V, 1, 1, 1, 1, 0, 700, 99
24552, V, 1, 1, 1, 1, 0, 700, 99
24553, V, 1, 1, 1, 1, 0, 700, 99
24554, V, 1, 1, 1, 1, 0, 700, 99
24555, V, 1, 1, 1, 1, 0, 700, 99
24556, V, 1, 1, 1, 1, 0, 700, 99
24557, V, 1, 1, 1, 1, 0, 700, 99
24558, V, 1, 1, 1, 1, 0, 700, 99
24559, V, 1, 1, 1, 1, 0, 700, 99
24560, V, 1, 1, 1, 1, 0, 700, 99
24561, V, 1, 1, 1, 1, 0, 700, 99
24562, V, 1, 1, 1, 1, 0, 700, 99
24563, V, 1, 1, 1, 1, 0, 700, 99
24564, V, 1, 1, 1, 1, 0, 700, 98
24565, V, 1, 1, 1, 1, 0, 700, 98
24566, V, 1, 1, 1, 1, 0, 700, 98
24567, V, 1, 1, 1, 1, 0, 700, 98
24568, V, 1, 1, 1, 1, 0, 700, 98
24569, V, 1, 1, 1, 1, 0, 700, 98
24570, V, 1, 1, 1, 1, 0, 700, 98
24571, V, 1, 1, 1, 1, 0, 700, 98
24572, V, 1, 1, 1, 1, 0, 700, 98
24573, V, 1, 1, 1, 1, 0, 700, 98
24574, V, 1, 1, 1, 1, 0, 700, 98
24576, V, 1, 1, 1, 1, 0, 700, 98
24577, V, 1, 1, 1, 1, 0, 700, 98
24578, V, 1, 1, 1, 1, 0, 700, 98
24579, V, 1, 1, 1, 1, 0, 700, 98
24580, V, 1, 1, 1, 1, 0, 700, 98
24581, V, 1, 1, 1, 1, 0, 700, 99
24582, V, 1, 1, 1, 1, 0, 700, 99
24583, V, 1, 1, 1, 1, 0, 700, 99
24584, V, 1, 1, 1, 1, 0, 700, 99
24585, V, 1, 1, 1, 1, 0, 700, 99
24586, V, 1, 1, 1, 1, 0, 700, 99
24587, V, 1, 1, 1, 1, 0, 700, 99
24588, V, 1, 1, 1, 1, 0, 700, 99
24589, V, 1, 1, 1, 1, 0, 700, 99
24590, V, 1, 1, 1, 1, 0, 700, 99
24591, V, 1, 1, 1, 1, 0, 700, 99
24592, V, 1, 1, 1, 1, 0, 700, 99
24593, V, 1, 1, 1, 1, 0, 700, 99
24594, V, 1, 1, 1, 1, 0, 700, 99
24595, V, 1, 1, 1, 1, 0, 700, 99
24596, V, 1, 1, 1, 1, 0, 700, 99
24597, V, 1, 1, 1, 1, 0, 700, 99
24598, V, 1, 1, 1, 1, 0, 700, 99
24599, V, 1, 1, 1, 1, 0, 700, 99
24600, V, 1, 1, 1, 1, 0, 700, 99
24601, V, 1, 1, 1, 1, 0, 700, 99
24602, V, 1, 1, 1, 1, 0, 700, 99
24603, V, 1, 1, 1, 1, 0, 700, 99
24604, V, 1, 1, 1, 1, 0, 700, 99
24605, V, 1, 1, 1, 1, 0, 700, 99
24606, V, 1, 1, 1, 1, 0, 700, 99
24607, V, 1, 1, 1, 1, 0, 700, 99
24608, V, 1, 1, 1, 1, 0, 700, 99
24609, V, 1, 1, 1, 1, 0, 700, 99
24610, V, 1, 1, 1, 1, 0, 700, 99
24611, V, 1, 1, 1, 1, 0, 700, 99
24612, V, 1, 1, 1, 1, 0, 700, 99
24613, V, 1, 1, 1, 1, 0, 700, 99
24614, V, 1, 1, 1, 1, 0, 700, 99
24615, V, 1, 1, 1, 1, 0, 700, 99
24616, V, 1, 1, 1, 1, 0, 700, 99
24617, V, 1, 1, 1, 1, 0, 700, 99
24619, V, 1, 1, 1, 1, 0, 700, 99
24620, V, 1, 1, 1, 1, 0, 700, 99
24621, V, 1, 1, 1, 1, 0, 700, 99
24622, V, 1, 1, 1, 1, 0, 700, 99
24623, V, 1, 1, 1, 1, 0, 700, 99
24624, V, 1, 1, 1, 1, 0, 700, 99
24625, V, 1, 1, 1, 1, 0, 700, 99
24626, V, 1, 1, 1, 1, 0, 700, 99
24627, V, 1, 1, 1, 1, 0, 700, 99
24628, V, 1, 1, 1, 1, 0, 700, 99
24629, V, 1, 1, 1, 1, 0, 700, 99
24630, V, 1, 1, 1, 1, 0, 700, 99
24631, V, 1, 1, 1, 1, 0, 700, 99
24632, V, 1, 1, 1, 1, 0, 700, 99
24633, V, 1, 1, 1, 1, 0, 700, 99
24634, V, 1, 1, 1, 1, 0, 700, 99
24635, V, 1, 1, 1, 1, 0, 700, 99
24636, V, 1, 1, 1, 1, 0, 700, 99
24637, V, 1, 1, 1, 1, 0, 700, 99
24638, V, 1, 1, 1, 1, 0, 700, 99
24639, V, 1, 1, 1, 1, 0, 700, 99
24640, V, 1, 1, 1, 1, 0, 700, 98
24641, V, 1, 1, 1, 1, 0, 700, 99
24642, V, 1, 1, 1, 1, 0, 700, 99
24643, V, 1, 1, 1, 1, 0, 700, 99
24644, V, 1, 1, 1, 1, 0, 700, 99
24645, V, 1, 1, 1, 1, 0, 700, 98
24646, V, 1, 1, 1, 1, 0, 700, 99
24647, V, 1, 1, 1, 1, 0, 700, 99
24648, V, 1, 1, 1, 1, 0, 700, 98
24649, V, 1, 1, 1, 1, 0, 700, 98
24650, V, 1, 1, 1, 1, 0, 700, 98
24651, V, 1, 1, 1, 1, 0, 700, 98
24652, V, 1, 1, 1, 1, 0, 700, 98
24653, V, 1, 1, 1, 1, 0, 700, 98
24654, V, 1, 1, 1, 1, 0, 700, 98
24655, V, 1, 1, 1, 1, 0, 700, 98
24656, V, 1, 1, 1, 1, 0, 700, 98
24657, V, 1, 1, 1, 1, 0, 700, 98
24658, V, 1, 1, 1, 1, 0, 700, 98
24659, V, 1, 1, 1, 1, 0, 700, 98
24660, V, 1, 1, 1, 1, 0, 700, 98
24662, V, 1, 1, 1, 1, 0, 700, 98
24663, V, 1, 1, 1, 1, 0, 700, 98
24664, V, 1, 1, 1, 1, 0, 700, 98
24665, V, 1, 1, 1, 1, 0, 700, 98
24666, V, 1, 1, 1, 1, 0, 700, 98
24667, V, 1, 1, 1, 1, 0, 700, 98
24668, V, 1, 1, 1, 1, 0, 700, 98
24669, V, 1, 1, 1, 1, 0, 700, 98
24670, V, 1, 1, 1, 1, 0, 700, 98
24671, V, 1, 1, 1, 1, 0, 700, 98
24672, V, 1, 1, 1, 1, 0, 700, 98
24673, V, 1, 1, 1, 1, 0, 700, 98
24674, V, 1, 1, 1, 1, 0, 700, 99
24675, V, 1, 1, 1, 1, 0, 700, 98
24676, V, 1, 1, 1, 1, 0, 700, 98
24677, V, 1, 1, 1, 1, 0, 700, 98
24678, V, 1, 1, 1, 1, 0, 700, 98
24679, V, 1, 1, 1, 1, 0, 700, 99
24680, V, 1, 1, 1, 1, 0, 700, 98
24681, V, 1, 1, 1, 1, 0, 700, 99
24682, V, 1, 1, 1, 1, 0, 700, 99
24683, V, 1, 1, 1, 1, 0, 700, 99
24684, V, 1, 1, 1, 1, 0, 700, 99
24685, V, 1, 1, 1, 1, 0, 700, 99
24686, V, 1, 1, 1, 1, 0, 700, 99
24687, V, 1, 1, 1, 1, 0, 700, 99
24688, V, 1, 1, 1, 1, 0, 700, 99
24689, V, 1, 1, 1, 1, 0, 700, 99
24690, V, 1, 1, 1, 1, 0, 700, 99
24691, V, 1, 1, 1, 1, 0, 700, 99
24692, V, 1, 1, 1, 1, 0, 700, 99
24693, V, 1, 1, 1, 1, 0, 700, 99
24694, V, 1, 1, 1, 1, 0, 700, 99
24695, V, 1, 1, 1, 1, 0, 700, 99
24696, V, 1, 1, 1, 1, 0, 700, 99
24697, V, 1, 1, 1, 1, 0, 700, 99
24698, V, 1, 1, 1, 1, 0, 700, 99
24699, V, 1, 1, 1, 1, 0, 700, 99
24700, V, 1, 1, 1, 1, 0, 700, 99
24701, V, 1, 1, 1, 1, 0, 700, 99
24702, V, 1, 1, 1, 1, 0, 700, 99
24704, V, 1, 1, 1, 1, 0, 700, 99
24705, V, 1, 1, 1, 1, 0, 700, 99
24706, V, 1, 1, 1, 1, 0, 700, 99
24707, V, 1, 1, 1, 1, 0, 700, 99
24708, V, 1, 1, 1, 1, 0, 700, 99
24709, V, 1, 1, 1, 1, 0, 700, 99
24710, V, 1, 1, 1, 1, 0, 700, 99
24711, V, 1, 1, 1, 1, 0, 700, 99
24712, V, 1, 1, 1, 1, 0, 700, 99
24713, V, 1, 1, 1, 1, 0, 700, 99
24714, V, 1, 1, 1, 1, 0, 700, 99
24715, V, 1, 1, 1, 1, 0, 700, 99
24716, V, 1, 1, 1, 1, 0, 700, 99
24717, V, 1, 1, 1, 1, 0, 700, 99
24718, V, 1, 1, 1, 1, 0, 700, 99
24719, V, 1, 1, 1, 1, 0, 700, 99
24720, V, 1, 1, 1, 1, 0, 700, 99
24721, V, 1, 1, 1, 1, 0, 700, 99
24722, V, 1, 1, 1, 1, 0, 700, 99
24723, V, 1, 1, 1, 1, 0, 700, 99
24724, V, 1, 1, 1, 1, 0, 700, 99
24725, V, 1, 1, 1, 1, 0, 700, 99
24726, V, 1, 1, 1, 1, 0, 700, 99
24727, V, 1, 1, 1, 1, 0, 700, 99
24728, V, 1, 1, 1, 1, 0, 700, 99
24729, V, 1, 1, 1, 1, 0, 700, 99
24730, V, 1, 1, 1, 1, 0, 700, 99
24731, V, 1, 1, 1, 1, 0, 700, 99
24732, V, 1, 1, 1, 1, 0, 700, 99
24733, V, 1, 1, 1, 1, 0, 700, 98
24734, V, 1, 1, 1, 1, 0, 700, 99
24735, V, 1, 1, 1, 1, 0, 700, 99
24736, V, 1, 1, 1, 1, 0, 700, 99
24737, V, 1, 1, 1, 1, 0, 700, 99
24738, V, 1, 1, 1, 1, 0, 700, 98
24739, V, 1, 1, 1, 1, 0, 700, 98
24740, V, 1, 1, 1, 1, 0, 700, 98
24741, V, 1, 1, 1, 1, 0, 700, 98
24742, V, 1, 1, 1, 1, 0, 700, 98
24743, V, 1, 1, 1, 1, 0, 700, 98
24744, V, 1, 1, 1, 1, 0, 700, 98
24745, V, 1, 1, 1, 1, 0, 700, 99
24747, V, 1, 1, 1, 1, 0, 700, 98
24748, V, 1, 1, 1, 1, 0, 700, 98
24749, V, 1, 1, 1, 1, 0, 700, 98
24750, V, 1, 1, 1, 1, 0, 700, 98
24751, V, 1, 1, 1, 1, 0, 700, 98
24752, V, 1, 1, 1, 1, 0, 700, 98
24753, V, 1, 1, 1, 1, 0, 700, 98
24754, V, 1, 1, 1, 1, 0, 700, 98
24755, V, 1, 1, 1, 1, 0, 700, 98
24756, V, 1, 1, 1, 1, 0, 700, 98
24757, V, 1, 1, 1, 1, 0, 700, 98
24758, V, 1, 1, 1, 1, 0, 700, 98
24759, V, 1, 1, 1, 1, 0, 700, 98
24760, V, 1, 1, 1, 1, 0, 700, 98
24761, V, 1, 1, 1, 1, 0, 700, 98
24762, V, 1, 1, 1, 1, 0, 700, 98
24763, V, 1, 1, 1, 1, 0, 700, 98
24764, V, 1, 1, 1, 1, 0, 700, 98
24765, V, 1, 1, 1, 1, 0, 700, 98
24766, V, 1, 1, 1, 1, 0, 700, 98
24767, V, 1, 1, 1, 1, 0, 700, 98
24768, V, 1, 1, 1, 1, 0, 700, 98
24769, V, 1, 1, 1, 1, 0, 700, 98
24770, V, 1, 1, 1, 1, 0, 700, 98
24771, V, 1, 1, 1, 1, 0, 700, 98
24772, V, 1, 1, 1, 1, 0, 700, 98
24773, V, 1, 1, 1, 1, 0, 700, 98
24774, V, 1, 1, 1, 1, 0, 700, 98
24775, V, 1, 1, 1, 1, 0, 700, 98
24776, V, 1, 1, 1, 1, 0, 700, 98
24777, V, 1, 1, 1, 1, 0, 700, 98
24778, V, 1, 1, 1, 1, 0, 700, 98
24779, V, 1, 1, 1, 1, 0, 700, 98
24780, V, 1, 1, 1, 1, 0, 700, 98
24781, V, 1, 1, 1, 1, 0, 700, 98
24782, V, 1, 1, 1, 1, 0, 700, 98
24783, V, 1, 1, 1, 1, 0, 700, 98
24784, V, 1, 1, 1, 1, 0, 700, 98
24785, V, 1, 1, 1, 1, 0, 700, 98
24786, V, 1, 1, 1, 1, 0, 700, 98
24787, V, 1, 1, 1, 1, 0, 700, 98
24788, V, 1, 1, 1, 1, 0, 700, 98
24790, V, 1, 1, 1, 1, 0, 700, 98
24791, V, 1, 1, 1, 1, 0, 700, 98
24792, V, 1, 1, 1, 1, 0, 700, 98
24793, V, 1, 1, 1, 1, 0, 700, 98
24794, V, 1, 1, 1, 1, 0, 700, 98
24795, V, 1, 1, 1, 1, 0, 700, 98
24796, V, 1, 1, 1, 1, 0, 700, 98
24797, V, 1, 1, 1, 1, 0, 700, 98
24798, V, 1, 1, 1, 1, 0, 700, 98
24799, V, 1, 1, 1, 1, 0, 700, 98
24800, V, 1, 1, 1, 1, 0, 700, 98
24801, V, 1, 1, 1, 1, 0, 700, 98
24802, V, 1, 1, 1, 1, 0, 700, 98
24803, V, 1, 1, 1, 1, 0, 700, 98
24804, V, 1, 1, 1, 1, 0, 700, 98
24805, V, 1, 1, 1, 1, 0, 700, 98
24806, V, 1, 1, 1, 1, 0, 700, 98
24807, V, 1, 1, 1, 1, 0, 700, 98
24808, V, 1, 1, 1, 1, 0, 700, 98
24809, V, 1, 1, 1, 1, 0, 700, 98
24810, V, 1, 1, 1, 1, 0, 700, 98
24811, V, 1, 1, 1, 1, 0, 700, 98
24812, V, 1, 1, 1, 1, 0, 700, 98
24813, V, 1, 1, 1, 1, 0, 700, 98
24814, V, 1, 1, 1, 1, 0, 700, 98
24815, V, 1, 1, 1, 1, 0, 700, 98
24816, V, 1, 1, 1, 1, 0, 700, 98
24817, V, 1, 1, 1, 1, 0, 700, 98
24818, V, 1, 1, 1, 1, 0, 700, 98
24819, V, 1, 1, 1, 1, 0, 700, 98
24820, V, 1, 1, 1, 1, 0, 700, 98
24821, V, 1, 1, 1, 1, 0, 700, 98
24822, V, 1, 1, 1, 1, 0, 700, 98
24823, V, 1, 1, 1, 1, 0, 700, 98
24824, V, 1, 1, 1, 1, 0, 700, 98
24825, V, 1, 1, 1, 1, 0, 700, 98
24826, V, 1, 1, 1, 1, 0, 700, 98
24827, V, 1, 1, 1, 1, 0, 700, 98
24828, V, 1, 1, 1, 1, 0, 700, 98
24829, V, 1, 1, 1, 1, 0, 700, 98
24830, V, 1, 1, 1, 1, 0, 700, 98
24832, V, 1, 1, 1, 1, 0, 700, 98
24833, V, 1, 1, 1, 1, 0, 700, 98
24834, V, 1, 1, 1, 1, 0, 700, 98
24835, V, 1, 1, 1, 1, 0, 700, 98
24836, V, 1, 1, 1, 1, 0, 700, 98
24837, V, 1, 1, 1, 1, 0, 700, 98
24838, V, 1, 1, 1, 1, 0, 700, 98
24839, V, 1, 1, 1, 1, 0, 700, 98
24840, V, 1, 1, 1, 1, 0, 700, 98
24841, V, 1, 1, 1, 1, 0, 700, 98
24842, V, 1, 1, 1, 1, 0, 700, 98
24843, V, 1, 1, 1, 1, 0, 700, 98
24844, V, 1, 1, 1, 1, 0, 700, 98
24845, V, 1, 1, 1, 1, 0, 700, 98
24846, V, 1, 1, 1, 1, 0, 700, 98
24847, V, 1, 1, 1, 1, 0, 700, 98
24848, V, 1, 1, 1, 1, 0, 700, 98
24849, V, 1, 1, 1, 1, 0, 700, 98
24850, V, 1, 1, 1, 1, 0, 700, 98
24851, V, 1, 1, 1, 1, 0, 700, 98
24852, V, 1, 1, 1, 1, 0, 700, 98
24853, V, 1, 1, 1, 1, 0, 700, 98
24854, V, 1, 1, 1, 1, 0, 700, 98
24855, V, 1, 1, 1, 1, 0, 700, 98
24856, V, 1, 1, 1, 1, 0, 700, 98
24857, V, 1, 1, 1, 1, 0, 700, 98
24858, V, 1, 1, 1, 1, 0, 700, 98
24859, V, 1, 1, 1, 1, 0, 700, 98
24860, V, 1, 1, 1, 1, 0, 700, 98
24861, V, 1, 1, 1, 1, 0, 700, 98
24862, V, 1, 1, 1, 1, 0, 700, 98
24863, V, 1, 1, 1, 1, 0, 700, 98
24864, V, 1, 1, 1, 1, 0, 700, 98
24865, V, 1, 1, 1, 1, 0, 700, 98
24866, V, 1, 1, 1, 1, 0, 700, 98
24867, V, 1, 1, 1, 1, 0, 700, 98
24868, V, 1, 1, 1, 1, 0, 700, 98
24869, V, 1, 1, 1, 1, 0, 700, 98
24870, V, 1, 1, 1, 1, 0, 700, 98
24871, V, 1, 1, 1, 1, 0, 700, 98
24872, V, 1, 1, 1, 1, 0, 700, 98
24873, V, 1, 1, 1, 1, 0, 700, 98
24875, V, 1, 1, 1, 1, 0, 700, 98
24876, V, 1, 1, 1, 1, 0, 700, 98
24877, V, 1, 1, 1, 1, 0, 700, 98
24878, V, 1, 1, 1, 1, 0, 700, 98
24879, V, 1, 1, 1, 1, 0, 700, 98
24880, V, 1, 1, 1, 1, 0, 700, 98
24881, V, 1, 1, 1, 1, 0, 700, 98
24882, V, 1, 1, 1, 1, 0, 700, 98
24883, V, 1, 1, 1, 1, 0, 700, 98
24884, V, 1, 1, 1, 1, 0, 700, 98
24885, V, 1, 1, 1, 1, 0, 700, 98
24886, V, 1, 1, 1, 1, 0, 700, 98
24887, V, 1, 1, 1, 1, 0, 700, 98
24888, V, 1, 1, 1, 1, 0, 700, 98
24889, V, 1, 1, 1, 1, 0, 700, 98
24890, V, 1, 1, 1, 1, 0, 700, 98
24891, V, 1, 1, 1, 1, 0, 700, 98
24892, V, 1, 1, 1, 1, 0, 700, 98
24893, V, 1, 1, 1, 1, 0, 700, 98
24894, V, 1, 1, 1, 1, 0, 700, 98
24895, V, 1, 1, 1, 1, 0, 700, 98
24896, V, 1, 1, 1, 1, 0, 700, 98
24897, V, 1, 1, 1, 1, 0, 700, 98
24898, V, 1, 1, 1, 1, 0, 700, 98
24899, V, 1, 1, 1, 1, 0, 700, 98
24900, V, 1, 1, 1, 1, 0, 700, 98
24901, V, 1, 1, 1, 1, 0, 700, 98
24902, V, 1, 1, 1, 1, 0, 700, 98
24903, V, 1, 1, 1, 1, 0, 700, 98
24904, V, 1, 1, 1, 1, 0, 700, 98
24905, V, 1, 1, 1, 1, 0, 700, 98
24906, V, 1, 1, 1, 1, 0, 700, 98
24907, V, 1, 1, 1, 1, 0, 700, 98
24908, V, 1, 1, 1, 1, 0, 700, 98
24909, V, 1, 1, 1, 1, 0, 700, 98
24910, V, 1, 1, 1, 1, 0, 700, 98
24911, V, 1, 1, 1, 1, 0, 700, 98
24912, V, 1, 1, 1, 1, 0, 700, 98
24913, V, 1, 1, 1, 1, 0, 700, 98
24914, V, 1, 1, 1, 1, 0, 700, 98
24915, V, 1, 1, 1, 1, 0, 700, 98
24916, V, 1, 1, 1, 1, 0, 700, 98
24918, V, 1, 1, 1, 1, 0, 700, 98
24919, V, 1, 1, 1, 1, 0, 700, 98
24920, V, 1, 1, 1, 1, 0, 700, 98
24921, V, 1, 1, 1, 1, 0, 700, 98
24922, V, 1, 1, 1, 1, 0, 700, 98
24923, V, 1, 1, 1, 1, 0, 700, 98
24924, V, 1, 1, 1, 1, 0, 700, 98
24925, V, 1, 1, 1, 1, 0, 700, 98
24926, V, 1, 1, 1, 1, 0, 700, 98
24927, V, 1, 1, 1, 1, 0, 700, 98
24928, V, 1, 1, 1, 1, 0, 700, 98
24929, V, 1, 1, 1, 1, 0, 700, 98
24930, V, 1, 1, 1, 1, 0, 700, 98
24931, V, 1, 1, 1, 1, 0, 700, 98
24932, V, 1, 1, 1, 1, 0, 700, 98
24933, V, 1, 1, 1, 1, 0, 700, 98
24934, V, 1, 1, 1, 1, 0, 700, 98
24935, V, 1, 1, 1, 1, 0, 700, 98
24936, V, 1, 1, 1, 1, 0, 700, 98
24937, V, 1, 1, 1, 1, 0, 700, 98
24938, V, 1, 1, 1, 1, 0, 700, 98
24939, V, 1, 1, 1, 1, 0, 700, 98
24940, V, 1, 1, 1, 1, 0, 700, 98
24941, V, 1, 1, 1, 1, 0, 700, 98
24942, V, 1, 1, 1, 1, 0, 700, 98
24943, V, 1, 1, 1, 1, 0, 700, 98
24944, V, 1, 1, 1, 1, 0, 700, 98
24945, V, 1, 1, 1, 1, 0, 700, 98
24946, V, 1, 1, 1, 1, 0, 700, 98
24947, V, 1, 1, 1, 1, 0, 700, 98
24948, V, 1, 1, 1, 1, 0, 700, 98
24949, V, 1, 1, 1, 1, 0, 700, 98
24950, V, 1, 1, 1, 1, 0, 700, 98
24951, V, 1, 1, 1, 1, 0, 700, 98
24952, V, 1, 1, 1, 1, 0, 700, 98
24953, V, 1, 1, 1, 1, 0, 700, 98
24954, V, 1, 1, 1, 1, 0, 700, 98
24955, V, 1, 1, 1, 1, 0, 700, 98
24956, V, 1, 1, 1, 1, 0, 700, 98
24957, V, 1, 1, 1, 1, 0, 700, 98
24958, V, 1, 1, 1, 1, 0, 700, 98
24960, V, 1, 1, 1, 1, 0, 700, 98
24961, V, 1, 1, 1, 1, 0, 700, 98
24962, V, 1, 1, 1, 1, 0, 700, 98
24963, V, 1, 1, 1, 1, 0, 700, 98
24964, V, 1, 1, 1, 1, 0, 700, 98
24965, V, 1, 1, 1, 1, 0, 700, 98
24966, V, 1, 1, 1, 1, 0, 700, 98
24967, V, 1, 1, 1, 1, 0, 700, 98
24968, V, 1, 1, 1, 1, 0, 700, 98
24969, V, 1, 1, 1, 1, 0, 700, 98
24970, V, 1, 1, 1, 1, 0, 700, 98
24971, V, 1, 1, 1, 1, 0, 700, 98
24972, V, 1, 1, 1, 1, 0, 700, 98
24973, V, 1, 1, 1, 1, 0, 700, 98
24974, V, 1, 1, 1, 1, 0, 700, 98
24975, V, 1, 1, 1, 1, 0, 700, 98
24976, V, 1, 1, 1, 1, 0, 700, 98
24977, V, 1, 1, 1, 1, 0, 700, 98
24978, V, 1, 1, 1, 1, 0, 700, 98
24979, V, 1, 1, 1, 1, 0, 700, 98
24980, V, 1, 1, 1, 1, 0, 700, 98
24981, V, 1, 1, 1, 1, 0, 700, 98
24982, V, 1, 1, 1, 1, 0, 700, 98
24983, V, 1, 1, 1, 1, 0, 700, 98
24984, V, 1, 1, 1, 1, 0, 700, 98
24985, V, 1, 1, 1, 1, 0, 700, 98
24986, V, 1, 1, 1, 1, 0, 700, 98
24987, V, 1, 1, 1, 1, 0, 700, 98
24988, V, 1, 1, 1, 1, 0, 700, 98
24989, V, 1, 1, 1, 1, 0, 700, 98
24990, V, 1, 1, 1, 1, 0, 700, 98
24991, V, 1, 1, 1, 1, 0, 700, 98
24992, V, 1, 1, 1, 1, 0, 700, 98
24993, V, 1, 1, 1, 1, 0, 700, 98
24994, V, 1, 1, 1, 1, 0, 700, 98
24995, V, 1, 1, 1, 1, 0, 700, 98
24996, V, 1, 1, 1, 1, 0, 700, 98
24997, V, 1, 1, 1, 1, 0, 700, 98
24998, V, 1, 1, 1, 1, 0, 700, 98
24999, V, 1, 1, 1, 1, 0, 700, 98
25000, V, 1, 1, 1, 1, 0, 700, 98
25001, V, 1, 1, 1, 1, 0, 700, 98
25003, V, 1, 1, 1, 1, 0, 700, 98
25004, V, 1, 1, 1, 1, 0, 700, 98
25005, V, 1, 1, 1, 1, 0, 700, 98
25006, V, 1, 1, 1, 1, 0, 700, 98
25007, V, 1, 1, 1, 1, 0, 700, 98
25008, V, 1, 1, 1, 1, 0, 700, 98
25009, V, 1, 1, 1, 1, 0, 700, 98
25010, V, 1, 1, 1, 1, 0, 700, 98
25011, V, 1, 1, 1, 1, 0, 700, 98
25012, V, 1, 1, 1, 1, 0, 700, 98
25013, V, 1, 1, 1, 1, 0, 700, 98
25014, V, 1, 1, 1, 1, 0, 700, 98
25015, V, 1, 1, 1, 1, 0, 700, 98
25016, V, 1, 1, 1, 1, 0, 700, 98
25017, V, 1, 1, 1, 1, 0, 700, 98
25018, V, 1, 1, 1, 1, 0, 700, 98
25019, V, 1, 1, 1, 1, 0, 700, 98
25020, V, 1, 1, 1, 1, 0, 700, 98
25021, V, 1, 1, 1, 1, 0, 700, 98
25022, V, 1, 1, 1, 1, 0, 700, 98
25023, V, 1, 1, 1, 1, 0, 700, 98
25024, V, 1, 1, 1, 1, 0, 700, 98
25025, V, 1, 1, 1, 1, 0, 700, 98
25026, V, 1, 1, 1, 1, 0, 700, 98
25027, V, 1, 1, 1, 1, 0, 700, 98
25028, V, 1, 1, 1, 1, 0, 700, 98
25029, V, 1, 1, 1, 1, 0, 700, 98
25030, V, 1, 1, 1, 1, 0, 700, 98
25031, V, 1, 1, 1, 1, 0, 700, 98
25032, V, 1, 1, 1, 1, 0, 700, 98
25033, V, 1, 1, 1, 1, 0, 700, 98
25034, V, 1, 1, 1, 1, 0, 700, 98
25035, V, 1, 1, 1, 1, 0, 700, 98
25036, V, 1, 1, 1, 1, 0, 700, 98
25037, V, 1, 1, 1, 1, 0, 700, 98
25038, V, 1, 1, 1, 1, 0, 700, 98
25039, V, 1, 1, 1, 1, 0, 700, 98
25040, V, 1, 1, 1, 1, 0, 700, 98
25041, V, 1, 1, 1, 1, 0, 700, 98
25042, V, 1, 1, 1, 1, 0, 700, 98
25043, V, 1, 1, 1, 1, 0, 700, 98
25044, V, 1, 1, 1, 1, 0, 700, 98
25046, V, 1, 1, 1, 1, 0, 700, 98
25047, V, 1, 1, 1, 1, 0, 700, 98
25048, V, 1, 1, 1, 1, 0, 700, 98
25049, V, 1, 1, 1, 1, 0, 700, 98
25050, V, 1, 1, 1, 1, 0, 700, 98
25051, V, 1, 1, 1, 1, 0, 700, 98
25052, V, 1, 1, 1, 1, 0, 700, 98
25053, V, 1, 1, 1, 1, 0, 700, 98
25054, V, 1, 1, 1, 1, 0, 700, 98
25055, V, 1, 1, 1, 1, 0, 700, 98
25056, V, 1, 1, 1, 1, 0, 700, 98
25057, V, 1, 1, 1, 1, 0, 700, 98
25058, V, 1, 1, 1, 1, 0, 700, 98
25059, V, 1, 1, 1, 1, 0, 700, 98
25060, V, 1, 1, 1, 1, 0, 700, 98
25061, V, 1, 1, 1, 1, 0, 700, 98
25062, V, 1, 1, 1, 1, 0, 700, 98
25063, V, 1, 1, 1, 1, 0, 700, 98
25064, V, 1, 1, 1, 1, 0, 700, 98
25065, V, 1, 1, 1, 1, 0, 700, 98
25066, V, 1, 1, 1, 1, 0, 700, 98
25067, V, 1, 1, 1, 1, 0, 700, 98
25068, V, 1, 1, 1, 1, 0, 700, 98
25069, V, 1, 0, 0, 1, 0, 700, 98
25069, V, 1, 0, 0, 0, 0, 700, 98
25070, V, 1, 1, 0, 0, 0, 700, 98
25070, V, 1, 1, 0, 0, 0, 700, 98
25071, V, 1, 1, 1, 1, 0, 700, 98
25072, V, 1, 1, 1, 1, 0, 700, 98
25073, V, 1, 1, 1, 1, 0, 700, 98
25074, V, 1, 1, 1, 1, 0, 700, 98
25075, V, 1, 1, 1, 1, 0, 700, 98
25076, V, 1, 1, 1, 1, 0, 700, 98
25077, V, 1, 1, 1, 1, 0, 700, 98
25078, V, 1, 1, 1, 1, 0, 700, 97
25079, V, 1, 1, 1, 1, 0, 700, 97
25080, V, 1, 1, 1, 1, 0, 700, 97
25081, V, 1, 1, 1, 1, 0, 700, 97
25082, V, 1, 1, 1, 1, 0, 700, 98
25083, V, 1, 1, 1, 1, 0, 700, 98
25084, V, 1, 1, 1, 1, 0, 700, 98
25085, V, 1, 1, 1, 1, 0, 700, 98
25086, V, 1, 1, 1, 1, 0, 700, 98
25088, V, 1, 1, 1, 1, 0, 700, 98
25089, V, 1, 1, 1, 1, 0, 700, 98
25090, V, 1, 1, 1, 1, 0, 700, 98
25091, V, 1, 1, 1, 1, 0, 700, 98
25092, V, 1, 1, 1, 1, 0, 700, 98
25093, V, 1, 1, 1, 1, 0, 700, 98
25094, V, 1, 1, 1, 1, 0, 700, 98
25095, V, 1, 1, 1, 1, 0, 700, 98
25096, V, 1, 1, 1, 1, 0, 700, 98
25097, V, 1, 1, 1, 1, 0, 700, 98
25098, V, 1, 1, 1, 1, 0, 700, 98
25099, V, 1, 1, 1, 1, 0, 700, 98
25100, V, 1, 1, 1, 1, 0, 700, 98
25101, V, 1, 1, 1, 1, 0, 700, 98
25102, V, 1, 1, 1, 1, 0, 700, 98
25103, V, 1, 1, 1, 1, 0, 700, 98
25104, V, 1, 1, 1, 1, 0, 700, 98
25105, V, 1, 1, 1, 1, 0, 700, 98
25106, V, 1, 1, 1, 1, 0, 700, 98
25107, V, 1, 1, 1, 1, 0, 700, 98
25108, V, 1, 1, 1, 1, 0, 700, 98
25109, V, 1, 1, 1, 1, 0, 700, 98
25110, V, 1, 1, 1, 1, 0, 700, 98
25111, V, 1, 1, 1, 1, 0, 700, 98
25112, V, 1, 1, 1, 1, 0, 700, 98
25113, V, 1, 1, 1, 1, 0, 700, 98
25114, V, 1, 1, 1, 1, 0, 700, 98
25115, V, 1, 1, 1, 1, 0, 700, 98
25116, V, 1, 1, 1, 1, 0, 700, 98
25117, V, 1, 1, 1, 1, 0, 700, 98
25118, V, 1, 1, 1, 1, 0, 700, 98
25119, V, 1, 1, 1, 1, 0, 700, 98
25120, V, 1, 1, 1, 1, 0, 700, 98
25121, V, 1, 1, 1, 1, 0, 700, 98
25122, V, 1, 1, 1, 1, 0, 700, 98
25123, V, 1, 1, 1, 1, 0, 700, 98
25124, V, 1, 1, 1, 1, 0, 700, 98
25125, V, 1, 1, 1, 1, 0, 700, 98
25126, V, 1, 1, 1, 1, 0, 700, 98
25127, V, 1, 1, 1, 1, 0, 700, 98
25128, V, 1, 1, 1, 1, 0, 700, 98
25129, V, 1, 1, 1, 1, 0, 700, 98
25131, V, 1, 1, 1, 1, 0, 700, 98
25132, V, 1, 1, 1, 1, 0, 700, 98
25133, V, 1, 1, 1, 1, 0, 700, 98
25134, V, 1, 1, 1, 1, 0, 700, 98
25135, V, 1, 1, 1, 1, 0, 700, 98
25136, V, 1, 1, 1, 1, 0, 700, 98
25137, V, 1, 1, 1, 1, 0, 700, 98
25138, V, 1, 1, 1, 1, 0, 700, 98
25139, V, 1, 1, 1, 1, 0, 700, 98
25140, V, 1, 1, 1, 1, 0, 700, 98
25141, V, 1, 1, 1, 1, 0, 700, 98
25142, V, 1, 1, 1, 1, 0, 700, 98
25143, V, 1, 1, 1, 1, 0, 700, 98
25144, V, 1, 1, 1, 1, 0, 700, 98
25145, V, 1, 1, 1, 1, 0, 700, 98
25146, V, 1, 1, 1, 1, 0, 700, 98
25147, V, 1, 1, 1, 1, 0, 700, 98
25148, V, 1, 1, 1, 1, 0, 700, 98
25149, V, 1, 1, 1, 1, 0, 700, 98
25150, V, 1, 1, 1, 1, 0, 700, 98
25151, V, 1, 1, 1, 1, 0, 700, 98
25152, V, 1, 1, 1, 1, 0, 700, 98
25153, V, 1, 1, 1, 1, 0, 700, 98
25154, V, 1, 1, 1, 1, 0, 700, 98
25155, V, 1, 1, 1, 1, 0, 700, 98
25156, V, 1, 1, 1, 1, 0, 700, 98
25157, V, 1, 1, 1, 1, 0, 700, 98
25158, V, 1, 1, 1, 1, 0, 700, 98
25159, V, 1, 1, 1, 1, 0, 700, 98
25160, V, 1, 1, 1, 1, 0, 700, 98
25161, V, 1, 1, 1, 1, 0, 700, 98
25162, V, 1, 1, 1, 1, 0, 700, 98
25163, V, 1, 1, 1, 1, 0, 700, 98
25164, V, 1, 1, 1, 1, 0, 700, 98
25165, V, 1, 1, 1, 1, 0, 700, 98
25166, V, 1, 1, 1, 1, 0, 700, 98
25167, V, 1, 1, 1, 1, 0, 700, 98
25168, V, 1, 1, 1, 1, 0, 700, 98
25169, V, 1, 1, 1, 1, 0, 700, 98
25170, V, 1, 1, 1, 1, 0, 700, 98
25171, V, 1, 1, 1, 1, 0, 700, 98
25172, V, 1, 1, 1, 1, 0, 700, 98
25174, V, 1, 1, 1, 1, 0, 700, 98
25175, V, 1, 1, 1, 1, 0, 700, 98
25176, V, 1, 1, 1, 1, 0, 700, 98
25177, V, 1, 1, 1, 1, 0, 700, 98
25178, V, 1, 1, 1, 1, 0, 700, 98
25179, V, 1, 1, 1, 1, 0, 700, 98
25180, V, 1, 1, 1, 1, 0, 700, 98
25181, V, 1, 1, 1, 1, 0, 700, 98
25182, V, 1, 1, 1, 1, 0, 700, 98
25183, V, 1, 1, 1, 1, 0, 700, 98
25184, V, 1, 1, 1, 1, 0, 700, 98
25185, V, 1, 1, 1, 1, 0, 700, 98
25186, V, 1, 1, 1, 1, 0, 700, 98
25187, V, 1, 1, 1, 1, 0, 700, 98
25188, V, 1, 1, 1, 1, 0, 700, 98
25189, V, 1, 1, 1, 1, 0, 700, 98
25190, V, 1, 1, 1, 1, 0, 700, 98
25191, V, 1, 1, 1, 1, 0, 700, 98
25192, V, 1, 1, 1, 1, 0, 700, 98
25193, V, 1, 1, 1, 1, 0, 700, 98
25194, V, 1, 1, 1, 1, 0, 700, 98
25195, V, 1, 1, 1, 1, 0, 700, 98
25196, V, 1, 1, 1, 1, 0, 700, 98
25197, V, 1, 1, 1, 1, 0, 700, 98
25198, V, 1, 1, 1, 1, 0, 700, 98
25199, V, 1, 1, 1, 1, 0, 700, 98
25200, V, 1, 1, 1, 1, 0, 700, 98
25201, V, 1, 1, 1, 1, 0, 700, 98
25202, V, 1, 1, 1, 1, 0, 700, 98
25203, V, 1, 1, 1, 1, 0, 700, 98
25204, V, 1, 1, 1, 1, 0, 700, 98
25205, V, 1, 1, 1, 1, 0, 700, 98
25206, V, 1, 1, 1, 1, 0, 700, 98
25207, V, 1, 1, 1, 1, 0, 700, 98
25208, V, 1, 1, 1, 1, 0, 700, 98
25209, V, 1, 1, 1, 1, 0, 700, 98
25210, V, 1, 1, 1, 1, 0, 700, 98
25211, V, 1, 1, 1, 1, 0, 700, 98
25212, V, 1, 1, 1, 1, 0, 700, 98
25213, V, 1, 1, 1, 1, 0, 700, 98
25214, V, 1, 1, 1, 1, 0, 700, 98
25216, V, 1, 1, 1, 1, 0, 700, 98
25217, V, 1, 1, 1, 1, 0, 700, 98
25218, V, 1, 1, 1, 1, 0, 700, 98
25219, V, 1, 1, 1, 1, 0, 700, 98
25220, V, 1, 1, 1, 1, 0, 700, 98
25221, V, 1, 1, 1, 1, 0, 700, 98
25222, V, 1, 1, 1, 1, 0, 700, 98
25223, V, 1, 1, 1, 1, 0, 700, 98
25224, V, 1, 1, 1, 1, 0, 700, 98
25225, V, 1, 1, 1, 1, 0, 700, 98
25226, V, 1, 1, 1, 1, 0, 700, 98
25227, V, 1, 1, 1, 1, 0, 700, 98
25228, V, 1, 1, 1, 1, 0, 700, 98
25229, V, 1, 1, 1, 1, 0, 700, 98
25230, V, 1, 1, 1, 1, 0, 700, 98
25231, V, 1, 1, 1, 1, 0, 700, 98
25232, V, 1, 1, 1, 1, 0, 700, 98
25233, V, 1, 1, 1, 1, 0, 700, 98
25234, V, 1, 1, 1, 1, 0, 700, 98
25235, V, 1, 1, 1, 1, 0, 700, 98
25236, V, 1, 1, 1, 1, 0, 700, 98
25237, V, 1, 1, 1, 1, 0, 700, 98
25238, V, 1, 1, 1, 1, 0, 700, 98
25239, V, 1, 1, 1, 1, 0, 700, 98
25240, V, 1, 1, 1, 1, 0, 700, 98
25241, V, 1, 1, 1, 1, 0, 700, 98
25242, V, 1, 1, 1, 1, 0, 700, 98
25243, V, 1, 1, 1, 1, 0, 700, 98
25244, V, 1, 1, 1, 1, 0, 700, 98
25245, V, 1, 1, 1, 1, 0, 700, 98
25246, V, 1, 1, 1, 1, 0, 700, 98
25247, V, 1, 1, 1, 1, 0, 700, 98
25248, V, 1, 1, 1, 1, 0, 700, 98
25249, V, 1, 1, 1, 1, 0, 700, 98
25250, V, 1, 1, 1, 1, 0, 700, 98
25251, V, 1, 1, 1, 1, 0, 700, 98
25252, V, 1, 1, 1, 1, 0, 700, 98
25253, V, 1, 1, 1, 1, 0, 700, 98
25254, V, 1, 1, 1, 1, 0, 700, 98
25255, V, 1, 1, 1, 1, 0, 700, 98
25256, V, 1, 1, 1, 1, 0, 700, 98
25257, V, 1, 1, 1, 1, 0, 700, 98
25259, V, 1, 1, 1, 1, 0, 700, 98
25260, V, 1, 1, 1, 1, 0, 700, 98
25261, V, 1, 1, 1, 1, 0, 700, 98
25262, V, 1, 1, 1, 1, 0, 700, 98
25263, V, 1, 1, 1, 1, 0, 700, 98
25264, V, 1, 1, 1, 1, 0, 700, 98
25265, V, 1, 1, 1, 1, 0, 700, 98
25266, V, 1, 1, 1, 1, 0, 700, 98
25267, V, 1, 1, 1, 1, 0, 700, 98
25268, V, 1, 1, 1, 1, 0, 700, 98
25269, V, 1, 1, 1, 1, 0, 700, 98
25270, V, 1, 1, 1, 1, 0, 700, 98
25271, V, 1, 1, 1, 1, 0, 700, 98
25272, V, 1, 1, 1, 1, 0, 700, 98
25273, V, 1, 1, 1, 1, 0, 700, 98
25274, V, 1, 1, 1, 1, 0, 700, 98
25275, V, 1, 1, 1, 1, 0, 700, 98
25276, V, 1, 1, 1, 1, 0, 700, 98
25277, V, 1, 1, 1, 1, 0, 700, 98
25278, V, 1, 1, 1, 1, 0, 700, 98
25279, V, 1, 1, 1, 1, 0, 700, 98
25280, V, 1, 1, 1, 1, 0, 700, 98
25281, V, 1, 1, 1, 1, 0, 700, 98
25282, V, 1, 1, 1, 1, 0, 700, 98
25283, V, 1, 1, 1, 1, 0, 700, 98
25284, V, 1, 1, 1, 1, 0, 700, 98
25285, V, 1, 1, 1, 1, 0, 700, 98
25286, V, 1, 1, 1, 1, 0, 700, 98
25287, V, 1, 1, 1, 1, 0, 700, 98
25288, V, 1, 1, 1, 1, 0, 700, 98
25289, V, 1, 1, 1, 1, 0, 700, 98
25290, V, 1, 1, 1, 1, 0, 700, 98
25291, V, 1, 1, 1, 1, 0, 700, 98
25292, V, 1, 1, 1, 1, 0, 700, 98
25293, V, 1, 1, 1, 1, 0, 700, 98
25294, V, 1, 1, 1, 1, 0, 700, 98
25295, V, 1, 1, 1, 1, 0, 700, 98
25296, V, 1, 1, 1, 1, 0, 700, 98
25297, V, 1, 1, 1, 1, 0, 700, 98
25298, V, 1, 1, 1, 1, 0, 700, 98
25299, V, 1, 1, 1, 1, 0, 700, 98
25300, V, 1, 1, 1, 1, 0, 700, 98
25302, V, 1, 1, 1, 1, 0, 700, 98
25303, V, 1, 1, 1, 1, 0, 700, 98
25304, V, 1, 1, 1, 1, 0, 700, 98
25305, V, 1, 1, 1, 1, 0, 700, 98
25306, V, 1, 1, 1, 1, 0, 700, 98
25307, V, 1, 1, 1, 1, 0, 700, 98
25308, V, 1, 1, 1, 1, 0, 700, 98
25309, V, 1, 1, 1, 1, 0, 700, 98
25310, V, 1, 1, 1, 1, 0, 700, 98
25311, V, 1, 1, 1, 1, 0, 700, 98
25312, V, 1, 1, 1, 1, 0, 700, 98
25313, V, 1, 1, 1, 1, 0, 700, 98
25314, V, 1, 1, 1, 1, 0, 700, 98
25315, V, 1, 1, 1, 1, 0, 700, 98
25316, V, 1, 1, 1, 1, 0, 700, 98
25317, V, 1, 1, 1, 1, 0, 700, 98
25318, V, 1, 1, 1, 1, 0, 700, 98
25319, V, 1, 1, 1, 1, 0, 700, 98
25320, V, 1, 1, 1, 1, 0, 700, 98
25321, V, 1, 1, 1, 1, 0, 700, 98
25322, V, 1, 1, 1, 1, 0, 700, 98
25323, V, 1, 1, 1, 1, 0, 700, 98
25324, V, 1, 1, 1, 1, 0, 700, 98
25325, V, 1, 1, 1, 1, 0, 700, 98
25326, V, 1, 1, 1, 1, 0, 700, 98
25327, V, 1, 1, 1, 1, 0, 700, 98
25328, V, 1, 1, 1, 1, 0, 700, 98
25329, V, 1, 1, 1, 1, 0, 700, 98
25330, V, 1, 1, 1, 1, 0, 700, 98
25331, V, 1, 1, 1, 1, 0, 700, 98
25332, V, 1, 1, 1, 1, 0, 700, 98
25333, V, 1, 1, 1, 1, 0, 700, 98
25334, V, 1, 1, 1, 1, 0, 700, 98
25335, V, 1, 1, 1, 1, 0, 700, 98
25336, V, 1, 1, 1, 1, 0, 700, 98
25337, V, 1, 1, 1, 1, 0, 700, 98
25338, V, 1, 1, 1, 1, 0, 700, 98
25339, V, 1, 1, 1, 1, 0, 700, 98
25340, V, 1, 1, 1, 1, 0, 700, 98
25341, V, 1, 1, 1, 1, 0, 700, 98
25342, V, 1, 1, 1, 1, 0, 700, 98
25344, V, 1, 1, 1, 1, 0, 700, 98
25345, V, 1, 1, 1, 1, 0, 700, 98
25346, V, 1, 1, 1, 1, 0, 700, 98
25347, V, 1, 1, 1, 1, 0, 700, 98
25348, V, 1, 1, 1, 1, 0, 700, 98
25349, V, 1, 1, 1, 1, 0, 700, 98
25350, V, 1, 1, 1, 1, 0, 700, 98
25351, V, 1, 1, 1, 1, 0, 700, 98
25352, V, 1, 1, 1, 1, 0, 700, 98
25353, V, 1, 1, 1, 1, 0, 700, 98
25354, V, 1, 1, 1, 1, 0, 700, 98
25355, V, 1, 1, 1, 1, 0, 700, 98
25356, V, 1, 1, 1, 1, 0, 700, 98
25357, V, 1, 1, 1, 1, 0, 700, 98
25358, V, 1, 1, 1, 1, 0, 700, 98
25359, V, 1, 1, 1, 1, 0, 700, 98
25360, V, 1, 1, 1, 1, 0, 700, 98
25361, V, 1, 1, 1, 1, 0, 700, 98
25362, V, 1, 1, 1, 1, 0, 700, 98
25363, V, 1, 1, 1, 1, 0, 700, 98
25364, V, 1, 1, 1, 1, 0, 700, 98
25365, V, 1, 1, 1, 1, 0, 700, 98
25366, V, 1, 1, 1, 1, 0, 700, 98
25367, V, 1, 1, 1, 1, 0, 700, 98
25368, V, 1, 1, 1, 1, 0, 700, 98
25369, V, 1, 1, 1, 1, 0, 700, 98
25370, V, 1, 1, 1, 1, 0, 700, 98
25371, V, 1, 1, 1, 1, 0, 700, 98
25372, V, 1, 1, 1, 1, 0, 700, 98
25373, V, 1, 1, 1, 1, 0, 700, 98
25374, V, 1, 1, 1, 1, 0, 700, 98
25375, V, 1, 1, 1, 1, 0, 700, 98
25376, V, 1, 1, 1, 1, 0, 700, 98
25377, V, 1, 1, 1, 1, 0, 700, 98
25378, V, 1, 1, 1, 1, 0, 700, 98
25379, V, 1, 1, 1, 1, 0, 700, 98
25380, V, 1, 1, 1, 1, 0, 700, 98
25381, V, 1, 1, 1, 1, 0, 700, 98
25382, V, 1, 1, 1, 1, 0, 700, 98
25383, V, 1, 1, 1, 1, 0, 700, 98
25384, V, 1, 1, 1, 1, 0, 700, 98
25385, V, 1, 1, 1, 1, 0, 700, 98
25387, V, 1, 1, 1, 1, 0, 700, 98
25388, V, 1, 1, 1, 1, 0, 700, 98
25389, V, 1, 1, 1, 1, 0, 700, 98
25390, V, 1, 1, 1, 1, 0, 700, 98
25391, V, 1, 1, 1, 1, 0, 700, 98
25392, V, 1, 1, 1, 1, 0, 700, 98
25393, V, 1, 1, 1, 1, 0, 700, 98
25394, V, 1, 1, 1, 1, 0, 700, 98
25395, V, 1, 1, 1, 1, 0, 700, 98
25396, V, 1, 1, 1, 1, 0, 700, 98
25397, V, 1, 1, 1, 1, 0, 700, 98
25398, V, 1, 1, 1, 1, 0, 700, 98
25399, V, 1, 1, 1, 1, 0, 700, 98
25400, V, 1, 1, 1, 1, 0, 700, 98
25401, V, 1, 1, 1, 1, 0, 700, 98
25402, V, 1, 1, 1, 1, 0, 700, 98
25403, V, 1, 1, 1, 1, 0, 700, 98
25404, V, 1, 1, 1, 1, 0, 700, 98
25405, V, 1, 1, 1, 1, 0, 700, 98
25406, V, 1, 1, 1, 1, 0, 700, 98
25407, V, 1, 1, 1, 1, 0, 700, 98
25408, V, 1, 1, 1, 1, 0, 700, 98
25409, V, 1, 1, 1, 1, 0, 700, 98
25410, V, 1, 1, 1, 1, 0, 700, 98
25411, V, 1, 1, 1, 1, 0, 700, 98
25412, V, 1, 1, 1, 1, 0, 700, 98
25413, V, 1, 1, 1, 1, 0, 700, 98
25414, V, 1, 1, 1, 1, 0, 700, 98
25415, V, 1, 1, 1, 1, 0, 700, 98
25416, V, 1, 1, 1, 1, 0, 700, 98
25417, V, 1, 1, 1, 1, 0, 700, 98
25418, V, 1, 1, 1, 1, 0, 700, 98
25419, V, 1, 1, 1, 1, 0, 700, 98
25420, V, 1, 1, 1, 1, 0, 700, 98
25421, V, 1, 1, 1, 1, 0, 700, 98
25422, V, 1, 1, 1, 1, 0, 700, 98
25423, V, 1, 1, 1, 1, 0, 700, 98
25424, V, 1, 1, 1, 1, 0, 700, 98
25425, V, 1, 1, 1, 1, 0, 700, 98
25426, V, 1, 1, 1, 1, 0, 700, 98
25427, V, 1, 1, 1, 1, 0, 700, 98
25428, V, 1, 1, 1, 1, 0, 700, 98
25430, V, 1, 1, 1, 1, 0, 700, 98
25431, V, 1, 1, 1, 1, 0, 700, 98
25432, V, 1, 1, 1, 1, 0, 700, 98
25433, V, 1, 1, 1, 1, 0, 700, 98
25434, V, 1, 1, 1, 1, 0, 700, 98
25435, V, 1, 1, 1, 1, 0, 700, 98
25436, V, 1, 1, 1, 1, 0, 700, 98
25437, V, 1, 1, 1, 1, 0, 700, 98
25438, V, 1, 1, 1, 1, 0, 700, 98
25439, V, 1, 1, 1, 1, 0, 700, 98
25440, V, 1, 1, 1, 1, 0, 700, 98
25441, V, 1, 1, 1, 1, 0, 700, 98
25442, V, 1, 1, 1, 1, 0, 700, 98
25443, V, 1, 1, 1, 1, 0, 700, 98
25444, V, 1, 1, 1, 1, 0, 700, 98
25445, V, 1, 1, 1, 1, 0, 700, 98
25446, V, 1, 1, 1, 1, 0, 700, 98
25447, V, 1, 1, 1, 1, 0, 700, 98
25448, V, 1, 1, 1, 1, 0, 700, 98
25449, V, 1, 1, 1, 1, 0, 700, 98
25450, V, 1, 1, 1, 1, 0, 700, 98
25451, V, 1, 1, 1, 1, 0, 700, 98
25452, V, 1, 1, 1, 1, 0, 700, 98
25453, V, 1, 1, 1, 1, 0, 700, 98
25454, V, 1, 1, 1, 1, 0, 700, 98
25455, V, 1, 1, 1, 1, 0, 700, 98
25456, V, 1, 1, 1, 1, 0, 700, 98
25457, V, 1, 1, 1, 1, 0, 700, 98
25458, V, 1, 1, 1, 1, 0, 700, 98
25459, V, 1, 1, 1, 1, 0, 700, 98
25460, V, 1, 1, 1, 1, 0, 700, 98
25461, V, 1, 1, 1, 1, 0, 700, 98
25462, V, 1, 1, 1, 1, 0, 700, 98
25463, V, 1, 1, 1, 1, 0, 700, 98
25464, V, 1, 1, 1, 1, 0, 700, 98
25465, V, 1, 1, 1, 1, 0, 700, 98
25466, V, 1, 1, 1, 1, 0, 700, 98
25467, V, 1, 1, 1, 1, 0, 700, 98
25468, V, 1, 1, 1, 1, 0, 700, 98
25469, V, 1, 1, 1, 1, 0, 700, 98
25470, V, 1, 1, 1, 1, 0, 700, 98
25472, V, 1, 1, 1, 1, 0, 700, 98
25473, V, 1, 1, 1, 1, 0, 700, 98
25474, V, 1, 1, 1, 1, 0, 700, 98
25475, V, 1, 1, 1, 1, 0, 700, 98
25476, V, 1, 1, 1, 1, 0, 700, 98
25477, V, 1, 1, 1, 1, 0, 700, 98
25478, V, 1, 1, 1, 1, 0, 700, 98
25479, V, 1, 1, 1, 1, 0, 700, 98
25480, V, 1, 1, 1, 1, 0, 700, 98
25481, V, 1, 1, 1, 1, 0, 700, 98
25482, V, 1, 1, 1, 1, 0, 700, 98
25483, V, 1, 1, 1, 1, 0, 700, 98
25484, V, 1, 1, 1, 1, 0, 700, 98
25485, V, 1, 1, 1, 1, 0, 700, 98
25486, V, 1, 1, 1, 1, 0, 700, 98
25487, V, 1, 1, 1, 1, 0, 700, 98
25488, V, 1, 1, 1, 1, 0, 700, 98
25489, V, 1, 1, 1, 1, 0, 700, 98
25490, V, 1, 1, 1, 1, 0, 700, 98
25491, V, 1, 1, 1, 1, 0, 700, 98
25492, V, 1, 1, 1, 1, 0, 700, 98
25493, V, 1, 1, 1, 1, 0, 700, 98
25494, V, 1, 1, 1, 1, 0, 700, 98
25495, V, 1, 1, 1, 1, 0, 700, 98
25496, V, 1, 1, 1, 1, 0, 700, 98
25497, V, 1, 1, 1, 1, 0, 700, 98
25498, V, 1, 1, 1, 1, 0, 700, 98
25499, V, 1, 1, 1, 1, 0, 700, 98
25500, V, 1, 1, 1, 1, 0, 700, 98
25501, V, 1, 1, 1, 1, 0, 700, 98
25502, V, 1, 1, 1, 1, 0, 700, 98
25503, V, 1, 1, 1, 1, 0, 700, 98
25504, V, 1, 1, 1, 1, 0, 700, 98
25505, V, 1, 1, 1, 1, 0, 700, 98
25506, V, 1, 1, 1, 1, 0, 700, 98
25507, V, 1, 1, 1, 1, 0, 700, 98
25508, V, 1, 1, 1, 1, 0, 700, 98
25509, V, 1, 1, 1, 1, 0, 700, 98
25510, V, 1, 1, 1, 1, 0, 700, 98
25511, V, 1, 1, 1, 1, 0, 700, 98
25512, V, 1, 1, 1, 1, 0, 700, 98
25513, V, 1, 1, 1, 1, 0, 700, 98
25515, V, 1, 1, 1, 1, 0, 700, 98
25516, V, 1, 1, 1, 1, 0, 700, 98
25517, V, 1, 1, 1, 1, 0, 700, 98
25518, V, 1, 1, 1, 1, 0, 700, 98
25519, V, 1, 1, 1, 1, 0, 700, 98
25520, V, 1, 1, 1, 1, 0, 700, 98
25521, V, 1, 1, 1, 1, 0, 700, 98
25522, V, 1, 1, 1, 1, 0, 700, 98
25523, V, 1, 1, 1, 1, 0, 700, 98
25524, V, 1, 1, 1, 1, 0, 700, 98
25525, V, 1, 1, 1, 1, 0, 700, 98
25526, V, 1, 1, 1, 1, 0, 700, 98
25527, V, 1, 1, 1, 1, 0, 700, 98
25528, V, 1, 1, 1, 1, 0, 700, 98
25529, V, 1, 1, 1, 1, 0, 700, 98
25530, V, 1, 1, 1, 1, 0, 700, 98
25531, V, 1, 1, 1, 1, 0, 700, 98
25532, V, 1, 1, 1, 1, 0, 700, 98
25533, V, 1, 1, 1, 1, 0, 700, 98
25534, V, 1, 1, 1, 1, 0, 700, 98
25535, V, 1, 1, 1, 1, 0, 700, 98
25536, V, 1, 1, 1, 1, 0, 700, 98
25537, V, 1, 1, 1, 1, 0, 700, 98
25538, V, 1, 1, 1, 1, 0, 700, 98
25539, V, 1, 1, 1, 1, 0, 700, 98
25540, V, 1, 1, 1, 1, 0, 700, 98
25541, V, 1, 1, 1, 1, 0, 700, 98
25542, V, 1, 1, 1, 1, 0, 700, 98
25543, V, 1, 1, 1, 1, 0, 700, 98
25544, V, 1, 1, 1, 1, 0, 700, 98
25545, V, 1, 1, 1, 1, 0, 700, 98
25546, V, 1, 1, 1, 1, 0, 700, 98
25547, V, 1, 1, 1, 1, 0, 700, 98
25548, V, 1, 1, 1, 1, 0, 700, 98
25549, V, 1, 1, 1, 1, 0, 700, 98
25550, V, 1, 1, 1, 1, 0, 700, 98
25551, V, 1, 1, 1, 1, 0, 700, 98
25552, V, 1, 1, 1, 1, 0, 700, 98
25553, V, 1, 1, 1, 1, 0, 700, 98
25554, V, 1, 1, 1, 1, 0, 700, 98
25555, V, 1, 1, 1, 1, 0, 700, 98
25556, V, 1, 1, 1, 1, 0, 700, 98
25558, V, 1, 1, 1, 1, 0, 700, 98
25559, V, 1, 1, 1, 1, 0, 700, 98
25560, V, 1, 1, 1, 1, 0, 700, 98
25561, V, 1, 1, 1, 1, 0, 700, 98
25562, V, 1, 0, 0, 1, 0, 700, 98
25562, V, 1, 0, 0, 0, 0, 700, 98
25563, V, 1, 1, 0, 0, 0, 700, 98
25563, V, 1, 1, 0, 0, 0, 700, 98
25564, V, 1, 1, 1, 1, 0, 700, 98
25565, V, 1, 1, 1, 1, 0, 700, 98
25566, V, 1, 1, 1, 1, 0, 700, 98
25567, V, 1, 1, 1, 1, 0, 700, 98
25568, V, 1, 1, 1, 1, 0, 700, 98
25569, V, 1, 1, 1, 1, 0, 700, 98
25570, V, 1, 1, 1, 1, 0, 700, 97
25571, V, 1, 1, 1, 1, 0, 700, 97
25572, V, 1, 1, 1, 1, 0, 700, 97
25573, V, 1, 1, 1, 1, 0, 700, 97
25574, V, 1, 1, 1, 1, 0, 700, 97
25575, V, 1, 1, 1, 1, 0, 700, 97
25576, V, 1, 1, 1, 1, 0, 700, 97
25577, V, 1, 1, 1, 1, 0, 700, 97
25578, V, 1, 1, 1, 1, 0, 700, 97
25579, V, 1, 1, 1, 1, 0, 700, 97
25580, V, 1, 1, 1, 1, 0, 700, 97
25581, V, 1, 1, 1, 1, 0, 700, 97
25582, V, 1, 1, 1, 1, 0, 700, 97
25583, V, 1, 1, 1, 1, 0, 700, 98
25584, V, 1, 1, 1, 1, 0, 700, 98
25585, V, 1, 1, 1, 1, 0, 700, 98
25586, V, 1, 1, 1, 1, 0, 700, 98
25587, V, 1, 1, 1, 1, 0, 700, 98
25588, V, 1, 1, 1, 1, 0, 700, 98
25589, V, 1, 1, 1, 1, 0, 700, 98
25590, V, 1, 1, 1, 1, 0, 700, 98
25591, V, 1, 1, 1, 1, 0, 700, 98
25592, V, 1, 1, 1, 1, 0, 700, 98
25593, V, 1, 1, 1, 1, 0, 700, 98
25594, V, 1, 1, 1, 1, 0, 700, 98
25595, V, 1, 1, 1, 1, 0, 700, 98
25596, V, 1, 1, 1, 1, 0, 700, 98
25597, V, 1, 1, 1, 1, 0, 700, 98
25598, V, 1, 1, 1, 1, 0, 700, 98
25600, V, 1, 1, 1, 1, 0, 700, 98
25601, V, 1, 1, 1, 1, 0, 700, 98
25602, V, 1, 1, 1, 1, 0, 700, 98
25603, V, 1, 1, 1, 1, 0, 700, 98
25604, V, 1, 1, 1, 1, 0, 700, 98
25605, V, 1, 1, 1, 1, 0, 700, 98
25606, V, 1, 1, 1, 1, 0, 700, 98
25607, V, 1, 1, 1, 1, 0, 700, 98
25608, V, 1, 1, 1, 1, 0, 700, 98
25609, V, 1, 1, 1, 1, 0, 700, 98
25610, V, 1, 1, 1, 1, 0, 700, 98
25611, V, 1, 1, 1, 1, 0, 700, 98
25612, V, 1, 1, 1, 1, 0, 700, 98
25613, V, 1, 1, 1, 1, 0, 700, 98
25614, V, 1, 1, 1, 1, 0, 700, 98
25615, V, 1, 1, 1, 1, 0, 700, 98
25616, V, 1, 1, 1, 1, 0, 700, 98
25617, V, 1, 1, 1, 1, 0, 700, 98
25618, V, 1, 1, 1, 1, 0, 700, 98
25619, V, 1, 1, 1, 1, 0, 700, 98
25620, V, 1, 1, 1, 1, 0, 700, 98
25621, V, 1, 1, 1, 1, 0, 700, 98
25622, V, 1, 1, 1, 1, 0, 700, 98
25623, V, 1, 1, 1, 1, 0, 700, 98
25624, V, 1, 1, 1, 1, 0, 700, 98
25625, V, 1, 1, 1, 1, 0, 700, 98
25626, V, 1, 1, 1, 1, 0, 700, 98
25627, V, 1, 1, 1, 1, 0, 700, 98
25628, V, 1, 1, 1, 1, 0, 700, 98
25629, V, 1, 1, 1, 1, 0, 700, 98
25630, V, 1, 1, 1, 1, 0, 700, 98
25631, V, 1, 1, 1, 1, 0, 700, 98
25632, V, 1, 1, 1, 1, 0, 700, 98
25633, V, 1, 1, 1, 1, 0, 700, 98
25634, V, 1, 1, 1, 1, 0, 700, 98
25635, V, 1, 1, 1, 1, 0, 700, 98
25636, V, 1, 1, 1, 1, 0, 700, 98
25637, V, 1, 1, 1, 1, 0, 700, 98
25638, V, 1, 1, 1, 1, 0, 700, 98
25639, V, 1, 1, 1, 1, 0, 700, 98
25640, V, 1, 1, 1, 1, 0, 700, 98
25641, V, 1, 1, 1, 1, 0, 700, 98
25643, V, 1, 1, 1, 1, 0, 700, 98
25644, V, 1, 1, 1, 1, 0, 700, 98
25645, V, 1, 1, 1, 1, 0, 700, 98
25646, V, 1, 1, 1, 1, 0, 700, 98
25647, V, 1, 1, 1, 1, 0, 700, 98
25648, V, 1, 1, 1, 1, 0, 700, 98
25649, V, 1, 1, 1, 1, 0, 700, 98
25650, V, 1, 1, 1, 1, 0, 700, 98
25651, V, 1, 1, 1, 1, 0, 700, 98
25652, V, 1, 1, 1, 1, 0, 700, 98
25653, V, 1, 1, 1, 1, 0, 700, 98
25654, V, 1, 1, 1, 1, 0, 700, 98
25655, V, 1, 1, 1, 1, 0, 700, 98
25656, V, 1, 1, 1, 1, 0, 700, 98
25657, V, 1, 1, 1, 1, 0, 700, 98
25658, V, 1, 1, 1, 1, 0, 700, 98
25659, V, 1, 1, 1, 1, 0, 700, 98
25660, V, 1, 1, 1, 1, 0, 700, 98
25661, V, 1, 1, 1, 1, 0, 700, 98
25662, V, 1, 1, 1, 1, 0, 700, 98
25663, V, 1, 1, 1, 1, 0, 700, 98
25664, V, 1, 1, 1, 1, 0, 700, 98
25665, V, 1, 1, 1, 1, 0, 700, 98
25666, V, 1, 1, 1, 1, 0, 700, 98
25667, V, 1, 1, 1, 1, 0, 700, 98
25668, V, 1, 1, 1, 1, 0, 700, 98
25669, V, 1, 1, 1, 1, 0, 700, 98
25670, V, 1, 1, 1, 1, 0, 700, 98
25671, V, 1, 1, 1, 1, 0, 700, 98
25672, V, 1, 1, 1, 1, 0, 700, 98
25673, V, 1, 1, 1, 1, 0, 700, 98
25674, V, 1, 1, 1, 1, 0, 700, 98
25675, V, 1, 1, 1, 1, 0, 700, 98
25676, V, 1, 1, 1, 1, 0, 700, 98
25677, V, 1, 1, 1, 1, 0, 700, 98
25678, V, 1, 1, 1, 1, 0, 700, 98
25679, V, 1, 1, 1, 1, 0, 700, 98
25680, V, 1, 1, 1, 1, 0, 700, 98
25681, V, 1, 1, 1, 1, 0, 700, 98
25682, V, 1, 1, 1, 1, 0, 700, 98
25683, V, 1, 1, 1, 1, 0, 700, 98
25684, V, 1, 1, 1, 1, 0, 700, 98
25686, V, 1, 1, 1, 1, 0, 700, 98
25687, V, 1, 1, 1, 1, 0, 700, 98
25688, V, 1, 1, 1, 1, 0, 700, 98
25689, V, 1, 1, 1, 1, 0, 700, 98
25690, V, 1, 1, 1, 1, 0, 700, 98
25691, V, 1, 1, 1, 1, 0, 700, 98
25692, V, 1, 1, 1, 1, 0, 700, 98
25693, V, 1, 1, 1, 1, 0, 700, 98
25694, V, 1, 1, 1, 1, 0, 700, 98
25695, V, 1, 1, 1, 1, 0, 700, 98
25696, V, 1, 1, 1, 1, 0, 700, 98
25697, V, 1, 1, 1, 1, 0, 700, 98
25698, V, 1, 1, 1, 1, 0, 700, 98
25699, V, 1, 1, 1, 1, 0, 700, 98
25700, V, 1, 1, 1, 1, 0, 700, 98
25701, V, 1, 1, 1, 1, 0, 700, 98
25702, V, 1, 1, 1, 1, 0, 700, 98
25703, V, 1, 1, 1, 1, 0, 700, 98
25704, V, 1, 1, 1, 1, 0, 700, 98
25705, V, 1, 1, 1, 1, 0, 700, 98
25706, V, 1, 1, 1, 1, 0, 700, 98
25707, V, 1, 1, 1, 1, 0, 700, 98
25708, V, 1, 1, 1, 1, 0, 700, 98
25709, V, 1, 1, 1, 1, 0, 700, 98
25710, V, 1, 1, 1, 1, 0, 700, 98
25711, V, 1, 1, 1, 1, 0, 700, 98
25712, V, 1, 1, 1, 1, 0, 700, 98
25713, V, 1, 1, 1, 1, 0, 700, 98
25714, V, 1, 1, 1, 1, 0, 700, 98
25715, V, 1, 1, 1, 1, 0, 700, 98
25716, V, 1, 1, 1, 1, 0, 700, 98
25717, V, 1, 1, 1, 1, 0, 700, 98
25718, V, 1, 1, 1, 1, 0, 700, 98
25719, V, 1, 1, 1, 1, 0, 700, 98
25720, V, 1, 1, 1, 1, 0, 700, 98
25721, V, 1, 1, 1, 1, 0, 700, 98
25722, V, 1, 1, 1, 1, 0, 700, 98
25723, V, 1, 1, 1, 1, 0, 700, 98
25724, V, 1, 1, 1, 1, 0, 700, 98
25725, V, 1, 1, 1, 1, 0, 700, 98
25726, V, 1, 1, 1, 1, 0, 700, 98
25728, V, 1, 1, 1, 1, 0, 700, 98
25729, V, 1, 1, 1, 1, 0, 700, 98
25730, V, 1, 1, 1, 1, 0, 700, 98
25731, V, 1, 1, 1, 1, 0, 700, 98
25732, V, 1, 1, 1, 1, 0, 700, 98
25733, V, 1, 1, 1, 1, 0, 700, 98
25734, V, 1, 1, 1, 1, 0, 700, 98
25735, V, 1, 1, 1, 1, 0, 700, 98
25736, V, 1, 1, 1, 1, 0, 700, 98
25737, V, 1, 1, 1, 1, 0, 700, 98
25738, V, 1, 1, 1, 1, 0, 700, 98
25739, V, 1, 1, 1, 1, 0, 700, 98
25740, V, 1, 1, 1, 1, 0, 700, 98
25741, V, 1, 1, 1, 1, 0, 700, 98
25742, V, 1, 1, 1, 1, 0, 700, 98
25743, V, 1, 1, 1, 1, 0, 700, 98
25744, V, 1, 1, 1, 1, 0, 700, 98
25745, V, 1, 1, 1, 1, 0, 700, 98
25746, V, 1, 1, 1, 1, 0, 700, 98
25747, V, 1, 1, 1, 1, 0, 700, 98
25748, V, 1, 1, 1, 1, 0, 700, 98
25749, V, 1, 1, 1, 1, 0, 700, 98
25750, V, 1, 1, 1, 1, 0, 700, 98
25751, V, 1, 1, 1, 1, 0, 700, 98
25752, V, 1, 1, 1, 1, 0, 700, 98
25753, V, 1, 1, 1, 1, 0, 700, 98
25754, V, 1, 1, 1, 1, 0, 700, 98
25755, V, 1, 1, 1, 1, 0, 700, 98
25756, V, 1, 1, 1, 1, 0, 700, 98
25757, V, 1, 1, 1, 1, 0, 700, 98
25758, V, 1, 1, 1, 1, 0, 700, 98
25759, V, 1, 1, 1, 1, 0, 700, 98
25760, V, 1, 1, 1, 1, 0, 700, 98
25761, V, 1, 1, 1, 1, 0, 700, 98
25762, V, 1, 1, 1, 1, 0, 700, 98
25763, V, 1, 1, 1, 1, 0, 700, 98
25764, V, 1, 1, 1, 1, 0, 700, 98
25765, V, 1, 1, 1, 1, 0, 700, 98
25766, V, 1, 1, 1, 1, 0, 700, 98
25767, V, 1, 1, 1, 1, 0, 700, 98
25768, V, 1, 1, 1, 1, 0, 700, 98
25769, V, 1, 1, 1, 1, 0, 700, 98
25771, V, 1, 1, 1, 1, 0, 700, 98
25772, V, 1, 1, 1, 1, 0, 700, 98
25773, V, 1, 1, 1, 1, 0, 700, 98
25774, V, 1, 1, 1, 1, 0, 700, 98
25775, V, 1, 1, 1, 1, 0, 700, 98
25776, V, 1, 1, 1, 1, 0, 700, 98
25777, V, 1, 1, 1, 1, 0, 700, 98
25778, V, 1, 1, 1, 1, 0, 700, 98
25779, V, 1, 1, 1, 1, 0, 700, 98
25780, V, 1, 1, 1, 1, 0, 700, 98
25781, V, 1, 1, 1, 1, 0, 700, 98
25782, V, 1, 1, 1, 1, 0, 700, 98
25783, V, 1, 1, 1, 1, 0, 700, 98
25784, V, 1, 1, 1, 1, 0, 700, 98
25785, V, 1, 1, 1, 1, 0, 700, 98
25786, V, 1, 1, 1, 1, 0, 700, 98
25787, V, 1, 1, 1, 1, 0, 700, 98
25788, V, 1, 1, 1, 1, 0, 700, 98
25789, V, 1, 1, 1, 1, 0, 700, 98
25790, V, 1, 1, 1, 1, 0, 700, 98
25791, V, 1, 1, 1, 1, 0, 700, 98
25792, V, 1, 1, 1, 1, 0, 700, 98
25793, V, 1, 1, 1, 1, 0, 700, 98
25794, V, 1, 1, 1, 1, 0, 700, 98
25795, V, 1, 1, 1, 1, 0, 700, 98
25796, V, 1, 1, 1, 1, 0, 700, 98
25797, V, 1, 1, 1, 1, 0, 700, 98
25798, V, 1, 1, 1, 1, 0, 700, 98
25799, V, 1, 1, 1, 1, 0, 700, 98
25800, V, 1, 1, 1, 1, 0, 700, 98
25801, V, 1, 1, 1, 1, 0, 700, 98
25802, V, 1, 1, 1, 1, 0, 700, 98
25803, V, 1, 1, 1, 1, 0, 700, 98
25804, V, 1, 1, 1, 1, 0, 700, 98
25805, V, 1, 1, 1, 1, 0, 700, 98
25806, V, 1, 1, 1, 1, 0, 700, 98
25807, V, 1, 1, 1, 1, 0, 700, 98
25808, V, 1, 1, 1, 1, 0, 700, 98
25809, V, 1, 1, 1, 1, 0, 700, 98
25810, V, 1, 1, 1, 1, 0, 700, 98
25811, V, 1, 1, 1, 1, 0, 700, 98
25812, V, 1, 1, 1, 1, 0, 700, 98
25814, V, 1, 1, 1, 1, 0, 700, 98
25815, V, 1, 1, 1, 1, 0, 700, 98
25816, V, 1, 1, 1, 1, 0, 700, 98
25817, V, 1, 1, 1, 1, 0, 700, 98
25818, V, 1, 1, 1, 1, 0, 700, 98
25819, V, 1, 1, 1, 1, 0, 700, 98
25820, V, 1, 1, 1, 1, 0, 700, 98
25821, V, 1, 1, 1, 1, 0, 700, 98
25822, V, 1, 1, 1, 1, 0, 700, 98
25823, V, 1, 1, 1, 1, 0, 700, 98
25824, V, 1, 1, 1, 1, 0, 700, 98
25825, V, 1, 1, 1, 1, 0, 700, 98
25826, V, 1, 1, 1, 1, 0, 700, 98
25827, V, 1, 1, 1, 1, 0, 700, 98
25828, V, 1, 1, 1, 1, 0, 700, 98
25829, V, 1, 1, 1, 1, 0, 700, 98
25830, V, 1, 1, 1, 1, 0, 700, 98
25831, V, 1, 1, 1, 1, 0, 700, 98
25832, V, 1, 1, 1, 1, 0, 700, 98
25833, V, 1, 1, 1, 1, 0, 700, 98
25834, V, 1, 1, 1, 1, 0, 700, 98
25835, V, 1, 1, 1, 1, 0, 700, 98
25836, V, 1, 1, 1, 1, 0, 700, 98
25837, V, 1, 1, 1, 1, 0, 700, 98
25838, V, 1, 1, 1, 1, 0, 700, 98
25839, V, 1, 1, 1, 1, 0, 700, 98
25840, V, 1, 1, 1, 1, 0, 700, 98
25841, V, 1, 1, 1, 1, 0, 700, 98
25842, V, 1, 1, 1, 1, 0, 700, 98
25843, V, 1, 1, 1, 1, 0, 700, 98
25844, V, 1, 1, 1, 1, 0, 700, 98
25845, V, 1, 1, 1, 1, 0, 700, 98
25846, V, 1, 1, 1, 1, 0, 700, 98
25847, V, 1, 1, 1, 1, 0, 700, 98
25848, V, 1, 1, 1, 1, 0, 700, 98
25849, V, 1, 1, 1, 1, 0, 700, 98
25850, V, 1, 1, 1, 1, 0, 700, 98
25851, V, 1, 1, 1, 1, 0, 700, 98
25852, V, 1, 1, 1, 1, 0, 700, 98
25853, V, 1, 1, 1, 1, 0, 700, 98
25854, V, 1, 1, 1, 1, 0, 700, 98
25856, V, 1, 1, 1, 1, 0, 700, 98
25857, V, 1, 1, 1, 1, 0, 700, 98
25858, V, 1, 1, 1, 1, 0, 700, 98
25859, V, 1, 1, 1, 1, 0, 700, 98
25860, V, 1, 1, 1, 1, 0, 700, 98
25861, V, 1, 1, 1, 1, 0, 700, 98
25862, V, 1, 1, 1, 1, 0, 700, 98
25863, V, 1, 1, 1, 1, 0, 700, 98
25864, V, 1, 1, 1, 1, 0, 700, 98
25865, V, 1, 1, 1, 1, 0, 700, 98
25866, V, 1, 1, 1, 1, 0, 700, 98
25867, V, 1, 1, 1, 1, 0, 700, 98
25868, V, 1, 1, 1, 1, 0, 700, 98
25869, V, 1, 1, 1, 1, 0, 700, 98
25870, V, 1, 1, 1, 1, 0, 700, 98
25871, V, 1, 1, 1, 1, 0, 700, 98
25872, V, 1, 1, 1, 1, 0, 700, 98
25873, V, 1, 1, 1, 1, 0, 700, 98
25874, V, 1, 1, 1, 1, 0, 700, 98
25875, V, 1, 1, 1, 1, 0, 700, 98
25876, V, 1, 1, 1, 1, 0, 700, 98
25877, V, 1, 1, 1, 1, 0, 700, 98
25878, V, 1, 1, 1, 1, 0, 700, 98
25879, V, 1, 1, 1, 1, 0, 700, 98
25880, V, 1, 1, 1, 1, 0, 700, 98
25881, V, 1, 1, 1, 1, 0, 700, 98
25882, V, 1, 1, 1, 1, 0, 700, 98
25883, V, 1, 1, 1, 1, 0, 700, 98
25884, V, 1, 1, 1, 1, 0, 700, 98
25885, V, 1, 1, 1, 1, 0, 700, 98
25886, V, 1, 1, 1, 1, 0, 700, 98
25887, V, 1, 1, 1, 1, 0, 700, 98
25888, V, 1, 1, 1, 1, 0, 700, 98
25889, V, 1, 1, 1, 1, 0, 700, 98
25890, V, 1, 1, 1, 1, 0, 700, 98
25891, V, 1, 1, 1, 1, 0, 700, 98
25892, V, 1, 1, 1, 1, 0, 700, 98
25893, V, 1, 1, 1, 1, 0, 700, 98
25894, V, 1, 1, 1, 1, 0, 700, 98
25895, V, 1, 1, 1, 1, 0, 700, 98
25896, V, 1, 1, 1, 1, 0, 700, 98
25897, V, 1, 1, 1, 1, 0, 700, 98
25899, V, 1, 1, 1, 1, 0, 700, 98
25900, V, 1, 1, 1, 1, 0, 700, 98
25901, V, 1, 1, 1, 1, 0, 700, 98
25902, V, 1, 1, 1, 1, 0, 700, 98
25903, V, 1, 1, 1, 1, 0, 700, 98
25904, V, 1, 1, 1, 1, 0, 700, 98
25905, V, 1, 1, 1, 1, 0, 700, 98
25906, V, 1, 1, 1, 1, 0, 700, 98
25907, V, 1, 1, 1, 1, 0, 700, 98
25908, V, 1, 1, 1, 1, 0, 700, 98
25909, V, 1, 1, 1, 1, 0, 700, 98
25910, V, 1, 1, 1, 1, 0, 700, 98
25911, V, 1, 1, 1, 1, 0, 700, 98
25912, V, 1, 1, 1, 1, 0, 700, 98
25913, V, 1, 1, 1, 1, 0, 700, 98
25914, V, 1, 1, 1, 1, 0, 700, 98
25915, V, 1, 1, 1, 1, 0, 700, 98
25916, V, 1, 1, 1, 1, 0, 700, 98
25917, V, 1, 1, 1, 1, 0, 700, 98
25918, V, 1, 1, 1, 1, 0, 700, 98
25919, V, 1, 1, 1, 1, 0, 700, 98
25920, V, 1, 1, 1, 1, 0, 700, 98
25921, V, 1, 1, 1, 1, 0, 700, 98
25922, V, 1, 1, 1, 1, 0, 700, 98
25923, V, 1, 1, 1, 1, 0, 700, 98
25924, V, 1, 1, 1, 1, 0, 700, 98
25925, V, 1, 1, 1, 1, 0, 700, 98
25926, V, 1, 1, 1, 1, 0, 700, 98
25927, V, 1, 1, 1, 1, 0, 700, 98
25928, V, 1, 1, 1, 1, 0, 700, 98
25929, V, 1, 1, 1, 1, 0, 700, 98
25930, V, 1, 1, 1, 1, 0, 700, 98
25931, V, 1, 1, 1, 1, 0, 700, 98
25932, V, 1, 1, 1, 1, 0, 700, 98
25933, V, 1, 1, 1, 1, 0, 700, 98
25934, V, 1, 1, 1, 1, 0, 700, 98
25935, V, 1, 1, 1, 1, 0, 700, 98
25936, V, 1, 1, 1, 1, 0, 700, 98
25937, V, 1, 1, 1, 1, 0, 700, 98
25938, V, 1, 1, 1, 1, 0, 700, 98
25939, V, 1, 1, 1, 1, 0, 700, 98
25940, V, 1, 1, 1, 1, 0, 700, 98
25942, V, 1, 1, 1, 1, 0, 700, 98
25943, V, 1, 1, 1, 1, 0, 700, 98
25944, V, 1, 1, 1, 1, 0, 700, 98
25945, V, 1, 1, 1, 1, 0, 700, 98
25946, V, 1, 1, 1, 1, 0, 700, 98
25947, V, 1, 1, 1, 1, 0, 700, 98
25948, V, 1, 1, 1, 1, 0, 700, 98
25949, V, 1, 1, 1, 1, 0, 700, 98
25950, V, 1, 1, 1, 1, 0, 700, 98
25951, V, 1, 1, 1, 1, 0, 700, 98
25952, V, 1, 1, 1, 1, 0, 700, 98
25953, V, 1, 1, 1, 1, 0, 700, 98
25954, V, 1, 1, 1, 1, 0, 700, 98
25955, V, 1, 1, 1, 1, 0, 700, 98
25956, V, 1, 1, 1, 1, 0, 700, 98
25957, V, 1, 1, 1, 1, 0, 700, 98
25958, V, 1, 1, 1, 1, 0, 700, 98
25959, V, 1, 1, 1, 1, 0, 700, 98
25960, V, 1, 1, 1, 1, 0, 700, 98
25961, V, 1, 1, 1, 1, 0, 700, 98
25962, V, 1, 1, 1, 1, 0, 700, 98
25963, V, 1, 1, 1, 1, 0, 700, 98
25964, V, 1, 1, 1, 1, 0, 700, 98
25965, V, 1, 1, 1, 1, 0, 700, 98
25966, V, 1, 1, 1, 1, 0, 700, 98
25967, V, 1, 1, 1, 1, 0, 700, 98
25968, V, 1, 1, 1, 1, 0, 700, 98
25969, V, 1, 1, 1, 1, 0, 700, 98
25970, V, 1, 1, 1, 1, 0, 700, 98
25971, V, 1, 1, 1, 1, 0, 700, 98
25972, V, 1, 1, 1, 1, 0, 700, 98
25973, V, 1, 1, 1, 1, 0, 700, 98
25974, V, 1, 1, 1, 1, 0, 700, 98
25975, V, 1, 1, 1, 1, 0, 700, 98
25976, V, 1, 1, 1, 1, 0, 700, 98
25977, V, 1, 1, 1, 1, 0, 700, 98
25978, V, 1, 1, 1, 1, 0, 700, 98
25979, V, 1, 1, 1, 1, 0, 700, 98
25980, V, 1, 1, 1, 1, 0, 700, 98
25981, V, 1, 1, 1, 1, 0, 700, 98
25982, V, 1, 1, 1, 1, 0, 700, 98
25984, V, 1, 1, 1, 1, 0, 700, 98
25985, V, 1, 1, 1, 1, 0, 700, 98
25986, V, 1, 1, 1, 1, 0, 700, 98
25987, V, 1, 1, 1, 1, 0, 700, 98
25988, V, 1, 1, 1, 1, 0, 700, 98
25989, V, 1, 1, 1, 1, 0, 700, 98
25990, V, 1, 1, 1, 1, 0, 700, 98
25991, V, 1, 1, 1, 1, 0, 700, 98
25992, V, 1, 1, 1, 1, 0, 700, 98
25993, V, 1, 1, 1, 1, 0, 700, 98
25994, V, 1, 1, 1, 1, 0, 700, 98
25995, V, 1, 1, 1, 1, 0, 700, 98
25996, V, 1, 1, 1, 1, 0, 700, 98
25997, V, 1, 1, 1, 1, 0, 700, 98
25998, V, 1, 1, 1, 1, 0, 700, 98
25999, V, 1, 1, 1, 1, 0, 700, 98
26000, V, 1, 1, 1, 1, 0, 700, 98
26001, V, 1, 1, 1, 1, 0, 700, 98
26002, V, 1, 1, 1, 1, 0, 700, 98
26003, V, 1, 1, 1, 1, 0, 700, 98
26004, V, 1, 1, 1, 1, 0, 700, 98
26005, V, 1, 1, 1, 1, 0, 700, 98
26006, V, 1, 1, 1, 1, 0, 700, 98
26007, V, 1, 1, 1, 1, 0, 700, 98
26008, V, 1, 1, 1, 1, 0, 700, 98
26009, V, 1, 1, 1, 1, 0, 700, 98
26010, V, 1, 1, 1, 1, 0, 700, 98
26011, V, 1, 0, 0, 1, 0, 700, 98
26011, V, 1, 0, 0, 0, 0, 700, 98
26012, V, 1, 1, 0, 0, 0, 700, 98
26012, V, 1, 1, 0, 0, 0, 700, 98
26013, V, 1, 1, 1, 1, 0, 700, 98
26014, V, 1, 1, 1, 1, 0, 700, 98
26015, V, 1, 1, 1, 1, 0, 700, 98
26016, V, 1, 1, 1, 1, 0, 700, 98
26017, V, 1, 1, 1, 1, 0, 700, 98
26018, V, 1, 1, 1, 1, 0, 700, 97
26019, V, 1, 1, 1, 1, 0, 700, 97
26020, V, 1, 1, 1, 1, 0, 700, 97
26021, V, 1, 1, 1, 1, 0, 700, 97
26022, V, 1, 1, 1, 1, 0, 700, 97
26023, V, 1, 1, 1, 1, 0, 700, 97
26024, V, 1, 1, 1, 1, 0, 700, 97
26025, V, 1, 1, 1, 1, 0, 700, 97
26027, V, 1, 1, 1, 1, 0, 700, 97
26028, V, 1, 1, 1, 1, 0, 700, 97
26029, V, 1, 1, 1, 1, 0, 700, 97
26030, V, 1, 1, 1, 1, 0, 700, 97
26031, V, 1, 1, 1, 1, 0, 700, 97
26032, V, 1, 1, 1, 1, 0, 700, 97
26033, V, 1, 1, 1, 1, 0, 700, 97
26034, V, 1, 1, 1, 1, 0, 700, 97
26035, V, 1, 1, 1, 1, 0, 700, 97
26036, V, 1, 1, 1, 1, 0, 700, 97
26037, V, 1, 1, 1, 1, 0, 700, 97
26038, V, 1, 1, 1, 1, 0, 700, 97
26039, V, 1, 1, 1, 1, 0, 700, 97
26040, V, 1, 1, 1, 1, 0, 700, 97
26041, V, 1, 1, 1, 1, 0, 700, 98
26042, V, 1, 1, 1, 1, 0, 700, 98
26043, V, 1, 1, 1, 1, 0, 700, 98
26044, V, 1, 1, 1, 1, 0, 700, 98
26045, V, 1, 1, 1, 1, 0, 700, 98
26046, V, 1, 1, 1, 1, 0, 700, 98
26047, V, 1, 1, 1, 1, 0, 700, 98
26048, V, 1, 1, 1, 1, 0, 700, 98
26049, V, 1, 1, 1, 1, 0, 700, 98
26050, V, 1, 1, 1, 1, 0, 700, 98
26051, V, 1, 1, 1, 1, 0, 700, 98
26052, V, 1, 1, 1, 1, 0, 700, 98
26053, V, 1, 1, 1, 1, 0, 700, 98
26054, V, 1, 1, 1, 1, 0, 700, 98
26055, V, 1, 1, 1, 1, 0, 700, 98
26056, V, 1, 1, 1, 1, 0, 700, 98
26057, V, 1, 1, 1, 1, 0, 700, 98
26058, V, 1, 1, 1, 1, 0, 700, 98
26059, V, 1, 1, 1, 1, 0, 700, 98
26060, V, 1, 1, 1, 1, 0, 700, 98
26061, V, 1, 1, 1, 1, 0, 700, 98
26062, V, 1, 1, 1, 1, 0, 700, 98
26063, V, 1, 1, 1, 1, 0, 700, 98
26064, V, 1, 1, 1, 1, 0, 700, 98
26065, V, 1, 1, 1, 1, 0, 700, 98
26066, V, 1, 1, 1, 1, 0, 700, 98
26067, V, 1, 1, 1, 1, 0, 700, 98
26068, V, 1, 1, 1, 1, 0, 700, 98
26070, V, 1, 1, 1, 1, 0, 700, 98
26071, V, 1, 1, 1, 1, 0, 700, 98
26072, V, 1, 1, 1, 1, 0, 700, 98
26073, V, 1, 1, 1, 1, 0, 700, 98
26074, V, 1, 1, 1, 1, 0, 700, 98
26075, V, 1, 1, 1, 1, 0, 700, 98
26076, V, 1, 1, 1, 1, 0, 700, 98
26077, V, 1, 1, 1, 1, 0, 700, 98
26078, V, 1, 1, 1, 1, 0, 700, 98
26079, V, 1, 1, 1, 1, 0, 700, 98
26080, V, 1, 1, 1, 1, 0, 700, 98
26081, V, 1, 1, 1, 1, 0, 700, 98
26082, V, 1, 1, 1, 1, 0, 700, 98
26083, V, 1, 1, 1, 1, 0, 700, 98
26084, V, 1, 1, 1, 1, 0, 700, 98
26085, V, 1, 1, 1, 1, 0, 700, 98
26086, V, 1, 1, 1, 1, 0, 700, 98
26087, V, 1, 1, 1, 1, 0, 700, 98
26088, V, 1, 1, 1, 1, 0, 700, 98
26089, V, 1, 1, 1, 1, 0, 700, 98
26090, V, 1, 1, 1, 1, 0, 700, 98
26091, V, 1, 1, 1, 1, 0, 700, 98
26092, V, 1, 1, 1, 1, 0, 700, 98
26093, V, 1, 1, 1, 1, 0, 700, 98
26094, V, 1, 1, 1, 1, 0, 700, 98
26095, V, 1, 1, 1, 1, 0, 700, 98
26096, V, 1, 1, 1, 1, 0, 700, 98
26097, V, 1, 1, 1, 1, 0, 700, 98
26098, V, 1, 1, 1, 1, 0, 700, 98
26099, V, 1, 1, 1, 1, 0, 700, 98
26100, V, 1, 1, 1, 1, 0, 700, 98
26101, V, 1, 1, 1, 1, 0, 700, 98
26102, V, 1, 1, 1, 1, 0, 700, 98
26103, V, 1, 1, 1, 1, 0, 700, 98
26104, V, 1, 1, 1, 1, 0, 700, 98
26105, V, 1, 1, 1, 1, 0, 700, 98
26106, V, 1, 1, 1, 1, 0, 700, 98
26107, V, 1, 1, 1, 1, 0, 700, 98
26108, V, 1, 1, 1, 1, 0, 700, 98
26109, V, 1, 1, 1, 1, 0, 700, 98
26110, V, 1, 1, 1, 1, 0, 700, 98
26112, V, 1, 1, 1, 1, 0, 700, 98
26113, V, 1, 1, 1, 1, 0, 700, 98
26114, V, 1, 1, 1, 1, 0, 700, 98
26115, V, 1, 1, 1, 1, 0, 700, 98
26116, V, 1, 1, 1, 1, 0, 700, 98
26117, V, 1, 1, 1, 1, 0, 700, 98
26118, V, 1, 1, 1, 1, 0, 700, 98
26119, V, 1, 1, 1, 1, 0, 700, 98
26120, V, 1, 1, 1, 1, 0, 700, 98
26121, V, 1, 1, 1, 1, 0, 700, 98
26122, V, 1, 1, 1, 1, 0, 700, 98
26123, V, 1, 1, 1, 1, 0, 700, 98
26124, V, 1, 1, 1, 1, 0, 700, 98
26125, V, 1, 1, 1, 1, 0, 700, 98
26126, V, 1, 1, 1, 1, 0, 700, 98
26127, V, 1, 1, 1, 1, 0, 700, 98
26128, V, 1, 1, 1, 1, 0, 700, 98
26129, V, 1, 1, 1, 1, 0, 700, 98
26130, V, 1, 1, 1, 1, 0, 700, 98
26131, V, 1, 1, 1, 1, 0, 700, 98
26132, V, 1, 1, 1, 1, 0, 700, 98
26133, V, 1, 1, 1, 1, 0, 700, 98
26134, V, 1, 1, 1, 1, 0, 700, 98
26135, V, 1, 1, 1, 1, 0, 700, 98
26136, V, 1, 1, 1, 1, 0, 700, 98
26137, V, 1, 1, 1, 1, 0, 700, 98
26138, V, 1, 1, 1, 1, 0, 700, 98
26139, V, 1, 1, 1, 1, 0, 700, 98
26140, V, 1, 1, 1, 1, 0, 700, 98
26141, V, 1, 1, 1, 1, 0, 700, 98
26142, V, 1, 1, 1, 1, 0, 700, 98
26143, V, 1, 1, 1, 1, 0, 700, 98
26144, V, 1, 1, 1, 1, 0, 700, 98
26145, V, 1, 1, 1, 1, 0, 700, 98
26146, V, 1, 1, 1, 1, 0, 700, 98
26147, V, 1, 1, 1, 1, 0, 700, 98
26148, V, 1, 1, 1, 1, 0, 700, 98
26149, V, 1, 1, 1, 1, 0, 700, 98
26150, V, 1, 1, 1, 1, 0, 700, 98
26151, V, 1, 1, 1, 1, 0, 700, 98
26152, V, 1, 1, 1, 1, 0, 700, 98
26153, V, 1, 1, 1, 1, 0, 700, 98
26155, V, 1, 1, 1, 1, 0, 700, 98
26156, V, 1, 1, 1, 1, 0, 700, 98
26157, V, 1, 1, 1, 1, 0, 700, 98
26158, V, 1, 1, 1, 1, 0, 700, 98
26159, V, 1, 1, 1, 1, 0, 700, 98
26160, V, 1, 1, 1, 1, 0, 700, 98
26161, V, 1, 1, 1, 1, 0, 700, 98
26162, V, 1, 1, 1, 1, 0, 700, 98
26163, V, 1, 1, 1, 1, 0, 700, 98
26164, V, 1, 1, 1, 1, 0, 700, 98
26165, V, 1, 1, 1, 1, 0, 700, 98
26166, V, 1, 1, 1, 1, 0, 700, 98
26167, V, 1, 1, 1, 1, 0, 700, 98
26168, V, 1, 1, 1, 1, 0, 700, 98
26169, V, 1, 1, 1, 1, 0, 700, 98
26170, V, 1, 1, 1, 1, 0, 700, 98
26171, V, 1, 1, 1, 1, 0, 700, 98
26172, V, 1, 1, 1, 1, 0, 700, 98
26173, V, 1, 1, 1, 1, 0, 700, 98
26174, V, 1, 1, 1, 1, 0, 700, 98
26175, V, 1, 1, 1, 1, 0, 700, 98
26176, V, 1, 1, 1, 1, 0, 700, 98
26177, V, 1, 1, 1, 1, 0, 700, 98
26178, V, 1, 1, 1, 1, 0, 700, 98
26179, V, 1, 1, 1, 1, 0, 700, 98
26180, V, 1, 1, 1, 1, 0, 700, 98
26181, V, 1, 1, 1, 1, 0, 700, 98
26182, V, 1, 1, 1, 1, 0, 700, 98
26183, V, 1, 1, 1, 1, 0, 700, 98
26184, V, 1, 1, 1, 1, 0, 700, 98
26185, V, 1, 1, 1, 1, 0, 700, 98
26186, V, 1, 1, 1, 1, 0, 700, 98
26187, V, 1, 1, 1, 1, 0, 700, 98
26188, V, 1, 1, 1, 1, 0, 700, 98
26189, V, 1, 1, 1, 1, 0, 700, 98
26190, V, 1, 1, 1, 1, 0, 700, 98
26191, V, 1, 1, 1, 1, 0, 700, 98
26192, V, 1, 1, 1, 1, 0, 700, 98
26193, V, 1, 1, 1, 1, 0, 700, 98
26194, V, 1, 1, 1, 1, 0, 700, 98
26195, V, 1, 1, 1, 1, 0, 700, 98
26196, V, 1, 1, 1, 1, 0, 700, 98
26198, V, 1, 1, 1, 1, 0, 700, 98
26199, V, 1, 1, 1, 1, 0, 700, 98
26200, V, 1, 1, 1, 1, 0, 700, 98
26201, V, 1, 1, 1, 1, 0, 700, 98
26202, V, 1, 1, 1, 1, 0, 700, 98
26203, V, 1, 1, 1, 1, 0, 700, 98
26204, V, 1, 1, 1, 1, 0, 700, 98
26205, V, 1, 1, 1, 1, 0, 700, 98
26206, V, 1, 1, 1, 1, 0, 700, 98
26207, V, 1, 1, 1, 1, 0, 700, 98
26208, V, 1, 1, 1, 1, 0, 700, 98
26209, V, 1, 1, 1, 1, 0, 700, 98
26210, V, 1, 1, 1, 1, 0, 700, 98
26211, V, 1, 1, 1, 1, 0, 700, 98
26212, V, 1, 1, 1, 1, 0, 700, 98
26213, V, 1, 1, 1, 1, 0, 700, 98
26214, V, 1, 1, 1, 1, 0, 700, 98
26215, V, 1, 1, 1, 1, 0, 700, 98
26216, V, 1, 1, 1, 1, 0, 700, 98
26217, V, 1, 1, 1, 1, 0, 700, 98
26218, V, 1, 1, 1, 1, 0, 700, 98
26219, V, 1, 1, 1, 1, 0, 700, 98
26220, V, 1, 1, 1, 1, 0, 700, 98
26221, V, 1, 1, 1, 1, 0, 700, 98
26222, V, 1, 1, 1, 1, 0, 700, 98
26223, V, 1, 1, 1, 1, 0, 700, 98
26224, V, 1, 1, 1, 1, 0, 700, 98
26225, V, 1, 1, 1, 1, 0, 700, 98
26226, V, 1, 1, 1, 1, 0, 700, 98
26227, V, 1, 1, 1, 1, 0, 700, 98
26228, V, 1, 1, 1, 1, 0, 700, 98
26229, V, 1, 1, 1, 1, 0, 700, 98
26230, V, 1, 1, 1, 1, 0, 700, 98
26231, V, 1, 1, 1, 1, 0, 700, 98
26232, V, 1, 1, 1, 1, 0, 700, 98
26233, V, 1, 1, 1, 1, 0, 700, 98
26234, V, 1, 1, 1, 1, 0, 700, 98
26235, V, 1, 1, 1, 1, 0, 700, 98
26236, V, 1, 1, 1, 1, 0, 700, 98
26237, V, 1, 1, 1, 1, 0, 700, 98
26238, V, 1, 1, 1, 1, 0, 700, 98
26240, V, 1, 1, 1, 1, 0, 700, 98
26241, V, 1, 1, 1, 1, 0, 700, 98
26242, V, 1, 1, 1, 1, 0, 700, 98
26243, V, 1, 1, 1, 1, 0, 700, 98
26244, V, 1, 1, 1, 1, 0, 700, 98
26245, V, 1, 1, 1, 1, 0, 700, 98
26246, V, 1, 1, 1, 1, 0, 700, 98
26247, V, 1, 1, 1, 1, 0, 700, 98
26248, V, 1, 1, 1, 1, 0, 700, 98
26249, V, 1, 1, 1, 1, 0, 700, 98
26250, V, 1, 1, 1, 1, 0, 700, 98
26251, V, 1, 1, 1, 1, 0, 700, 98
26252, V, 1, 1, 1, 1, 0, 700, 98
26253, V, 1, 1, 1, 1, 0, 700, 98
26254, V, 1, 1, 1, 1, 0, 700, 98
26255, V, 1, 1, 1, 1, 0, 700, 98
26256, V, 1, 1, 1, 1, 0, 700, 98
26257, V, 1, 1, 1, 1, 0, 700, 98
26258, V, 1, 1, 1, 1, 0, 700, 98
26259, V, 1, 1, 1, 1, 0, 700, 98
26260, V, 1, 1, 1, 1, 0, 700, 98
26261, V, 1, 1, 1, 1, 0, 700, 98
26262, V, 1, 1, 1, 1, 0, 700, 98
26263, V, 1, 1, 1, 1, 0, 700, 98
26264, V, 1, 1, 1, 1, 0, 700, 98
26265, V, 1, 1, 1, 1, 0, 700, 98
26266, V, 1, 1, 1, 1, 0, 700, 98
26267, V, 1, 1, 1, 1, 0, 700, 98
26268, V, 1, 1, 1, 1, 0, 700, 98
26269, V, 1, 1, 1, 1, 0, 700, 98
26270, V, 1, 1, 1, 1, 0, 700, 98
26271, V, 1, 1, 1, 1, 0, 700, 98
26272, V, 1, 1, 1, 1, 0, 700, 98
26273, V, 1, 1, 1, 1, 0, 700, 98
26274, V, 1, 1, 1, 1, 0, 700, 98
26275, V, 1, 1, 1, 1, 0, 700, 98
26276, V, 1, 1, 1, 1, 0, 700, 98
26277, V, 1, 1, 1, 1, 0, 700, 98
26278, V, 1, 1, 1, 1, 0, 700, 98
26279, V, 1, 1, 1, 1, 0, 700, 98
26280, V, 1, 1, 1, 1, 0, 700, 98
26281, V, 1, 1, 1, 1, 0, 700, 98
26283, V, 1, 1, 1, 1, 0, 700, 98
26284, V, 1, 1, 1, 1, 0, 700, 98
26285, V, 1, 1, 1, 1, 0, 700, 98
26286, V, 1, 1, 1, 1, 0, 700, 98
26287, V, 1, 1, 1, 1, 0, 700, 98
26288, V, 1, 1, 1, 1, 0, 700, 98
26289, V, 1, 1, 1, 1, 0, 700, 98
26290, V, 1, 1, 1, 1, 0, 700, 98
26291, V, 1, 1, 1, 1, 0, 700, 98
26292, V, 1, 1, 1, 1, 0, 700, 98
26293, V, 1, 1, 1, 1, 0, 700, 98
26294, V, 1, 1, 1, 1, 0, 700, 98
26295, V, 1, 1, 1, 1, 0, 700, 98
26296, V, 1, 1, 1, 1, 0, 700, 98
26297, V, 1, 1, 1, 1, 0, 700, 98
26298, V, 1, 1, 1, 1, 0, 700, 98
26299, V, 1, 1, 1, 1, 0, 700, 98
26300, V, 1, 1, 1, 1, 0, 700, 98
26301, V, 1, 1, 1, 1, 0, 700, 98
26302, V, 1, 1, 1, 1, 0, 700, 98
26303, V, 1, 1, 1, 1, 0, 700, 98
26304, V, 1, 1, 1, 1, 0, 700, 98
26305, V, 1, 1, 1, 1, 0, 700, 98
26306, V, 1, 1, 1, 1, 0, 700, 98
26307, V, 1, 1, 1, 1, 0, 700, 98
26308, V, 1, 1, 1, 1, 0, 700, 98
26309, V, 1, 1, 1, 1, 0, 700, 98
26310, V, 1, 1, 1, 1, 0, 700, 98
26311, V, 1, 1, 1, 1, 0, 700, 98
26312, V, 1, 1, 1, 1, 0, 700, 98
26313, V, 1, 1, 1, 1, 0, 700, 98
26314, V, 1, 1, 1, 1, 0, 700, 98
26315, V, 1, 1, 1, 1, 0, 700, 98
26316, V, 1, 1, 1, 1, 0, 700, 98
26317, V, 1, 1, 1, 1, 0, 700, 98
26318, V, 1, 1, 1, 1, 0, 700, 98
26319, V, 1, 1, 1, 1, 0, 700, 98
26320, V, 1, 1, 1, 1, 0, 700, 98
26321, V, 1, 1, 1, 1, 0, 700, 98
26322, V, 1, 1, 1, 1, 0, 700, 98
26323, V, 1, 1, 1, 1, 0, 700, 98
26324, V, 1, 1, 1, 1, 0, 700, 98
26326, V, 1, 1, 1, 1, 0, 700, 98
26327, V, 1, 1, 1, 1, 0, 700, 98
26328, V, 1, 1, 1, 1, 0, 700, 98
26329, V, 1, 1, 1, 1, 0, 700, 98
26330, V, 1, 1, 1, 1, 0, 700, 98
26331, V, 1, 1, 1, 1, 0, 700, 98
26332, V, 1, 1, 1, 1, 0, 700, 98
26333, V, 1, 1, 1, 1, 0, 700, 98
26334, V, 1, 1, 1, 1, 0, 700, 98
26335, V, 1, 1, 1, 1, 0, 700, 98
26336, V, 1, 1, 1, 1, 0, 700, 98
26337, V, 1, 1, 1, 1, 0, 700, 98
26338, V, 1, 1, 1, 1, 0, 700, 98
26339, V, 1, 1, 1, 1, 0, 700, 98
26340, V, 1, 1, 1, 1, 0, 700, 98
26341, V, 1, 1, 1, 1, 0, 700, 98
26342, V, 1, 1, 1, 1, 0, 700, 98
26343, V, 1, 1, 1, 1, 0, 700, 98
26344, V, 1, 1, 1, 1, 0, 700, 98
26345, V, 1, 1, 1, 1, 0, 700, 98
26346, V, 1, 1, 1, 1, 0, 700, 98
26347, V, 1, 1, 1, 1, 0, 700, 98
26348, V, 1, 1, 1, 1, 0, 700, 98
26349, V, 1, 1, 1, 1, 0, 700, 98
26350, V, 1, 1, 1, 1, 0, 700, 98
26351, V, 1, 1, 1, 1, 0, 700, 98
26352, V, 1, 1, 1, 1, 0, 700, 98
26353, V, 1, 1, 1, 1, 0, 700, 98
26354, V, 1, 1, 1, 1, 0, 700, 98
26355, V, 1, 1, 1, 1, 0, 700, 98
26356, V, 1, 1, 1, 1, 0, 700, 98
26357, V, 1, 1, 1, 1, 0, 700, 98
26358, V, 1, 1, 1, 1, 0, 700, 98
26359, V, 1, 1, 1, 1, 0, 700, 98
26360, V, 1, 1, 1, 1, 0, 700, 98
26361, V, 1, 1, 1, 1, 0, 700, 98
26362, V, 1, 1, 1, 1, 0, 700, 98
26363, V, 1, 1, 1, 1, 0, 700, 98
26364, V, 1, 1, 1, 1, 0, 700, 98
26365, V, 1, 1, 1, 1, 0, 700, 98
26366, V, 1, 1, 1, 1, 0, 700, 98
26368, V, 1, 1, 1, 1, 0, 700, 98
26369, V, 1, 1, 1, 1, 0, 700, 98
26370, V, 1, 1, 1, 1, 0, 700, 98
26371, V, 1, 1, 1, 1, 0, 700, 98
26372, V, 1, 1, 1, 1, 0, 700, 98
26373, V, 1, 1, 1, 1, 0, 700, 98
26374, V, 1, 1, 1, 1, 0, 700, 98
26375, V, 1, 1, 1, 1, 0, 700, 98
26376, V, 1, 1, 1, 1, 0, 700, 98
26377, V, 1, 1, 1, 1, 0, 700, 98
26378, V, 1, 1, 1, 1, 0, 700, 98
26379, V, 1, 1, 1, 1, 0, 700, 98
26380, V, 1, 1, 1, 1, 0, 700, 98
26381, V, 1, 1, 1, 1, 0, 700, 98
26382, V, 1, 1, 1, 1, 0, 700, 98
26383, V, 1, 1, 1, 1, 0, 700, 98
26384, V, 1, 1, 1, 1, 0, 700, 98
26385, V, 1, 1, 1, 1, 0, 700, 98
26386, V, 1, 1, 1, 1, 0, 700, 98
26387, V, 1, 1, 1, 1, 0, 700, 98
26388, V, 1, 1, 1, 1, 0, 700, 98
26389, V, 1, 1, 1, 1, 0, 700, 98
26390, V, 1, 1, 1, 1, 0, 700, 98
26391, V, 1, 1, 1, 1, 0, 700, 98
26392, V, 1, 1, 1, 1, 0, 700, 98
26393, V, 1, 1, 1, 1, 0, 700, 98
26394, V, 1, 1, 1, 1, 0, 700, 98
26395, V, 1, 1, 1, 1, 0, 700, 98
26396, V, 1, 1, 1, 1, 0, 700, 98
26397, V, 1, 1, 1, 1, 0, 700, 98
26398, V, 1, 1, 1, 1, 0, 700, 98
26399, V, 1, 1, 1, 1, 0, 700, 98
26400, V, 1, 1, 1, 1, 0, 700, 98
26401, V, 1, 1, 1, 1, 0, 700, 98
26402, V, 1, 1, 1, 1, 0, 700, 98
26403, V, 1, 1, 1, 1, 0, 700, 98
26404, V, 1, 1, 1, 1, 0, 700, 98
26405, V, 1, 1, 1, 1, 0, 700, 98
26406, V, 1, 1, 1, 1, 0, 700, 98
26407, V, 1, 1, 1, 1, 0, 700, 98
26408, V, 1, 1, 1, 1, 0, 700, 98
26409, V, 1, 1, 1, 1, 0, 700, 98
26411, V, 1, 1, 1, 1, 0, 700, 98
26412, V, 1, 1, 1, 1, 0, 700, 98
26413, V, 1, 1, 1, 1, 0, 700, 98
26414, V, 1, 1, 1, 1, 0, 700, 98
26415, V, 1, 1, 1, 1, 0, 700, 98
26416, V, 1, 1, 1, 1, 0, 700, 98
26417, V, 1, 1, 1, 1, 0, 700, 98
26418, V, 1, 1, 1, 1, 0, 700, 98
26419, V, 1, 1, 1, 1, 0, 700, 98
26420, V, 1, 1, 1, 1, 0, 700, 98
26421, V, 1, 1, 1, 1, 0, 700, 98
26422, V, 1, 1, 1, 1, 0, 700, 98
26423, V, 1, 1, 1, 1, 0, 700, 98
26424, V, 1, 1, 1, 1, 0, 700, 98
26425, V, 1, 1, 1, 1, 0, 700, 98
26426, V, 1, 1, 1, 1, 0, 700, 98
26427, V, 1, 1, 1, 1, 0, 700, 98
26428, V, 1, 1, 1, 1, 0, 700, 98
26429, V, 1, 1, 1, 1, 0, 700, 98
26430, V, 1, 1, 1, 1, 0, 700, 98
26431, V, 1, 1, 1, 1, 0, 700, 98
26432, V, 1, 1, 1, 1, 0, 700, 98
26433, V, 1, 1, 1, 1, 0, 700, 98
26434, V, 1, 1, 1, 1, 0, 700, 98
26435, V, 1, 1, 1, 1, 0, 700, 98
26436, V, 1, 1, 1, 1, 0, 700, 98
26437, V, 1, 1, 1, 1, 0, 700, 98
26438, V, 1, 1, 1, 1, 0, 700, 98
26439, V, 1, 1, 1, 1, 0, 700, 98
26440, V, 1, 1, 1, 1, 0, 700, 98
26441, V, 1, 1, 1, 1, 0, 700, 98
26442, V, 1, 1, 1, 1, 0, 700, 98
26443, V, 1, 1, 1, 1, 0, 700, 98
26444, V, 1, 1, 1, 1, 0, 700, 98
26445, V, 1, 1, 1, 1, 0, 700, 98
26446, V, 1, 1, 1, 1, 0, 700, 98
26447, V, 1, 1, 1, 1, 0, 700, 98
26448, V, 1, 1, 1, 1, 0, 700, 98
26449, V, 1, 1, 1, 1, 0, 700, 98
26450, V, 1, 1, 1, 1, 0, 700, 98
26451, V, 1, 1, 1, 1, 0, 700, 98
26452, V, 1, 1, 1, 1, 0, 700, 98
26454, V, 1, 1, 1, 1, 0, 700, 98
26455, V, 1, 1, 1, 1, 0, 700, 98
26456, V, 1, 1, 1, 1, 0, 700, 98
26457, V, 1, 1, 1, 1, 0, 700, 98
26458, V, 1, 1, 1, 1, 0, 700, 98
26459, V, 1, 1, 1, 1, 0, 700, 98
26460, V, 1, 1, 1, 1, 0, 700, 98
26461, V, 1, 1, 1, 1, 0, 700, 98
26462, V, 1, 1, 1, 1, 0, 700, 98
26463, V, 1, 1, 1, 1, 0, 700, 98
26464, V, 1, 1, 1, 1, 0, 700, 98
26465, V, 1, 1, 1, 1, 0, 700, 98
26466, V, 1, 1, 1, 1, 0, 700, 98
26467, V, 1, 1, 1, 1, 0, 700, 98
26468, V, 1, 1, 1, 1, 0, 700, 98
26469, V, 1, 1, 1, 1, 0, 700, 98
26470, V, 1, 1, 1, 1, 0, 700, 98
26471, V, 1, 1, 1, 1, 0, 700, 98
26472, V, 1, 1, 1, 1, 0, 700, 98
26473, V, 1, 1, 1, 1, 0, 700, 98
26474, V, 1, 1, 1, 1, 0, 700, 98
26475, V, 1, 1, 1, 1, 0, 700, 98
26476, V, 1, 1, 1, 1, 0, 700, 98
26477, V, 1, 1, 1, 1, 0, 700, 98
26478, V, 1, 1, 1, 1, 0, 700, 98
26479, V, 1, 1, 1, 1, 0, 700, 98
26480, V, 1, 1, 1, 1, 0, 700, 98
26481, V, 1, 1, 1, 1, 0, 700, 98
26482, V, 1, 1, 1, 1, 0, 700, 98
26483, V, 1, 1, 1, 1, 0, 700, 98
26484, V, 1, 1, 1, 1, 0, 700, 98
26485, V, 1, 1, 1, 1, 0, 700, 98
26486, V, 1, 1, 1, 1, 0, 700, 98
26487, V, 1, 1, 1, 1, 0, 700, 98
26488, V, 1, 1, 1, 1, 0, 700, 98
26489, V, 1, 1, 1, 1, 0, 700, 98
26490, V, 1, 1, 1, 1, 0, 700, 98
26491, V, 1, 1, 1, 1, 0, 700, 98
26492, V, 1, 1, 1, 1, 0, 700, 98
26493, V, 1, 1, 1, 1, 0, 700, 98
26494, V, 1, 1, 1, 1, 0, 700, 98
26496, V, 1, 1, 1, 1, 0, 700, 98
26497, V, 1, 1, 1, 1, 0, 700, 98
26498, V, 1, 1, 1, 1, 0, 700, 98
26499, V, 1, 1, 1, 1, 0, 700, 98
26500, V, 1, 1, 1, 1, 0, 700, 98
26501, V, 1, 1, 1, 1, 0, 700, 98
26502, V, 1, 1, 1, 1, 0, 700, 98
26503, V, 1, 1, 1, 1, 0, 700, 98
26504, V, 1, 1, 1, 1, 0, 700, 98
26505, V, 1, 1, 1, 1, 0, 700, 98
26506, V, 1, 1, 1, 1, 0, 700, 98
26507, V, 1, 1, 1, 1, 0, 700, 98
26508, V, 1, 1, 1, 1, 0, 700, 98
26509, V, 1, 1, 1, 1, 0, 700, 98
26510, V, 1, 1, 1, 1, 0, 700, 98
26511, V, 1, 1, 1, 1, 0, 700, 98
26512, V, 1, 1, 1, 1, 0, 700, 98
26513, V, 1, 1, 1, 1, 0, 700, 98
26514, V, 1, 1, 1, 1, 0, 700, 98
26515, V, 1, 1, 1, 1, 0, 700, 98
26516, V, 1, 1, 1, 1, 0, 700, 98
26517, V, 1, 1, 1, 1, 0, 700, 98
26518, V, 1, 1, 1, 1, 0, 700, 98
26519, V, 1, 1, 1, 1, 0, 700, 98
26520, V, 1, 1, 1, 1, 0, 700, 98
26521, V, 1, 1, 1, 1, 0, 700, 98
26522, V, 1, 1, 1, 1, 0, 700, 98
26523, V, 1, 1, 1, 1, 0, 700, 98
26524, V, 1, 1, 1, 1, 0, 700, 98
26525, V, 1, 1, 1, 1, 0, 700, 98
26526, V, 1, 1, 1, 1, 0, 700, 98
26527, V, 1, 1, 1, 1, 0, 700, 98
26528, V, 1, 1, 1, 1, 0, 700, 98
26529, V, 1, 1, 1, 1, 0, 700, 98
26530, V, 1, 1, 1, 1, 0, 700, 98
26531, V, 1, 1, 1, 1, 0, 700, 98
26532, V, 1, 1, 1, 1, 0, 700, 98
26533, V, 1, 1, 1, 1, 0, 700, 98
26534, V, 1, 1, 1, 1, 0, 700, 98
26535, V, 1, 1, 1, 1, 0, 700, 98
26536, V, 1, 1, 1, 1, 0, 700, 98
26537, V, 1, 1, 1, 1, 0, 700, 98
26539, V, 1, 1, 1, 1, 0, 700, 98
26540, V, 1, 1, 1, 1, 0, 700, 98
26541, V, 1, 1, 1, 1, 0, 700, 98
26542, V, 1, 1, 1, 1, 0, 700, 98
26543, V, 1, 1, 1, 1, 0, 700, 98
26544, V, 1, 1, 1, 1, 0, 700, 98
26545, V, 1, 1, 1, 1, 0, 700, 98
26546, V, 1, 1, 1, 1, 0, 700, 98
26547, V, 1, 1, 1, 1, 0, 700, 98
26548, V, 1, 1, 1, 1, 0, 700, 98
26549, V, 1, 1, 1, 1, 0, 700, 98
26550, V, 1, 1, 1, 1, 0, 700, 98
26551, V, 1, 1, 1, 1, 0, 700, 98
26552, V, 1, 1, 1, 1, 0, 700, 98
26553, V, 1, 1, 1, 1, 0, 700, 98
26554, V, 1, 1, 1, 1, 0, 700, 98
26555, V, 1, 1, 1, 1, 0, 700, 98
26556, V, 1, 1, 1, 1, 0, 700, 98
26557, V, 1, 1, 1, 1, 0, 700, 98
26558, V, 1, 1, 1, 1, 0, 700, 98
26559, V, 1, 1, 1, 1, 0, 700, 98
26560, V, 1, 1, 1, 1, 0, 700, 98
26561, V, 1, 1, 1, 1, 0, 700, 98
26562, V, 1, 1, 1, 1, 0, 700, 98
26563, V, 1, 1, 1, 1, 0, 700, 98
26564, V, 1, 1, 1, 1, 0, 700, 98
26565, V, 1, 1, 1, 1, 0, 700, 98
26566, V, 1, 1, 1, 1, 0, 700, 98
26567, V, 1, 1, 1, 1, 0, 700, 98
26568, V, 1, 1, 1, 1, 0, 700, 98
26569, V, 1, 1, 1, 1, 0, 700, 98
26570, V, 1, 1, 1, 1, 0, 700, 98
26571, V, 1, 1, 1, 1, 0, 700, 98
26572, V, 1, 1, 1, 1, 0, 700, 98
26573, V, 1, 1, 1, 1, 0, 700, 98
26574, V, 1, 1, 1, 1, 0, 700, 98
26575, V, 1, 1, 1, 1, 0, 700, 98
26576, V, 1, 1, 1, 1, 0, 700, 98
26577, V, 1, 1, 1, 1, 0, 700, 98
26578, V, 1, 1, 1, 1, 0, 700, 98
26579, V, 1, 1, 1, 1, 0, 700, 98
26580, V, 1, 1, 1, 1, 0, 700, 98
26582, V, 1, 1, 1, 1, 0, 700, 98
26583, V, 1, 1, 1, 1, 0, 700, 98
26584, V, 1, 1, 1, 1, 0, 700, 98
26585, V, 1, 1, 1, 1, 0, 700, 98
26586, V, 1, 1, 1, 1, 0, 700, 98
26587, V, 1, 1, 1, 1, 0, 700, 98
26588, V, 1, 1, 1, 1, 0, 700, 98
26589, V, 1, 1, 1, 1, 0, 700, 98
26590, V, 1, 1, 1, 1, 0, 700, 98
26591, V, 1, 1, 1, 1, 0, 700, 98
26592, V, 1, 1, 1, 1, 0, 700, 98
26593, V, 1, 1, 1, 1, 0, 700, 98
26594, V, 1, 1, 1, 1, 0, 700, 98
26595, V, 1, 1, 1, 1, 0, 700, 98
26596, V, 1, 1, 1, 1, 0, 700, 98
26597, V, 1, 1, 1, 1, 0, 700, 98
26598, V, 1, 1, 1, 1, 0, 700, 98
26599, V, 1, 1, 1, 1, 0, 700, 98
26600, V, 1, 1, 1, 1, 0, 700, 98
26601, V, 1, 1, 1, 1, 0, 700, 98
26602, V, 1, 1, 1, 1, 0, 700, 98
26603, V, 1, 1, 1, 1, 0, 700, 98
26604, V, 1, 1, 1, 1, 0, 700, 98
26605, V, 1, 1, 1, 1, 0, 700, 98
26606, V, 1, 1, 1, 1, 0, 700, 98
26607, V, 1, 1, 1, 1, 0, 700, 98
26608, V, 1, 1, 1, 1, 0, 700, 98
26609, V, 1, 1, 1, 1, 0, 700, 98
26610, V, 1, 1, 1, 1, 0, 700, 98
26611, V, 1, 1, 1, 1, 0, 700, 98
26612, V, 1, 1, 1, 1, 0, 700, 98
26613, V, 1, 1, 1, 1, 0, 700, 98
26614, V, 1, 1, 1, 1, 0, 700, 98
26615, V, 1, 1, 1, 1, 0, 700, 98
26616, V, 1, 1, 1, 1, 0, 700, 98
26617, V, 1, 1, 1, 1, 0, 700, 98
26618, V, 1, 1, 1, 1, 0, 700, 98
26619, V, 1, 1, 1, 1, 0, 700, 98
26620, V, 1, 1, 1, 1, 0, 700, 98
26621, V, 1, 1, 1, 1, 0, 700, 98
26622, V, 1, 1, 1, 1, 0, 700, 98
26624, V, 1, 1, 1, 1, 0, 700, 98
26625, V, 1, 1, 1, 1, 0, 700, 98
26626, V, 1, 1, 1, 1, 0, 700, 98
26627, V, 1, 1, 1, 1, 0, 700, 98
26628, V, 1, 1, 1, 1, 0, 700, 98
26629, V, 1, 1, 1, 1, 0, 700, 98
26630, V, 1, 1, 1, 1, 0, 700, 98
26631, V, 1, 1, 1, 1, 0, 700, 98
26632, V, 1, 1, 1, 1, 0, 700, 98
26633, V, 1, 1, 1, 1, 0, 700, 98
26634, V, 1, 1, 1, 1, 0, 700, 98
26635, V, 1, 1, 1, 1, 0, 700, 98
26636, V, 1, 1, 1, 1, 0, 700, 98
26637, V, 1, 1, 1, 1, 0, 700, 98
26638, V, 1, 1, 1, 1, 0, 700, 98
26639, V, 1, 1, 1, 1, 0, 700, 98
26640, V, 1, 1, 1, 1, 0, 700, 98
26641, V, 1, 1, 1, 1, 0, 700, 98
26642, V, 1, 1, 1, 1, 0, 700, 98
26643, V, 1, 1, 1, 1, 0, 700, 98
26644, V, 1, 1, 1, 1, 0, 700, 98
26645, V, 1, 1, 1, 1, 0, 700, 98
26646, V, 1, 1, 1, 1, 0, 700, 98
26647, V, 1, 1, 1, 1, 0, 700, 98
26648, V, 1, 1, 1, 1, 0, 700, 98
26649, V, 1, 1, 1, 1, 0, 700, 98
26650, V, 1, 1, 1, 1, 0, 700, 98
26651, V, 1, 1, 1, 1, 0, 700, 98
26652, V, 1, 1, 1, 1, 0, 700, 98
26653, V, 1, 1, 1, 1, 0, 700, 98
26654, V, 1, 1, 1, 1, 0, 700, 98
26655, V, 1, 1, 1, 1, 0, 700, 98
26656, V, 1, 1, 1, 1, 0, 700, 98
26657, V, 1, 1, 1, 1, 0, 700, 98
26658, V, 1, 1, 1, 1, 0, 700, 98
26659, V, 1, 1, 1, 1, 0, 700, 98
26660, V, 1, 1, 1, 1, 0, 700, 98
26661, V, 1, 1, 1, 1, 0, 700, 98
26662, V, 1, 1, 1, 1, 0, 700, 98
26663, V, 1, 1, 1, 1, 0, 700, 98
26664, V, 1, 1, 1, 1, 0, 700, 98
26665, V, 1, 1, 1, 1, 0, 700, 98
26667, V, 1, 1, 1, 1, 0, 700, 98
26668, V, 1, 1, 1, 1, 0, 700, 98
26669, V, 1, 1, 1, 1, 0, 700, 98
26670, V, 1, 1, 1, 1, 0, 700, 98
26671, V, 1, 1, 1, 1, 0, 700, 98
26672, V, 1, 1, 1, 1, 0, 700, 98
26673, V, 1, 1, 1, 1, 0, 700, 98
26674, V, 1, 1, 1, 1, 0, 700, 98
26675, V, 1, 1, 1, 1, 0, 700, 98
26676, V, 1, 1, 1, 1, 0, 700, 98
26677, V, 1, 1, 1, 1, 0, 700, 98
26678, V, 1, 1, 1, 1, 0, 700, 98
26679, V, 1, 1, 1, 1, 0, 700, 98
26680, V, 1, 1, 1, 1, 0, 700, 98
26681, V, 1, 1, 1, 1, 0, 700, 98
26682, V, 1, 1, 1, 1, 0, 700, 98
26683, V, 1, 1, 1, 1, 0, 700, 98
26684, V, 1, 1, 1, 1, 0, 700, 98
26685, V, 1, 1, 1, 1, 0, 700, 98
26686, V, 1, 1, 1, 1, 0, 700, 98
26687, V, 1, 1, 1, 1, 0, 700, 98
26688, V, 1, 1, 1, 1, 0, 700, 98
26689, V, 1, 1, 1, 1, 0, 700, 98
26690, V, 1, 1, 1, 1, 0, 700, 98
26691, V, 1, 1, 1, 1, 0, 700, 98
26692, V, 1, 1, 1, 1, 0, 700, 98
26693, V, 1, 1, 1, 1, 0, 700, 98
26694, V, 1, 1, 1, 1, 0, 700, 98
26695, V, 1, 1, 1, 1, 0, 700, 98
26696, V, 1, 1, 1, 1, 0, 700, 98
26697, V, 1, 1, 1, 1, 0, 700, 98
26698, V, 1, 1, 1, 1, 0, 700, 98
26699, V, 1, 1, 1, 1, 0, 700, 98
26700, V, 1, 1, 1, 1, 0, 700, 98
26701, V, 1, 1, 1, 1, 0, 700, 98
26702, V, 1, 1, 1, 1, 0, 700, 98
26703, V, 1, 1, 1, 1, 0, 700, 98
26704, V, 1, 1, 1, 1, 0, 700, 98
26705, V, 1, 1, 1, 1, 0, 700, 98
26706, V, 1, 1, 1, 1, 0, 700, 98
26707, V, 1, 1, 1, 1, 0, 700, 98
26708, V, 1, 1, 1, 1, 0, 700, 98
26710, V, 1, 1, 1, 1, 0, 700, 98
26711, V, 1, 1, 1, 1, 0, 700, 98
26712, V, 1, 1, 1, 1, 0, 700, 98
26713, V, 1, 1, 1, 1, 0, 700, 98
26714, V, 1, 1, 1, 1, 0, 700, 98
26715, V, 1, 1, 1, 1, 0, 700, 98
26716, V, 1, 1, 1, 1, 0, 700, 98
26717, V, 1, 1, 1, 1, 0, 700, 98
26718, V, 1, 1, 1, 1, 0, 700, 98
26719, V, 1, 1, 1, 1, 0, 700, 98
26720, V, 1, 1, 1, 1, 0, 700, 98
26721, V, 1, 1, 1, 1, 0, 700, 98
26722, V, 1, 1, 1, 1, 0, 700, 98
26723, V, 1, 1, 1, 1, 0, 700, 98
26724, V, 1, 1, 1, 1, 0, 700, 98
26725, V, 1, 1, 1, 1, 0, 700, 98
26726, V, 1, 1, 1, 1, 0, 700, 98
26727, V, 1, 1, 1, 1, 0, 700, 98
26728, V, 1, 1, 1, 1, 0, 700, 98
26729, V, 1, 1, 1, 1, 0, 700, 98
26730, V, 1, 1, 1, 1, 0, 700, 98
26731, V, 1, 1, 1, 1, 0, 700, 98
26732, V, 1, 1, 1, 1, 0, 700, 98
26733, V, 1, 1, 1, 1, 0, 700, 98
26734, V, 1, 1, 1, 1, 0, 700, 98
26735, V, 1, 1, 1, 1, 0, 700, 98
26736, V, 1, 1, 1, 1, 0, 700, 98
26737, V, 1, 1, 1, 1, 0, 700, 98
26738, V, 1, 1, 1, 1, 0, 700, 98
26739, V, 1, 1, 1, 1, 0, 700, 98
26740, V, 1, 1, 1, 1, 0, 700, 98
26741, V, 1, 1, 1, 1, 0, 700, 98
26742, V, 1, 1, 1, 1, 0, 700, 98
26743, V, 1, 1, 1, 1, 0, 700, 98
26744, V, 1, 1, 1, 1, 0, 700, 98
26745, V, 1, 1, 1, 1, 0, 700, 98
26746, V, 1, 1, 1, 1, 0, 700, 98
26747, V, 1, 1, 1, 1, 0, 700, 98
26748, V, 1, 1, 1, 1, 0, 700, 98
26749, V, 1, 1, 1, 1, 0, 700, 98
26750, V, 1, 1, 1, 1, 0, 700, 98
26752, V, 1, 1, 1, 1, 0, 700, 98
26753, V, 1, 1, 1, 1, 0, 700, 98
26754, V, 1, 1, 1, 1, 0, 700, 98
26755, V, 1, 1, 1, 1, 0, 700, 98
26756, V, 1, 1, 1, 1, 0, 700, 98
26757, V, 1, 1, 1, 1, 0, 700, 98
26758, V, 1, 1, 1, 1, 0, 700, 98
26759, V, 1, 1, 1, 1, 0, 700, 98
26760, V, 1, 1, 1, 1, 0, 700, 98
26761, V, 1, 1, 1, 1, 0, 700, 98
26762, V, 1, 1, 1, 1, 0, 700, 98
26763, V, 1, 1, 1, 1, 0, 700, 98
26764, V, 1, 1, 1, 1, 0, 700, 98
26765, V, 1, 1, 1, 1, 0, 700, 98
26766, V, 1, 1, 1, 1, 0, 700, 98
26767, V, 1, 1, 1, 1, 0, 700, 98
26768, V, 1, 1, 1, 1, 0, 700, 98
26769, V, 1, 1, 1, 1, 0, 700, 98
26770, V, 1, 1, 1, 1, 0, 700, 98
26771, V, 1, 1, 1, 1, 0, 700, 98
26772, V, 1, 1, 1, 1, 0, 700, 98
26773, V, 1, 1, 1, 1, 0, 700, 98
26774, V, 1, 1, 1, 1, 0, 700, 98
26775, V, 1, 1, 1, 1, 0, 700, 98
26776, V, 1, 1, 1, 1, 0, 700, 98
26777, V, 1, 1, 1, 1, 0, 700, 98
26778, V, 1, 1, 1, 1, 0, 700, 98
26779, V, 1, 1, 1, 1, 0, 700, 98
26780, V, 1, 1, 1, 1, 0, 700, 98
26781, V, 1, 1, 1, 1, 0, 700, 98
26782, V, 1, 1, 1, 1, 0, 700, 98
26783, V, 1, 1, 1, 1, 0, 700, 98
26784, V, 1, 1, 1, 1, 0, 700, 98
26785, V, 1, 1, 1, 1, 0, 700, 98
26786, V, 1, 1, 1, 1, 0, 700, 98
26787, V, 1, 1, 1, 1, 0, 700, 98
26788, V, 1, 1, 1, 1, 0, 700, 98
26789, V, 1, 1, 1, 1, 0, 700, 98
26790, V, 1, 1, 1, 1, 0, 700, 98
26791, V, 1, 1, 1, 1, 0, 700, 98
26792, V, 1, 1, 1, 1, 0, 700, 98
26793, V, 1, 1, 1, 1, 0, 700, 98
26795, V, 1, 1, 1, 1, 0, 700, 98
26796, V, 1, 1, 1, 1, 0, 700, 98
26797, V, 1, 1, 1, 1, 0, 700, 98
26798, V, 1, 1, 1, 1, 0, 700, 98
26799, V, 1, 1, 1, 1, 0, 700, 98
26800, V, 1, 1, 1, 1, 0, 700, 98
26801, V, 1, 1, 1, 1, 0, 700, 98
26802, V, 1, 1, 1, 1, 0, 700, 98
26803, V, 1, 1, 1, 1, 0, 700, 98
26804, V, 1, 1, 1, 1, 0, 700, 98
26805, V, 1, 1, 1, 1, 0, 700, 98
26806, V, 1, 1, 1, 1, 0, 700, 98
26807, V, 1, 1, 1, 1, 0, 700, 98
26808, V, 1, 1, 1, 1, 0, 700, 98
26809, V, 1, 1, 1, 1, 0, 700, 98
26810, V, 1, 1, 1, 1, 0, 700, 98
26811, V, 1, 1, 1, 1, 0, 700, 98
26812, V, 1, 1, 1, 1, 0, 700, 98
26813, V, 1, 1, 1, 1, 0, 700, 98
26814, V, 1, 1, 1, 1, 0, 700, 98
26815, V, 1, 1, 1, 1, 0, 700, 98
26816, V, 1, 1, 1, 1, 0, 700, 98
26817, V, 1, 1, 1, 1, 0, 700, 98
26818, V, 1, 1, 1, 1, 0, 700, 98
26819, V, 1, 1, 1, 1, 0, 700, 98
26820, V, 1, 1, 1, 1, 0, 700, 98
26821, V, 1, 1, 1, 1, 0, 700, 98
26822, V, 1, 1, 1, 1, 0, 700, 98
26823, V, 1, 1, 1, 1, 0, 700, 98
26824, V, 1, 1, 1, 1, 0, 700, 98
26825, V, 1, 1, 1, 1, 0, 700, 98
26826, V, 1, 1, 1, 1, 0, 700, 98
26827, V, 1, 1, 1, 1, 0, 700, 98
26828, V, 1, 1, 1, 1, 0, 700, 98
26829, V, 1, 1, 1, 1, 0, 700, 98
26830, V, 1, 1, 1, 1, 0, 700, 98
26831, V, 1, 1, 1, 1, 0, 700, 98
26832, V, 1, 1, 1, 1, 0, 700, 98
26833, V, 1, 1, 1, 1, 0, 700, 98
26834, V, 1, 1, 1, 1, 0, 700, 98
26835, V, 1, 1, 1, 1, 0, 700, 98
26836, V, 1, 1, 1, 1, 0, 700, 98
26838, V, 1, 1, 1, 1, 0, 700, 98
26839, V, 1, 1, 1, 1, 0, 700, 98
26840, V, 1, 1, 1, 1, 0, 700, 98
26841, V, 1, 1, 1, 1, 0, 700, 98
26842, V, 1, 1, 1, 1, 0, 700, 98
26843, V, 1, 1, 1, 1, 0, 700, 98
26844, V, 1, 1, 1, 1, 0, 700, 98
26845, V, 1, 1, 1, 1, 0, 700, 98
26846, V, 1, 1, 1, 1, 0, 700, 98
26847, V, 1, 1, 1, 1, 0, 700, 98
26848, V, 1, 1, 1, 1, 0, 700, 98
26849, V, 1, 1, 1, 1, 0, 700, 98
26850, V, 1, 1, 1, 1, 0, 700, 98
26851, V, 1, 1, 1, 1, 0, 700, 98
26852, V, 1, 1, 1, 1, 0, 700, 98
26853, V, 1, 1, 1, 1, 0, 700, 98
26854, V, 1, 1, 1, 1, 0, 700, 98
26855, V, 1, 1, 1, 1, 0, 700, 98
26856, V, 1, 1, 1, 1, 0, 700, 98
26857, V, 1, 1, 1, 1, 0, 700, 98
26858, V, 1, 1, 1, 1, 0, 700, 98
26859, V, 1, 1, 1, 1, 0, 700, 98
26860, V, 1, 1, 1, 1, 0, 700, 98
26861, V, 1, 1, 1, 1, 0, 700, 98
26862, V, 1, 1, 1, 1, 0, 700, 98
26863, V, 1, 1, 1, 1, 0, 700, 98
26864, V, 1, 1, 1, 1, 0, 700, 98
26865, V, 1, 1, 1, 1, 0, 700, 98
26866, V, 1, 1, 1, 1, 0, 700, 98
26867, V, 1, 1, 1, 1, 0, 700, 98
26868, V, 1, 1, 1, 1, 0, 700, 98
26869, V, 1, 1, 1, 1, 0, 700, 98
26870, V, 1, 1, 1, 1, 0, 700, 98
26871, V, 1, 1, 1, 1, 0, 700, 98
26872, V, 1, 1, 1, 1, 0, 700, 98
26873, V, 1, 1, 1, 1, 0, 700, 98
26874, V, 1, 1, 1, 1, 0, 700, 98
26875, V, 1, 1, 1, 1, 0, 700, 98
26876, V, 1, 1, 1, 1, 0, 700, 98
26877, V, 1, 1, 1, 1, 0, 700, 98
26878, V, 1, 1, 1, 1, 0, 700, 98
26880, V, 1, 1, 1, 1, 0, 700, 98
26881, V, 1, 1, 1, 1, 0, 700, 98
26882, V, 1, 1, 1, 1, 0, 700, 98
26883, V, 1, 1, 1, 1, 0, 700, 98
26884, V, 1, 1, 1, 1, 0, 700, 98
26885, V, 1, 1, 1, 1, 0, 700, 98
26886, V, 1, 1, 1, 1, 0, 700, 98
26887, V, 1, 1, 1, 1, 0, 700, 98
26888, V, 1, 1, 1, 1, 0, 700, 98
26889, V, 1, 1, 1, 1, 0, 700, 98
26890, V, 1, 1, 1, 1, 0, 700, 98
26891, V, 1, 1, 1, 1, 0, 700, 98
26892, V, 1, 1, 1, 1, 0, 700, 98
26893, V, 1, 1, 1, 1, 0, 700, 98
26894, V, 1, 1, 1, 1, 0, 700, 98
26895, V, 1, 1, 1, 1, 0, 700, 98
26896, V, 1, 1, 1, 1, 0, 700, 98
26897, V, 1, 1, 1, 1, 0, 700, 98
26898, V, 1, 1, 1, 1, 0, 700, 98
26899, V, 1, 1, 1, 1, 0, 700, 98
26900, V, 1, 1, 1, 1, 0, 700, 98
26901, V, 1, 1, 1, 1, 0, 700, 98
26902, V, 1, 1, 1, 1, 0, 700, 98
26903, V, 1, 1, 1, 1, 0, 700, 98
26904, V, 1, 1, 1, 1, 0, 700, 98
26905, V, 1, 1, 1, 1, 0, 700, 98
26906, V, 1, 1, 1, 1, 0, 700, 98
26907, V, 1, 1, 1, 1, 0, 700, 98
26908, V, 1, 1, 1, 1, 0, 700, 98
26909, V, 1, 1, 1, 1, 0, 700, 98
26910, V, 1, 1, 1, 1, 0, 700, 98
26911, V, 1, 1, 1, 1, 0, 700, 98
26912, V, 1, 1, 1, 1, 0, 700, 98
26913, V, 1, 1, 1, 1, 0, 700, 98
26914, V, 1, 1, 1, 1, 0, 700, 98
26915, V, 1, 1, 1, 1, 0, 700, 98
26916, V, 1, 1, 1, 1, 0, 700, 98
26917, V, 1, 1, 1, 1, 0, 700, 98
26918, V, 1, 1, 1, 1, 0, 700, 98
26919, V, 1, 1, 1, 1, 0, 700, 98
26920, V, 1, 1, 1, 1, 0, 700, 98
26921, V, 1, 1, 1, 1, 0, 700, 98
26923, V, 1, 1, 1, 1, 0, 700, 98
26924, V, 1, 1, 1, 1, 0, 700, 98
26925, V, 1, 1, 1, 1, 0, 700, 98
26926, V, 1, 1, 1, 1, 0, 700, 98
26927, V, 1, 1, 1, 1, 0, 700, 98
26928, V, 1, 1, 1, 1, 0, 700, 98
26929, V, 1, 1, 1, 1, 0, 700, 98
26930, V, 1, 1, 1, 1, 0, 700, 98
26931, V, 1, 1, 1, 1, 0, 700, 98
26932, V, 1, 1, 1, 1, 0, 700, 98
26933, V, 1, 1, 1, 1, 0, 700, 98
26934, V, 1, 1, 1, 1, 0, 700, 98
26935, V, 1, 1, 1, 1, 0, 700, 98
26936, V, 1, 1, 1, 1, 0, 700, 98
26937, V, 1, 1, 1, 1, 0, 700, 98
26938, V, 1, 1, 1, 1, 0, 700, 98
26939, V, 1, 1, 1, 1, 0, 700, 98
26940, V, 1, 1, 1, 1, 0, 700, 98
26941, V, 1, 1, 1, 1, 0, 700, 98
26942, V, 1, 1, 1, 1, 0, 700, 98
26943, V, 1, 1, 1, 1, 0, 700, 98
26944, V, 1, 1, 1, 1, 0, 700, 98
26945, V, 1, 1, 1, 1, 0, 700, 98
26946, V, 1, 1, 1, 1, 0, 700, 98
26947, V, 1, 1, 1, 1, 0, 700, 98
26948, V, 1, 1, 1, 1, 0, 700, 98
26949, V, 1, 1, 1, 1, 0, 700, 98
26950, V, 1, 1, 1, 1, 0, 700, 98
26951, V, 1, 1, 1, 1, 0, 700, 98
26952, V, 1, 1, 1, 1, 0, 700, 98
26953, V, 1, 1, 1, 1, 0, 700, 98
26954, V, 1, 1, 1, 1, 0, 700, 98
26955, V, 1, 1, 1, 1, 0, 700, 98
26956, V, 1, 1, 1, 1, 0, 700, 98
26957, V, 1, 1, 1, 1, 0, 700, 98
26958, V, 1, 1, 1, 1, 0, 700, 98
26959, V, 1, 1, 1, 1, 0, 700, 98
26960, V, 1, 1, 1, 1, 0, 700, 98
26961, V, 1, 1, 1, 1, 0, 700, 98
26962, V, 1, 1, 1, 1, 0, 700, 98
26963, V, 1, 1, 1, 1, 0, 700, 98
26964, V, 1, 1, 1, 1, 0, 700, 98
26966, V, 1, 1, 1, 1, 0, 700, 98
26967, V, 1, 1, 1, 1, 0, 700, 98
26968, V, 1, 1, 1, 1, 0, 700, 98
26969, V, 1, 1, 1, 1, 0, 700, 98
26970, V, 1, 1, 1, 1, 0, 700, 98
26971, V, 1, 1, 1, 1, 0, 700, 98
26972, V, 1, 1, 1, 1, 0, 700, 98
26973, V, 1, 1, 1, 1, 0, 700, 98
26974, V, 1, 1, 1, 1, 0, 700, 98
26975, V, 1, 1, 1, 1, 0, 700, 98
26976, V, 1, 1, 1, 1, 0, 700, 98
26977, V, 1, 1, 1, 1, 0, 700, 98
26978, V, 1, 1, 1, 1, 0, 700, 98
26979, V, 1, 1, 1, 1, 0, 700, 98
26980, V, 1, 1, 1, 1, 0, 700, 98
26981, V, 1, 1, 1, 1, 0, 700, 98
26982, V, 1, 1, 1, 1, 0, 700, 98
26983, V, 1, 1, 1, 1, 0, 700, 98
26984, V, 1, 1, 1, 1, 0, 700, 98
26985, V, 1, 1, 1, 1, 0, 700, 98
26986, V, 1, 1, 1, 1, 0, 700, 98
26987, V, 1, 1, 1, 1, 0, 700, 98
26988, V, 1, 1, 1, 1, 0, 700, 98
26989, V, 1, 1, 1, 1, 0, 700, 98
26990, V, 1, 1, 1, 1, 0, 700, 98
26991, V, 1, 1, 1, 1, 0, 700, 98
26992, V, 1, 1, 1, 1, 0, 700, 98
26993, V, 1, 1, 1, 1, 0, 700, 98
26994, V, 1, 1, 1, 1, 0, 700, 98
26995, V, 1, 1, 1, 1, 0, 700, 98
26996, V, 1, 1, 1, 1, 0, 700, 98
26997, V, 1, 1, 1, 1, 0, 700, 98
26998, V, 1, 1, 1, 1, 0, 700, 98
26999, V, 1, 1, 1, 1, 0, 700, 98
27000, V, 1, 1, 1, 1, 0, 700, 98
27001, V, 1, 1, 1, 1, 0, 700, 98
27002, V, 1, 1, 1, 1, 0, 700, 98
27003, V, 1, 1, 1, 1, 0, 700, 98
27004, V, 1, 1, 1, 1, 0, 700, 98
27005, V, 1, 1, 1, 1, 0, 700, 98
27006, V, 1, 1, 1, 1, 0, 700, 98
27008, V, 1, 1, 1, 1, 0, 700, 98
27009, V, 1, 1, 1, 1, 0, 700, 98
27010, V, 1, 1, 1, 1, 0, 700, 98
27011, V, 1, 1, 1, 1, 0, 700, 98
27012, V, 1, 1, 1, 1, 0, 700, 98
27013, V, 1, 1, 1, 1, 0, 700, 98
27014, V, 1, 1, 1, 1, 0, 700, 98
27015, V, 1, 1, 1, 1, 0, 700, 98
27016, V, 1, 1, 1, 1, 0, 700, 98
27017, V, 1, 1, 1, 1, 0, 700, 98
27018, V, 1, 1, 1, 1, 0, 700, 98
27019, V, 1, 1, 1, 1, 0, 700, 98
27020, V, 1, 1, 1, 1, 0, 700, 98
27021, V, 1, 1, 1, 1, 0, 700, 98
27022, V, 1, 1, 1, 1, 0, 700, 98
27023, V, 1, 1, 1, 1, 0, 700, 98
27024, V, 1, 1, 1, 1, 0, 700, 98
27025, V, 1, 1, 1, 1, 0, 700, 98
27026, V, 1, 1, 1, 1, 0, 700, 98
27027, V, 1, 1, 1, 1, 0, 700, 98
27028, V, 1, 1, 1, 1, 0, 700, 98
27029, V, 1, 1, 1, 1, 0, 700, 98
27030, V, 1, 1, 1, 1, 0, 700, 98
27031, V, 1, 1, 1, 1, 0, 700, 98
27032, V, 1, 1, 1, 1, 0, 700, 98
27033, V, 1, 1, 1, 1, 0, 700, 98
27034, V, 1, 1, 1, 1, 0, 700, 98
27035, V, 1, 1, 1, 1, 0, 700, 98
27036, V, 1, 1, 1, 1, 0, 700, 98
27037, V, 1, 1, 1, 1, 0, 700, 98
27038, V, 1, 1, 1, 1, 0, 700, 98
27039, V, 1, 1, 1, 1, 0, 700, 98
27040, V, 1, 1, 1, 1, 0, 700, 98
27041, V, 1, 1, 1, 1, 0, 700, 98
27042, V, 1, 1, 1, 1, 0, 700, 98
27043, V, 1, 1, 1, 1, 0, 700, 98
27044, V, 1, 1, 1, 1, 0, 700, 98
27045, V, 1, 1, 1, 1, 0, 700, 98
27046, V, 1, 1, 1, 1, 0, 700, 98
27047, V, 1, 1, 1, 1, 0, 700, 98
27048, V, 1, 1, 1, 1, 0, 700, 98
27049, V, 1, 1, 1, 1, 0, 700, 98
27051, V, 1, 1, 1, 1, 0, 700, 98
27052, V, 1, 1, 1, 1, 0, 700, 98
27053, V, 1, 1, 1, 1, 0, 700, 98
27054, V, 1, 1, 1, 1, 0, 700, 98
27055, V, 1, 1, 1, 1, 0, 700, 98
27056, V, 1, 1, 1, 1, 0, 700, 98
27057, V, 1, 1, 1, 1, 0, 700, 98
27058, V, 1, 1, 1, 1, 0, 700, 98
27059, V, 1, 1, 1, 1, 0, 700, 98
27060, V, 1, 1, 1, 1, 0, 700, 98
27061, V, 1, 1, 1, 1, 0, 700, 98
27062, V, 1, 1, 1, 1, 0, 700, 98
27063, V, 1, 1, 1, 1, 0, 700, 98
27064, V, 1, 1, 1, 1, 0, 700, 98
27065, V, 1, 1, 1, 1, 0, 700, 98
27066, V, 1, 1, 1, 1, 0, 700, 98
27067, V, 1, 1, 1, 1, 0, 700, 98
27068, V, 1, 1, 1, 1, 0, 700, 98
27069, V, 1, 1, 1, 1, 0, 700, 98
27070, V, 1, 1, 1, 1, 0, 700, 98
27071, V, 1, 1, 1, 1, 0, 700, 98
27072, V, 1, 1, 1, 1, 0, 700, 98
27073, V, 1, 1, 1, 1, 0, 700, 98
27074, V, 1, 1, 1, 1, 0, 700, 98
27075, V, 1, 1, 1, 1, 0, 700, 98
27076, V, 1, 1, 1, 1, 0, 700, 98
27077, V, 1, 1, 1, 1, 0, 700, 98
27078, V, 1, 1, 1, 1, 0, 700, 98
27079, V, 1, 1, 1, 1, 0, 700, 98
27080, V, 1, 1, 1, 1, 0, 700, 98
27081, V, 1, 1, 1, 1, 0, 700, 98
27082, V, 1, 1, 1, 1, 0, 700, 98
27083, V, 1, 1, 1, 1, 0, 700, 98
27084, V, 1, 1, 1, 1, 0, 700, 98
27085, V, 1, 1, 1, 1, 0, 700, 98
27086, V, 1, 1, 1, 1, 0, 700, 98
27087, V, 1, 1, 1, 1, 0, 700, 98
27088, V, 1, 1, 1, 1, 0, 700, 98
27089, V, 1, 1, 1, 1, 0, 700, 98
27090, V, 1, 1, 1, 1, 0, 700, 98
27091, V, 1, 1, 1, 1, 0, 700, 98
27092, V, 1, 1, 1, 1, 0, 700, 98
27094, V, 1, 1, 1, 1, 0, 700, 97
27095, V, 1, 1, 1, 1, 0, 700, 98
27096, V, 1, 1, 1, 1, 0, 700, 97
27097, V, 1, 1, 1, 1, 0, 700, 98
27098, V, 1, 1, 1, 1, 0, 700, 98
27099, V, 1, 1, 1, 1, 0, 700, 98
27100, V, 1, 1, 1, 1, 0, 700, 98
27101, V, 1, 1, 1, 1, 0, 700, 98
27102, V, 1, 1, 1, 1, 0, 700, 98
27103, V, 1, 1, 1, 1, 0, 700, 98
27104, V, 1, 1, 1, 1, 0, 700, 98
27105, V, 1, 1, 1, 1, 0, 700, 98
27106, V, 1, 1, 1, 1, 0, 700, 98
27107, V, 1, 1, 1, 1, 0, 700, 98
27108, V, 1, 1, 1, 1, 0, 700, 98
27109, V, 1, 1, 1, 1, 0, 700, 98
27110, V, 1, 1, 1, 1, 0, 700, 98
27111, V, 1, 1, 1, 1, 0, 700, 98
27112, V, 1, 1, 1, 1, 0, 700, 98
27113, V, 1, 1, 1, 1, 0, 700, 98
27114, V, 1, 1, 1, 1, 0, 700, 98
27115, V, 1, 1, 1, 1, 0, 700, 98
27116, V, 1, 1, 1, 1, 0, 700, 98
27117, V, 1, 1, 1, 1, 0, 700, 98
27118, V, 1, 1, 1, 1, 0, 700, 98
27119, V, 1, 1, 1, 1, 0, 700, 98
27120, V, 1, 1, 1, 1, 0, 700, 98
27121, V, 1, 1, 1, 1, 0, 700, 98
27122, V, 1, 1, 1, 1, 0, 700, 98
27123, V, 1, 1, 1, 1, 0, 700, 98
27124, V, 1, 1, 1, 1, 0, 700, 98
27125, V, 1, 1, 1, 1, 0, 700, 98
27126, V, 1, 1, 1, 1, 0, 700, 98
27127, V, 1, 1, 1, 1, 0, 700, 98
27128, V, 1, 1, 1, 1, 0, 700, 98
27129, V, 1, 1, 1, 1, 0, 700, 98
27130, V, 1, 1, 1, 1, 0, 700, 98
27131, V, 1, 1, 1, 1, 0, 700, 98
27132, V, 1, 1, 1, 1, 0, 700, 98
27133, V, 1, 1, 1, 1, 0, 700, 98
27134, V, 1, 1, 1, 1, 0, 700, 98
27136, V, 1, 1, 1, 1, 0, 700, 98
27137, V, 1, 1, 1, 1, 0, 700, 98
27138, V, 1, 1, 1, 1, 0, 700, 98
27139, V, 1, 1, 1, 1, 0, 700, 98
27140, V, 1, 1, 1, 1, 0, 700, 98
27141, V, 1, 1, 1, 1, 0, 700, 98
27142, V, 1, 1, 1, 1, 0, 700, 98
27143, V, 1, 1, 1, 1, 0, 700, 98
27144, V, 1, 1, 1, 1, 0, 700, 98
27145, V, 1, 1, 1, 1, 0, 700, 98
27146, V, 1, 1, 1, 1, 0, 700, 98
27147, V, 1, 1, 1, 1, 0, 700, 98
27148, V, 1, 1, 1, 1, 0, 700, 98
27149, V, 1, 1, 1, 1, 0, 700, 98
27150, V, 1, 1, 1, 1, 0, 700, 98
27151, V, 1, 1, 1, 1, 0, 700, 98
27152, V, 1, 1, 1, 1, 0, 700, 98
27153, V, 1, 1, 1, 1, 0, 700, 98
27154, V, 1, 1, 1, 1, 0, 700, 98
27155, V, 1, 1, 1, 1, 0, 700, 98
27156, V, 1, 1, 1, 1, 0, 700, 98
27157, V, 1, 1, 1, 1, 0, 700, 98
27158, V, 1, 1, 1, 1, 0, 700, 98
27159, V, 1, 1, 1, 1, 0, 700, 98
27160, V, 1, 1, 1, 1, 0, 700, 98
27161, V, 1, 1, 1, 1, 0, 700, 98
27162, V, 1, 1, 1, 1, 0, 700, 98
27163, V, 1, 1, 1, 1, 0, 700, 98
27164, V, 1, 1, 1, 1, 0, 700, 98
27165, V, 1, 1, 1, 1, 0, 700, 98
27166, V, 1, 1, 1, 1, 0, 700, 98
27167, V, 1, 1, 1, 1, 0, 700, 98
27168, V, 1, 1, 1, 1, 0, 700, 98
27169, V, 1, 1, 1, 1, 0, 700, 98
27170, V, 1, 1, 1, 1, 0, 700, 98
27171, V, 1, 1, 1, 1, 0, 700, 98
27172, V, 1, 1, 1, 1, 0, 700, 98
27173, V, 1, 1, 1, 1, 0, 700, 98
27174, V, 1, 1, 1, 1, 0, 700, 98
27175, V, 1, 1, 1, 1, 0, 700, 98
27176, V, 1, 1, 1, 1, 0, 700, 98
27177, V, 1, 1, 1, 1, 0, 700, 98
27179, V, 1, 1, 1, 1, 0, 700, 98
27180, V, 1, 1, 1, 1, 0, 700, 98
27181, V, 1, 1, 1, 1, 0, 700, 98
27182, V, 1, 1, 1, 1, 0, 700, 98
27183, V, 1, 1, 1, 1, 0, 700, 98
27184, V, 1, 1, 1, 1, 0, 700, 98
27185, V, 1, 1, 1, 1, 0, 700, 98
27186, V, 1, 1, 1, 1, 0, 700, 98
27187, V, 1, 1, 1, 1, 0, 700, 98
27188, V, 1, 1, 1, 1, 0, 700, 98
27189, V, 1, 1, 1, 1, 0, 700, 98
27190, V, 1, 1, 1, 1, 0, 700, 98
27191, V, 1, 1, 1, 1, 0, 700, 98
27192, V, 1, 1, 1, 1, 0, 700, 98
27193, V, 1, 1, 1, 1, 0, 700, 98
27194, V, 1, 1, 1, 1, 0, 700, 98
27195, V, 1, 1, 1, 1, 0, 700, 98
27196, V, 1, 1, 1, 1, 0, 700, 98
27197, V, 1, 1, 1, 1, 0, 700, 98
27198, V, 1, 1, 1, 1, 0, 700, 98
27199, V, 1, 1, 1, 1, 0, 700, 98
27200, V, 1, 1, 1, 1, 0, 700, 98
27201, V, 1, 1, 1, 1, 0, 700, 98
27202, V, 1, 1, 1, 1, 0, 700, 98
27203, V, 1, 1, 1, 1, 0, 700, 98
27204, V, 1, 1, 1, 1, 0, 700, 98
27205, V, 1, 1, 1, 1, 0, 700, 98
27206, V, 1, 1, 1, 1, 0, 700, 98
27207, V, 1, 1, 1, 1, 0, 700, 98
27208, V, 1, 1, 1, 1, 0, 700, 98
27209, V, 1, 1, 1, 1, 0, 700, 98
27210, V, 1, 1, 1, 1, 0, 700, 98
27211, V, 1, 1, 1, 1, 0, 700, 98
27212, V, 1, 1, 1, 1, 0, 700, 98
27213, V, 1, 1, 1, 1, 0, 700, 98
27214, V, 1, 1, 1, 1, 0, 700, 98
27215, V, 1, 1, 1, 1, 0, 700, 98
27216, V, 1, 1, 1, 1, 0, 700, 98
27217, V, 1, 1, 1, 1, 0, 700, 98
27218, V, 1, 1, 1, 1, 0, 700, 98
27219, V, 1, 1, 1, 1, 0, 700, 98
27220, V, 1, 1, 1, 1, 0, 700, 98
27222, V, 1, 1, 1, 1, 0, 700, 98
27223, V, 1, 1, 1, 1, 0, 700, 98
27224, V, 1, 1, 1, 1, 0, 700, 98
27225, V, 1, 1, 1, 1, 0, 700, 98
27226, V, 1, 1, 1, 1, 0, 700, 98
27227, V, 1, 1, 1, 1, 0, 700, 98
27228, V, 1, 1, 1, 1, 0, 700, 98
27229, V, 1, 1, 1, 1, 0, 700, 98
27230, V, 1, 1, 1, 1, 0, 700, 98
27231, V, 1, 1, 1, 1, 0, 700, 98
27232, V, 1, 1, 1, 1, 0, 700, 98
27233, V, 1, 1, 1, 1, 0, 700, 98
27234, V, 1, 1, 1, 1, 0, 700, 98
27235, V, 1, 1, 1, 1, 0, 700, 98
27236, V, 1, 1, 1, 1, 0, 700, 98
27237, V, 1, 1, 1, 1, 0, 700, 98
27238, V, 1, 1, 1, 1, 0, 700, 98
27239, V, 1, 1, 1, 1, 0, 700, 98
27240, V, 1, 1, 1, 1, 0, 700, 98
27241, V, 1, 1, 1, 1, 0, 700, 98
27242, V, 1, 1, 1, 1, 0, 700, 98
27243, V, 1, 1, 1, 1, 0, 700, 98
27244, V, 1, 1, 1, 1, 0, 700, 98
27245, V, 1, 1, 1, 1, 0, 700, 98
27246, V, 1, 1, 1, 1, 0, 700, 98
27247, V, 1, 1, 1, 1, 0, 700, 98
27248, V, 1, 1, 1, 1, 0, 700, 98
27249, V, 1, 1, 1, 1, 0, 700, 98
27250, V, 1, 1, 1, 1, 0, 700, 98
27251, V, 1, 1, 1, 1, 0, 700, 98
27252, V, 1, 1, 1, 1, 0, 700, 98
27253, V, 1, 1, 1, 1, 0, 700, 98
27254, V, 1, 1, 1, 1, 0, 700, 98
27255, V, 1, 1, 1, 1, 0, 700, 98
27256, V, 1, 1, 1, 1, 0, 700, 98
27257, V, 1, 1, 1, 1, 0, 700, 98
27258, V, 1, 1, 1, 1, 0, 700, 98
27259, V, 1, 1, 1, 1, 0, 700, 98
27260, V, 1, 1, 1, 1, 0, 700, 98
27261, V, 1, 1, 1, 1, 0, 700, 98
27262, V, 1, 1, 1, 1, 0, 700, 98
27264, V, 1, 1, 1, 1, 0, 700, 98
27265, V, 1, 1, 1, 1, 0, 700, 98
27266, V, 1, 1, 1, 1, 0, 700, 98
27267, V, 1, 1, 1, 1, 0, 700, 98
27268, V, 1, 1, 1, 1, 0, 700, 98
27269, V, 1, 1, 1, 1, 0, 700, 98
27270, V, 1, 1, 1, 1, 0, 700, 98
27271, V, 1, 1, 1, 1, 0, 700, 98
27272, V, 1, 1, 1, 1, 0, 700, 98
27273, V, 1, 1, 1, 1, 0, 700, 98
27274, V, 1, 1, 1, 1, 0, 700, 98
27275, V, 1, 1, 1, 1, 0, 700, 98
27276, V, 1, 1, 1, 1, 0, 700, 98
27277, V, 1, 1, 1, 1, 0, 700, 98
27278, V, 1, 1, 1, 1, 0, 700, 98
27279, V, 1, 1, 1, 1, 0, 700, 98
27280, V, 1, 1, 1, 1, 0, 700, 98
27281, V, 1, 1, 1, 1, 0, 700, 98
27282, V, 1, 1, 1, 1, 0, 700, 98
27283, V, 1, 1, 1, 1, 0, 700, 98
27284, V, 1, 1, 1, 1, 0, 700, 98
27285, V, 1, 1, 1, 1, 0, 700, 98
27286, V, 1, 1, 1, 1, 0, 700, 98
27287, V, 1, 1, 1, 1, 0, 700, 98
27288, V, 1, 1, 1, 1, 0, 700, 98
27289, V, 1, 1, 1, 1, 0, 700, 98
27290, V, 1, 1, 1, 1, 0, 700, 98
27291, V, 1, 1, 1, 1, 0, 700, 98
27292, V, 1, 1, 1, 1, 0, 700, 98
27293, V, 1, 1, 1, 1, 0, 700, 98
27294, V, 1, 1, 1, 1, 0, 700, 98
27295, V, 1, 1, 1, 1, 0, 700, 98
27296, V, 1, 1, 1, 1, 0, 700, 98
27297, V, 1, 1, 1, 1, 0, 700, 98
27298, V, 1, 1, 1, 1, 0, 700, 98
27299, V, 1, 1, 1, 1, 0, 700, 98
27300, V, 1, 1, 1, 1, 0, 700, 98
27301, V, 1, 1, 1, 1, 0, 700, 98
27302, V, 1, 1, 1, 1, 0, 700, 98
27303, V, 1, 1, 1, 1, 0, 700, 98
27304, V, 1, 1, 1, 1, 0, 700, 98
27305, V, 1, 1, 1, 1, 0, 700, 98
27307, V, 1, 1, 1, 1, 0, 700, 98
27308, V, 1, 1, 1, 1, 0, 700, 98
27309, V, 1, 1, 1, 1, 0, 700, 98
27310, V, 1, 1, 1, 1, 0, 700, 98
27311, V, 1, 1, 1, 1, 0, 700, 98
27312, V, 1, 1, 1, 1, 0, 700, 98
27313, V, 1, 1, 1, 1, 0, 700, 98
27314, V, 1, 1, 1, 1, 0, 700, 98
27315, V, 1, 1, 1, 1, 0, 700, 98
27316, V, 1, 1, 1, 1, 0, 700, 98
27317, V, 1, 1, 1, 1, 0, 700, 98
27318, V, 1, 1, 1, 1, 0, 700, 98
27319, V, 1, 1, 1, 1, 0, 700, 98
27320, V, 1, 1, 1, 1, 0, 700, 98
27321, V, 1, 1, 1, 1, 0, 700, 98
27322, V, 1, 1, 1, 1, 0, 700, 98
27323, V, 1, 1, 1, 1, 0, 700, 98
27324, V, 1, 1, 1, 1, 0, 700, 98
27325, V, 1, 1, 1, 1, 0, 700, 98
27326, V, 1, 1, 1, 1, 0, 700, 98
27327, V, 1, 1, 1, 1, 0, 700, 98
27328, V, 1, 1, 1, 1, 0, 700, 98
27329, V, 1, 1, 1, 1, 0, 700, 98
27330, V, 1, 1, 1, 1, 0, 700, 98
27331, V, 1, 1, 1, 1, 0, 700, 98
27332, V, 1, 1, 1, 1, 0, 700, 98
27333, V, 1, 1, 1, 1, 0, 700, 98
27334, V, 1, 1, 1, 1, 0, 700, 98
27335, V, 1, 1, 1, 1, 0, 700, 98
27336, V, 1, 1, 1, 1, 0, 700, 98
27337, V, 1, 1, 1, 1, 0, 700, 98
27338, V, 1, 1, 1, 1, 0, 700, 98
27339, V, 1, 1, 1, 1, 0, 700, 98
27340, V, 1, 0, 0, 1, 0, 700, 98
27340, V, 1, 0, 0, 0, 0, 700, 98
27341, V, 1, 1, 0, 0, 0, 700, 98
27341, V, 1, 1, 0, 0, 0, 700, 98
27342, V, 1, 1, 1, 1, 0, 700, 98
27343, V, 1, 1, 1, 1, 0, 700, 98
27344, V, 1, 1, 1, 1, 0, 700, 98
27345, V, 1, 1, 1, 1, 0, 700, 98
27346, V, 1, 1, 1, 1, 0, 700, 98
27347, V, 1, 1, 1, 1, 0, 700, 98
27348, V, 1, 1, 1, 1, 0, 700, 98
27350, V, 1, 1, 1, 1, 0, 700, 98
27351, V, 1, 1, 1, 1, 0, 700, 98
27352, V, 1, 1, 1, 1, 0, 700, 98
27353, V, 1, 1, 1, 1, 0, 700, 98
27354, V, 1, 1, 1, 1, 0, 700, 98
27355, V, 1, 1, 1, 1, 0, 700, 98
27356, V, 1, 1, 1, 1, 0, 700, 98
27357, V, 1, 1, 1, 1, 0, 700, 98
27358, V, 1, 1, 1, 1, 0, 700, 98
27359, V, 1, 1, 1, 1, 0, 700, 98
27360, V, 1, 1, 1, 1, 0, 700, 98
27361, V, 1, 1, 1, 1, 0, 700, 98
27362, V, 1, 1, 1, 1, 0, 700, 98
27363, V, 1, 1, 1, 1, 0, 700, 98
27364, V, 1, 1, 1, 1, 0, 700, 98
27365, V, 1, 1, 1, 1, 0, 700, 98
27366, V, 1, 1, 1, 1, 0, 700, 98
27367, V, 1, 1, 1, 1, 0, 700, 98
27368, V, 1, 1, 1, 1, 0, 700, 98
27369, V, 1, 1, 1, 1, 0, 700, 98
27370, V, 1, 1, 1, 1, 0, 700, 98
27371, V, 1, 1, 1, 1, 0, 700, 98
27372, V, 1, 1, 1, 1, 0, 700, 98
27373, V, 1, 1, 1, 1, 0, 700, 98
27374, V, 1, 1, 1, 1, 0, 700, 98
27375, V, 1, 1, 1, 1, 0, 700, 98
27376, V, 1, 1, 1, 1, 0, 700, 98
27377, V, 1, 1, 1, 1, 0, 700, 98
27378, V, 1, 1, 1, 1, 0, 700, 98
27379, V, 1, 1, 1, 1, 0, 700, 98
27380, V, 1, 1, 1, 1, 0, 700, 98
27381, V, 1, 1, 1, 1, 0, 700, 98
27382, V, 1, 1, 1, 1, 0, 700, 98
27383, V, 1, 1, 1, 1, 0, 700, 98
27384, V, 1, 1, 1, 1, 0, 700, 98
27385, V, 1, 1, 1, 1, 0, 700, 98
27386, V, 1, 1, 1, 1, 0, 700, 98
27387, V, 1, 1, 1, 1, 0, 700, 98
27388, V, 1, 1, 1, 1, 0, 700, 98
27389, V, 1, 1, 1, 1, 0, 700, 98
27390, V, 1, 1, 1, 1, 0, 700, 98
27392, V, 1, 1, 1, 1, 0, 700, 98
27393, V, 1, 1, 1, 1, 0, 700, 98
27394, V, 1, 1, 1, 1, 0, 700, 98
27395, V, 1, 1, 1, 1, 0, 700, 98
27396, V, 1, 1, 1, 1, 0, 700, 98
27397, V, 1, 1, 1, 1, 0, 700, 98
27398, V, 1, 1, 1, 1, 0, 700, 98
27399, V, 1, 1, 1, 1, 0, 700, 98
27400, V, 1, 1, 1, 1, 0, 700, 98
27401, V, 1, 1, 1, 1, 0, 700, 98
27402, V, 1, 1, 1, 1, 0, 700, 98
27403, V, 1, 1, 1, 1, 0, 700, 98
27404, V, 1, 1, 1, 1, 0, 700, 98
27405, V, 1, 1, 1, 1, 0, 700, 98
27406, V, 1, 1, 1, 1, 0, 700, 98
27407, V, 1, 1, 1, 1, 0, 700, 98
27408, V, 1, 1, 1, 1, 0, 700, 98
27409, V, 1, 1, 1, 1, 0, 700, 98
27410, V, 1, 1, 1, 1, 0, 700, 98
27411, V, 1, 1, 1, 1, 0, 700, 98
27412, V, 1, 1, 1, 1, 0, 700, 98
27413, V, 1, 1, 1, 1, 0, 700, 98
27414, V, 1, 1, 1, 1, 0, 700, 98
27415, V, 1, 1, 1, 1, 0, 700, 98
27416, V, 1, 1, 1, 1, 0, 700, 98
27417, V, 1, 1, 1, 1, 0, 700, 98
27418, V, 1, 1, 1, 1, 0, 700, 98
27419, V, 1, 1, 1, 1, 0, 700, 98
27420, V, 1, 1, 1, 1, 0, 700, 98
27421, V, 1, 1, 1, 1, 0, 700, 98
27422, V, 1, 1, 1, 1, 0, 700, 98
27423, V, 1, 1, 1, 1, 0, 700, 98
27424, V, 1, 1, 1, 1, 0, 700, 98
27425, V, 1, 1, 1, 1, 0, 700, 98
27426, V, 1, 1, 1, 1, 0, 700, 98
27427, V, 1, 1, 1, 1, 0, 700, 98
27428, V, 1, 1, 1, 1, 0, 700, 98
27429, V, 1, 1, 1, 1, 0, 700, 98
27430, V, 1, 1, 1, 1, 0, 700, 98
27431, V, 1, 1, 1, 1, 0, 700, 98
27432, V, 1, 1, 1, 1, 0, 700, 98
27433, V, 1, 1, 1, 1, 0, 700, 98
27435, V, 1, 1, 1, 1, 0, 700, 98
27436, V, 1, 1, 1, 1, 0, 700, 98
27437, V, 1, 1, 1, 1, 0, 700, 98
27438, V, 1, 1, 1, 1, 0, 700, 98
27439, V, 1, 1, 1, 1, 0, 700, 98
27440, V, 1, 1, 1, 1, 0, 700, 98
27441, V, 1, 1, 1, 1, 0, 700, 98
27442, V, 1, 1, 1, 1, 0, 700, 98
27443, V, 1, 1, 1, 1, 0, 700, 98
27444, V, 1, 1, 1, 1, 0, 700, 98
27445, V, 1, 1, 1, 1, 0, 700, 98
27446, V, 1, 1, 1, 1, 0, 700, 98
27447, V, 1, 1, 1, 1, 0, 700, 98
27448, V, 1, 1, 1, 1, 0, 700, 98
27449, V, 1, 1, 1, 1, 0, 700, 98
27450, V, 1, 1, 1, 1, 0, 700, 98
27451, V, 1, 1, 1, 1, 0, 700, 98
27452, V, 1, 1, 1, 1, 0, 700, 98
27453, V, 1, 1, 1, 1, 0, 700, 98
27454, V, 1, 1, 1, 1, 0, 700, 98
27455, V, 1, 1, 1, 1, 0, 700, 98
27456, V, 1, 1, 1, 1, 0, 700, 98
27457, V, 1, 1, 1, 1, 0, 700, 98
27458, V, 1, 1, 1, 1, 0, 700, 98
27459, V, 1, 1, 1, 1, 0, 700, 98
27460, V, 1, 1, 1, 1, 0, 700, 98
27461, V, 1, 1, 1, 1, 0, 700, 98
27462, V, 1, 1, 1, 1, 0, 700, 98
27463, V, 1, 1, 1, 1, 0, 700, 98
27464, V, 1, 1, 1, 1, 0, 700, 98
27465, V, 1, 1, 1, 1, 0, 700, 98
27466, V, 1, 1, 1, 1, 0, 700, 98
27467, V, 1, 1, 1, 1, 0, 700, 98
27468, V, 1, 1, 1, 1, 0, 700, 98
27469, V, 1, 1, 1, 1, 0, 700, 98
27470, V, 1, 1, 1, 1, 0, 700, 98
27471, V, 1, 1, 1, 1, 0, 700, 98
27472, V, 1, 1, 1, 1, 0, 700, 98
27473, V, 1, 1, 1, 1, 0, 700, 98
27474, V, 1, 1, 1, 1, 0, 700, 98
27475, V, 1, 1, 1, 1, 0, 700, 98
27476, V, 1, 1, 1, 1, 0, 700, 98
27478, V, 1, 1, 1, 1, 0, 700, 98
27479, V, 1, 1, 1, 1, 0, 700, 98
27480, V, 1, 1, 1, 1, 0, 700, 98
27481, V, 1, 1, 1, 1, 0, 700, 98
27482, V, 1, 1, 1, 1, 0, 700, 98
27483, V, 1, 1, 1, 1, 0, 700, 98
27484, V, 1, 1, 1, 1, 0, 700, 98
27485, V, 1, 1, 1, 1, 0, 700, 98
27486, V, 1, 1, 1, 1, 0, 700, 98
27487, V, 1, 1, 1, 1, 0, 700, 98
27488, V, 1, 1, 1, 1, 0, 700, 98
27489, V, 1, 1, 1, 1, 0, 700, 98
27490, V, 1, 1, 1, 1, 0, 700, 98
27491, V, 1, 1, 1, 1, 0, 700, 98
27492, V, 1, 1, 1, 1, 0, 700, 98
27493, V, 1, 1, 1, 1, 0, 700, 98
27494, V, 1, 1, 1, 1, 0, 700, 98
27495, V, 1, 1, 1, 1, 0, 700, 98
27496, V, 1, 1, 1, 1, 0, 700, 98
27497, V, 1, 1, 1, 1, 0, 700, 98
27498, V, 1, 1, 1, 1, 0, 700, 98
27499, V, 1, 1, 1, 1, 0, 700, 98
27500, V, 1, 1, 1, 1, 0, 700, 98
27501, V, 1, 1, 1, 1, 0, 700, 98
27502, V, 1, 1, 1, 1, 0, 700, 98
27503, V, 1, 1, 1, 1, 0, 700, 98
27504, V, 1, 1, 1, 1, 0, 700, 98
27505, V, 1, 1, 1, 1, 0, 700, 98
27506, V, 1, 1, 1, 1, 0, 700, 98
27507, V, 1, 1, 1, 1, 0, 700, 98
27508, V, 1, 1, 1, 1, 0, 700, 98
27509, V, 1, 1, 1, 1, 0, 700, 98
27510, V, 1, 1, 1, 1, 0, 700, 98
27511, V, 1, 1, 1, 1, 0, 700, 98
27512, V, 1, 1, 1, 1, 0, 700, 98
27513, V, 1, 1, 1, 1, 0, 700, 98
27514, V, 1, 1, 1, 1, 0, 700, 98
27515, V, 1, 1, 1, 1, 0, 700, 98
27516, V, 1, 1, 1, 1, 0, 700, 98
27517, V, 1, 1, 1, 1, 0, 700, 98
27518, V, 1, 1, 1, 1, 0, 700, 98
27520, V, 1, 1, 1, 1, 0, 700, 98
27521, V, 1, 1, 1, 1, 0, 700, 98
27522, V, 1, 1, 1, 1, 0, 700, 98
27523, V, 1, 1, 1, 1, 0, 700, 98
27524, V, 1, 1, 1, 1, 0, 700, 98
27525, V, 1, 1, 1, 1, 0, 700, 98
27526, V, 1, 1, 1, 1, 0, 700, 98
27527, V, 1, 1, 1, 1, 0, 700, 98
27528, V, 1, 1, 1, 1, 0, 700, 98
27529, V, 1, 1, 1, 1, 0, 700, 98
27530, V, 1, 1, 1, 1, 0, 700, 98
27531, V, 1, 1, 1, 1, 0, 700, 98
27532, V, 1, 1, 1, 1, 0, 700, 98
27533, V, 1, 1, 1, 1, 0, 700, 98
27534, V, 1, 1, 1, 1, 0, 700, 98
27535, V, 1, 1, 1, 1, 0, 700, 98
27536, V, 1, 1, 1, 1, 0, 700, 98
27537, V, 1, 1, 1, 1, 0, 700, 98
27538, V, 1, 1, 1, 1, 0, 700, 98
27539, V, 1, 1, 1, 1, 0, 700, 98
27540, V, 1, 1, 1, 1, 0, 700, 98
27541, V, 1, 1, 1, 1, 0, 700, 98
27542, V, 1, 1, 1, 1, 0, 700, 98
27543, V, 1, 1, 1, 1, 0, 700, 98
27544, V, 1, 1, 1, 1, 0, 700, 98
27545, V, 1, 1, 1, 1, 0, 700, 98
27546, V, 1, 1, 1, 1, 0, 700, 98
27547, V, 1, 1, 1, 1, 0, 700, 98
27548, V, 1, 1, 1, 1, 0, 700, 98
27549, V, 1, 1, 1, 1, 0, 700, 98
27550, V, 1, 1, 1, 1, 0, 700, 98
27551, V, 1, 1, 1, 1, 0, 700, 98
27552, V, 1, 1, 1, 1, 0, 700, 98
27553, V, 1, 1, 1, 1, 0, 700, 98
27554, V, 1, 1, 1, 1, 0, 700, 98
27555, V, 1, 1, 1, 1, 0, 700, 98
27556, V, 1, 1, 1, 1, 0, 700, 98
27557, V, 1, 1, 1, 1, 0, 700, 98
27558, V, 1, 1, 1, 1, 0, 700, 98
27559, V, 1, 1, 1, 1, 0, 700, 98
27560, V, 1, 1, 1, 1, 0, 700, 98
27561, V, 1, 1, 1, 1, 0, 700, 98
27563, V, 1, 1, 1, 1, 0, 700, 98
27564, V, 1, 1, 1, 1, 0, 700, 98
27565, V, 1, 1, 1, 1, 0, 700, 98
27566, V, 1, 1, 1, 1, 0, 700, 98
27567, V, 1, 1, 1, 1, 0, 700, 98
27568, V, 1, 1, 1, 1, 0, 700, 98
27569, V, 1, 1, 1, 1, 0, 700, 98
27570, V, 1, 1, 1, 1, 0, 700, 98
27571, V, 1, 1, 1, 1, 0, 700, 98
27572, V, 1, 1, 1, 1, 0, 700, 98
27573, V, 1, 1, 1, 1, 0, 700, 98
27574, V, 1, 1, 1, 1, 0, 700, 98
27575, V, 1, 1, 1, 1, 0, 700, 98
27576, V, 1, 1, 1, 1, 0, 700, 98
27577, V, 1, 1, 1, 1, 0, 700, 98
27578, V, 1, 1, 1, 1, 0, 700, 98
27579, V, 1, 1, 1, 1, 0, 700, 98
27580, V, 1, 1, 1, 1, 0, 700, 98
27581, V, 1, 1, 1, 1, 0, 700, 98
27582, V, 1, 1, 1, 1, 0, 700, 98
27583, V, 1, 1, 1, 1, 0, 700, 98
27584, V, 1, 1, 1, 1, 0, 700, 98
27585, V, 1, 1, 1, 1, 0, 700, 98
27586, V, 1, 1, 1, 1, 0, 700, 98
27587, V, 1, 1, 1, 1, 0, 700, 98
27588, V, 1, 1, 1, 1, 0, 700, 98
27589, V, 1, 1, 1, 1, 0, 700, 98
27590, V, 1, 1, 1, 1, 0, 700, 98
27591, V, 1, 1, 1, 1, 0, 700, 98
27592, V, 1, 1, 1, 1, 0, 700, 98
27593, V, 1, 1, 1, 1, 0, 700, 98
27594, V, 1, 1, 1, 1, 0, 700, 98
27595, V, 1, 1, 1, 1, 0, 700, 98
27596, V, 1, 1, 1, 1, 0, 700, 98
27597, V, 1, 1, 1, 1, 0, 700, 98
27598, V, 1, 1, 1, 1, 0, 700, 98
27599, V, 1, 1, 1, 1, 0, 700, 98
27600, V, 1, 1, 1, 1, 0, 700, 98
27601, V, 1, 1, 1, 1, 0, 700, 98
27602, V, 1, 1, 1, 1, 0, 700, 98
27603, V, 1, 1, 1, 1, 0, 700, 98
27604, V, 1, 1, 1, 1, 0, 700, 98
27606, V, 1, 1, 1, 1, 0, 700, 98
27607, V, 1, 1, 1, 1, 0, 700, 98
27608, V, 1, 1, 1, 1, 0, 700, 98
27609, V, 1, 1, 1, 1, 0, 700, 98
27610, V, 1, 1, 1, 1, 0, 700, 98
27611, V, 1, 1, 1, 1, 0, 700, 98
27612, V, 1, 1, 1, 1, 0, 700, 98
27613, V, 1, 1, 1, 1, 0, 700, 98
27614, V, 1, 1, 1, 1, 0, 700, 98
27615, V, 1, 1, 1, 1, 0, 700, 98
27616, V, 1, 1, 1, 1, 0, 700, 98
27617, V, 1, 1, 1, 1, 0, 700, 98
27618, V, 1, 1, 1, 1, 0, 700, 98
27619, V, 1, 1, 1, 1, 0, 700, 98
27620, V, 1, 1, 1, 1, 0, 700, 98
27621, V, 1, 1, 1, 1, 0, 700, 98
27622, V, 1, 1, 1, 1, 0, 700, 98
27623, V, 1, 1, 1, 1, 0, 700, 98
27624, V, 1, 1, 1, 1, 0, 700, 98
27625, V, 1, 1, 1, 1, 0, 700, 98
27626, V, 1, 1, 1, 1, 0, 700, 98
27627, V, 1, 1, 1, 1, 0, 700, 98
27628, V, 1, 1, 1, 1, 0, 700, 98
27629, V, 1, 1, 1, 1, 0, 700, 98
27630, V, 1, 1, 1, 1, 0, 700, 98
27631, V, 1, 1, 1, 1, 0, 700, 98
27632, V, 1, 1, 1, 1, 0, 700, 98
27633, V, 1, 1, 1, 1, 0, 700, 98
27634, V, 1, 1, 1, 1, 0, 700, 98
27635, V, 1, 1, 1, 1, 0, 700, 98
27636, V, 1, 1, 1, 1, 0, 700, 98
27637, V, 1, 1, 1, 1, 0, 700, 98
27638, V, 1, 1, 1, 1, 0, 700, 98
27639, V, 1, 1, 1, 1, 0, 700, 98
27640, V, 1, 1, 1, 1, 0, 700, 98
27641, V, 1, 1, 1, 1, 0, 700, 98
27642, V, 1, 1, 1, 1, 0, 700, 98
27643, V, 1, 1, 1, 1, 0, 700, 98
27644, V, 1, 1, 1, 1, 0, 700, 98
27645, V, 1, 1, 1, 1, 0, 700, 98
27646, V, 1, 1, 1, 1, 0, 700, 98
27648, V, 1, 1, 1, 1, 0, 700, 98
27649, V, 1, 1, 1, 1, 0, 700, 98
27650, V, 1, 1, 1, 1, 0, 700, 98
27651, V, 1, 1, 1, 1, 0, 700, 98
27652, V, 1, 1, 1, 1, 0, 700, 98
27653, V, 1, 1, 1, 1, 0, 700, 98
27654, V, 1, 1, 1, 1, 0, 700, 98
27655, V, 1, 1, 1, 1, 0, 700, 98
27656, V, 1, 1, 1, 1, 0, 700, 98
27657, V, 1, 1, 1, 1, 0, 700, 98
27658, V, 1, 1, 1, 1, 0, 700, 98
27659, V, 1, 1, 1, 1, 0, 700, 98
27660, V, 1, 1, 1, 1, 0, 700, 98
27661, V, 1, 1, 1, 1, 0, 700, 98
27662, V, 1, 1, 1, 1, 0, 700, 98
27663, V, 1, 1, 1, 1, 0, 700, 98
27664, V, 1, 1, 1, 1, 0, 700, 98
27665, V, 1, 1, 1, 1, 0, 700, 98
27666, V, 1, 1, 1, 1, 0, 700, 98
27667, V, 1, 1, 1, 1, 0, 700, 98
27668, V, 1, 1, 1, 1, 0, 700, 98
27669, V, 1, 1, 1, 1, 0, 700, 98
27670, V, 1, 1, 1, 1, 0, 700, 98
27671, V, 1, 1, 1, 1, 0, 700, 98
27672, V, 1, 1, 1, 1, 0, 700, 98
27673, V, 1, 1, 1, 1, 0, 700, 98
27674, V, 1, 1, 1, 1, 0, 700, 98
27675, V, 1, 1, 1, 1, 0, 700, 98
27676, V, 1, 1, 1, 1, 0, 700, 98
27677, V, 1, 1, 1, 1, 0, 700, 98
27678, V, 1, 1, 1, 1, 0, 700, 98
27679, V, 1, 1, 1, 1, 0, 700, 98
27680, V, 1, 1, 1, 1, 0, 700, 98
27681, V, 1, 1, 1, 1, 0, 700, 98
27682, V, 1, 1, 1, 1, 0, 700, 98
27683, V, 1, 1, 1, 1, 0, 700, 98
27684, V, 1, 1, 1, 1, 0, 700, 98
27685, V, 1, 1, 1, 1, 0, 700, 98
27686, V, 1, 1, 1, 1, 0, 700, 98
27687, V, 1, 1, 1, 1, 0, 700, 98
27688, V, 1, 1, 1, 1, 0, 700, 98
27689, V, 1, 1, 1, 1, 0, 700, 98
27691, V, 1, 1, 1, 1, 0, 700, 98
27692, V, 1, 1, 1, 1, 0, 700, 98
27693, V, 1, 1, 1, 1, 0, 700, 98
27694, V, 1, 1, 1, 1, 0, 700, 98
27695, V, 1, 1, 1, 1, 0, 700, 98
27696, V, 1, 1, 1, 1, 0, 700, 98
27697, V, 1, 1, 1, 1, 0, 700, 98
27698, V, 1, 1, 1, 1, 0, 700, 98
27699, V, 1, 1, 1, 1, 0, 700, 98
27700, V, 1, 1, 1, 1, 0, 700, 98
27701, V, 1, 1, 1, 1, 0, 700, 98
27702, V, 1, 1, 1, 1, 0, 700, 98
27703, V, 1, 1, 1, 1, 0, 700, 98
27704, V, 1, 1, 1, 1, 0, 700, 98
27705, V, 1, 1, 1, 1, 0, 700, 98
27706, V, 1, 1, 1, 1, 0, 700, 98
27707, V, 1, 1, 1, 1, 0, 700, 98
27708, V, 1, 1, 1, 1, 0, 700, 98
27709, V, 1, 1, 1, 1, 0, 700, 98
27710, V, 1, 1, 1, 1, 0, 700, 98
27711, V, 1, 1, 1, 1, 0, 700, 98
27712, V, 1, 1, 1, 1, 0, 700, 98
27713, V, 1, 1, 1, 1, 0, 700, 98
27714, V, 1, 1, 1, 1, 0, 700, 98
27715, V, 1, 1, 1, 1, 0, 700, 98
27716, V, 1, 1, 1, 1, 0, 700, 98
27717, V, 1, 1, 1, 1, 0, 700, 98
27718, V, 1, 1, 1, 1, 0, 700, 98
27719, V, 1, 1, 1, 1, 0, 700, 98
27720, V, 1, 1, 1, 1, 0, 700, 98
27721, V, 1, 1, 1, 1, 0, 700, 98
27722, V, 1, 1, 1, 1, 0, 700, 98
27723, V, 1, 1, 1, 1, 0, 700, 98
27724, V, 1, 1, 1, 1, 0, 700, 98
27725, V, 1, 1, 1, 1, 0, 700, 98
27726, V, 1, 1, 1, 1, 0, 700, 98
27727, V, 1, 1, 1, 1, 0, 700, 98
27728, V, 1, 1, 1, 1, 0, 700, 98
27729, V, 1, 1, 1, 1, 0, 700, 98
27730, V, 1, 1, 1, 1, 0, 700, 98
27731, V, 1, 1, 1, 1, 0, 700, 98
27732, V, 1, 1, 1, 1, 0, 700, 98
27734, V, 1, 1, 1, 1, 0, 700, 98
27735, V, 1, 1, 1, 1, 0, 700, 98
27736, V, 1, 1, 1, 1, 0, 700, 98
27737, V, 1, 1, 1, 1, 0, 700, 98
27738, V, 1, 1, 1, 1, 0, 700, 98
27739, V, 1, 1, 1, 1, 0, 700, 98
27740, V, 1, 1, 1, 1, 0, 700, 98
27741, V, 1, 1, 1, 1, 0, 700, 98
27742, V, 1, 1, 1, 1, 0, 700, 98
27743, V, 1, 1, 1, 1, 0, 700, 98
27744, V, 1, 1, 1, 1, 0, 700, 98
27745, V, 1, 1, 1, 1, 0, 700, 98
27746, V, 1, 1, 1, 1, 0, 700, 98
27747, V, 1, 1, 1, 1, 0, 700, 98
27748, V, 1, 1, 1, 1, 0, 700, 98
27749, V, 1, 1, 1, 1, 0, 700, 98
27750, V, 1, 1, 1, 1, 0, 700, 98
27751, V, 1, 1, 1, 1, 0, 700, 98
27752, V, 1, 1, 1, 1, 0, 700, 98
27753, V, 1, 1, 1, 1, 0, 700, 98
27754, V, 1, 1, 1, 1, 0, 700, 98
27755, V, 1, 1, 1, 1, 0, 700, 98
27756, V, 1, 1, 1, 1, 0, 700, 98
27757, V, 1, 1, 1, 1, 0, 700, 98
27758, V, 1, 1, 1, 1, 0, 700, 98
27759, V, 1, 1, 1, 1, 0, 700, 98
27760, V, 1, 1, 1, 1, 0, 700, 98
27761, V, 1, 1, 1, 1, 0, 700, 98
27762, V, 1, 1, 1, 1, 0, 700, 98
27763, V, 1, 1, 1, 1, 0, 700, 98
27764, V, 1, 1, 1, 1, 0, 700, 98
27765, V, 1, 1, 1, 1, 0, 700, 98
27766, V, 1, 1, 1, 1, 0, 700, 98
27767, V, 1, 1, 1, 1, 0, 700, 98
27768, V, 1, 1, 1, 1, 0, 700, 98
27769, V, 1, 1, 1, 1, 0, 700, 98
27770, V, 1, 1, 1, 1, 0, 700, 98
27771, V, 1, 1, 1, 1, 0, 700, 98
27772, V, 1, 1, 1, 1, 0, 700, 98
27773, V, 1, 1, 1, 1, 0, 700, 98
27774, V, 1, 1, 1, 1, 0, 700, 98
27776, V, 1, 1, 1, 1, 0, 700, 98
27777, V, 1, 1, 1, 1, 0, 700, 98
27778, V, 1, 1, 1, 1, 0, 700, 98
27779, V, 1, 1, 1, 1, 0, 700, 98
27780, V, 1, 1, 1, 1, 0, 700, 98
27781, V, 1, 1, 1, 1, 0, 700, 98
27782, V, 1, 1, 1, 1, 0, 700, 98
27783, V, 1, 1, 1, 1, 0, 700, 98
27784, V, 1, 1, 1, 1, 0, 700, 98
27785, V, 1, 1, 1, 1, 0, 700, 98
27786, V, 1, 1, 1, 1, 0, 700, 98
27787, V, 1, 1, 1, 1, 0, 700, 98
27788, V, 1, 1, 1, 1, 0, 700, 98
27789, V, 1, 1, 1, 1, 0, 700, 98
27790, V, 1, 1, 1, 1, 0, 700, 98
27791, V, 1, 1, 1, 1, 0, 700, 98
27792, V, 1, 1, 1, 1, 0, 700, 98
27793, V, 1, 1, 1, 1, 0, 700, 98
27794, V, 1, 1, 1, 1, 0, 700, 98
27795, V, 1, 1, 1, 1, 0, 700, 98
27796, V, 1, 1, 1, 1, 0, 700, 98
27797, V, 1, 1, 1, 1, 0, 700, 98
27798, V, 1, 1, 1, 1, 0, 700, 98
27799, V, 1, 1, 1, 1, 0, 700, 98
27800, V, 1, 1, 1, 1, 0, 700, 98
27801, V, 1, 1, 1, 1, 0, 700, 98
27802, V, 1, 1, 1, 1, 0, 700, 98
27803, V, 1, 1, 1, 1, 0, 700, 98
27804, V, 1, 1, 1, 1, 0, 700, 98
27805, V, 1, 1, 1, 1, 0, 700, 98
27806, V, 1, 1, 1, 1, 0, 700, 98
27807, V, 1, 1, 1, 1, 0, 700, 98
27808, V, 1, 1, 1, 1, 0, 700, 98
27809, V, 1, 1, 1, 1, 0, 700, 98
27810, V, 1, 1, 1, 1, 0, 700, 98
27811, V, 1, 1, 1, 1, 0, 700, 98
27812, V, 1, 1, 1, 1, 0, 700, 98
27813, V, 1, 1, 1, 1, 0, 700, 98
27814, V, 1, 1, 1, 1, 0, 700, 98
27815, V, 1, 1, 1, 1, 0, 700, 98
27816, V, 1, 1, 1, 1, 0, 700, 98
27817, V, 1, 1, 1, 1, 0, 700, 98
27819, V, 1, 1, 1, 1, 0, 700, 98
27820, V, 1, 1, 1, 1, 0, 700, 98
27821, V, 1, 1, 1, 1, 0, 700, 98
27822, V, 1, 1, 1, 1, 0, 700, 98
27823, V, 1, 1, 1, 1, 0, 700, 98
27824, V, 1, 1, 1, 1, 0, 700, 98
27825, V, 1, 1, 1, 1, 0, 700, 98
27826, V, 1, 1, 1, 1, 0, 700, 98
27827, V, 1, 1, 1, 1, 0, 700, 98
27828, V, 1, 1, 1, 1, 0, 700, 98
27829, V, 1, 1, 1, 1, 0, 700, 98
27830, V, 1, 1, 1, 1, 0, 700, 98
27831, V, 1, 1, 1, 1, 0, 700, 98
27832, V, 1, 1, 1, 1, 0, 700, 98
27833, V, 1, 1, 1, 1, 0, 700, 98
27834, V, 1, 1, 1, 1, 0, 700, 98
27835, V, 1, 1, 1, 1, 0, 700, 98
27836, V, 1, 1, 1, 1, 0, 700, 98
27837, V, 1, 1, 1, 1, 0, 700, 98
27838, V, 1, 1, 1, 1, 0, 700, 98
27839, V, 1, 1, 1, 1, 0, 700, 98
27840, V, 1, 1, 1, 1, 0, 700, 98
27841, V, 1, 1, 1, 1, 0, 700, 98
27842, V, 1, 1, 1, 1, 0, 700, 98
27843, V, 1, 1, 1, 1, 0, 700, 98
27844, V, 1, 1, 1, 1, 0, 700, 98
27845, V, 1, 1, 1, 1, 0, 700, 98
27846, V, 1, 1, 1, 1, 0, 700, 98
27847, V, 1, 1, 1, 1, 0, 700, 98
27848, V, 1, 1, 1, 1, 0, 700, 98
27849, V, 1, 1, 1, 1, 0, 700, 98
27850, V, 1, 1, 1, 1, 0, 700, 98
27851, V, 1, 1, 1, 1, 0, 700, 98
27852, V, 1, 1, 1, 1, 0, 700, 98
27853, V, 1, 1, 1, 1, 0, 700, 98
27854, V, 1, 1, 1, 1, 0, 700, 98
27855, V, 1, 1, 1, 1, 0, 700, 98
27856, V, 1, 1, 1, 1, 0, 700, 98
27857, V, 1, 1, 1, 1, 0, 700, 98
27858, V, 1, 1, 1, 1, 0, 700, 98
27859, V, 1, 1, 1, 1, 0, 700, 98
27860, V, 1, 1, 1, 1, 0, 700, 98
27862, V, 1, 1, 1, 1, 0, 700, 98
27863, V, 1, 1, 1, 1, 0, 700, 98
27864, V, 1, 1, 1, 1, 0, 700, 98
27865, V, 1, 1, 1, 1, 0, 700, 98
27866, V, 1, 1, 1, 1, 0, 700, 98
27867, V, 1, 1, 1, 1, 0, 700, 98
27868, V, 1, 1, 1, 1, 0, 700, 98
27869, V, 1, 1, 1, 1, 0, 700, 98
27870, V, 1, 1, 1, 1, 0, 700, 98
27871, V, 1, 1, 1, 1, 0, 700, 98
27872, V, 1, 1, 1, 1, 0, 700, 98
27873, V, 1, 1, 1, 1, 0, 700, 98
27874, V, 1, 1, 1, 1, 0, 700, 98
27875, V, 1, 1, 1, 1, 0, 700, 98
27876, V, 1, 1, 1, 1, 0, 700, 98
27877, V, 1, 1, 1, 1, 0, 700, 98
27878, V, 1, 1, 1, 1, 0, 700, 98
27879, V, 1, 1, 1, 1, 0, 700, 98
27880, V, 1, 1, 1, 1, 0, 700, 98
27881, V, 1, 1, 1, 1, 0, 700, 98
27882, V, 1, 1, 1, 1, 0, 700, 98
27883, V, 1, 1, 1, 1, 0, 700, 98
27884, V, 1, 1, 1, 1, 0, 700, 98
27885, V, 1, 1, 1, 1, 0, 700, 98
27886, V, 1, 1, 1, 1, 0, 700, 98
27887, V, 1, 1, 1, 1, 0, 700, 98
27888, V, 1, 1, 1, 1, 0, 700, 98
27889, V, 1, 1, 1, 1, 0, 700, 98
27890, V, 1, 1, 1, 1, 0, 700, 98
27891, V, 1, 1, 1, 1, 0, 700, 98
27892, V, 1, 1, 1, 1, 0, 700, 98
27893, V, 1, 1, 1, 1, 0, 700, 98
27894, V, 1, 1, 1, 1, 0, 700, 98
27895, V, 1, 1, 1, 1, 0, 700, 98
27896, V, 1, 1, 1, 1, 0, 700, 98
27897, V, 1, 1, 1, 1, 0, 700, 98
27898, V, 1, 1, 1, 1, 0, 700, 98
27899, V, 1, 1, 1, 1, 0, 700, 98
27900, V, 1, 1, 1, 1, 0, 700, 98
27901, V, 1, 1, 1, 1, 0, 700, 98
27902, V, 1, 1, 1, 1, 0, 700, 98
27904, V, 1, 1, 1, 1, 0, 700, 98
27905, V, 1, 1, 1, 1, 0, 700, 98
27906, V, 1, 1, 1, 1, 0, 700, 98
27907, V, 1, 1, 1, 1, 0, 700, 98
27908, V, 1, 1, 1, 1, 0, 700, 98
27909, V, 1, 1, 1, 1, 0, 700, 98
27910, V, 1, 1, 1, 1, 0, 700, 98
27911, V, 1, 1, 1, 1, 0, 700, 98
27912, V, 1, 1, 1, 1, 0, 700, 98
27913, V, 1, 1, 1, 1, 0, 700, 98
27914, V, 1, 1, 1, 1, 0, 700, 98
27915, V, 1, 1, 1, 1, 0, 700, 98
27916, V, 1, 1, 1, 1, 0, 700, 98
27917, V, 1, 1, 1, 1, 0, 700, 98
27918, V, 1, 1, 1, 1, 0, 700, 98
27919, V, 1, 1, 1, 1, 0, 700, 98
27920, V, 1, 1, 1, 1, 0, 700, 98
27921, V, 1, 1, 1, 1, 0, 700, 98
27922, V, 1, 1, 1, 1, 0, 700, 98
27923, V, 1, 1, 1, 1, 0, 700, 98
27924, V, 1, 1, 1, 1, 0, 700, 98
27925, V, 1, 1, 1, 1, 0, 700, 98
27926, V, 1, 1, 1, 1, 0, 700, 98
27927, V, 1, 1, 1, 1, 0, 700, 98
27928, V, 1, 1, 1, 1, 0, 700, 98
27929, V, 1, 1, 1, 1, 0, 700, 98
27930, V, 1, 1, 1, 1, 0, 700, 98
27931, V, 1, 1, 1, 1, 0, 700, 98
27932, V, 1, 1, 1, 1, 0, 700, 98
27933, V, 1, 1, 1, 1, 0, 700, 98
27934, V, 1, 1, 1, 1, 0, 700, 98
27935, V, 1, 1, 1, 1, 0, 700, 98
27936, V, 1, 1, 1, 1, 0, 700, 98
27937, V, 1, 1, 1, 1, 0, 700, 98
27938, V, 1, 1, 1, 1, 0, 700, 98
27939, V, 1, 1, 1, 1, 0, 700, 98
27940, V, 1, 1, 1, 1, 0, 700, 98
27941, V, 1, 1, 1, 1, 0, 700, 98
27942, V, 1, 1, 1, 1, 0, 700, 98
27943, V, 1, 1, 1, 1, 0, 700, 98
27944, V, 1, 1, 1, 1, 0, 700, 98
27945, V, 1, 1, 1, 1, 0, 700, 98
27947, V, 1, 1, 1, 1, 0, 700, 98
27948, V, 1, 1, 1, 1, 0, 700, 98
27949, V, 1, 1, 1, 1, 0, 700, 98
27950, V, 1, 1, 1, 1, 0, 700, 98
27951, V, 1, 1, 1, 1, 0, 700, 98
27952, V, 1, 1, 1, 1, 0, 700, 98
27953, V, 1, 1, 1, 1, 0, 700, 98
27954, V, 1, 1, 1, 1, 0, 700, 98
27955, V, 1, 1, 1, 1, 0, 700, 98
27956, V, 1, 1, 1, 1, 0, 700, 98
27957, V, 1, 1, 1, 1, 0, 700, 98
27958, V, 1, 1, 1, 1, 0, 700, 98
27959, V, 1, 1, 1, 1, 0, 700, 98
27960, V, 1, 1, 1, 1, 0, 700, 98
27961, V, 1, 1, 1, 1, 0, 700, 98
27962, V, 1, 1, 1, 1, 0, 700, 98
27963, V, 1, 1, 1, 1, 0, 700, 98
27964, V, 1, 1, 1, 1, 0, 700, 98
27965, V, 1, 1, 1, 1, 0, 700, 98
27966, V, 1, 1, 1, 1, 0, 700, 98
27967, V, 1, 1, 1, 1, 0, 700, 98
27968, V, 1, 1, 1, 1, 0, 700, 98
27969, V, 1, 1, 1, 1, 0, 700, 98
27970, V, 1, 1, 1, 1, 0, 700, 98
27971, V, 1, 1, 1, 1, 0, 700, 98
27972, V, 1, 1, 1, 1, 0, 700, 98
27973, V, 1, 1, 1, 1, 0, 700, 98
27974, V, 1, 1, 1, 1, 0, 700, 98
27975, V, 1, 1, 1, 1, 0, 700, 98
27976, V, 1, 1, 1, 1, 0, 700, 98
27977, V, 1, 1, 1, 1, 0, 700, 98
27978, V, 1, 1, 1, 1, 0, 700, 98
27979, V, 1, 1, 1, 1, 0, 700, 98
27980, V, 1, 1, 1, 1, 0, 700, 98
27981, V, 1, 1, 1, 1, 0, 700, 98
27982, V, 1, 1, 1, 1, 0, 700, 98
27983, V, 1, 1, 1, 1, 0, 700, 98
27984, V, 1, 1, 1, 1, 0, 700, 98
27985, V, 1, 1, 1, 1, 0, 700, 98
27986, V, 1, 1, 1, 1, 0, 700, 98
27987, V, 1, 1, 1, 1, 0, 700, 98
27988, V, 1, 1, 1, 1, 0, 700, 98
27990, V, 1, 1, 1, 1, 0, 700, 98
27991, V, 1, 1, 1, 1, 0, 700, 98
27992, V, 1, 1, 1, 1, 0, 700, 98
27993, V, 1, 1, 1, 1, 0, 700, 98
27994, V, 1, 1, 1, 1, 0, 700, 98
27995, V, 1, 1, 1, 1, 0, 700, 98
27996, V, 1, 1, 1, 1, 0, 700, 98
27997, V, 1, 1, 1, 1, 0, 700, 98
27998, V, 1, 1, 1, 1, 0, 700, 98
27999, V, 1, 1, 1, 1, 0, 700, 98
28000, V, 1, 1, 1, 1, 0, 700, 98
28001, V, 1, 1, 1, 1, 0, 700, 98
28002, V, 1, 1, 1, 1, 0, 700, 98
28003, V, 1, 1, 1, 1, 0, 700, 98
28004, V, 1, 1, 1, 1, 0, 700, 98
28005, V, 1, 1, 1, 1, 0, 700, 98
28006, V, 1, 1, 1, 1, 0, 700, 98
28007, V, 1, 1, 1, 1, 0, 700, 98
28008, V, 1, 1, 1, 1, 0, 700, 98
28009, V, 1, 1, 1, 1, 0, 700, 98
28010, V, 1, 1, 1, 1, 0, 700, 98
28011, V, 1, 1, 1, 1, 0, 700, 98
28012, V, 1, 1, 1, 1, 0, 700, 98
28013, V, 1, 1, 1, 1, 0, 700, 98
28014, V, 1, 1, 1, 1, 0, 700, 98
28015, V, 1, 1, 1, 1, 0, 700, 98
28016, V, 1, 1, 1, 1, 0, 700, 98
28017, V, 1, 1, 1, 1, 0, 700, 98
28018, V, 1, 1, 1, 1, 0, 700, 98
28019, V, 1, 1, 1, 1, 0, 700, 98
28020, V, 1, 1, 1, 1, 0, 700, 98
28021, V, 1, 1, 1, 1, 0, 700, 98
28022, V, 1, 1, 1, 1, 0, 700, 98
28023, V, 1, 1, 1, 1, 0, 700, 98
28024, V, 1, 1, 1, 1, 0, 700, 98
28025, V, 1, 1, 1, 1, 0, 700, 98
28026, V, 1, 1, 1, 1, 0, 700, 98
28027, V, 1, 1, 1, 1, 0, 700, 98
28028, V, 1, 1, 1, 1, 0, 700, 98
28029, V, 1, 1, 1, 1, 0, 700, 98
28030, V, 1, 1, 1, 1, 0, 700, 98
28032, V, 1, 1, 1, 1, 0, 700, 98
28033, V, 1, 1, 1, 1, 0, 700, 98
28034, V, 1, 1, 1, 1, 0, 700, 98
28035, V, 1, 1, 1, 1, 0, 700, 98
28036, V, 1, 1, 1, 1, 0, 700, 98
28037, V, 1, 1, 1, 1, 0, 700, 98
28038, V, 1, 1, 1, 1, 0, 700, 98
28039, V, 1, 1, 1, 1, 0, 700, 98
28040, V, 1, 1, 1, 1, 0, 700, 98
28041, V, 1, 1, 1, 1, 0, 700, 98
28042, V, 1, 1, 1, 1, 0, 700, 98
28043, V, 1, 1, 1, 1, 0, 700, 98
28044, V, 1, 1, 1, 1, 0, 700, 98
28045, V, 1, 1, 1, 1, 0, 700, 98
28046, V, 1, 1, 1, 1, 0, 700, 98
28047, V, 1, 1, 1, 1, 0, 700, 98
28048, V, 1, 1, 1, 1, 0, 700, 98
28049, V, 1, 1, 1, 1, 0, 700, 98
28050, V, 1, 1, 1, 1, 0, 700, 98
28051, V, 1, 1, 1, 1, 0, 700, 98
28052, V, 1, 1, 1, 1, 0, 700, 98
28053, V, 1, 1, 1, 1, 0, 700, 98
28054, V, 1, 1, 1, 1, 0, 700, 98
28055, V, 1, 1, 1, 1, 0, 700, 98
28056, V, 1, 1, 1, 1, 0, 700, 98
28057, V, 1, 1, 1, 1, 0, 700, 98
28058, V, 1, 1, 1, 1, 0, 700, 98
28059, V, 1, 1, 1, 1, 0, 700, 98
28060, V, 1, 1, 1, 1, 0, 700, 98
28061, V, 1, 1, 1, 1, 0, 700, 98
28062, V, 1, 1, 1, 1, 0, 700, 98
28063, V, 1, 1, 1, 1, 0, 700, 98
28064, V, 1, 1, 1, 1, 0, 700, 98
28065, V, 1, 1, 1, 1, 0, 700, 98
28066, V, 1, 1, 1, 1, 0, 700, 98
28067, V, 1, 1, 1, 1, 0, 700, 98
28068, V, 1, 1, 1, 1, 0, 700, 98
28069, V, 1, 1, 1, 1, 0, 700, 98
28070, V, 1, 1, 1, 1, 0, 700, 98
28071, V, 1, 1, 1, 1, 0, 700, 98
28072, V, 1, 1, 1, 1, 0, 700, 98
28073, V, 1, 1, 1, 1, 0, 700, 98
28075, V, 1, 1, 1, 1, 0, 700, 98
28076, V, 1, 1, 1, 1, 0, 700, 98
28077, V, 1, 1, 1, 1, 0, 700, 98
28078, V, 1, 1, 1, 1, 0, 700, 98
28079, V, 1, 1, 1, 1, 0, 700, 98
28080, V, 1, 1, 1, 1, 0, 700, 98
28081, V, 1, 1, 1, 1, 0, 700, 98
28082, V, 1, 1, 1, 1, 0, 700, 98
28083, V, 1, 1, 1, 1, 0, 700, 98
28084, V, 1, 1, 1, 1, 0, 700, 98
28085, V, 1, 1, 1, 1, 0, 700, 98
28086, V, 1, 1, 1, 1, 0, 700, 98
28087, V, 1, 1, 1, 1, 0, 700, 98
28088, V, 1, 1, 1, 1, 0, 700, 98
28089, V, 1, 1, 1, 1, 0, 700, 98
28090, V, 1, 1, 1, 1, 0, 700, 98
28091, V, 1, 1, 1, 1, 0, 700, 98
28092, V, 1, 1, 1, 1, 0, 700, 98
28093, V, 1, 1, 1, 1, 0, 700, 98
28094, V, 1, 1, 1, 1, 0, 700, 98
28095, V, 1, 1, 1, 1, 0, 700, 98
28096, V, 1, 1, 1, 1, 0, 700, 98
28097, V, 1, 1, 1, 1, 0, 700, 98
28098, V, 1, 1, 1, 1, 0, 700, 98
28099, V, 1, 1, 1, 1, 0, 700, 98
28100, V, 1, 1, 1, 1, 0, 700, 98
28101, V, 1, 1, 1, 1, 0, 700, 98
28102, V, 1, 1, 1, 1, 0, 700, 98
28103, V, 1, 1, 1, 1, 0, 700, 98
28104, V, 1, 1, 1, 1, 0, 700, 98
28105, V, 1, 1, 1, 1, 0, 700, 98
28106, V, 1, 1, 1, 1, 0, 700, 98
28107, V, 1, 1, 1, 1, 0, 700, 98
28108, V, 1, 1, 1, 1, 0, 700, 98
28109, V, 1, 1, 1, 1, 0, 700, 98
28110, V, 1, 1, 1, 1, 0, 700, 98
28111, V, 1, 1, 1, 1, 0, 700, 98
28112, V, 1, 1, 1, 1, 0, 700, 98
28113, V, 1, 1, 1, 1, 0, 700, 98
28114, V, 1, 1, 1, 1, 0, 700, 98
28115, V, 1, 1, 1, 1, 0, 700, 98
28116, V, 1, 1, 1, 1, 0, 700, 98
28118, V, 1, 1, 1, 1, 0, 700, 98
28119, V, 1, 1, 1, 1, 0, 700, 98
28120, V, 1, 1, 1, 1, 0, 700, 98
28121, V, 1, 1, 1, 1, 0, 700, 98
28122, V, 1, 1, 1, 1, 0, 700, 98
28123, V, 1, 1, 1, 1, 0, 700, 98
28124, V, 1, 1, 1, 1, 0, 700, 98
28125, V, 1, 1, 1, 1, 0, 700, 98
28126, V, 1, 1, 1, 1, 0, 700, 98
28127, V, 1, 1, 1, 1, 0, 700, 98
28128, V, 1, 1, 1, 1, 0, 700, 98
28129, V, 1, 1, 1, 1, 0, 700, 98
28130, V, 1, 1, 1, 1, 0, 700, 98
28131, V, 1, 1, 1, 1, 0, 700, 98
28132, V, 1, 1, 1, 1, 0, 700, 98
28133, V, 1, 1, 1, 1, 0, 700, 98
28134, V, 1, 1, 1, 1, 0, 700, 98
28135, V, 1, 1, 1, 1, 0, 700, 98
28136, V, 1, 1, 1, 1, 0, 700, 98
28137, V, 1, 1, 1, 1, 0, 700, 98
28138, V, 1, 1, 1, 1, 0, 700, 98
28139, V, 1, 1, 1, 1, 0, 700, 98
28140, V, 1, 1, 1, 1, 0, 700, 98
28141, V, 1, 1, 1, 1, 0, 700, 98
28142, V, 1, 1, 1, 1, 0, 700, 98
28143, V, 1, 1, 1, 1, 0, 700, 98
28144, V, 1, 1, 1, 1, 0, 700, 98
28145, V, 1, 1, 1, 1, 0, 700, 98
28146, V, 1, 1, 1, 1, 0, 700, 98
28147, V, 1, 1, 1, 1, 0, 700, 98
28148, V, 1, 1, 1, 1, 0, 700, 98
28149, V, 1, 1, 1, 1, 0, 700, 98
28150, V, 1, 1, 1, 1, 0, 700, 98
28151, V, 1, 1, 1, 1, 0, 700, 98
28152, V, 1, 1, 1, 1, 0, 700, 98
28153, V, 1, 1, 1, 1, 0, 700, 98
28154, V, 1, 1, 1, 1, 0, 700, 98
28155, V, 1, 1, 1, 1, 0, 700, 98
28156, V, 1, 1, 1, 1, 0, 700, 98
28157, V, 1, 1, 1, 1, 0, 700, 98
28158, V, 1, 1, 1, 1, 0, 700, 98
28160, V, 1, 1, 1, 1, 0, 700, 98
28161, V, 1, 1, 1, 1, 0, 700, 98
28162, V, 1, 1, 1, 1, 0, 700, 98
28163, V, 1, 1, 1, 1, 0, 700, 98
28164, V, 1, 1, 1, 1, 0, 700, 98
28165, V, 1, 1, 1, 1, 0, 700, 98
28166, V, 1, 1, 1, 1, 0, 700, 98
28167, V, 1, 1, 1, 1, 0, 700, 98
28168, V, 1, 1, 1, 1, 0, 700, 98
28169, V, 1, 1, 1, 1, 0, 700, 98
28170, V, 1, 1, 1, 1, 0, 700, 98
28171, V, 1, 1, 1, 1, 0, 700, 98
28172, V, 1, 1, 1, 1, 0, 700, 98
28173, V, 1, 1, 1, 1, 0, 700, 98
28174, V, 1, 1, 1, 1, 0, 700, 98
28175, V, 1, 1, 1, 1, 0, 700, 98
28176, V, 1, 1, 1, 1, 0, 700, 98
28177, V, 1, 1, 1, 1, 0, 700, 98
28178, V, 1, 1, 1, 1, 0, 700, 98
28179, V, 1, 1, 1, 1, 0, 700, 98
28180, V, 1, 1, 1, 1, 0, 700, 98
28181, V, 1, 1, 1, 1, 0, 700, 98
28182, V, 1, 1, 1, 1, 0, 700, 98
28183, V, 1, 1, 1, 1, 0, 700, 98
28184, V, 1, 1, 1, 1, 0, 700, 98
28185, V, 1, 1, 1, 1, 0, 700, 98
28186, V, 1, 1, 1, 1, 0, 700, 98
28187, V, 1, 1, 1, 1, 0, 700, 98
28188, V, 1, 1, 1, 1, 0, 700, 98
28189, V, 1, 1, 1, 1, 0, 700, 98
28190, V, 1, 1, 1, 1, 0, 700, 98
28191, V, 1, 1, 1, 1, 0, 700, 98
28192, V, 1, 1, 1, 1, 0, 700, 98
28193, V, 1, 1, 1, 1, 0, 700, 98
28194, V, 1, 1, 1, 1, 0, 700, 98
28195, V, 1, 1, 1, 1, 0, 700, 98
28196, V, 1, 1, 1, 1, 0, 700, 98
28197, V, 1, 1, 1, 1, 0, 700, 98
28198, V, 1, 1, 1, 1, 0, 700, 98
28199, V, 1, 1, 1, 1, 0, 700, 98
28200, V, 1, 1, 1, 1, 0, 700, 98
28201, V, 1, 1, 1, 1, 0, 700, 98
28203, V, 1, 1, 1, 1, 0, 700, 98
28204, V, 1, 1, 1, 1, 0, 700, 98
28205, V, 1, 1, 1, 1, 0, 700, 98
28206, V, 1, 1, 1, 1, 0, 700, 98
28207, V, 1, 1, 1, 1, 0, 700, 98
28208, V, 1, 1, 1, 1, 0, 700, 98
28209, V, 1, 1, 1, 1, 0, 700, 98
28210, V, 1, 1, 1, 1, 0, 700, 98
28211, V, 1, 1, 1, 1, 0, 700, 98
28212, V, 1, 1, 1, 1, 0, 700, 98
28213, V, 1, 1, 1, 1, 0, 700, 98
28214, V, 1, 1, 1, 1, 0, 700, 98
28215, V, 1, 1, 1, 1, 0, 700, 98
28216, V, 1, 1, 1, 1, 0, 700, 98
28217, V, 1, 1, 1, 1, 0, 700, 98
28218, V, 1, 1, 1, 1, 0, 700, 98
28219, V, 1, 1, 1, 1, 0, 700, 98
28220, V, 1, 1, 1, 1, 0, 700, 98
28221, V, 1, 1, 1, 1, 0, 700, 98
28222, V, 1, 1, 1, 1, 0, 700, 98
28223, V, 1, 1, 1, 1, 0, 700, 98
28224, V, 1, 1, 1, 1, 0, 700, 98
28225, V, 1, 1, 1, 1, 0, 700, 98
28226, V, 1, 1, 1, 1, 0, 700, 98
28227, V, 1, 1, 1, 1, 0, 700, 98
28228, V, 1, 1, 1, 1, 0, 700, 98
28229, V, 1, 1, 1, 1, 0, 700, 98
28230, V, 1, 1, 1, 1, 0, 700, 98
28231, V, 1, 1, 1, 1, 0, 700, 98
28232, V, 1, 1, 1, 1, 0, 700, 98
28233, V, 1, 1, 1, 1, 0, 700, 98
28234, V, 1, 1, 1, 1, 0, 700, 98
28235, V, 1, 1, 1, 1, 0, 700, 98
28236, V, 1, 1, 1, 1, 0, 700, 98
28237, V, 1, 1, 1, 1, 0, 700, 98
28238, V, 1, 1, 1, 1, 0, 700, 98
28239, V, 1, 1, 1, 1, 0, 700, 98
28240, V, 1, 1, 1, 1, 0, 700, 98
28241, V, 1, 1, 1, 1, 0, 700, 98
28242, V, 1, 1, 1, 1, 0, 700, 98
28243, V, 1, 1, 1, 1, 0, 700, 98
28244, V, 1, 1, 1, 1, 0, 700, 98
28246, V, 1, 1, 1, 1, 0, 700, 98
28247, V, 1, 1, 1, 1, 0, 700, 98
28248, V, 1, 1, 1, 1, 0, 700, 98
28249, V, 1, 1, 1, 1, 0, 700, 98
28250, V, 1, 1, 1, 1, 0, 700, 98
28251, V, 1, 1, 1, 1, 0, 700, 98
28252, V, 1, 1, 1, 1, 0, 700, 98
28253, V, 1, 1, 1, 1, 0, 700, 98
28254, V, 1, 1, 1, 1, 0, 700, 98
28255, V, 1, 1, 1, 1, 0, 700, 98
28256, V, 1, 1, 1, 1, 0, 700, 98
28257, V, 1, 1, 1, 1, 0, 700, 98
28258, V, 1, 1, 1, 1, 0, 700, 98
28259, V, 1, 1, 1, 1, 0, 700, 98
28260, V, 1, 1, 1, 1, 0, 700, 98
28261, V, 1, 1, 1, 1, 0, 700, 98
28262, V, 1, 1, 1, 1, 0, 700, 98
28263, V, 1, 1, 1, 1, 0, 700, 98
28264, V, 1, 1, 1, 1, 0, 700, 98
28265, V, 1, 1, 1, 1, 0, 700, 98
28266, V, 1, 1, 1, 1, 0, 700, 98
28267, V, 1, 1, 1, 1, 0, 700, 98
28268, V, 1, 1, 1, 1, 0, 700, 98
28269, V, 1, 1, 1, 1, 0, 700, 98
28270, V, 1, 1, 1, 1, 0, 700, 98
28271, V, 1, 1, 1, 1, 0, 700, 98
28272, V, 1, 1, 1, 1, 0, 700, 98
28273, V, 1, 1, 1, 1, 0, 700, 98
28274, V, 1, 1, 1, 1, 0, 700, 98
28275, V, 1, 1, 1, 1, 0, 700, 98
28276, V, 1, 1, 1, 1, 0, 700, 98
28277, V, 1, 1, 1, 1, 0, 700, 98
28278, V, 1, 1, 1, 1, 0, 700, 98
28279, V, 1, 1, 1, 1, 0, 700, 98
28280, V, 1, 1, 1, 1, 0, 700, 98
28281, V, 1, 1, 1, 1, 0, 700, 98
28282, V, 1, 1, 1, 1, 0, 700, 98
28283, V, 1, 1, 1, 1, 0, 700, 98
28284, V, 1, 1, 1, 1, 0, 700, 98
28285, V, 1, 1, 1, 1, 0, 700, 98
28286, V, 1, 1, 1, 1, 0, 700, 98
28288, V, 1, 1, 1, 1, 0, 700, 98
28289, V, 1, 1, 1, 1, 0, 700, 98
28290, V, 1, 1, 1, 1, 0, 700, 98
28291, V, 1, 1, 1, 1, 0, 700, 98
28292, V, 1, 1, 1, 1, 0, 700, 98
28293, V, 1, 1, 1, 1, 0, 700, 98
28294, V, 1, 1, 1, 1, 0, 700, 98
28295, V, 1, 1, 1, 1, 0, 700, 98
28296, V, 1, 1, 1, 1, 0, 700, 98
28297, V, 1, 1, 1, 1, 0, 700, 98
28298, V, 1, 1, 1, 1, 0, 700, 98
28299, V, 1, 1, 1, 1, 0, 700, 98
28300, V, 1, 1, 1, 1, 0, 700, 98
28301, V, 1, 1, 1, 1, 0, 700, 98
28302, V, 1, 1, 1, 1, 0, 700, 98
28303, V, 1, 1, 1, 1, 0, 700, 98
28304, V, 1, 1, 1, 1, 0, 700, 98
28305, V, 1, 1, 1, 1, 0, 700, 98
28306, V, 1, 1, 1, 1, 0, 700, 98
28307, V, 1, 1, 1, 1, 0, 700, 98
28308, V, 1, 1, 1, 1, 0, 700, 98
28309, V, 1, 1, 1, 1, 0, 700, 98
28310, V, 1, 1, 1, 1, 0, 700, 98
28311, V, 1, 1, 1, 1, 0, 700, 98
28312, V, 1, 1, 1, 1, 0, 700, 98
28313, V, 1, 1, 1, 1, 0, 700, 98
28314, V, 1, 1, 1, 1, 0, 700, 98
28315, V, 1, 1, 1, 1, 0, 700, 98
28316, V, 1, 1, 1, 1, 0, 700, 98
28317, V, 1, 1, 1, 1, 0, 700, 98
28318, V, 1, 1, 1, 1, 0, 700, 98
28319, V, 1, 1, 1, 1, 0, 700, 98
28320, V, 1, 1, 1, 1, 0, 700, 98
28321, V, 1, 1, 1, 1, 0, 700, 98
28322, V, 1, 1, 1, 1, 0, 700, 98
28323, V, 1, 1, 1, 1, 0, 700, 98
28324, V, 1, 1, 1, 1, 0, 700, 98
28325, V, 1, 1, 1, 1, 0, 700, 98
28326, V, 1, 1, 1, 1, 0, 700, 98
28327, V, 1, 1, 1, 1, 0, 700, 98
28328, V, 1, 1, 1, 1, 0, 700, 98
28329, V, 1, 1, 1, 1, 0, 700, 98
28331, V, 1, 1, 1, 1, 0, 700, 98
28332, V, 1, 1, 1, 1, 0, 700, 98
28333, V, 1, 1, 1, 1, 0, 700, 98
28334, V, 1, 1, 1, 1, 0, 700, 98
28335, V, 1, 1, 1, 1, 0, 700, 98
28336, V, 1, 1, 1, 1, 0, 700, 98
28337, V, 1, 1, 1, 1, 0, 700, 98
28338, V, 1, 1, 1, 1, 0, 700, 98
28339, V, 1, 1, 1, 1, 0, 700, 98
28340, V, 1, 1, 1, 1, 0, 700, 98
28341, V, 1, 1, 1, 1, 0, 700, 98
28342, V, 1, 1, 1, 1, 0, 700, 98
28343, V, 1, 1, 1, 1, 0, 700, 98
28344, V, 1, 1, 1, 1, 0, 700, 98
28345, V, 1, 1, 1, 1, 0, 700, 98
28346, V, 1, 1, 1, 1, 0, 700, 98
28347, V, 1, 1, 1, 1, 0, 700, 98
28348, V, 1, 1, 1, 1, 0, 700, 98
28349, V, 1, 1, 1, 1, 0, 700, 98
28350, V, 1, 1, 1, 1, 0, 700, 98
28351, V, 1, 1, 1, 1, 0, 700, 98
28352, V, 1, 1, 1, 1, 0, 700, 98
28353, V, 1, 1, 1, 1, 0, 700, 98
28354, V, 1, 1, 1, 1, 0, 700, 98
28355, V, 1, 1, 1, 1, 0, 700, 98
28356, V, 1, 1, 1, 1, 0, 700, 98
28357, V, 1, 1, 1, 1, 0, 700, 98
28358, V, 1, 1, 1, 1, 0, 700, 98
28359, V, 1, 1, 1, 1, 0, 700, 98
28360, V, 1, 1, 1, 1, 0, 700, 98
28361, V, 1, 1, 1, 1, 0, 700, 98
28362, V, 1, 1, 1, 1, 0, 700, 98
28363, V, 1, 1, 1, 1, 0, 700, 98
28364, V, 1, 1, 1, 1, 0, 700, 98
28365, V, 1, 1, 1, 1, 0, 700, 98
28366, V, 1, 1, 1, 1, 0, 700, 98
28367, V, 1, 1, 1, 1, 0, 700, 98
28368, V, 1, 1, 1, 1, 0, 700, 98
28369, V, 1, 1, 1, 1, 0, 700, 98
28370, V, 1, 1, 1, 1, 0, 700, 98
28371, V, 1, 1, 1, 1, 0, 700, 98
28372, V, 1, 1, 1, 1, 0, 700, 98
28374, V, 1, 1, 1, 1, 0, 700, 98
28375, V, 1, 1, 1, 1, 0, 700, 98
28376, V, 1, 1, 1, 1, 0, 700, 98
28377, V, 1, 1, 1, 1, 0, 700, 98
28378, V, 1, 1, 1, 1, 0, 700, 98
28379, V, 1, 1, 1, 1, 0, 700, 98
28380, V, 1, 1, 1, 1, 0, 700, 98
28381, V, 1, 1, 1, 1, 0, 700, 98
28382, V, 1, 1, 1, 1, 0, 700, 98
28383, V, 1, 1, 1, 1, 0, 700, 98
28384, V, 1, 1, 1, 1, 0, 700, 98
28385, V, 1, 1, 1, 1, 0, 700, 98
28386, V, 1, 1, 1, 1, 0, 700, 98
28387, V, 1, 1, 1, 1, 0, 700, 98
28388, V, 1, 1, 1, 1, 0, 700, 98
28389, V, 1, 1, 1, 1, 0, 700, 98
28390, V, 1, 1, 1, 1, 0, 700, 98
28391, V, 1, 1, 1, 1, 0, 700, 98
28392, V, 1, 1, 1, 1, 0, 700, 98
28393, V, 1, 1, 1, 1, 0, 700, 98
28394, V, 1, 1, 1, 1, 0, 700, 98
28395, V, 1, 1, 1, 1, 0, 700, 98
28396, V, 1, 1, 1, 1, 0, 700, 98
28397, V, 1, 1, 1, 1, 0, 700, 98
28398, V, 1, 1, 1, 1, 0, 700, 98
28399, V, 1, 1, 1, 1, 0, 700, 98
28400, V, 1, 1, 1, 1, 0, 700, 98
28401, V, 1, 1, 1, 1, 0, 700, 98
28402, V, 1, 1, 1, 1, 0, 700, 98
28403, V, 1, 1, 1, 1, 0, 700, 98
28404, V, 1, 1, 1, 1, 0, 700, 98
28405, V, 1, 1, 1, 1, 0, 700, 98
28406, V, 1, 1, 1, 1, 0, 700, 98
28407, V, 1, 1, 1, 1, 0, 700, 98
28408, V, 1, 1, 1, 1, 0, 700, 98
28409, V, 1, 1, 1, 1, 0, 700, 98
28410, V, 1, 1, 1, 1, 0, 700, 98
28411, V, 1, 1, 1, 1, 0, 700, 98
28412, V, 1, 1, 1, 1, 0, 700, 98
28413, V, 1, 1, 1, 1, 0, 700, 98
28414, V, 1, 1, 1, 1, 0, 700, 98
28416, V, 1, 1, 1, 1, 0, 700, 98
28417, V, 1, 1, 1, 1, 0, 700, 98
28418, V, 1, 1, 1, 1, 0, 700, 98
28419, V, 1, 1, 1, 1, 0, 700, 98
28420, V, 1, 1, 1, 1, 0, 700, 98
28421, V, 1, 1, 1, 1, 0, 700, 98
28422, V, 1, 1, 1, 1, 0, 700, 98
28423, V, 1, 1, 1, 1, 0, 700, 98
28424, V, 1, 1, 1, 1, 0, 700, 98
28425, V, 1, 1, 1, 1, 0, 700, 98
28426, V, 1, 1, 1, 1, 0, 700, 98
28427, V, 1, 1, 1, 1, 0, 700, 98
28428, V, 1, 1, 1, 1, 0, 700, 98
28429, V, 1, 1, 1, 1, 0, 700, 98
28430, V, 1, 1, 1, 1, 0, 700, 98
28431, V, 1, 1, 1, 1, 0, 700, 98
28432, V, 1, 1, 1, 1, 0, 700, 98
28433, V, 1, 1, 1, 1, 0, 700, 98
28434, V, 1, 1, 1, 1, 0, 700, 98
28435, V, 1, 1, 1, 1, 0, 700, 98
28436, V, 1, 1, 1, 1, 0, 700, 98
28437, V, 1, 1, 1, 1, 0, 700, 98
28438, V, 1, 1, 1, 1, 0, 700, 98
28439, V, 1, 1, 1, 1, 0, 700, 98
28440, V, 1, 1, 1, 1, 0, 700, 98
28441, V, 1, 1, 1, 1, 0, 700, 98
28442, V, 1, 1, 1, 1, 0, 700, 98
28443, V, 1, 1, 1, 1, 0, 700, 98
28444, V, 1, 1, 1, 1, 0, 700, 98
28445, V, 1, 1, 1, 1, 0, 700, 98
28446, V, 1, 1, 1, 1, 0, 700, 98
28447, V, 1, 1, 1, 1, 0, 700, 98
28448, V, 1, 1, 1, 1, 0, 700, 98
28449, V, 1, 1, 1, 1, 0, 700, 98
28450, V, 1, 1, 1, 1, 0, 700, 98
28451, V, 1, 1, 1, 1, 0, 700, 98
28452, V, 1, 1, 1, 1, 0, 700, 98
28453, V, 1, 1, 1, 1, 0, 700, 98
28454, V, 1, 1, 1, 1, 0, 700, 98
28455, V, 1, 1, 1, 1, 0, 700, 98
28456, V, 1, 1, 1, 1, 0, 700, 98
28457, V, 1, 1, 1, 1, 0, 700, 98
28459, V, 1, 1, 1, 1, 0, 700, 98
28460, V, 1, 1, 1, 1, 0, 700, 98
28461, V, 1, 1, 1, 1, 0, 700, 98
28462, V, 1, 1, 1, 1, 0, 700, 98
28463, V, 1, 1, 1, 1, 0, 700, 98
28464, V, 1, 1, 1, 1, 0, 700, 98
28465, V, 1, 1, 1, 1, 0, 700, 98
28466, V, 1, 1, 1, 1, 0, 700, 98
28467, V, 1, 1, 1, 1, 0, 700, 98
28468, V, 1, 1, 1, 1, 0, 700, 98
28469, V, 1, 1, 1, 1, 0, 700, 98
28470, V, 1, 1, 1, 1, 0, 700, 98
28471, V, 1, 1, 1, 1, 0, 700, 98
28472, V, 1, 1, 1, 1, 0, 700, 98
28473, V, 1, 1, 1, 1, 0, 700, 98
28474, V, 1, 1, 1, 1, 0, 700, 98
28475, V, 1, 1, 1, 1, 0, 700, 98
28476, V, 1, 1, 1, 1, 0, 700, 98
28477, V, 1, 1, 1, 1, 0, 700, 98
28478, V, 1, 1, 1, 1, 0, 700, 98
28479, V, 1, 1, 1, 1, 0, 700, 98
28480, V, 1, 1, 1, 1, 0, 700, 98
28481, V, 1, 1, 1, 1, 0, 700, 98
28482, V, 1, 1, 1, 1, 0, 700, 98
28483, V, 1, 1, 1, 1, 0, 700, 98
28484, V, 1, 1, 1, 1, 0, 700, 98
28485, V, 1, 1, 1, 1, 0, 700, 98
28486, V, 1, 1, 1, 1, 0, 700, 98
28487, V, 1, 1, 1, 1, 0, 700, 98
28488, V, 1, 1, 1, 1, 0, 700, 98
28489, V, 1, 1, 1, 1, 0, 700, 98
28490, V, 1, 1, 1, 1, 0, 700, 98
28491, V, 1, 1, 1, 1, 0, 700, 98
28492, V, 1, 1, 1, 1, 0, 700, 98
28493, V, 1, 1, 1, 1, 0, 700, 98
28494, V, 1, 1, 1, 1, 0, 700, 98
28495, V, 1, 1, 1, 1, 0, 700, 98
28496, V, 1, 1, 1, 1, 0, 700, 98
28497, V, 1, 1, 1, 1, 0, 700, 98
28498, V, 1, 1, 1, 1, 0, 700, 98
28499, V, 1, 1, 1, 1, 0, 700, 98
28500, V, 1, 1, 1, 1, 0, 700, 98
28502, V, 1, 1, 1, 1, 0, 700, 98
28503, V, 1, 1, 1, 1, 0, 700, 98
28504, V, 1, 1, 1, 1, 0, 700, 98
28505, V, 1, 1, 1, 1, 0, 700, 98
28506, V, 1, 1, 1, 1, 0, 700, 98
28507, V, 1, 1, 1, 1, 0, 700, 98
28508, V, 1, 1, 1, 1, 0, 700, 98
28509, V, 1, 1, 1, 1, 0, 700, 98
28510, V, 1, 1, 1, 1, 0, 700, 98
28511, V, 1, 1, 1, 1, 0, 700, 98
28512, V, 1, 1, 1, 1, 0, 700, 98
28513, V, 1, 1, 1, 1, 0, 700, 98
28514, V, 1, 1, 1, 1, 0, 700, 98
28515, V, 1, 1, 1, 1, 0, 700, 98
28516, V, 1, 1, 1, 1, 0, 700, 98
28517, V, 1, 1, 1, 1, 0, 700, 98
28518, V, 1, 1, 1, 1, 0, 700, 98
28519, V, 1, 1, 1, 1, 0, 700, 98
28520, V, 1, 1, 1, 1, 0, 700, 98
28521, V, 1, 1, 1, 1, 0, 700, 98
28522, V, 1, 1, 1, 1, 0, 700, 98
28523, V, 1, 1, 1, 1, 0, 700, 98
28524, V, 1, 1, 1, 1, 0, 700, 98
28525, V, 1, 1, 1, 1, 0, 700, 98
28526, V, 1, 1, 1, 1, 0, 700, 98
28527, V, 1, 1, 1, 1, 0, 700, 98
28528, V, 1, 1, 1, 1, 0, 700, 98
28529, V, 1, 1, 1, 1, 0, 700, 98
28530, V, 1, 1, 1, 1, 0, 700, 98
28531, V, 1, 1, 1, 1, 0, 700, 98
28532, V, 1, 1, 1, 1, 0, 700, 98
28533, V, 1, 1, 1, 1, 0, 700, 98
28534, V, 1, 1, 1, 1, 0, 700, 98
28535, V, 1, 1, 1, 1, 0, 700, 98
28536, V, 1, 1, 1, 1, 0, 700, 98
28537, V, 1, 1, 1, 1, 0, 700, 98
28538, V, 1, 1, 1, 1, 0, 700, 98
28539, V, 1, 1, 1, 1, 0, 700, 98
28540, V, 1, 1, 1, 1, 0, 700, 98
28541, V, 1, 1, 1, 1, 0, 700, 98
28542, V, 1, 1, 1, 1, 0, 700, 98
28544, V, 1, 1, 1, 1, 0, 700, 98
28545, V, 1, 1, 1, 1, 0, 700, 98
28546, V, 1, 1, 1, 1, 0, 700, 98
28547, V, 1, 1, 1, 1, 0, 700, 98
28548, V, 1, 1, 1, 1, 0, 700, 98
28549, V, 1, 1, 1, 1, 0, 700, 98
28550, V, 1, 1, 1, 1, 0, 700, 98
28551, V, 1, 1, 1, 1, 0, 700, 98
28552, V, 1, 1, 1, 1, 0, 700, 98
28553, V, 1, 1, 1, 1, 0, 700, 98
28554, V, 1, 1, 1, 1, 0, 700, 98
28555, V, 1, 1, 1, 1, 0, 700, 98
28556, V, 1, 1, 1, 1, 0, 700, 98
28557, V, 1, 1, 1, 1, 0, 700, 98
28558, V, 1, 1, 1, 1, 0, 700, 98
28559, V, 1, 1, 1, 1, 0, 700, 98
28560, V, 1, 1, 1, 1, 0, 700, 98
28561, V, 1, 1, 1, 1, 0, 700, 98
28562, V, 1, 1, 1, 1, 0, 700, 98
28563, V, 1, 1, 1, 1, 0, 700, 98
28564, V, 1, 1, 1, 1, 0, 700, 98
28565, V, 1, 1, 1, 1, 0, 700, 98
28566, V, 1, 1, 1, 1, 0, 700, 98
28567, V, 1, 1, 1, 1, 0, 700, 98
28568, V, 1, 1, 1, 1, 0, 700, 98
28569, V, 1, 1, 1, 1, 0, 700, 98
28570, V, 1, 1, 1, 1, 0, 700, 98
28571, V, 1, 1, 1, 1, 0, 700, 98
28572, V, 1, 1, 1, 1, 0, 700, 98
28573, V, 1, 1, 1, 1, 0, 700, 98
28574, V, 1, 1, 1, 1, 0, 700, 98
28575, V, 1, 1, 1, 1, 0, 700, 98
28576, V, 1, 1, 1, 1, 0, 700, 98
28577, V, 1, 1, 1, 1, 0, 700, 98
28578, V, 1, 1, 1, 1, 0, 700, 98
28579, V, 1, 1, 1, 1, 0, 700, 98
28580, V, 1, 1, 1, 1, 0, 700, 98
28581, V, 1, 1, 1, 1, 0, 700, 98
28582, V, 1, 1, 1, 1, 0, 700, 98
28583, V, 1, 1, 1, 1, 0, 700, 98
28584, V, 1, 1, 1, 1, 0, 700, 98
28585, V, 1, 1, 1, 1, 0, 700, 98
28587, V, 1, 1, 1, 1, 0, 700, 98
28588, V, 1, 1, 1, 1, 0, 700, 98
28589, V, 1, 1, 1, 1, 0, 700, 98
28590, V, 1, 1, 1, 1, 0, 700, 98
28591, V, 1, 1, 1, 1, 0, 700, 98
28592, V, 1, 1, 1, 1, 0, 700, 98
28593, V, 1, 1, 1, 1, 0, 700, 98
28594, V, 1, 1, 1, 1, 0, 700, 98
28595, V, 1, 1, 1, 1, 0, 700, 98
28596, V, 1, 1, 1, 1, 0, 700, 98
28597, V, 1, 1, 1, 1, 0, 700, 98
28598, V, 1, 1, 1, 1, 0, 700, 98
28599, V, 1, 1, 1, 1, 0, 700, 98
28600, V, 1, 1, 1, 1, 0, 700, 98
28601, V, 1, 1, 1, 1, 0, 700, 98
28602, V, 1, 1, 1, 1, 0, 700, 98
28603, V, 1, 1, 1, 1, 0, 700, 98
28604, V, 1, 1, 1, 1, 0, 700, 98
28605, V, 1, 1, 1, 1, 0, 700, 98
28606, V, 1, 1, 1, 1, 0, 700, 98
28607, V, 1, 1, 1, 1, 0, 700, 98
28608, V, 1, 1, 1, 1, 0, 700, 98
28609, V, 1, 1, 1, 1, 0, 700, 98
28610, V, 1, 1, 1, 1, 0, 700, 98
28611, V, 1, 1, 1, 1, 0, 700, 98
28612, V, 1, 1, 1, 1, 0, 700, 98
28613, V, 1, 1, 1, 1, 0, 700, 98
28614, V, 1, 1, 1, 1, 0, 700, 98
28615, V, 1, 1, 1, 1, 0, 700, 98
28616, V, 1, 1, 1, 1, 0, 700, 98
28617, V, 1, 1, 1, 1, 0, 700, 98
28618, V, 1, 1, 1, 1, 0, 700, 98
28619, V, 1, 1, 1, 1, 0, 700, 98
28620, V, 1, 1, 1, 1, 0, 700, 98
28621, V, 1, 1, 1, 1, 0, 700, 98
28622, V, 1, 1, 1, 1, 0, 700, 98
28623, V, 1, 1, 1, 1, 0, 700, 98
28624, V, 1, 1, 1, 1, 0, 700, 98
28625, V, 1, 1, 1, 1, 0, 700, 98
28626, V, 1, 1, 1, 1, 0, 700, 98
28627, V, 1, 1, 1, 1, 0, 700, 98
28628, V, 1, 1, 1, 1, 0, 700, 98
28630, V, 1, 1, 1, 1, 0, 700, 98
28631, V, 1, 1, 1, 1, 0, 700, 98
28632, V, 1, 1, 1, 1, 0, 700, 98
28633, V, 1, 1, 1, 1, 0, 700, 98
28634, V, 1, 1, 1, 1, 0, 700, 98
28635, V, 1, 1, 1, 1, 0, 700, 98
28636, V, 1, 1, 1, 1, 0, 700, 98
28637, V, 1, 1, 1, 1, 0, 700, 98
28638, V, 1, 1, 1, 1, 0, 700, 98
28639, V, 1, 1, 1, 1, 0, 700, 98
28640, V, 1, 1, 1, 1, 0, 700, 98
28641, V, 1, 1, 1, 1, 0, 700, 98
28642, V, 1, 1, 1, 1, 0, 700, 98
28643, V, 1, 1, 1, 1, 0, 700, 98
28644, V, 1, 1, 1, 1, 0, 700, 98
28645, V, 1, 1, 1, 1, 0, 700, 98
28646, V, 1, 1, 1, 1, 0, 700, 98
28647, V, 1, 1, 1, 1, 0, 700, 98
28648, V, 1, 1, 1, 1, 0, 700, 98
28649, V, 1, 1, 1, 1, 0, 700, 98
28650, V, 1, 1, 1, 1, 0, 700, 98
28651, V, 1, 1, 1, 1, 0, 700, 98
28652, V, 1, 1, 1, 1, 0, 700, 98
28653, V, 1, 1, 1, 1, 0, 700, 98
28654, V, 1, 1, 1, 1, 0, 700, 98
28655, V, 1, 1, 1, 1, 0, 700, 98
28656, V, 1, 1, 1, 1, 0, 700, 98
28657, V, 1, 1, 1, 1, 0, 700, 98
28658, V, 1, 1, 1, 1, 0, 700, 98
28659, V, 1, 1, 1, 1, 0, 700, 98
28660, V, 1, 1, 1, 1, 0, 700, 98
28661, V, 1, 1, 1, 1, 0, 700, 98
28662, V, 1, 1, 1, 1, 0, 700, 98
28663, V, 1, 1, 1, 1, 0, 700, 98
28664, V, 1, 1, 1, 1, 0, 700, 98
28665, V, 1, 1, 1, 1, 0, 700, 98
28666, V, 1, 1, 1, 1, 0, 700, 98
28667, V, 1, 1, 1, 1, 0, 700, 98
28668, V, 1, 1, 1, 1, 0, 700, 98
28669, V, 1, 1, 1, 1, 0, 700, 98
28670, V, 1, 1, 1, 1, 0, 700, 98
28672, V, 1, 1, 1, 1, 0, 700, 98
28673, V, 1, 1, 1, 1, 0, 700, 98
28674, V, 1, 1, 1, 1, 0, 700, 98
28675, V, 1, 1, 1, 1, 0, 700, 98
28676, V, 1, 1, 1, 1, 0, 700, 98
28677, V, 1, 1, 1, 1, 0, 700, 98
28678, V, 1, 1, 1, 1, 0, 700, 98
28679, V, 1, 1, 1, 1, 0, 700, 98
28680, V, 1, 1, 1, 1, 0, 700, 98
28681, V, 1, 1, 1, 1, 0, 700, 98
28682, V, 1, 1, 1, 1, 0, 700, 98
28683, V, 1, 1, 1, 1, 0, 700, 98
28684, V, 1, 1, 1, 1, 0, 700, 98
28685, V, 1, 1, 1, 1, 0, 700, 98
28686, V, 1, 1, 1, 1, 0, 700, 98
28687, V, 1, 1, 1, 1, 0, 700, 98
28688, V, 1, 1, 1, 1, 0, 700, 98
28689, V, 1, 1, 1, 1, 0, 700, 98
28690, V, 1, 1, 1, 1, 0, 700, 98
28691, V, 1, 1, 1, 1, 0, 700, 98
28692, V, 1, 1, 1, 1, 0, 700, 98
28693, V, 1, 1, 1, 1, 0, 700, 98
28694, V, 1, 1, 1, 1, 0, 700, 98
28695, V, 1, 1, 1, 1, 0, 700, 98
28696, V, 1, 1, 1, 1, 0, 700, 98
28697, V, 1, 1, 1, 1, 0, 700, 98
28698, V, 1, 1, 1, 1, 0, 700, 98
28699, V, 1, 1, 1, 1, 0, 700, 98
28700, V, 1, 1, 1, 1, 0, 700, 98
28701, V, 1, 1, 1, 1, 0, 700, 98
28702, V, 1, 1, 1, 1, 0, 700, 98
28703, V, 1, 1, 1, 1, 0, 700, 98
28704, V, 1, 1, 1, 1, 0, 700, 98
28705, V, 1, 1, 1, 1, 0, 700, 98
28706, V, 1, 1, 1, 1, 0, 700, 98
28707, V, 1, 1, 1, 1, 0, 700, 98
28708, V, 1, 1, 1, 1, 0, 700, 98
28709, V, 1, 1, 1, 1, 0, 700, 98
28710, V, 1, 1, 1, 1, 0, 700, 98
28711, V, 1, 1, 1, 1, 0, 700, 98
28712, V, 1, 1, 1, 1, 0, 700, 98
28713, V, 1, 1, 1, 1, 0, 700, 98
28715, V, 1, 1, 1, 1, 0, 700, 98
28716, V, 1, 1, 1, 1, 0, 700, 98
28717, V, 1, 1, 1, 1, 0, 700, 98
28718, V, 1, 1, 1, 1, 0, 700, 98
28719, V, 1, 1, 1, 1, 0, 700, 98
28720, V, 1, 1, 1, 1, 0, 700, 98
28721, V, 1, 1, 1, 1, 0, 700, 98
28722, V, 1, 1, 1, 1, 0, 700, 98
28723, V, 1, 1, 1, 1, 0, 700, 98
28724, V, 1, 1, 1, 1, 0, 700, 98
28725, V, 1, 1, 1, 1, 0, 700, 98
28726, V, 1, 1, 1, 1, 0, 700, 98
28727, V, 1, 1, 1, 1, 0, 700, 98
28728, V, 1, 1, 1, 1, 0, 700, 98
28729, V, 1, 1, 1, 1, 0, 700, 98
28730, V, 1, 1, 1, 1, 0, 700, 98
28731, V, 1, 1, 1, 1, 0, 700, 98
28732, V, 1, 1, 1, 1, 0, 700, 98
28733, V, 1, 1, 1, 1, 0, 700, 98
28734, V, 1, 1, 1, 1, 0, 700, 98
28735, V, 1, 1, 1, 1, 0, 700, 98
28736, V, 1, 1, 1, 1, 0, 700, 98
28737, V, 1, 1, 1, 1, 0, 700, 98
28738, V, 1, 1, 1, 1, 0, 700, 98
28739, V, 1, 1, 1, 1, 0, 700, 98
28740, V, 1, 1, 1, 1, 0, 700, 98
28741, V, 1, 1, 1, 1, 0, 700, 98
28742, V, 1, 1, 1, 1, 0, 700, 98
28743, V, 1, 1, 1, 1, 0, 700, 98
28744, V, 1, 1, 1, 1, 0, 700, 98
28745, V, 1, 1, 1, 1, 0, 700, 98
28746, V, 1, 1, 1, 1, 0, 700, 98
28747, V, 1, 1, 1, 1, 0, 700, 98
28748, V, 1, 1, 1, 1, 0, 700, 98
28749, V, 1, 1, 1, 1, 0, 700, 98
28750, V, 1, 1, 1, 1, 0, 700, 98
28751, V, 1, 1, 1, 1, 0, 700, 98
28752, V, 1, 1, 1, 1, 0, 700, 98
28753, V, 1, 1, 1, 1, 0, 700, 98
28754, V, 1, 1, 1, 1, 0, 700, 98
28755, V, 1, 1, 1, 1, 0, 700, 98
28756, V, 1, 1, 1, 1, 0, 700, 98
28758, V, 1, 1, 1, 1, 0, 700, 98
28759, V, 1, 1, 1, 1, 0, 700, 98
28760, V, 1, 1, 1, 1, 0, 700, 98
28761, V, 1, 1, 1, 1, 0, 700, 98
28762, V, 1, 1, 1, 1, 0, 700, 98
28763, V, 1, 1, 1, 1, 0, 700, 98
28764, V, 1, 1, 1, 1, 0, 700, 98
28765, V, 1, 1, 1, 1, 0, 700, 98
28766, V, 1, 1, 1, 1, 0, 700, 98
28767, V, 1, 1, 1, 1, 0, 700, 98
28768, V, 1, 1, 1, 1, 0, 700, 98
28769, V, 1, 1, 1, 1, 0, 700, 98
28770, V, 1, 1, 1, 1, 0, 700, 98
28771, V, 1, 1, 1, 1, 0, 700, 98
28772, V, 1, 1, 1, 1, 0, 700, 98
28773, V, 1, 1, 1, 1, 0, 700, 98
28774, V, 1, 1, 1, 1, 0, 700, 98
28775, V, 1, 1, 1, 1, 0, 700, 98
28776, V, 1, 1, 1, 1, 0, 700, 98
28777, V, 1, 1, 1, 1, 0, 700, 98
28778, V, 1, 1, 1, 1, 0, 700, 98
28779, V, 1, 1, 1, 1, 0, 700, 98
28780, V, 1, 1, 1, 1, 0, 700, 98
28781, V, 1, 1, 1, 1, 0, 700, 98
28782, V, 1, 1, 1, 1, 0, 700, 98
28783, V, 1, 1, 1, 1, 0, 700, 98
28784, V, 1, 1, 1, 1, 0, 700, 98
28785, V, 1, 1, 1, 1, 0, 700, 98
28786, V, 1, 1, 1, 1, 0, 700, 98
28787, V, 1, 1, 1, 1, 0, 700, 98
28788, V, 1, 1, 1, 1, 0, 700, 98
28789, V, 1, 1, 1, 1, 0, 700, 98
28790, V, 1, 1, 1, 1, 0, 700, 98
28791, V, 1, 1, 1, 1, 0, 700, 98
28792, V, 1, 1, 1, 1, 0, 700, 98
28793, V, 1, 1, 1, 1, 0, 700, 98
28794, V, 1, 1, 1, 1, 0, 700, 98
28795, V, 1, 1, 1, 1, 0, 700, 98
28796, V, 1, 1, 1, 1, 0, 700, 98
28797, V, 1, 1, 1, 1, 0, 700, 98
28798, V, 1, 1, 1, 1, 0, 700, 98
28800, V, 1, 1, 1, 1, 0, 700, 98
28801, V, 1, 1, 1, 1, 0, 700, 98
28802, V, 1, 1, 1, 1, 0, 700, 98
28803, V, 1, 1, 1, 1, 0, 700, 98
28804, V, 1, 1, 1, 1, 0, 700, 98
28805, V, 1, 1, 1, 1, 0, 700, 98
28806, V, 1, 1, 1, 1, 0, 700, 98
28807, V, 1, 1, 1, 1, 0, 700, 98
28808, V, 1, 1, 1, 1, 0, 700, 98
28809, V, 1, 1, 1, 1, 0, 700, 98
28810, V, 1, 1, 1, 1, 0, 700, 98
28811, V, 1, 1, 1, 1, 0, 700, 98
28812, V, 1, 1, 1, 1, 0, 700, 98
28813, V, 1, 1, 1, 1, 0, 700, 98
28814, V, 1, 1, 1, 1, 0, 700, 98
28815, V, 1, 1, 1, 1, 0, 700, 98
28816, V, 1, 1, 1, 1, 0, 700, 98
28817, V, 1, 1, 1, 1, 0, 700, 98
28818, V, 1, 1, 1, 1, 0, 700, 98
28819, V, 1, 1, 1, 1, 0, 700, 98
28820, V, 1, 1, 1, 1, 0, 700, 98
28821, V, 1, 1, 1, 1, 0, 700, 98
28822, V, 1, 1, 1, 1, 0, 700, 98
28823, V, 1, 1, 1, 1, 0, 700, 98
28824, V, 1, 1, 1, 1, 0, 700, 98
28825, V, 1, 1, 1, 1, 0, 700, 98
28826, V, 1, 1, 1, 1, 0, 700, 98
28827, V, 1, 1, 1, 1, 0, 700, 98
28828, V, 1, 1, 1, 1, 0, 700, 98
28829, V, 1, 1, 1, 1, 0, 700, 98
28830, V, 1, 1, 1, 1, 0, 700, 98
28831, V, 1, 1, 1, 1, 0, 700, 98
28832, V, 1, 1, 1, 1, 0, 700, 98
28833, V, 1, 1, 1, 1, 0, 700, 98
28834, V, 1, 1, 1, 1, 0, 700, 98
28835, V, 1, 1, 1, 1, 0, 700, 98
28836, V, 1, 1, 1, 1, 0, 700, 98
28837, V, 1, 1, 1, 1, 0, 700, 98
28838, V, 1, 1, 1, 1, 0, 700, 98
28839, V, 1, 1, 1, 1, 0, 700, 98
28840, V, 1, 1, 1, 1, 0, 700, 98
28841, V, 1, 1, 1, 1, 0, 700, 98
28843, V, 1, 1, 1, 1, 0, 700, 98
28844, V, 1, 1, 1, 1, 0, 700, 98
28845, V, 1, 1, 1, 1, 0, 700, 98
28846, V, 1, 1, 1, 1, 0, 700, 98
28847, V, 1, 1, 1, 1, 0, 700, 98
28848, V, 1, 1, 1, 1, 0, 700, 98
28849, V, 1, 1, 1, 1, 0, 700, 98
28850, V, 1, 1, 1, 1, 0, 700, 98
28851, V, 1, 1, 1, 1, 0, 700, 98
28852, V, 1, 1, 1, 1, 0, 700, 98
28853, V, 1, 1, 1, 1, 0, 700, 98
28854, V, 1, 1, 1, 1, 0, 700, 98
28855, V, 1, 1, 1, 1, 0, 700, 98
28856, V, 1, 1, 1, 1, 0, 700, 98
28857, V, 1, 1, 1, 1, 0, 700, 98
28858, V, 1, 1, 1, 1, 0, 700, 98
28859, V, 1, 1, 1, 1, 0, 700, 98
28860, V, 1, 1, 1, 1, 0, 700, 98
28861, V, 1, 1, 1, 1, 0, 700, 98
28862, V, 1, 1, 1, 1, 0, 700, 98
28863, V, 1, 1, 1, 1, 0, 700, 98
28864, V, 1, 1, 1, 1, 0, 700, 98
28865, V, 1, 1, 1, 1, 0, 700, 98
28866, V, 1, 1, 1, 1, 0, 700, 98
28867, V, 1, 1, 1, 1, 0, 700, 98
28868, V, 1, 1, 1, 1, 0, 700, 98
28869, V, 1, 1, 1, 1, 0, 700, 98
28870, V, 1, 1, 1, 1, 0, 700, 98
28871, V, 1, 1, 1, 1, 0, 700, 98
28872, V, 1, 1, 1, 1, 0, 700, 98
28873, V, 1, 1, 1, 1, 0, 700, 98
28874, V, 1, 1, 1, 1, 0, 700, 98
28875, V, 1, 1, 1, 1, 0, 700, 98
28876, V, 1, 1, 1, 1, 0, 700, 98
28877, V, 1, 1, 1, 1, 0, 700, 98
28878, V, 1, 1, 1, 1, 0, 700, 98
28879, V, 1, 1, 1, 1, 0, 700, 98
28880, V, 1, 1, 1, 1, 0, 700, 98
28881, V, 1, 1, 1, 1, 0, 700, 98
28882, V, 1, 1, 1, 1, 0, 700, 98
28883, V, 1, 1, 1, 1, 0, 700, 98
28884, V, 1, 1, 1, 1, 0, 700, 98
28886, V, 1, 1, 1, 1, 0, 700, 98
28887, V, 1, 1, 1, 1, 0, 700, 98
28888, V, 1, 1, 1, 1, 0, 700, 98
28889, V, 1, 1, 1, 1, 0, 700, 98
28890, V, 1, 1, 1, 1, 0, 700, 98
28891, V, 1, 1, 1, 1, 0, 700, 98
28892, V, 1, 1, 1, 1, 0, 700, 98
28893, V, 1, 1, 1, 1, 0, 700, 98
28894, V, 1, 1, 1, 1, 0, 700, 98
28895, V, 1, 1, 1, 1, 0, 700, 98
28896, V, 1, 1, 1, 1, 0, 700, 98
28897, V, 1, 1, 1, 1, 0, 700, 98
28898, V, 1, 1, 1, 1, 0, 700, 98
28899, V, 1, 1, 1, 1, 0, 700, 98
28900, V, 1, 1, 1, 1, 0, 700, 98
28901, V, 1, 1, 1, 1, 0, 700, 98
28902, V, 1, 1, 1, 1, 0, 700, 98
28903, V, 1, 1, 1, 1, 0, 700, 98
28904, V, 1, 1, 1, 1, 0, 700, 98
28905, V, 1, 1, 1, 1, 0, 700, 98
28906, V, 1, 1, 1, 1, 0, 700, 98
28907, V, 1, 1, 1, 1, 0, 700, 98
28908, V, 1, 1, 1, 1, 0, 700, 98
28909, V, 1, 1, 1, 1, 0, 700, 98
28910, V, 1, 1, 1, 1, 0, 700, 98
28911, V, 1, 1, 1, 1, 0, 700, 98
28912, V, 1, 1, 1, 1, 0, 700, 98
28913, V, 1, 1, 1, 1, 0, 700, 98
28914, V, 1, 1, 1, 1, 0, 700, 98
28915, V, 1, 1, 1, 1, 0, 700, 98
28916, V, 1, 1, 1, 1, 0, 700, 98
28917, V, 1, 1, 1, 1, 0, 700, 98
28918, V, 1, 1, 1, 1, 0, 700, 98
28919, V, 1, 1, 1, 1, 0, 700, 98
28920, V, 1, 1, 1, 1, 0, 700, 98
28921, V, 1, 1, 1, 1, 0, 700, 98
28922, V, 1, 1, 1, 1, 0, 700, 98
28923, V, 1, 1, 1, 1, 0, 700, 98
28924, V, 1, 1, 1, 1, 0, 700, 98
28925, V, 1, 1, 1, 1, 0, 700, 98
28926, V, 1, 1, 1, 1, 0, 700, 98
28928, V, 1, 1, 1, 1, 0, 700, 98
28929, V, 1, 1, 1, 1, 0, 700, 98
28930, V, 1, 1, 1, 1, 0, 700, 98
28931, V, 1, 1, 1, 1, 0, 700, 98
28932, V, 1, 1, 1, 1, 0, 700, 98
28933, V, 1, 1, 1, 1, 0, 700, 98
28934, V, 1, 1, 1, 1, 0, 700, 98
28935, V, 1, 1, 1, 1, 0, 700, 98
28936, V, 1, 1, 1, 1, 0, 700, 98
28937, V, 1, 0, 0, 1, 0, 700, 98
28937, V, 1, 0, 0, 0, 0, 700, 98
28938, V, 1, 1, 0, 0, 0, 700, 98
28938, V, 1, 1, 0, 0, 0, 700, 98
28939, V, 1, 1, 1, 1, 0, 700, 98
28940, V, 1, 1, 1, 1, 0, 700, 98
28941, V, 1, 1, 1, 1, 0, 700, 98
28942, V, 1, 1, 1, 1, 0, 700, 98
28943, V, 1, 1, 1, 1, 0, 700, 98
28944, V, 1, 1, 1, 1, 0, 700, 97
28945, V, 1, 1, 1, 1, 0, 700, 97
28946, V, 1, 1, 1, 1, 0, 700, 97
28947, V, 1, 1, 1, 1, 0, 700, 97
28948, V, 1, 1, 1, 1, 0, 700, 97
28949, V, 1, 1, 1, 1, 0, 700, 97
28950, V, 1, 1, 1, 1, 0, 700, 97
28951, V, 1, 1, 1, 1, 0, 700, 97
28952, V, 1, 1, 1, 1, 0, 700, 97
28953, V, 1, 1, 1, 1, 0, 700, 97
28954, V, 1, 1, 1, 1, 0, 700, 97
28955, V, 1, 1, 1, 1, 0, 700, 97
28956, V, 1, 1, 1, 1, 0, 700, 97
28957, V, 1, 1, 1, 1, 0, 700, 97
28958, V, 1, 1, 1, 1, 0, 700, 97
28959, V, 1, 1, 1, 1, 0, 700, 97
28960, V, 1, 1, 1, 1, 0, 700, 97
28961, V, 1, 1, 1, 1, 0, 700, 97
28962, V, 1, 1, 1, 1, 0, 700, 98
28963, V, 1, 1, 1, 1, 0, 700, 98
28964, V, 1, 1, 1, 1, 0, 700, 98
28965, V, 1, 1, 1, 1, 0, 700, 98
28966, V, 1, 1, 1, 1, 0, 700, 98
28967, V, 1, 1, 1, 1, 0, 700, 98
28968, V, 1, 1, 1, 1, 0, 700, 98
28969, V, 1, 1, 1, 1, 0, 700, 98
28971, V, 1, 1, 1, 1, 0, 700, 98
28972, V, 1, 1, 1, 1, 0, 700, 98
28973, V, 1, 1, 1, 1, 0, 700, 98
28974, V, 1, 1, 1, 1, 0, 700, 98
28975, V, 1, 1, 1, 1, 0, 700, 98
28976, V, 1, 1, 1, 1, 0, 700, 98
28977, V, 1, 1, 1, 1, 0, 700, 98
28978, V, 1, 1, 1, 1, 0, 700, 98
28979, V, 1, 1, 1, 1, 0, 700, 98
28980, V, 1, 1, 1, 1, 0, 700, 98
28981, V, 1, 1, 1, 1, 0, 700, 98
28982, V, 1, 1, 1, 1, 0, 700, 98
28983, V, 1, 1, 1, 1, 0, 700, 98
28984, V, 1, 1, 1, 1, 0, 700, 98
28985, V, 1, 1, 1, 1, 0, 700, 98
28986, V, 1, 1, 1, 1, 0, 700, 98
28987, V, 1, 1, 1, 1, 0, 700, 98
28988, V, 1, 1, 1, 1, 0, 700, 98
28989, V, 1, 1, 1, 1, 0, 700, 98
28990, V, 1, 1, 1, 1, 0, 700, 98
28991, V, 1, 1, 1, 1, 0, 700, 98
28992, V, 1, 1, 1, 1, 0, 700, 98
28993, V, 1, 1, 1, 1, 0, 700, 98
28994, V, 1, 1, 1, 1, 0, 700, 98
28995, V, 1, 1, 1, 1, 0, 700, 98
28996, V, 1, 1, 1, 1, 0, 700, 98
28997, V, 1, 1, 1, 1, 0, 700, 98
28998, V, 1, 1, 1, 1, 0, 700, 98
28999, V, 1, 1, 1, 1, 0, 700, 98
29000, V, 1, 1, 1, 1, 0, 700, 98
29001, V, 1, 1, 1, 1, 0, 700, 98
29002, V, 1, 1, 1, 1, 0, 700, 98
29003, V, 1, 1, 1, 1, 0, 700, 98
29004, V, 1, 1, 1, 1, 0, 700, 98
29005, V, 1, 1, 1, 1, 0, 700, 98
29006, V, 1, 1, 1, 1, 0, 700, 98
29007, V, 1, 1, 1, 1, 0, 700, 98
29008, V, 1, 1, 1, 1, 0, 700, 98
29009, V, 1, 1, 1, 1, 0, 700, 98
29010, V, 1, 1, 1, 1, 0, 700, 98
29011, V, 1, 1, 1, 1, 0, 700, 98
29012, V, 1, 1, 1, 1, 0, 700, 98
29014, V, 1, 1, 1, 1, 0, 700, 98
29015, V, 1, 1, 1, 1, 0, 700, 98
29016, V, 1, 1, 1, 1, 0, 700, 98
29017, V, 1, 1, 1, 1, 0, 700, 98
29018, V, 1, 1, 1, 1, 0, 700, 98
29019, V, 1, 1, 1, 1, 0, 700, 98
29020, V, 1, 1, 1, 1, 0, 700, 98
29021, V, 1, 1, 1, 1, 0, 700, 98
29022, V, 1, 1, 1, 1, 0, 700, 98
29023, V, 1, 1, 1, 1, 0, 700, 98
29024, V, 1, 1, 1, 1, 0, 700, 98
29025, V, 1, 1, 1, 1, 0, 700, 98
29026, V, 1, 1, 1, 1, 0, 700, 98
29027, V, 1, 1, 1, 1, 0, 700, 98
29028, V, 1, 1, 1, 1, 0, 700, 98
29029, V, 1, 1, 1, 1, 0, 700, 98
29030, V, 1, 1, 1, 1, 0, 700, 98
29031, V, 1, 1, 1, 1, 0, 700, 98
29032, V, 1, 1, 1, 1, 0, 700, 98
29033, V, 1, 1, 1, 1, 0, 700, 98
29034, V, 1, 1, 1, 1, 0, 700, 98
29035, V, 1, 1, 1, 1, 0, 700, 98
29036, V, 1, 1, 1, 1, 0, 700, 98
29037, V, 1, 1, 1, 1, 0, 700, 98
29038, V, 1, 1, 1, 1, 0, 700, 98
29039, V, 1, 1, 1, 1, 0, 700, 98
29040, V, 1, 1, 1, 1, 0, 700, 98
29041, V, 1, 1, 1, 1, 0, 700, 98
29042, V, 1, 1, 1, 1, 0, 700, 98
29043, V, 1, 1, 1, 1, 0, 700, 98
29044, V, 1, 1, 1, 1, 0, 700, 98
29045, V, 1, 1, 1, 1, 0, 700, 98
29046, V, 1, 1, 1, 1, 0, 700, 98
29047, V, 1, 1, 1, 1, 0, 700, 98
29048, V, 1, 1, 1, 1, 0, 700, 98
29049, V, 1, 1, 1, 1, 0, 700, 98
29050, V, 1, 1, 1, 1, 0, 700, 98
29051, V, 1, 1, 1, 1, 0, 700, 98
29052, V, 1, 1, 1, 1, 0, 700, 98
29053, V, 1, 1, 1, 1, 0, 700, 98
29054, V, 1, 1, 1, 1, 0, 700, 98
29056, V, 1, 1, 1, 1, 0, 700, 98
29057, V, 1, 1, 1, 1, 0, 700, 98
29058, V, 1, 1, 1, 1, 0, 700, 98
29059, V, 1, 1, 1, 1, 0, 700, 98
29060, V, 1, 1, 1, 1, 0, 700, 98
29061, V, 1, 1, 1, 1, 0, 700, 98
29062, V, 1, 1, 1, 1, 0, 700, 98
29063, V, 1, 1, 1, 1, 0, 700, 98
29064, V, 1, 1, 1, 1, 0, 700, 98
29065, V, 1, 1, 1, 1, 0, 700, 98
29066, V, 1, 1, 1, 1, 0, 700, 98
29067, V, 1, 1, 1, 1, 0, 700, 98
29068, V, 1, 1, 1, 1, 0, 700, 98
29069, V, 1, 1, 1, 1, 0, 700, 98
29070, V, 1, 1, 1, 1, 0, 700, 98
29071, V, 1, 1, 1, 1, 0, 700, 98
29072, V, 1, 1, 1, 1, 0, 700, 98
29073, V, 1, 1, 1, 1, 0, 700, 98
29074, V, 1, 1, 1, 1, 0, 700, 98
29075, V, 1, 1, 1, 1, 0, 700, 98
29076, V, 1, 1, 1, 1, 0, 700, 98
29077, V, 1, 1, 1, 1, 0, 700, 98
29078, V, 1, 1, 1, 1, 0, 700, 98
29079, V, 1, 1, 1, 1, 0, 700, 98
29080, V, 1, 1, 1, 1, 0, 700, 98
29081, V, 1, 1, 1, 1, 0, 700, 98
29082, V, 1, 1, 1, 1, 0, 700, 98
29083, V, 1, 1, 1, 1, 0, 700, 98
29084, V, 1, 1, 1, 1, 0, 700, 98
29085, V, 1, 1, 1, 1, 0, 700, 98
29086, V, 1, 1, 1, 1, 0, 700, 98
29087, V, 1, 1, 1, 1, 0, 700, 98
29088, V, 1, 1, 1, 1, 0, 700, 98
29089, V, 1, 1, 1, 1, 0, 700, 98
29090, V, 1, 1, 1, 1, 0, 700, 98
29091, V, 1, 1, 1, 1, 0, 700, 98
29092, V, 1, 1, 1, 1, 0, 700, 98
29093, V, 1, 1, 1, 1, 0, 700, 98
29094, V, 1, 1, 1, 1, 0, 700, 98
29095, V, 1, 1, 1, 1, 0, 700, 98
29096, V, 1, 1, 1, 1, 0, 700, 98
29097, V, 1, 1, 1, 1, 0, 700, 98
29099, V, 1, 1, 1, 1, 0, 700, 98
29100, V, 1, 1, 1, 1, 0, 700, 98
29101, V, 1, 1, 1, 1, 0, 700, 98
29102, V, 1, 1, 1, 1, 0, 700, 98
29103, V, 1, 1, 1, 1, 0, 700, 98
29104, V, 1, 1, 1, 1, 0, 700, 98
29105, V, 1, 1, 1, 1, 0, 700, 98
29106, V, 1, 1, 1, 1, 0, 700, 98
29107, V, 1, 1, 1, 1, 0, 700, 98
29108, V, 1, 1, 1, 1, 0, 700, 98
29109, V, 1, 1, 1, 1, 0, 700, 98
29110, V, 1, 1, 1, 1, 0, 700, 98
29111, V, 1, 1, 1, 1, 0, 700, 98
29112, V, 1, 1, 1, 1, 0, 700, 98
29113, V, 1, 1, 1, 1, 0, 700, 98
29114, V, 1, 1, 1, 1, 0, 700, 98
29115, V, 1, 1, 1, 1, 0, 700, 98
29116, V, 1, 1, 1, 1, 0, 700, 98
29117, V, 1, 1, 1, 1, 0, 700, 98
29118, V, 1, 1, 1, 1, 0, 700, 98
29119, V, 1, 1, 1, 1, 0, 700, 98
29120, V, 1, 1, 1, 1, 0, 700, 98
29121, V, 1, 1, 1, 1, 0, 700, 98
29122, V, 1, 1, 1, 1, 0, 700, 98
29123, V, 1, 1, 1, 1, 0, 700, 98
29124, V, 1, 1, 1, 1, 0, 700, 98
29125, V, 1, 1, 1, 1, 0, 700, 98
29126, V, 1, 1, 1, 1, 0, 700, 98
29127, V, 1, 1, 1, 1, 0, 700, 98
29128, V, 1, 1, 1, 1, 0, 700, 98
29129, V, 1, 1, 1, 1, 0, 700, 98
29130, V, 1, 1, 1, 1, 0, 700, 98
29131, V, 1, 1, 1, 1, 0, 700, 98
29132, V, 1, 1, 1, 1, 0, 700, 98
29133, V, 1, 1, 1, 1, 0, 700, 98
29134, V, 1, 1, 1, 1, 0, 700, 98
29135, V, 1, 1, 1, 1, 0, 700, 98
29136, V, 1, 1, 1, 1, 0, 700, 98
29137, V, 1, 1, 1, 1, 0, 700, 98
29138, V, 1, 1, 1, 1, 0, 700, 98
29139, V, 1, 1, 1, 1, 0, 700, 98
29140, V, 1, 1, 1, 1, 0, 700, 98
29142, V, 1, 1, 1, 1, 0, 700, 98
29143, V, 1, 1, 1, 1, 0, 700, 98
29144, V, 1, 1, 1, 1, 0, 700, 98
29145, V, 1, 1, 1, 1, 0, 700, 98
29146, V, 1, 1, 1, 1, 0, 700, 98
29147, V, 1, 1, 1, 1, 0, 700, 98
29148, V, 1, 1, 1, 1, 0, 700, 98
29149, V, 1, 1, 1, 1, 0, 700, 98
29150, V, 1, 1, 1, 1, 0, 700, 98
29151, V, 1, 1, 1, 1, 0, 700, 98
29152, V, 1, 1, 1, 1, 0, 700, 98
29153, V, 1, 1, 1, 1, 0, 700, 98
29154, V, 1, 1, 1, 1, 0, 700, 98
29155, V, 1, 1, 1, 1, 0, 700, 98
29156, V, 1, 1, 1, 1, 0, 700, 98
29157, V, 1, 1, 1, 1, 0, 700, 98
29158, V, 1, 1, 1, 1, 0, 700, 98
29159, V, 1, 1, 1, 1, 0, 700, 98
29160, V, 1, 1, 1, 1, 0, 700, 98
29161, V, 1, 1, 1, 1, 0, 700, 98
29162, V, 1, 1, 1, 1, 0, 700, 98
29163, V, 1, 1, 1, 1, 0, 700, 98
29164, V, 1, 1, 1, 1, 0, 700, 98
29165, V, 1, 1, 1, 1, 0, 700, 98
29166, V, 1, 1, 1, 1, 0, 700, 98
29167, V, 1, 1, 1, 1, 0, 700, 98
29168, V, 1, 1, 1, 1, 0, 700, 98
29169, V, 1, 1, 1, 1, 0, 700, 98
29170, V, 1, 1, 1, 1, 0, 700, 98
29171, V, 1, 1, 1, 1, 0, 700, 98
29172, V, 1, 1, 1, 1, 0, 700, 98
29173, V, 1, 1, 1, 1, 0, 700, 98
29174, V, 1, 1, 1, 1, 0, 700, 98
29175, V, 1, 1, 1, 1, 0, 700, 98
29176, V, 1, 1, 1, 1, 0, 700, 98
29177, V, 1, 1, 1, 1, 0, 700, 98
29178, V, 1, 1, 1, 1, 0, 700, 98
29179, V, 1, 1, 1, 1, 0, 700, 98
29180, V, 1, 1, 1, 1, 0, 700, 98
29181, V, 1, 1, 1, 1, 0, 700, 98
29182, V, 1, 1, 1, 1, 0, 700, 98
29184, V, 1, 1, 1, 1, 0, 700, 98
29185, V, 1, 1, 1, 1, 0, 700, 98
29186, V, 1, 1, 1, 1, 0, 700, 98
29187, V, 1, 1, 1, 1, 0, 700, 98
29188, V, 1, 1, 1, 1, 0, 700, 98
29189, V, 1, 1, 1, 1, 0, 700, 98
29190, V, 1, 1, 1, 1, 0, 700, 98
29191, V, 1, 1, 1, 1, 0, 700, 98
29192, V, 1, 1, 1, 1, 0, 700, 98
29193, V, 1, 1, 1, 1, 0, 700, 98
29194, V, 1, 1, 1, 1, 0, 700, 98
29195, V, 1, 1, 1, 1, 0, 700, 98
29196, V, 1, 1, 1, 1, 0, 700, 98
29197, V, 1, 1, 1, 1, 0, 700, 98
29198, V, 1, 1, 1, 1, 0, 700, 98
29199, V, 1, 1, 1, 1, 0, 700, 98
29200, V, 1, 1, 1, 1, 0, 700, 98
29201, V, 1, 1, 1, 1, 0, 700, 98
29202, V, 1, 1, 1, 1, 0, 700, 98
29203, V, 1, 1, 1, 1, 0, 700, 98
29204, V, 1, 1, 1, 1, 0, 700, 98
29205, V, 1, 1, 1, 1, 0, 700, 98
29206, V, 1, 1, 1, 1, 0, 700, 98
29207, V, 1, 1, 1, 1, 0, 700, 98
29208, V, 1, 1, 1, 1, 0, 700, 98
29209, V, 1, 1, 1, 1, 0, 700, 98
29210, V, 1, 1, 1, 1, 0, 700, 98
29211, V, 1, 1, 1, 1, 0, 700, 98
29212, V, 1, 1, 1, 1, 0, 700, 98
29213, V, 1, 1, 1, 1, 0, 700, 98
29214, V, 1, 1, 1, 1, 0, 700, 98
29215, V, 1, 1, 1, 1, 0, 700, 98
29216, V, 1, 1, 1, 1, 0, 700, 98
29217, V, 1, 1, 1, 1, 0, 700, 98
29218, V, 1, 1, 1, 1, 0, 700, 98
29219, V, 1, 1, 1, 1, 0, 700, 98
29220, V, 1, 1, 1, 1, 0, 700, 98
29221, V, 1, 1, 1, 1, 0, 700, 98
29222, V, 1, 1, 1, 1, 0, 700, 98
29223, V, 1, 1, 1, 1, 0, 700, 98
29224, V, 1, 1, 1, 1, 0, 700, 98
29225, V, 1, 1, 1, 1, 0, 700, 98
29227, V, 1, 1, 1, 1, 0, 700, 98
29228, V, 1, 1, 1, 1, 0, 700, 98
29229, V, 1, 1, 1, 1, 0, 700, 98
29230, V, 1, 1, 1, 1, 0, 700, 98
29231, V, 1, 1, 1, 1, 0, 700, 98
29232, V, 1, 1, 1, 1, 0, 700, 98
29233, V, 1, 1, 1, 1, 0, 700, 98
29234, V, 1, 1, 1, 1, 0, 700, 98
29235, V, 1, 1, 1, 1, 0, 700, 98
29236, V, 1, 1, 1, 1, 0, 700, 98
29237, V, 1, 1, 1, 1, 0, 700, 98
29238, V, 1, 1, 1, 1, 0, 700, 98
29239, V, 1, 1, 1, 1, 0, 700, 98
29240, V, 1, 1, 1, 1, 0, 700, 98
29241, V, 1, 1, 1, 1, 0, 700, 98
29242, V, 1, 1, 1, 1, 0, 700, 98
29243, V, 1, 1, 1, 1, 0, 700, 98
29244, V, 1, 1, 1, 1, 0, 700, 98
29245, V, 1, 1, 1, 1, 0, 700, 98
29246, V, 1, 1, 1, 1, 0, 700, 98
29247, V, 1, 1, 1, 1, 0, 700, 98
29248, V, 1, 1, 1, 1, 0, 700, 98
29249, V, 1, 1, 1, 1, 0, 700, 98
29250, V, 1, 1, 1, 1, 0, 700, 98
29251, V, 1, 1, 1, 1, 0, 700, 98
29252, V, 1, 1, 1, 1, 0, 700, 98
29253, V, 1, 1, 1, 1, 0, 700, 98
29254, V, 1, 1, 1, 1, 0, 700, 98
29255, V, 1, 1, 1, 1, 0, 700, 98
29256, V, 1, 1, 1, 1, 0, 700, 98
29257, V, 1, 1, 1, 1, 0, 700, 98
29258, V, 1, 1, 1, 1, 0, 700, 98
29259, V, 1, 1, 1, 1, 0, 700, 98
29260, V, 1, 1, 1, 1, 0, 700, 98
29261, V, 1, 1, 1, 1, 0, 700, 98
29262, V, 1, 1, 1, 1, 0, 700, 98
29263, V, 1, 1, 1, 1, 0, 700, 98
29264, V, 1, 1, 1, 1, 0, 700, 98
29265, V, 1, 1, 1, 1, 0, 700, 98
29266, V, 1, 1, 1, 1, 0, 700, 98
29267, V, 1, 1, 1, 1, 0, 700, 98
29268, V, 1, 1, 1, 1, 0, 700, 98
29270, V, 1, 1, 1, 1, 0, 700, 98
29271, V, 1, 1, 1, 1, 0, 700, 98
29272, V, 1, 1, 1, 1, 0, 700, 98
29273, V, 1, 1, 1, 1, 0, 700, 98
29274, V, 1, 1, 1, 1, 0, 700, 98
29275, V, 1, 1, 1, 1, 0, 700, 98
29276, V, 1, 1, 1, 1, 0, 700, 98
29277, V, 1, 1, 1, 1, 0, 700, 98
29278, V, 1, 1, 1, 1, 0, 700, 98
29279, V, 1, 1, 1, 1, 0, 700, 98
29280, V, 1, 1, 1, 1, 0, 700, 98
29281, V, 1, 1, 1, 1, 0, 700, 98
29282, V, 1, 1, 1, 1, 0, 700, 98
29283, V, 1, 1, 1, 1, 0, 700, 98
29284, V, 1, 1, 1, 1, 0, 700, 98
29285, V, 1, 1, 1, 1, 0, 700, 98
29286, V, 1, 1, 1, 1, 0, 700, 98
29287, V, 1, 1, 1, 1, 0, 700, 98
29288, V, 1, 1, 1, 1, 0, 700, 98
29289, V, 1, 1, 1, 1, 0, 700, 98
29290, V, 1, 1, 1, 1, 0, 700, 98
29291, V, 1, 1, 1, 1, 0, 700, 98
29292, V, 1, 1, 1, 1, 0, 700, 98
29293, V, 1, 1, 1, 1, 0, 700, 98
29294, V, 1, 1, 1, 1, 0, 700, 98
29295, V, 1, 1, 1, 1, 0, 700, 98
29296, V, 1, 1, 1, 1, 0, 700, 98
29297, V, 1, 1, 1, 1, 0, 700, 98
29298, V, 1, 1, 1, 1, 0, 700, 98
29299, V, 1, 1, 1, 1, 0, 700, 98
29300, V, 1, 1, 1, 1, 0, 700, 98
29301, V, 1, 1, 1, 1, 0, 700, 98
29302, V, 1, 1, 1, 1, 0, 700, 98
29303, V, 1, 1, 1, 1, 0, 700, 98
29304, V, 1, 1, 1, 1, 0, 700, 98
29305, V, 1, 1, 1, 1, 0, 700, 98
29306, V, 1, 1, 1, 1, 0, 700, 98
29307, V, 1, 1, 1, 1, 0, 700, 98
29308, V, 1, 1, 1, 1, 0, 700, 98
29309, V, 1, 1, 1, 1, 0, 700, 98
29310, V, 1, 1, 1, 1, 0, 700, 98
29312, V, 1, 1, 1, 1, 0, 700, 98
29313, V, 1, 1, 1, 1, 0, 700, 98
29314, V, 1, 1, 1, 1, 0, 700, 98
29315, V, 1, 1, 1, 1, 0, 700, 98
29316, V, 1, 1, 1, 1, 0, 700, 98
29317, V, 1, 1, 1, 1, 0, 700, 98
29318, V, 1, 1, 1, 1, 0, 700, 98
29319, V, 1, 1, 1, 1, 0, 700, 98
29320, V, 1, 1, 1, 1, 0, 700, 98
29321, V, 1, 1, 1, 1, 0, 700, 98
29322, V, 1, 1, 1, 1, 0, 700, 98
29323, V, 1, 1, 1, 1, 0, 700, 98
29324, V, 1, 1, 1, 1, 0, 700, 98
29325, V, 1, 1, 1, 1, 0, 700, 98
29326, V, 1, 1, 1, 1, 0, 700, 98
29327, V, 1, 1, 1, 1, 0, 700, 98
29328, V, 1, 1, 1, 1, 0, 700, 98
29329, V, 1, 1, 1, 1, 0, 700, 98
29330, V, 1, 1, 1, 1, 0, 700, 98
29331, V, 1, 1, 1, 1, 0, 700, 98
29332, V, 1, 1, 1, 1, 0, 700, 98
29333, V, 1, 1, 1, 1, 0, 700, 98
29334, V, 1, 1, 1, 1, 0, 700, 98
29335, V, 1, 1, 1, 1, 0, 700, 98
29336, V, 1, 1, 1, 1, 0, 700, 98
29337, V, 1, 1, 1, 1, 0, 700, 98
29338, V, 1, 1, 1, 1, 0, 700, 98
29339, V, 1, 1, 1, 1, 0, 700, 98
29340, V, 1, 1, 1, 1, 0, 700, 98
29341, V, 1, 1, 1, 1, 0, 700, 98
29342, V, 1, 1, 1, 1, 0, 700, 98
29343, V, 1, 1, 1, 1, 0, 700, 98
29344, V, 1, 1, 1, 1, 0, 700, 98
29345, V, 1, 1, 1, 1, 0, 700, 98
29346, V, 1, 1, 1, 1, 0, 700, 98
29347, V, 1, 1, 1, 1, 0, 700, 98
29348, V, 1, 1, 1, 1, 0, 700, 98
29349, V, 1, 1, 1, 1, 0, 700, 98
29350, V, 1, 1, 1, 1, 0, 700, 98
29351, V, 1, 1, 1, 1, 0, 700, 98
29352, V, 1, 1, 1, 1, 0, 700, 98
29353, V, 1, 1, 1, 1, 0, 700, 98
29355, V, 1, 1, 1, 1, 0, 700, 98
29356, V, 1, 1, 1, 1, 0, 700, 98
29357, V, 1, 1, 1, 1, 0, 700, 98
29358, V, 1, 1, 1, 1, 0, 700, 98
29359, V, 1, 1, 1, 1, 0, 700, 98
29360, V, 1, 1, 1, 1, 0, 700, 98
29361, V, 1, 1, 1, 1, 0, 700, 98
29362, V, 1, 1, 1, 1, 0, 700, 98
29363, V, 1, 1, 1, 1, 0, 700, 98
29364, V, 1, 1, 1, 1, 0, 700, 98
29365, V, 1, 1, 1, 1, 0, 700, 98
29366, V, 1, 1, 1, 1, 0, 700, 98
29367, V, 1, 1, 1, 1, 0, 700, 98
29368, V, 1, 1, 1, 1, 0, 700, 98
29369, V, 1, 1, 1, 1, 0, 700, 98
29370, V, 1, 1, 1, 1, 0, 700, 98
29371, V, 1, 1, 1, 1, 0, 700, 98
29372, V, 1, 1, 1, 1, 0, 700, 98
29373, V, 1, 1, 1, 1, 0, 700, 98
29374, V, 1, 1, 1, 1, 0, 700, 98
29375, V, 1, 1, 1, 1, 0, 700, 98
29376, V, 1, 1, 1, 1, 0, 700, 98
29377, V, 1, 1, 1, 1, 0, 700, 98
29378, V, 1, 1, 1, 1, 0, 700, 98
29379, V, 1, 1, 1, 1, 0, 700, 98
29380, V, 1, 1, 1, 1, 0, 700, 98
29381, V, 1, 1, 1, 1, 0, 700, 98
29382, V, 1, 1, 1, 1, 0, 700, 98
29383, V, 1, 1, 1, 1, 0, 700, 98
29384, V, 1, 1, 1, 1, 0, 700, 98
29385, V, 1, 1, 1, 1, 0, 700, 98
29386, V, 1, 1, 1, 1, 0, 700, 98
29387, V, 1, 1, 1, 1, 0, 700, 98
29388, V, 1, 1, 1, 1, 0, 700, 98
29389, V, 1, 1, 1, 1, 0, 700, 98
29390, V, 1, 1, 1, 1, 0, 700, 98
29391, V, 1, 1, 1, 1, 0, 700, 98
29392, V, 1, 1, 1, 1, 0, 700, 98
29393, V, 1, 1, 1, 1, 0, 700, 98
29394, V, 1, 1, 1, 1, 0, 700, 98
29395, V, 1, 1, 1, 1, 0, 700, 98
29396, V, 1, 1, 1, 1, 0, 700, 98
29398, V, 1, 1, 1, 1, 0, 700, 98
29399, V, 1, 1, 1, 1, 0, 700, 98
29400, V, 1, 1, 1, 1, 0, 700, 98
29401, V, 1, 1, 1, 1, 0, 700, 98
29402, V, 1, 1, 1, 1, 0, 700, 98
29403, V, 1, 1, 1, 1, 0, 700, 98
29404, V, 1, 1, 1, 1, 0, 700, 98
29405, V, 1, 1, 1, 1, 0, 700, 98
29406, V, 1, 1, 1, 1, 0, 700, 98
29407, V, 1, 1, 1, 1, 0, 700, 98
29408, V, 1, 1, 1, 1, 0, 700, 98
29409, V, 1, 1, 1, 1, 0, 700, 98
29410, V, 1, 1, 1, 1, 0, 700, 98
29411, V, 1, 1, 1, 1, 0, 700, 98
29412, V, 1, 1, 1, 1, 0, 700, 98
29413, V, 1, 1, 1, 1, 0, 700, 98
29414, V, 1, 1, 1, 1, 0, 700, 98
29415, V, 1, 1, 1, 1, 0, 700, 98
29416, V, 1, 1, 1, 1, 0, 700, 98
29417, V, 1, 1, 1, 1, 0, 700, 98
29418, V, 1, 1, 1, 1, 0, 700, 98
29419, V, 1, 1, 1, 1, 0, 700, 98
29420, V, 1, 1, 1, 1, 0, 700, 98
29421, V, 1, 1, 1, 1, 0, 700, 98
29422, V, 1, 1, 1, 1, 0, 700, 98
29423, V, 1, 1, 1, 1, 0, 700, 98
29424, V, 1, 1, 1, 1, 0, 700, 98
29425, V, 1, 1, 1, 1, 0, 700, 98
29426, V, 1, 1, 1, 1, 0, 700, 98
29427, V, 1, 1, 1, 1, 0, 700, 98
29428, V, 1, 1, 1, 1, 0, 700, 98
29429, V, 1, 1, 1, 1, 0, 700, 98
29430, V, 1, 1, 1, 1, 0, 700, 98
29431, V, 1, 1, 1, 1, 0, 700, 98
29432, V, 1, 1, 1, 1, 0, 700, 98
29433, V, 1, 1, 1, 1, 0, 700, 98
29434, V, 1, 1, 1, 1, 0, 700, 98
29435, V, 1, 1, 1, 1, 0, 700, 98
29436, V, 1, 1, 1, 1, 0, 700, 98
29437, V, 1, 1, 1, 1, 0, 700, 98
29438, V, 1, 1, 1, 1, 0, 700, 98
29440, V, 1, 1, 1, 1, 0, 700, 98
29441, V, 1, 1, 1, 1, 0, 700, 98
29442, V, 1, 1, 1, 1, 0, 700, 98
29443, V, 1, 0, 0, 1, 0, 700, 98
29443, V, 1, 0, 0, 0, 0, 700, 98
29444, V, 1, 1, 0, 0, 0, 700, 98
29444, V, 1, 1, 0, 0, 0, 700, 98
29445, V, 1, 1, 1, 1, 0, 700, 98
29446, V, 1, 1, 1, 1, 0, 700, 98
29447, V, 1, 1, 1, 1, 0, 700, 98
29448, V, 1, 1, 1, 1, 0, 700, 98
29449, V, 1, 1, 1, 1, 0, 700, 97
29450, V, 1, 1, 1, 1, 0, 700, 97
29451, V, 1, 1, 1, 1, 0, 700, 97
29452, V, 1, 1, 1, 1, 0, 700, 97
29453, V, 1, 1, 1, 1, 0, 700, 97
29454, V, 1, 1, 1, 1, 0, 700, 97
29455, V, 1, 1, 1, 1, 0, 700, 97
29456, V, 1, 1, 1, 1, 0, 700, 97
29457, V, 1, 1, 1, 1, 0, 700, 97
29458, V, 1, 1, 1, 1, 0, 700, 97
29459, V, 1, 1, 1, 1, 0, 700, 97
29460, V, 1, 1, 1, 1, 0, 700, 97
29461, V, 1, 1, 1, 1, 0, 700, 97
29462, V, 1, 1, 1, 1, 0, 700, 97
29463, V, 1, 1, 1, 1, 0, 700, 97
29464, V, 1, 1, 1, 1, 0, 700, 97
29465, V, 1, 1, 1, 1, 0, 700, 97
29466, V, 1, 1, 1, 1, 0, 700, 97
29467, V, 1, 1, 1, 1, 0, 700, 97
29468, V, 1, 1, 1, 1, 0, 700, 97
29469, V, 1, 1, 1, 1, 0, 700, 97
29470, V, 1, 1, 1, 1, 0, 700, 97
29471, V, 1, 1, 1, 1, 0, 700, 97
29472, V, 1, 1, 1, 1, 0, 700, 97
29473, V, 1, 1, 1, 1, 0, 700, 97
29474, V, 1, 1, 1, 1, 0, 700, 98
29475, V, 1, 1, 1, 1, 0, 700, 97
29476, V, 1, 1, 1, 1, 0, 700, 97
29477, V, 1, 1, 1, 1, 0, 700, 97
29478, V, 1, 1, 1, 1, 0, 700, 97
29479, V, 1, 1, 1, 1, 0, 700, 98
29480, V, 1, 1, 1, 1, 0, 700, 98
29481, V, 1, 1, 1, 1, 0, 700, 98
29483, V, 1, 1, 1, 1, 0, 700, 98
29484, V, 1, 1, 1, 1, 0, 700, 98
29485, V, 1, 1, 1, 1, 0, 700, 98
29486, V, 1, 1, 1, 1, 0, 700, 98
29487, V, 1, 1, 1, 1, 0, 700, 98
29488, V, 1, 1, 1, 1, 0, 700, 98
29489, V, 1, 1, 1, 1, 0, 700, 98
29490, V, 1, 1, 1, 1, 0, 700, 98
29491, V, 1, 1, 1, 1, 0, 700, 98
29492, V, 1, 1, 1, 1, 0, 700, 98
29493, V, 1, 1, 1, 1, 0, 700, 98
29494, V, 1, 1, 1, 1, 0, 700, 98
29495, V, 1, 1, 1, 1, 0, 700, 98
29496, V, 1, 1, 1, 1, 0, 700, 98
29497, V, 1, 1, 1, 1, 0, 700, 98
29498, V, 1, 1, 1, 1, 0, 700, 98
29499, V, 1, 1, 1, 1, 0, 700, 98
29500, V, 1, 1, 1, 1, 0, 700, 98
29501, V, 1, 1, 1, 1, 0, 700, 98
29502, V, 1, 1, 1, 1, 0, 700, 98
29503, V, 1, 1, 1, 1, 0, 700, 98
29504, V, 1, 1, 1, 1, 0, 700, 98
29505, V, 1, 1, 1, 1, 0, 700, 98
29506, V, 1, 1, 1, 1, 0, 700, 98
29507, V, 1, 1, 1, 1, 0, 700, 98
29508, V, 1, 1, 1, 1, 0, 700, 98
29509, V, 1, 1, 1, 1, 0, 700, 98
29510, V, 1, 1, 1, 1, 0, 700, 98
29511, V, 1, 1, 1, 1, 0, 700, 98
29512, V, 1, 1, 1, 1, 0, 700, 98
29513, V, 1, 1, 1, 1, 0, 700, 98
29514, V, 1, 1, 1, 1, 0, 700, 98
29515, V, 1, 1, 1, 1, 0, 700, 98
29516, V, 1, 1, 1, 1, 0, 700, 98
29517, V, 1, 1, 1, 1, 0, 700, 98
29518, V, 1, 1, 1, 1, 0, 700, 98
29519, V, 1, 1, 1, 1, 0, 700, 98
29520, V, 1, 1, 1, 1, 0, 700, 98
29521, V, 1, 1, 1, 1, 0, 700, 98
29522, V, 1, 1, 1, 1, 0, 700, 98
29523, V, 1, 1, 1, 1, 0, 700, 98
29524, V, 1, 1, 1, 1, 0, 700, 98
29526, V, 1, 1, 1, 1, 0, 700, 98
29527, V, 1, 1, 1, 1, 0, 700, 98
29528, V, 1, 1, 1, 1, 0, 700, 98
29529, V, 1, 1, 1, 1, 0, 700, 98
29530, V, 1, 1, 1, 1, 0, 700, 98
29531, V, 1, 1, 1, 1, 0, 700, 98
29532, V, 1, 1, 1, 1, 0, 700, 98
29533, V, 1, 1, 1, 1, 0, 700, 98
29534, V, 1, 1, 1, 1, 0, 700, 98
29535, V, 1, 1, 1, 1, 0, 700, 98
29536, V, 1, 1, 1, 1, 0, 700, 98
29537, V, 1, 1, 1, 1, 0, 700, 98
29538, V, 1, 1, 1, 1, 0, 700, 98
29539, V, 1, 1, 1, 1, 0, 700, 98
29540, V, 1, 1, 1, 1, 0, 700, 98
29541, V, 1, 1, 1, 1, 0, 700, 98
29542, V, 1, 1, 1, 1, 0, 700, 98
29543, V, 1, 1, 1, 1, 0, 700, 98
29544, V, 1, 1, 1, 1, 0, 700, 98
29545, V, 1, 1, 1, 1, 0, 700, 98
29546, V, 1, 1, 1, 1, 0, 700, 98
29547, V, 1, 1, 1, 1, 0, 700, 98
29548, V, 1, 1, 1, 1, 0, 700, 98
29549, V, 1, 1, 1, 1, 0, 700, 98
29550, V, 1, 1, 1, 1, 0, 700, 98
29551, V, 1, 1, 1, 1, 0, 700, 98
29552, V, 1, 1, 1, 1, 0, 700, 98
29553, V, 1, 1, 1, 1, 0, 700, 98
29554, V, 1, 1, 1, 1, 0, 700, 98
29555, V, 1, 1, 1, 1, 0, 700, 98
29556, V, 1, 1, 1, 1, 0, 700, 98
29557, V, 1, 1, 1, 1, 0, 700, 98
29558, V, 1, 1, 1, 1, 0, 700, 98
29559, V, 1, 1, 1, 1, 0, 700, 98
29560, V, 1, 1, 1, 1, 0, 700, 98
29561, V, 1, 1, 1, 1, 0, 700, 98
29562, V, 1, 1, 1, 1, 0, 700, 98
29563, V, 1, 1, 1, 1, 0, 700, 98
29564, V, 1, 1, 1, 1, 0, 700, 98
29565, V, 1, 1, 1, 1, 0, 700, 98
29566, V, 1, 1, 1, 1, 0, 700, 98
29568, V, 1, 1, 1, 1, 0, 700, 98
29569, V, 1, 1, 1, 1, 0, 700, 98
29570, V, 1, 1, 1, 1, 0, 700, 98
29571, V, 1, 1, 1, 1, 0, 700, 98
29572, V, 1, 1, 1, 1, 0, 700, 98
29573, V, 1, 1, 1, 1, 0, 700, 98
29574, V, 1, 1, 1, 1, 0, 700, 98
29575, V, 1, 1, 1, 1, 0, 700, 98
29576, V, 1, 1, 1, 1, 0, 700, 98
29577, V, 1, 1, 1, 1, 0, 700, 98
29578, V, 1, 1, 1, 1, 0, 700, 98
29579, V, 1, 1, 1, 1, 0, 700, 98
29580, V, 1, 1, 1, 1, 0, 700, 98
29581, V, 1, 1, 1, 1, 0, 700, 98
29582, V, 1, 1, 1, 1, 0, 700, 98
29583, V, 1, 1, 1, 1, 0, 700, 98
29584, V, 1, 1, 1, 1, 0, 700, 98
29585, V, 1, 1, 1, 1, 0, 700, 98
29586, V, 1, 1, 1, 1, 0, 700, 98
29587, V, 1, 1, 1, 1, 0, 700, 98
29588, V, 1, 1, 1, 1, 0, 700, 98
29589, V, 1, 1, 1, 1, 0, 700, 98
29590, V, 1, 1, 1, 1, 0, 700, 98
29591, V, 1, 1, 1, 1, 0, 700, 98
29592, V, 1, 1, 1, 1, 0, 700, 98
29593, V, 1, 1, 1, 1, 0, 700, 98
29594, V, 1, 1, 1, 1, 0, 700, 98
29595, V, 1, 1, 1, 1, 0, 700, 98
29596, V, 1, 1, 1, 1, 0, 700, 98
29597, V, 1, 1, 1, 1, 0, 700, 98
29598, V, 1, 1, 1, 1, 0, 700, 98
29599, V, 1, 1, 1, 1, 0, 700, 98
29600, V, 1, 1, 1, 1, 0, 700, 98
29601, V, 1, 1, 1, 1, 0, 700, 98
29602, V, 1, 1, 1, 1, 0, 700, 98
29603, V, 1, 1, 1, 1, 0, 700, 98
29604, V, 1, 1, 1, 1, 0, 700, 98
29605, V, 1, 1, 1, 1, 0, 700, 98
29606, V, 1, 1, 1, 1, 0, 700, 98
29607, V, 1, 1, 1, 1, 0, 700, 98
29608, V, 1, 1, 1, 1, 0, 700, 98
29609, V, 1, 1, 1, 1, 0, 700, 98
29611, V, 1, 1, 1, 1, 0, 700, 98
29612, V, 1, 1, 1, 1, 0, 700, 98
29613, V, 1, 1, 1, 1, 0, 700, 98
29614, V, 1, 1, 1, 1, 0, 700, 98
29615, V, 1, 1, 1, 1, 0, 700, 98
29616, V, 1, 1, 1, 1, 0, 700, 98
29617, V, 1, 1, 1, 1, 0, 700, 98
29618, V, 1, 1, 1, 1, 0, 700, 98
29619, V, 1, 1, 1, 1, 0, 700, 98
29620, V, 1, 1, 1, 1, 0, 700, 98
29621, V, 1, 1, 1, 1, 0, 700, 98
29622, V, 1, 1, 1, 1, 0, 700, 98
29623, V, 1, 1, 1, 1, 0, 700, 98
29624, V, 1, 1, 1, 1, 0, 700, 98
29625, V, 1, 1, 1, 1, 0, 700, 98
29626, V, 1, 1, 1, 1, 0, 700, 98
29627, V, 1, 1, 1, 1, 0, 700, 98
29628, V, 1, 1, 1, 1, 0, 700, 98
29629, V, 1, 1, 1, 1, 0, 700, 98
29630, V, 1, 1, 1, 1, 0, 700, 98
29631, V, 1, 1, 1, 1, 0, 700, 98
29632, V, 1, 1, 1, 1, 0, 700, 98
29633, V, 1, 1, 1, 1, 0, 700, 98
29634, V, 1, 1, 1, 1, 0, 700, 98
29635, V, 1, 1, 1, 1, 0, 700, 98
29636, V, 1, 1, 1, 1, 0, 700, 98
29637, V, 1, 1, 1, 1, 0, 700, 98
29638, V, 1, 1, 1, 1, 0, 700, 98
29639, V, 1, 1, 1, 1, 0, 700, 98
29640, V, 1, 1, 1, 1, 0, 700, 98
29641, V, 1, 1, 1, 1, 0, 700, 98
29642, V, 1, 1, 1, 1, 0, 700, 98
29643, V, 1, 1, 1, 1, 0, 700, 98
29644, V, 1, 1, 1, 1, 0, 700, 98
29645, V, 1, 1, 1, 1, 0, 700, 98
29646, V, 1, 1, 1, 1, 0, 700, 98
29647, V, 1, 1, 1, 1, 0, 700, 98
29648, V, 1, 1, 1, 1, 0, 700, 98
29649, V, 1, 1, 1, 1, 0, 700, 98
29650, V, 1, 1, 1, 1, 0, 700, 98
29651, V, 1, 1, 1, 1, 0, 700, 98
29652, V, 1, 1, 1, 1, 0, 700, 98
29654, V, 1, 1, 1, 1, 0, 700, 98
29655, V, 1, 1, 1, 1, 0, 700, 98
29656, V, 1, 1, 1, 1, 0, 700, 98
29657, V, 1, 1, 1, 1, 0, 700, 98
29658, V, 1, 1, 1, 1, 0, 700, 98
29659, V, 1, 1, 1, 1, 0, 700, 98
29660, V, 1, 1, 1, 1, 0, 700, 98
29661, V, 1, 1, 1, 1, 0, 700, 98
29662, V, 1, 1, 1, 1, 0, 700, 98
29663, V, 1, 1, 1, 1, 0, 700, 98
29664, V, 1, 1, 1, 1, 0, 700, 98
29665, V, 1, 1, 1, 1, 0, 700, 98
29666, V, 1, 1, 1, 1, 0, 700, 98
29667, V, 1, 1, 1, 1, 0, 700, 98
29668, V, 1, 1, 1, 1, 0, 700, 98
29669, V, 1, 1, 1, 1, 0, 700, 98
29670, V, 1, 1, 1, 1, 0, 700, 98
29671, V, 1, 1, 1, 1, 0, 700, 98
29672, V, 1, 1, 1, 1, 0, 700, 98
29673, V, 1, 1, 1, 1, 0, 700, 98
29674, V, 1, 1, 1, 1, 0, 700, 98
29675, V, 1, 1, 1, 1, 0, 700, 98
29676, V, 1, 1, 1, 1, 0, 700, 98
29677, V, 1, 1, 1, 1, 0, 700, 98
29678, V, 1, 1, 1, 1, 0, 700, 98
29679, V, 1, 1, 1, 1, 0, 700, 98
29680, V, 1, 1, 1, 1, 0, 700, 98
29681, V, 1, 1, 1, 1, 0, 700, 98
29682, V, 1, 1, 1, 1, 0, 700, 98
29683, V, 1, 1, 1, 1, 0, 700, 98
29684, V, 1, 1, 1, 1, 0, 700, 98
29685, V, 1, 1, 1, 1, 0, 700, 98
29686, V, 1, 1, 1, 1, 0, 700, 98
29687, V, 1, 1, 1, 1, 0, 700, 98
29688, V, 1, 1, 1, 1, 0, 700, 98
29689, V, 1, 1, 1, 1, 0, 700, 98
29690, V, 1, 1, 1, 1, 0, 700, 98
29691, V, 1, 1, 1, 1, 0, 700, 98
29692, V, 1, 1, 1, 1, 0, 700, 98
29693, V, 1, 1, 1, 1, 0, 700, 98
29694, V, 1, 1, 1, 1, 0, 700, 98
29696, V, 1, 1, 1, 1, 0, 700, 98
29697, V, 1, 1, 1, 1, 0, 700, 98
29698, V, 1, 1, 1, 1, 0, 700, 98
29699, V, 1, 1, 1, 1, 0, 700, 98
29700, V, 1, 1, 1, 1, 0, 700, 98
29701, V, 1, 1, 1, 1, 0, 700, 98
29702, V, 1, 1, 1, 1, 0, 700, 98
29703, V, 1, 1, 1, 1, 0, 700, 98
29704, V, 1, 1, 1, 1, 0, 700, 98
29705, V, 1, 1, 1, 1, 0, 700, 98
29706, V, 1, 1, 1, 1, 0, 700, 98
29707, V, 1, 1, 1, 1, 0, 700, 98
29708, V, 1, 1, 1, 1, 0, 700, 98
29709, V, 1, 1, 1, 1, 0, 700, 98
29710, V, 1, 1, 1, 1, 0, 700, 98
29711, V, 1, 1, 1, 1, 0, 700, 98
29712, V, 1, 1, 1, 1, 0, 700, 98
29713, V, 1, 1, 1, 1, 0, 700, 98
29714, V, 1, 1, 1, 1, 0, 700, 98
29715, V, 1, 1, 1, 1, 0, 700, 98
29716, V, 1, 1, 1, 1, 0, 700, 98
29717, V, 1, 1, 1, 1, 0, 700, 98
29718, V, 1, 1, 1, 1, 0, 700, 98
29719, V, 1, 1, 1, 1, 0, 700, 98
29720, V, 1, 1, 1, 1, 0, 700, 98
29721, V, 1, 1, 1, 1, 0, 700, 98
29722, V, 1, 1, 1, 1, 0, 700, 98
29723, V, 1, 1, 1, 1, 0, 700, 98
29724, V, 1, 1, 1, 1, 0, 700, 98
29725, V, 1, 1, 1, 1, 0, 700, 98
29726, V, 1, 1, 1, 1, 0, 700, 98
29727, V, 1, 1, 1, 1, 0, 700, 98
29728, V, 1, 1, 1, 1, 0, 700, 98
29729, V, 1, 1, 1, 1, 0, 700, 98
29730, V, 1, 1, 1, 1, 0, 700, 98
29731, V, 1, 1, 1, 1, 0, 700, 98
29732, V, 1, 1, 1, 1, 0, 700, 98
29733, V, 1, 1, 1, 1, 0, 700, 98
29734, V, 1, 1, 1, 1, 0, 700, 98
29735, V, 1, 1, 1, 1, 0, 700, 98
29736, V, 1, 1, 1, 1, 0, 700, 98
29737, V, 1, 1, 1, 1, 0, 700, 98
29739, V, 1, 1, 1, 1, 0, 700, 98
29740, V, 1, 1, 1, 1, 0, 700, 98
29741, V, 1, 1, 1, 1, 0, 700, 98
29742, V, 1, 1, 1, 1, 0, 700, 98
29743, V, 1, 1, 1, 1, 0, 700, 98
29744, V, 1, 1, 1, 1, 0, 700, 98
29745, V, 1, 1, 1, 1, 0, 700, 98
29746, V, 1, 1, 1, 1, 0, 700, 98
29747, V, 1, 1, 1, 1, 0, 700, 98
29748, V, 1, 1, 1, 1, 0, 700, 98
29749, V, 1, 1, 1, 1, 0, 700, 98
29750, V, 1, 1, 1, 1, 0, 700, 98
29751, V, 1, 1, 1, 1, 0, 700, 98
29752, V, 1, 1, 1, 1, 0, 700, 98
29753, V, 1, 1, 1, 1, 0, 700, 98
29754, V, 1, 1, 1, 1, 0, 700, 98
29755, V, 1, 1, 1, 1, 0, 700, 98
29756, V, 1, 1, 1, 1, 0, 700, 98
29757, V, 1, 1, 1, 1, 0, 700, 98
29758, V, 1, 1, 1, 1, 0, 700, 98
29759, V, 1, 1, 1, 1, 0, 700, 98
29760, V, 1, 1, 1, 1, 0, 700, 98
29761, V, 1, 1, 1, 1, 0, 700, 98
29762, V, 1, 1, 1, 1, 0, 700, 98
29763, V, 1, 1, 1, 1, 0, 700, 98
29764, V, 1, 1, 1, 1, 0, 700, 98
29765, V, 1, 1, 1, 1, 0, 700, 98
29766, V, 1, 1, 1, 1, 0, 700, 98
29767, V, 1, 1, 1, 1, 0, 700, 98
29768, V, 1, 1, 1, 1, 0, 700, 98
29769, V, 1, 1, 1, 1, 0, 700, 98
29770, V, 1, 1, 1, 1, 0, 700, 98
29771, V, 1, 1, 1, 1, 0, 700, 98
29772, V, 1, 1, 1, 1, 0, 700, 98
29773, V, 1, 1, 1, 1, 0, 700, 98
29774, V, 1, 1, 1, 1, 0, 700, 98
29775, V, 1, 1, 1, 1, 0, 700, 98
29776, V, 1, 1, 1, 1, 0, 700, 98
29777, V, 1, 1, 1, 1, 0, 700, 98
29778, V, 1, 1, 1, 1, 0, 700, 98
29779, V, 1, 1, 1, 1, 0, 700, 98
29780, V, 1, 1, 1, 1, 0, 700, 98
29782, V, 1, 1, 1, 1, 0, 700, 98
29783, V, 1, 1, 1, 1, 0, 700, 98
29784, V, 1, 1, 1, 1, 0, 700, 98
29785, V, 1, 1, 1, 1, 0, 700, 98
29786, V, 1, 1, 1, 1, 0, 700, 98
29787, V, 1, 1, 1, 1, 0, 700, 98
29788, V, 1, 1, 1, 1, 0, 700, 98
29789, V, 1, 1, 1, 1, 0, 700, 98
29790, V, 1, 1, 1, 1, 0, 700, 98
29791, V, 1, 1, 1, 1, 0, 700, 98
29792, V, 1, 1, 1, 1, 0, 700, 98
29793, V, 1, 1, 1, 1, 0, 700, 98
29794, V, 1, 1, 1, 1, 0, 700, 98
29795, V, 1, 1, 1, 1, 0, 700, 98
29796, V, 1, 1, 1, 1, 0, 700, 98
29797, V, 1, 1, 1, 1, 0, 700, 98
29798, V, 1, 1, 1, 1, 0, 700, 98
29799, V, 1, 1, 1, 1, 0, 700, 98
29800, V, 1, 1, 1, 1, 0, 700, 98
29801, V, 1, 1, 1, 1, 0, 700, 98
29802, V, 1, 1, 1, 1, 0, 700, 98
29803, V, 1, 1, 1, 1, 0, 700, 98
29804, V, 1, 1, 1, 1, 0, 700, 98
29805, V, 1, 1, 1, 1, 0, 700, 98
29806, V, 1, 1, 1, 1, 0, 700, 98
29807, V, 1, 1, 1, 1, 0, 700, 98
29808, V, 1, 1, 1, 1, 0, 700, 98
29809, V, 1, 1, 1, 1, 0, 700, 98
29810, V, 1, 1, 1, 1, 0, 700, 98
29811, V, 1, 1, 1, 1, 0, 700, 98
29812, V, 1, 1, 1, 1, 0, 700, 98
29813, V, 1, 1, 1, 1, 0, 700, 98
29814, V, 1, 1, 1, 1, 0, 700, 98
29815, V, 1, 1, 1, 1, 0, 700, 98
29816, V, 1, 1, 1, 1, 0, 700, 98
29817, V, 1, 1, 1, 1, 0, 700, 98
29818, V, 1, 1, 1, 1, 0, 700, 98
29819, V, 1, 1, 1, 1, 0, 700, 98
29820, V, 1, 1, 1, 1, 0, 700, 98
29821, V, 1, 1, 1, 1, 0, 700, 98
29822, V, 1, 1, 1, 1, 0, 700, 98
29824, V, 1, 1, 1, 1, 0, 700, 98
29825, V, 1, 1, 1, 1, 0, 700, 98
29826, V, 1, 1, 1, 1, 0, 700, 98
29827, V, 1, 1, 1, 1, 0, 700, 98
29828, V, 1, 1, 1, 1, 0, 700, 98
29829, V, 1, 1, 1, 1, 0, 700, 98
29830, V, 1, 1, 1, 1, 0, 700, 98
29831, V, 1, 1, 1, 1, 0, 700, 98
29832, V, 1, 1, 1, 1, 0, 700, 98
29833, V, 1, 1, 1, 1, 0, 700, 98
29834, V, 1, 1, 1, 1, 0, 700, 98
29835, V, 1, 1, 1, 1, 0, 700, 98
29836, V, 1, 1, 1, 1, 0, 700, 98
29837, V, 1, 1, 1, 1, 0, 700, 98
29838, V, 1, 1, 1, 1, 0, 700, 98
29839, V, 1, 1, 1, 1, 0, 700, 98
29840, V, 1, 1, 1, 1, 0, 700, 98
29841, V, 1, 1, 1, 1, 0, 700, 98
29842, V, 1, 1, 1, 1, 0, 700, 98
29843, V, 1, 1, 1, 1, 0, 700, 98
29844, V, 1, 1, 1, 1, 0, 700, 98
29845, V, 1, 1, 1, 1, 0, 700, 98
29846, V, 1, 1, 1, 1, 0, 700, 98
29847, V, 1, 1, 1, 1, 0, 700, 98
29848, V, 1, 1, 1, 1, 0, 700, 98
29849, V, 1, 1, 1, 1, 0, 700, 98
29850, V, 1, 1, 1, 1, 0, 700, 98
29851, V, 1, 1, 1, 1, 0, 700, 98
29852, V, 1, 1, 1, 1, 0, 700, 98
29853, V, 1, 1, 1, 1, 0, 700, 98
29854, V, 1, 1, 1, 1, 0, 700, 98
29855, V, 1, 1, 1, 1, 0, 700, 98
29856, V, 1, 1, 1, 1, 0, 700, 98
29857, V, 1, 1, 1, 1, 0, 700, 98
29858, V, 1, 1, 1, 1, 0, 700, 98
29859, V, 1, 1, 1, 1, 0, 700, 98
29860, V, 1, 1, 1, 1, 0, 700, 98
29861, V, 1, 1, 1, 1, 0, 700, 98
29862, V, 1, 1, 1, 1, 0, 700, 98
29863, V, 1, 1, 1, 1, 0, 700, 98
29864, V, 1, 1, 1, 1, 0, 700, 98
29865, V, 1, 1, 1, 1, 0, 700, 98
29867, V, 1, 1, 1, 1, 0, 700, 98
29868, V, 1, 1, 1, 1, 0, 700, 98
29869, V, 1, 1, 1, 1, 0, 700, 98
29870, V, 1, 1, 1, 1, 0, 700, 98
29871, V, 1, 1, 1, 1, 0, 700, 98
29872, V, 1, 1, 1, 1, 0, 700, 98
29873, V, 1, 1, 1, 1, 0, 700, 98
29874, V, 1, 1, 1, 1, 0, 700, 98
29875, V, 1, 1, 1, 1, 0, 700, 98
29876, V, 1, 1, 1, 1, 0, 700, 98
29877, V, 1, 1, 1, 1, 0, 700, 98
29878, V, 1, 1, 1, 1, 0, 700, 98
29879, V, 1, 1, 1, 1, 0, 700, 98
29880, V, 1, 1, 1, 1, 0, 700, 98
29881, V, 1, 1, 1, 1, 0, 700, 98
29882, V, 1, 1, 1, 1, 0, 700, 98
29883, V, 1, 1, 1, 1, 0, 700, 98
29884, V, 1, 1, 1, 1, 0, 700, 98
29885, V, 1, 1, 1, 1, 0, 700, 98
29886, V, 1, 1, 1, 1, 0, 700, 98
29887, V, 1, 1, 1, 1, 0, 700, 98
29888, V, 1, 1, 1, 1, 0, 700, 98
29889, V, 1, 1, 1, 1, 0, 700, 98
29890, V, 1, 1, 1, 1, 0, 700, 98
29891, V, 1, 1, 1, 1, 0, 700, 98
29892, V, 1, 1, 1, 1, 0, 700, 98
29893, V, 1, 1, 1, 1, 0, 700, 98
29894, V, 1, 1, 1, 1, 0, 700, 98
29895, V, 1, 1, 1, 1, 0, 700, 98
29896, V, 1, 1, 1, 1, 0, 700, 98
29897, V, 1, 1, 1, 1, 0, 700, 98
29898, V, 1, 1, 1, 1, 0, 700, 98
29899, V, 1, 1, 1, 1, 0, 700, 98
29900, V, 1, 1, 1, 1, 0, 700, 98
29901, V, 1, 1, 1, 1, 0, 700, 98
29902, V, 1, 1, 1, 1, 0, 700, 98
29903, V, 1, 1, 1, 1, 0, 700, 98
29904, V, 1, 1, 1, 1, 0, 700, 98
29905, V, 1, 1, 1, 1, 0, 700, 98
29906, V, 1, 1, 1, 1, 0, 700, 98
29907, V, 1, 1, 1, 1, 0, 700, 98
29908, V, 1, 1, 1, 1, 0, 700, 98
29910, V, 1, 1, 1, 1, 0, 700, 98
29911, V, 1, 1, 1, 1, 0, 700, 98
29912, V, 1, 1, 1, 1, 0, 700, 98
29913, V, 1, 1, 1, 1, 0, 700, 98
29914, V, 1, 1, 1, 1, 0, 700, 98
29915, V, 1, 1, 1, 1, 0, 700, 98
29916, V, 1, 1, 1, 1, 0, 700, 98
29917, V, 1, 1, 1, 1, 0, 700, 98
29918, V, 1, 1, 1, 1, 0, 700, 98
29919, V, 1, 1, 1, 1, 0, 700, 98
29920, V, 1, 1, 1, 1, 0, 700, 98
29921, V, 1, 1, 1, 1, 0, 700, 98
29922, V, 1, 1, 1, 1, 0, 700, 98
29923, V, 1, 1, 1, 1, 0, 700, 98
29924, V, 1, 1, 1, 1, 0, 700, 98
29925, V, 1, 1, 1, 1, 0, 700, 98
29926, V, 1, 1, 1, 1, 0, 700, 98
29927, V, 1, 1, 1, 1, 0, 700, 98
29928, V, 1, 1, 1, 1, 0, 700, 98
29929, V, 1, 1, 1, 1, 0, 700, 98
29930, V, 1, 1, 1, 1, 0, 700, 98
29931, V, 1, 1, 1, 1, 0, 700, 98
29932, V, 1, 1, 1, 1, 0, 700, 98
29933, V, 1, 1, 1, 1, 0, 700, 98
29934, V, 1, 1, 1, 1, 0, 700, 98
29935, V, 1, 1, 1, 1, 0, 700, 98
29936, V, 1, 1, 1, 1, 0, 700, 98
29937, V, 1, 1, 1, 1, 0, 700, 98
29938, V, 1, 1, 1, 1, 0, 700, 98
29939, V, 1, 1, 1, 1, 0, 700, 98
29940, V, 1, 1, 1, 1, 0, 700, 98
29941, V, 1, 1, 1, 1, 0, 700, 98
29942, V, 1, 1, 1, 1, 0, 700, 98
29943, V, 1, 1, 1, 1, 0, 700, 98
29944, V, 1, 1, 1, 1, 0, 700, 98
29945, V, 1, 1, 1, 1, 0, 700, 98
29946, V, 1, 1, 1, 1, 0, 700, 98
29947, V, 1, 1, 1, 1, 0, 700, 98
29948, V, 1, 1, 1, 1, 0, 700, 98
29949, V, 1, 1, 1, 1, 0, 700, 98
29950, V, 1, 1, 1, 1, 0, 700, 98
29952, V, 1, 1, 1, 1, 0, 700, 98
29953, V, 1, 1, 1, 1, 0, 700, 98
29954, V, 1, 1, 1, 1, 0, 700, 98
29955, V, 1, 1, 1, 1, 0, 700, 98
29956, V, 1, 1, 1, 1, 0, 700, 98
29957, V, 1, 1, 1, 1, 0, 700, 98
29958, V, 1, 1, 1, 1, 0, 700, 98
29959, V, 1, 1, 1, 1, 0, 700, 98
29960, V, 1, 1, 1, 1, 0, 700, 98
29961, V, 1, 1, 1, 1, 0, 700, 98
29962, V, 1, 1, 1, 1, 0, 700, 98
29963, V, 1, 1, 1, 1, 0, 700, 98
29964, V, 1, 1, 1, 1, 0, 700, 98
29965, V, 1, 1, 1, 1, 0, 700, 98
29966, V, 1, 1, 1, 1, 0, 700, 98
29967, V, 1, 1, 1, 1, 0, 700, 98
29968, V, 1, 1, 1, 1, 0, 700, 98
29969, V, 1, 1, 1, 1, 0, 700, 98
29970, V, 1, 1, 1, 1, 0, 700, 98
29971, V, 1, 1, 1, 1, 0, 700, 98
29972, V, 1, 1, 1, 1, 0, 700, 98
29973, V, 1, 1, 1, 1, 0, 700, 98
29974, V, 1, 1, 1, 1, 0, 700, 98
29975, V, 1, 1, 1, 1, 0, 700, 98
29976, V, 1, 1, 1, 1, 0, 700, 98
29977, V, 1, 1, 1, 1, 0, 700, 98
29978, V, 1, 1, 1, 1, 0, 700, 98
29979, V, 1, 1, 1, 1, 0, 700, 98
29980, V, 1, 1, 1, 1, 0, 700, 98
29981, V, 1, 1, 1, 1, 0, 700, 98
29982, V, 1, 1, 1, 1, 0, 700, 98
29983, V, 1, 1, 1, 1, 0, 700, 98
29984, V, 1, 1, 1, 1, 0, 700, 98
29985, V, 1, 1, 1, 1, 0, 700, 98
29986, V, 1, 1, 1, 1, 0, 700, 98
29987, V, 1, 1, 1, 1, 0, 700, 98
29988, V, 1, 1, 1, 1, 0, 700, 98
29989, V, 1, 1, 1, 1, 0, 700, 98
29990, V, 1, 1, 1, 1, 0, 700, 98
29991, V, 1, 1, 1, 1, 0, 700, 98
29992, V, 1, 1, 1, 1, 0, 700, 98
29993, V, 1, 1, 1, 1, 0, 700, 98
29995, V, 1, 1, 1, 1, 0, 700, 98
29996, V, 1, 1, 1, 1, 0, 700, 98
29997, V, 1, 1, 1, 1, 0, 700, 98
29998, V, 1, 1, 1, 1, 0, 700, 98
29999, V, 1, 1, 1, 1, 0, 700, 98
30000, V, 1, 1, 1, 1, 0, 700, 98
30001, V, 1, 1, 1, 1, 0, 700, 98
30002, V, 1, 1, 1, 1, 0, 700, 98
30003, V, 1, 1, 1, 1, 0, 700, 98
30004, V, 1, 1, 1, 1, 0, 700, 98
30005, V, 1, 1, 1, 1, 0, 700, 98
30006, V, 1, 1, 1, 1, 0, 700, 98
30007, V, 1, 1, 1, 1, 0, 700, 98
30008, V, 1, 1, 1, 1, 0, 700, 98
30009, V, 1, 1, 1, 1, 0, 700, 98
30010, V, 1, 1, 1, 1, 0, 700, 98
30011, V, 1, 1, 1, 1, 0, 700, 98
30012, V, 1, 1, 1, 1, 0, 700, 98
30013, V, 1, 1, 1, 1, 0, 700, 98
30014, V, 1, 1, 1, 1, 0, 700, 98
30015, V, 1, 1, 1, 1, 0, 700, 98
30016, V, 1, 1, 1, 1, 0, 700, 98
30017, V, 1, 1, 1, 1, 0, 700, 98
30018, V, 1, 1, 1, 1, 0, 700, 98
30019, V, 1, 1, 1, 1, 0, 700, 98
30020, V, 1, 1, 1, 1, 0, 700, 98
30021, V, 1, 1, 1, 1, 0, 700, 98
30022, V, 1, 1, 1, 1, 0, 700, 98
30023, V, 1, 1, 1, 1, 0, 700, 98
30024, V, 1, 1, 1, 1, 0, 700, 98
30025, V, 1, 1, 1, 1, 0, 700, 98
30026, V, 1, 1, 1, 1, 0, 700, 98
30027, V, 1, 1, 1, 1, 0, 700, 98
30028, V, 1, 1, 1, 1, 0, 700, 98
30029, V, 1, 1, 1, 1, 0, 700, 98
30030, V, 1, 1, 1, 1, 0, 700, 98
30031, V, 1, 1, 1, 1, 0, 700, 98
30032, V, 1, 1, 1, 1, 0, 700, 98
30033, V, 1, 1, 1, 1, 0, 700, 98
30034, V, 1, 1, 1, 1, 0, 700, 98
30035, V, 1, 1, 1, 1, 0, 700, 98
30036, V, 1, 1, 1, 1, 0, 700, 98
30038, V, 1, 1, 1, 1, 0, 700, 98
30039, V, 1, 1, 1, 1, 0, 700, 98
30040, V, 1, 1, 1, 1, 0, 700, 98
30041, V, 1, 1, 1, 1, 0, 700, 98
30042, V, 1, 1, 1, 1, 0, 700, 98
30043, V, 1, 1, 1, 1, 0, 700, 98
30044, V, 1, 1, 1, 1, 0, 700, 98
30045, V, 1, 1, 1, 1, 0, 700, 98
30046, V, 1, 1, 1, 1, 0, 700, 98
30047, V, 1, 1, 1, 1, 0, 700, 98
30048, V, 1, 1, 1, 1, 0, 700, 98
30049, V, 1, 1, 1, 1, 0, 700, 98
30050, V, 1, 1, 1, 1, 0, 700, 98
30051, V, 1, 1, 1, 1, 0, 700, 98
30052, V, 1, 1, 1, 1, 0, 700, 98
30053, V, 1, 1, 1, 1, 0, 700, 98
30054, V, 1, 1, 1, 1, 0, 700, 98
30055, V, 1, 1, 1, 1, 0, 700, 98
30056, V, 1, 1, 1, 1, 0, 700, 98
30057, V, 1, 1, 1, 1, 0, 700, 98
30058, V, 1, 1, 1, 1, 0, 700, 98
30059, V, 1, 1, 1, 1, 0, 700, 98
30060, V, 1, 1, 1, 1, 0, 700, 98
30061, V, 1, 1, 1, 1, 0, 700, 98
30062, V, 1, 1, 1, 1, 0, 700, 98
30063, V, 1, 1, 1, 1, 0, 700, 98
30064, V, 1, 1, 1, 1, 0, 700, 98
30065, V, 1, 1, 1, 1, 0, 700, 98
30066, V, 1, 1, 1, 1, 0, 700, 98
30067, V, 1, 1, 1, 1, 0, 700, 98
30068, V, 1, 1, 1, 1, 0, 700, 98
30069, V, 1, 1, 1, 1, 0, 700, 98
30070, V, 1, 1, 1, 1, 0, 700, 98
30071, V, 1, 1, 1, 1, 0, 700, 98
30072, V, 1, 1, 1, 1, 0, 700, 98
30073, V, 1, 1, 1, 1, 0, 700, 98
30074, V, 1, 1, 1, 1, 0, 700, 98
30075, V, 1, 1, 1, 1, 0, 700, 98
30076, V, 1, 1, 1, 1, 0, 700, 98
30077, V, 1, 1, 1, 1, 0, 700, 98
30078, V, 1, 1, 1, 1, 0, 700, 98
30080, V, 1, 1, 1, 1, 0, 700, 98
30081, V, 1, 1, 1, 1, 0, 700, 98
30082, V, 1, 1, 1, 1, 0, 700, 98
30083, V, 1, 1, 1, 1, 0, 700, 98
30084, V, 1, 1, 1, 1, 0, 700, 98
30085, V, 1, 1, 1, 1, 0, 700, 98
30086, V, 1, 1, 1, 1, 0, 700, 98
30087, V, 1, 1, 1, 1, 0, 700, 98
30088, V, 1, 1, 1, 1, 0, 700, 98
30089, V, 1, 1, 1, 1, 0, 700, 98
30090, V, 1, 1, 1, 1, 0, 700, 98
30091, V, 1, 1, 1, 1, 0, 700, 98
30092, V, 1, 1, 1, 1, 0, 700, 98
30093, V, 1, 1, 1, 1, 0, 700, 98
30094, V, 1, 1, 1, 1, 0, 700, 98
30095, V, 1, 1, 1, 1, 0, 700, 98
30096, V, 1, 1, 1, 1, 0, 700, 98
30097, V, 1, 1, 1, 1, 0, 700, 98
30098, V, 1, 1, 1, 1, 0, 700, 98
30099, V, 1, 1, 1, 1, 0, 700, 98
30100, V, 1, 1, 1, 1, 0, 700, 98
30101, V, 1, 1, 1, 1, 0, 700, 98
30102, V, 1, 1, 1, 1, 0, 700, 98
30103, V, 1, 1, 1, 1, 0, 700, 98
30104, V, 1, 1, 1, 1, 0, 700, 98
30105, V, 1, 1, 1, 1, 0, 700, 98
30106, V, 1, 1, 1, 1, 0, 700, 98
30107, V, 1, 1, 1, 1, 0, 700, 98
30108, V, 1, 1, 1, 1, 0, 700, 98
30109, V, 1, 1, 1, 1, 0, 700, 98
30110, V, 1, 1, 1, 1, 0, 700, 98
30111, V, 1, 1, 1, 1, 0, 700, 98
30112, V, 1, 1, 1, 1, 0, 700, 98
30113, V, 1, 1, 1, 1, 0, 700, 98
30114, V, 1, 1, 1, 1, 0, 700, 98
30115, V, 1, 1, 1, 1, 0, 700, 98
30116, V, 1, 1, 1, 1, 0, 700, 98
30117, V, 1, 1, 1, 1, 0, 700, 98
30118, V, 1, 1, 1, 1, 0, 700, 98
30119, V, 1, 1, 1, 1, 0, 700, 98
30120, V, 1, 1, 1, 1, 0, 700, 98
30121, V, 1, 1, 1, 1, 0, 700, 98
30123, V, 1, 1, 1, 1, 0, 700, 98
30124, V, 1, 1, 1, 1, 0, 700, 98
30125, V, 1, 1, 1, 1, 0, 700, 98
30126, V, 1, 1, 1, 1, 0, 700, 98
30127, V, 1, 1, 1, 1, 0, 700, 98
30128, V, 1, 1, 1, 1, 0, 700, 98
30129, V, 1, 1, 1, 1, 0, 700, 98
30130, V, 1, 1, 1, 1, 0, 700, 98
30131, V, 1, 1, 1, 1, 0, 700, 98
30132, V, 1, 1, 1, 1, 0, 700, 98
30133, V, 1, 1, 1, 1, 0, 700, 98
30134, V, 1, 1, 1, 1, 0, 700, 98
30135, V, 1, 1, 1, 1, 0, 700, 98
30136, V, 1, 1, 1, 1, 0, 700, 98
30137, V, 1, 1, 1, 1, 0, 700, 98
30138, V, 1, 1, 1, 1, 0, 700, 98
30139, V, 1, 1, 1, 1, 0, 700, 98
30140, V, 1, 1, 1, 1, 0, 700, 98
30141, V, 1, 1, 1, 1, 0, 700, 98
30142, V, 1, 1, 1, 1, 0, 700, 98
30143, V, 1, 1, 1, 1, 0, 700, 98
30144, V, 1, 1, 1, 1, 0, 700, 98
30145, V, 1, 1, 1, 1, 0, 700, 98
30146, V, 1, 1, 1, 1, 0, 700, 98
30147, V, 1, 1, 1, 1, 0, 700, 98
30148, V, 1, 1, 1, 1, 0, 700, 98
30149, V, 1, 1, 1, 1, 0, 700, 98
30150, V, 1, 1, 1, 1, 0, 700, 98
30151, V, 1, 1, 1, 1, 0, 700, 98
30152, V, 1, 1, 1, 1, 0, 700, 98
30153, V, 1, 1, 1, 1, 0, 700, 98
30154, V, 1, 1, 1, 1, 0, 700, 98
30155, V, 1, 1, 1, 1, 0, 700, 98
30156, V, 1, 1, 1, 1, 0, 700, 98
30157, V, 1, 1, 1, 1, 0, 700, 98
30158, V, 1, 1, 1, 1, 0, 700, 98
30159, V, 1, 1, 1, 1, 0, 700, 98
30160, V, 1, 1, 1, 1, 0, 700, 98
30161, V, 1, 1, 1, 1, 0, 700, 98
30162, V, 1, 1, 1, 1, 0, 700, 98
30163, V, 1, 1, 1, 1, 0, 700, 98
30164, V, 1, 1, 1, 1, 0, 700, 98
30166, V, 1, 1, 1, 1, 0, 700, 98
30167, V, 1, 1, 1, 1, 0, 700, 98
30168, V, 1, 1, 1, 1, 0, 700, 98
30169, V, 1, 1, 1, 1, 0, 700, 98
30170, V, 1, 1, 1, 1, 0, 700, 98
30171, V, 1, 1, 1, 1, 0, 700, 98
30172, V, 1, 1, 1, 1, 0, 700, 98
30173, V, 1, 1, 1, 1, 0, 700, 98
30174, V, 1, 1, 1, 1, 0, 700, 98
30175, V, 1, 1, 1, 1, 0, 700, 98
30176, V, 1, 1, 1, 1, 0, 700, 98
30177, V, 1, 1, 1, 1, 0, 700, 98
30178, V, 1, 1, 1, 1, 0, 700, 98
30179, V, 1, 1, 1, 1, 0, 700, 98
30180, V, 1, 1, 1, 1, 0, 700, 98
30181, V, 1, 1, 1, 1, 0, 700, 98
30182, V, 1, 1, 1, 1, 0, 700, 98
30183, V, 1, 1, 1, 1, 0, 700, 98
30184, V, 1, 1, 1, 1, 0, 700, 98
30185, V, 1, 1, 1, 1, 0, 700, 98
30186, V, 1, 1, 1, 1, 0, 700, 98
30187, V, 1, 1, 1, 1, 0, 700, 98
30188, V, 1, 1, 1, 1, 0, 700, 98
30189, V, 1, 1, 1, 1, 0, 700, 98
30190, V, 1, 1, 1, 1, 0, 700, 98
30191, V, 1, 1, 1, 1, 0, 700, 98
30192, V, 1, 1, 1, 1, 0, 700, 98
30193, V, 1, 1, 1, 1, 0, 700, 98
30194, V, 1, 1, 1, 1, 0, 700, 98
30195, V, 1, 1, 1, 1, 0, 700, 98
30196, V, 1, 1, 1, 1, 0, 700, 98
30197, V, 1, 1, 1, 1, 0, 700, 98
30198, V, 1, 1, 1, 1, 0, 700, 98
30199, V, 1, 1, 1, 1, 0, 700, 98
30200, V, 1, 1, 1, 1, 0, 700, 98
30201, V, 1, 1, 1, 1, 0, 700, 98
30202, V, 1, 1, 1, 1, 0, 700, 98
30203, V, 1, 1, 1, 1, 0, 700, 98
30204, V, 1, 1, 1, 1, 0, 700, 98
30205, V, 1, 1, 1, 1, 0, 700, 98
30206, V, 1, 1, 1, 1, 0, 700, 98
30208, V, 1, 1, 1, 1, 0, 700, 98
30209, V, 1, 1, 1, 1, 0, 700, 98
30210, V, 1, 1, 1, 1, 0, 700, 98
30211, V, 1, 1, 1, 1, 0, 700, 98
30212, V, 1, 1, 1, 1, 0, 700, 98
30213, V, 1, 1, 1, 1, 0, 700, 98
30214, V, 1, 1, 1, 1, 0, 700, 98
30215, V, 1, 1, 1, 1, 0, 700, 98
30216, V, 1, 1, 1, 1, 0, 700, 98
30217, V, 1, 1, 1, 1, 0, 700, 98
30218, V, 1, 1, 1, 1, 0, 700, 98
30219, V, 1, 1, 1, 1, 0, 700, 98
30220, V, 1, 1, 1, 1, 0, 700, 98
30221, V, 1, 1, 1, 1, 0, 700, 98
30222, V, 1, 1, 1, 1, 0, 700, 98
30223, V, 1, 1, 1, 1, 0, 700, 98
30224, V, 1, 1, 1, 1, 0, 700, 98
30225, V, 1, 1, 1, 1, 0, 700, 98
30226, V, 1, 1, 1, 1, 0, 700, 98
30227, V, 1, 1, 1, 1, 0, 700, 98
30228, V, 1, 1, 1, 1, 0, 700, 98
30229, V, 1, 1, 1, 1, 0, 700, 98
30230, V, 1, 1, 1, 1, 0, 700, 98
30231, V, 1, 1, 1, 1, 0, 700, 98
30232, V, 1, 1, 1, 1, 0, 700, 98
30233, V, 1, 1, 1, 1, 0, 700, 98
30234, V, 1, 1, 1, 1, 0, 700, 98
30235, V, 1, 1, 1, 1, 0, 700, 98
30236, V, 1, 1, 1, 1, 0, 700, 98
30237, V, 1, 1, 1, 1, 0, 700, 98
30238, V, 1, 1, 1, 1, 0, 700, 98
30239, V, 1, 1, 1, 1, 0, 700, 98
30240, V, 1, 1, 1, 1, 0, 700, 98
30241, V, 1, 1, 1, 1, 0, 700, 98
30242, V, 1, 1, 1, 1, 0, 700, 98
30243, V, 1, 1, 1, 1, 0, 700, 98
30244, V, 1, 1, 1, 1, 0, 700, 98
30245, V, 1, 1, 1, 1, 0, 700, 98
30246, V, 1, 1, 1, 1, 0, 700, 98
30247, V, 1, 1, 1, 1, 0, 700, 98
30248, V, 1, 1, 1, 1, 0, 700, 98
30249, V, 1, 1, 1, 1, 0, 700, 98
30251, V, 1, 1, 1, 1, 0, 700, 98
30252, V, 1, 1, 1, 1, 0, 700, 98
30253, V, 1, 1, 1, 1, 0, 700, 98
30254, V, 1, 1, 1, 1, 0, 700, 98
30255, V, 1, 1, 1, 1, 0, 700, 98
30256, V, 1, 1, 1, 1, 0, 700, 98
30257, V, 1, 1, 1, 1, 0, 700, 98
30258, V, 1, 1, 1, 1, 0, 700, 98
30259, V, 1, 1, 1, 1, 0, 700, 98
30260, V, 1, 1, 1, 1, 0, 700, 98
30261, V, 1, 1, 1, 1, 0, 700, 98
30262, V, 1, 1, 1, 1, 0, 700, 98
30263, V, 1, 1, 1, 1, 0, 700, 98
30264, V, 1, 1, 1, 1, 0, 700, 98
30265, V, 1, 1, 1, 1, 0, 700, 98
30266, V, 1, 1, 1, 1, 0, 700, 98
30267, V, 1, 1, 1, 1, 0, 700, 98
30268, V, 1, 1, 1, 1, 0, 700, 98
30269, V, 1, 1, 1, 1, 0, 700, 98
30270, V, 1, 1, 1, 1, 0, 700, 98
30271, V, 1, 1, 1, 1, 0, 700, 98
30272, V, 1, 1, 1, 1, 0, 700, 98
30273, V, 1, 1, 1, 1, 0, 700, 98
30274, V, 1, 1, 1, 1, 0, 700, 98
30275, V, 1, 1, 1, 1, 0, 700, 98
30276, V, 1, 1, 1, 1, 0, 700, 98
30277, V, 1, 1, 1, 1, 0, 700, 98
30278, V, 1, 1, 1, 1, 0, 700, 98
30279, V, 1, 1, 1, 1, 0, 700, 98
30280, V, 1, 1, 1, 1, 0, 700, 98
30281, V, 1, 1, 1, 1, 0, 700, 98
30282, V, 1, 1, 1, 1, 0, 700, 98
30283, V, 1, 1, 1, 1, 0, 700, 98
30284, V, 1, 1, 1, 1, 0, 700, 98
30285, V, 1, 1, 1, 1, 0, 700, 98
30286, V, 1, 1, 1, 1, 0, 700, 98
30287, V, 1, 1, 1, 1, 0, 700, 98
30288, V, 1, 1, 1, 1, 0, 700, 98
30289, V, 1, 1, 1, 1, 0, 700, 98
30290, V, 1, 1, 1, 1, 0, 700, 98
30291, V, 1, 1, 1, 1, 0, 700, 98
30292, V, 1, 1, 1, 1, 0, 700, 98
30294, V, 1, 1, 1, 1, 0, 700, 98
30295, V, 1, 1, 1, 1, 0, 700, 98
30296, V, 1, 1, 1, 1, 0, 700, 98
30297, V, 1, 1, 1, 1, 0, 700, 98
30298, V, 1, 1, 1, 1, 0, 700, 98
30299, V, 1, 1, 1, 1, 0, 700, 98
30300, V, 1, 1, 1, 1, 0, 700, 98
30301, V, 1, 1, 1, 1, 0, 700, 98
30302, V, 1, 1, 1, 1, 0, 700, 98
30303, V, 1, 1, 1, 1, 0, 700, 98
30304, V, 1, 1, 1, 1, 0, 700, 98
30305, V, 1, 1, 1, 1, 0, 700, 98
30306, V, 1, 1, 1, 1, 0, 700, 98
30307, V, 1, 1, 1, 1, 0, 700, 98
30308, V, 1, 1, 1, 1, 0, 700, 98
30309, V, 1, 1, 1, 1, 0, 700, 98
30310, V, 1, 1, 1, 1, 0, 700, 98
30311, V, 1, 1, 1, 1, 0, 700, 98
30312, V, 1, 1, 1, 1, 0, 700, 98
30313, V, 1, 1, 1, 1, 0, 700, 98
30314, V, 1, 1, 1, 1, 0, 700, 98
30315, V, 1, 1, 1, 1, 0, 700, 98
30316, V, 1, 1, 1, 1, 0, 700, 98
30317, V, 1, 1, 1, 1, 0, 700, 98
30318, V, 1, 1, 1, 1, 0, 700, 98
30319, V, 1, 1, 1, 1, 0, 700, 98
30320, V, 1, 1, 1, 1, 0, 700, 98
30321, V, 1, 1, 1, 1, 0, 700, 98
30322, V, 1, 1, 1, 1, 0, 700, 98
30323, V, 1, 1, 1, 1, 0, 700, 98
30324, V, 1, 1, 1, 1, 0, 700, 98
30325, V, 1, 1, 1, 1, 0, 700, 98
30326, V, 1, 1, 1, 1, 0, 700, 98
30327, V, 1, 1, 1, 1, 0, 700, 98
30328, V, 1, 1, 1, 1, 0, 700, 98
30329, V, 1, 1, 1, 1, 0, 700, 98
30330, V, 1, 1, 1, 1, 0, 700, 98
30331, V, 1, 1, 1, 1, 0, 700, 98
30332, V, 1, 1, 1, 1, 0, 700, 98
30333, V, 1, 1, 1, 1, 0, 700, 98
30334, V, 1, 1, 1, 1, 0, 700, 98
30336, V, 1, 1, 1, 1, 0, 700, 98
30337, V, 1, 1, 1, 1, 0, 700, 98
30338, V, 1, 1, 1, 1, 0, 700, 98
30339, V, 1, 1, 1, 1, 0, 700, 98
30340, V, 1, 1, 1, 1, 0, 700, 98
30341, V, 1, 1, 1, 1, 0, 700, 98
30342, V, 1, 1, 1, 1, 0, 700, 98
30343, V, 1, 1, 1, 1, 0, 700, 98
30344, V, 1, 1, 1, 1, 0, 700, 98
30345, V, 1, 1, 1, 1, 0, 700, 98
30346, V, 1, 1, 1, 1, 0, 700, 98
30347, V, 1, 1, 1, 1, 0, 700, 98
30348, V, 1, 1, 1, 1, 0, 700, 98
30349, V, 1, 1, 1, 1, 0, 700, 98
30350, V, 1, 1, 1, 1, 0, 700, 98
30351, V, 1, 1, 1, 1, 0, 700, 98
30352, V, 1, 1, 1, 1, 0, 700, 98
30353, V, 1, 1, 1, 1, 0, 700, 98
30354, V, 1, 1, 1, 1, 0, 700, 98
30355, V, 1, 1, 1, 1, 0, 700, 98
30356, V, 1, 1, 1, 1, 0, 700, 98
30357, V, 1, 1, 1, 1, 0, 700, 98
30358, V, 1, 1, 1, 1, 0, 700, 98
30359, V, 1, 1, 1, 1, 0, 700, 98
30360, V, 1, 1, 1, 1, 0, 700, 98
30361, V, 1, 1, 1, 1, 0, 700, 98
30362, V, 1, 1, 1, 1, 0, 700, 98
30363, V, 1, 1, 1, 1, 0, 700, 98
30364, V, 1, 1, 1, 1, 0, 700, 98
30365, V, 1, 1, 1, 1, 0, 700, 98
30366, V, 1, 1, 1, 1, 0, 700, 98
30367, V, 1, 1, 1, 1, 0, 700, 98
30368, V, 1, 1, 1, 1, 0, 700, 98
30369, V, 1, 1, 1, 1, 0, 700, 98
30370, V, 1, 1, 1, 1, 0, 700, 98
30371, V, 1, 1, 1, 1, 0, 700, 98
30372, V, 1, 1, 1, 1, 0, 700, 98
30373, V, 1, 1, 1, 1, 0, 700, 98
30374, V, 1, 1, 1, 1, 0, 700, 98
30375, V, 1, 1, 1, 1, 0, 700, 98
30376, V, 1, 1, 1, 1, 0, 700, 98
30377, V, 1, 1, 1, 1, 0, 700, 98
30379, V, 1, 1, 1, 1, 0, 700, 98
30380, V, 1, 1, 1, 1, 0, 700, 98
30381, V, 1, 1, 1, 1, 0, 700, 98
30382, V, 1, 1, 1, 1, 0, 700, 98
30383, V, 1, 1, 1, 1, 0, 700, 98
30384, V, 1, 1, 1, 1, 0, 700, 98
30385, V, 1, 1, 1, 1, 0, 700, 98
30386, V, 1, 1, 1, 1, 0, 700, 98
30387, V, 1, 1, 1, 1, 0, 700, 98
30388, V, 1, 1, 1, 1, 0, 700, 98
30389, V, 1, 1, 1, 1, 0, 700, 98
30390, V, 1, 1, 1, 1, 0, 700, 98
30391, V, 1, 1, 1, 1, 0, 700, 98
30392, V, 1, 1, 1, 1, 0, 700, 98
30393, V, 1, 1, 1, 1, 0, 700, 98
30394, V, 1, 1, 1, 1, 0, 700, 98
30395, V, 1, 1, 1, 1, 0, 700, 98
30396, V, 1, 1, 1, 1, 0, 700, 98
30397, V, 1, 1, 1, 1, 0, 700, 98
30398, V, 1, 1, 1, 1, 0, 700, 98
30399, V, 1, 1, 1, 1, 0, 700, 98
30400, V, 1, 1, 1, 1, 0, 700, 98
30401, V, 1, 1, 1, 1, 0, 700, 98
30402, V, 1, 1, 1, 1, 0, 700, 98
30403, V, 1, 1, 1, 1, 0, 700, 98
30404, V, 1, 1, 1, 1, 0, 700, 98
30405, V, 1, 1, 1, 1, 0, 700, 98
30406, V, 1, 1, 1, 1, 0, 700, 98
30407, V, 1, 1, 1, 1, 0, 700, 98
30408, V, 1, 1, 1, 1, 0, 700, 98
30409, V, 1, 1, 1, 1, 0, 700, 98
30410, V, 1, 1, 1, 1, 0, 700, 98
30411, V, 1, 1, 1, 1, 0, 700, 98
30412, V, 1, 1, 1, 1, 0, 700, 98
30413, V, 1, 1, 1, 1, 0, 700, 98
30414, V, 1, 1, 1, 1, 0, 700, 98
30415, V, 1, 1, 1, 1, 0, 700, 98
30416, V, 1, 1, 1, 1, 0, 700, 98
30417, V, 1, 1, 1, 1, 0, 700, 98
30418, V, 1, 1, 1, 1, 0, 700, 98
30419, V, 1, 1, 1, 1, 0, 700, 98
30420, V, 1, 1, 1, 1, 0, 700, 98
30422, V, 1, 1, 1, 1, 0, 700, 98
30423, V, 1, 1, 1, 1, 0, 700, 98
30424, V, 1, 1, 1, 1, 0, 700, 98
30425, V, 1, 1, 1, 1, 0, 700, 98
30426, V, 1, 1, 1, 1, 0, 700, 98
30427, V, 1, 1, 1, 1, 0, 700, 98
30428, V, 1, 1, 1, 1, 0, 700, 98
30429, V, 1, 1, 1, 1, 0, 700, 98
30430, V, 1, 1, 1, 1, 0, 700, 98
30431, V, 1, 1, 1, 1, 0, 700, 98
30432, V, 1, 1, 1, 1, 0, 700, 98
30433, V, 1, 1, 1, 1, 0, 700, 98
30434, V, 1, 1, 1, 1, 0, 700, 98
30435, V, 1, 1, 1, 1, 0, 700, 98
30436, V, 1, 1, 1, 1, 0, 700, 98
30437, V, 1, 1, 1, 1, 0, 700, 98
30438, V, 1, 1, 1, 1, 0, 700, 98
30439, V, 1, 1, 1, 1, 0, 700, 98
30440, V, 1, 1, 1, 1, 0, 700, 98
30441, V, 1, 1, 1, 1, 0, 700, 98
30442, V, 1, 1, 1, 1, 0, 700, 98
30443, V, 1, 1, 1, 1, 0, 700, 98
30444, V, 1, 1, 1, 1, 0, 700, 98
30445, V, 1, 1, 1, 1, 0, 700, 98
30446, V, 1, 1, 1, 1, 0, 700, 98
30447, V, 1, 1, 1, 1, 0, 700, 98
30448, V, 1, 1, 1, 1, 0, 700, 98
30449, V, 1, 1, 1, 1, 0, 700, 98
30450, V, 1, 1, 1, 1, 0, 700, 98
30451, V, 1, 1, 1, 1, 0, 700, 98
30452, V, 1, 1, 1, 1, 0, 700, 98
30453, V, 1, 1, 1, 1, 0, 700, 98
30454, V, 1, 1, 1, 1, 0, 700, 98
30455, V, 1, 1, 1, 1, 0, 700, 98
30456, V, 1, 1, 1, 1, 0, 700, 98
30457, V, 1, 1, 1, 1, 0, 700, 98
30458, V, 1, 1, 1, 1, 0, 700, 98
30459, V, 1, 1, 1, 1, 0, 700, 98
30460, V, 1, 1, 1, 1, 0, 700, 98
30461, V, 1, 1, 1, 1, 0, 700, 98
30462, V, 1, 1, 1, 1, 0, 700, 98
30464, V, 1, 1, 1, 1, 0, 700, 98
30465, V, 1, 1, 1, 1, 0, 700, 98
30466, V, 1, 1, 1, 1, 0, 700, 98
30467, V, 1, 1, 1, 1, 0, 700, 98
30468, V, 1, 1, 1, 1, 0, 700, 98
30469, V, 1, 1, 1, 1, 0, 700, 98
30470, V, 1, 1, 1, 1, 0, 700, 98
30471, V, 1, 1, 1, 1, 0, 700, 98
30472, V, 1, 1, 1, 1, 0, 700, 98
30473, V, 1, 1, 1, 1, 0, 700, 98
30474, V, 1, 1, 1, 1, 0, 700, 98
30475, V, 1, 1, 1, 1, 0, 700, 98
30476, V, 1, 1, 1, 1, 0, 700, 98
30477, V, 1, 1, 1, 1, 0, 700, 98
30478, V, 1, 1, 1, 1, 0, 700, 98
30479, V, 1, 1, 1, 1, 0, 700, 98
30480, V, 1, 1, 1, 1, 0, 700, 98
30481, V, 1, 1, 1, 1, 0, 700, 98
30482, V, 1, 1, 1, 1, 0, 700, 98
30483, V, 1, 1, 1, 1, 0, 700, 98
30484, V, 1, 1, 1, 1, 0, 700, 98
30485, V, 1, 1, 1, 1, 0, 700, 98
30486, V, 1, 1, 1, 1, 0, 700, 98
30487, V, 1, 1, 1, 1, 0, 700, 98
30488, V, 1, 1, 1, 1, 0, 700, 98
30489, V, 1, 1, 1, 1, 0, 700, 98
30490, V, 1, 1, 1, 1, 0, 700, 98
30491, V, 1, 1, 1, 1, 0, 700, 98
30492, V, 1, 1, 1, 1, 0, 700, 98
30493, V, 1, 1, 1, 1, 0, 700, 98
30494, V, 1, 1, 1, 1, 0, 700, 98
30495, V, 1, 1, 1, 1, 0, 700, 98
30496, V, 1, 1, 1, 1, 0, 700, 98
30497, V, 1, 1, 1, 1, 0, 700, 98
30498, V, 1, 1, 1, 1, 0, 700, 98
30499, V, 1, 1, 1, 1, 0, 700, 98
30500, V, 1, 1, 1, 1, 0, 700, 98
30501, V, 1, 1, 1, 1, 0, 700, 98
30502, V, 1, 1, 1, 1, 0, 700, 98
30503, V, 1, 1, 1, 1, 0, 700, 98
30504, V, 1, 1, 1, 1, 0, 700, 98
30505, V, 1, 1, 1, 1, 0, 700, 98
30507, V, 1, 1, 1, 1, 0, 700, 98
30508, V, 1, 1, 1, 1, 0, 700, 98
30509, V, 1, 1, 1, 1, 0, 700, 98
30510, V, 1, 1, 1, 1, 0, 700, 98
30511, V, 1, 1, 1, 1, 0, 700, 98
30512, V, 1, 1, 1, 1, 0, 700, 98
30513, V, 1, 1, 1, 1, 0, 700, 98
30514, V, 1, 1, 1, 1, 0, 700, 98
30515, V, 1, 1, 1, 1, 0, 700, 98
30516, V, 1, 1, 1, 1, 0, 700, 98
30517, V, 1, 1, 1, 1, 0, 700, 98
30518, V, 1, 1, 1, 1, 0, 700, 98
30519, V, 1, 1, 1, 1, 0, 700, 98
30520, V, 1, 1, 1, 1, 0, 700, 98
30521, V, 1, 1, 1, 1, 0, 700, 98
30522, V, 1, 1, 1, 1, 0, 700, 98
30523, V, 1, 1, 1, 1, 0, 700, 98
30524, V, 1, 1, 1, 1, 0, 700, 98
30525, V, 1, 1, 1, 1, 0, 700, 98
30526, V, 1, 1, 1, 1, 0, 700, 98
30527, V, 1, 1, 1, 1, 0, 700, 98
30528, V, 1, 1, 1, 1, 0, 700, 98
30529, V, 1, 1, 1, 1, 0, 700, 98
30530, V, 1, 1, 1, 1, 0, 700, 98
30531, V, 1, 1, 1, 1, 0, 700, 98
30532, V, 1, 1, 1, 1, 0, 700, 98
30533, V, 1, 1, 1, 1, 0, 700, 98
30534, V, 1, 1, 1, 1, 0, 700, 98
30535, V, 1, 1, 1, 1, 0, 700, 98
30536, V, 1, 1, 1, 1, 0, 700, 98
30537, V, 1, 1, 1, 1, 0, 700, 98
30538, V, 1, 1, 1, 1, 0, 700, 98
30539, V, 1, 1, 1, 1, 0, 700, 98
30540, V, 1, 1, 1, 1, 0, 700, 98
30541, V, 1, 1, 1, 1, 0, 700, 98
30542, V, 1, 1, 1, 1, 0, 700, 98
30543, V, 1, 1, 1, 1, 0, 700, 98
30544, V, 1, 1, 1, 1, 0, 700, 98
30545, V, 1, 1, 1, 1, 0, 700, 98
30546, V, 1, 1, 1, 1, 0, 700, 98
30547, V, 1, 1, 1, 1, 0, 700, 98
30548, V, 1, 1, 1, 1, 0, 700, 98
30550, V, 1, 1, 1, 1, 0, 700, 98
30551, V, 1, 1, 1, 1, 0, 700, 98
30552, V, 1, 1, 1, 1, 0, 700, 98
30553, V, 1, 1, 1, 1, 0, 700, 98
30554, V, 1, 1, 1, 1, 0, 700, 98
30555, V, 1, 1, 1, 1, 0, 700, 98
30556, V, 1, 1, 1, 1, 0, 700, 98
30557, V, 1, 1, 1, 1, 0, 700, 98
30558, V, 1, 1, 1, 1, 0, 700, 98
30559, V, 1, 1, 1, 1, 0, 700, 98
30560, V, 1, 1, 1, 1, 0, 700, 98
30561, V, 1, 1, 1, 1, 0, 700, 98
30562, V, 1, 1, 1, 1, 0, 700, 98
30563, V, 1, 1, 1, 1, 0, 700, 98
30564, V, 1, 1, 1, 1, 0, 700, 98
30565, V, 1, 1, 1, 1, 0, 700, 98
30566, V, 1, 1, 1, 1, 0, 700, 98
30567, V, 1, 1, 1, 1, 0, 700, 98
30568, V, 1, 1, 1, 1, 0, 700, 98
30569, V, 1, 1, 1, 1, 0, 700, 98
30570, V, 1, 1, 1, 1, 0, 700, 98
30571, V, 1, 1, 1, 1, 0, 700, 98
30572, V, 1, 1, 1, 1, 0, 700, 98
30573, V, 1, 1, 1, 1, 0, 700, 98
30574, V, 1, 1, 1, 1, 0, 700, 98
30575, V, 1, 1, 1, 1, 0, 700, 98
30576, V, 1, 1, 1, 1, 0, 700, 98
30577, V, 1, 1, 1, 1, 0, 700, 98
30578, V, 1, 1, 1, 1, 0, 700, 98
30579, V, 1, 1, 1, 1, 0, 700, 98
30580, V, 1, 1, 1, 1, 0, 700, 98
30581, V, 1, 1, 1, 1, 0, 700, 98
30582, V, 1, 1, 1, 1, 0, 700, 98
30583, V, 1, 1, 1, 1, 0, 700, 98
30584, V, 1, 1, 1, 1, 0, 700, 98
30585, V, 1, 1, 1, 1, 0, 700, 98
30586, V, 1, 1, 1, 1, 0, 700, 98
30587, V, 1, 1, 1, 1, 0, 700, 98
30588, V, 1, 1, 1, 1, 0, 700, 98
30589, V, 1, 1, 1, 1, 0, 700, 98
30590, V, 1, 1, 1, 1, 0, 700, 98
30592, V, 1, 1, 1, 1, 0, 700, 98
30593, V, 1, 1, 1, 1, 0, 700, 98
30594, V, 1, 1, 1, 1, 0, 700, 98
30595, V, 1, 1, 1, 1, 0, 700, 98
30596, V, 1, 1, 1, 1, 0, 700, 98
30597, V, 1, 1, 1, 1, 0, 700, 98
30598, V, 1, 1, 1, 1, 0, 700, 98
30599, V, 1, 1, 1, 1, 0, 700, 98
30600, V, 1, 1, 1, 1, 0, 700, 98
30601, V, 1, 1, 1, 1, 0, 700, 98
30602, V, 1, 1, 1, 1, 0, 700, 98
30603, V, 1, 1, 1, 1, 0, 700, 98
30604, V, 1, 1, 1, 1, 0, 700, 98
30605, V, 1, 1, 1, 1, 0, 700, 98
30606, V, 1, 1, 1, 1, 0, 700, 98
30607, V, 1, 1, 1, 1, 0, 700, 98
30608, V, 1, 1, 1, 1, 0, 700, 98
30609, V, 1, 1, 1, 1, 0, 700, 98
30610, V, 1, 1, 1, 1, 0, 700, 98
30611, V, 1, 1, 1, 1, 0, 700, 98
30612, V, 1, 1, 1, 1, 0, 700, 98
30613, V, 1, 1, 1, 1, 0, 700, 98
30614, V, 1, 1, 1, 1, 0, 700, 98
30615, V, 1, 1, 1, 1, 0, 700, 98
30616, V, 1, 1, 1, 1, 0, 700, 98
30617, V, 1, 1, 1, 1, 0, 700, 98
30618, V, 1, 1, 1, 1, 0, 700, 98
30619, V, 1, 1, 1, 1, 0, 700, 98
30620, V, 1, 1, 1, 1, 0, 700, 98
30621, V, 1, 1, 1, 1, 0, 700, 98
30622, V, 1, 1, 1, 1, 0, 700, 98
30623, V, 1, 1, 1, 1, 0, 700, 98
30624, V, 1, 1, 1, 1, 0, 700, 98
30625, V, 1, 1, 1, 1, 0, 700, 98
30626, V, 1, 1, 1, 1, 0, 700, 98
30627, V, 1, 1, 1, 1, 0, 700, 98
30628, V, 1, 1, 1, 1, 0, 700, 98
30629, V, 1, 1, 1, 1, 0, 700, 98
30630, V, 1, 1, 1, 1, 0, 700, 98
30631, V, 1, 1, 1, 1, 0, 700, 98
30632, V, 1, 1, 1, 1, 0, 700, 98
30633, V, 1, 1, 1, 1, 0, 700, 98
30635, V, 1, 1, 1, 1, 0, 700, 98
30636, V, 1, 1, 1, 1, 0, 700, 98
30637, V, 1, 1, 1, 1, 0, 700, 98
30638, V, 1, 1, 1, 1, 0, 700, 98
30639, V, 1, 1, 1, 1, 0, 700, 98
30640, V, 1, 1, 1, 1, 0, 700, 98
30641, V, 1, 1, 1, 1, 0, 700, 98
30642, V, 1, 1, 1, 1, 0, 700, 98
30643, V, 1, 1, 1, 1, 0, 700, 98
30644, V, 1, 1, 1, 1, 0, 700, 98
30645, V, 1, 1, 1, 1, 0, 700, 98
30646, V, 1, 1, 1, 1, 0, 700, 98
30647, V, 1, 1, 1, 1, 0, 700, 98
30648, V, 1, 1, 1, 1, 0, 700, 98
30649, V, 1, 1, 1, 1, 0, 700, 98
30650, V, 1, 1, 1, 1, 0, 700, 98
30651, V, 1, 1, 1, 1, 0, 700, 98
30652, V, 1, 1, 1, 1, 0, 700, 98
30653, V, 1, 1, 1, 1, 0, 700, 98
30654, V, 1, 1, 1, 1, 0, 700, 98
30655, V, 1, 1, 1, 1, 0, 700, 98
30656, V, 1, 1, 1, 1, 0, 700, 98
30657, V, 1, 1, 1, 1, 0, 700, 98
30658, V, 1, 1, 1, 1, 0, 700, 98
30659, V, 1, 1, 1, 1, 0, 700, 98
30660, V, 1, 1, 1, 1, 0, 700, 98
30661, V, 1, 1, 1, 1, 0, 700, 98
30662, V, 1, 1, 1, 1, 0, 700, 98
30663, V, 1, 1, 1, 1, 0, 700, 98
30664, V, 1, 1, 1, 1, 0, 700, 98
30665, V, 1, 1, 1, 1, 0, 700, 98
30666, V, 1, 1, 1, 1, 0, 700, 98
30667, V, 1, 1, 1, 1, 0, 700, 98
30668, V, 1, 1, 1, 1, 0, 700, 98
30669, V, 1, 1, 1, 1, 0, 700, 98
30670, V, 1, 1, 1, 1, 0, 700, 98
30671, V, 1, 1, 1, 1, 0, 700, 98
30672, V, 1, 1, 1, 1, 0, 700, 98
30673, V, 1, 1, 1, 1, 0, 700, 98
30674, V, 1, 1, 1, 1, 0, 700, 98
30675, V, 1, 1, 1, 1, 0, 700, 98
30676, V, 1, 1, 1, 1, 0, 700, 98
30678, V, 1, 1, 1, 1, 0, 700, 98
30679, V, 1, 1, 1, 1, 0, 700, 98
30680, V, 1, 1, 1, 1, 0, 700, 98
30681, V, 1, 1, 1, 1, 0, 700, 98
30682, V, 1, 1, 1, 1, 0, 700, 98
30683, V, 1, 1, 1, 1, 0, 700, 98
30684, V, 1, 1, 1, 1, 0, 700, 98
30685, V, 1, 1, 1, 1, 0, 700, 98
30686, V, 1, 1, 1, 1, 0, 700, 98
30687, V, 1, 1, 1, 1, 0, 700, 98
30688, V, 1, 1, 1, 1, 0, 700, 98
30689, V, 1, 1, 1, 1, 0, 700, 98
30690, V, 1, 1, 1, 1, 0, 700, 98
30691, V, 1, 1, 1, 1, 0, 700, 98
30692, V, 1, 1, 1, 1, 0, 700, 98
30693, V, 1, 1, 1, 1, 0, 700, 98
30694, V, 1, 1, 1, 1, 0, 700, 98
30695, V, 1, 1, 1, 1, 0, 700, 98
30696, V, 1, 1, 1, 1, 0, 700, 98
30697, V, 1, 1, 1, 1, 0, 700, 98
30698, V, 1, 1, 1, 1, 0, 700, 98
30699, V, 1, 1, 1, 1, 0, 700, 98
30700, V, 1, 1, 1, 1, 0, 700, 98
30701, V, 1, 1, 1, 1, 0, 700, 98
30702, V, 1, 1, 1, 1, 0, 700, 98
30703, V, 1, 1, 1, 1, 0, 700, 98
30704, V, 1, 1, 1, 1, 0, 700, 98
30705, V, 1, 1, 1, 1, 0, 700, 98
30706, V, 1, 1, 1, 1, 0, 700, 98
30707, V, 1, 1, 1, 1, 0, 700, 98
30708, V, 1, 1, 1, 1, 0, 700, 98
30709, V, 1, 1, 1, 1, 0, 700, 98
30710, V, 1, 1, 1, 1, 0, 700, 98
30711, V, 1, 1, 1, 1, 0, 700, 98
30712, V, 1, 1, 1, 1, 0, 700, 98
30713, V, 1, 1, 1, 1, 0, 700, 98
30714, V, 1, 1, 1, 1, 0, 700, 98
30715, V, 1, 1, 1, 1, 0, 700, 98
30716, V, 1, 1, 1, 1, 0, 700, 98
30717, V, 1, 1, 1, 1, 0, 700, 98
30718, V, 1, 1, 1, 1, 0, 700, 98
30720, V, 1, 1, 1, 1, 0, 700, 98
30721, V, 1, 1, 1, 1, 0, 700, 98
30722, V, 1, 1, 1, 1, 0, 700, 98
30723, V, 1, 1, 1, 1, 0, 700, 98
30724, V, 1, 1, 1, 1, 0, 700, 98
30725, V, 1, 1, 1, 1, 0, 700, 98
30726, V, 1, 1, 1, 1, 0, 700, 98
30727, V, 1, 1, 1, 1, 0, 700, 98
30728, V, 1, 1, 1, 1, 0, 700, 98
30729, V, 1, 1, 1, 1, 0, 700, 98
30730, V, 1, 1, 1, 1, 0, 700, 98
30731, V, 1, 1, 1, 1, 0, 700, 98
30732, V, 1, 1, 1, 1, 0, 700, 98
30733, V, 1, 1, 1, 1, 0, 700, 98
30734, V, 1, 1, 1, 1, 0, 700, 98
30735, V, 1, 1, 1, 1, 0, 700, 98
30736, V, 1, 1, 1, 1, 0, 700, 98
30737, V, 1, 1, 1, 1, 0, 700, 98
30738, V, 1, 1, 1, 1, 0, 700, 98
30739, V, 1, 1, 1, 1, 0, 700, 98
30740, V, 1, 1, 1, 1, 0, 700, 98
30741, V, 1, 1, 1, 1, 0, 700, 98
30742, V, 1, 1, 1, 1, 0, 700, 98
30743, V, 1, 1, 1, 1, 0, 700, 98
30744, V, 1, 1, 1, 1, 0, 700, 98
30745, V, 1, 1, 1, 1, 0, 700, 98
30746, V, 1, 1, 1, 1, 0, 700, 98
30747, V, 1, 1, 1, 1, 0, 700, 98
30748, V, 1, 1, 1, 1, 0, 700, 98
30749, V, 1, 1, 1, 1, 0, 700, 98
30750, V, 1, 1, 1, 1, 0, 700, 98
30751, V, 1, 1, 1, 1, 0, 700, 98
30752, V, 1, 1, 1, 1, 0, 700, 98
30753, V, 1, 1, 1, 1, 0, 700, 98
30754, V, 1, 1, 1, 1, 0, 700, 98
30755, V, 1, 1, 1, 1, 0, 700, 98
30756, V, 1, 1, 1, 1, 0, 700, 98
30757, V, 1, 1, 1, 1, 0, 700, 98
30758, V, 1, 1, 1, 1, 0, 700, 98
30759, V, 1, 1, 1, 1, 0, 700, 98
30760, V, 1, 1, 1, 1, 0, 700, 98
30761, V, 1, 1, 1, 1, 0, 700, 98
30763, V, 1, 1, 1, 1, 0, 700, 98
30764, V, 1, 1, 1, 1, 0, 700, 98
30765, V, 1, 1, 1, 1, 0, 700, 98
30766, V, 1, 1, 1, 1, 0, 700, 98
30767, V, 1, 1, 1, 1, 0, 700, 98
30768, V, 1, 1, 1, 1, 0, 700, 98
30769, V, 1, 1, 1, 1, 0, 700, 98
30770, V, 1, 1, 1, 1, 0, 700, 98
30771, V, 1, 1, 1, 1, 0, 700, 98
30772, V, 1, 1, 1, 1, 0, 700, 98
30773, V, 1, 1, 1, 1, 0, 700, 98
30774, V, 1, 1, 1, 1, 0, 700, 98
30775, V, 1, 1, 1, 1, 0, 700, 98
30776, V, 1, 1, 1, 1, 0, 700, 98
30777, V, 1, 1, 1, 1, 0, 700, 98
30778, V, 1, 1, 1, 1, 0, 700, 98
30779, V, 1, 1, 1, 1, 0, 700, 98
30780, V, 1, 1, 1, 1, 0, 700, 98
30781, V, 1, 1, 1, 1, 0, 700, 98
30782, V, 1, 1, 1, 1, 0, 700, 98
30783, V, 1, 1, 1, 1, 0, 700, 98
30784, V, 1, 1, 1, 1, 0, 700, 98
30785, V, 1, 1, 1, 1, 0, 700, 98
30786, V, 1, 1, 1, 1, 0, 700, 98
30787, V, 1, 1, 1, 1, 0, 700, 98
30788, V, 1, 1, 1, 1, 0, 700, 98
30789, V, 1, 1, 1, 1, 0, 700, 98
30790, V, 1, 1, 1, 1, 0, 700, 98
30791, V, 1, 1, 1, 1, 0, 700, 98
30792, V, 1, 1, 1, 1, 0, 700, 98
30793, V, 1, 1, 1, 1, 0, 700, 98
30794, V, 1, 1, 1, 1, 0, 700, 98
30795, V, 1, 1, 1, 1, 0, 700, 98
30796, V, 1, 1, 1, 1, 0, 700, 98
30797, V, 1, 1, 1, 1, 0, 700, 98
30798, V, 1, 1, 1, 1, 0, 700, 98
30799, V, 1, 1, 1, 1, 0, 700, 98
30800, V, 1, 1, 1, 1, 0, 700, 98
30801, V, 1, 1, 1, 1, 0, 700, 98
30802, V, 1, 1, 1, 1, 0, 700, 98
30803, V, 1, 1, 1, 1, 0, 700, 98
30804, V, 1, 1, 1, 1, 0, 700, 98
30806, V, 1, 1, 1, 1, 0, 700, 98
30807, V, 1, 1, 1, 1, 0, 700, 99
30808, V, 1, 1, 1, 1, 0, 700, 98
30809, V, 1, 1, 1, 1, 0, 700, 98
30810, V, 1, 1, 1, 1, 0, 700, 98
30811, V, 1, 1, 1, 1, 0, 700, 98
30812, V, 1, 1, 1, 1, 0, 700, 98
30813, V, 1, 1, 1, 1, 0, 700, 98
30814, V, 1, 1, 1, 1, 0, 700, 98
30815, V, 1, 1, 1, 1, 0, 700, 98
30816, V, 1, 1, 1, 1, 0, 700, 98
30817, V, 1, 1, 1, 1, 0, 700, 98
30818, V, 1, 1, 1, 1, 0, 700, 98
30819, V, 1, 1, 1, 1, 0, 700, 98
30820, V, 1, 1, 1, 1, 0, 700, 98
30821, V, 1, 1, 1, 1, 0, 700, 98
30822, V, 1, 1, 1, 1, 0, 700, 98
30823, V, 1, 1, 1, 1, 0, 700, 98
30824, V, 1, 1, 1, 1, 0, 700, 98
30825, V, 1, 1, 1, 1, 0, 700, 98
30826, V, 1, 1, 1, 1, 0, 700, 98
30827, V, 1, 1, 1, 1, 0, 700, 98
30828, V, 1, 1, 1, 1, 0, 700, 98
30829, V, 1, 1, 1, 1, 0, 700, 98
30830, V, 1, 1, 1, 1, 0, 700, 98
30831, V, 1, 1, 1, 1, 0, 700, 98
30832, V, 1, 1, 1, 1, 0, 700, 98
30833, V, 1, 1, 1, 1, 0, 700, 98
30834, V, 1, 1, 1, 1, 0, 700, 98
30835, V, 1, 1, 1, 1, 0, 700, 98
30836, V, 1, 1, 1, 1, 0, 700, 98
30837, V, 1, 1, 1, 1, 0, 700, 98
30838, V, 1, 1, 1, 1, 0, 700, 98
30839, V, 1, 1, 1, 1, 0, 700, 98
30840, V, 1, 1, 1, 1, 0, 700, 98
30841, V, 1, 1, 1, 1, 0, 700, 98
30842, V, 1, 1, 1, 1, 0, 700, 98
30843, V, 1, 1, 1, 1, 0, 700, 98
30844, V, 1, 1, 1, 1, 0, 700, 98
30845, V, 1, 1, 1, 1, 0, 700, 98
30846, V, 1, 1, 1, 1, 0, 700, 98
30848, V, 1, 1, 1, 1, 0, 700, 98
30849, V, 1, 1, 1, 1, 0, 700, 98
30850, V, 1, 1, 1, 1, 0, 700, 98
30851, V, 1, 1, 1, 1, 0, 700, 98
30852, V, 1, 1, 1, 1, 0, 700, 98
30853, V, 1, 1, 1, 1, 0, 700, 98
30854, V, 1, 1, 1, 1, 0, 700, 98
30855, V, 1, 1, 1, 1, 0, 700, 98
30856, V, 1, 1, 1, 1, 0, 700, 98
30857, V, 1, 1, 1, 1, 0, 700, 98
30858, V, 1, 1, 1, 1, 0, 700, 98
30859, V, 1, 1, 1, 1, 0, 700, 98
30860, V, 1, 1, 1, 1, 0, 700, 98
30861, V, 1, 1, 1, 1, 0, 700, 98
30862, V, 1, 1, 1, 1, 0, 700, 98
30863, V, 1, 1, 1, 1, 0, 700, 98
30864, V, 1, 1, 1, 1, 0, 700, 98
30865, V, 1, 1, 1, 1, 0, 700, 98
30866, V, 1, 1, 1, 1, 0, 700, 98
30867, V, 1, 1, 1, 1, 0, 700, 98
30868, V, 1, 1, 1, 1, 0, 700, 98
30869, V, 1, 1, 1, 1, 0, 700, 98
30870, V, 1, 1, 1, 1, 0, 700, 98
30871, V, 1, 1, 1, 1, 0, 700, 98
30872, V, 1, 1, 1, 1, 0, 700, 98
30873, V, 1, 1, 1, 1, 0, 700, 98
30874, V, 1, 1, 1, 1, 0, 700, 98
30875, V, 1, 1, 1, 1, 0, 700, 98
30876, V, 1, 1, 1, 1, 0, 700, 98
30877, V, 1, 1, 1, 1, 0, 700, 98
30878, V, 1, 1, 1, 1, 0, 700, 98
30879, V, 1, 1, 1, 1, 0, 700, 98
30880, V, 1, 1, 1, 1, 0, 700, 98
30881, V, 1, 1, 1, 1, 0, 700, 98
30882, V, 1, 1, 1, 1, 0, 700, 98
30883, V, 1, 1, 1, 1, 0, 700, 98
30884, V, 1, 1, 1, 1, 0, 700, 98
30885, V, 1, 1, 1, 1, 0, 700, 98
30886, V, 1, 1, 1, 1, 0, 700, 98
30887, V, 1, 1, 1, 1, 0, 700, 98
30888, V, 1, 1, 1, 1, 0, 700, 98
30889, V, 1, 1, 1, 1, 0, 700, 98
30891, V, 1, 1, 1, 1, 0, 700, 98
30892, V, 1, 1, 1, 1, 0, 700, 98
30893, V, 1, 1, 1, 1, 0, 700, 98
30894, V, 1, 1, 1, 1, 0, 700, 98
30895, V, 1, 1, 1, 1, 0, 700, 98
30896, V, 1, 1, 1, 1, 0, 700, 98
30897, V, 1, 1, 1, 1, 0, 700, 98
30898, V, 1, 1, 1, 1, 0, 700, 98
30899, V, 1, 1, 1, 1, 0, 700, 98
30900, V, 1, 1, 1, 1, 0, 700, 98
30901, V, 1, 1, 1, 1, 0, 700, 98
30902, V, 1, 1, 1, 1, 0, 700, 98
30903, V, 1, 1, 1, 1, 0, 700, 98
30904, V, 1, 1, 1, 1, 0, 700, 98
30905, V, 1, 1, 1, 1, 0, 700, 98
30906, V, 1, 1, 1, 1, 0, 700, 98
30907, V, 1, 1, 1, 1, 0, 700, 98
30908, V, 1, 1, 1, 1, 0, 700, 98
30909, V, 1, 1, 1, 1, 0, 700, 98
30910, V, 1, 1, 1, 1, 0, 700, 98
30911, V, 1, 1, 1, 1, 0, 700, 98
30912, V, 1, 1, 1, 1, 0, 700, 98
30913, V, 1, 1, 1, 1, 0, 700, 98
30914, V, 1, 1, 1, 1, 0, 700, 98
30915, V, 1, 1, 1, 1, 0, 700, 98
30916, V, 1, 1, 1, 1, 0, 700, 98
30917, V, 1, 1, 1, 1, 0, 700, 98
30918, V, 1, 1, 1, 1, 0, 700, 98
30919, V, 1, 1, 1, 1, 0, 700, 98
30920, V, 1, 1, 1, 1, 0, 700, 98
30921, V, 1, 1, 1, 1, 0, 700, 98
30922, V, 1, 1, 1, 1, 0, 700, 98
30923, V, 1, 1, 1, 1, 0, 700, 98
30924, V, 1, 1, 1, 1, 0, 700, 98
30925, V, 1, 1, 1, 1, 0, 700, 98
30926, V, 1, 1, 1, 1, 0, 700, 98
30927, V, 1, 1, 1, 1, 0, 700, 98
30928, V, 1, 1, 1, 1, 0, 700, 98
30929, V, 1, 1, 1, 1, 0, 700, 98
30930, V, 1, 1, 1, 1, 0, 700, 98
30931, V, 1, 1, 1, 1, 0, 700, 98
30932, V, 1, 1, 1, 1, 0, 700, 98
30934, V, 1, 1, 1, 1, 0, 700, 98
30935, V, 1, 1, 1, 1, 0, 700, 98
30936, V, 1, 1, 1, 1, 0, 700, 98
30937, V, 1, 1, 1, 1, 0, 700, 98
30938, V, 1, 1, 1, 1, 0, 700, 98
30939, V, 1, 1, 1, 1, 0, 700, 98
30940, V, 1, 1, 1, 1, 0, 700, 98
30941, V, 1, 1, 1, 1, 0, 700, 98
30942, V, 1, 1, 1, 1, 0, 700, 98
30943, V, 1, 1, 1, 1, 0, 700, 98
30944, V, 1, 1, 1, 1, 0, 700, 98
30945, V, 1, 1, 1, 1, 0, 700, 98
30946, V, 1, 1, 1, 1, 0, 700, 98
30947, V, 1, 1, 1, 1, 0, 700, 98
30948, V, 1, 1, 1, 1, 0, 700, 98
30949, V, 1, 1, 1, 1, 0, 700, 98
30950, V, 1, 1, 1, 1, 0, 700, 98
30951, V, 1, 1, 1, 1, 0, 700, 98
30952, V, 1, 1, 1, 1, 0, 700, 98
30953, V, 1, 1, 1, 1, 0, 700, 98
30954, V, 1, 1, 1, 1, 0, 700, 98
30955, V, 1, 1, 1, 1, 0, 700, 98
30956, V, 1, 1, 1, 1, 0, 700, 98
30957, V, 1, 1, 1, 1, 0, 700, 98
30958, V, 1, 1, 1, 1, 0, 700, 98
30959, V, 1, 1, 1, 1, 0, 700, 98
30960, V, 1, 1, 1, 1, 0, 700, 98
30961, V, 1, 1, 1, 1, 0, 700, 98
30962, V, 1, 1, 1, 1, 0, 700, 98
30963, V, 1, 1, 1, 1, 0, 700, 98
30964, V, 1, 1, 1, 1, 0, 700, 98
30965, V, 1, 1, 1, 1, 0, 700, 98
30966, V, 1, 1, 1, 1, 0, 700, 98
30967, V, 1, 1, 1, 1, 0, 700, 98
30968, V, 1, 1, 1, 1, 0, 700, 98
30969, V, 1, 1, 1, 1, 0, 700, 98
30970, V, 1, 1, 1, 1, 0, 700, 98
30971, V, 1, 1, 1, 1, 0, 700, 98
30972, V, 1, 1, 1, 1, 0, 700, 98
30973, V, 1, 1, 1, 1, 0, 700, 98
30974, V, 1, 1, 1, 1, 0, 700, 98
30976, V, 1, 1, 1, 1, 0, 700, 98
30977, V, 1, 1, 1, 1, 0, 700, 98
30978, V, 1, 1, 1, 1, 0, 700, 98
30979, V, 1, 1, 1, 1, 0, 700, 98
30980, V, 1, 1, 1, 1, 0, 700, 98
30981, V, 1, 1, 1, 1, 0, 700, 98
30982, V, 1, 1, 1, 1, 0, 700, 98
30983, V, 1, 1, 1, 1, 0, 700, 98
30984, V, 1, 1, 1, 1, 0, 700, 98
30985, V, 1, 1, 1, 1, 0, 700, 98
30986, V, 1, 1, 1, 1, 0, 700, 98
30987, V, 1, 1, 1, 1, 0, 700, 98
30988, V, 1, 1, 1, 1, 0, 700, 98
30989, V, 1, 1, 1, 1, 0, 700, 98
30990, V, 1, 1, 1, 1, 0, 700, 98
30991, V, 1, 1, 1, 1, 0, 700, 98
30992, V, 1, 1, 1, 1, 0, 700, 98
30993, V, 1, 1, 1, 1, 0, 700, 98
30994, V, 1, 1, 1, 1, 0, 700, 98
30995, V, 1, 1, 1, 1, 0, 700, 98
30996, V, 1, 1, 1, 1, 0, 700, 98
30997, V, 1, 1, 1, 1, 0, 700, 98
30998, V, 1, 1, 1, 1, 0, 700, 98
30999, V, 1, 1, 1, 1, 0, 700, 98
31000, V, 1, 1, 1, 1, 0, 700, 98
31001, V, 1, 1, 1, 1, 0, 700, 98
31002, V, 1, 1, 1, 1, 0, 700, 98
31003, V, 1, 1, 1, 1, 0, 700, 98
31004, V, 1, 1, 1, 1, 0, 700, 98
31005, V, 1, 1, 1, 1, 0, 700, 98
31006, V, 1, 1, 1, 1, 0, 700, 98
31007, V, 1, 1, 1, 1, 0, 700, 98
31008, V, 1, 1, 1, 1, 0, 700, 98
31009, V, 1, 1, 1, 1, 0, 700, 98
31010, V, 1, 1, 1, 1, 0, 700, 98
31011, V, 1, 1, 1, 1, 0, 700, 98
31012, V, 1, 1, 1, 1, 0, 700, 98
31013, V, 1, 1, 1, 1, 0, 700, 98
31014, V, 1, 1, 1, 1, 0, 700, 98
31015, V, 1, 1, 1, 1, 0, 700, 98
31016, V, 1, 1, 1, 1, 0, 700, 98
31017, V, 1, 1, 1, 1, 0, 700, 98
31019, V, 1, 1, 1, 1, 0, 700, 98
31020, V, 1, 1, 1, 1, 0, 700, 98
31021, V, 1, 1, 1, 1, 0, 700, 98
31022, V, 1, 1, 1, 1, 0, 700, 98
31023, V, 1, 1, 1, 1, 0, 700, 98
31024, V, 1, 1, 1, 1, 0, 700, 99
31025, V, 1, 1, 1, 1, 0, 700, 98
31026, V, 1, 1, 1, 1, 0, 700, 98
31027, V, 1, 1, 1, 1, 0, 700, 98
31028, V, 1, 1, 1, 1, 0, 700, 99
31029, V, 1, 1, 1, 1, 0, 700, 98
31030, V, 1, 1, 1, 1, 0, 700, 99
31031, V, 1, 1, 1, 1, 0, 700, 98
31032, V, 1, 1, 1, 1, 0, 700, 98
31033, V, 1, 1, 1, 1, 0, 700, 99
31034, V, 1, 1, 1, 1, 0, 700, 98
31035, V, 1, 1, 1, 1, 0, 700, 98
31036, V, 1, 1, 1, 1, 0, 700, 99
31037, V, 1, 1, 1, 1, 0, 700, 98
31038, V, 1, 1, 1, 1, 0, 700, 98
31039, V, 1, 1, 1, 1, 0, 700, 98
31040, V, 1, 1, 1, 1, 0, 700, 99
31041, V, 1, 1, 1, 1, 0, 700, 99
31042, V, 1, 1, 1, 1, 0, 700, 99
31043, V, 1, 1, 1, 1, 0, 700, 99
31044, V, 1, 1, 1, 1, 0, 700, 98
31045, V, 1, 1, 1, 1, 0, 700, 99
31046, V, 1, 1, 1, 1, 0, 700, 98
31047, V, 1, 1, 1, 1, 0, 700, 98
31048, V, 1, 1, 1, 1, 0, 700, 98
31049, V, 1, 1, 1, 1, 0, 700, 99
31050, V, 1, 1, 1, 1, 0, 700, 99
31051, V, 1, 1, 1, 1, 0, 700, 98
31052, V, 1, 1, 1, 1, 0, 700, 99
31053, V, 1, 1, 1, 1, 0, 700, 99
31054, V, 1, 1, 1, 1, 0, 700, 98
31055, V, 1, 1, 1, 1, 0, 700, 98
31056, V, 1, 1, 1, 1, 0, 700, 98
31057, V, 1, 1, 1, 1, 0, 700, 98
31058, V, 1, 1, 1, 1, 0, 700, 98
31059, V, 1, 1, 1, 1, 0, 700, 98
31060, V, 1, 1, 1, 1, 0, 700, 98
31062, V, 1, 1, 1, 1, 0, 700, 98
31063, V, 1, 1, 1, 1, 0, 700, 98
31064, V, 1, 1, 1, 1, 0, 700, 98
31065, V, 1, 1, 1, 1, 0, 700, 98
31066, V, 1, 1, 1, 1, 0, 700, 98
31067, V, 1, 1, 1, 1, 0, 700, 98
31068, V, 1, 1, 1, 1, 0, 700, 98
31069, V, 1, 1, 1, 1, 0, 700, 98
31070, V, 1, 1, 1, 1, 0, 700, 98
31071, V, 1, 1, 1, 1, 0, 700, 98
31072, V, 1, 1, 1, 1, 0, 700, 98
31073, V, 1, 1, 1, 1, 0, 700, 98
31074, V, 1, 1, 1, 1, 0, 700, 98
31075, V, 1, 1, 1, 1, 0, 700, 98
31076, V, 1, 1, 1, 1, 0, 700, 98
31077, V, 1, 1, 1, 1, 0, 700, 98
31078, V, 1, 1, 1, 1, 0, 700, 98
31079, V, 1, 1, 1, 1, 0, 700, 98
31080, V, 1, 1, 1, 1, 0, 700, 98
31081, V, 1, 1, 1, 1, 0, 700, 98
31082, V, 1, 1, 1, 1, 0, 700, 98
31083, V, 1, 1, 1, 1, 0, 700, 98
31084, V, 1, 1, 1, 1, 0, 700, 98
31085, V, 1, 1, 1, 1, 0, 700, 98
31086, V, 1, 1, 1, 1, 0, 700, 98
31087, V, 1, 1, 1, 1, 0, 700, 98
31088, V, 1, 1, 1, 1, 0, 700, 98
31089, V, 1, 1, 1, 1, 0, 700, 98
31090, V, 1, 1, 1, 1, 0, 700, 98
31091, V, 1, 1, 1, 1, 0, 700, 98
31092, V, 1, 1, 1, 1, 0, 700, 98
31093, V, 1, 1, 1, 1, 0, 700, 98
31094, V, 1, 1, 1, 1, 0, 700, 98
31095, V, 1, 1, 1, 1, 0, 700, 98
31096, V, 1, 1, 1, 1, 0, 700, 98
31097, V, 1, 1, 1, 1, 0, 700, 98
31098, V, 1, 1, 1, 1, 0, 700, 98
31099, V, 1, 1, 1, 1, 0, 700, 98
31100, V, 1, 1, 1, 1, 0, 700, 98
31101, V, 1, 1, 1, 1, 0, 700, 98
31102, V, 1, 1, 1, 1, 0, 700, 98
31104, V, 1, 1, 1, 1, 0, 700, 98
31105, V, 1, 1, 1, 1, 0, 700, 98
31106, V, 1, 1, 1, 1, 0, 700, 98
31107, V, 1, 1, 1, 1, 0, 700, 98
31108, V, 1, 1, 1, 1, 0, 700, 98
31109, V, 1, 1, 1, 1, 0, 700, 98
31110, V, 1, 1, 1, 1, 0, 700, 98
31111, V, 1, 1, 1, 1, 0, 700, 98
31112, V, 1, 1, 1, 1, 0, 700, 98
31113, V, 1, 1, 1, 1, 0, 700, 98
31114, V, 1, 1, 1, 1, 0, 700, 98
31115, V, 1, 1, 1, 1, 0, 700, 98
31116, V, 1, 1, 1, 1, 0, 700, 98
31117, V, 1, 1, 1, 1, 0, 700, 98
31118, V, 1, 1, 1, 1, 0, 700, 98
31119, V, 1, 1, 1, 1, 0, 700, 98
31120, V, 1, 1, 1, 1, 0, 700, 98
31121, V, 1, 1, 1, 1, 0, 700, 98
31122, V, 1, 1, 1, 1, 0, 700, 98
31123, V, 1, 1, 1, 1, 0, 700, 98
31124, V, 1, 1, 1, 1, 0, 700, 98
31125, V, 1, 1, 1, 1, 0, 700, 98
31126, V, 1, 1, 1, 1, 0, 700, 98
31127, V, 1, 1, 1, 1, 0, 700, 98
31128, V, 1, 1, 1, 1, 0, 700, 98
31129, V, 1, 1, 1, 1, 0, 700, 98
31130, V, 1, 1, 1, 1, 0, 700, 98
31131, V, 1, 1, 1, 1, 0, 700, 98
31132, V, 1, 1, 1, 1, 0, 700, 98
31133, V, 1, 1, 1, 1, 0, 700, 98
31134, V, 1, 1, 1, 1, 0, 700, 98
31135, V, 1, 1, 1, 1, 0, 700, 98
31136, V, 1, 1, 1, 1, 0, 700, 98
31137, V, 1, 1, 1, 1, 0, 700, 98
31138, V, 1, 1, 1, 1, 0, 700, 98
31139, V, 1, 1, 1, 1, 0, 700, 98
31140, V, 1, 1, 1, 1, 0, 700, 98
31141, V, 1, 1, 1, 1, 0, 700, 98
31142, V, 1, 1, 1, 1, 0, 700, 98
31143, V, 1, 1, 1, 1, 0, 700, 98
31144, V, 1, 1, 1, 1, 0, 700, 98
31145, V, 1, 1, 1, 1, 0, 700, 98
31147, V, 1, 1, 1, 1, 0, 700, 98
31148, V, 1, 1, 1, 1, 0, 700, 98
31149, V, 1, 1, 1, 1, 0, 700, 98
31150, V, 1, 1, 1, 1, 0, 700, 98
31151, V, 1, 1, 1, 1, 0, 700, 98
31152, V, 1, 1, 1, 1, 0, 700, 98
31153, V, 1, 1, 1, 1, 0, 700, 98
31154, V, 1, 1, 1, 1, 0, 700, 98
31155, V, 1, 1, 1, 1, 0, 700, 98
31156, V, 1, 1, 1, 1, 0, 700, 98
31157, V, 1, 1, 1, 1, 0, 700, 98
31158, V, 1, 1, 1, 1, 0, 700, 98
31159, V, 1, 1, 1, 1, 0, 700, 98
31160, V, 1, 1, 1, 1, 0, 700, 98
31161, V, 1, 1, 1, 1, 0, 700, 98
31162, V, 1, 1, 1, 1, 0, 700, 98
31163, V, 1, 1, 1, 1, 0, 700, 98
31164, V, 1, 1, 1, 1, 0, 700, 98
31165, V, 1, 1, 1, 1, 0, 700, 98
31166, V, 1, 1, 1, 1, 0, 700, 98
31167, V, 1, 1, 1, 1, 0, 700, 98
31168, V, 1, 1, 1, 1, 0, 700, 98
31169, V, 1, 1, 1, 1, 0, 700, 98
31170, V, 1, 1, 1, 1, 0, 700, 98
31171, V, 1, 1, 1, 1, 0, 700, 98
31172, V, 1, 1, 1, 1, 0, 700, 98
31173, V, 1, 1, 1, 1, 0, 700, 98
31174, V, 1, 1, 1, 1, 0, 700, 98
31175, V, 1, 1, 1, 1, 0, 700, 98
31176, V, 1, 1, 1, 1, 0, 700, 98
31177, V, 1, 1, 1, 1, 0, 700, 98
31178, V, 1, 1, 1, 1, 0, 700, 98
31179, V, 1, 1, 1, 1, 0, 700, 98
31180, V, 1, 1, 1, 1, 0, 700, 98
31181, V, 1, 1, 1, 1, 0, 700, 98
31182, V, 1, 1, 1, 1, 0, 700, 98
31183, V, 1, 1, 1, 1, 0, 700, 98
31184, V, 1, 1, 1, 1, 0, 700, 98
31185, V, 1, 1, 1, 1, 0, 700, 98
31186, V, 1, 1, 1, 1, 0, 700, 98
31187, V, 1, 1, 1, 1, 0, 700, 98
31188, V, 1, 1, 1, 1, 0, 700, 98
31190, V, 1, 1, 1, 1, 0, 700, 98
31191, V, 1, 1, 1, 1, 0, 700, 98
31192, V, 1, 1, 1, 1, 0, 700, 98
31193, V, 1, 1, 1, 1, 0, 700, 98
31194, V, 1, 1, 1, 1, 0, 700, 98
31195, V, 1, 1, 1, 1, 0, 700, 98
31196, V, 1, 1, 1, 1, 0, 700, 98
31197, V, 1, 1, 1, 1, 0, 700, 98
31198, V, 1, 1, 1, 1, 0, 700, 98
31199, V, 1, 1, 1, 1, 0, 700, 98
31200, V, 1, 1, 1, 1, 0, 700, 98
31201, V, 1, 1, 1, 1, 0, 700, 98
31202, V, 1, 1, 1, 1, 0, 700, 98
31203, V, 1, 1, 1, 1, 0, 700, 98
31204, V, 1, 1, 1, 1, 0, 700, 98
31205, V, 1, 1, 1, 1, 0, 700, 98
31206, V, 1, 1, 1, 1, 0, 700, 98
31207, V, 1, 1, 1, 1, 0, 700, 98
31208, V, 1, 1, 1, 1, 0, 700, 98
31209, V, 1, 1, 1, 1, 0, 700, 98
31210, V, 1, 1, 1, 1, 0, 700, 98
31211, V, 1, 1, 1, 1, 0, 700, 98
31212, V, 1, 1, 1, 1, 0, 700, 98
31213, V, 1, 1, 1, 1, 0, 700, 98
31214, V, 1, 1, 1, 1, 0, 700, 98
31215, V, 1, 1, 1, 1, 0, 700, 98
31216, V, 1, 1, 1, 1, 0, 700, 98
31217, V, 1, 1, 1, 1, 0, 700, 98
31218, V, 1, 1, 1, 1, 0, 700, 98
31219, V, 1, 1, 1, 1, 0, 700, 98
31220, V, 1, 1, 1, 1, 0, 700, 98
31221, V, 1, 1, 1, 1, 0, 700, 98
31222, V, 1, 1, 1, 1, 0, 700, 98
31223, V, 1, 1, 1, 1, 0, 700, 98
31224, V, 1, 1, 1, 1, 0, 700, 98
31225, V, 1, 1, 1, 1, 0, 700, 98
31226, V, 1, 1, 1, 1, 0, 700, 98
31227, V, 1, 1, 1, 1, 0, 700, 98
31228, V, 1, 1, 1, 1, 0, 700, 98
31229, V, 1, 1, 1, 1, 0, 700, 98
31230, V, 1, 1, 1, 1, 0, 700, 98
31232, V, 1, 1, 1, 1, 0, 700, 98
31233, V, 1, 1, 1, 1, 0, 700, 98
31234, V, 1, 1, 1, 1, 0, 700, 98
31235, V, 1, 1, 1, 1, 0, 700, 98
31236, V, 1, 1, 1, 1, 0, 700, 98
31237, V, 1, 1, 1, 1, 0, 700, 98
31238, V, 1, 1, 1, 1, 0, 700, 98
31239, V, 1, 1, 1, 1, 0, 700, 98
31240, V, 1, 1, 1, 1, 0, 700, 98
31241, V, 1, 1, 1, 1, 0, 700, 98
31242, V, 1, 1, 1, 1, 0, 700, 98
31243, V, 1, 1, 1, 1, 0, 700, 98
31244, V, 1, 1, 1, 1, 0, 700, 98
31245, V, 1, 1, 1, 1, 0, 700, 98
31246, V, 1, 1, 1, 1, 0, 700, 98
31247, V, 1, 1, 1, 1, 0, 700, 98
31248, V, 1, 1, 1, 1, 0, 700, 98
31249, V, 1, 1, 1, 1, 0, 700, 98
31250, V, 1, 1, 1, 1, 0, 700, 98
31251, V, 1, 1, 1, 1, 0, 700, 98
31252, V, 1, 1, 1, 1, 0, 700, 98
31253, V, 1, 1, 1, 1, 0, 700, 98
31254, V, 1, 1, 1, 1, 0, 700, 98
31255, V, 1, 1, 1, 1, 0, 700, 98
31256, V, 1, 1, 1, 1, 0, 700, 98
31257, V, 1, 1, 1, 1, 0, 700, 98
31258, V, 1, 1, 1, 1, 0, 700, 98
31259, V, 1, 1, 1, 1, 0, 700, 98
31260, V, 1, 1, 1, 1, 0, 700, 98
31261, V, 1, 1, 1, 1, 0, 700, 98
31262, V, 1, 1, 1, 1, 0, 700, 98
31263, V, 1, 1, 1, 1, 0, 700, 98
31264, V, 1, 1, 1, 1, 0, 700, 98
31265, V, 1, 1, 1, 1, 0, 700, 98
31266, V, 1, 1, 1, 1, 0, 700, 98
31267, V, 1, 1, 1, 1, 0, 700, 98
31268, V, 1, 1, 1, 1, 0, 700, 98
31269, V, 1, 1, 1, 1, 0, 700, 98
31270, V, 1, 1, 1, 1, 0, 700, 98
31271, V, 1, 1, 1, 1, 0, 700, 98
31272, V, 1, 1, 1, 1, 0, 700, 98
31273, V, 1, 1, 1, 1, 0, 700, 98
31275, V, 1, 1, 1, 1, 0, 700, 98
31276, V, 1, 1, 1, 1, 0, 700, 98
31277, V, 1, 1, 1, 1, 0, 700, 98
31278, V, 1, 1, 1, 1, 0, 700, 98
31279, V, 1, 1, 1, 1, 0, 700, 98
31280, V, 1, 1, 1, 1, 0, 700, 98
31281, V, 1, 1, 1, 1, 0, 700, 98
31282, V, 1, 1, 1, 1, 0, 700, 98
31283, V, 1, 1, 1, 1, 0, 700, 98
31284, V, 1, 1, 1, 1, 0, 700, 98
31285, V, 1, 1, 1, 1, 0, 700, 98
31286, V, 1, 1, 1, 1, 0, 700, 98
31287, V, 1, 1, 1, 1, 0, 700, 98
31288, V, 1, 1, 1, 1, 0, 700, 98
31289, V, 1, 1, 1, 1, 0, 700, 98
31290, V, 1, 1, 1, 1, 0, 700, 98
31291, V, 1, 1, 1, 1, 0, 700, 98
31292, V, 1, 1, 1, 1, 0, 700, 98
31293, V, 1, 1, 1, 1, 0, 700, 98
31294, V, 1, 1, 1, 1, 0, 700, 98
31295, V, 1, 1, 1, 1, 0, 700, 98
31296, V, 1, 1, 1, 1, 0, 700, 98
31297, V, 1, 1, 1, 1, 0, 700, 98
31298, V, 1, 1, 1, 1, 0, 700, 98
31299, V, 1, 1, 1, 1, 0, 700, 98
31300, V, 1, 1, 1, 1, 0, 700, 98
31301, V, 1, 1, 1, 1, 0, 700, 98
31302, V, 1, 1, 1, 1, 0, 700, 98
31303, V, 1, 1, 1, 1, 0, 700, 98
31304, V, 1, 1, 1, 1, 0, 700, 98
31305, V, 1, 1, 1, 1, 0, 700, 98
31306, V, 1, 1, 1, 1, 0, 700, 98
31307, V, 1, 1, 1, 1, 0, 700, 98
31308, V, 1, 1, 1, 1, 0, 700, 98
31309, V, 1, 1, 1, 1, 0, 700, 98
31310, V, 1, 1, 1, 1, 0, 700, 98
31311, V, 1, 1, 1, 1, 0, 700, 98
31312, V, 1, 1, 1, 1, 0, 700, 98
31313, V, 1, 1, 1, 1, 0, 700, 98
31314, V, 1, 1, 1, 1, 0, 700, 98
31315, V, 1, 1, 1, 1, 0, 700, 98
31316, V, 1, 1, 1, 1, 0, 700, 98
31318, V, 1, 1, 1, 1, 0, 700, 98
31319, V, 1, 1, 1, 1, 0, 700, 98
31320, V, 1, 1, 1, 1, 0, 700, 98
31321, V, 1, 1, 1, 1, 0, 700, 98
31322, V, 1, 1, 1, 1, 0, 700, 98
31323, V, 1, 1, 1, 1, 0, 700, 98
31324, V, 1, 1, 1, 1, 0, 700, 98
31325, V, 1, 1, 1, 1, 0, 700, 98
31326, V, 1, 1, 1, 1, 0, 700, 98
31327, V, 1, 1, 1, 1, 0, 700, 98
31328, V, 1, 1, 1, 1, 0, 700, 98
31329, V, 1, 1, 1, 1, 0, 700, 98
31330, V, 1, 1, 1, 1, 0, 700, 98
31331, V, 1, 1, 1, 1, 0, 700, 98
31332, V, 1, 1, 1, 1, 0, 700, 98
31333, V, 1, 1, 1, 1, 0, 700, 98
31334, V, 1, 1, 1, 1, 0, 700, 98
31335, V, 1, 1, 1, 1, 0, 700, 98
31336, V, 1, 1, 1, 1, 0, 700, 98
31337, V, 1, 1, 1, 1, 0, 700, 98
31338, V, 1, 1, 1, 1, 0, 700, 98
31339, V, 1, 1, 1, 1, 0, 700, 98
31340, V, 1, 1, 1, 1, 0, 700, 98
31341, V, 1, 1, 1, 1, 0, 700, 98
31342, V, 1, 1, 1, 1, 0, 700, 98
31343, V, 1, 1, 1, 1, 0, 700, 98
31344, V, 1, 1, 1, 1, 0, 700, 98
31345, V, 1, 1, 1, 1, 0, 700, 98
31346, V, 1, 1, 1, 1, 0, 700, 98
31347, V, 1, 1, 1, 1, 0, 700, 98
31348, V, 1, 1, 1, 1, 0, 700, 98
31349, V, 1, 1, 1, 1, 0, 700, 98
31350, V, 1, 1, 1, 1, 0, 700, 98
31351, V, 1, 1, 1, 1, 0, 700, 98
31352, V, 1, 1, 1, 1, 0, 700, 98
31353, V, 1, 1, 1, 1, 0, 700, 98
31354, V, 1, 1, 1, 1, 0, 700, 98
31355, V, 1, 1, 1, 1, 0, 700, 98
31356, V, 1, 1, 1, 1, 0, 700, 98
31357, V, 1, 1, 1, 1, 0, 700, 98
31358, V, 1, 1, 1, 1, 0, 700, 98
31360, V, 1, 1, 1, 1, 0, 700, 98
31361, V, 1, 1, 1, 1, 0, 700, 98
31362, V, 1, 1, 1, 1, 0, 700, 98
31363, V, 1, 1, 1, 1, 0, 700, 98
31364, V, 1, 1, 1, 1, 0, 700, 98
31365, V, 1, 1, 1, 1, 0, 700, 98
31366, V, 1, 1, 1, 1, 0, 700, 98
31367, V, 1, 1, 1, 1, 0, 700, 98
31368, V, 1, 1, 1, 1, 0, 700, 98
31369, V, 1, 1, 1, 1, 0, 700, 98
31370, V, 1, 1, 1, 1, 0, 700, 98
31371, V, 1, 1, 1, 1, 0, 700, 98
31372, V, 1, 1, 1, 1, 0, 700, 98
31373, V, 1, 1, 1, 1, 0, 700, 98
31374, V, 1, 1, 1, 1, 0, 700, 98
31375, V, 1, 1, 1, 1, 0, 700, 98
31376, V, 1, 1, 1, 1, 0, 700, 98
31377, V, 1, 1, 1, 1, 0, 700, 98
31378, V, 1, 1, 1, 1, 0, 700, 98
31379, V, 1, 1, 1, 1, 0, 700, 98
31380, V, 1, 1, 1, 1, 0, 700, 98
31381, V, 1, 1, 1, 1, 0, 700, 98
31382, V, 1, 1, 1, 1, 0, 700, 98
31383, V, 1, 1, 1, 1, 0, 700, 98
31384, V, 1, 1, 1, 1, 0, 700, 98
31385, V, 1, 1, 1, 1, 0, 700, 98
31386, V, 1, 1, 1, 1, 0, 700, 98
31387, V, 1, 1, 1, 1, 0, 700, 98
31388, V, 1, 1, 1, 1, 0, 700, 98
31389, V, 1, 1, 1, 1, 0, 700, 98
31390, V, 1, 1, 1, 1, 0, 700, 98
31391, V, 1, 1, 1, 1, 0, 700, 98
31392, V, 1, 1, 1, 1, 0, 700, 98
31393, V, 1, 1, 1, 1, 0, 700, 98
31394, V, 1, 1, 1, 1, 0, 700, 98
31395, V, 1, 1, 1, 1, 0, 700, 98
31396, V, 1, 1, 1, 1, 0, 700, 98
31397, V, 1, 1, 1, 1, 0, 700, 98
31398, V, 1, 1, 1, 1, 0, 700, 98
31399, V, 1, 1, 1, 1, 0, 700, 98
31400, V, 1, 1, 1, 1, 0, 700, 98
31401, V, 1, 1, 1, 1, 0, 700, 98
31403, V, 1, 1, 1, 1, 0, 700, 98
31404, V, 1, 1, 1, 1, 0, 700, 98
31405, V, 1, 1, 1, 1, 0, 700, 98
31406, V, 1, 1, 1, 1, 0, 700, 98
31407, V, 1, 1, 1, 1, 0, 700, 98
31408, V, 1, 1, 1, 1, 0, 700, 98
31409, V, 1, 1, 1, 1, 0, 700, 98
31410, V, 1, 1, 1, 1, 0, 700, 98
31411, V, 1, 1, 1, 1, 0, 700, 98
31412, V, 1, 1, 1, 1, 0, 700, 98
31413, V, 1, 1, 1, 1, 0, 700, 98
31414, V, 1, 1, 1, 1, 0, 700, 98
31415, V, 1, 1, 1, 1, 0, 700, 98
31416, V, 1, 1, 1, 1, 0, 700, 98
31417, V, 1, 1, 1, 1, 0, 700, 98
31418, V, 1, 1, 1, 1, 0, 700, 98
31419, V, 1, 1, 1, 1, 0, 700, 98
31420, V, 1, 1, 1, 1, 0, 700, 98
31421, V, 1, 1, 1, 1, 0, 700, 98
31422, V, 1, 1, 1, 1, 0, 700, 98
31423, V, 1, 1, 1, 1, 0, 700, 98
31424, V, 1, 1, 1, 1, 0, 700, 98
31425, V, 1, 1, 1, 1, 0, 700, 98
31426, V, 1, 1, 1, 1, 0, 700, 98
31427, V, 1, 1, 1, 1, 0, 700, 98
31428, V, 1, 1, 1, 1, 0, 700, 98
31429, V, 1, 1, 1, 1, 0, 700, 98
31430, V, 1, 1, 1, 1, 0, 700, 98
31431, V, 1, 1, 1, 1, 0, 700, 98
31432, V, 1, 1, 1, 1, 0, 700, 98
31433, V, 1, 1, 1, 1, 0, 700, 98
31434, V, 1, 1, 1, 1, 0, 700, 98
31435, V, 1, 1, 1, 1, 0, 700, 98
31436, V, 1, 1, 1, 1, 0, 700, 98
31437, V, 1, 1, 1, 1, 0, 700, 98
31438, V, 1, 1, 1, 1, 0, 700, 98
31439, V, 1, 1, 1, 1, 0, 700, 98
31440, V, 1, 1, 1, 1, 0, 700, 98
31441, V, 1, 1, 1, 1, 0, 700, 98
31442, V, 1, 1, 1, 1, 0, 700, 98
31443, V, 1, 1, 1, 1, 0, 700, 98
31444, V, 1, 1, 1, 1, 0, 700, 98
31446, V, 1, 1, 1, 1, 0, 700, 98
31447, V, 1, 1, 1, 1, 0, 700, 98
31448, V, 1, 1, 1, 1, 0, 700, 98
31449, V, 1, 1, 1, 1, 0, 700, 98
31450, V, 1, 1, 1, 1, 0, 700, 98
31451, V, 1, 1, 1, 1, 0, 700, 98
31452, V, 1, 1, 1, 1, 0, 700, 98
31453, V, 1, 1, 1, 1, 0, 700, 98
31454, V, 1, 1, 1, 1, 0, 700, 98
31455, V, 1, 1, 1, 1, 0, 700, 98
31456, V, 1, 1, 1, 1, 0, 700, 98
31457, V, 1, 1, 1, 1, 0, 700, 98
31458, V, 1, 1, 1, 1, 0, 700, 98
31459, V, 1, 1, 1, 1, 0, 700, 98
31460, V, 1, 1, 1, 1, 0, 700, 98
31461, V, 1, 1, 1, 1, 0, 700, 98
31462, V, 1, 1, 1, 1, 0, 700, 98
31463, V, 1, 1, 1, 1, 0, 700, 98
31464, V, 1, 1, 1, 1, 0, 700, 98
31465, V, 1, 1, 1, 1, 0, 700, 98
31466, V, 1, 1, 1, 1, 0, 700, 98
31467, V, 1, 1, 1, 1, 0, 700, 98
31468, V, 1, 1, 1, 1, 0, 700, 98
31469, V, 1, 1, 1, 1, 0, 700, 98
31470, V, 1, 1, 1, 1, 0, 700, 98
31471, V, 1, 1, 1, 1, 0, 700, 98
31472, V, 1, 1, 1, 1, 0, 700, 98
31473, V, 1, 1, 1, 1, 0, 700, 98
31474, V, 1, 1, 1, 1, 0, 700, 98
31475, V, 1, 1, 1, 1, 0, 700, 98
31476, V, 1, 1, 1, 1, 0, 700, 98
31477, V, 1, 1, 1, 1, 0, 700, 98
31478, V, 1, 1, 1, 1, 0, 700, 98
31479, V, 1, 1, 1, 1, 0, 700, 98
31480, V, 1, 1, 1, 1, 0, 700, 98
31481, V, 1, 1, 1, 1, 0, 700, 98
31482, V, 1, 1, 1, 1, 0, 700, 98
31483, V, 1, 1, 1, 1, 0, 700, 98
31484, V, 1, 1, 1, 1, 0, 700, 98
31485, V, 1, 1, 1, 1, 0, 700, 98
31486, V, 1, 1, 1, 1, 0, 700, 98
31488, V, 1, 1, 1, 1, 0, 700, 98
31489, V, 1, 1, 1, 1, 0, 700, 98
31490, V, 1, 1, 1, 1, 0, 700, 98
31491, V, 1, 1, 1, 1, 0, 700, 98
31492, V, 1, 1, 1, 1, 0, 700, 98
31493, V, 1, 1, 1, 1, 0, 700, 98
31494, V, 1, 1, 1, 1, 0, 700, 98
31495, V, 1, 1, 1, 1, 0, 700, 98
31496, V, 1, 1, 1, 1, 0, 700, 98
31497, V, 1, 1, 1, 1, 0, 700, 98
31498, V, 1, 1, 1, 1, 0, 700, 98
31499, V, 1, 1, 1, 1, 0, 700, 98
31500, V, 1, 1, 1, 1, 0, 700, 98
31501, V, 1, 1, 1, 1, 0, 700, 98
31502, V, 1, 1, 1, 1, 0, 700, 98
31503, V, 1, 1, 1, 1, 0, 700, 98
31504, V, 1, 1, 1, 1, 0, 700, 98
31505, V, 1, 1, 1, 1, 0, 700, 98
31506, V, 1, 1, 1, 1, 0, 700, 98
31507, V, 1, 1, 1, 1, 0, 700, 98
31508, V, 1, 1, 1, 1, 0, 700, 98
31509, V, 1, 1, 1, 1, 0, 700, 98
31510, V, 1, 1, 1, 1, 0, 700, 98
31511, V, 1, 1, 1, 1, 0, 700, 98
31512, V, 1, 1, 1, 1, 0, 700, 98
31513, V, 1, 1, 1, 1, 0, 700, 98
31514, V, 1, 1, 1, 1, 0, 700, 98
31515, V, 1, 1, 1, 1, 0, 700, 98
31516, V, 1, 1, 1, 1, 0, 700, 98
31517, V, 1, 1, 1, 1, 0, 700, 98
31518, V, 1, 1, 1, 1, 0, 700, 98
31519, V, 1, 1, 1, 1, 0, 700, 98
31520, V, 1, 1, 1, 1, 0, 700, 98
31521, V, 1, 1, 1, 1, 0, 700, 98
31522, V, 1, 1, 1, 1, 0, 700, 98
31523, V, 1, 1, 1, 1, 0, 700, 98
31524, V, 1, 1, 1, 1, 0, 700, 98
31525, V, 1, 1, 1, 1, 0, 700, 98
31526, V, 1, 1, 1, 1, 0, 700, 98
31527, V, 1, 1, 1, 1, 0, 700, 98
31528, V, 1, 1, 1, 1, 0, 700, 98
31529, V, 1, 1, 1, 1, 0, 700, 98
31531, V, 1, 1, 1, 1, 0, 700, 98
31532, V, 1, 1, 1, 1, 0, 700, 98
31533, V, 1, 1, 1, 1, 0, 700, 98
31534, V, 1, 1, 1, 1, 0, 700, 98
31535, V, 1, 1, 1, 1, 0, 700, 98
31536, V, 1, 1, 1, 1, 0, 700, 98
31537, V, 1, 1, 1, 1, 0, 700, 98
31538, V, 1, 1, 1, 1, 0, 700, 98
31539, V, 1, 1, 1, 1, 0, 700, 98
31540, V, 1, 1, 1, 1, 0, 700, 98
31541, V, 1, 1, 1, 1, 0, 700, 98
31542, V, 1, 1, 1, 1, 0, 700, 98
31543, V, 1, 1, 1, 1, 0, 700, 98
31544, V, 1, 1, 1, 1, 0, 700, 98
31545, V, 1, 1, 1, 1, 0, 700, 98
31546, V, 1, 1, 1, 1, 0, 700, 98
31547, V, 1, 1, 1, 1, 0, 700, 98
31548, V, 1, 1, 1, 1, 0, 700, 98
31549, V, 1, 1, 1, 1, 0, 700, 98
31550, V, 1, 1, 1, 1, 0, 700, 98
31551, V, 1, 1, 1, 1, 0, 700, 98
31552, V, 1, 1, 1, 1, 0, 700, 98
31553, V, 1, 1, 1, 1, 0, 700, 98
31554, V, 1, 1, 1, 1, 0, 700, 98
31555, V, 1, 1, 1, 1, 0, 700, 98
31556, V, 1, 1, 1, 1, 0, 700, 98
31557, V, 1, 1, 1, 1, 0, 700, 98
31558, V, 1, 1, 1, 1, 0, 700, 98
31559, V, 1, 1, 1, 1, 0, 700, 98
31560, V, 1, 1, 1, 1, 0, 700, 98
31561, V, 1, 1, 1, 1, 0, 700, 98
31562, V, 1, 1, 1, 1, 0, 700, 98
31563, V, 1, 1, 1, 1, 0, 700, 98
31564, V, 1, 1, 1, 1, 0, 700, 98
31565, V, 1, 1, 1, 1, 0, 700, 98
31566, V, 1, 1, 1, 1, 0, 700, 98
31567, V, 1, 1, 1, 1, 0, 700, 98
31568, V, 1, 1, 1, 1, 0, 700, 98
31569, V, 1, 1, 1, 1, 0, 700, 98
31570, V, 1, 1, 1, 1, 0, 700, 98
31571, V, 1, 1, 1, 1, 0, 700, 98
31572, V, 1, 1, 1, 1, 0, 700, 98
31574, V, 1, 1, 1, 1, 0, 700, 98
31575, V, 1, 1, 1, 1, 0, 700, 98
31576, V, 1, 1, 1, 1, 0, 700, 98
31577, V, 1, 1, 1, 1, 0, 700, 98
31578, V, 1, 1, 1, 1, 0, 700, 98
31579, V, 1, 1, 1, 1, 0, 700, 98
31580, V, 1, 1, 1, 1, 0, 700, 98
31581, V, 1, 1, 1, 1, 0, 700, 98
31582, V, 1, 1, 1, 1, 0, 700, 98
31583, V, 1, 1, 1, 1, 0, 700, 98
31584, V, 1, 1, 1, 1, 0, 700, 98
31585, V, 1, 1, 1, 1, 0, 700, 98
31586, V, 1, 1, 1, 1, 0, 700, 98
31587, V, 1, 1, 1, 1, 0, 700, 98
31588, V, 1, 1, 1, 1, 0, 700, 98
31589, V, 1, 1, 1, 1, 0, 700, 98
31590, V, 1, 1, 1, 1, 0, 700, 98
31591, V, 1, 1, 1, 1, 0, 700, 98
31592, V, 1, 1, 1, 1, 0, 700, 98
31593, V, 1, 1, 1, 1, 0, 700, 98
31594, V, 1, 1, 1, 1, 0, 700, 98
31595, V, 1, 1, 1, 1, 0, 700, 98
31596, V, 1, 1, 1, 1, 0, 700, 98
31597, V, 1, 1, 1, 1, 0, 700, 98
31598, V, 1, 1, 1, 1, 0, 700, 98
31599, V, 1, 1, 1, 1, 0, 700, 98
31600, V, 1, 1, 1, 1, 0, 700, 98
31601, V, 1, 1, 1, 1, 0, 700, 98
31602, V, 1, 1, 1, 1, 0, 700, 98
31603, V, 1, 1, 1, 1, 0, 700, 98
31604, V, 1, 1, 1, 1, 0, 700, 98
31605, V, 1, 1, 1, 1, 0, 700, 98
31606, V, 1, 1, 1, 1, 0, 700, 98
31607, V, 1, 1, 1, 1, 0, 700, 98
31608, V, 1, 1, 1, 1, 0, 700, 98
31609, V, 1, 1, 1, 1, 0, 700, 98
31610, V, 1, 1, 1, 1, 0, 700, 98
31611, V, 1, 1, 1, 1, 0, 700, 98
31612, V, 1, 1, 1, 1, 0, 700, 98
31613, V, 1, 1, 1, 1, 0, 700, 98
31614, V, 1, 1, 1, 1, 0, 700, 98
31616, V, 1, 1, 1, 1, 0, 700, 98
31617, V, 1, 1, 1, 1, 0, 700, 98
31618, V, 1, 1, 1, 1, 0, 700, 98
31619, V, 1, 1, 1, 1, 0, 700, 98
31620, V, 1, 1, 1, 1, 0, 700, 98
31621, V, 1, 1, 1, 1, 0, 700, 98
31622, V, 1, 1, 1, 1, 0, 700, 98
31623, V, 1, 1, 1, 1, 0, 700, 98
31624, V, 1, 1, 1, 1, 0, 700, 98
31625, V, 1, 1, 1, 1, 0, 700, 98
31626, V, 1, 1, 1, 1, 0, 700, 98
31627, V, 1, 1, 1, 1, 0, 700, 98
31628, V, 1, 1, 1, 1, 0, 700, 98
31629, V, 1, 1, 1, 1, 0, 700, 98
31630, V, 1, 1, 1, 1, 0, 700, 98
31631, V, 1, 1, 1, 1, 0, 700, 98
31632, V, 1, 1, 1, 1, 0, 700, 98
31633, V, 1, 1, 1, 1, 0, 700, 98
31634, V, 1, 1, 1, 1, 0, 700, 98
31635, V, 1, 1, 1, 1, 0, 700, 98
31636, V, 1, 1, 1, 1, 0, 700, 98
31637, V, 1, 1, 1, 1, 0, 700, 98
31638, V, 1, 1, 1, 1, 0, 700, 98
31639, V, 1, 1, 1, 1, 0, 700, 98
31640, V, 1, 1, 1, 1, 0, 700, 98
31641, V, 1, 1, 1, 1, 0, 700, 98
31642, V, 1, 1, 1, 1, 0, 700, 98
31643, V, 1, 1, 1, 1, 0, 700, 98
31644, V, 1, 1, 1, 1, 0, 700, 98
31645, V, 1, 1, 1, 1, 0, 700, 98
31646, V, 1, 1, 1, 1, 0, 700, 98
31647, V, 1, 1, 1, 1, 0, 700, 98
31648, V, 1, 1, 1, 1, 0, 700, 98
31649, V, 1, 1, 1, 1, 0, 700, 98
31650, V, 1, 1, 1, 1, 0, 700, 98
31651, V, 1, 1, 1, 1, 0, 700, 98
31652, V, 1, 1, 1, 1, 0, 700, 98
31653, V, 1, 1, 1, 1, 0, 700, 98
31654, V, 1, 1, 1, 1, 0, 700, 98
31655, V, 1, 1, 1, 1, 0, 700, 98
31656, V, 1, 1, 1, 1, 0, 700, 98
31657, V, 1, 1, 1, 1, 0, 700, 98
31659, V, 1, 1, 1, 1, 0, 700, 98
31660, V, 1, 1, 1, 1, 0, 700, 98
31661, V, 1, 1, 1, 1, 0, 700, 98
31662, V, 1, 1, 1, 1, 0, 700, 98
31663, V, 1, 1, 1, 1, 0, 700, 98
31664, V, 1, 1, 1, 1, 0, 700, 98
31665, V, 1, 1, 1, 1, 0, 700, 98
31666, V, 1, 1, 1, 1, 0, 700, 98
31667, V, 1, 1, 1, 1, 0, 700, 98
31668, V, 1, 1, 1, 1, 0, 700, 98
31669, V, 1, 1, 1, 1, 0, 700, 98
31670, V, 1, 1, 1, 1, 0, 700, 98
31671, V, 1, 1, 1, 1, 0, 700, 98
31672, V, 1, 1, 1, 1, 0, 700, 98
31673, V, 1, 1, 1, 1, 0, 700, 98
31674, V, 1, 1, 1, 1, 0, 700, 98
31675, V, 1, 1, 1, 1, 0, 700, 98
31676, V, 1, 1, 1, 1, 0, 700, 98
31677, V, 1, 1, 1, 1, 0, 700, 98
31678, V, 1, 1, 1, 1, 0, 700, 98
31679, V, 1, 1, 1, 1, 0, 700, 98
31680, V, 1, 1, 1, 1, 0, 700, 98
31681, V, 1, 1, 1, 1, 0, 700, 98
31682, V, 1, 1, 1, 1, 0, 700, 98
31683, V, 1, 1, 1, 1, 0, 700, 98
31684, V, 1, 1, 1, 1, 0, 700, 98
31685, V, 1, 1, 1, 1, 0, 700, 98
31686, V, 1, 1, 1, 1, 0, 700, 98
31687, V, 1, 1, 1, 1, 0, 700, 98
31688, V, 1, 1, 1, 1, 0, 700, 98
31689, V, 1, 1, 1, 1, 0, 700, 98
31690, V, 1, 1, 1, 1, 0, 700, 98
31691, V, 1, 1, 1, 1, 0, 700, 98
31692, V, 1, 1, 1, 1, 0, 700, 98
31693, V, 1, 1, 1, 1, 0, 700, 98
31694, V, 1, 1, 1, 1, 0, 700, 98
31695, V, 1, 1, 1, 1, 0, 700, 98
31696, V, 1, 1, 1, 1, 0, 700, 98
31697, V, 1, 1, 1, 1, 0, 700, 98
31698, V, 1, 1, 1, 1, 0, 700, 98
31699, V, 1, 1, 1, 1, 0, 700, 98
31700, V, 1, 1, 1, 1, 0, 700, 98
31702, V, 1, 1, 1, 1, 0, 700, 98
31703, V, 1, 1, 1, 1, 0, 700, 98
31704, V, 1, 1, 1, 1, 0, 700, 98
31705, V, 1, 1, 1, 1, 0, 700, 98
31706, V, 1, 1, 1, 1, 0, 700, 98
31707, V, 1, 1, 1, 1, 0, 700, 98
31708, V, 1, 1, 1, 1, 0, 700, 98
31709, V, 1, 1, 1, 1, 0, 700, 98
31710, V, 1, 1, 1, 1, 0, 700, 98
31711, V, 1, 1, 1, 1, 0, 700, 98
31712, V, 1, 1, 1, 1, 0, 700, 98
31713, V, 1, 1, 1, 1, 0, 700, 98
31714, V, 1, 1, 1, 1, 0, 700, 98
31715, V, 1, 1, 1, 1, 0, 700, 98
31716, V, 1, 1, 1, 1, 0, 700, 98
31717, V, 1, 1, 1, 1, 0, 700, 98
31718, V, 1, 1, 1, 1, 0, 700, 98
31719, V, 1, 1, 1, 1, 0, 700, 98
31720, V, 1, 1, 1, 1, 0, 700, 98
31721, V, 1, 1, 1, 1, 0, 700, 98
31722, V, 1, 1, 1, 1, 0, 700, 98
31723, V, 1, 1, 1, 1, 0, 700, 98
31724, V, 1, 1, 1, 1, 0, 700, 98
31725, V, 1, 1, 1, 1, 0, 700, 98
31726, V, 1, 1, 1, 1, 0, 700, 98
31727, V, 1, 1, 1, 1, 0, 700, 98
31728, V, 1, 1, 1, 1, 0, 700, 98
31729, V, 1, 1, 1, 1, 0, 700, 98
31730, V, 1, 1, 1, 1, 0, 700, 98
31731, V, 1, 1, 1, 1, 0, 700, 98
31732, V, 1, 1, 1, 1, 0, 700, 98
31733, V, 1, 1, 1, 1, 0, 700, 98
31734, V, 1, 1, 1, 1, 0, 700, 98
31735, V, 1, 1, 1, 1, 0, 700, 98
31736, V, 1, 1, 1, 1, 0, 700, 98
31737, V, 1, 1, 1, 1, 0, 700, 98
31738, V, 1, 1, 1, 1, 0, 700, 98
31739, V, 1, 1, 1, 1, 0, 700, 98
31740, V, 1, 1, 1, 1, 0, 700, 98
31741, V, 1, 1, 1, 1, 0, 700, 98
31742, V, 1, 1, 1, 1, 0, 700, 98
31744, V, 1, 1, 1, 1, 0, 700, 98
31745, V, 1, 1, 1, 1, 0, 700, 98
31746, V, 1, 1, 1, 1, 0, 700, 98
31747, V, 1, 1, 1, 1, 0, 700, 98
31748, V, 1, 1, 1, 1, 0, 700, 98
31749, V, 1, 1, 1, 1, 0, 700, 98
31750, V, 1, 1, 1, 1, 0, 700, 98
31751, V, 1, 1, 1, 1, 0, 700, 98
31752, V, 1, 1, 1, 1, 0, 700, 98
31753, V, 1, 1, 1, 1, 0, 700, 98
31754, V, 1, 1, 1, 1, 0, 700, 98
31755, V, 1, 1, 1, 1, 0, 700, 98
31756, V, 1, 1, 1, 1, 0, 700, 98
31757, V, 1, 1, 1, 1, 0, 700, 98
31758, V, 1, 1, 1, 1, 0, 700, 98
31759, V, 1, 1, 1, 1, 0, 700, 98
31760, V, 1, 1, 1, 1, 0, 700, 98
31761, V, 1, 1, 1, 1, 0, 700, 98
31762, V, 1, 1, 1, 1, 0, 700, 98
31763, V, 1, 1, 1, 1, 0, 700, 98
31764, V, 1, 1, 1, 1, 0, 700, 98
31765, V, 1, 1, 1, 1, 0, 700, 98
31766, V, 1, 1, 1, 1, 0, 700, 98
31767, V, 1, 1, 1, 1, 0, 700, 98
31768, V, 1, 1, 1, 1, 0, 700, 98
31769, V, 1, 1, 1, 1, 0, 700, 98
31770, V, 1, 1, 1, 1, 0, 700, 98
31771, V, 1, 1, 1, 1, 0, 700, 98
31772, V, 1, 1, 1, 1, 0, 700, 98
31773, V, 1, 1, 1, 1, 0, 700, 98
31774, V, 1, 1, 1, 1, 0, 700, 98
31775, V, 1, 1, 1, 1, 0, 700, 98
31776, V, 1, 1, 1, 1, 0, 700, 98
31777, V, 1, 1, 1, 1, 0, 700, 98
31778, V, 1, 1, 1, 1, 0, 700, 98
31779, V, 1, 1, 1, 1, 0, 700, 98
31780, V, 1, 1, 1, 1, 0, 700, 98
31781, V, 1, 1, 1, 1, 0, 700, 98
31782, V, 1, 1, 1, 1, 0, 700, 98
31783, V, 1, 1, 1, 1, 0, 700, 98
31784, V, 1, 1, 1, 1, 0, 700, 98
31785, V, 1, 1, 1, 1, 0, 700, 98
31787, V, 1, 1, 1, 1, 0, 700, 98
31788, V, 1, 1, 1, 1, 0, 700, 98
31789, V, 1, 1, 1, 1, 0, 700, 98
31790, V, 1, 1, 1, 1, 0, 700, 98
31791, V, 1, 1, 1, 1, 0, 700, 98
31792, V, 1, 1, 1, 1, 0, 700, 98
31793, V, 1, 1, 1, 1, 0, 700, 98
31794, V, 1, 1, 1, 1, 0, 700, 98
31795, V, 1, 1, 1, 1, 0, 700, 98
31796, V, 1, 1, 1, 1, 0, 700, 98
31797, V, 1, 1, 1, 1, 0, 700, 98
31798, V, 1, 1, 1, 1, 0, 700, 98
31799, V, 1, 1, 1, 1, 0, 700, 98
31800, V, 1, 1, 1, 1, 0, 700, 98
31801, V, 1, 1, 1, 1, 0, 700, 98
31802, V, 1, 1, 1, 1, 0, 700, 98
31803, V, 1, 1, 1, 1, 0, 700, 98
31804, V, 1, 1, 1, 1, 0, 700, 98
31805, V, 1, 1, 1, 1, 0, 700, 98
31806, V, 1, 1, 1, 1, 0, 700, 98
31807, V, 1, 1, 1, 1, 0, 700, 98
31808, V, 1, 1, 1, 1, 0, 700, 98
31809, V, 1, 1, 1, 1, 0, 700, 98
31810, V, 1, 1, 1, 1, 0, 700, 98
31811, V, 1, 1, 1, 1, 0, 700, 98
31812, V, 1, 1, 1, 1, 0, 700, 98
31813, V, 1, 1, 1, 1, 0, 700, 98
31814, V, 1, 1, 1, 1, 0, 700, 98
31815, V, 1, 1, 1, 1, 0, 700, 98
31816, V, 1, 1, 1, 1, 0, 700, 98
31817, V, 1, 1, 1, 1, 0, 700, 98
31818, V, 1, 1, 1, 1, 0, 700, 98
31819, V, 1, 1, 1, 1, 0, 700, 98
31820, V, 1, 1, 1, 1, 0, 700, 98
31821, V, 1, 1, 1, 1, 0, 700, 98
31822, V, 1, 1, 1, 1, 0, 700, 98
31823, V, 1, 1, 1, 1, 0, 700, 98
31824, V, 1, 1, 1, 1, 0, 700, 98
31825, V, 1, 1, 1, 1, 0, 700, 98
31826, V, 1, 1, 1, 1, 0, 700, 98
31827, V, 1, 1, 1, 1, 0, 700, 98
31828, V, 1, 1, 1, 1, 0, 700, 98
31830, V, 1, 1, 1, 1, 0, 700, 98
31831, V, 1, 1, 1, 1, 0, 700, 98
31832, V, 1, 1, 1, 1, 0, 700, 98
31833, V, 1, 1, 1, 1, 0, 700, 98
31834, V, 1, 1, 1, 1, 0, 700, 98
31835, V, 1, 1, 1, 1, 0, 700, 98
31836, V, 1, 1, 1, 1, 0, 700, 98
31837, V, 1, 1, 1, 1, 0, 700, 98
31838, V, 1, 1, 1, 1, 0, 700, 98
31839, V, 1, 1, 1, 1, 0, 700, 98
31840, V, 1, 1, 1, 1, 0, 700, 98
31841, V, 1, 1, 1, 1, 0, 700, 98
31842, V, 1, 1, 1, 1, 0, 700, 98
31843, V, 1, 1, 1, 1, 0, 700, 98
31844, V, 1, 1, 1, 1, 0, 700, 98
31845, V, 1, 1, 1, 1, 0, 700, 98
31846, V, 1, 1, 1, 1, 0, 700, 98
31847, V, 1, 1, 1, 1, 0, 700, 98
31848, V, 1, 1, 1, 1, 0, 700, 98
31849, V, 1, 1, 1, 1, 0, 700, 98
31850, V, 1, 1, 1, 1, 0, 700, 98
31851, V, 1, 1, 1, 1, 0, 700, 98
31852, V, 1, 1, 1, 1, 0, 700, 98
31853, V, 1, 1, 1, 1, 0, 700, 98
31854, V, 1, 1, 1, 1, 0, 700, 98
31855, V, 1, 1, 1, 1, 0, 700, 98
31856, V, 1, 1, 1, 1, 0, 700, 98
31857, V, 1, 1, 1, 1, 0, 700, 98
31858, V, 1, 1, 1, 1, 0, 700, 98
31859, V, 1, 1, 1, 1, 0, 700, 98
31860, V, 1, 1, 1, 1, 0, 700, 98
31861, V, 1, 1, 1, 1, 0, 700, 98
31862, V, 1, 1, 1, 1, 0, 700, 98
31863, V, 1, 1, 1, 1, 0, 700, 98
31864, V, 1, 1, 1, 1, 0, 700, 98
31865, V, 1, 1, 1, 1, 0, 700, 98
31866, V, 1, 1, 1, 1, 0, 700, 98
31867, V, 1, 1, 1, 1, 0, 700, 98
31868, V, 1, 1, 1, 1, 0, 700, 98
31869, V, 1, 1, 1, 1, 0, 700, 98
31870, V, 1, 1, 1, 1, 0, 700, 98
31872, V, 1, 1, 1, 1, 0, 700, 98
31873, V, 1, 1, 1, 1, 0, 700, 98
31874, V, 1, 1, 1, 1, 0, 700, 98
31875, V, 1, 1, 1, 1, 0, 700, 98
31876, V, 1, 1, 1, 1, 0, 700, 98
31877, V, 1, 1, 1, 1, 0, 700, 98
31878, V, 1, 1, 1, 1, 0, 700, 98
31879, V, 1, 1, 1, 1, 0, 700, 98
31880, V, 1, 1, 1, 1, 0, 700, 98
31881, V, 1, 1, 1, 1, 0, 700, 98
31882, V, 1, 1, 1, 1, 0, 700, 98
31883, V, 1, 1, 1, 1, 0, 700, 98
31884, V, 1, 1, 1, 1, 0, 700, 98
31885, V, 1, 1, 1, 1, 0, 700, 98
31886, V, 1, 1, 1, 1, 0, 700, 98
31887, V, 1, 1, 1, 1, 0, 700, 98
31888, V, 1, 1, 1, 1, 0, 700, 98
31889, V, 1, 1, 1, 1, 0, 700, 98
31890, V, 1, 1, 1, 1, 0, 700, 98
31891, V, 1, 1, 1, 1, 0, 700, 98
31892, V, 1, 1, 1, 1, 0, 700, 98
31893, V, 1, 1, 1, 1, 0, 700, 98
31894, V, 1, 1, 1, 1, 0, 700, 98
31895, V, 1, 1, 1, 1, 0, 700, 98
31896, V, 1, 1, 1, 1, 0, 700, 98
31897, V, 1, 1, 1, 1, 0, 700, 98
31898, V, 1, 1, 1, 1, 0, 700, 98
31899, V, 1, 1, 1, 1, 0, 700, 98
31900, V, 1, 1, 1, 1, 0, 700, 98
31901, V, 1, 1, 1, 1, 0, 700, 98
31902, V, 1, 1, 1, 1, 0, 700, 98
31903, V, 1, 1, 1, 1, 0, 700, 98
31904, V, 1, 1, 1, 1, 0, 700, 98
31905, V, 1, 1, 1, 1, 0, 700, 98
31906, V, 1, 1, 1, 1, 0, 700, 98
31907, V, 1, 1, 1, 1, 0, 700, 98
31908, V, 1, 1, 1, 1, 0, 700, 98
31909, V, 1, 1, 1, 1, 0, 700, 98
31910, V, 1, 1, 1, 1, 0, 700, 98
31911, V, 1, 1, 1, 1, 0, 700, 98
31912, V, 1, 1, 1, 1, 0, 700, 98
31913, V, 1, 1, 1, 1, 0, 700, 98
31915, V, 1, 1, 1, 1, 0, 700, 98
31916, V, 1, 1, 1, 1, 0, 700, 98
31917, V, 1, 1, 1, 1, 0, 700, 98
31918, V, 1, 1, 1, 1, 0, 700, 98
31919, V, 1, 1, 1, 1, 0, 700, 98
31920, V, 1, 1, 1, 1, 0, 700, 98
31921, V, 1, 1, 1, 1, 0, 700, 98
31922, V, 1, 1, 1, 1, 0, 700, 98
31923, V, 1, 1, 1, 1, 0, 700, 98
31924, V, 1, 1, 1, 1, 0, 700, 98
31925, V, 1, 1, 1, 1, 0, 700, 98
31926, V, 1, 1, 1, 1, 0, 700, 98
31927, V, 1, 1, 1, 1, 0, 700, 98
31928, V, 1, 1, 1, 1, 0, 700, 98
31929, V, 1, 1, 1, 1, 0, 700, 98
31930, V, 1, 1, 1, 1, 0, 700, 98
31931, V, 1, 1, 1, 1, 0, 700, 98
31932, V, 1, 1, 1, 1, 0, 700, 98
31933, V, 1, 1, 1, 1, 0, 700, 98
31934, V, 1, 1, 1, 1, 0, 700, 98
31935, V, 1, 1, 1, 1, 0, 700, 98
31936, V, 1, 1, 1, 1, 0, 700, 98
31937, V, 1, 1, 1, 1, 0, 700, 98
31938, V, 1, 1, 1, 1, 0, 700, 98
31939, V, 1, 1, 1, 1, 0, 700, 98
31940, V, 1, 1, 1, 1, 0, 700, 98
31941, V, 1, 1, 1, 1, 0, 700, 98
31942, V, 1, 1, 1, 1, 0, 700, 98
31943, V, 1, 1, 1, 1, 0, 700, 98
31944, V, 1, 1, 1, 1, 0, 700, 98
31945, V, 1, 1, 1, 1, 0, 700, 98
31946, V, 1, 1, 1, 1, 0, 700, 98
31947, V, 1, 1, 1, 1, 0, 700, 98
31948, V, 1, 1, 1, 1, 0, 700, 98
31949, V, 1, 1, 1, 1, 0, 700, 98
31950, V, 1, 1, 1, 1, 0, 700, 98
31951, V, 1, 1, 1, 1, 0, 700, 98
31952, V, 1, 1, 1, 1, 0, 700, 98
31953, V, 1, 1, 1, 1, 0, 700, 98
31954, V, 1, 1, 1, 1, 0, 700, 98
31955, V, 1, 1, 1, 1, 0, 700, 98
31956, V, 1, 1, 1, 1, 0, 700, 98
31958, V, 1, 1, 1, 1, 0, 700, 98
31959, V, 1, 1, 1, 1, 0, 700, 98
31960, V, 1, 1, 1, 1, 0, 700, 98
31961, V, 1, 1, 1, 1, 0, 700, 98
31962, V, 1, 1, 1, 1, 0, 700, 98
31963, V, 1, 1, 1, 1, 0, 700, 98
31964, V, 1, 1, 1, 1, 0, 700, 98
31965, V, 1, 1, 1, 1, 0, 700, 98
31966, V, 1, 1, 1, 1, 0, 700, 98
31967, V, 1, 1, 1, 1, 0, 700, 98
31968, V, 1, 1, 1, 1, 0, 700, 98
31969, V, 1, 1, 1, 1, 0, 700, 98
31970, V, 1, 1, 1, 1, 0, 700, 98
31971, V, 1, 1, 1, 1, 0, 700, 98
31972, V, 1, 1, 1, 1, 0, 700, 98
31973, V, 1, 1, 1, 1, 0, 700, 98
31974, V, 1, 1, 1, 1, 0, 700, 98
31975, V, 1, 1, 1, 1, 0, 700, 98
31976, V, 1, 1, 1, 1, 0, 700, 98
31977, V, 1, 1, 1, 1, 0, 700, 98
31978, V, 1, 1, 1, 1, 0, 700, 98
31979, V, 1, 1, 1, 1, 0, 700, 98
31980, V, 1, 1, 1, 1, 0, 700, 98
31981, V, 1, 1, 1, 1, 0, 700, 98
31982, V, 1, 1, 1, 1, 0, 700, 98
31983, V, 1, 1, 1, 1, 0, 700, 98
31984, V, 1, 1, 1, 1, 0, 700, 98
31985, V, 1, 1, 1, 1, 0, 700, 98
31986, V, 1, 1, 1, 1, 0, 700, 98
31987, V, 1, 1, 1, 1, 0, 700, 98
31988, V, 1, 1, 1, 1, 0, 700, 98
31989, V, 1, 1, 1, 1, 0, 700, 98
31990, V, 1, 1, 1, 1, 0, 700, 98
31991, V, 1, 1, 1, 1, 0, 700, 98
31992, V, 1, 1, 1, 1, 0, 700, 98
31993, V, 1, 1, 1, 1, 0, 700, 98
31994, V, 1, 1, 1, 1, 0, 700, 98
31995, V, 1, 1, 1, 1, 0, 700, 98
31996, V, 1, 1, 1, 1, 0, 700, 98
31997, V, 1, 1, 1, 1, 0, 700, 98
31998, V, 1, 1, 1, 1, 0, 700, 98
32000, V, 1, 1, 1, 1, 0, 700, 98
32001, V, 1, 1, 1, 1, 0, 700, 98
32002, V, 1, 1, 1, 1, 0, 700, 98
32003, V, 1, 1, 1, 1, 0, 700, 98
32004, V, 1, 1, 1, 1, 0, 700, 98
32005, V, 1, 1, 1, 1, 0, 700, 98
32006, V, 1, 1, 1, 1, 0, 700, 98
32007, V, 1, 1, 1, 1, 0, 700, 98
32008, V, 1, 1, 1, 1, 0, 700, 98
32009, V, 1, 1, 1, 1, 0, 700, 98
32010, V, 1, 1, 1, 1, 0, 700, 98
32011, V, 1, 1, 1, 1, 0, 700, 98
32012, V, 1, 1, 1, 1, 0, 700, 98
32013, V, 1, 1, 1, 1, 0, 700, 98
32014, V, 1, 1, 1, 1, 0, 700, 98
32015, V, 1, 1, 1, 1, 0, 700, 98
32016, V, 1, 1, 1, 1, 0, 700, 98
32017, V, 1, 1, 1, 1, 0, 700, 98
32018, V, 1, 1, 1, 1, 0, 700, 98
32019, V, 1, 1, 1, 1, 0, 700, 98
32020, V, 1, 1, 1, 1, 0, 700, 98
32021, V, 1, 1, 1, 1, 0, 700, 98
32022, V, 1, 1, 1, 1, 0, 700, 98
32023, V, 1, 1, 1, 1, 0, 700, 98
32024, V, 1, 1, 1, 1, 0, 700, 98
32025, V, 1, 1, 1, 1, 0, 700, 98
32026, V, 1, 1, 1, 1, 0, 700, 98
32027, V, 1, 1, 1, 1, 0, 700, 98
32028, V, 1, 1, 1, 1, 0, 700, 98
32029, V, 1, 1, 1, 1, 0, 700, 98
32030, V, 1, 1, 1, 1, 0, 700, 98
32031, V, 1, 1, 1, 1, 0, 700, 98
32032, V, 1, 1, 1, 1, 0, 700, 98
32033, V, 1, 1, 1, 1, 0, 700, 98
32034, V, 1, 1, 1, 1, 0, 700, 98
32035, V, 1, 1, 1, 1, 0, 700, 98
32036, V, 1, 1, 1, 1, 0, 700, 98
32037, V, 1, 1, 1, 1, 0, 700, 98
32038, V, 1, 1, 1, 1, 0, 700, 98
32039, V, 1, 1, 1, 1, 0, 700, 98
32040, V, 1, 1, 1, 1, 0, 700, 98
32041, V, 1, 1, 1, 1, 0, 700, 98
32043, V, 1, 1, 1, 1, 0, 700, 98
32044, V, 1, 1, 1, 1, 0, 700, 98
32045, V, 1, 1, 1, 1, 0, 700, 98
32046, V, 1, 1, 1, 1, 0, 700, 98
32047, V, 1, 1, 1, 1, 0, 700, 98
32048, V, 1, 1, 1, 1, 0, 700, 98
32049, V, 1, 1, 1, 1, 0, 700, 98
32050, V, 1, 1, 1, 1, 0, 700, 98
32051, V, 1, 1, 1, 1, 0, 700, 98
32052, V, 1, 1, 1, 1, 0, 700, 98
32053, V, 1, 1, 1, 1, 0, 700, 98
32054, V, 1, 1, 1, 1, 0, 700, 98
32055, V, 1, 1, 1, 1, 0, 700, 98
32056, V, 1, 1, 1, 1, 0, 700, 98
32057, V, 1, 1, 1, 1, 0, 700, 98
32058, V, 1, 1, 1, 1, 0, 700, 98
32059, V, 1, 1, 1, 1, 0, 700, 98
32060, V, 1, 1, 1, 1, 0, 700, 98
32061, V, 1, 1, 1, 1, 0, 700, 98
32062, V, 1, 1, 1, 1, 0, 700, 98
32063, V, 1, 1, 1, 1, 0, 700, 98
32064, V, 1, 1, 1, 1, 0, 700, 98
32065, V, 1, 1, 1, 1, 0, 700, 98
32066, V, 1, 1, 1, 1, 0, 700, 98
32067, V, 1, 1, 1, 1, 0, 700, 98
32068, V, 1, 1, 1, 1, 0, 700, 98
32069, V, 1, 1, 1, 1, 0, 700, 98
32070, V, 1, 1, 1, 1, 0, 700, 98
32071, V, 1, 1, 1, 1, 0, 700, 98
32072, V, 1, 1, 1, 1, 0, 700, 98
32073, V, 1, 1, 1, 1, 0, 700, 98
32074, V, 1, 1, 1, 1, 0, 700, 98
32075, V, 1, 1, 1, 1, 0, 700, 98
32076, V, 1, 1, 1, 1, 0, 700, 98
32077, V, 1, 1, 1, 1, 0, 700, 98
32078, V, 1, 1, 1, 1, 0, 700, 98
32079, V, 1, 1, 1, 1, 0, 700, 98
32080, V, 1, 1, 1, 1, 0, 700, 98
32081, V, 1, 1, 1, 1, 0, 700, 98
32082, V, 1, 1, 1, 1, 0, 700, 98
32083, V, 1, 1, 1, 1, 0, 700, 98
32084, V, 1, 1, 1, 1, 0, 700, 98
32086, V, 1, 1, 1, 1, 0, 700, 98
32087, V, 1, 1, 1, 1, 0, 700, 98
32088, V, 1, 1, 1, 1, 0, 700, 98
32089, V, 1, 1, 1, 1, 0, 700, 98
32090, V, 1, 1, 1, 1, 0, 700, 98
32091, V, 1, 1, 1, 1, 0, 700, 98
32092, V, 1, 1, 1, 1, 0, 700, 98
32093, V, 1, 1, 1, 1, 0, 700, 98
32094, V, 1, 1, 1, 1, 0, 700, 98
32095, V, 1, 1, 1, 1, 0, 700, 98
32096, V, 1, 1, 1, 1, 0, 700, 98
32097, V, 1, 1, 1, 1, 0, 700, 98
32098, V, 1, 1, 1, 1, 0, 700, 98
32099, V, 1, 1, 1, 1, 0, 700, 98
32100, V, 1, 1, 1, 1, 0, 700, 98
32101, V, 1, 1, 1, 1, 0, 700, 98
32102, V, 1, 1, 1, 1, 0, 700, 98
32103, V, 1, 1, 1, 1, 0, 700, 98
32104, V, 1, 1, 1, 1, 0, 700, 98
32105, V, 1, 1, 1, 1, 0, 700, 98
32106, V, 1, 1, 1, 1, 0, 700, 98
32107, V, 1, 1, 1, 1, 0, 700, 98
32108, V, 1, 1, 1, 1, 0, 700, 98
32109, V, 1, 1, 1, 1, 0, 700, 98
32110, V, 1, 1, 1, 1, 0, 700, 98
32111, V, 1, 1, 1, 1, 0, 700, 98
32112, V, 1, 1, 1, 1, 0, 700, 98
32113, V, 1, 1, 1, 1, 0, 700, 98
32114, V, 1, 1, 1, 1, 0, 700, 98
32115, V, 1, 1, 1, 1, 0, 700, 98
32116, V, 1, 1, 1, 1, 0, 700, 98
32117, V, 1, 1, 1, 1, 0, 700, 98
32118, V, 1, 1, 1, 1, 0, 700, 98
32119, V, 1, 1, 1, 1, 0, 700, 98
32120, V, 1, 1, 1, 1, 0, 700, 98
32121, V, 1, 1, 1, 1, 0, 700, 98
32122, V, 1, 1, 1, 1, 0, 700, 98
32123, V, 1, 1, 1, 1, 0, 700, 98
32124, V, 1, 1, 1, 1, 0, 700, 98
32125, V, 1, 1, 1, 1, 0, 700, 98
32126, V, 1, 1, 1, 1, 0, 700, 98
32128, V, 1, 1, 1, 1, 0, 700, 98
32129, V, 1, 1, 1, 1, 0, 700, 98
32130, V, 1, 1, 1, 1, 0, 700, 98
32131, V, 1, 1, 1, 1, 0, 700, 98
32132, V, 1, 1, 1, 1, 0, 700, 98
32133, V, 1, 1, 1, 1, 0, 700, 98
32134, V, 1, 1, 1, 1, 0, 700, 98
32135, V, 1, 1, 1, 1, 0, 700, 98
32136, V, 1, 1, 1, 1, 0, 700, 98
32137, V, 1, 1, 1, 1, 0, 700, 98
32138, V, 1, 1, 1, 1, 0, 700, 98
32139, V, 1, 1, 1, 1, 0, 700, 98
32140, V, 1, 1, 1, 1, 0, 700, 98
32141, V, 1, 1, 1, 1, 0, 700, 98
32142, V, 1, 1, 1, 1, 0, 700, 98
32143, V, 1, 1, 1, 1, 0, 700, 98
32144, V, 1, 1, 1, 1, 0, 700, 98
32145, V, 1, 1, 1, 1, 0, 700, 98
32146, V, 1, 1, 1, 1, 0, 700, 98
32147, V, 1, 1, 1, 1, 0, 700, 98
32148, V, 1, 1, 1, 1, 0, 700, 98
32149, V, 1, 1, 1, 1, 0, 700, 98
32150, V, 1, 1, 1, 1, 0, 700, 98
32151, V, 1, 1, 1, 1, 0, 700, 98
32152, V, 1, 1, 1, 1, 0, 700, 98
32153, V, 1, 1, 1, 1, 0, 700, 98
32154, V, 1, 1, 1, 1, 0, 700, 98
32155, V, 1, 1, 1, 1, 0, 700, 98
32156, V, 1, 1, 1, 1, 0, 700, 98
32157, V, 1, 1, 1, 1, 0, 700, 98
32158, V, 1, 1, 1, 1, 0, 700, 98
32159, V, 1, 1, 1, 1, 0, 700, 98
32160, V, 1, 1, 1, 1, 0, 700, 98
32161, V, 1, 1, 1, 1, 0, 700, 98
32162, V, 1, 1, 1, 1, 0, 700, 98
32163, V, 1, 1, 1, 1, 0, 700, 98
32164, V, 1, 1, 1, 1, 0, 700, 98
32165, V, 1, 1, 1, 1, 0, 700, 98
32166, V, 1, 1, 1, 1, 0, 700, 98
32167, V, 1, 1, 1, 1, 0, 700, 98
32168, V, 1, 1, 1, 1, 0, 700, 98
32169, V, 1, 1, 1, 1, 0, 700, 98
32171, V, 1, 1, 1, 1, 0, 700, 98
32172, V, 1, 1, 1, 1, 0, 700, 98
32173, V, 1, 1, 1, 1, 0, 700, 98
32174, V, 1, 1, 1, 1, 0, 700, 98
32175, V, 1, 1, 1, 1, 0, 700, 98
32176, V, 1, 1, 1, 1, 0, 700, 98
32177, V, 1, 1, 1, 1, 0, 700, 98
32178, V, 1, 1, 1, 1, 0, 700, 98
32179, V, 1, 1, 1, 1, 0, 700, 98
32180, V, 1, 1, 1, 1, 0, 700, 98
32181, V, 1, 1, 1, 1, 0, 700, 98
32182, V, 1, 1, 1, 1, 0, 700, 98
32183, V, 1, 1, 1, 1, 0, 700, 98
32184, V, 1, 1, 1, 1, 0, 700, 98
32185, V, 1, 1, 1, 1, 0, 700, 98
32186, V, 1, 1, 1, 1, 0, 700, 98
32187, V, 1, 1, 1, 1, 0, 700, 98
32188, V, 1, 1, 1, 1, 0, 700, 98
32189, V, 1, 1, 1, 1, 0, 700, 98
32190, V, 1, 1, 1, 1, 0, 700, 98
32191, V, 1, 1, 1, 1, 0, 700, 98
32192, V, 1, 1, 1, 1, 0, 700, 98
32193, V, 1, 1, 1, 1, 0, 700, 98
32194, V, 1, 1, 1, 1, 0, 700, 98
32195, V, 1, 1, 1, 1, 0, 700, 98
32196, V, 1, 1, 1, 1, 0, 700, 98
32197, V, 1, 1, 1, 1, 0, 700, 98
32198, V, 1, 1, 1, 1, 0, 700, 98
32199, V, 1, 1, 1, 1, 0, 700, 98
32200, V, 1, 1, 1, 1, 0, 700, 98
32201, V, 1, 1, 1, 1, 0, 700, 98
32202, V, 1, 1, 1, 1, 0, 700, 98
32203, V, 1, 1, 1, 1, 0, 700, 98
32204, V, 1, 1, 1, 1, 0, 700, 98
32205, V, 1, 1, 1, 1, 0, 700, 98
32206, V, 1, 1, 1, 1, 0, 700, 98
32207, V, 1, 1, 1, 1, 0, 700, 98
32208, V, 1, 1, 1, 1, 0, 700, 98
32209, V, 1, 1, 1, 1, 0, 700, 98
32210, V, 1, 1, 1, 1, 0, 700, 98
32211, V, 1, 1, 1, 1, 0, 700, 98
32212, V, 1, 1, 1, 1, 0, 700, 98
32214, V, 1, 1, 1, 1, 0, 700, 98
32215, V, 1, 1, 1, 1, 0, 700, 98
32216, V, 1, 1, 1, 1, 0, 700, 98
32217, V, 1, 1, 1, 1, 0, 700, 98
32218, V, 1, 1, 1, 1, 0, 700, 98
32219, V, 1, 1, 1, 1, 0, 700, 98
32220, V, 1, 1, 1, 1, 0, 700, 98
32221, V, 1, 1, 1, 1, 0, 700, 98
32222, V, 1, 1, 1, 1, 0, 700, 98
32223, V, 1, 1, 1, 1, 0, 700, 98
32224, V, 1, 1, 1, 1, 0, 700, 98
32225, V, 1, 1, 1, 1, 0, 700, 98
32226, V, 1, 1, 1, 1, 0, 700, 98
32227, V, 1, 1, 1, 1, 0, 700, 98
32228, V, 1, 1, 1, 1, 0, 700, 98
32229, V, 1, 1, 1, 1, 0, 700, 98
32230, V, 1, 1, 1, 1, 0, 700, 98
32231, V, 1, 1, 1, 1, 0, 700, 98
32232, V, 1, 1, 1, 1, 0, 700, 98
32233, V, 1, 1, 1, 1, 0, 700, 98
32234, V, 1, 1, 1, 1, 0, 700, 98
32235, V, 1, 1, 1, 1, 0, 700, 98
32236, V, 1, 1, 1, 1, 0, 700, 98
32237, V, 1, 1, 1, 1, 0, 700, 98
32238, V, 1, 1, 1, 1, 0, 700, 98
32239, V, 1, 1, 1, 1, 0, 700, 98
32240, V, 1, 1, 1, 1, 0, 700, 98
32241, V, 1, 1, 1, 1, 0, 700, 98
32242, V, 1, 1, 1, 1, 0, 700, 98
32243, V, 1, 1, 1, 1, 0, 700, 98
32244, V, 1, 1, 1, 1, 0, 700, 98
32245, V, 1, 1, 1, 1, 0, 700, 98
32246, V, 1, 1, 1, 1, 0, 700, 98
32247, V, 1, 1, 1, 1, 0, 700, 98
32248, V, 1, 1, 1, 1, 0, 700, 98
32249, V, 1, 1, 1, 1, 0, 700, 98
32250, V, 1, 1, 1, 1, 0, 700, 98
32251, V, 1, 1, 1, 1, 0, 700, 98
32252, V, 1, 1, 1, 1, 0, 700, 98
32253, V, 1, 1, 1, 1, 0, 700, 98
32254, V, 1, 1, 1, 1, 0, 700, 98
32256, V, 1, 1, 1, 1, 0, 700, 98
32257, V, 1, 1, 1, 1, 0, 700, 98
32258, V, 1, 1, 1, 1, 0, 700, 98
32259, V, 1, 1, 1, 1, 0, 700, 98
32260, V, 1, 1, 1, 1, 0, 700, 98
32261, V, 1, 1, 1, 1, 0, 700, 98
32262, V, 1, 1, 1, 1, 0, 700, 98
32263, V, 1, 1, 1, 1, 0, 700, 98
32264, V, 1, 1, 1, 1, 0, 700, 98
32265, V, 1, 1, 1, 1, 0, 700, 98
32266, V, 1, 1, 1, 1, 0, 700, 98
32267, V, 1, 1, 1, 1, 0, 700, 98
32268, V, 1, 1, 1, 1, 0, 700, 98
32269, V, 1, 1, 1, 1, 0, 700, 98
32270, V, 1, 1, 1, 1, 0, 700, 98
32271, V, 1, 1, 1, 1, 0, 700, 98
32272, V, 1, 1, 1, 1, 0, 700, 98
32273, V, 1, 1, 1, 1, 0, 700, 98
32274, V, 1, 1, 1, 1, 0, 700, 98
32275, V, 1, 1, 1, 1, 0, 700, 98
32276, V, 1, 1, 1, 1, 0, 700, 98
32277, V, 1, 1, 1, 1, 0, 700, 98
32278, V, 1, 1, 1, 1, 0, 700, 98
32279, V, 1, 1, 1, 1, 0, 700, 98
32280, V, 1, 1, 1, 1, 0, 700, 98
32281, V, 1, 1, 1, 1, 0, 700, 98
32282, V, 1, 1, 1, 1, 0, 700, 98
32283, V, 1, 1, 1, 1, 0, 700, 98
32284, V, 1, 1, 1, 1, 0, 700, 98
32285, V, 1, 1, 1, 1, 0, 700, 98
32286, V, 1, 1, 1, 1, 0, 700, 98
32287, V, 1, 1, 1, 1, 0, 700, 98
32288, V, 1, 1, 1, 1, 0, 700, 98
32289, V, 1, 1, 1, 1, 0, 700, 98
32290, V, 1, 1, 1, 1, 0, 700, 98
32291, V, 1, 1, 1, 1, 0, 700, 98
32292, V, 1, 1, 1, 1, 0, 700, 98
32293, V, 1, 1, 1, 1, 0, 700, 98
32294, V, 1, 1, 1, 1, 0, 700, 98
32295, V, 1, 1, 1, 1, 0, 700, 98
32296, V, 1, 1, 1, 1, 0, 700, 98
32297, V, 1, 1, 1, 1, 0, 700, 98
32299, V, 1, 1, 1, 1, 0, 700, 98
32300, V, 1, 1, 1, 1, 0, 700, 98
32301, V, 1, 1, 1, 1, 0, 700, 98
32302, V, 1, 1, 1, 1, 0, 700, 98
32303, V, 1, 1, 1, 1, 0, 700, 98
32304, V, 1, 1, 1, 1, 0, 700, 98
32305, V, 1, 1, 1, 1, 0, 700, 98
32306, V, 1, 1, 1, 1, 0, 700, 98
32307, V, 1, 1, 1, 1, 0, 700, 98
32308, V, 1, 1, 1, 1, 0, 700, 98
32309, V, 1, 1, 1, 1, 0, 700, 98
32310, V, 1, 1, 1, 1, 0, 700, 98
32311, V, 1, 1, 1, 1, 0, 700, 98
32312, V, 1, 1, 1, 1, 0, 700, 98
32313, V, 1, 1, 1, 1, 0, 700, 98
32314, V, 1, 1, 1, 1, 0, 700, 98
32315, V, 1, 1, 1, 1, 0, 700, 98
32316, V, 1, 1, 1, 1, 0, 700, 98
32317, V, 1, 1, 1, 1, 0, 700, 98
32318, V, 1, 1, 1, 1, 0, 700, 98
32319, V, 1, 1, 1, 1, 0, 700, 98
32320, V, 1, 1, 1, 1, 0, 700, 98
32321, V, 1, 1, 1, 1, 0, 700, 98
32322, V, 1, 1, 1, 1, 0, 700, 98
32323, V, 1, 1, 1, 1, 0, 700, 98
32324, V, 1, 1, 1, 1, 0, 700, 98
32325, V, 1, 1, 1, 1, 0, 700, 98
32326, V, 1, 1, 1, 1, 0, 700, 98
32327, V, 1, 1, 1, 1, 0, 700, 98
32328, V, 1, 1, 1, 1, 0, 700, 98
32329, V, 1, 1, 1, 1, 0, 700, 98
32330, V, 1, 1, 1, 1, 0, 700, 98
32331, V, 1, 1, 1, 1, 0, 700, 98
32332, V, 1, 1, 1, 1, 0, 700, 98
32333, V, 1, 1, 1, 1, 0, 700, 98
32334, V, 1, 1, 1, 1, 0, 700, 98
32335, V, 1, 1, 1, 1, 0, 700, 98
32336, V, 1, 1, 1, 1, 0, 700, 98
32337, V, 1, 1, 1, 1, 0, 700, 98
32338, V, 1, 1, 1, 1, 0, 700, 98
32339, V, 1, 1, 1, 1, 0, 700, 98
32340, V, 1, 1, 1, 1, 0, 700, 98
32342, V, 1, 1, 1, 1, 0, 700, 98
32343, V, 1, 1, 1, 1, 0, 700, 98
32344, V, 1, 1, 1, 1, 0, 700, 98
32345, V, 1, 1, 1, 1, 0, 700, 98
32346, V, 1, 1, 1, 1, 0, 700, 98
32347, V, 1, 1, 1, 1, 0, 700, 98
32348, V, 1, 1, 1, 1, 0, 700, 98
32349, V, 1, 1, 1, 1, 0, 700, 98
32350, V, 1, 1, 1, 1, 0, 700, 98
32351, V, 1, 1, 1, 1, 0, 700, 98
32352, V, 1, 1, 1, 1, 0, 700, 98
32353, V, 1, 1, 1, 1, 0, 700, 98
32354, V, 1, 1, 1, 1, 0, 700, 98
32355, V, 1, 1, 1, 1, 0, 700, 98
32356, V, 1, 1, 1, 1, 0, 700, 98
32357, V, 1, 1, 1, 1, 0, 700, 98
32358, V, 1, 1, 1, 1, 0, 700, 98
32359, V, 1, 1, 1, 1, 0, 700, 98
32360, V, 1, 1, 1, 1, 0, 700, 98
32361, V, 1, 1, 1, 1, 0, 700, 98
32362, V, 1, 1, 1, 1, 0, 700, 98
32363, V, 1, 1, 1, 1, 0, 700, 98
32364, V, 1, 1, 1, 1, 0, 700, 98
32365, V, 1, 1, 1, 1, 0, 700, 98
32366, V, 1, 1, 1, 1, 0, 700, 98
32367, V, 1, 1, 1, 1, 0, 700, 98
32368, V, 1, 1, 1, 1, 0, 700, 98
32369, V, 1, 1, 1, 1, 0, 700, 98
32370, V, 1, 1, 1, 1, 0, 700, 98
32371, V, 1, 1, 1, 1, 0, 700, 98
32372, V, 1, 1, 1, 1, 0, 700, 98
32373, V, 1, 1, 1, 1, 0, 700, 98
32374, V, 1, 1, 1, 1, 0, 700, 98
32375, V, 1, 1, 1, 1, 0, 700, 98
32376, V, 1, 1, 1, 1, 0, 700, 98
32377, V, 1, 1, 1, 1, 0, 700, 98
32378, V, 1, 1, 1, 1, 0, 700, 98
32379, V, 1, 1, 1, 1, 0, 700, 98
32380, V, 1, 1, 1, 1, 0, 700, 98
32381, V, 1, 1, 1, 1, 0, 700, 98
32382, V, 1, 1, 1, 1, 0, 700, 98
32384, V, 1, 1, 1, 1, 0, 700, 98
32385, V, 1, 1, 1, 1, 0, 700, 98
32386, V, 1, 1, 1, 1, 0, 700, 98
32387, V, 1, 1, 1, 1, 0, 700, 98
32388, V, 1, 1, 1, 1, 0, 700, 98
32389, V, 1, 1, 1, 1, 0, 700, 98
32390, V, 1, 1, 1, 1, 0, 700, 98
32391, V, 1, 1, 1, 1, 0, 700, 98
32392, V, 1, 1, 1, 1, 0, 700, 98
32393, V, 1, 1, 1, 1, 0, 700, 98
32394, V, 1, 1, 1, 1, 0, 700, 98
32395, V, 1, 1, 1, 1, 0, 700, 98
32396, V, 1, 1, 1, 1, 0, 700, 98
32397, V, 1, 1, 1, 1, 0, 700, 98
32398, V, 1, 1, 1, 1, 0, 700, 98
32399, V, 1, 1, 1, 1, 0, 700, 98
32400, V, 1, 1, 1, 1, 0, 700, 98
32401, V, 1, 1, 1, 1, 0, 700, 98
32402, V, 1, 1, 1, 1, 0, 700, 98
32403, V, 1, 1, 1, 1, 0, 700, 98
32404, V, 1, 1, 1, 1, 0, 700, 98
32405, V, 1, 1, 1, 1, 0, 700, 98
32406, V, 1, 1, 1, 1, 0, 700, 98
32407, V, 1, 1, 1, 1, 0, 700, 98
32408, V, 1, 1, 1, 1, 0, 700, 98
32409, V, 1, 1, 1, 1, 0, 700, 98
32410, V, 1, 1, 1, 1, 0, 700, 98
32411, V, 1, 1, 1, 1, 0, 700, 98
32412, V, 1, 1, 1, 1, 0, 700, 98
32413, V, 1, 1, 1, 1, 0, 700, 98
32414, V, 1, 1, 1, 1, 0, 700, 98
32415, V, 1, 1, 1, 1, 0, 700, 98
32416, V, 1, 1, 1, 1, 0, 700, 98
32417, V, 1, 1, 1, 1, 0, 700, 98
32418, V, 1, 1, 1, 1, 0, 700, 98
32419, V, 1, 1, 1, 1, 0, 700, 98
32420, V, 1, 1, 1, 1, 0, 700, 98
32421, V, 1, 1, 1, 1, 0, 700, 98
32422, V, 1, 1, 1, 1, 0, 700, 98
32423, V, 1, 1, 1, 1, 0, 700, 98
32424, V, 1, 1, 1, 1, 0, 700, 98
32425, V, 1, 1, 1, 1, 0, 700, 98
32427, V, 1, 1, 1, 1, 0, 700, 98
32428, V, 1, 1, 1, 1, 0, 700, 98
32429, V, 1, 1, 1, 1, 0, 700, 98
32430, V, 1, 1, 1, 1, 0, 700, 98
32431, V, 1, 1, 1, 1, 0, 700, 98
32432, V, 1, 1, 1, 1, 0, 700, 98
32433, V, 1, 1, 1, 1, 0, 700, 98
32434, V, 1, 1, 1, 1, 0, 700, 98
32435, V, 1, 1, 1, 1, 0, 700, 98
32436, V, 1, 1, 1, 1, 0, 700, 98
32437, V, 1, 1, 1, 1, 0, 700, 98
32438, V, 1, 1, 1, 1, 0, 700, 98
32439, V, 1, 1, 1, 1, 0, 700, 98
32440, V, 1, 1, 1, 1, 0, 700, 98
32441, V, 1, 1, 1, 1, 0, 700, 98
32442, V, 1, 1, 1, 1, 0, 700, 98
32443, V, 1, 1, 1, 1, 0, 700, 98
32444, V, 1, 1, 1, 1, 0, 700, 98
32445, V, 1, 1, 1, 1, 0, 700, 98
32446, V, 1, 1, 1, 1, 0, 700, 98
32447, V, 1, 1, 1, 1, 0, 700, 98
32448, V, 1, 1, 1, 1, 0, 700, 98
32449, V, 1, 1, 1, 1, 0, 700, 98
32450, V, 1, 1, 1, 1, 0, 700, 98
32451, V, 1, 1, 1, 1, 0, 700, 98
32452, V, 1, 1, 1, 1, 0, 700, 98
32453, V, 1, 1, 1, 1, 0, 700, 98
32454, V, 1, 1, 1, 1, 0, 700, 98
32455, V, 1, 1, 1, 1, 0, 700, 98
32456, V, 1, 1, 1, 1, 0, 700, 98
32457, V, 1, 1, 1, 1, 0, 700, 98
32458, V, 1, 1, 1, 1, 0, 700, 98
32459, V, 1, 1, 1, 1, 0, 700, 98
32460, V, 1, 1, 1, 1, 0, 700, 98
32461, V, 1, 1, 1, 1, 0, 700, 98
32462, V, 1, 1, 1, 1, 0, 700, 98
32463, V, 1, 1, 1, 1, 0, 700, 98
32464, V, 1, 1, 1, 1, 0, 700, 98
32465, V, 1, 1, 1, 1, 0, 700, 98
32466, V, 1, 1, 1, 1, 0, 700, 98
32467, V, 1, 1, 1, 1, 0, 700, 98
32468, V, 1, 1, 1, 1, 0, 700, 98
32470, V, 1, 1, 1, 1, 0, 700, 98
32471, V, 1, 1, 1, 1, 0, 700, 98
32472, V, 1, 1, 1, 1, 0, 700, 98
32473, V, 1, 1, 1, 1, 0, 700, 98
32474, V, 1, 1, 1, 1, 0, 700, 98
32475, V, 1, 1, 1, 1, 0, 700, 98
32476, V, 1, 1, 1, 1, 0, 700, 98
32477, V, 1, 1, 1, 1, 0, 700, 98
32478, V, 1, 1, 1, 1, 0, 700, 98
32479, V, 1, 1, 1, 1, 0, 700, 98
32480, V, 1, 1, 1, 1, 0, 700, 98
32481, V, 1, 1, 1, 1, 0, 700, 98
32482, V, 1, 1, 1, 1, 0, 700, 98
32483, V, 1, 1, 1, 1, 0, 700, 98
32484, V, 1, 1, 1, 1, 0, 700, 98
32485, V, 1, 1, 1, 1, 0, 700, 98
32486, V, 1, 1, 1, 1, 0, 700, 98
32487, V, 1, 1, 1, 1, 0, 700, 98
32488, V, 1, 1, 1, 1, 0, 700, 98
32489, V, 1, 1, 1, 1, 0, 700, 98
32490, V, 1, 1, 1, 1, 0, 700, 98
32491, V, 1, 1, 1, 1, 0, 700, 98
32492, V, 1, 1, 1, 1, 0, 700, 98
32493, V, 1, 1, 1, 1, 0, 700, 98
32494, V, 1, 1, 1, 1, 0, 700, 98
32495, V, 1, 1, 1, 1, 0, 700, 98
32496, V, 1, 1, 1, 1, 0, 700, 98
32497, V, 1, 1, 1, 1, 0, 700, 98
32498, V, 1, 1, 1, 1, 0, 700, 98
32499, V, 1, 1, 1, 1, 0, 700, 98
32500, V, 1, 1, 1, 1, 0, 700, 98
32501, V, 1, 1, 1, 1, 0, 700, 98
32502, V, 1, 1, 1, 1, 0, 700, 98
32503, V, 1, 1, 1, 1, 0, 700, 98
32504, V, 1, 1, 1, 1, 0, 700, 98
32505, V, 1, 1, 1, 1, 0, 700, 98
32506, V, 1, 1, 1, 1, 0, 700, 98
32507, V, 1, 1, 1, 1, 0, 700, 98
32508, V, 1, 1, 1, 1, 0, 700, 98
32509, V, 1, 1, 1, 1, 0, 700, 98
32510, V, 1, 1, 1, 1, 0, 700, 98
32512, V, 1, 1, 1, 1, 0, 700, 98
32513, V, 1, 1, 1, 1, 0, 700, 98
32514, V, 1, 1, 1, 1, 0, 700, 98
32515, V, 1, 1, 1, 1, 0, 700, 98
32516, V, 1, 1, 1, 1, 0, 700, 98
32517, V, 1, 1, 1, 1, 0, 700, 98
32518, V, 1, 1, 1, 1, 0, 700, 98
32519, V, 1, 1, 1, 1, 0, 700, 98
32520, V, 1, 1, 1, 1, 0, 700, 98
32521, V, 1, 1, 1, 1, 0, 700, 98
32522, V, 1, 1, 1, 1, 0, 700, 98
32523, V, 1, 1, 1, 1, 0, 700, 98
32524, V, 1, 1, 1, 1, 0, 700, 98
32525, V, 1, 1, 1, 1, 0, 700, 98
32526, V, 1, 1, 1, 1, 0, 700, 98
32527, V, 1, 1, 1, 1, 0, 700, 98
32528, V, 1, 1, 1, 1, 0, 700, 98
32529, V, 1, 1, 1, 1, 0, 700, 98
32530, V, 1, 1, 1, 1, 0, 700, 98
32531, V, 1, 1, 1, 1, 0, 700, 98
32532, V, 1, 1, 1, 1, 0, 700, 98
32533, V, 1, 1, 1, 1, 0, 700, 98
32534, V, 1, 1, 1, 1, 0, 700, 98
32535, V, 1, 1, 1, 1, 0, 700, 98
32536, V, 1, 1, 1, 1, 0, 700, 98
32537, V, 1, 1, 1, 1, 0, 700, 98
32538, V, 1, 1, 1, 1, 0, 700, 98
32539, V, 1, 1, 1, 1, 0, 700, 98
32540, V, 1, 1, 1, 1, 0, 700, 98
32541, V, 1, 1, 1, 1, 0, 700, 98
32542, V, 1, 1, 1, 1, 0, 700, 98
32543, V, 1, 1, 1, 1, 0, 700, 98
32544, V, 1, 1, 1, 1, 0, 700, 98
32545, V, 1, 1, 1, 1, 0, 700, 98
32546, V, 1, 1, 1, 1, 0, 700, 98
32547, V, 1, 1, 1, 1, 0, 700, 98
32548, V, 1, 1, 1, 1, 0, 700, 98
32549, V, 1, 1, 1, 1, 0, 700, 98
32550, V, 1, 1, 1, 1, 0, 700, 98
32551, V, 1, 1, 1, 1, 0, 700, 98
32552, V, 1, 1, 1, 1, 0, 700, 98
32553, V, 1, 1, 1, 1, 0, 700, 98
32555, V, 1, 1, 1, 1, 0, 700, 98
32556, V, 1, 1, 1, 1, 0, 700, 98
32557, V, 1, 1, 1, 1, 0, 700, 98
32558, V, 1, 1, 1, 1, 0, 700, 98
32559, V, 1, 1, 1, 1, 0, 700, 98
32560, V, 1, 1, 1, 1, 0, 700, 98
32561, V, 1, 1, 1, 1, 0, 700, 98
32562, V, 1, 1, 1, 1, 0, 700, 98
32563, V, 1, 1, 1, 1, 0, 700, 98
32564, V, 1, 1, 1, 1, 0, 700, 98
32565, V, 1, 1, 1, 1, 0, 700, 98
32566, V, 1, 1, 1, 1, 0, 700, 98
32567, V, 1, 1, 1, 1, 0, 700, 98
32568, V, 1, 1, 1, 1, 0, 700, 98
32569, V, 1, 1, 1, 1, 0, 700, 98
32570, V, 1, 1, 1, 1, 0, 700, 98
32571, V, 1, 1, 1, 1, 0, 700, 98
32572, V, 1, 1, 1, 1, 0, 700, 98
32573, V, 1, 1, 1, 1, 0, 700, 98
32574, V, 1, 1, 1, 1, 0, 700, 98
32575, V, 1, 1, 1, 1, 0, 700, 98
32576, V, 1, 1, 1, 1, 0, 700, 98
32577, V, 1, 1, 1, 1, 0, 700, 98
32578, V, 1, 1, 1, 1, 0, 700, 98
32579, V, 1, 1, 1, 1, 0, 700, 98
32580, V, 1, 1, 1, 1, 0, 700, 98
32581, V, 1, 1, 1, 1, 0, 700, 98
32582, V, 1, 1, 1, 1, 0, 700, 98
32583, V, 1, 1, 1, 1, 0, 700, 98
32584, V, 1, 1, 1, 1, 0, 700, 98
32585, V, 1, 1, 1, 1, 0, 700, 98
32586, V, 1, 1, 1, 1, 0, 700, 98
32587, V, 1, 1, 1, 1, 0, 700, 98
32588, V, 1, 1, 1, 1, 0, 700, 98
32589, V, 1, 1, 1, 1, 0, 700, 98
32590, V, 1, 1, 1, 1, 0, 700, 98
32591, V, 1, 1, 1, 1, 0, 700, 98
32592, V, 1, 1, 1, 1, 0, 700, 98
32593, V, 1, 1, 1, 1, 0, 700, 98
32594, V, 1, 1, 1, 1, 0, 700, 98
32595, V, 1, 1, 1, 1, 0, 700, 98
32596, V, 1, 1, 1, 1, 0, 700, 98
32598, V, 1, 1, 1, 1, 0, 700, 98
32599, V, 1, 1, 1, 1, 0, 700, 98
32600, V, 1, 1, 1, 1, 0, 700, 98
32601, V, 1, 1, 1, 1, 0, 700, 98
32602, V, 1, 1, 1, 1, 0, 700, 98
32603, V, 1, 1, 1, 1, 0, 700, 98
32604, V, 1, 1, 1, 1, 0, 700, 98
32605, V, 1, 1, 1, 1, 0, 700, 98
32606, V, 1, 1, 1, 1, 0, 700, 98
32607, V, 1, 1, 1, 1, 0, 700, 98
32608, V, 1, 1, 1, 1, 0, 700, 98
32609, V, 1, 1, 1, 1, 0, 700, 98
32610, V, 1, 1, 1, 1, 0, 700, 98
32611, V, 1, 1, 1, 1, 0, 700, 98
32612, V, 1, 1, 1, 1, 0, 700, 98
32613, V, 1, 1, 1, 1, 0, 700, 98
32614, V, 1, 1, 1, 1, 0, 700, 98
32615, V, 1, 1, 1, 1, 0, 700, 98
32616, V, 1, 1, 1, 1, 0, 700, 98
32617, V, 1, 1, 1, 1, 0, 700, 98
32618, V, 1, 1, 1, 1, 0, 700, 98
32619, V, 1, 1, 1, 1, 0, 700, 98
32620, V, 1, 1, 1, 1, 0, 700, 98
32621, V, 1, 1, 1, 1, 0, 700, 98
32622, V, 1, 1, 1, 1, 0, 700, 98
32623, V, 1, 1, 1, 1, 0, 700, 98
32624, V, 1, 1, 1, 1, 0, 700, 98
32625, V, 1, 1, 1, 1, 0, 700, 98
32626, V, 1, 1, 1, 1, 0, 700, 98
32627, V, 1, 1, 1, 1, 0, 700, 98
32628, V, 1, 1, 1, 1, 0, 700, 98
32629, V, 1, 1, 1, 1, 0, 700, 98
32630, V, 1, 1, 1, 1, 0, 700, 98
32631, V, 1, 1, 1, 1, 0, 700, 98
32632, V, 1, 1, 1, 1, 0, 700, 98
32633, V, 1, 1, 1, 1, 0, 700, 98
32634, V, 1, 1, 1, 1, 0, 700, 98
32635, V, 1, 1, 1, 1, 0, 700, 98
32636, V, 1, 1, 1, 1, 0, 700, 98
32637, V, 1, 1, 1, 1, 0, 700, 98
32638, V, 1, 1, 1, 1, 0, 700, 98
32640, V, 1, 1, 1, 1, 0, 700, 98
32641, V, 1, 1, 1, 1, 0, 700, 98
32642, V, 1, 1, 1, 1, 0, 700, 98
32643, V, 1, 1, 1, 1, 0, 700, 98
32644, V, 1, 1, 1, 1, 0, 700, 98
32645, V, 1, 1, 1, 1, 0, 700, 98
32646, V, 1, 1, 1, 1, 0, 700, 98
32647, V, 1, 1, 1, 1, 0, 700, 98
32648, V, 1, 1, 1, 1, 0, 700, 98
32649, V, 1, 1, 1, 1, 0, 700, 98
32650, V, 1, 1, 1, 1, 0, 700, 98
32651, V, 1, 1, 1, 1, 0, 700, 98
32652, V, 1, 1, 1, 1, 0, 700, 98
32653, V, 1, 1, 1, 1, 0, 700, 98
32654, V, 1, 1, 1, 1, 0, 700, 98
32655, V, 1, 1, 1, 1, 0, 700, 98
32656, V, 1, 1, 1, 1, 0, 700, 98
32657, V, 1, 1, 1, 1, 0, 700, 98
32658, V, 1, 1, 1, 1, 0, 700, 98
32659, V, 1, 1, 1, 1, 0, 700, 98
32660, V, 1, 1, 1, 1, 0, 700, 98
32661, V, 1, 1, 1, 1, 0, 700, 98
32662, V, 1, 1, 1, 1, 0, 700, 98
32663, V, 1, 1, 1, 1, 0, 700, 98
32664, V, 1, 1, 1, 1, 0, 700, 98
32665, V, 1, 1, 1, 1, 0, 700, 98
32666, V, 1, 1, 1, 1, 0, 700, 98
32667, V, 1, 1, 1, 1, 0, 700, 98
32668, V, 1, 1, 1, 1, 0, 700, 98
32669, V, 1, 1, 1, 1, 0, 700, 98
32670, V, 1, 1, 1, 1, 0, 700, 98
32671, V, 1, 1, 1, 1, 0, 700, 98
32672, V, 1, 1, 1, 1, 0, 700, 98
32673, V, 1, 1, 1, 1, 0, 700, 98
32674, V, 1, 1, 1, 1, 0, 700, 98
32675, V, 1, 1, 1, 1, 0, 700, 98
32676, V, 1, 1, 1, 1, 0, 700, 98
32677, V, 1, 1, 1, 1, 0, 700, 98
32678, V, 1, 1, 1, 1, 0, 700, 98
32679, V, 1, 1, 1, 1, 0, 700, 98
32680, V, 1, 1, 1, 1, 0, 700, 98
32681, V, 1, 1, 1, 1, 0, 700, 98
32683, V, 1, 1, 1, 1, 0, 700, 98
32684, V, 1, 1, 1, 1, 0, 700, 98
32685, V, 1, 1, 1, 1, 0, 700, 98
32686, V, 1, 1, 1, 1, 0, 700, 98
32687, V, 1, 1, 1, 1, 0, 700, 98
32688, V, 1, 1, 1, 1, 0, 700, 98
32689, V, 1, 1, 1, 1, 0, 700, 98
32690, V, 1, 1, 1, 1, 0, 700, 98
32691, V, 1, 1, 1, 1, 0, 700, 98
32692, V, 1, 1, 1, 1, 0, 700, 98
32693, V, 1, 1, 1, 1, 0, 700, 98
32694, V, 1, 1, 1, 1, 0, 700, 98
32695, V, 1, 1, 1, 1, 0, 700, 98
32696, V, 1, 1, 1, 1, 0, 700, 98
32697, V, 1, 1, 1, 1, 0, 700, 98
32698, V, 1, 1, 1, 1, 0, 700, 98
32699, V, 1, 1, 1, 1, 0, 700, 98
32700, V, 1, 1, 1, 1, 0, 700, 98
32701, V, 1, 1, 1, 1, 0, 700, 98
32702, V, 1, 1, 1, 1, 0, 700, 98
32703, V, 1, 1, 1, 1, 0, 700, 98
32704, V, 1, 1, 1, 1, 0, 700, 98
32705, V, 1, 1, 1, 1, 0, 700, 98
32706, V, 1, 1, 1, 1, 0, 700, 98
32707, V, 1, 1, 1, 1, 0, 700, 98
32708, V, 1, 1, 1, 1, 0, 700, 98
32709, V, 1, 1, 1, 1, 0, 700, 98
32710, V, 1, 1, 1, 1, 0, 700, 98
32711, V, 1, 1, 1, 1, 0, 700, 98
32712, V, 1, 1, 1, 1, 0, 700, 98
32713, V, 1, 1, 1, 1, 0, 700, 98
32714, V, 1, 1, 1, 1, 0, 700, 98
32715, V, 1, 1, 1, 1, 0, 700, 98
32716, V, 1, 1, 1, 1, 0, 700, 98
32717, V, 1, 1, 1, 1, 0, 700, 98
32718, V, 1, 1, 1, 1, 0, 700, 98
32719, V, 1, 1, 1, 1, 0, 700, 98
32720, V, 1, 1, 1, 1, 0, 700, 98
32721, V, 1, 1, 1, 1, 0, 700, 98
32722, V, 1, 1, 1, 1, 0, 700, 98
32723, V, 1, 1, 1, 1, 0, 700, 98
32724, V, 1, 1, 1, 1, 0, 700, 98
32726, V, 1, 1, 1, 1, 0, 700, 98
32727, V, 1, 1, 1, 1, 0, 700, 98
32728, V, 1, 1, 1, 1, 0, 700, 98
32729, V, 1, 1, 1, 1, 0, 700, 98
32730, V, 1, 1, 1, 1, 0, 700, 98
32731, V, 1, 1, 1, 1, 0, 700, 98
32732, V, 1, 1, 1, 1, 0, 700, 98
32733, V, 1, 1, 1, 1, 0, 700, 98
32734, V, 1, 1, 1, 1, 0, 700, 98
32735, V, 1, 1, 1, 1, 0, 700, 98
32736, V, 1, 1, 1, 1, 0, 700, 98
32737, V, 1, 1, 1, 1, 0, 700, 98
32738, V, 1, 1, 1, 1, 0, 700, 98
32739, V, 1, 1, 1, 1, 0, 700, 98
32740, V, 1, 1, 1, 1, 0, 700, 98
32741, V, 1, 1, 1, 1, 0, 700, 98
32742, V, 1, 1, 1, 1, 0, 700, 98
32743, V, 1, 1, 1, 1, 0, 700, 98
32744, V, 1, 1, 1, 1, 0, 700, 98
32745, V, 1, 1, 1, 1, 0, 700, 98
32746, V, 1, 1, 1, 1, 0, 700, 98
32747, V, 1, 1, 1, 1, 0, 700, 98
32748, V, 1, 1, 1, 1, 0, 700, 98
32749, V, 1, 1, 1, 1, 0, 700, 98
32750, V, 1, 1, 1, 1, 0, 700, 98
32751, V, 1, 1, 1, 1, 0, 700, 98
32752, V, 1, 1, 1, 1, 0, 700, 98
32753, V, 1, 1, 1, 1, 0, 700, 98
32754, V, 1, 1, 1, 1, 0, 700, 98
32755, V, 1, 1, 1, 1, 0, 700, 98
32756, V, 1, 1, 1, 1, 0, 700, 98
32757, V, 1, 1, 1, 1, 0, 700, 98
32758, V, 1, 1, 1, 1, 0, 700, 98
32759, V, 1, 1, 1, 1, 0, 700, 98
32760, V, 1, 1, 1, 1, 0, 700, 98
32761, V, 1, 1, 1, 1, 0, 700, 98
32762, V, 1, 1, 1, 1, 0, 700, 98
32763, V, 1, 1, 1, 1, 0, 700, 98
32764, V, 1, 1, 1, 1, 0, 700, 98
32765, V, 1, 1, 1, 1, 0, 700, 98
32766, V, 1, 1, 1, 1, 0, 700, 98
32768, V, 1, 1, 1, 1, 0, 700, 98
32769, V, 1, 1, 1, 1, 0, 700, 98
32770, V, 1, 1, 1, 1, 0, 700, 98
32771, V, 1, 1, 1, 1, 0, 700, 98
32772, V, 1, 1, 1, 1, 0, 700, 98
32773, V, 1, 1, 1, 1, 0, 700, 98
32774, V, 1, 1, 1, 1, 0, 700, 98
32775, V, 1, 1, 1, 1, 0, 700, 98
32776, V, 1, 1, 1, 1, 0, 700, 98
32777, V, 1, 1, 1, 1, 0, 700, 98
32778, V, 1, 1, 1, 1, 0, 700, 98
32779, V, 1, 1, 1, 1, 0, 700, 98
32780, V, 1, 1, 1, 1, 0, 700, 98
32781, V, 1, 1, 1, 1, 0, 700, 98
32782, V, 1, 1, 1, 1, 0, 700, 98
32783, V, 1, 1, 1, 1, 0, 700, 98
32784, V, 1, 1, 1, 1, 0, 700, 98
32785, V, 1, 1, 1, 1, 0, 700, 98
32786, V, 1, 1, 1, 1, 0, 700, 98
32787, V, 1, 1, 1, 1, 0, 700, 98
32788, V, 1, 1, 1, 1, 0, 700, 98
32789, V, 1, 1, 1, 1, 0, 700, 98
32790, V, 1, 1, 1, 1, 0, 700, 98
32791, V, 1, 1, 1, 1, 0, 700, 98
32792, V, 1, 1, 1, 1, 0, 700, 98
32793, V, 1, 1, 1, 1, 0, 700, 98
32794, V, 1, 1, 1, 1, 0, 700, 98
32795, V, 1, 1, 1, 1, 0, 700, 98
32796, V, 1, 1, 1, 1, 0, 700, 98
32797, V, 1, 1, 1, 1, 0, 700, 98
32798, V, 1, 1, 1, 1, 0, 700, 98
32799, V, 1, 1, 1, 1, 0, 700, 98
32800, V, 1, 1, 1, 1, 0, 700, 98
32801, V, 1, 1, 1, 1, 0, 700, 98
32802, V, 1, 1, 1, 1, 0, 700, 98
32803, V, 1, 1, 1, 1, 0, 700, 98
32804, V, 1, 1, 1, 1, 0, 700, 98
32805, V, 1, 1, 1, 1, 0, 700, 98
32806, V, 1, 1, 1, 1, 0, 700, 98
32807, V, 1, 1, 1, 1, 0, 700, 98
32808, V, 1, 1, 1, 1, 0, 700, 98
32809, V, 1, 1, 1, 1, 0, 700, 98
32811, V, 1, 1, 1, 1, 0, 700, 98
32812, V, 1, 1, 1, 1, 0, 700, 98
32813, V, 1, 1, 1, 1, 0, 700, 98
32814, V, 1, 1, 1, 1, 0, 700, 98
32815, V, 1, 1, 1, 1, 0, 700, 98
32816, V, 1, 1, 1, 1, 0, 700, 98
32817, V, 1, 1, 1, 1, 0, 700, 98
32818, V, 1, 1, 1, 1, 0, 700, 98
32819, V, 1, 1, 1, 1, 0, 700, 98
32820, V, 1, 1, 1, 1, 0, 700, 98
32821, V, 1, 1, 1, 1, 0, 700, 98
32822, V, 1, 1, 1, 1, 0, 700, 98
32823, V, 1, 1, 1, 1, 0, 700, 98
32824, V, 1, 1, 1, 1, 0, 700, 98
32825, V, 1, 1, 1, 1, 0, 700, 98
32826, V, 1, 1, 1, 1, 0, 700, 98
32827, V, 1, 1, 1, 1, 0, 700, 98
32828, V, 1, 1, 1, 1, 0, 700, 98
32829, V, 1, 1, 1, 1, 0, 700, 98
32830, V, 1, 1, 1, 1, 0, 700, 98
32831, V, 1, 1, 1, 1, 0, 700, 98
32832, V, 1, 1, 1, 1, 0, 700, 98
32833, V, 1, 1, 1, 1, 0, 700, 98
32834, V, 1, 1, 1, 1, 0, 700, 98
32835, V, 1, 1, 1, 1, 0, 700, 98
32836, V, 1, 1, 1, 1, 0, 700, 98
32837, V, 1, 1, 1, 1, 0, 700, 98
32838, V, 1, 1, 1, 1, 0, 700, 98
32839, V, 1, 1, 1, 1, 0, 700, 98
32840, V, 1, 1, 1, 1, 0, 700, 98
32841, V, 1, 1, 1, 1, 0, 700, 98
32842, V, 1, 1, 1, 1, 0, 700, 98
32843, V, 1, 1, 1, 1, 0, 700, 98
32844, V, 1, 1, 1, 1, 0, 700, 98
32845, V, 1, 1, 1, 1, 0, 700, 98
32846, V, 1, 1, 1, 1, 0, 700, 98
32847, V, 1, 1, 1, 1, 0, 700, 98
32848, V, 1, 1, 1, 1, 0, 700, 98
32849, V, 1, 1, 1, 1, 0, 700, 98
32850, V, 1, 1, 1, 1, 0, 700, 98
32851, V, 1, 1, 1, 1, 0, 700, 98
32852, V, 1, 1, 1, 1, 0, 700, 98
32854, V, 1, 1, 1, 1, 0, 700, 98
32855, V, 1, 1, 1, 1, 0, 700, 98
32856, V, 1, 1, 1, 1, 0, 700, 98
32857, V, 1, 1, 1, 1, 0, 700, 98
32858, V, 1, 1, 1, 1, 0, 700, 98
32859, V, 1, 1, 1, 1, 0, 700, 98
32860, V, 1, 1, 1, 1, 0, 700, 98
32861, V, 1, 1, 1, 1, 0, 700, 98
32862, V, 1, 1, 1, 1, 0, 700, 98
32863, V, 1, 1, 1, 1, 0, 700, 98
32864, V, 1, 1, 1, 1, 0, 700, 98
32865, V, 1, 1, 1, 1, 0, 700, 98
32866, V, 1, 1, 1, 1, 0, 700, 98
32867, V, 1, 1, 1, 1, 0, 700, 98
32868, V, 1, 1, 1, 1, 0, 700, 98
32869, V, 1, 1, 1, 1, 0, 700, 98
32870, V, 1, 1, 1, 1, 0, 700, 98
32871, V, 1, 1, 1, 1, 0, 700, 98
32872, V, 1, 1, 1, 1, 0, 700, 98
32873, V, 1, 1, 1, 1, 0, 700, 98
32874, V, 1, 1, 1, 1, 0, 700, 98
32875, V, 1, 1, 1, 1, 0, 700, 98
32876, V, 1, 1, 1, 1, 0, 700, 98
32877, V, 1, 1, 1, 1, 0, 700, 98
32878, V, 1, 1, 1, 1, 0, 700, 98
32879, V, 1, 1, 1, 1, 0, 700, 98
32880, V, 1, 1, 1, 1, 0, 700, 98
32881, V, 1, 1, 1, 1, 0, 700, 98
32882, V, 1, 1, 1, 1, 0, 700, 98
32883, V, 1, 1, 1, 1, 0, 700, 98
32884, V, 1, 1, 1, 1, 0, 700, 98
32885, V, 1, 1, 1, 1, 0, 700, 98
32886, V, 1, 1, 1, 1, 0, 700, 98
32887, V, 1, 1, 1, 1, 0, 700, 98
32888, V, 1, 1, 1, 1, 0, 700, 98
32889, V, 1, 1, 1, 1, 0, 700, 98
32890, V, 1, 1, 1, 1, 0, 700, 98
32891, V, 1, 1, 1, 1, 0, 700, 98
32892, V, 1, 1, 1, 1, 0, 700, 98
32893, V, 1, 1, 1, 1, 0, 700, 98
32894, V, 1, 1, 1, 1, 0, 700, 98
32896, V, 1, 1, 1, 1, 0, 700, 98
32897, V, 1, 1, 1, 1, 0, 700, 98
32898, V, 1, 1, 1, 1, 0, 700, 98
32899, V, 1, 1, 1, 1, 0, 700, 98
32900, V, 1, 1, 1, 1, 0, 700, 98
32901, V, 1, 1, 1, 1, 0, 700, 98
32902, V, 1, 1, 1, 1, 0, 700, 98
32903, V, 1, 1, 1, 1, 0, 700, 98
32904, V, 1, 1, 1, 1, 0, 700, 98
32905, V, 1, 1, 1, 1, 0, 700, 98
32906, V, 1, 1, 1, 1, 0, 700, 98
32907, V, 1, 1, 1, 1, 0, 700, 98
32908, V, 1, 1, 1, 1, 0, 700, 98
32909, V, 1, 1, 1, 1, 0, 700, 98
32910, V, 1, 1, 1, 1, 0, 700, 98
32911, V, 1, 1, 1, 1, 0, 700, 98
32912, V, 1, 1, 1, 1, 0, 700, 98
32913, V, 1, 1, 1, 1, 0, 700, 98
32914, V, 1, 1, 1, 1, 0, 700, 98
32915, V, 1, 1, 1, 1, 0, 700, 98
32916, V, 1, 1, 1, 1, 0, 700, 98
32917, V, 1, 1, 1, 1, 0, 700, 98
32918, V, 1, 1, 1, 1, 0, 700, 98
32919, V, 1, 1, 1, 1, 0, 700, 98
32920, V, 1, 1, 1, 1, 0, 700, 98
32921, V, 1, 1, 1, 1, 0, 700, 98
32922, V, 1, 1, 1, 1, 0, 700, 98
32923, V, 1, 1, 1, 1, 0, 700, 98
32924, V, 1, 1, 1, 1, 0, 700, 98
32925, V, 1, 1, 1, 1, 0, 700, 98
32926, V, 1, 1, 1, 1, 0, 700, 98
32927, V, 1, 1, 1, 1, 0, 700, 98
32928, V, 1, 1, 1, 1, 0, 700, 98
32929, V, 1, 1, 1, 1, 0, 700, 98
32930, V, 1, 1, 1, 1, 0, 700, 98
32931, V, 1, 1, 1, 1, 0, 700, 98
32932, V, 1, 1, 1, 1, 0, 700, 98
32933, V, 1, 1, 1, 1, 0, 700, 98
32934, V, 1, 1, 1, 1, 0, 700, 98
32935, V, 1, 1, 1, 1, 0, 700, 98
32936, V, 1, 1, 1, 1, 0, 700, 98
32937, V, 1, 1, 1, 1, 0, 700, 98
32939, V, 1, 1, 1, 1, 0, 700, 98
32940, V, 1, 1, 1, 1, 0, 700, 98
32941, V, 1, 1, 1, 1, 0, 700, 98
32942, V, 1, 1, 1, 1, 0, 700, 98
32943, V, 1, 1, 1, 1, 0, 700, 98
32944, V, 1, 1, 1, 1, 0, 700, 98
32945, V, 1, 1, 1, 1, 0, 700, 98
32946, V, 1, 1, 1, 1, 0, 700, 98
32947, V, 1, 1, 1, 1, 0, 700, 98
32948, V, 1, 1, 1, 1, 0, 700, 98
32949, V, 1, 1, 1, 1, 0, 700, 98
32950, V, 1, 1, 1, 1, 0, 700, 98
32951, V, 1, 1, 1, 1, 0, 700, 98
32952, V, 1, 1, 1, 1, 0, 700, 98
32953, V, 1, 1, 1, 1, 0, 700, 98
32954, V, 1, 1, 1, 1, 0, 700, 98
32955, V, 1, 1, 1, 1, 0, 700, 98
32956, V, 1, 1, 1, 1, 0, 700, 98
32957, V, 1, 1, 1, 1, 0, 700, 98
32958, V, 1, 1, 1, 1, 0, 700, 98
32959, V, 1, 1, 1, 1, 0, 700, 98
32960, V, 1, 1, 1, 1, 0, 700, 98
32961, V, 1, 1, 1, 1, 0, 700, 98
32962, V, 1, 1, 1, 1, 0, 700, 98
32963, V, 1, 1, 1, 1, 0, 700, 98
32964, V, 1, 1, 1, 1, 0, 700, 98
32965, V, 1, 1, 1, 1, 0, 700, 98
32966, V, 1, 1, 1, 1, 0, 700, 98
32967, V, 1, 1, 1, 1, 0, 700, 98
32968, V, 1, 1, 1, 1, 0, 700, 98
32969, V, 1, 1, 1, 1, 0, 700, 98
32970, V, 1, 1, 1, 1, 0, 700, 98
32971, V, 1, 1, 1, 1, 0, 700, 98
32972, V, 1, 1, 1, 1, 0, 700, 98
32973, V, 1, 1, 1, 1, 0, 700, 98
32974, V, 1, 1, 1, 1, 0, 700, 98
32975, V, 1, 1, 1, 1, 0, 700, 98
32976, V, 1, 1, 1, 1, 0, 700, 98
32977, V, 1, 1, 1, 1, 0, 700, 98
32978, V, 1, 1, 1, 1, 0, 700, 98
32979, V, 1, 1, 1, 1, 0, 700, 98
32980, V, 1, 1, 1, 1, 0, 700, 98
32982, V, 1, 1, 1, 1, 0, 700, 98
32983, V, 1, 1, 1, 1, 0, 700, 98
32984, V, 1, 1, 1, 1, 0, 700, 98
32985, V, 1, 1, 1, 1, 0, 700, 98
32986, V, 1, 1, 1, 1, 0, 700, 98
32987, V, 1, 1, 1, 1, 0, 700, 98
32988, V, 1, 1, 1, 1, 0, 700, 98
32989, V, 1, 1, 1, 1, 0, 700, 98
32990, V, 1, 1, 1, 1, 0, 700, 98
32991, V, 1, 1, 1, 1, 0, 700, 98
32992, V, 1, 1, 1, 1, 0, 700, 98
32993, V, 1, 1, 1, 1, 0, 700, 98
32994, V, 1, 1, 1, 1, 0, 700, 98
32995, V, 1, 1, 1, 1, 0, 700, 98
32996, V, 1, 1, 1, 1, 0, 700, 98
32997, V, 1, 1, 1, 1, 0, 700, 98
32998, V, 1, 1, 1, 1, 0, 700, 98
32999, V, 1, 1, 1, 1, 0, 700, 98
33000, V, 1, 1, 1, 1, 0, 700, 98
33001, V, 1, 1, 1, 1, 0, 700, 98
33002, V, 1, 1, 1, 1, 0, 700, 98
33003, V, 1, 1, 1, 1, 0, 700, 98
33004, V, 1, 1, 1, 1, 0, 700, 98
33005, V, 1, 1, 1, 1, 0, 700, 98
33006, V, 1, 1, 1, 1, 0, 700, 98
33007, V, 1, 1, 1, 1, 0, 700, 98
33008, V, 1, 1, 1, 1, 0, 700, 98
33009, V, 1, 1, 1, 1, 0, 700, 98
33010, V, 1, 1, 1, 1, 0, 700, 98
33011, V, 1, 1, 1, 1, 0, 700, 98
33012, V, 1, 1, 1, 1, 0, 700, 98
33013, V, 1, 1, 1, 1, 0, 700, 98
33014, V, 1, 1, 1, 1, 0, 700, 98
33015, V, 1, 1, 1, 1, 0, 700, 98
33016, V, 1, 1, 1, 1, 0, 700, 98
33017, V, 1, 1, 1, 1, 0, 700, 98
33018, V, 1, 1, 1, 1, 0, 700, 98
33019, V, 1, 1, 1, 1, 0, 700, 98
33020, V, 1, 1, 1, 1, 0, 700, 98
33021, V, 1, 1, 1, 1, 0, 700, 98
33022, V, 1, 1, 1, 1, 0, 700, 98
33024, V, 1, 1, 1, 1, 0, 700, 98
33025, V, 1, 1, 1, 1, 0, 700, 98
33026, V, 1, 1, 1, 1, 0, 700, 98
33027, V, 1, 1, 1, 1, 0, 700, 98
33028, V, 1, 1, 1, 1, 0, 700, 98
33029, V, 1, 1, 1, 1, 0, 700, 98
33030, V, 1, 1, 1, 1, 0, 700, 98
33031, V, 1, 1, 1, 1, 0, 700, 98
33032, V, 1, 1, 1, 1, 0, 700, 98
33033, V, 1, 1, 1, 1, 0, 700, 98
33034, V, 1, 1, 1, 1, 0, 700, 98
33035, V, 1, 1, 1, 1, 0, 700, 98
33036, V, 1, 1, 1, 1, 0, 700, 98
33037, V, 1, 1, 1, 1, 0, 700, 98
33038, V, 1, 1, 1, 1, 0, 700, 98
33039, V, 1, 1, 1, 1, 0, 700, 98
33040, V, 1, 1, 1, 1, 0, 700, 98
33041, V, 1, 1, 1, 1, 0, 700, 98
33042, V, 1, 1, 1, 1, 0, 700, 98
33043, V, 1, 1, 1, 1, 0, 700, 98
33044, V, 1, 1, 1, 1, 0, 700, 98
33045, V, 1, 1, 1, 1, 0, 700, 98
33046, V, 1, 1, 1, 1, 0, 700, 98
33047, V, 1, 1, 1, 1, 0, 700, 98
33048, V, 1, 1, 1, 1, 0, 700, 98
33049, V, 1, 1, 1, 1, 0, 700, 98
33050, V, 1, 1, 1, 1, 0, 700, 98
33051, V, 1, 1, 1, 1, 0, 700, 98
33052, V, 1, 1, 1, 1, 0, 700, 98
33053, V, 1, 1, 1, 1, 0, 700, 98
33054, V, 1, 1, 1, 1, 0, 700, 98
33055, V, 1, 1, 1, 1, 0, 700, 98
33056, V, 1, 1, 1, 1, 0, 700, 98
33057, V, 1, 1, 1, 1, 0, 700, 98
33058, V, 1, 1, 1, 1, 0, 700, 98
33059, V, 1, 1, 1, 1, 0, 700, 98
33060, V, 1, 1, 1, 1, 0, 700, 98
33061, V, 1, 1, 1, 1, 0, 700, 98
33062, V, 1, 1, 1, 1, 0, 700, 98
33063, V, 1, 1, 1, 1, 0, 700, 98
33064, V, 1, 1, 1, 1, 0, 700, 98
33065, V, 1, 1, 1, 1, 0, 700, 98
33067, V, 1, 1, 1, 1, 0, 700, 98
33068, V, 1, 1, 1, 1, 0, 700, 98
33069, V, 1, 1, 1, 1, 0, 700, 98
33070, V, 1, 1, 1, 1, 0, 700, 98
33071, V, 1, 1, 1, 1, 0, 700, 98
33072, V, 1, 1, 1, 1, 0, 700, 98
33073, V, 1, 1, 1, 1, 0, 700, 98
33074, V, 1, 1, 1, 1, 0, 700, 98
33075, V, 1, 1, 1, 1, 0, 700, 98
33076, V, 1, 1, 1, 1, 0, 700, 98
33077, V, 1, 1, 1, 1, 0, 700, 98
33078, V, 1, 1, 1, 1, 0, 700, 98
33079, V, 1, 1, 1, 1, 0, 700, 98
33080, V, 1, 1, 1, 1, 0, 700, 98
33081, V, 1, 1, 1, 1, 0, 700, 98
33082, V, 1, 1, 1, 1, 0, 700, 98
33083, V, 1, 1, 1, 1, 0, 700, 98
33084, V, 1, 1, 1, 1, 0, 700, 98
33085, V, 1, 1, 1, 1, 0, 700, 98
33086, V, 1, 1, 1, 1, 0, 700, 98
33087, V, 1, 1, 1, 1, 0, 700, 98
33088, V, 1, 1, 1, 1, 0, 700, 98
33089, V, 1, 1, 1, 1, 0, 700, 98
33090, V, 1, 1, 1, 1, 0, 700, 98
33091, V, 1, 1, 1, 1, 0, 700, 98
33092, V, 1, 1, 1, 1, 0, 700, 98
33093, V, 1, 1, 1, 1, 0, 700, 98
33094, V, 1, 1, 1, 1, 0, 700, 98
33095, V, 1, 1, 1, 1, 0, 700, 98
33096, V, 1, 1, 1, 1, 0, 700, 98
33097, V, 1, 1, 1, 1, 0, 700, 98
33098, V, 1, 1, 1, 1, 0, 700, 98
33099, V, 1, 1, 1, 1, 0, 700, 98
33100, V, 1, 1, 1, 1, 0, 700, 98
33101, V, 1, 1, 1, 1, 0, 700, 98
33102, V, 1, 1, 1, 1, 0, 700, 98
33103, V, 1, 1, 1, 1, 0, 700, 98
33104, V, 1, 1, 1, 1, 0, 700, 98
33105, V, 1, 1, 1, 1, 0, 700, 98
33106, V, 1, 1, 1, 1, 0, 700, 98
33107, V, 1, 1, 1, 1, 0, 700, 98
33108, V, 1, 1, 1, 1, 0, 700, 98
33110, V, 1, 1, 1, 1, 0, 700, 98
33111, V, 1, 1, 1, 1, 0, 700, 98
33112, V, 1, 1, 1, 1, 0, 700, 98
33113, V, 1, 1, 1, 1, 0, 700, 98
33114, V, 1, 1, 1, 1, 0, 700, 98
33115, V, 1, 1, 1, 1, 0, 700, 98
33116, V, 1, 1, 1, 1, 0, 700, 98
33117, V, 1, 1, 1, 1, 0, 700, 98
33118, V, 1, 1, 1, 1, 0, 700, 98
33119, V, 1, 1, 1, 1, 0, 700, 98
33120, V, 1, 1, 1, 1, 0, 700, 98
33121, V, 1, 1, 1, 1, 0, 700, 98
33122, V, 1, 1, 1, 1, 0, 700, 98
33123, V, 1, 1, 1, 1, 0, 700, 98
33124, V, 1, 1, 1, 1, 0, 700, 98
33125, V, 1, 1, 1, 1, 0, 700, 98
33126, V, 1, 1, 1, 1, 0, 700, 98
33127, V, 1, 1, 1, 1, 0, 700, 98
33128, V, 1, 1, 1, 1, 0, 700, 98
33129, V, 1, 1, 1, 1, 0, 700, 98
33130, V, 1, 1, 1, 1, 0, 700, 98
33131, V, 1, 1, 1, 1, 0, 700, 98
33132, V, 1, 1, 1, 1, 0, 700, 98
33133, V, 1, 1, 1, 1, 0, 700, 98
33134, V, 1, 1, 1, 1, 0, 700, 98
33135, V, 1, 1, 1, 1, 0, 700, 98
33136, V, 1, 1, 1, 1, 0, 700, 98
33137, V, 1, 1, 1, 1, 0, 700, 98
33138, V, 1, 1, 1, 1, 0, 700, 98
33139, V, 1, 1, 1, 1, 0, 700, 98
33140, V, 1, 1, 1, 1, 0, 700, 98
33141, V, 1, 1, 1, 1, 0, 700, 98
33142, V, 1, 1, 1, 1, 0, 700, 98
33143, V, 1, 1, 1, 1, 0, 700, 98
33144, V, 1, 1, 1, 1, 0, 700, 98
33145, V, 1, 1, 1, 1, 0, 700, 98
33146, V, 1, 1, 1, 1, 0, 700, 98
33147, V, 1, 1, 1, 1, 0, 700, 98
33148, V, 1, 1, 1, 1, 0, 700, 98
33149, V, 1, 1, 1, 1, 0, 700, 98
33150, V, 1, 1, 1, 1, 0, 700, 98
33152, V, 1, 1, 1, 1, 0, 700, 98
33153, V, 1, 1, 1, 1, 0, 700, 98
33154, V, 1, 1, 1, 1, 0, 700, 98
33155, V, 1, 1, 1, 1, 0, 700, 98
33156, V, 1, 1, 1, 1, 0, 700, 98
33157, V, 1, 1, 1, 1, 0, 700, 98
33158, V, 1, 1, 1, 1, 0, 700, 98
33159, V, 1, 1, 1, 1, 0, 700, 98
33160, V, 1, 0, 0, 1, 0, 700, 98
33160, V, 1, 0, 0, 0, 0, 700, 98
33161, V, 1, 1, 0, 0, 0, 700, 98
33161, V, 1, 1, 0, 0, 0, 700, 98
33162, V, 1, 1, 1, 1, 0, 700, 98
33163, V, 1, 1, 1, 1, 0, 700, 98
33164, V, 1, 1, 1, 1, 0, 700, 98
33165, V, 1, 1, 1, 1, 0, 700, 98
33166, V, 1, 1, 1, 1, 0, 700, 98
33167, V, 1, 1, 1, 1, 0, 700, 98
33168, V, 1, 1, 1, 1, 0, 700, 98
33169, V, 1, 1, 1, 1, 0, 700, 98
33170, V, 1, 1, 1, 1, 0, 700, 98
33171, V, 1, 1, 1, 1, 0, 700, 98
33172, V, 1, 1, 1, 1, 0, 700, 98
33173, V, 1, 1, 1, 1, 0, 700, 98
33174, V, 1, 1, 1, 1, 0, 700, 98
33175, V, 1, 1, 1, 1, 0, 700, 98
33176, V, 1, 1, 1, 1, 0, 700, 98
33177, V, 1, 1, 1, 1, 0, 700, 98
33178, V, 1, 1, 1, 1, 0, 700, 98
33179, V, 1, 1, 1, 1, 0, 700, 98
33180, V, 1, 1, 1, 1, 0, 700, 98
33181, V, 1, 1, 1, 1, 0, 700, 98
33182, V, 1, 1, 1, 1, 0, 700, 98
33183, V, 1, 1, 1, 1, 0, 700, 98
33184, V, 1, 1, 1, 1, 0, 700, 98
33185, V, 1, 1, 1, 1, 0, 700, 98
33186, V, 1, 1, 1, 1, 0, 700, 98
33187, V, 1, 1, 1, 1, 0, 700, 98
33188, V, 1, 1, 1, 1, 0, 700, 98
33189, V, 1, 1, 1, 1, 0, 700, 98
33190, V, 1, 1, 1, 1, 0, 700, 98
33191, V, 1, 1, 1, 1, 0, 700, 98
33192, V, 1, 1, 1, 1, 0, 700, 98
33193, V, 1, 1, 1, 1, 0, 700, 98
33195, V, 1, 1, 1, 1, 0, 700, 98
33196, V, 1, 1, 1, 1, 0, 700, 98
33197, V, 1, 1, 1, 1, 0, 700, 98
33198, V, 1, 1, 1, 1, 0, 700, 98
33199, V, 1, 1, 1, 1, 0, 700, 98
33200, V, 1, 1, 1, 1, 0, 700, 98
33201, V, 1, 1, 1, 1, 0, 700, 98
33202, V, 1, 1, 1, 1, 0, 700, 98
33203, V, 1, 1, 1, 1, 0, 700, 98
33204, V, 1, 1, 1, 1, 0, 700, 98
33205, V, 1, 1, 1, 1, 0, 700, 98
33206, V, 1, 1, 1, 1, 0, 700, 98
33207, V, 1, 1, 1, 1, 0, 700, 98
33208, V, 1, 1, 1, 1, 0, 700, 98
33209, V, 1, 1, 1, 1, 0, 700, 98
33210, V, 1, 1, 1, 1, 0, 700, 98
33211, V, 1, 1, 1, 1, 0, 700, 98
33212, V, 1, 1, 1, 1, 0, 700, 98
33213, V, 1, 1, 1, 1, 0, 700, 98
33214, V, 1, 1, 1, 1, 0, 700, 98
33215, V, 1, 1, 1, 1, 0, 700, 98
33216, V, 1, 1, 1, 1, 0, 700, 98
33217, V, 1, 1, 1, 1, 0, 700, 98
33218, V, 1, 1, 1, 1, 0, 700, 98
33219, V, 1, 1, 1, 1, 0, 700, 98
33220, V, 1, 1, 1, 1, 0, 700, 98
33221, V, 1, 1, 1, 1, 0, 700, 98
33222, V, 1, 1, 1, 1, 0, 700, 98
33223, V, 1, 1, 1, 1, 0, 700, 98
33224, V, 1, 1, 1, 1, 0, 700, 98
33225, V, 1, 1, 1, 1, 0, 700, 98
33226, V, 1, 1, 1, 1, 0, 700, 98
33227, V, 1, 1, 1, 1, 0, 700, 98
33228, V, 1, 1, 1, 1, 0, 700, 98
33229, V, 1, 1, 1, 1, 0, 700, 98
33230, V, 1, 1, 1, 1, 0, 700, 98
33231, V, 1, 1, 1, 1, 0, 700, 98
33232, V, 1, 1, 1, 1, 0, 700, 98
33233, V, 1, 1, 1, 1, 0, 700, 98
33234, V, 1, 1, 1, 1, 0, 700, 98
33235, V, 1, 1, 1, 1, 0, 700, 98
33236, V, 1, 1, 1, 1, 0, 700, 98
33238, V, 1, 1, 1, 1, 0, 700, 98
33239, V, 1, 1, 1, 1, 0, 700, 98
33240, V, 1, 1, 1, 1, 0, 700, 98
33241, V, 1, 1, 1, 1, 0, 700, 98
33242, V, 1, 1, 1, 1, 0, 700, 98
33243, V, 1, 1, 1, 1, 0, 700, 98
33244, V, 1, 1, 1, 1, 0, 700, 98
33245, V, 1, 1, 1, 1, 0, 700, 98
33246, V, 1, 1, 1, 1, 0, 700, 98
33247, V, 1, 1, 1, 1, 0, 700, 98
33248, V, 1, 1, 1, 1, 0, 700, 98
33249, V, 1, 1, 1, 1, 0, 700, 98
33250, V, 1, 1, 1, 1, 0, 700, 98
33251, V, 1, 1, 1, 1, 0, 700, 98
33252, V, 1, 1, 1, 1, 0, 700, 98
33253, V, 1, 1, 1, 1, 0, 700, 98
33254, V, 1, 1, 1, 1, 0, 700, 98
33255, V, 1, 1, 1, 1, 0, 700, 98
33256, V, 1, 1, 1, 1, 0, 700, 98
33257, V, 1, 1, 1, 1, 0, 700, 98
33258, V, 1, 1, 1, 1, 0, 700, 98
33259, V, 1, 1, 1, 1, 0, 700, 98
33260, V, 1, 1, 1, 1, 0, 700, 98
33261, V, 1, 1, 1, 1, 0, 700, 98
33262, V, 1, 1, 1, 1, 0, 700, 98
33263, V, 1, 1, 1, 1, 0, 700, 98
33264, V, 1, 1, 1, 1, 0, 700, 98
33265, V, 1, 1, 1, 1, 0, 700, 98
33266, V, 1, 1, 1, 1, 0, 700, 98
33267, V, 1, 1, 1, 1, 0, 700, 98
33268, V, 1, 1, 1, 1, 0, 700, 98
33269, V, 1, 1, 1, 1, 0, 700, 98
33270, V, 1, 1, 1, 1, 0, 700, 98
33271, V, 1, 1, 1, 1, 0, 700, 98
33272, V, 1, 1, 1, 1, 0, 700, 98
33273, V, 1, 1, 1, 1, 0, 700, 98
33274, V, 1, 1, 1, 1, 0, 700, 98
33275, V, 1, 1, 1, 1, 0, 700, 98
33276, V, 1, 1, 1, 1, 0, 700, 98
33277, V, 1, 1, 1, 1, 0, 700, 98
33278, V, 1, 1, 1, 1, 0, 700, 98
33280, V, 1, 1, 1, 1, 0, 700, 98
33281, V, 1, 1, 1, 1, 0, 700, 98
33282, V, 1, 1, 1, 1, 0, 700, 98
33283, V, 1, 1, 1, 1, 0, 700, 98
33284, V, 1, 1, 1, 1, 0, 700, 98
33285, V, 1, 1, 1, 1, 0, 700, 98
33286, V, 1, 1, 1, 1, 0, 700, 98
33287, V, 1, 1, 1, 1, 0, 700, 98
33288, V, 1, 1, 1, 1, 0, 700, 98
33289, V, 1, 1, 1, 1, 0, 700, 98
33290, V, 1, 1, 1, 1, 0, 700, 98
33291, V, 1, 1, 1, 1, 0, 700, 98
33292, V, 1, 1, 1, 1, 0, 700, 98
33293, V, 1, 1, 1, 1, 0, 700, 98
33294, V, 1, 1, 1, 1, 0, 700, 98
33295, V, 1, 1, 1, 1, 0, 700, 98
33296, V, 1, 1, 1, 1, 0, 700, 98
33297, V, 1, 1, 1, 1, 0, 700, 98
33298, V, 1, 1, 1, 1, 0, 700, 98
33299, V, 1, 1, 1, 1, 0, 700, 98
33300, V, 1, 1, 1, 1, 0, 700, 98
33301, V, 1, 1, 1, 1, 0, 700, 98
33302, V, 1, 1, 1, 1, 0, 700, 98
33303, V, 1, 1, 1, 1, 0, 700, 98
33304, V, 1, 1, 1, 1, 0, 700, 98
33305, V, 1, 1, 1, 1, 0, 700, 98
33306, V, 1, 1, 1, 1, 0, 700, 98
33307, V, 1, 1, 1, 1, 0, 700, 98
33308, V, 1, 1, 1, 1, 0, 700, 98
33309, V, 1, 1, 1, 1, 0, 700, 98
33310, V, 1, 1, 1, 1, 0, 700, 98
33311, V, 1, 1, 1, 1, 0, 700, 98
33312, V, 1, 1, 1, 1, 0, 700, 98
33313, V, 1, 1, 1, 1, 0, 700, 98
33314, V, 1, 1, 1, 1, 0, 700, 98
33315, V, 1, 1, 1, 1, 0, 700, 98
33316, V, 1, 1, 1, 1, 0, 700, 98
33317, V, 1, 1, 1, 1, 0, 700, 98
33318, V, 1, 1, 1, 1, 0, 700, 98
33319, V, 1, 1, 1, 1, 0, 700, 98
33320, V, 1, 1, 1, 1, 0, 700, 98
33321, V, 1, 1, 1, 1, 0, 700, 98
33323, V, 1, 1, 1, 1, 0, 700, 98
33324, V, 1, 1, 1, 1, 0, 700, 98
33325, V, 1, 1, 1, 1, 0, 700, 98
33326, V, 1, 1, 1, 1, 0, 700, 98
33327, V, 1, 1, 1, 1, 0, 700, 98
33328, V, 1, 1, 1, 1, 0, 700, 98
33329, V, 1, 1, 1, 1, 0, 700, 98
33330, V, 1, 1, 1, 1, 0, 700, 98
33331, V, 1, 1, 1, 1, 0, 700, 98
33332, V, 1, 1, 1, 1, 0, 700, 98
33333, V, 1, 1, 1, 1, 0, 700, 98
33334, V, 1, 1, 1, 1, 0, 700, 98
33335, V, 1, 1, 1, 1, 0, 700, 98
33336, V, 1, 1, 1, 1, 0, 700, 98
33337, V, 1, 1, 1, 1, 0, 700, 98
33338, V, 1, 1, 1, 1, 0, 700, 98
33339, V, 1, 1, 1, 1, 0, 700, 98
33340, V, 1, 1, 1, 1, 0, 700, 98
33341, V, 1, 1, 1, 1, 0, 700, 98
33342, V, 1, 1, 1, 1, 0, 700, 98
33343, V, 1, 1, 1, 1, 0, 700, 98
33344, V, 1, 1, 1, 1, 0, 700, 98
33345, V, 1, 1, 1, 1, 0, 700, 98
33346, V, 1, 1, 1, 1, 0, 700, 98
33347, V, 1, 1, 1, 1, 0, 700, 98
33348, V, 1, 1, 1, 1, 0, 700, 98
33349, V, 1, 1, 1, 1, 0, 700, 98
33350, V, 1, 1, 1, 1, 0, 700, 98
33351, V, 1, 1, 1, 1, 0, 700, 98
33352, V, 1, 1, 1, 1, 0, 700, 98
33353, V, 1, 1, 1, 1, 0, 700, 98
33354, V, 1, 1, 1, 1, 0, 700, 98
33355, V, 1, 1, 1, 1, 0, 700, 98
33356, V, 1, 1, 1, 1, 0, 700, 98
33357, V, 1, 1, 1, 1, 0, 700, 98
33358, V, 1, 1, 1, 1, 0, 700, 98
33359, V, 1, 1, 1, 1, 0, 700, 98
33360, V, 1, 1, 1, 1, 0, 700, 98
33361, V, 1, 1, 1, 1, 0, 700, 98
33362, V, 1, 1, 1, 1, 0, 700, 98
33363, V, 1, 1, 1, 1, 0, 700, 98
33364, V, 1, 1, 1, 1, 0, 700, 98
33366, V, 1, 1, 1, 1, 0, 700, 98
33367, V, 1, 1, 1, 1, 0, 700, 98
33368, V, 1, 1, 1, 1, 0, 700, 98
33369, V, 1, 1, 1, 1, 0, 700, 98
33370, V, 1, 1, 1, 1, 0, 700, 98
33371, V, 1, 1, 1, 1, 0, 700, 98
33372, V, 1, 1, 1, 1, 0, 700, 98
33373, V, 1, 1, 1, 1, 0, 700, 98
33374, V, 1, 1, 1, 1, 0, 700, 98
33375, V, 1, 1, 1, 1, 0, 700, 98
33376, V, 1, 1, 1, 1, 0, 700, 98
33377, V, 1, 1, 1, 1, 0, 700, 98
33378, V, 1, 1, 1, 1, 0, 700, 98
33379, V, 1, 1, 1, 1, 0, 700, 98
33380, V, 1, 1, 1, 1, 0, 700, 98
33381, V, 1, 1, 1, 1, 0, 700, 98
33382, V, 1, 1, 1, 1, 0, 700, 98
33383, V, 1, 1, 1, 1, 0, 700, 98
33384, V, 1, 1, 1, 1, 0, 700, 98
33385, V, 1, 1, 1, 1, 0, 700, 98
33386, V, 1, 1, 1, 1, 0, 700, 98
33387, V, 1, 1, 1, 1, 0, 700, 98
33388, V, 1, 1, 1, 1, 0, 700, 98
33389, V, 1, 1, 1, 1, 0, 700, 98
33390, V, 1, 1, 1, 1, 0, 700, 98
33391, V, 1, 1, 1, 1, 0, 700, 98
33392, V, 1, 1, 1, 1, 0, 700, 98
33393, V, 1, 1, 1, 1, 0, 700, 98
33394, V, 1, 1, 1, 1, 0, 700, 98
33395, V, 1, 1, 1, 1, 0, 700, 98
33396, V, 1, 1, 1, 1, 0, 700, 98
33397, V, 1, 1, 1, 1, 0, 700, 98
33398, V, 1, 1, 1, 1, 0, 700, 98
33399, V, 1, 1, 1, 1, 0, 700, 98
33400, V, 1, 1, 1, 1, 0, 700, 98
33401, V, 1, 1, 1, 1, 0, 700, 98
33402, V, 1, 1, 1, 1, 0, 700, 98
33403, V, 1, 1, 1, 1, 0, 700, 98
33404, V, 1, 1, 1, 1, 0, 700, 98
33405, V, 1, 1, 1, 1, 0, 700, 98
33406, V, 1, 1, 1, 1, 0, 700, 98
33408, V, 1, 1, 1, 1, 0, 700, 98
33409, V, 1, 1, 1, 1, 0, 700, 98
33410, V, 1, 1, 1, 1, 0, 700, 98
33411, V, 1, 1, 1, 1, 0, 700, 98
33412, V, 1, 1, 1, 1, 0, 700, 98
33413, V, 1, 1, 1, 1, 0, 700, 98
33414, V, 1, 1, 1, 1, 0, 700, 98
33415, V, 1, 1, 1, 1, 0, 700, 98
33416, V, 1, 1, 1, 1, 0, 700, 98
33417, V, 1, 1, 1, 1, 0, 700, 98
33418, V, 1, 1, 1, 1, 0, 700, 98
33419, V, 1, 1, 1, 1, 0, 700, 98
33420, V, 1, 1, 1, 1, 0, 700, 98
33421, V, 1, 1, 1, 1, 0, 700, 98
33422, V, 1, 1, 1, 1, 0, 700, 98
33423, V, 1, 1, 1, 1, 0, 700, 98
33424, V, 1, 1, 1, 1, 0, 700, 98
33425, V, 1, 1, 1, 1, 0, 700, 98
33426, V, 1, 1, 1, 1, 0, 700, 98
33427, V, 1, 1, 1, 1, 0, 700, 98
33428, V, 1, 1, 1, 1, 0, 700, 98
33429, V, 1, 1, 1, 1, 0, 700, 98
33430, V, 1, 1, 1, 1, 0, 700, 98
33431, V, 1, 1, 1, 1, 0, 700, 98
33432, V, 1, 1, 1, 1, 0, 700, 98
33433, V, 1, 1, 1, 1, 0, 700, 98
33434, V, 1, 1, 1, 1, 0, 700, 98
33435, V, 1, 1, 1, 1, 0, 700, 98
33436, V, 1, 1, 1, 1, 0, 700, 98
33437, V, 1, 1, 1, 1, 0, 700, 98
33438, V, 1, 1, 1, 1, 0, 700, 98
33439, V, 1, 1, 1, 1, 0, 700, 98
33440, V, 1, 1, 1, 1, 0, 700, 98
33441, V, 1, 1, 1, 1, 0, 700, 98
33442, V, 1, 1, 1, 1, 0, 700, 98
33443, V, 1, 1, 1, 1, 0, 700, 98
33444, V, 1, 1, 1, 1, 0, 700, 98
33445, V, 1, 1, 1, 1, 0, 700, 98
33446, V, 1, 1, 1, 1, 0, 700, 98
33447, V, 1, 1, 1, 1, 0, 700, 98
33448, V, 1, 1, 1, 1, 0, 700, 98
33449, V, 1, 1, 1, 1, 0, 700, 98
33451, V, 1, 1, 1, 1, 0, 700, 98
33452, V, 1, 1, 1, 1, 0, 700, 98
33453, V, 1, 1, 1, 1, 0, 700, 98
33454, V, 1, 1, 1, 1, 0, 700, 98
33455, V, 1, 1, 1, 1, 0, 700, 98
33456, V, 1, 1, 1, 1, 0, 700, 98
33457, V, 1, 1, 1, 1, 0, 700, 98
33458, V, 1, 1, 1, 1, 0, 700, 98
33459, V, 1, 1, 1, 1, 0, 700, 98
33460, V, 1, 1, 1, 1, 0, 700, 98
33461, V, 1, 1, 1, 1, 0, 700, 98
33462, V, 1, 1, 1, 1, 0, 700, 98
33463, V, 1, 1, 1, 1, 0, 700, 98
33464, V, 1, 1, 1, 1, 0, 700, 98
33465, V, 1, 1, 1, 1, 0, 700, 98
33466, V, 1, 1, 1, 1, 0, 700, 98
33467, V, 1, 1, 1, 1, 0, 700, 98
33468, V, 1, 1, 1, 1, 0, 700, 98
33469, V, 1, 1, 1, 1, 0, 700, 98
33470, V, 1, 1, 1, 1, 0, 700, 98
33471, V, 1, 1, 1, 1, 0, 700, 98
33472, V, 1, 1, 1, 1, 0, 700, 98
33473, V, 1, 1, 1, 1, 0, 700, 98
33474, V, 1, 1, 1, 1, 0, 700, 98
33475, V, 1, 1, 1, 1, 0, 700, 98
33476, V, 1, 1, 1, 1, 0, 700, 98
33477, V, 1, 1, 1, 1, 0, 700, 98
33478, V, 1, 1, 1, 1, 0, 700, 98
33479, V, 1, 1, 1, 1, 0, 700, 98
33480, V, 1, 1, 1, 1, 0, 700, 98
33481, V, 1, 1, 1, 1, 0, 700, 98
33482, V, 1, 1, 1, 1, 0, 700, 98
33483, V, 1, 1, 1, 1, 0, 700, 98
33484, V, 1, 1, 1, 1, 0, 700, 98
33485, V, 1, 1, 1, 1, 0, 700, 98
33486, V, 1, 1, 1, 1, 0, 700, 98
33487, V, 1, 1, 1, 1, 0, 700, 98
33488, V, 1, 1, 1, 1, 0, 700, 98
33489, V, 1, 1, 1, 1, 0, 700, 98
33490, V, 1, 1, 1, 1, 0, 700, 98
33491, V, 1, 1, 1, 1, 0, 700, 98
33492, V, 1, 1, 1, 1, 0, 700, 98
33494, V, 1, 1, 1, 1, 0, 700, 98
33495, V, 1, 1, 1, 1, 0, 700, 98
33496, V, 1, 1, 1, 1, 0, 700, 98
33497, V, 1, 1, 1, 1, 0, 700, 98
33498, V, 1, 1, 1, 1, 0, 700, 98
33499, V, 1, 1, 1, 1, 0, 700, 98
33500, V, 1, 1, 1, 1, 0, 700, 98
33501, V, 1, 1, 1, 1, 0, 700, 98
33502, V, 1, 1, 1, 1, 0, 700, 98
33503, V, 1, 1, 1, 1, 0, 700, 98
33504, V, 1, 1, 1, 1, 0, 700, 98
33505, V, 1, 1, 1, 1, 0, 700, 98
33506, V, 1, 1, 1, 1, 0, 700, 98
33507, V, 1, 1, 1, 1, 0, 700, 98
33508, V, 1, 1, 1, 1, 0, 700, 98
33509, V, 1, 1, 1, 1, 0, 700, 98
33510, V, 1, 1, 1, 1, 0, 700, 98
33511, V, 1, 1, 1, 1, 0, 700, 98
33512, V, 1, 1, 1, 1, 0, 700, 98
33513, V, 1, 1, 1, 1, 0, 700, 98
33514, V, 1, 1, 1, 1, 0, 700, 98
33515, V, 1, 1, 1, 1, 0, 700, 98
33516, V, 1, 1, 1, 1, 0, 700, 98
33517, V, 1, 1, 1, 1, 0, 700, 98
33518, V, 1, 1, 1, 1, 0, 700, 98
33519, V, 1, 1, 1, 1, 0, 700, 98
33520, V, 1, 1, 1, 1, 0, 700, 98
33521, V, 1, 1, 1, 1, 0, 700, 98
33522, V, 1, 1, 1, 1, 0, 700, 98
33523, V, 1, 1, 1, 1, 0, 700, 98
33524, V, 1, 1, 1, 1, 0, 700, 98
33525, V, 1, 1, 1, 1, 0, 700, 98
33526, V, 1, 1, 1, 1, 0, 700, 98
33527, V, 1, 1, 1, 1, 0, 700, 98
33528, V, 1, 1, 1, 1, 0, 700, 98
33529, V, 1, 1, 1, 1, 0, 700, 98
33530, V, 1, 1, 1, 1, 0, 700, 98
33531, V, 1, 1, 1, 1, 0, 700, 98
33532, V, 1, 1, 1, 1, 0, 700, 98
33533, V, 1, 1, 1, 1, 0, 700, 98
33534, V, 1, 1, 1, 1, 0, 700, 98
33536, V, 1, 1, 1, 1, 0, 700, 98
33537, V, 1, 1, 1, 1, 0, 700, 98
33538, V, 1, 1, 1, 1, 0, 700, 98
33539, V, 1, 1, 1, 1, 0, 700, 98
33540, V, 1, 1, 1, 1, 0, 700, 98
33541, V, 1, 1, 1, 1, 0, 700, 98
33542, V, 1, 1, 1, 1, 0, 700, 98
33543, V, 1, 1, 1, 1, 0, 700, 98
33544, V, 1, 1, 1, 1, 0, 700, 98
33545, V, 1, 1, 1, 1, 0, 700, 98
33546, V, 1, 1, 1, 1, 0, 700, 98
33547, V, 1, 1, 1, 1, 0, 700, 98
33548, V, 1, 1, 1, 1, 0, 700, 98
33549, V, 1, 1, 1, 1, 0, 700, 98
33550, V, 1, 1, 1, 1, 0, 700, 98
33551, V, 1, 1, 1, 1, 0, 700, 98
33552, V, 1, 1, 1, 1, 0, 700, 98
33553, V, 1, 1, 1, 1, 0, 700, 98
33554, V, 1, 1, 1, 1, 0, 700, 98
33555, V, 1, 1, 1, 1, 0, 700, 98
33556, V, 1, 1, 1, 1, 0, 700, 98
33557, V, 1, 1, 1, 1, 0, 700, 98
33558, V, 1, 1, 1, 1, 0, 700, 98
33559, V, 1, 1, 1, 1, 0, 700, 98
33560, V, 1, 1, 1, 1, 0, 700, 98
33561, V, 1, 1, 1, 1, 0, 700, 98
33562, V, 1, 1, 1, 1, 0, 700, 98
33563, V, 1, 1, 1, 1, 0, 700, 98
33564, V, 1, 1, 1, 1, 0, 700, 98
33565, V, 1, 1, 1, 1, 0, 700, 98
33566, V, 1, 1, 1, 1, 0, 700, 98
33567, V, 1, 1, 1, 1, 0, 700, 98
33568, V, 1, 1, 1, 1, 0, 700, 98
33569, V, 1, 1, 1, 1, 0, 700, 98
33570, V, 1, 1, 1, 1, 0, 700, 98
33571, V, 1, 1, 1, 1, 0, 700, 98
33572, V, 1, 1, 1, 1, 0, 700, 98
33573, V, 1, 1, 1, 1, 0, 700, 98
33574, V, 1, 1, 1, 1, 0, 700, 98
33575, V, 1, 1, 1, 1, 0, 700, 98
33576, V, 1, 1, 1, 1, 0, 700, 98
33577, V, 1, 1, 1, 1, 0, 700, 98
33579, V, 1, 1, 1, 1, 0, 700, 98
33580, V, 1, 1, 1, 1, 0, 700, 98
33581, V, 1, 1, 1, 1, 0, 700, 98
33582, V, 1, 1, 1, 1, 0, 700, 98
33583, V, 1, 1, 1, 1, 0, 700, 98
33584, V, 1, 1, 1, 1, 0, 700, 98
33585, V, 1, 1, 1, 1, 0, 700, 98
33586, V, 1, 1, 1, 1, 0, 700, 98
33587, V, 1, 1, 1, 1, 0, 700, 98
33588, V, 1, 1, 1, 1, 0, 700, 98
33589, V, 1, 1, 1, 1, 0, 700, 98
33590, V, 1, 1, 1, 1, 0, 700, 98
33591, V, 1, 1, 1, 1, 0, 700, 98
33592, V, 1, 1, 1, 1, 0, 700, 98
33593, V, 1, 1, 1, 1, 0, 700, 98
33594, V, 1, 1, 1, 1, 0, 700, 98
33595, V, 1, 1, 1, 1, 0, 700, 98
33596, V, 1, 1, 1, 1, 0, 700, 98
33597, V, 1, 1, 1, 1, 0, 700, 98
33598, V, 1, 1, 1, 1, 0, 700, 98
33599, V, 1, 1, 1, 1, 0, 700, 98
33600, V, 1, 1, 1, 1, 0, 700, 98
33601, V, 1, 1, 1, 1, 0, 700, 98
33602, V, 1, 1, 1, 1, 0, 700, 98
33603, V, 1, 1, 1, 1, 0, 700, 98
33604, V, 1, 1, 1, 1, 0, 700, 98
33605, V, 1, 1, 1, 1, 0, 700, 98
33606, V, 1, 1, 1, 1, 0, 700, 98
33607, V, 1, 1, 1, 1, 0, 700, 98
33608, V, 1, 1, 1, 1, 0, 700, 98
33609, V, 1, 1, 1, 1, 0, 700, 98
33610, V, 1, 1, 1, 1, 0, 700, 98
33611, V, 1, 1, 1, 1, 0, 700, 98
33612, V, 1, 1, 1, 1, 0, 700, 98
33613, V, 1, 1, 1, 1, 0, 700, 98
33614, V, 1, 1, 1, 1, 0, 700, 98
33615, V, 1, 1, 1, 1, 0, 700, 98
33616, V, 1, 1, 1, 1, 0, 700, 98
33617, V, 1, 1, 1, 1, 0, 700, 98
33618, V, 1, 1, 1, 1, 0, 700, 98
33619, V, 1, 1, 1, 1, 0, 700, 98
33620, V, 1, 1, 1, 1, 0, 700, 98
33622, V, 1, 1, 1, 1, 0, 700, 98
33623, V, 1, 1, 1, 1, 0, 700, 98
33624, V, 1, 1, 1, 1, 0, 700, 98
33625, V, 1, 1, 1, 1, 0, 700, 98
33626, V, 1, 1, 1, 1, 0, 700, 98
33627, V, 1, 1, 1, 1, 0, 700, 98
33628, V, 1, 1, 1, 1, 0, 700, 98
33629, V, 1, 1, 1, 1, 0, 700, 98
33630, V, 1, 1, 1, 1, 0, 700, 98
33631, V, 1, 1, 1, 1, 0, 700, 98
33632, V, 1, 1, 1, 1, 0, 700, 98
33633, V, 1, 1, 1, 1, 0, 700, 98
33634, V, 1, 1, 1, 1, 0, 700, 98
33635, V, 1, 1, 1, 1, 0, 700, 98
33636, V, 1, 1, 1, 1, 0, 700, 98
33637, V, 1, 1, 1, 1, 0, 700, 98
33638, V, 1, 1, 1, 1, 0, 700, 98
33639, V, 1, 1, 1, 1, 0, 700, 98
33640, V, 1, 1, 1, 1, 0, 700, 98
33641, V, 1, 1, 1, 1, 0, 700, 98
33642, V, 1, 1, 1, 1, 0, 700, 98
33643, V, 1, 1, 1, 1, 0, 700, 98
33644, V, 1, 1, 1, 1, 0, 700, 98
33645, V, 1, 1, 1, 1, 0, 700, 98
33646, V, 1, 1, 1, 1, 0, 700, 98
33647, V, 1, 1, 1, 1, 0, 700, 98
33648, V, 1, 1, 1, 1, 0, 700, 98
33649, V, 1, 1, 1, 1, 0, 700, 98
33650, V, 1, 1, 1, 1, 0, 700, 98
33651, V, 1, 1, 1, 1, 0, 700, 98
33652, V, 1, 1, 1, 1, 0, 700, 98
33653, V, 1, 1, 1, 1, 0, 700, 98
33654, V, 1, 1, 1, 1, 0, 700, 98
33655, V, 1, 1, 1, 1, 0, 700, 98
33656, V, 1, 1, 1, 1, 0, 700, 98
33657, V, 1, 1, 1, 1, 0, 700, 98
33658, V, 1, 1, 1, 1, 0, 700, 98
33659, V, 1, 1, 1, 1, 0, 700, 98
33660, V, 1, 1, 1, 1, 0, 700, 98
33661, V, 1, 1, 1, 1, 0, 700, 98
33662, V, 1, 1, 1, 1, 0, 700, 98
33664, V, 1, 1, 1, 1, 0, 700, 98
33665, V, 1, 1, 1, 1, 0, 700, 98
33666, V, 1, 1, 1, 1, 0, 700, 98
33667, V, 1, 1, 1, 1, 0, 700, 98
33668, V, 1, 1, 1, 1, 0, 700, 98
33669, V, 1, 1, 1, 1, 0, 700, 98
33670, V, 1, 1, 1, 1, 0, 700, 98
33671, V, 1, 1, 1, 1, 0, 700, 98
33672, V, 1, 1, 1, 1, 0, 700, 98
33673, V, 1, 1, 1, 1, 0, 700, 98
33674, V, 1, 1, 1, 1, 0, 700, 98
33675, V, 1, 1, 1, 1, 0, 700, 98
33676, V, 1, 1, 1, 1, 0, 700, 98
33677, V, 1, 0, 0, 1, 0, 700, 98
33677, V, 1, 0, 0, 0, 0, 700, 98
33678, V, 1, 1, 0, 0, 0, 700, 98
33678, V, 1, 1, 0, 0, 0, 700, 98
33679, V, 1, 1, 1, 1, 0, 700, 98
33680, V, 1, 1, 1, 1, 0, 700, 98
33681, V, 1, 1, 1, 1, 0, 700, 98
33682, V, 1, 1, 1, 1, 0, 700, 98
33683, V, 1, 1, 1, 1, 0, 700, 98
33684, V, 1, 1, 1, 1, 0, 700, 98
33685, V, 1, 1, 1, 1, 0, 700, 98
33686, V, 1, 1, 1, 1, 0, 700, 98
33687, V, 1, 1, 1, 1, 0, 700, 98
33688, V, 1, 1, 1, 1, 0, 700, 98
33689, V, 1, 1, 1, 1, 0, 700, 98
33690, V, 1, 1, 1, 1, 0, 700, 98
33691, V, 1, 1, 1, 1, 0, 700, 98
33692, V, 1, 1, 1, 1, 0, 700, 98
33693, V, 1, 1, 1, 1, 0, 700, 98
33694, V, 1, 1, 1, 1, 0, 700, 98
33695, V, 1, 1, 1, 1, 0, 700, 98
33696, V, 1, 1, 1, 1, 0, 700, 98
33697, V, 1, 1, 1, 1, 0, 700, 98
33698, V, 1, 1, 1, 1, 0, 700, 98
33699, V, 1, 1, 1, 1, 0, 700, 98
33700, V, 1, 1, 1, 1, 0, 700, 98
33701, V, 1, 1, 1, 1, 0, 700, 98
33702, V, 1, 1, 1, 1, 0, 700, 98
33703, V, 1, 1, 1, 1, 0, 700, 98
33704, V, 1, 1, 1, 1, 0, 700, 98
33705, V, 1, 1, 1, 1, 0, 700, 98
33707, V, 1, 1, 1, 1, 0, 700, 98
33708, V, 1, 1, 1, 1, 0, 700, 98
33709, V, 1, 1, 1, 1, 0, 700, 98
33710, V, 1, 1, 1, 1, 0, 700, 98
33711, V, 1, 1, 1, 1, 0, 700, 98
33712, V, 1, 1, 1, 1, 0, 700, 98
33713, V, 1, 1, 1, 1, 0, 700, 98
33714, V, 1, 1, 1, 1, 0, 700, 98
33715, V, 1, 1, 1, 1, 0, 700, 98
33716, V, 1, 1, 1, 1, 0, 700, 98
33717, V, 1, 1, 1, 1, 0, 700, 98
33718, V, 1, 1, 1, 1, 0, 700, 98
33719, V, 1, 1, 1, 1, 0, 700, 98
33720, V, 1, 1, 1, 1, 0, 700, 98
33721, V, 1, 1, 1, 1, 0, 700, 98
33722, V, 1, 1, 1, 1, 0, 700, 98
33723, V, 1, 1, 1, 1, 0, 700, 98
33724, V, 1, 1, 1, 1, 0, 700, 98
33725, V, 1, 1, 1, 1, 0, 700, 98
33726, V, 1, 1, 1, 1, 0, 700, 98
33727, V, 1, 1, 1, 1, 0, 700, 98
33728, V, 1, 1, 1, 1, 0, 700, 98
33729, V, 1, 1, 1, 1, 0, 700, 98
33730, V, 1, 1, 1, 1, 0, 700, 98
33731, V, 1, 1, 1, 1, 0, 700, 98
33732, V, 1, 1, 1, 1, 0, 700, 98
33733, V, 1, 1, 1, 1, 0, 700, 98
33734, V, 1, 1, 1, 1, 0, 700, 98
33735, V, 1, 1, 1, 1, 0, 700, 98
33736, V, 1, 1, 1, 1, 0, 700, 98
33737, V, 1, 1, 1, 1, 0, 700, 98
33738, V, 1, 1, 1, 1, 0, 700, 98
33739, V, 1, 1, 1, 1, 0, 700, 98
33740, V, 1, 1, 1, 1, 0, 700, 98
33741, V, 1, 1, 1, 1, 0, 700, 98
33742, V, 1, 1, 1, 1, 0, 700, 98
33743, V, 1, 1, 1, 1, 0, 700, 98
33744, V, 1, 1, 1, 1, 0, 700, 98
33745, V, 1, 1, 1, 1, 0, 700, 98
33746, V, 1, 1, 1, 1, 0, 700, 98
33747, V, 1, 1, 1, 1, 0, 700, 98
33748, V, 1, 1, 1, 1, 0, 700, 98
33750, V, 1, 1, 1, 1, 0, 700, 98
33751, V, 1, 1, 1, 1, 0, 700, 98
33752, V, 1, 1, 1, 1, 0, 700, 98
33753, V, 1, 1, 1, 1, 0, 700, 98
33754, V, 1, 1, 1, 1, 0, 700, 98
33755, V, 1, 1, 1, 1, 0, 700, 98
33756, V, 1, 1, 1, 1, 0, 700, 98
33757, V, 1, 1, 1, 1, 0, 700, 98
33758, V, 1, 1, 1, 1, 0, 700, 98
33759, V, 1, 1, 1, 1, 0, 700, 98
33760, V, 1, 1, 1, 1, 0, 700, 98
33761, V, 1, 1, 1, 1, 0, 700, 98
33762, V, 1, 1, 1, 1, 0, 700, 98
33763, V, 1, 1, 1, 1, 0, 700, 98
33764, V, 1, 1, 1, 1, 0, 700, 98
33765, V, 1, 1, 1, 1, 0, 700, 98
33766, V, 1, 1, 1, 1, 0, 700, 98
33767, V, 1, 1, 1, 1, 0, 700, 98
33768, V, 1, 1, 1, 1, 0, 700, 98
33769, V, 1, 1, 1, 1, 0, 700, 98
33770, V, 1, 1, 1, 1, 0, 700, 98
33771, V, 1, 1, 1, 1, 0, 700, 98
33772, V, 1, 1, 1, 1, 0, 700, 98
33773, V, 1, 1, 1, 1, 0, 700, 98
33774, V, 1, 1, 1, 1, 0, 700, 98
33775, V, 1, 1, 1, 1, 0, 700, 98
33776, V, 1, 1, 1, 1, 0, 700, 98
33777, V, 1, 1, 1, 1, 0, 700, 98
33778, V, 1, 1, 1, 1, 0, 700, 98
33779, V, 1, 1, 1, 1, 0, 700, 98
33780, V, 1, 1, 1, 1, 0, 700, 98
33781, V, 1, 1, 1, 1, 0, 700, 98
33782, V, 1, 1, 1, 1, 0, 700, 98
33783, V, 1, 1, 1, 1, 0, 700, 98
33784, V, 1, 1, 1, 1, 0, 700, 98
33785, V, 1, 1, 1, 1, 0, 700, 98
33786, V, 1, 1, 1, 1, 0, 700, 98
33787, V, 1, 1, 1, 1, 0, 700, 98
33788, V, 1, 1, 1, 1, 0, 700, 98
33789, V, 1, 1, 1, 1, 0, 700, 98
33790, V, 1, 1, 1, 1, 0, 700, 98
33792, V, 1, 1, 1, 1, 0, 700, 98
33793, V, 1, 1, 1, 1, 0, 700, 98
33794, V, 1, 1, 1, 1, 0, 700, 98
33795, V, 1, 1, 1, 1, 0, 700, 98
33796, V, 1, 1, 1, 1, 0, 700, 98
33797, V, 1, 1, 1, 1, 0, 700, 98
33798, V, 1, 1, 1, 1, 0, 700, 98
33799, V, 1, 1, 1, 1, 0, 700, 98
33800, V, 1, 1, 1, 1, 0, 700, 98
33801, V, 1, 1, 1, 1, 0, 700, 98
33802, V, 1, 1, 1, 1, 0, 700, 98
33803, V, 1, 1, 1, 1, 0, 700, 98
33804, V, 1, 1, 1, 1, 0, 700, 98
33805, V, 1, 1, 1, 1, 0, 700, 98
33806, V, 1, 1, 1, 1, 0, 700, 98
33807, V, 1, 1, 1, 1, 0, 700, 98
33808, V, 1, 1, 1, 1, 0, 700, 98
33809, V, 1, 1, 1, 1, 0, 700, 98
33810, V, 1, 1, 1, 1, 0, 700, 98
33811, V, 1, 1, 1, 1, 0, 700, 98
33812, V, 1, 1, 1, 1, 0, 700, 98
33813, V, 1, 1, 1, 1, 0, 700, 98
33814, V, 1, 1, 1, 1, 0, 700, 98
33815, V, 1, 1, 1, 1, 0, 700, 98
33816, V, 1, 1, 1, 1, 0, 700, 98
33817, V, 1, 1, 1, 1, 0, 700, 98
33818, V, 1, 1, 1, 1, 0, 700, 98
33819, V, 1, 1, 1, 1, 0, 700, 98
33820, V, 1, 1, 1, 1, 0, 700, 98
33821, V, 1, 1, 1, 1, 0, 700, 98
33822, V, 1, 1, 1, 1, 0, 700, 98
33823, V, 1, 1, 1, 1, 0, 700, 98
33824, V, 1, 1, 1, 1, 0, 700, 98
33825, V, 1, 1, 1, 1, 0, 700, 98
33826, V, 1, 1, 1, 1, 0, 700, 98
33827, V, 1, 1, 1, 1, 0, 700, 98
33828, V, 1, 1, 1, 1, 0, 700, 98
33829, V, 1, 1, 1, 1, 0, 700, 98
33830, V, 1, 1, 1, 1, 0, 700, 98
33831, V, 1, 1, 1, 1, 0, 700, 98
33832, V, 1, 1, 1, 1, 0, 700, 98
33833, V, 1, 1, 1, 1, 0, 700, 98
33835, V, 1, 1, 1, 1, 0, 700, 98
33836, V, 1, 1, 1, 1, 0, 700, 98
33837, V, 1, 1, 1, 1, 0, 700, 98
33838, V, 1, 1, 1, 1, 0, 700, 98
33839, V, 1, 1, 1, 1, 0, 700, 98
33840, V, 1, 1, 1, 1, 0, 700, 98
33841, V, 1, 1, 1, 1, 0, 700, 98
33842, V, 1, 1, 1, 1, 0, 700, 98
33843, V, 1, 1, 1, 1, 0, 700, 98
33844, V, 1, 1, 1, 1, 0, 700, 98
33845, V, 1, 1, 1, 1, 0, 700, 98
33846, V, 1, 1, 1, 1, 0, 700, 98
33847, V, 1, 1, 1, 1, 0, 700, 98
33848, V, 1, 1, 1, 1, 0, 700, 98
33849, V, 1, 1, 1, 1, 0, 700, 98
33850, V, 1, 1, 1, 1, 0, 700, 98
33851, V, 1, 1, 1, 1, 0, 700, 98
33852, V, 1, 1, 1, 1, 0, 700, 98
33853, V, 1, 1, 1, 1, 0, 700, 98
33854, V, 1, 1, 1, 1, 0, 700, 98
33855, V, 1, 1, 1, 1, 0, 700, 98
33856, V, 1, 1, 1, 1, 0, 700, 98
33857, V, 1, 1, 1, 1, 0, 700, 98
33858, V, 1, 1, 1, 1, 0, 700, 98
33859, V, 1, 1, 1, 1, 0, 700, 98
33860, V, 1, 1, 1, 1, 0, 700, 98
33861, V, 1, 1, 1, 1, 0, 700, 98
33862, V, 1, 1, 1, 1, 0, 700, 98
33863, V, 1, 1, 1, 1, 0, 700, 98
33864, V, 1, 1, 1, 1, 0, 700, 98
33865, V, 1, 1, 1, 1, 0, 700, 98
33866, V, 1, 1, 1, 1, 0, 700, 98
33867, V, 1, 1, 1, 1, 0, 700, 98
33868, V, 1, 1, 1, 1, 0, 700, 98
33869, V, 1, 1, 1, 1, 0, 700, 98
33870, V, 1, 1, 1, 1, 0, 700, 98
33871, V, 1, 1, 1, 1, 0, 700, 98
33872, V, 1, 1, 1, 1, 0, 700, 98
33873, V, 1, 1, 1, 1, 0, 700, 98
33874, V, 1, 1, 1, 1, 0, 700, 98
33875, V, 1, 1, 1, 1, 0, 700, 98
33876, V, 1, 1, 1, 1, 0, 700, 98
33878, V, 1, 1, 1, 1, 0, 700, 98
33879, V, 1, 1, 1, 1, 0, 700, 98
33880, V, 1, 1, 1, 1, 0, 700, 98
33881, V, 1, 1, 1, 1, 0, 700, 98
33882, V, 1, 1, 1, 1, 0, 700, 98
33883, V, 1, 1, 1, 1, 0, 700, 98
33884, V, 1, 1, 1, 1, 0, 700, 98
33885, V, 1, 1, 1, 1, 0, 700, 98
33886, V, 1, 1, 1, 1, 0, 700, 98
33887, V, 1, 1, 1, 1, 0, 700, 98
33888, V, 1, 1, 1, 1, 0, 700, 98
33889, V, 1, 1, 1, 1, 0, 700, 98
33890, V, 1, 1, 1, 1, 0, 700, 98
33891, V, 1, 1, 1, 1, 0, 700, 98
33892, V, 1, 1, 1, 1, 0, 700, 98
33893, V, 1, 1, 1, 1, 0, 700, 98
33894, V, 1, 1, 1, 1, 0, 700, 98
33895, V, 1, 1, 1, 1, 0, 700, 98
33896, V, 1, 1, 1, 1, 0, 700, 98
33897, V, 1, 1, 1, 1, 0, 700, 98
33898, V, 1, 1, 1, 1, 0, 700, 98
33899, V, 1, 1, 1, 1, 0, 700, 98
33900, V, 1, 1, 1, 1, 0, 700, 98
33901, V, 1, 1, 1, 1, 0, 700, 98
33902, V, 1, 1, 1, 1, 0, 700, 98
33903, V, 1, 1, 1, 1, 0, 700, 98
33904, V, 1, 1, 1, 1, 0, 700, 98
33905, V, 1, 1, 1, 1, 0, 700, 98
33906, V, 1, 1, 1, 1, 0, 700, 98
33907, V, 1, 1, 1, 1, 0, 700, 98
33908, V, 1, 1, 1, 1, 0, 700, 98
33909, V, 1, 1, 1, 1, 0, 700, 98
33910, V, 1, 1, 1, 1, 0, 700, 98
33911, V, 1, 1, 1, 1, 0, 700, 98
33912, V, 1, 1, 1, 1, 0, 700, 98
33913, V, 1, 1, 1, 1, 0, 700, 98
33914, V, 1, 1, 1, 1, 0, 700, 98
33915, V, 1, 1, 1, 1, 0, 700, 98
33916, V, 1, 1, 1, 1, 0, 700, 98
33917, V, 1, 1, 1, 1, 0, 700, 98
33918, V, 1, 1, 1, 1, 0, 700, 98
33920, V, 1, 1, 1, 1, 0, 700, 98
33921, V, 1, 1, 1, 1, 0, 700, 98
33922, V, 1, 1, 1, 1, 0, 700, 98
33923, V, 1, 1, 1, 1, 0, 700, 98
33924, V, 1, 1, 1, 1, 0, 700, 98
33925, V, 1, 1, 1, 1, 0, 700, 98
33926, V, 1, 1, 1, 1, 0, 700, 98
33927, V, 1, 1, 1, 1, 0, 700, 98
33928, V, 1, 1, 1, 1, 0, 700, 98
33929, V, 1, 1, 1, 1, 0, 700, 98
33930, V, 1, 1, 1, 1, 0, 700, 98
33931, V, 1, 1, 1, 1, 0, 700, 98
33932, V, 1, 1, 1, 1, 0, 700, 98
33933, V, 1, 1, 1, 1, 0, 700, 98
33934, V, 1, 1, 1, 1, 0, 700, 98
33935, V, 1, 1, 1, 1, 0, 700, 98
33936, V, 1, 1, 1, 1, 0, 700, 98
33937, V, 1, 1, 1, 1, 0, 700, 98
33938, V, 1, 1, 1, 1, 0, 700, 98
33939, V, 1, 1, 1, 1, 0, 700, 98
33940, V, 1, 1, 1, 1, 0, 700, 98
33941, V, 1, 1, 1, 1, 0, 700, 98
33942, V, 1, 1, 1, 1, 0, 700, 98
33943, V, 1, 1, 1, 1, 0, 700, 98
33944, V, 1, 1, 1, 1, 0, 700, 98
33945, V, 1, 1, 1, 1, 0, 700, 98
33946, V, 1, 1, 1, 1, 0, 700, 98
33947, V, 1, 1, 1, 1, 0, 700, 98
33948, V, 1, 1, 1, 1, 0, 700, 98
33949, V, 1, 1, 1, 1, 0, 700, 98
33950, V, 1, 1, 1, 1, 0, 700, 98
33951, V, 1, 1, 1, 1, 0, 700, 98
33952, V, 1, 1, 1, 1, 0, 700, 98
33953, V, 1, 1, 1, 1, 0, 700, 98
33954, V, 1, 1, 1, 1, 0, 700, 98
33955, V, 1, 1, 1, 1, 0, 700, 98
33956, V, 1, 1, 1, 1, 0, 700, 98
33957, V, 1, 1, 1, 1, 0, 700, 98
33958, V, 1, 1, 1, 1, 0, 700, 98
33959, V, 1, 1, 1, 1, 0, 700, 98
33960, V, 1, 1, 1, 1, 0, 700, 98
33961, V, 1, 1, 1, 1, 0, 700, 98
33963, V, 1, 1, 1, 1, 0, 700, 98
33964, V, 1, 1, 1, 1, 0, 700, 98
33965, V, 1, 1, 1, 1, 0, 700, 98
33966, V, 1, 1, 1, 1, 0, 700, 98
33967, V, 1, 1, 1, 1, 0, 700, 98
33968, V, 1, 1, 1, 1, 0, 700, 98
33969, V, 1, 1, 1, 1, 0, 700, 98
33970, V, 1, 1, 1, 1, 0, 700, 98
33971, V, 1, 1, 1, 1, 0, 700, 98
33972, V, 1, 1, 1, 1, 0, 700, 98
33973, V, 1, 1, 1, 1, 0, 700, 98
33974, V, 1, 1, 1, 1, 0, 700, 98
33975, V, 1, 1, 1, 1, 0, 700, 98
33976, V, 1, 1, 1, 1, 0, 700, 98
33977, V, 1, 1, 1, 1, 0, 700, 98
33978, V, 1, 1, 1, 1, 0, 700, 98
33979, V, 1, 1, 1, 1, 0, 700, 98
33980, V, 1, 1, 1, 1, 0, 700, 98
33981, V, 1, 1, 1, 1, 0, 700, 98
33982, V, 1, 1, 1, 1, 0, 700, 98
33983, V, 1, 1, 1, 1, 0, 700, 98
33984, V, 1, 1, 1, 1, 0, 700, 98
33985, V, 1, 1, 1, 1, 0, 700, 98
33986, V, 1, 1, 1, 1, 0, 700, 98
33987, V, 1, 1, 1, 1, 0, 700, 98
33988, V, 1, 1, 1, 1, 0, 700, 98
33989, V, 1, 1, 1, 1, 0, 700, 98
33990, V, 1, 1, 1, 1, 0, 700, 98
33991, V, 1, 1, 1, 1, 0, 700, 98
33992, V, 1, 1, 1, 1, 0, 700, 98
33993, V, 1, 1, 1, 1, 0, 700, 98
33994, V, 1, 1, 1, 1, 0, 700, 98
33995, V, 1, 1, 1, 1, 0, 700, 98
33996, V, 1, 1, 1, 1, 0, 700, 98
33997, V, 1, 1, 1, 1, 0, 700, 98
33998, V, 1, 1, 1, 1, 0, 700, 98
33999, V, 1, 1, 1, 1, 0, 700, 98
34000, V, 1, 1, 1, 1, 0, 700, 98
34001, V, 1, 1, 1, 1, 0, 700, 98
34002, V, 1, 1, 1, 1, 0, 700, 98
34003, V, 1, 1, 1, 1, 0, 700, 98
34004, V, 1, 1, 1, 1, 0, 700, 98
34006, V, 1, 1, 1, 1, 0, 700, 98
34007, V, 1, 1, 1, 1, 0, 700, 98
34008, V, 1, 1, 1, 1, 0, 700, 98
34009, V, 1, 1, 1, 1, 0, 700, 98
34010, V, 1, 1, 1, 1, 0, 700, 98
34011, V, 1, 1, 1, 1, 0, 700, 98
34012, V, 1, 1, 1, 1, 0, 700, 98
34013, V, 1, 1, 1, 1, 0, 700, 98
34014, V, 1, 1, 1, 1, 0, 700, 99
34015, V, 1, 1, 1, 1, 0, 700, 98
34016, V, 1, 1, 1, 1, 0, 700, 98
34017, V, 1, 1, 1, 1, 0, 700, 98
34018, V, 1, 1, 1, 1, 0, 700, 98
34019, V, 1, 1, 1, 1, 0, 700, 98
34020, V, 1, 1, 1, 1, 0, 700, 98
34021, V, 1, 1, 1, 1, 0, 700, 98
34022, V, 1, 1, 1, 1, 0, 700, 98
34023, V, 1, 1, 1, 1, 0, 700, 98
34024, V, 1, 1, 1, 1, 0, 700, 99
34025, V, 1, 1, 1, 1, 0, 700, 98
34026, V, 1, 1, 1, 1, 0, 700, 98
34027, V, 1, 1, 1, 1, 0, 700, 98
34028, V, 1, 1, 1, 1, 0, 700, 98
34029, V, 1, 1, 1, 1, 0, 700, 98
34030, V, 1, 1, 1, 1, 0, 700, 98
34031, V, 1, 1, 1, 1, 0, 700, 98
34032, V, 1, 1, 1, 1, 0, 700, 98
34033, V, 1, 1, 1, 1, 0, 700, 98
34034, V, 1, 1, 1, 1, 0, 700, 98
34035, V, 1, 1, 1, 1, 0, 700, 98
34036, V, 1, 1, 1, 1, 0, 700, 98
34037, V, 1, 1, 1, 1, 0, 700, 98
34038, V, 1, 1, 1, 1, 0, 700, 98
34039, V, 1, 1, 1, 1, 0, 700, 98
34040, V, 1, 1, 1, 1, 0, 700, 98
34041, V, 1, 1, 1, 1, 0, 700, 98
34042, V, 1, 1, 1, 1, 0, 700, 98
34043, V, 1, 1, 1, 1, 0, 700, 98
34044, V, 1, 1, 1, 1, 0, 700, 98
34045, V, 1, 1, 1, 1, 0, 700, 98
34046, V, 1, 1, 1, 1, 0, 700, 98
34048, V, 1, 1, 1, 1, 0, 700, 98
34049, V, 1, 1, 1, 1, 0, 700, 98
34050, V, 1, 1, 1, 1, 0, 700, 98
34051, V, 1, 1, 1, 1, 0, 700, 98
34052, V, 1, 1, 1, 1, 0, 700, 98
34053, V, 1, 1, 1, 1, 0, 700, 98
34054, V, 1, 1, 1, 1, 0, 700, 98
34055, V, 1, 1, 1, 1, 0, 700, 98
34056, V, 1, 1, 1, 1, 0, 700, 98
34057, V, 1, 1, 1, 1, 0, 700, 98
34058, V, 1, 1, 1, 1, 0, 700, 98
34059, V, 1, 1, 1, 1, 0, 700, 98
34060, V, 1, 1, 1, 1, 0, 700, 98
34061, V, 1, 1, 1, 1, 0, 700, 98
34062, V, 1, 1, 1, 1, 0, 700, 98
34063, V, 1, 1, 1, 1, 0, 700, 98
34064, V, 1, 1, 1, 1, 0, 700, 98
34065, V, 1, 1, 1, 1, 0, 700, 98
34066, V, 1, 1, 1, 1, 0, 700, 98
34067, V, 1, 1, 1, 1, 0, 700, 98
34068, V, 1, 1, 1, 1, 0, 700, 98
34069, V, 1, 1, 1, 1, 0, 700, 98
34070, V, 1, 1, 1, 1, 0, 700, 98
34071, V, 1, 1, 1, 1, 0, 700, 98
34072, V, 1, 1, 1, 1, 0, 700, 98
34073, V, 1, 1, 1, 1, 0, 700, 98
34074, V, 1, 1, 1, 1, 0, 700, 98
34075, V, 1, 1, 1, 1, 0, 700, 98
34076, V, 1, 1, 1, 1, 0, 700, 98
34077, V, 1, 1, 1, 1, 0, 700, 98
34078, V, 1, 1, 1, 1, 0, 700, 98
34079, V, 1, 1, 1, 1, 0, 700, 98
34080, V, 1, 1, 1, 1, 0, 700, 98
34081, V, 1, 1, 1, 1, 0, 700, 98
34082, V, 1, 1, 1, 1, 0, 700, 99
34083, V, 1, 1, 1, 1, 0, 700, 99
34084, V, 1, 1, 1, 1, 0, 700, 98
34085, V, 1, 1, 1, 1, 0, 700, 98
34086, V, 1, 1, 1, 1, 0, 700, 98
34087, V, 1, 1, 1, 1, 0, 700, 98
34088, V, 1, 1, 1, 1, 0, 700, 98
34089, V, 1, 1, 1, 1, 0, 700, 98
34091, V, 1, 1, 1, 1, 0, 700, 98
34092, V, 1, 1, 1, 1, 0, 700, 98
34093, V, 1, 1, 1, 1, 0, 700, 98
34094, V, 1, 1, 1, 1, 0, 700, 98
34095, V, 1, 1, 1, 1, 0, 700, 98
34096, V, 1, 1, 1, 1, 0, 700, 98
34097, V, 1, 1, 1, 1, 0, 700, 98
34098, V, 1, 1, 1, 1, 0, 700, 98
34099, V, 1, 1, 1, 1, 0, 700, 98
34100, V, 1, 1, 1, 1, 0, 700, 98
34101, V, 1, 1, 1, 1, 0, 700, 98
34102, V, 1, 1, 1, 1, 0, 700, 98
34103, V, 1, 1, 1, 1, 0, 700, 98
34104, V, 1, 1, 1, 1, 0, 700, 98
34105, V, 1, 1, 1, 1, 0, 700, 98
34106, V, 1, 1, 1, 1, 0, 700, 98
34107, V, 1, 1, 1, 1, 0, 700, 98
34108, V, 1, 1, 1, 1, 0, 700, 98
34109, V, 1, 1, 1, 1, 0, 700, 98
34110, V, 1, 1, 1, 1, 0, 700, 98
34111, V, 1, 1, 1, 1, 0, 700, 98
34112, V, 1, 1, 1, 1, 0, 700, 98
34113, V, 1, 1, 1, 1, 0, 700, 98
34114, V, 1, 1, 1, 1, 0, 700, 98
34115, V, 1, 1, 1, 1, 0, 700, 98
34116, V, 1, 1, 1, 1, 0, 700, 98
34117, V, 1, 1, 1, 1, 0, 700, 98
34118, V, 1, 1, 1, 1, 0, 700, 98
34119, V, 1, 1, 1, 1, 0, 700, 98
34120, V, 1, 1, 1, 1, 0, 700, 98
34121, V, 1, 1, 1, 1, 0, 700, 98
34122, V, 1, 1, 1, 1, 0, 700, 98
34123, V, 1, 1, 1, 1, 0, 700, 98
34124, V, 1, 1, 1, 1, 0, 700, 98
34125, V, 1, 1, 1, 1, 0, 700, 98
34126, V, 1, 1, 1, 1, 0, 700, 98
34127, V, 1, 1, 1, 1, 0, 700, 98
34128, V, 1, 1, 1, 1, 0, 700, 98
34129, V, 1, 1, 1, 1, 0, 700, 98
34130, V, 1, 1, 1, 1, 0, 700, 98
34131, V, 1, 1, 1, 1, 0, 700, 98
34132, V, 1, 1, 1, 1, 0, 700, 98
34134, V, 1, 1, 1, 1, 0, 700, 98
34135, V, 1, 1, 1, 1, 0, 700, 98
34136, V, 1, 1, 1, 1, 0, 700, 98
34137, V, 1, 1, 1, 1, 0, 700, 98
34138, V, 1, 1, 1, 1, 0, 700, 98
34139, V, 1, 1, 1, 1, 0, 700, 98
34140, V, 1, 1, 1, 1, 0, 700, 98
34141, V, 1, 1, 1, 1, 0, 700, 98
34142, V, 1, 1, 1, 1, 0, 700, 98
34143, V, 1, 1, 1, 1, 0, 700, 98
34144, V, 1, 1, 1, 1, 0, 700, 98
34145, V, 1, 1, 1, 1, 0, 700, 98
34146, V, 1, 1, 1, 1, 0, 700, 98
34147, V, 1, 1, 1, 1, 0, 700, 98
34148, V, 1, 1, 1, 1, 0, 700, 98
34149, V, 1, 1, 1, 1, 0, 700, 98
34150, V, 1, 1, 1, 1, 0, 700, 98
34151, V, 1, 1, 1, 1, 0, 700, 98
34152, V, 1, 1, 1, 1, 0, 700, 98
34153, V, 1, 1, 1, 1, 0, 700, 98
34154, V, 1, 1, 1, 1, 0, 700, 98
34155, V, 1, 1, 1, 1, 0, 700, 98
34156, V, 1, 1, 1, 1, 0, 700, 99
34157, V, 1, 1, 1, 1, 0, 700, 98
34158, V, 1, 1, 1, 1, 0, 700, 98
34159, V, 1, 1, 1, 1, 0, 700, 98
34160, V, 1, 1, 1, 1, 0, 700, 98
34161, V, 1, 1, 1, 1, 0, 700, 98
34162, V, 1, 1, 1, 1, 0, 700, 98
34163, V, 1, 1, 1, 1, 0, 700, 99
34164, V, 1, 1, 1, 1, 0, 700, 99
34165, V, 1, 1, 1, 1, 0, 700, 98
34166, V, 1, 1, 1, 1, 0, 700, 98
34167, V, 1, 1, 1, 1, 0, 700, 98
34168, V, 1, 1, 1, 1, 0, 700, 98
34169, V, 1, 1, 1, 1, 0, 700, 99
34170, V, 1, 1, 1, 1, 0, 700, 98
34171, V, 1, 1, 1, 1, 0, 700, 99
34172, V, 1, 1, 1, 1, 0, 700, 98
34173, V, 1, 1, 1, 1, 0, 700, 98
34174, V, 1, 1, 1, 1, 0, 700, 98
34176, V, 1, 1, 1, 1, 0, 700, 98
34177, V, 1, 1, 1, 1, 0, 700, 98
34178, V, 1, 1, 1, 1, 0, 700, 98
34179, V, 1, 1, 1, 1, 0, 700, 98
34180, V, 1, 1, 1, 1, 0, 700, 98
34181, V, 1, 1, 1, 1, 0, 700, 98
34182, V, 1, 1, 1, 1, 0, 700, 98
34183, V, 1, 1, 1, 1, 0, 700, 98
34184, V, 1, 1, 1, 1, 0, 700, 98
34185, V, 1, 1, 1, 1, 0, 700, 98
34186, V, 1, 1, 1, 1, 0, 700, 98
34187, V, 1, 1, 1, 1, 0, 700, 98
34188, V, 1, 1, 1, 1, 0, 700, 98
34189, V, 1, 1, 1, 1, 0, 700, 98
34190, V, 1, 1, 1, 1, 0, 700, 98
34191, V, 1, 1, 1, 1, 0, 700, 98
34192, V, 1, 1, 1, 1, 0, 700, 98
34193, V, 1, 1, 1, 1, 0, 700, 98
34194, V, 1, 1, 1, 1, 0, 700, 98
34195, V, 1, 1, 1, 1, 0, 700, 98
34196, V, 1, 1, 1, 1, 0, 700, 98
34197, V, 1, 1, 1, 1, 0, 700, 98
34198, V, 1, 1, 1, 1, 0, 700, 98
34199, V, 1, 1, 1, 1, 0, 700, 98
34200, V, 1, 1, 1, 1, 0, 700, 98
34201, V, 1, 1, 1, 1, 0, 700, 98
34202, V, 1, 1, 1, 1, 0, 700, 98
34203, V, 1, 1, 1, 1, 0, 700, 98
34204, V, 1, 1, 1, 1, 0, 700, 98
34205, V, 1, 1, 1, 1, 0, 700, 98
34206, V, 1, 1, 1, 1, 0, 700, 98
34207, V, 1, 1, 1, 1, 0, 700, 98
34208, V, 1, 1, 1, 1, 0, 700, 98
34209, V, 1, 1, 1, 1, 0, 700, 98
34210, V, 1, 1, 1, 1, 0, 700, 98
34211, V, 1, 1, 1, 1, 0, 700, 98
34212, V, 1, 1, 1, 1, 0, 700, 98
34213, V, 1, 1, 1, 1, 0, 700, 98
34214, V, 1, 1, 1, 1, 0, 700, 98
34215, V, 1, 1, 1, 1, 0, 700, 98
34216, V, 1, 1, 1, 1, 0, 700, 98
34217, V, 1, 1, 1, 1, 0, 700, 98
34219, V, 1, 1, 1, 1, 0, 700, 98
34220, V, 1, 1, 1, 1, 0, 700, 98
34221, V, 1, 1, 1, 1, 0, 700, 98
34222, V, 1, 1, 1, 1, 0, 700, 98
34223, V, 1, 1, 1, 1, 0, 700, 98
34224, V, 1, 1, 1, 1, 0, 700, 98
34225, V, 1, 1, 1, 1, 0, 700, 98
34226, V, 1, 1, 1, 1, 0, 700, 98
34227, V, 1, 1, 1, 1, 0, 700, 99
34228, V, 1, 1, 1, 1, 0, 700, 98
34229, V, 1, 1, 1, 1, 0, 700, 99
34230, V, 1, 1, 1, 1, 0, 700, 98
34231, V, 1, 1, 1, 1, 0, 700, 98
34232, V, 1, 1, 1, 1, 0, 700, 98
34233, V, 1, 1, 1, 1, 0, 700, 98
34234, V, 1, 1, 1, 1, 0, 700, 98
34235, V, 1, 1, 1, 1, 0, 700, 98
34236, V, 1, 1, 1, 1, 0, 700, 98
34237, V, 1, 1, 1, 1, 0, 700, 98
34238, V, 1, 1, 1, 1, 0, 700, 98
34239, V, 1, 1, 1, 1, 0, 700, 98
34240, V, 1, 1, 1, 1, 0, 700, 98
34241, V, 1, 1, 1, 1, 0, 700, 98
34242, V, 1, 1, 1, 1, 0, 700, 98
34243, V, 1, 1, 1, 1, 0, 700, 98
34244, V, 1, 1, 1, 1, 0, 700, 98
34245, V, 1, 1, 1, 1, 0, 700, 99
34246, V, 1, 1, 1, 1, 0, 700, 98
34247, V, 1, 1, 1, 1, 0, 700, 99
34248, V, 1, 1, 1, 1, 0, 700, 99
34249, V, 1, 1, 1, 1, 0, 700, 99
34250, V, 1, 1, 1, 1, 0, 700, 98
34251, V, 1, 1, 1, 1, 0, 700, 98
34252, V, 1, 1, 1, 1, 0, 700, 98
34253, V, 1, 1, 1, 1, 0, 700, 98
34254, V, 1, 1, 1, 1, 0, 700, 98
34255, V, 1, 1, 1, 1, 0, 700, 98
34256, V, 1, 1, 1, 1, 0, 700, 98
34257, V, 1, 1, 1, 1, 0, 700, 99
34258, V, 1, 1, 1, 1, 0, 700, 98
34259, V, 1, 1, 1, 1, 0, 700, 98
34260, V, 1, 1, 1, 1, 0, 700, 98
34262, V, 1, 1, 1, 1, 0, 700, 98
34263, V, 1, 1, 1, 1, 0, 700, 98
34264, V, 1, 1, 1, 1, 0, 700, 98
34265, V, 1, 1, 1, 1, 0, 700, 98
34266, V, 1, 1, 1, 1, 0, 700, 98
34267, V, 1, 1, 1, 1, 0, 700, 98
34268, V, 1, 1, 1, 1, 0, 700, 98
34269, V, 1, 1, 1, 1, 0, 700, 98
34270, V, 1, 1, 1, 1, 0, 700, 98
34271, V, 1, 1, 1, 1, 0, 700, 98
34272, V, 1, 1, 1, 1, 0, 700, 98
34273, V, 1, 1, 1, 1, 0, 700, 98
34274, V, 1, 1, 1, 1, 0, 700, 98
34275, V, 1, 1, 1, 1, 0, 700, 98
34276, V, 1, 1, 1, 1, 0, 700, 98
34277, V, 1, 1, 1, 1, 0, 700, 98
34278, V, 1, 1, 1, 1, 0, 700, 98
34279, V, 1, 1, 1, 1, 0, 700, 98
34280, V, 1, 1, 1, 1, 0, 700, 98
34281, V, 1, 1, 1, 1, 0, 700, 98
34282, V, 1, 1, 1, 1, 0, 700, 98
34283, V, 1, 1, 1, 1, 0, 700, 98
34284, V, 1, 1, 1, 1, 0, 700, 98
34285, V, 1, 1, 1, 1, 0, 700, 98
34286, V, 1, 1, 1, 1, 0, 700, 98
34287, V, 1, 1, 1, 1, 0, 700, 98
34288, V, 1, 1, 1, 1, 0, 700, 98
34289, V, 1, 1, 1, 1, 0, 700, 98
34290, V, 1, 1, 1, 1, 0, 700, 98
34291, V, 1, 1, 1, 1, 0, 700, 98
34292, V, 1, 1, 1, 1, 0, 700, 98
34293, V, 1, 1, 1, 1, 0, 700, 98
34294, V, 1, 1, 1, 1, 0, 700, 98
34295, V, 1, 1, 1, 1, 0, 700, 99
34296, V, 1, 1, 1, 1, 0, 700, 98
34297, V, 1, 1, 1, 1, 0, 700, 99
34298, V, 1, 1, 1, 1, 0, 700, 98
34299, V, 1, 1, 1, 1, 0, 700, 98
34300, V, 1, 1, 1, 1, 0, 700, 99
34301, V, 1, 1, 1, 1, 0, 700, 99
34302, V, 1, 1, 1, 1, 0, 700, 99
34304, V, 1, 1, 1, 1, 0, 700, 99
34305, V, 1, 1, 1, 1, 0, 700, 99
34306, V, 1, 1, 1, 1, 0, 700, 99
34307, V, 1, 1, 1, 1, 0, 700, 99
34308, V, 1, 1, 1, 1, 0, 700, 99
34309, V, 1, 1, 1, 1, 0, 700, 99
34310, V, 1, 1, 1, 1, 0, 700, 99
34311, V, 1, 1, 1, 1, 0, 700, 99
34312, V, 1, 1, 1, 1, 0, 700, 99
34313, V, 1, 1, 1, 1, 0, 700, 99
34314, V, 1, 1, 1, 1, 0, 700, 99
34315, V, 1, 1, 1, 1, 0, 700, 99
34316, V, 1, 1, 1, 1, 0, 700, 99
34317, V, 1, 1, 1, 1, 0, 700, 99
34318, V, 1, 1, 1, 1, 0, 700, 99
34319, V, 1, 1, 1, 1, 0, 700, 99
34320, V, 1, 1, 1, 1, 0, 700, 99
34321, V, 1, 1, 1, 1, 0, 700, 99
34322, V, 1, 1, 1, 1, 0, 700, 99
34323, V, 1, 1, 1, 1, 0, 700, 99
34324, V, 1, 1, 1, 1, 0, 700, 99
34325, V, 1, 1, 1, 1, 0, 700, 99
34326, V, 1, 1, 1, 1, 0, 700, 99
34327, V, 1, 1, 1, 1, 0, 700, 99
34328, V, 1, 1, 1, 1, 0, 700, 99
34329, V, 1, 1, 1, 1, 0, 700, 99
34330, V, 1, 1, 1, 1, 0, 700, 99
34331, V, 1, 1, 1, 1, 0, 700, 99
34332, V, 1, 1, 1, 1, 0, 700, 99
34333, V, 1, 1, 1, 1, 0, 700, 99
34334, V, 1, 1, 1, 1, 0, 700, 99
34335, V, 1, 1, 1, 1, 0, 700, 99
34336, V, 1, 1, 1, 1, 0, 700, 99
34337, V, 1, 1, 1, 1, 0, 700, 99
34338, V, 1, 1, 1, 1, 0, 700, 99
34339, V, 1, 1, 1, 1, 0, 700, 99
34340, V, 1, 1, 1, 1, 0, 700, 99
34341, V, 1, 1, 1, 1, 0, 700, 99
34342, V, 1, 1, 1, 1, 0, 700, 98
34343, V, 1, 1, 1, 1, 0, 700, 99
34344, V, 1, 1, 1, 1, 0, 700, 98
34345, V, 1, 1, 1, 1, 0, 700, 98
34347, V, 1, 1, 1, 1, 0, 700, 98
34348, V, 1, 1, 1, 1, 0, 700, 99
34349, V, 1, 1, 1, 1, 0, 700, 99
34350, V, 1, 1, 1, 1, 0, 700, 99
34351, V, 1, 1, 1, 1, 0, 700, 99
34352, V, 1, 1, 1, 1, 0, 700, 98
34353, V, 1, 1, 1, 1, 0, 700, 99
34354, V, 1, 1, 1, 1, 0, 700, 98
34355, V, 1, 1, 1, 1, 0, 700, 99
34356, V, 1, 1, 1, 1, 0, 700, 99
34357, V, 1, 1, 1, 1, 0, 700, 98
34358, V, 1, 1, 1, 1, 0, 700, 99
34359, V, 1, 1, 1, 1, 0, 700, 99
34360, V, 1, 1, 1, 1, 0, 700, 99
34361, V, 1, 1, 1, 1, 0, 700, 99
34362, V, 1, 1, 1, 1, 0, 700, 99
34363, V, 1, 1, 1, 1, 0, 700, 99
34364, V, 1, 1, 1, 1, 0, 700, 99
34365, V, 1, 1, 1, 1, 0, 700, 99
34366, V, 1, 1, 1, 1, 0, 700, 99
34367, V, 1, 1, 1, 1, 0, 700, 99
34368, V, 1, 1, 1, 1, 0, 700, 99
34369, V, 1, 1, 1, 1, 0, 700, 99
34370, V, 1, 1, 1, 1, 0, 700, 99
34371, V, 1, 1, 1, 1, 0, 700, 99
34372, V, 1, 1, 1, 1, 0, 700, 99
34373, V, 1, 1, 1, 1, 0, 700, 99
34374, V, 1, 1, 1, 1, 0, 700, 99
34375, V, 1, 1, 1, 1, 0, 700, 99
34376, V, 1, 1, 1, 1, 0, 700, 99
34377, V, 1, 1, 1, 1, 0, 700, 99
34378, V, 1, 1, 1, 1, 0, 700, 99
34379, V, 1, 1, 1, 1, 0, 700, 99
34380, V, 1, 1, 1, 1, 0, 700, 99
34381, V, 1, 1, 1, 1, 0, 700, 99
34382, V, 1, 1, 1, 1, 0, 700, 99
34383, V, 1, 1, 1, 1, 0, 700, 99
34384, V, 1, 1, 1, 1, 0, 700, 99
34385, V, 1, 1, 1, 1, 0, 700, 99
34386, V, 1, 1, 1, 1, 0, 700, 99
34387, V, 1, 1, 1, 1, 0, 700, 99
34388, V, 1, 1, 1, 1, 0, 700, 99
34390, V, 1, 1, 1, 1, 0, 700, 99
34391, V, 1, 1, 1, 1, 0, 700, 99
34392, V, 1, 1, 1, 1, 0, 700, 99
34393, V, 1, 1, 1, 1, 0, 700, 99
34394, V, 1, 1, 1, 1, 0, 700, 99
34395, V, 1, 1, 1, 1, 0, 700, 99
34396, V, 1, 1, 1, 1, 0, 700, 99
34397, V, 1, 1, 1, 1, 0, 700, 99
34398, V, 1, 1, 1, 1, 0, 700, 99
34399, V, 1, 1, 1, 1, 0, 700, 99
34400, V, 1, 1, 1, 1, 0, 700, 99
34401, V, 1, 1, 1, 1, 0, 700, 99
34402, V, 1, 1, 1, 1, 0, 700, 99
34403, V, 1, 1, 1, 1, 0, 700, 99
34404, V, 1, 1, 1, 1, 0, 700, 99
34405, V, 1, 1, 1, 1, 0, 700, 99
34406, V, 1, 1, 1, 1, 0, 700, 99
34407, V, 1, 1, 1, 1, 0, 700, 99
34408, V, 1, 1, 1, 1, 0, 700, 99
34409, V, 1, 1, 1, 1, 0, 700, 99
34410, V, 1, 1, 1, 1, 0, 700, 99
34411, V, 1, 1, 1, 1, 0, 700, 99
34412, V, 1, 1, 1, 1, 0, 700, 99
34413, V, 1, 1, 1, 1, 0, 700, 99
34414, V, 1, 1, 1, 1, 0, 700, 99
34415, V, 1, 1, 1, 1, 0, 700, 99
34416, V, 1, 1, 1, 1, 0, 700, 99
34417, V, 1, 1, 1, 1, 0, 700, 99
34418, V, 1, 1, 1, 1, 0, 700, 99
34419, V, 1, 1, 1, 1, 0, 700, 99
34420, V, 1, 1, 1, 1, 0, 700, 99
34421, V, 1, 1, 1, 1, 0, 700, 99
34422, V, 1, 1, 1, 1, 0, 700, 99
34423, V, 1, 1, 1, 1, 0, 700, 99
34424, V, 1, 1, 1, 1, 0, 700, 99
34425, V, 1, 1, 1, 1, 0, 700, 99
34426, V, 1, 1, 1, 1, 0, 700, 99
34427, V, 1, 1, 1, 1, 0, 700, 99
34428, V, 1, 1, 1, 1, 0, 700, 99
34429, V, 1, 1, 1, 1, 0, 700, 99
34430, V, 1, 1, 1, 1, 0, 700, 99
34432, V, 1, 1, 1, 1, 0, 700, 99
34433, V, 1, 1, 1, 1, 0, 700, 99
34434, V, 1, 1, 1, 1, 0, 700, 99
34435, V, 1, 1, 1, 1, 0, 700, 99
34436, V, 1, 1, 1, 1, 0, 700, 99
34437, V, 1, 1, 1, 1, 0, 700, 99
34438, V, 1, 1, 1, 1, 0, 700, 99
34439, V, 1, 1, 1, 1, 0, 700, 99
34440, V, 1, 1, 1, 1, 0, 700, 99
34441, V, 1, 1, 1, 1, 0, 700, 99
34442, V, 1, 1, 1, 1, 0, 700, 99
34443, V, 1, 1, 1, 1, 0, 700, 99
34444, V, 1, 1, 1, 1, 0, 700, 99
34445, V, 1, 1, 1, 1, 0, 700, 99
34446, V, 1, 1, 1, 1, 0, 700, 99
34447, V, 1, 1, 1, 1, 0, 700, 99
34448, V, 1, 1, 1, 1, 0, 700, 99
34449, V, 1, 1, 1, 1, 0, 700, 99
34450, V, 1, 1, 1, 1, 0, 700, 99
34451, V, 1, 1, 1, 1, 0, 700, 99
34452, V, 1, 1, 1, 1, 0, 700, 99
34453, V, 1, 1, 1, 1, 0, 700, 99
34454, V, 1, 1, 1, 1, 0, 700, 99
34455, V, 1, 1, 1, 1, 0, 700, 99
34456, V, 1, 1, 1, 1, 0, 700, 99
34457, V, 1, 1, 1, 1, 0, 700, 99
34458, V, 1, 1, 1, 1, 0, 700, 98
34459, V, 1, 1, 1, 1, 0, 700, 99
34460, V, 1, 1, 1, 1, 0, 700, 99
34461, V, 1, 1, 1, 1, 0, 700, 99
34462, V, 1, 1, 1, 1, 0, 700, 99
34463, V, 1, 1, 1, 1, 0, 700, 99
34464, V, 1, 1, 1, 1, 0, 700, 99
34465, V, 1, 1, 1, 1, 0, 700, 99
34466, V, 1, 1, 1, 1, 0, 700, 99
34467, V, 1, 1, 1, 1, 0, 700, 99
34468, V, 1, 1, 1, 1, 0, 700, 99
34469, V, 1, 1, 1, 1, 0, 700, 99
34470, V, 1, 1, 1, 1, 0, 700, 99
34471, V, 1, 1, 1, 1, 0, 700, 99
34472, V, 1, 1, 1, 1, 0, 700, 99
34473, V, 1, 1, 1, 1, 0, 700, 99
34475, V, 1, 1, 1, 1, 0, 700, 99
34476, V, 1, 1, 1, 1, 0, 700, 98
34477, V, 1, 1, 1, 1, 0, 700, 99
34478, V, 1, 1, 1, 1, 0, 700, 99
34479, V, 1, 1, 1, 1, 0, 700, 99
34480, V, 1, 1, 1, 1, 0, 700, 99
34481, V, 1, 1, 1, 1, 0, 700, 99
34482, V, 1, 1, 1, 1, 0, 700, 99
34483, V, 1, 1, 1, 1, 0, 700, 99
34484, V, 1, 1, 1, 1, 0, 700, 98
34485, V, 1, 1, 1, 1, 0, 700, 99
34486, V, 1, 1, 1, 1, 0, 700, 99
34487, V, 1, 1, 1, 1, 0, 700, 99
34488, V, 1, 1, 1, 1, 0, 700, 98
34489, V, 1, 1, 1, 1, 0, 700, 99
34490, V, 1, 1, 1, 1, 0, 700, 98
34491, V, 1, 1, 1, 1, 0, 700, 98
34492, V, 1, 1, 1, 1, 0, 700, 98
34493, V, 1, 1, 1, 1, 0, 700, 98
34494, V, 1, 1, 1, 1, 0, 700, 98
34495, V, 1, 1, 1, 1, 0, 700, 98
34496, V, 1, 1, 1, 1, 0, 700, 98
34497, V, 1, 1, 1, 1, 0, 700, 98
34498, V, 1, 1, 1, 1, 0, 700, 98
34499, V, 1, 1, 1, 1, 0, 700, 98
34500, V, 1, 1, 1, 1, 0, 700, 98
34501, V, 1, 1, 1, 1, 0, 700, 98
34502, V, 1, 1, 1, 1, 0, 700, 98
34503, V, 1, 1, 1, 1, 0, 700, 98
34504, V, 1, 1, 1, 1, 0, 700, 98
34505, V, 1, 1, 1, 1, 0, 700, 98
34506, V, 1, 1, 1, 1, 0, 700, 98
34507, V, 1, 1, 1, 1, 0, 700, 98
34508, V, 1, 1, 1, 1, 0, 700, 98
34509, V, 1, 1, 1, 1, 0, 700, 98
34510, V, 1, 1, 1, 1, 0, 700, 98
34511, V, 1, 1, 1, 1, 0, 700, 98
34512, V, 1, 1, 1, 1, 0, 700, 98
34513, V, 1, 1, 1, 1, 0, 700, 98
34514, V, 1, 1, 1, 1, 0, 700, 98
34515, V, 1, 1, 1, 1, 0, 700, 98
34516, V, 1, 1, 1, 1, 0, 700, 98
34518, V, 1, 1, 1, 1, 0, 700, 98
34519, V, 1, 1, 1, 1, 0, 700, 98
34520, V, 1, 1, 1, 1, 0, 700, 98
34521, V, 1, 1, 1, 1, 0, 700, 98
34522, V, 1, 1, 1, 1, 0, 700, 98
34523, V, 1, 1, 1, 1, 0, 700, 98
34524, V, 1, 1, 1, 1, 0, 700, 98
34525, V, 1, 1, 1, 1, 0, 700, 98
34526, V, 1, 1, 1, 1, 0, 700, 98
34527, V, 1, 1, 1, 1, 0, 700, 98
34528, V, 1, 1, 1, 1, 0, 700, 98
34529, V, 1, 1, 1, 1, 0, 700, 98
34530, V, 1, 1, 1, 1, 0, 700, 98
34531, V, 1, 1, 1, 1, 0, 700, 98
34532, V, 1, 1, 1, 1, 0, 700, 98
34533, V, 1, 1, 1, 1, 0, 700, 98
34534, V, 1, 1, 1, 1, 0, 700, 98
34535, V, 1, 1, 1, 1, 0, 700, 98
34536, V, 1, 1, 1, 1, 0, 700, 98
34537, V, 1, 1, 1, 1, 0, 700, 98
34538, V, 1, 1, 1, 1, 0, 700, 98
34539, V, 1, 1, 1, 1, 0, 700, 98
34540, V, 1, 1, 1, 1, 0, 700, 99
34541, V, 1, 1, 1, 1, 0, 700, 98
34542, V, 1, 1, 1, 1, 0, 700, 98
34543, V, 1, 1, 1, 1, 0, 700, 99
34544, V, 1, 1, 1, 1, 0, 700, 98
34545, V, 1, 1, 1, 1, 0, 700, 99
34546, V, 1, 1, 1, 1, 0, 700, 99
34547, V, 1, 1, 1, 1, 0, 700, 99
34548, V, 1, 1, 1, 1, 0, 700, 99
34549, V, 1, 1, 1, 1, 0, 700, 99
34550, V, 1, 1, 1, 1, 0, 700, 98
34551, V, 1, 1, 1, 1, 0, 700, 98
34552, V, 1, 1, 1, 1, 0, 700, 99
34553, V, 1, 1, 1, 1, 0, 700, 99
34554, V, 1, 1, 1, 1, 0, 700, 98
34555, V, 1, 1, 1, 1, 0, 700, 99
34556, V, 1, 1, 1, 1, 0, 700, 99
34557, V, 1, 1, 1, 1, 0, 700, 99
34558, V, 1, 1, 1, 1, 0, 700, 99
34560, V, 1, 1, 1, 1, 0, 700, 98
34561, V, 1, 1, 1, 1, 0, 700, 98
34562, V, 1, 1, 1, 1, 0, 700, 98
34563, V, 1, 1, 1, 1, 0, 700, 99
34564, V, 1, 1, 1, 1, 0, 700, 99
34565, V, 1, 1, 1, 1, 0, 700, 98
34566, V, 1, 1, 1, 1, 0, 700, 99
34567, V, 1, 1, 1, 1, 0, 700, 99
34568, V, 1, 1, 1, 1, 0, 700, 98
34569, V, 1, 1, 1, 1, 0, 700, 99
34570, V, 1, 1, 1, 1, 0, 700, 99
34571, V, 1, 1, 1, 1, 0, 700, 99
34572, V, 1, 1, 1, 1, 0, 700, 99
34573, V, 1, 1, 1, 1, 0, 700, 99
34574, V, 1, 1, 1, 1, 0, 700, 99
34575, V, 1, 1, 1, 1, 0, 700, 98
34576, V, 1, 1, 1, 1, 0, 700, 99
34577, V, 1, 1, 1, 1, 0, 700, 98
34578, V, 1, 1, 1, 1, 0, 700, 99
34579, V, 1, 1, 1, 1, 0, 700, 99
34580, V, 1, 1, 1, 1, 0, 700, 99
34581, V, 1, 1, 1, 1, 0, 700, 99
34582, V, 1, 1, 1, 1, 0, 700, 99
34583, V, 1, 1, 1, 1, 0, 700, 99
34584, V, 1, 1, 1, 1, 0, 700, 99
34585, V, 1, 1, 1, 1, 0, 700, 99
34586, V, 1, 1, 1, 1, 0, 700, 99
34587, V, 1, 1, 1, 1, 0, 700, 99
34588, V, 1, 1, 1, 1, 0, 700, 99
34589, V, 1, 1, 1, 1, 0, 700, 99
34590, V, 1, 1, 1, 1, 0, 700, 99
34591, V, 1, 1, 1, 1, 0, 700, 99
34592, V, 1, 1, 1, 1, 0, 700, 99
34593, V, 1, 1, 1, 1, 0, 700, 99
34594, V, 1, 1, 1, 1, 0, 700, 99
34595, V, 1, 1, 1, 1, 0, 700, 99
34596, V, 1, 1, 1, 1, 0, 700, 99
34597, V, 1, 1, 1, 1, 0, 700, 99
34598, V, 1, 1, 1, 1, 0, 700, 99
34599, V, 1, 1, 1, 1, 0, 700, 99
34600, V, 1, 1, 1, 1, 0, 700, 99
34601, V, 1, 1, 1, 1, 0, 700, 99
34603, V, 1, 1, 1, 1, 0, 700, 99
34604, V, 1, 1, 1, 1, 0, 700, 99
34605, V, 1, 1, 1, 1, 0, 700, 99
34606, V, 1, 1, 1, 1, 0, 700, 99
34607, V, 1, 1, 1, 1, 0, 700, 99
34608, V, 1, 1, 1, 1, 0, 700, 99
34609, V, 1, 1, 1, 1, 0, 700, 99
34610, V, 1, 1, 1, 1, 0, 700, 99
34611, V, 1, 1, 1, 1, 0, 700, 99
34612, V, 1, 1, 1, 1, 0, 700, 99
34613, V, 1, 1, 1, 1, 0, 700, 99
34614, V, 1, 1, 1, 1, 0, 700, 99
34615, V, 1, 1, 1, 1, 0, 700, 99
34616, V, 1, 1, 1, 1, 0, 700, 99
34617, V, 1, 1, 1, 1, 0, 700, 99
34618, V, 1, 1, 1, 1, 0, 700, 99
34619, V, 1, 1, 1, 1, 0, 700, 99
34620, V, 1, 1, 1, 1, 0, 700, 99
34621, V, 1, 1, 1, 1, 0, 700, 99
34622, V, 1, 1, 1, 1, 0, 700, 99
34623, V, 1, 1, 1, 1, 0, 700, 99
34624, V, 1, 1, 1, 1, 0, 700, 99
34625, V, 1, 1, 1, 1, 0, 700, 99
34626, V, 1, 1, 1, 1, 0, 700, 99
34627, V, 1, 1, 1, 1, 0, 700, 99
34628, V, 1, 1, 1, 1, 0, 700, 99
34629, V, 1, 1, 1, 1, 0, 700, 99
34630, V, 1, 1, 1, 1, 0, 700, 99
34631, V, 1, 1, 1, 1, 0, 700, 99
34632, V, 1, 1, 1, 1, 0, 700, 99
34633, V, 1, 1, 1, 1, 0, 700, 99
34634, V, 1, 1, 1, 1, 0, 700, 99
34635, V, 1, 1, 1, 1, 0, 700, 99
34636, V, 1, 1, 1, 1, 0, 700, 99
34637, V, 1, 1, 1, 1, 0, 700, 99
34638, V, 1, 1, 1, 1, 0, 700, 99
34639, V, 1, 1, 1, 1, 0, 700, 99
34640, V, 1, 1, 1, 1, 0, 700, 99
34641, V, 1, 1, 1, 1, 0, 700, 99
34642, V, 1, 1, 1, 1, 0, 700, 99
34643, V, 1, 1, 1, 1, 0, 700, 99
34644, V, 1, 1, 1, 1, 0, 700, 99
34646, V, 1, 1, 1, 1, 0, 700, 99
34647, V, 1, 1, 1, 1, 0, 700, 99
34648, V, 1, 1, 1, 1, 0, 700, 99
34649, V, 1, 1, 1, 1, 0, 700, 99
34650, V, 1, 1, 1, 1, 0, 700, 99
34651, V, 1, 1, 1, 1, 0, 700, 99
34652, V, 1, 1, 1, 1, 0, 700, 99
34653, V, 1, 1, 1, 1, 0, 700, 99
34654, V, 1, 1, 1, 1, 0, 700, 99
34655, V, 1, 1, 1, 1, 0, 700, 99
34656, V, 1, 1, 1, 1, 0, 700, 99
34657, V, 1, 1, 1, 1, 0, 700, 99
34658, V, 1, 1, 1, 1, 0, 700, 99
34659, V, 1, 1, 1, 1, 0, 700, 99
34660, V, 1, 1, 1, 1, 0, 700, 99
34661, V, 1, 1, 1, 1, 0, 700, 99
34662, V, 1, 1, 1, 1, 0, 700, 99
34663, V, 1, 1, 1, 1, 0, 700, 99
34664, V, 1, 1, 1, 1, 0, 700, 99
34665, V, 1, 1, 1, 1, 0, 700, 99
34666, V, 1, 1, 1, 1, 0, 700, 99
34667, V, 1, 1, 1, 1, 0, 700, 99
34668, V, 1, 1, 1, 1, 0, 700, 99
34669, V, 1, 1, 1, 1, 0, 700, 99
34670, V, 1, 1, 1, 1, 0, 700, 99
34671, V, 1, 1, 1, 1, 0, 700, 99
34672, V, 1, 1, 1, 1, 0, 700, 99
34673, V, 1, 1, 1, 1, 0, 700, 99
34674, V, 1, 1, 1, 1, 0, 700, 98
34675, V, 1, 1, 1, 1, 0, 700, 98
34676, V, 1, 1, 1, 1, 0, 700, 98
34677, V, 1, 1, 1, 1, 0, 700, 98
34678, V, 1, 1, 1, 1, 0, 700, 98
34679, V, 1, 1, 1, 1, 0, 700, 98
34680, V, 1, 1, 1, 1, 0, 700, 98
34681, V, 1, 1, 1, 1, 0, 700, 98
34682, V, 1, 1, 1, 1, 0, 700, 99
34683, V, 1, 1, 1, 1, 0, 700, 98
34684, V, 1, 1, 1, 1, 0, 700, 98
34685, V, 1, 1, 1, 1, 0, 700, 98
34686, V, 1, 1, 1, 1, 0, 700, 98
34688, V, 1, 1, 1, 1, 0, 700, 98
34689, V, 1, 1, 1, 1, 0, 700, 98
34690, V, 1, 1, 1, 1, 0, 700, 98
34691, V, 1, 1, 1, 1, 0, 700, 98
34692, V, 1, 1, 1, 1, 0, 700, 98
34693, V, 1, 1, 1, 1, 0, 700, 98
34694, V, 1, 1, 1, 1, 0, 700, 98
34695, V, 1, 1, 1, 1, 0, 700, 98
34696, V, 1, 1, 1, 1, 0, 700, 98
34697, V, 1, 1, 1, 1, 0, 700, 99
34698, V, 1, 1, 1, 1, 0, 700, 98
34699, V, 1, 1, 1, 1, 0, 700, 98
34700, V, 1, 1, 1, 1, 0, 700, 98
34701, V, 1, 1, 1, 1, 0, 700, 98
34702, V, 1, 1, 1, 1, 0, 700, 98
34703, V, 1, 1, 1, 1, 0, 700, 98
34704, V, 1, 1, 1, 1, 0, 700, 98
34705, V, 1, 1, 1, 1, 0, 700, 99
34706, V, 1, 1, 1, 1, 0, 700, 99
34707, V, 1, 1, 1, 1, 0, 700, 99
34708, V, 1, 1, 1, 1, 0, 700, 99
34709, V, 1, 1, 1, 1, 0, 700, 99
34710, V, 1, 1, 1, 1, 0, 700, 99
34711, V, 1, 1, 1, 1, 0, 700, 99
34712, V, 1, 1, 1, 1, 0, 700, 99
34713, V, 1, 1, 1, 1, 0, 700, 98
34714, V, 1, 1, 1, 1, 0, 700, 99
34715, V, 1, 1, 1, 1, 0, 700, 99
34716, V, 1, 1, 1, 1, 0, 700, 99
34717, V, 1, 1, 1, 1, 0, 700, 99
34718, V, 1, 1, 1, 1, 0, 700, 99
34719, V, 1, 1, 1, 1, 0, 700, 99
34720, V, 1, 1, 1, 1, 0, 700, 99
34721, V, 1, 1, 1, 1, 0, 700, 99
34722, V, 1, 1, 1, 1, 0, 700, 99
34723, V, 1, 1, 1, 1, 0, 700, 99
34724, V, 1, 1, 1, 1, 0, 700, 99
34725, V, 1, 1, 1, 1, 0, 700, 99
34726, V, 1, 1, 1, 1, 0, 700, 99
34727, V, 1, 1, 1, 1, 0, 700, 99
34728, V, 1, 1, 1, 1, 0, 700, 99
34729, V, 1, 1, 1, 1, 0, 700, 99
34731, V, 1, 1, 1, 1, 0, 700, 99
34732, V, 1, 1, 1, 1, 0, 700, 99
34733, V, 1, 1, 1, 1, 0, 700, 99
34734, V, 1, 1, 1, 1, 0, 700, 99
34735, V, 1, 1, 1, 1, 0, 700, 99
34736, V, 1, 1, 1, 1, 0, 700, 99
34737, V, 1, 1, 1, 1, 0, 700, 99
34738, V, 1, 1, 1, 1, 0, 700, 99
34739, V, 1, 1, 1, 1, 0, 700, 99
34740, V, 1, 1, 1, 1, 0, 700, 99
34741, V, 1, 1, 1, 1, 0, 700, 99
34742, V, 1, 1, 1, 1, 0, 700, 99
34743, V, 1, 1, 1, 1, 0, 700, 99
34744, V, 1, 1, 1, 1, 0, 700, 99
34745, V, 1, 1, 1, 1, 0, 700, 99
34746, V, 1, 1, 1, 1, 0, 700, 99
34747, V, 1, 1, 1, 1, 0, 700, 99
34748, V, 1, 1, 1, 1, 0, 700, 99
34749, V, 1, 1, 1, 1, 0, 700, 99
34750, V, 1, 1, 1, 1, 0, 700, 99
34751, V, 1, 1, 1, 1, 0, 700, 99
34752, V, 1, 1, 1, 1, 0, 700, 99
34753, V, 1, 1, 1, 1, 0, 700, 99
34754, V, 1, 1, 1, 1, 0, 700, 99
34755, V, 1, 1, 1, 1, 0, 700, 99
34756, V, 1, 1, 1, 1, 0, 700, 99
34757, V, 1, 1, 1, 1, 0, 700, 99
34758, V, 1, 1, 1, 1, 0, 700, 99
34759, V, 1, 1, 1, 1, 0, 700, 99
34760, V, 1, 1, 1, 1, 0, 700, 99
34761, V, 1, 1, 1, 1, 0, 700, 99
34762, V, 1, 1, 1, 1, 0, 700, 99
34763, V, 1, 1, 1, 1, 0, 700, 99
34764, V, 1, 1, 1, 1, 0, 700, 99
34765, V, 1, 1, 1, 1, 0, 700, 99
34766, V, 1, 1, 1, 1, 0, 700, 99
34767, V, 1, 1, 1, 1, 0, 700, 99
34768, V, 1, 1, 1, 1, 0, 700, 99
34769, V, 1, 1, 1, 1, 0, 700, 99
34770, V, 1, 1, 1, 1, 0, 700, 99
34771, V, 1, 1, 1, 1, 0, 700, 99
34772, V, 1, 1, 1, 1, 0, 700, 99
34774, V, 1, 1, 1, 1, 0, 700, 99
34775, V, 1, 1, 1, 1, 0, 700, 99
34776, V, 1, 1, 1, 1, 0, 700, 99
34777, V, 1, 1, 1, 1, 0, 700, 99
34778, V, 1, 1, 1, 1, 0, 700, 99
34779, V, 1, 1, 1, 1, 0, 700, 99
34780, V, 1, 1, 1, 1, 0, 700, 99
34781, V, 1, 1, 1, 1, 0, 700, 99
34782, V, 1, 1, 1, 1, 0, 700, 99
34783, V, 1, 1, 1, 1, 0, 700, 99
34784, V, 1, 1, 1, 1, 0, 700, 99
34785, V, 1, 1, 1, 1, 0, 700, 99
34786, V, 1, 1, 1, 1, 0, 700, 99
34787, V, 1, 1, 1, 1, 0, 700, 99
34788, V, 1, 1, 1, 1, 0, 700, 99
34789, V, 1, 1, 1, 1, 0, 700, 99
34790, V, 1, 1, 1, 1, 0, 700, 99
34791, V, 1, 1, 1, 1, 0, 700, 99
34792, V, 1, 1, 1, 1, 0, 700, 99
34793, V, 1, 1, 1, 1, 0, 700, 99
34794, V, 1, 1, 1, 1, 0, 700, 99
34795, V, 1, 1, 1, 1, 0, 700, 99
34796, V, 1, 1, 1, 1, 0, 700, 99
34797, V, 1, 1, 1, 1, 0, 700, 99
34798, V, 1, 1, 1, 1, 0, 700, 99
34799, V, 1, 1, 1, 1, 0, 700, 99
34800, V, 1, 1, 1, 1, 0, 700, 99
34801, V, 1, 1, 1, 1, 0, 700, 99
34802, V, 1, 1, 1, 1, 0, 700, 99
34803, V, 1, 1, 1, 1, 0, 700, 99
34804, V, 1, 1, 1, 1, 0, 700, 99
34805, V, 1, 1, 1, 1, 0, 700, 99
34806, V, 1, 1, 1, 1, 0, 700, 99
34807, V, 1, 1, 1, 1, 0, 700, 99
34808, V, 1, 1, 1, 1, 0, 700, 99
34809, V, 1, 1, 1, 1, 0, 700, 99
34810, V, 1, 1, 1, 1, 0, 700, 99
34811, V, 1, 1, 1, 1, 0, 700, 99
34812, V, 1, 1, 1, 1, 0, 700, 99
34813, V, 1, 1, 1, 1, 0, 700, 99
34814, V, 1, 1, 1, 1, 0, 700, 99
34816, V, 1, 1, 1, 1, 0, 700, 99
34817, V, 1, 1, 1, 1, 0, 700, 99
34818, V, 1, 1, 1, 1, 0, 700, 99
34819, V, 1, 1, 1, 1, 0, 700, 99
34820, V, 1, 1, 1, 1, 0, 700, 99
34821, V, 1, 1, 1, 1, 0, 700, 99
34822, V, 1, 1, 1, 1, 0, 700, 99
34823, V, 1, 1, 1, 1, 0, 700, 99
34824, V, 1, 1, 1, 1, 0, 700, 99
34825, V, 1, 1, 1, 1, 0, 700, 99
34826, V, 1, 1, 1, 1, 0, 700, 99
34827, V, 1, 1, 1, 1, 0, 700, 99
34828, V, 1, 1, 1, 1, 0, 700, 99
34829, V, 1, 1, 1, 1, 0, 700, 99
34830, V, 1, 1, 1, 1, 0, 700, 99
34831, V, 1, 1, 1, 1, 0, 700, 99
34832, V, 1, 1, 1, 1, 0, 700, 99
34833, V, 1, 1, 1, 1, 0, 700, 99
34834, V, 1, 1, 1, 1, 0, 700, 99
34835, V, 1, 1, 1, 1, 0, 700, 99
34836, V, 1, 1, 1, 1, 0, 700, 99
34837, V, 1, 1, 1, 1, 0, 700, 98
34838, V, 1, 1, 1, 1, 0, 700, 99
34839, V, 1, 1, 1, 1, 0, 700, 99
34840, V, 1, 1, 1, 1, 0, 700, 99
34841, V, 1, 1, 1, 1, 0, 700, 99
34842, V, 1, 1, 1, 1, 0, 700, 99
34843, V, 1, 1, 1, 1, 0, 700, 99
34844, V, 1, 1, 1, 1, 0, 700, 99
34845, V, 1, 1, 1, 1, 0, 700, 99
34846, V, 1, 1, 1, 1, 0, 700, 99
34847, V, 1, 1, 1, 1, 0, 700, 99
34848, V, 1, 1, 1, 1, 0, 700, 99
34849, V, 1, 1, 1, 1, 0, 700, 99
34850, V, 1, 1, 1, 1, 0, 700, 99
34851, V, 1, 1, 1, 1, 0, 700, 99
34852, V, 1, 1, 1, 1, 0, 700, 99
34853, V, 1, 1, 1, 1, 0, 700, 99
34854, V, 1, 1, 1, 1, 0, 700, 99
34855, V, 1, 1, 1, 1, 0, 700, 99
34856, V, 1, 1, 1, 1, 0, 700, 99
34857, V, 1, 1, 1, 1, 0, 700, 99
34859, V, 1, 1, 1, 1, 0, 700, 99
34860, V, 1, 1, 1, 1, 0, 700, 99
34861, V, 1, 1, 1, 1, 0, 700, 99
34862, V, 1, 1, 1, 1, 0, 700, 99
34863, V, 1, 1, 1, 1, 0, 700, 99
34864, V, 1, 1, 1, 1, 0, 700, 99
34865, V, 1, 1, 1, 1, 0, 700, 99
34866, V, 1, 1, 1, 1, 0, 700, 99
34867, V, 1, 1, 1, 1, 0, 700, 99
34868, V, 1, 1, 1, 1, 0, 700, 99
34869, V, 1, 1, 1, 1, 0, 700, 99
34870, V, 1, 1, 1, 1, 0, 700, 99
34871, V, 1, 1, 1, 1, 0, 700, 99
34872, V, 1, 1, 1, 1, 0, 700, 99
34873, V, 1, 1, 1, 1, 0, 700, 99
34874, V, 1, 1, 1, 1, 0, 700, 99
34875, V, 1, 1, 1, 1, 0, 700, 99
34876, V, 1, 1, 1, 1, 0, 700, 99
34877, V, 1, 1, 1, 1, 0, 700, 99
34878, V, 1, 1, 1, 1, 0, 700, 99
34879, V, 1, 1, 1, 1, 0, 700, 99
34880, V, 1, 1, 1, 1, 0, 700, 99
34881, V, 1, 1, 1, 1, 0, 700, 99
34882, V, 1, 1, 1, 1, 0, 700, 99
34883, V, 1, 1, 1, 1, 0, 700, 99
34884, V, 1, 1, 1, 1, 0, 700, 99
34885, V, 1, 1, 1, 1, 0, 700, 99
34886, V, 1, 1, 1, 1, 0, 700, 99
34887, V, 1, 1, 1, 1, 0, 700, 99
34888, V, 1, 1, 1, 1, 0, 700, 99
34889, V, 1, 1, 1, 1, 0, 700, 99
34890, V, 1, 1, 1, 1, 0, 700, 99
34891, V, 1, 1, 1, 1, 0, 700, 99
34892, V, 1, 1, 1, 1, 0, 700, 99
34893, V, 1, 1, 1, 1, 0, 700, 99
34894, V, 1, 1, 1, 1, 0, 700, 99
34895, V, 1, 1, 1, 1, 0, 700, 99
34896, V, 1, 1, 1, 1, 0, 700, 99
34897, V, 1, 1, 1, 1, 0, 700, 99
34898, V, 1, 1, 1, 1, 0, 700, 99
34899, V, 1, 1, 1, 1, 0, 700, 99
34900, V, 1, 1, 1, 1, 0, 700, 99
34902, V, 1, 1, 1, 1, 0, 700, 99
34903, V, 1, 1, 1, 1, 0, 700, 99
34904, V, 1, 1, 1, 1, 0, 700, 99
34905, V, 1, 1, 1, 1, 0, 700, 99
34906, V, 1, 1, 1, 1, 0, 700, 99
34907, V, 1, 1, 1, 1, 0, 700, 99
34908, V, 1, 1, 1, 1, 0, 700, 99
34909, V, 1, 1, 1, 1, 0, 700, 99
34910, V, 1, 1, 1, 1, 0, 700, 99
34911, V, 1, 1, 1, 1, 0, 700, 99
34912, V, 1, 1, 1, 1, 0, 700, 99
34913, V, 1, 1, 1, 1, 0, 700, 99
34914, V, 1, 1, 1, 1, 0, 700, 99
34915, V, 1, 1, 1, 1, 0, 700, 99
34916, V, 1, 1, 1, 1, 0, 700, 99
34917, V, 1, 1, 1, 1, 0, 700, 99
34918, V, 1, 1, 1, 1, 0, 700, 99
34919, V, 1, 1, 1, 1, 0, 700, 99
34920, V, 1, 1, 1, 1, 0, 700, 99
34921, V, 1, 1, 1, 1, 0, 700, 99
34922, V, 1, 1, 1, 1, 0, 700, 99
34923, V, 1, 1, 1, 1, 0, 700, 99
34924, V, 1, 1, 1, 1, 0, 700, 99
34925, V, 1, 1, 1, 1, 0, 700, 99
34926, V, 1, 1, 1, 1, 0, 700, 99
34927, V, 1, 1, 1, 1, 0, 700, 99
34928, V, 1, 1, 1, 1, 0, 700, 99
34929, V, 1, 1, 1, 1, 0, 700, 99
34930, V, 1, 1, 1, 1, 0, 700, 99
34931, V, 1, 1, 1, 1, 0, 700, 99
34932, V, 1, 1, 1, 1, 0, 700, 99
34933, V, 1, 1, 1, 1, 0, 700, 99
34934, V, 1, 1, 1, 1, 0, 700, 99
34935, V, 1, 1, 1, 1, 0, 700, 99
34936, V, 1, 1, 1, 1, 0, 700, 99
34937, V, 1, 1, 1, 1, 0, 700, 99
34938, V, 1, 1, 1, 1, 0, 700, 99
34939, V, 1, 1, 1, 1, 0, 700, 99
34940, V, 1, 1, 1, 1, 0, 700, 99
34941, V, 1, 1, 1, 1, 0, 700, 99
34942, V, 1, 1, 1, 1, 0, 700, 99
34944, V, 1, 1, 1, 1, 0, 700, 99
34945, V, 1, 1, 1, 1, 0, 700, 99
34946, V, 1, 1, 1, 1, 0, 700, 99
34947, V, 1, 1, 1, 1, 0, 700, 99
34948, V, 1, 1, 1, 1, 0, 700, 99
34949, V, 1, 1, 1, 1, 0, 700, 99
34950, V, 1, 1, 1, 1, 0, 700, 99
34951, V, 1, 1, 1, 1, 0, 700, 99
34952, V, 1, 1, 1, 1, 0, 700, 99
34953, V, 1, 1, 1, 1, 0, 700, 99
34954, V, 1, 1, 1, 1, 0, 700, 99
34955, V, 1, 1, 1, 1, 0, 700, 99
34956, V, 1, 1, 1, 1, 0, 700, 99
34957, V, 1, 1, 1, 1, 0, 700, 99
34958, V, 1, 1, 1, 1, 0, 700, 99
34959, V, 1, 1, 1, 1, 0, 700, 99
34960, V, 1, 1, 1, 1, 0, 700, 99
34961, V, 1, 1, 1, 1, 0, 700, 99
34962, V, 1, 1, 1, 1, 0, 700, 99
34963, V, 1, 1, 1, 1, 0, 700, 99
34964, V, 1, 1, 1, 1, 0, 700, 99
34965, V, 1, 1, 1, 1, 0, 700, 99
34966, V, 1, 1, 1, 1, 0, 700, 99
34967, V, 1, 1, 1, 1, 0, 700, 99
34968, V, 1, 1, 1, 1, 0, 700, 99
34969, V, 1, 1, 1, 1, 0, 700, 99
34970, V, 1, 1, 1, 1, 0, 700, 99
34971, V, 1, 1, 1, 1, 0, 700, 99
34972, V, 1, 1, 1, 1, 0, 700, 99
34973, V, 1, 1, 1, 1, 0, 700, 99
34974, V, 1, 1, 1, 1, 0, 700, 99
34975, V, 1, 1, 1, 1, 0, 700, 99
34976, V, 1, 1, 1, 1, 0, 700, 99
34977, V, 1, 1, 1, 1, 0, 700, 99
34978, V, 1, 1, 1, 1, 0, 700, 99
34979, V, 1, 1, 1, 1, 0, 700, 99
34980, V, 1, 1, 1, 1, 0, 700, 99
34981, V, 1, 1, 1, 1, 0, 700, 99
34982, V, 1, 1, 1, 1, 0, 700, 99
34983, V, 1, 1, 1, 1, 0, 700, 99
34984, V, 1, 1, 1, 1, 0, 700, 99
34985, V, 1, 1, 1, 1, 0, 700, 99
34987, V, 1, 1, 1, 1, 0, 700, 99
34988, V, 1, 1, 1, 1, 0, 700, 99
34989, V, 1, 1, 1, 1, 0, 700, 99
34990, V, 1, 1, 1, 1, 0, 700, 99
34991, V, 1, 1, 1, 1, 0, 700, 99
34992, V, 1, 1, 1, 1, 0, 700, 99
34993, V, 1, 1, 1, 1, 0, 700, 99
34994, V, 1, 1, 1, 1, 0, 700, 99
34995, V, 1, 1, 1, 1, 0, 700, 99
34996, V, 1, 1, 1, 1, 0, 700, 99
34997, V, 1, 1, 1, 1, 0, 700, 99
34998, V, 1, 1, 1, 1, 0, 700, 99
34999, V, 1, 1, 1, 1, 0, 700, 99
35000, V, 1, 1, 1, 1, 0, 700, 99
35001, V, 1, 1, 1, 1, 0, 700, 99
35002, V, 1, 1, 1, 1, 0, 700, 99
35003, V, 1, 1, 1, 1, 0, 700, 99
35004, V, 1, 1, 1, 1, 0, 700, 99
35005, V, 1, 1, 1, 1, 0, 700, 99
35006, V, 1, 1, 1, 1, 0, 700, 99
35007, V, 1, 1, 1, 1, 0, 700, 99
35008, V, 1, 1, 1, 1, 0, 700, 99
35009, V, 1, 1, 1, 1, 0, 700, 99
35010, V, 1, 1, 1, 1, 0, 700, 99
35011, V, 1, 1, 1, 1, 0, 700, 99
35012, V, 1, 1, 1, 1, 0, 700, 99
35013, V, 1, 1, 1, 1, 0, 700, 99
35014, V, 1, 1, 1, 1, 0, 700, 99
35015, V, 1, 1, 1, 1, 0, 700, 99
35016, V, 1, 1, 1, 1, 0, 700, 99
35017, V, 1, 1, 1, 1, 0, 700, 99
35018, V, 1, 1, 1, 1, 0, 700, 99
35019, V, 1, 1, 1, 1, 0, 700, 99
35020, V, 1, 1, 1, 1, 0, 700, 99
35021, V, 1, 1, 1, 1, 0, 700, 99
35022, V, 1, 1, 1, 1, 0, 700, 99
35023, V, 1, 1, 1, 1, 0, 700, 99
35024, V, 1, 1, 1, 1, 0, 700, 99
35025, V, 1, 1, 1, 1, 0, 700, 99
35026, V, 1, 1, 1, 1, 0, 700, 99
35027, V, 1, 1, 1, 1, 0, 700, 99
35028, V, 1, 1, 1, 1, 0, 700, 99
35030, V, 1, 1, 1, 1, 0, 700, 99
35031, V, 1, 1, 1, 1, 0, 700, 99
35032, V, 1, 1, 1, 1, 0, 700, 99
35033, V, 1, 1, 1, 1, 0, 700, 99
35034, V, 1, 1, 1, 1, 0, 700, 99
35035, V, 1, 1, 1, 1, 0, 700, 99
35036, V, 1, 1, 1, 1, 0, 700, 99
35037, V, 1, 1, 1, 1, 0, 700, 99
35038, V, 1, 1, 1, 1, 0, 700, 99
35039, V, 1, 1, 1, 1, 0, 700, 99
35040, V, 1, 1, 1, 1, 0, 700, 99
35041, V, 1, 1, 1, 1, 0, 700, 99
35042, V, 1, 1, 1, 1, 0, 700, 99
35043, V, 1, 1, 1, 1, 0, 700, 99
35044, V, 1, 1, 1, 1, 0, 700, 99
35045, V, 1, 1, 1, 1, 0, 700, 99
35046, V, 1, 1, 1, 1, 0, 700, 99
35047, V, 1, 1, 1, 1, 0, 700, 99
35048, V, 1, 1, 1, 1, 0, 700, 99
35049, V, 1, 1, 1, 1, 0, 700, 99
35050, V, 1, 1, 1, 1, 0, 700, 99
35051, V, 1, 1, 1, 1, 0, 700, 99
35052, V, 1, 1, 1, 1, 0, 700, 99
35053, V, 1, 1, 1, 1, 0, 700, 99
35054, V, 1, 1, 1, 1, 0, 700, 99
35055, V, 1, 1, 1, 1, 0, 700, 99
35056, V, 1, 1, 1, 1, 0, 700, 99
35057, V, 1, 1, 1, 1, 0, 700, 99
35058, V, 1, 1, 1, 1, 0, 700, 99
35059, V, 1, 1, 1, 1, 0, 700, 99
35060, V, 1, 1, 1, 1, 0, 700, 99
35061, V, 1, 1, 1, 1, 0, 700, 99
35062, V, 1, 1, 1, 1, 0, 700, 99
35063, V, 1, 1, 1, 1, 0, 700, 99
35064, V, 1, 1, 1, 1, 0, 700, 99
35065, V, 1, 1, 1, 1, 0, 700, 99
35066, V, 1, 1, 1, 1, 0, 700, 99
35067, V, 1, 1, 1, 1, 0, 700, 99
35068, V, 1, 1, 1, 1, 0, 700, 99
35069, V, 1, 1, 1, 1, 0, 700, 99
35070, V, 1, 1, 1, 1, 0, 700, 99
35072, V, 1, 1, 1, 1, 0, 700, 99
35073, V, 1, 1, 1, 1, 0, 700, 99
35074, V, 1, 1, 1, 1, 0, 700, 99
35075, V, 1, 1, 1, 1, 0, 700, 99
35076, V, 1, 1, 1, 1, 0, 700, 99
35077, V, 1, 1, 1, 1, 0, 700, 99
35078, V, 1, 1, 1, 1, 0, 700, 99
35079, V, 1, 1, 1, 1, 0, 700, 99
35080, V, 1, 1, 1, 1, 0, 700, 99
35081, V, 1, 1, 1, 1, 0, 700, 99
35082, V, 1, 1, 1, 1, 0, 700, 99
35083, V, 1, 1, 1, 1, 0, 700, 99
35084, V, 1, 1, 1, 1, 0, 700, 99
35085, V, 1, 1, 1, 1, 0, 700, 99
35086, V, 1, 1, 1, 1, 0, 700, 99
35087, V, 1, 1, 1, 1, 0, 700, 99
35088, V, 1, 1, 1, 1, 0, 700, 99
35089, V, 1, 1, 1, 1, 0, 700, 99
35090, V, 1, 1, 1, 1, 0, 700, 99
35091, V, 1, 1, 1, 1, 0, 700, 99
35092, V, 1, 1, 1, 1, 0, 700, 99
35093, V, 1, 1, 1, 1, 0, 700, 99
35094, V, 1, 1, 1, 1, 0, 700, 99
35095, V, 1, 1, 1, 1, 0, 700, 99
35096, V, 1, 1, 1, 1, 0, 700, 99
35097, V, 1, 1, 1, 1, 0, 700, 99
35098, V, 1, 1, 1, 1, 0, 700, 99
35099, V, 1, 1, 1, 1, 0, 700, 99
35100, V, 1, 1, 1, 1, 0, 700, 99
35101, V, 1, 1, 1, 1, 0, 700, 99
35102, V, 1, 1, 1, 1, 0, 700, 99
35103, V, 1, 1, 1, 1, 0, 700, 99
35104, V, 1, 1, 1, 1, 0, 700, 99
35105, V, 1, 1, 1, 1, 0, 700, 99
35106, V, 1, 1, 1, 1, 0, 700, 99
35107, V, 1, 1, 1, 1, 0, 700, 99
35108, V, 1, 1, 1, 1, 0, 700, 99
35109, V, 1, 1, 1, 1, 0, 700, 99
35110, V, 1, 1, 1, 1, 0, 700, 99
35111, V, 1, 1, 1, 1, 0, 700, 99
35112, V, 1, 1, 1, 1, 0, 700, 99
35113, V, 1, 1, 1, 1, 0, 700, 99
35115, V, 1, 1, 1, 1, 0, 700, 99
35116, V, 1, 1, 1, 1, 0, 700, 99
35117, V, 1, 1, 1, 1, 0, 700, 99
35118, V, 1, 1, 1, 1, 0, 700, 99
35119, V, 1, 1, 1, 1, 0, 700, 99
35120, V, 1, 1, 1, 1, 0, 700, 99
35121, V, 1, 1, 1, 1, 0, 700, 99
35122, V, 1, 1, 1, 1, 0, 700, 99
35123, V, 1, 1, 1, 1, 0, 700, 99
35124, V, 1, 1, 1, 1, 0, 700, 99
35125, V, 1, 1, 1, 1, 0, 700, 99
35126, V, 1, 1, 1, 1, 0, 700, 99
35127, V, 1, 1, 1, 1, 0, 700, 99
35128, V, 1, 1, 1, 1, 0, 700, 99
35129, V, 1, 1, 1, 1, 0, 700, 99
35130, V, 1, 1, 1, 1, 0, 700, 99
35131, V, 1, 1, 1, 1, 0, 700, 99
35132, V, 1, 1, 1, 1, 0, 700, 99
35133, V, 1, 1, 1, 1, 0, 700, 99
35134, V, 1, 1, 1, 1, 0, 700, 99
35135, V, 1, 1, 1, 1, 0, 700, 99
35136, V, 1, 1, 1, 1, 0, 700, 99
35137, V, 1, 1, 1, 1, 0, 700, 99
35138, V, 1, 1, 1, 1, 0, 700, 99
35139, V, 1, 1, 1, 1, 0, 700, 99
35140, V, 1, 1, 1, 1, 0, 700, 99
35141, V, 1, 1, 1, 1, 0, 700, 99
35142, V, 1, 1, 1, 1, 0, 700, 99
35143, V, 1, 1, 1, 1, 0, 700, 99
35144, V, 1, 1, 1, 1, 0, 700, 99
35145, V, 1, 1, 1, 1, 0, 700, 99
35146, V, 1, 1, 1, 1, 0, 700, 99
35147, V, 1, 1, 1, 1, 0, 700, 99
35148, V, 1, 1, 1, 1, 0, 700, 99
35149, V, 1, 1, 1, 1, 0, 700, 99
35150, V, 1, 1, 1, 1, 0, 700, 99
35151, V, 1, 1, 1, 1, 0, 700, 99
35152, V, 1, 1, 1, 1, 0, 700, 99
35153, V, 1, 1, 1, 1, 0, 700, 99
35154, V, 1, 1, 1, 1, 0, 700, 99
35155, V, 1, 1, 1, 1, 0, 700, 99
35156, V, 1, 1, 1, 1, 0, 700, 99
35158, V, 1, 1, 1, 1, 0, 700, 99
35159, V, 1, 1, 1, 1, 0, 700, 99
35160, V, 1, 1, 1, 1, 0, 700, 99
35161, V, 1, 1, 1, 1, 0, 700, 99
35162, V, 1, 1, 1, 1, 0, 700, 99
35163, V, 1, 1, 1, 1, 0, 700, 99
35164, V, 1, 1, 1, 1, 0, 700, 99
35165, V, 1, 1, 1, 1, 0, 700, 99
35166, V, 1, 1, 1, 1, 0, 700, 99
35167, V, 1, 1, 1, 1, 0, 700, 99
35168, V, 1, 1, 1, 1, 0, 700, 99
35169, V, 1, 1, 1, 1, 0, 700, 99
35170, V, 1, 1, 1, 1, 0, 700, 99
35171, V, 1, 1, 1, 1, 0, 700, 99
35172, V, 1, 1, 1, 1, 0, 700, 99
35173, V, 1, 1, 1, 1, 0, 700, 99
35174, V, 1, 1, 1, 1, 0, 700, 99
35175, V, 1, 1, 1, 1, 0, 700, 99
35176, V, 1, 1, 1, 1, 0, 700, 99
35177, V, 1, 1, 1, 1, 0, 700, 99
35178, V, 1, 1, 1, 1, 0, 700, 99
35179, V, 1, 1, 1, 1, 0, 700, 99
35180, V, 1, 1, 1, 1, 0, 700, 99
35181, V, 1, 1, 1, 1, 0, 700, 99
35182, V, 1, 1, 1, 1, 0, 700, 99
35183, V, 1, 1, 1, 1, 0, 700, 99
35184, V, 1, 1, 1, 1, 0, 700, 99
35185, V, 1, 1, 1, 1, 0, 700, 99
35186, V, 1, 1, 1, 1, 0, 700, 99
35187, V, 1, 1, 1, 1, 0, 700, 99
35188, V, 1, 1, 1, 1, 0, 700, 99
35189, V, 1, 1, 1, 1, 0, 700, 99
35190, V, 1, 1, 1, 1, 0, 700, 99
35191, V, 1, 1, 1, 1, 0, 700, 99
35192, V, 1, 1, 1, 1, 0, 700, 99
35193, V, 1, 1, 1, 1, 0, 700, 99
35194, V, 1, 1, 1, 1, 0, 700, 99
35195, V, 1, 1, 1, 1, 0, 700, 99
35196, V, 1, 1, 1, 1, 0, 700, 99
35197, V, 1, 1, 1, 1, 0, 700, 99
35198, V, 1, 1, 1, 1, 0, 700, 99
35200, V, 1, 1, 1, 1, 0, 700, 99
35201, V, 1, 1, 1, 1, 0, 700, 99
35202, V, 1, 1, 1, 1, 0, 700, 99
35203, V, 1, 1, 1, 1, 0, 700, 99
35204, V, 1, 1, 1, 1, 0, 700, 99
35205, V, 1, 1, 1, 1, 0, 700, 99
35206, V, 1, 1, 1, 1, 0, 700, 99
35207, V, 1, 1, 1, 1, 0, 700, 99
35208, V, 1, 1, 1, 1, 0, 700, 99
35209, V, 1, 1, 1, 1, 0, 700, 99
35210, V, 1, 1, 1, 1, 0, 700, 99
35211, V, 1, 1, 1, 1, 0, 700, 99
35212, V, 1, 1, 1, 1, 0, 700, 99
35213, V, 1, 1, 1, 1, 0, 700, 99
35214, V, 1, 1, 1, 1, 0, 700, 99
35215, V, 1, 1, 1, 1, 0, 700, 99
35216, V, 1, 1, 1, 1, 0, 700, 99
35217, V, 1, 1, 1, 1, 0, 700, 99
35218, V, 1, 1, 1, 1, 0, 700, 99
35219, V, 1, 1, 1, 1, 0, 700, 99
35220, V, 1, 1, 1, 1, 0, 700, 99
35221, V, 1, 1, 1, 1, 0, 700, 99
35222, V, 1, 1, 1, 1, 0, 700, 99
35223, V, 1, 1, 1, 1, 0, 700, 99
35224, V, 1, 1, 1, 1, 0, 700, 99
35225, V, 1, 1, 1, 1, 0, 700, 99
35226, V, 1, 1, 1, 1, 0, 700, 99
35227, V, 1, 1, 1, 1, 0, 700, 99
35228, V, 1, 1, 1, 1, 0, 700, 99
35229, V, 1, 1, 1, 1, 0, 700, 99
35230, V, 1, 1, 1, 1, 0, 700, 99
35231, V, 1, 1, 1, 1, 0, 700, 99
35232, V, 1, 1, 1, 1, 0, 700, 99
35233, V, 1, 1, 1, 1, 0, 700, 99
35234, V, 1, 1, 1, 1, 0, 700, 99
35235, V, 1, 1, 1, 1, 0, 700, 99
35236, V, 1, 1, 1, 1, 0, 700, 99
35237, V, 1, 1, 1, 1, 0, 700, 99
35238, V, 1, 1, 1, 1, 0, 700, 99
35239, V, 1, 1, 1, 1, 0, 700, 99
35240, V, 1, 1, 1, 1, 0, 700, 99
35241, V, 1, 1, 1, 1, 0, 700, 99
35243, V, 1, 1, 1, 1, 0, 700, 99
35244, V, 1, 1, 1, 1, 0, 700, 99
35245, V, 1, 1, 1, 1, 0, 700, 99
35246, V, 1, 1, 1, 1, 0, 700, 99
35247, V, 1, 1, 1, 1, 0, 700, 99
35248, V, 1, 1, 1, 1, 0, 700, 99
35249, V, 1, 1, 1, 1, 0, 700, 99
35250, V, 1, 1, 1, 1, 0, 700, 99
35251, V, 1, 1, 1, 1, 0, 700, 99
35252, V, 1, 1, 1, 1, 0, 700, 99
35253, V, 1, 1, 1, 1, 0, 700, 99
35254, V, 1, 1, 1, 1, 0, 700, 99
35255, V, 1, 1, 1, 1, 0, 700, 99
35256, V, 1, 1, 1, 1, 0, 700, 99
35257, V, 1, 1, 1, 1, 0, 700, 99
35258, V, 1, 1, 1, 1, 0, 700, 99
35259, V, 1, 1, 1, 1, 0, 700, 99
35260, V, 1, 1, 1, 1, 0, 700, 99
35261, V, 1, 1, 1, 1, 0, 700, 99
35262, V, 1, 1, 1, 1, 0, 700, 99
35263, V, 1, 1, 1, 1, 0, 700, 99
35264, V, 1, 1, 1, 1, 0, 700, 99
35265, V, 1, 1, 1, 1, 0, 700, 99
35266, V, 1, 1, 1, 1, 0, 700, 99
35267, V, 1, 1, 1, 1, 0, 700, 99
35268, V, 1, 1, 1, 1, 0, 700, 99
35269, V, 1, 1, 1, 1, 0, 700, 99
35270, V, 1, 1, 1, 1, 0, 700, 99
35271, V, 1, 1, 1, 1, 0, 700, 99
35272, V, 1, 1, 1, 1, 0, 700, 99
35273, V, 1, 1, 1, 1, 0, 700, 99
35274, V, 1, 1, 1, 1, 0, 700, 99
35275, V, 1, 1, 1, 1, 0, 700, 99
35276, V, 1, 1, 1, 1, 0, 700, 99
35277, V, 1, 1, 1, 1, 0, 700, 99
35278, V, 1, 1, 1, 1, 0, 700, 99
35279, V, 1, 1, 1, 1, 0, 700, 99
35280, V, 1, 1, 1, 1, 0, 700, 99
35281, V, 1, 1, 1, 1, 0, 700, 99
35282, V, 1, 1, 1, 1, 0, 700, 99
35283, V, 1, 1, 1, 1, 0, 700, 99
35284, V, 1, 1, 1, 1, 0, 700, 99
35286, V, 1, 1, 1, 1, 0, 700, 99
35287, V, 1, 1, 1, 1, 0, 700, 99
35288, V, 1, 1, 1, 1, 0, 700, 99
35289, V, 1, 1, 1, 1, 0, 700, 99
35290, V, 1, 1, 1, 1, 0, 700, 99
35291, V, 1, 1, 1, 1, 0, 700, 99
35292, V, 1, 1, 1, 1, 0, 700, 99
35293, V, 1, 1, 1, 1, 0, 700, 99
35294, V, 1, 1, 1, 1, 0, 700, 99
35295, V, 1, 1, 1, 1, 0, 700, 99
35296, V, 1, 1, 1, 1, 0, 700, 99
35297, V, 1, 1, 1, 1, 0, 700, 99
35298, V, 1, 1, 1, 1, 0, 700, 99
35299, V, 1, 1, 1, 1, 0, 700, 99
35300, V, 1, 1, 1, 1, 0, 700, 99
35301, V, 1, 1, 1, 1, 0, 700, 99
35302, V, 1, 1, 1, 1, 0, 700, 99
35303, V, 1, 1, 1, 1, 0, 700, 99
35304, V, 1, 1, 1, 1, 0, 700, 99
35305, V, 1, 1, 1, 1, 0, 700, 99
35306, V, 1, 1, 1, 1, 0, 700, 99
35307, V, 1, 1, 1, 1, 0, 700, 99
35308, V, 1, 1, 1, 1, 0, 700, 99
35309, V, 1, 1, 1, 1, 0, 700, 99
35310, V, 1, 1, 1, 1, 0, 700, 99
35311, V, 1, 1, 1, 1, 0, 700, 99
35312, V, 1, 1, 1, 1, 0, 700, 99
35313, V, 1, 1, 1, 1, 0, 700, 99
35314, V, 1, 1, 1, 1, 0, 700, 99
35315, V, 1, 1, 1, 1, 0, 700, 99
35316, V, 1, 1, 1, 1, 0, 700, 99
35317, V, 1, 1, 1, 1, 0, 700, 99
35318, V, 1, 1, 1, 1, 0, 700, 99
35319, V, 1, 1, 1, 1, 0, 700, 99
35320, V, 1, 1, 1, 1, 0, 700, 99
35321, V, 1, 1, 1, 1, 0, 700, 99
35322, V, 1, 1, 1, 1, 0, 700, 99
35323, V, 1, 1, 1, 1, 0, 700, 99
35324, V, 1, 1, 1, 1, 0, 700, 99
35325, V, 1, 1, 1, 1, 0, 700, 99
35326, V, 1, 1, 1, 1, 0, 700, 99
35328, V, 1, 1, 1, 1, 0, 700, 99
35329, V, 1, 1, 1, 1, 0, 700, 99
35330, V, 1, 1, 1, 1, 0, 700, 99
35331, V, 1, 1, 1, 1, 0, 700, 99
35332, V, 1, 1, 1, 1, 0, 700, 99
35333, V, 1, 1, 1, 1, 0, 700, 99
35334, V, 1, 1, 1, 1, 0, 700, 99
35335, V, 1, 1, 1, 1, 0, 700, 99
35336, V, 1, 1, 1, 1, 0, 700, 99
35337, V, 1, 1, 1, 1, 0, 700, 99
35338, V, 1, 1, 1, 1, 0, 700, 99
35339, V, 1, 1, 1, 1, 0, 700, 99
35340, V, 1, 1, 1, 1, 0, 700, 99
35341, V, 1, 1, 1, 1, 0, 700, 99
35342, V, 1, 1, 1, 1, 0, 700, 99
35343, V, 1, 1, 1, 1, 0, 700, 99
35344, V, 1, 1, 1, 1, 0, 700, 99
35345, V, 1, 1, 1, 1, 0, 700, 99
35346, V, 1, 1, 1, 1, 0, 700, 99
35347, V, 1, 1, 1, 1, 0, 700, 99
35348, V, 1, 1, 1, 1, 0, 700, 99
35349, V, 1, 1, 1, 1, 0, 700, 99
35350, V, 1, 1, 1, 1, 0, 700, 99
35351, V, 1, 1, 1, 1, 0, 700, 99
35352, V, 1, 1, 1, 1, 0, 700, 99
35353, V, 1, 1, 1, 1, 0, 700, 99
35354, V, 1, 1, 1, 1, 0, 700, 99
35355, V, 1, 1, 1, 1, 0, 700, 99
35356, V, 1, 1, 1, 1, 0, 700, 99
35357, V, 1, 1, 1, 1, 0, 700, 99
35358, V, 1, 1, 1, 1, 0, 700, 99
35359, V, 1, 1, 1, 1, 0, 700, 99
35360, V, 1, 1, 1, 1, 0, 700, 99
35361, V, 1, 1, 1, 1, 0, 700, 99
35362, V, 1, 1, 1, 1, 0, 700, 99
35363, V, 1, 1, 1, 1, 0, 700, 99
35364, V, 1, 1, 1, 1, 0, 700, 99
35365, V, 1, 1, 1, 1, 0, 700, 99
35366, V, 1, 1, 1, 1, 0, 700, 99
35367, V, 1, 1, 1, 1, 0, 700, 99
35368, V, 1, 1, 1, 1, 0, 700, 99
35369, V, 1, 1, 1, 1, 0, 700, 99
35371, V, 1, 1, 1, 1, 0, 700, 99
35372, V, 1, 1, 1, 1, 0, 700, 99
35373, V, 1, 1, 1, 1, 0, 700, 99
35374, V, 1, 1, 1, 1, 0, 700, 99
35375, V, 1, 1, 1, 1, 0, 700, 99
35376, V, 1, 1, 1, 1, 0, 700, 99
35377, V, 1, 1, 1, 1, 0, 700, 99
35378, V, 1, 1, 1, 1, 0, 700, 99
35379, V, 1, 1, 1, 1, 0, 700, 99
35380, V, 1, 1, 1, 1, 0, 700, 99
35381, V, 1, 1, 1, 1, 0, 700, 99
35382, V, 1, 1, 1, 1, 0, 700, 99
35383, V, 1, 1, 1, 1, 0, 700, 99
35384, V, 1, 1, 1, 1, 0, 700, 99
35385, V, 1, 1, 1, 1, 0, 700, 99
35386, V, 1, 1, 1, 1, 0, 700, 99
35387, V, 1, 1, 1, 1, 0, 700, 99
35388, V, 1, 1, 1, 1, 0, 700, 99
35389, V, 1, 1, 1, 1, 0, 700, 99
35390, V, 1, 1, 1, 1, 0, 700, 99
35391, V, 1, 1, 1, 1, 0, 700, 99
35392, V, 1, 1, 1, 1, 0, 700, 99
35393, V, 1, 1, 1, 1, 0, 700, 99
35394, V, 1, 1, 1, 1, 0, 700, 99
35395, V, 1, 1, 1, 1, 0, 700, 99
35396, V, 1, 1, 1, 1, 0, 700, 99
35397, V, 1, 1, 1, 1, 0, 700, 99
35398, V, 1, 1, 1, 1, 0, 700, 99
35399, V, 1, 1, 1, 1, 0, 700, 99
35400, V, 1, 1, 1, 1, 0, 700, 99
35401, V, 1, 1, 1, 1, 0, 700, 99
35402, V, 1, 1, 1, 1, 0, 700, 99
35403, V, 1, 1, 1, 1, 0, 700, 99
35404, V, 1, 1, 1, 1, 0, 700, 99
35405, V, 1, 1, 1, 1, 0, 700, 99
35406, V, 1, 1, 1, 1, 0, 700, 99
35407, V, 1, 1, 1, 1, 0, 700, 99
35408, V, 1, 1, 1, 1, 0, 700, 99
35409, V, 1, 1, 1, 1, 0, 700, 99
35410, V, 1, 1, 1, 1, 0, 700, 99
35411, V, 1, 1, 1, 1, 0, 700, 99
35412, V, 1, 1, 1, 1, 0, 700, 99
35414, V, 1, 1, 1, 1, 0, 700, 99
35415, V, 1, 1, 1, 1, 0, 700, 99
35416, V, 1, 1, 1, 1, 0, 700, 99
35417, V, 1, 1, 1, 1, 0, 700, 99
35418, V, 1, 1, 1, 1, 0, 700, 99
35419, V, 1, 1, 1, 1, 0, 700, 99
35420, V, 1, 1, 1, 1, 0, 700, 99
35421, V, 1, 1, 1, 1, 0, 700, 99
35422, V, 1, 1, 1, 1, 0, 700, 99
35423, V, 1, 1, 1, 1, 0, 700, 99
35424, V, 1, 1, 1, 1, 0, 700, 99
35425, V, 1, 1, 1, 1, 0, 700, 99
35426, V, 1, 1, 1, 1, 0, 700, 99
35427, V, 1, 1, 1, 1, 0, 700, 99
35428, V, 1, 1, 1, 1, 0, 700, 99
35429, V, 1, 1, 1, 1, 0, 700, 99
35430, V, 1, 1, 1, 1, 0, 700, 99
35431, V, 1, 1, 1, 1, 0, 700, 99
35432, V, 1, 1, 1, 1, 0, 700, 99
35433, V, 1, 1, 1, 1, 0, 700, 99
35434, V, 1, 1, 1, 1, 0, 700, 99
35435, V, 1, 1, 1, 1, 0, 700, 99
35436, V, 1, 1, 1, 1, 0, 700, 99
35437, V, 1, 1, 1, 1, 0, 700, 99
35438, V, 1, 1, 1, 1, 0, 700, 99
35439, V, 1, 1, 1, 1, 0, 700, 99
35440, V, 1, 1, 1, 1, 0, 700, 99
35441, V, 1, 1, 1, 1, 0, 700, 99
35442, V, 1, 1, 1, 1, 0, 700, 99
35443, V, 1, 1, 1, 1, 0, 700, 99
35444, V, 1, 1, 1, 1, 0, 700, 99
35445, V, 1, 1, 1, 1, 0, 700, 99
35446, V, 1, 1, 1, 1, 0, 700, 99
35447, V, 1, 1, 1, 1, 0, 700, 99
35448, V, 1, 1, 1, 1, 0, 700, 99
35449, V, 1, 1, 1, 1, 0, 700, 99
35450, V, 1, 1, 1, 1, 0, 700, 99
35451, V, 1, 1, 1, 1, 0, 700, 99
35452, V, 1, 1, 1, 1, 0, 700, 99
35453, V, 1, 1, 1, 1, 0, 700, 99
35454, V, 1, 1, 1, 1, 0, 700, 99
35456, V, 1, 1, 1, 1, 0, 700, 99
35457, V, 1, 1, 1, 1, 0, 700, 99
35458, V, 1, 1, 1, 1, 0, 700, 99
35459, V, 1, 1, 1, 1, 0, 700, 99
35460, V, 1, 1, 1, 1, 0, 700, 99
35461, V, 1, 1, 1, 1, 0, 700, 99
35462, V, 1, 1, 1, 1, 0, 700, 99
35463, V, 1, 1, 1, 1, 0, 700, 99
35464, V, 1, 1, 1, 1, 0, 700, 99
35465, V, 1, 1, 1, 1, 0, 700, 99
35466, V, 1, 1, 1, 1, 0, 700, 99
35467, V, 1, 1, 1, 1, 0, 700, 99
35468, V, 1, 1, 1, 1, 0, 700, 99
35469, V, 1, 1, 1, 1, 0, 700, 99
35470, V, 1, 1, 1, 1, 0, 700, 99
35471, V, 1, 1, 1, 1, 0, 700, 99
35472, V, 1, 1, 1, 1, 0, 700, 99
35473, V, 1, 1, 1, 1, 0, 700, 99
35474, V, 1, 1, 1, 1, 0, 700, 99
35475, V, 1, 1, 1, 1, 0, 700, 99
35476, V, 1, 1, 1, 1, 0, 700, 99
35477, V, 1, 1, 1, 1, 0, 700, 99
35478, V, 1, 1, 1, 1, 0, 700, 99
35479, V, 1, 1, 1, 1, 0, 700, 99
35480, V, 1, 1, 1, 1, 0, 700, 99
35481, V, 1, 1, 1, 1, 0, 700, 99
35482, V, 1, 1, 1, 1, 0, 700, 99
35483, V, 1, 1, 1, 1, 0, 700, 99
35484, V, 1, 1, 1, 1, 0, 700, 99
35485, V, 1, 1, 1, 1, 0, 700, 99
35486, V, 1, 1, 1, 1, 0, 700, 99
35487, V, 1, 1, 1, 1, 0, 700, 99
35488, V, 1, 1, 1, 1, 0, 700, 99
35489, V, 1, 1, 1, 1, 0, 700, 99
35490, V, 1, 1, 1, 1, 0, 700, 99
35491, V, 1, 1, 1, 1, 0, 700, 99
35492, V, 1, 1, 1, 1, 0, 700, 99
35493, V, 1, 1, 1, 1, 0, 700, 99
35494, V, 1, 1, 1, 1, 0, 700, 99
35495, V, 1, 1, 1, 1, 0, 700, 99
35496, V, 1, 1, 1, 1, 0, 700, 99
35497, V, 1, 1, 1, 1, 0, 700, 99
35499, V, 1, 1, 1, 1, 0, 700, 99
35500, V, 1, 1, 1, 1, 0, 700, 99
35501, V, 1, 1, 1, 1, 0, 700, 99
35502, V, 1, 1, 1, 1, 0, 700, 99
35503, V, 1, 1, 1, 1, 0, 700, 99
35504, V, 1, 1, 1, 1, 0, 700, 99
35505, V, 1, 1, 1, 1, 0, 700, 99
35506, V, 1, 1, 1, 1, 0, 700, 99
35507, V, 1, 1, 1, 1, 0, 700, 99
35508, V, 1, 1, 1, 1, 0, 700, 99
35509, V, 1, 1, 1, 1, 0, 700, 99
35510, V, 1, 1, 1, 1, 0, 700, 99
35511, V, 1, 1, 1, 1, 0, 700, 99
35512, V, 1, 1, 1, 1, 0, 700, 99
35513, V, 1, 1, 1, 1, 0, 700, 99
35514, V, 1, 1, 1, 1, 0, 700, 99
35515, V, 1, 1, 1, 1, 0, 700, 99
35516, V, 1, 1, 1, 1, 0, 700, 99
35517, V, 1, 1, 1, 1, 0, 700, 99
35518, V, 1, 1, 1, 1, 0, 700, 99
35519, V, 1, 1, 1, 1, 0, 700, 99
35520, V, 1, 1, 1, 1, 0, 700, 99
35521, V, 1, 1, 1, 1, 0, 700, 99
35522, V, 1, 1, 1, 1, 0, 700, 99
35523, V, 1, 1, 1, 1, 0, 700, 99
35524, V, 1, 1, 1, 1, 0, 700, 99
35525, V, 1, 1, 1, 1, 0, 700, 99
35526, V, 1, 1, 1, 1, 0, 700, 99
35527, V, 1, 1, 1, 1, 0, 700, 99
35528, V, 1, 1, 1, 1, 0, 700, 99
35529, V, 1, 1, 1, 1, 0, 700, 99
35530, V, 1, 1, 1, 1, 0, 700, 99
35531, V, 1, 1, 1, 1, 0, 700, 99
35532, V, 1, 1, 1, 1, 0, 700, 99
35533, V, 1, 1, 1, 1, 0, 700, 99
35534, V, 1, 1, 1, 1, 0, 700, 99
35535, V, 1, 1, 1, 1, 0, 700, 99
35536, V, 1, 1, 1, 1, 0, 700, 99
35537, V, 1, 1, 1, 1, 0, 700, 99
35538, V, 1, 1, 1, 1, 0, 700, 99
35539, V, 1, 1, 1, 1, 0, 700, 99
35540, V, 1, 1, 1, 1, 0, 700, 99
35542, V, 1, 1, 1, 1, 0, 700, 99
35543, V, 1, 1, 1, 1, 0, 700, 99
35544, V, 1, 1, 1, 1, 0, 700, 99
35545, V, 1, 1, 1, 1, 0, 700, 99
35546, V, 1, 1, 1, 1, 0, 700, 99
35547, V, 1, 1, 1, 1, 0, 700, 99
35548, V, 1, 1, 1, 1, 0, 700, 99
35549, V, 1, 1, 1, 1, 0, 700, 99
35550, V, 1, 1, 1, 1, 0, 700, 99
35551, V, 1, 1, 1, 1, 0, 700, 99
35552, V, 1, 1, 1, 1, 0, 700, 99
35553, V, 1, 1, 1, 1, 0, 700, 99
35554, V, 1, 1, 1, 1, 0, 700, 99
35555, V, 1, 1, 1, 1, 0, 700, 99
35556, V, 1, 1, 1, 1, 0, 700, 99
35557, V, 1, 1, 1, 1, 0, 700, 99
35558, V, 1, 1, 1, 1, 0, 700, 99
35559, V, 1, 1, 1, 1, 0, 700, 99
35560, V, 1, 1, 1, 1, 0, 700, 99
35561, V, 1, 1, 1, 1, 0, 700, 99
35562, V, 1, 1, 1, 1, 0, 700, 99
35563, V, 1, 1, 1, 1, 0, 700, 99
35564, V, 1, 1, 1, 1, 0, 700, 99
35565, V, 1, 1, 1, 1, 0, 700, 99
35566, V, 1, 1, 1, 1, 0, 700, 99
35567, V, 1, 1, 1, 1, 0, 700, 99
35568, V, 1, 1, 1, 1, 0, 700, 99
35569, V, 1, 1, 1, 1, 0, 700, 99
35570, V, 1, 1, 1, 1, 0, 700, 99
35571, V, 1, 1, 1, 1, 0, 700, 99
35572, V, 1, 1, 1, 1, 0, 700, 99
35573, V, 1, 1, 1, 1, 0, 700, 99
35574, V, 1, 1, 1, 1, 0, 700, 99
35575, V, 1, 1, 1, 1, 0, 700, 99
35576, V, 1, 1, 1, 1, 0, 700, 99
35577, V, 1, 1, 1, 1, 0, 700, 99
35578, V, 1, 1, 1, 1, 0, 700, 99
35579, V, 1, 1, 1, 1, 0, 700, 99
35580, V, 1, 1, 1, 1, 0, 700, 99
35581, V, 1, 1, 1, 1, 0, 700, 99
35582, V, 1, 1, 1, 1, 0, 700, 99
35584, V, 1, 1, 1, 1, 0, 700, 99
35585, V, 1, 1, 1, 1, 0, 700, 99
35586, V, 1, 1, 1, 1, 0, 700, 99
35587, V, 1, 1, 1, 1, 0, 700, 99
35588, V, 1, 1, 1, 1, 0, 700, 99
35589, V, 1, 1, 1, 1, 0, 700, 99
35590, V, 1, 1, 1, 1, 0, 700, 99
35591, V, 1, 1, 1, 1, 0, 700, 99
35592, V, 1, 1, 1, 1, 0, 700, 99
35593, V, 1, 1, 1, 1, 0, 700, 99
35594, V, 1, 1, 1, 1, 0, 700, 99
35595, V, 1, 1, 1, 1, 0, 700, 99
35596, V, 1, 1, 1, 1, 0, 700, 99
35597, V, 1, 1, 1, 1, 0, 700, 99
35598, V, 1, 1, 1, 1, 0, 700, 99
35599, V, 1, 1, 1, 1, 0, 700, 99
35600, V, 1, 1, 1, 1, 0, 700, 99
35601, V, 1, 1, 1, 1, 0, 700, 99
35602, V, 1, 1, 1, 1, 0, 700, 99
35603, V, 1, 1, 1, 1, 0, 700, 99
35604, V, 1, 1, 1, 1, 0, 700, 99
35605, V, 1, 1, 1, 1, 0, 700, 99
35606, V, 1, 1, 1, 1, 0, 700, 99
35607, V, 1, 1, 1, 1, 0, 700, 99
35608, V, 1, 1, 1, 1, 0, 700, 99
35609, V, 1, 1, 1, 1, 0, 700, 99
35610, V, 1, 1, 1, 1, 0, 700, 99
35611, V, 1, 1, 1, 1, 0, 700, 99
35612, V, 1, 1, 1, 1, 0, 700, 99
35613, V, 1, 1, 1, 1, 0, 700, 99
35614, V, 1, 1, 1, 1, 0, 700, 99
35615, V, 1, 1, 1, 1, 0, 700, 99
35616, V, 1, 1, 1, 1, 0, 700, 99
35617, V, 1, 1, 1, 1, 0, 700, 99
35618, V, 1, 1, 1, 1, 0, 700, 99
35619, V, 1, 1, 1, 1, 0, 700, 99
35620, V, 1, 1, 1, 1, 0, 700, 99
35621, V, 1, 1, 1, 1, 0, 700, 99
35622, V, 1, 1, 1, 1, 0, 700, 99
35623, V, 1, 1, 1, 1, 0, 700, 99
35624, V, 1, 1, 1, 1, 0, 700, 99
35625, V, 1, 1, 1, 1, 0, 700, 99
35627, V, 1, 1, 1, 1, 0, 700, 99
35628, V, 1, 1, 1, 1, 0, 700, 99
35629, V, 1, 1, 1, 1, 0, 700, 99
35630, V, 1, 1, 1, 1, 0, 700, 99
35631, V, 1, 1, 1, 1, 0, 700, 99
35632, V, 1, 1, 1, 1, 0, 700, 99
35633, V, 1, 1, 1, 1, 0, 700, 99
35634, V, 1, 1, 1, 1, 0, 700, 99
35635, V, 1, 1, 1, 1, 0, 700, 99
35636, V, 1, 1, 1, 1, 0, 700, 99
35637, V, 1, 1, 1, 1, 0, 700, 99
35638, V, 1, 1, 1, 1, 0, 700, 99
35639, V, 1, 1, 1, 1, 0, 700, 99
35640, V, 1, 1, 1, 1, 0, 700, 99
35641, V, 1, 1, 1, 1, 0, 700, 99
35642, V, 1, 1, 1, 1, 0, 700, 99
35643, V, 1, 1, 1, 1, 0, 700, 99
35644, V, 1, 1, 1, 1, 0, 700, 99
35645, V, 1, 1, 1, 1, 0, 700, 99
35646, V, 1, 1, 1, 1, 0, 700, 99
35647, V, 1, 1, 1, 1, 0, 700, 99
35648, V, 1, 1, 1, 1, 0, 700, 99
35649, V, 1, 1, 1, 1, 0, 700, 99
35650, V, 1, 1, 1, 1, 0, 700, 99
35651, V, 1, 1, 1, 1, 0, 700, 99
35652, V, 1, 1, 1, 1, 0, 700, 99
35653, V, 1, 1, 1, 1, 0, 700, 99
35654, V, 1, 1, 1, 1, 0, 700, 99
35655, V, 1, 1, 1, 1, 0, 700, 99
35656, V, 1, 1, 1, 1, 0, 700, 99
35657, V, 1, 1, 1, 1, 0, 700, 99
35658, V, 1, 1, 1, 1, 0, 700, 99
35659, V, 1, 1, 1, 1, 0, 700, 99
35660, V, 1, 1, 1, 1, 0, 700, 99
35661, V, 1, 1, 1, 1, 0, 700, 99
35662, V, 1, 1, 1, 1, 0, 700, 99
35663, V, 1, 1, 1, 1, 0, 700, 99
35664, V, 1, 1, 1, 1, 0, 700, 99
35665, V, 1, 1, 1, 1, 0, 700, 99
35666, V, 1, 1, 1, 1, 0, 700, 99
35667, V, 1, 1, 1, 1, 0, 700, 99
35668, V, 1, 1, 1, 1, 0, 700, 99
35670, V, 1, 1, 1, 1, 0, 700, 99
35671, V, 1, 1, 1, 1, 0, 700, 99
35672, V, 1, 1, 1, 1, 0, 700, 99
35673, V, 1, 1, 1, 1, 0, 700, 99
35674, V, 1, 1, 1, 1, 0, 700, 99
35675, V, 1, 1, 1, 1, 0, 700, 99
35676, V, 1, 1, 1, 1, 0, 700, 99
35677, V, 1, 1, 1, 1, 0, 700, 99
35678, V, 1, 1, 1, 1, 0, 700, 99
35679, V, 1, 1, 1, 1, 0, 700, 99
35680, V, 1, 1, 1, 1, 0, 700, 99
35681, V, 1, 1, 1, 1, 0, 700, 99
35682, V, 1, 1, 1, 1, 0, 700, 99
35683, V, 1, 1, 1, 1, 0, 700, 99
35684, V, 1, 1, 1, 1, 0, 700, 99
35685, V, 1, 1, 1, 1, 0, 700, 99
35686, V, 1, 1, 1, 1, 0, 700, 99
35687, V, 1, 1, 1, 1, 0, 700, 99
35688, V, 1, 1, 1, 1, 0, 700, 99
35689, V, 1, 1, 1, 1, 0, 700, 99
35690, V, 1, 1, 1, 1, 0, 700, 99
35691, V, 1, 1, 1, 1, 0, 700, 99
35692, V, 1, 1, 1, 1, 0, 700, 99
35693, V, 1, 1, 1, 1, 0, 700, 99
35694, V, 1, 1, 1, 1, 0, 700, 99
35695, V, 1, 1, 1, 1, 0, 700, 99
35696, V, 1, 1, 1, 1, 0, 700, 99
35697, V, 1, 1, 1, 1, 0, 700, 99
35698, V, 1, 1, 1, 1, 0, 700, 99
35699, V, 1, 1, 1, 1, 0, 700, 99
35700, V, 1, 1, 1, 1, 0, 700, 99
35701, V, 1, 1, 1, 1, 0, 700, 99
35702, V, 1, 1, 1, 1, 0, 700, 99
35703, V, 1, 1, 1, 1, 0, 700, 99
35704, V, 1, 1, 1, 1, 0, 700, 99
35705, V, 1, 1, 1, 1, 0, 700, 99
35706, V, 1, 1, 1, 1, 0, 700, 99
35707, V, 1, 1, 1, 1, 0, 700, 99
35708, V, 1, 1, 1, 1, 0, 700, 99
35709, V, 1, 1, 1, 1, 0, 700, 99
35710, V, 1, 1, 1, 1, 0, 700, 99
35712, V, 1, 1, 1, 1, 0, 700, 99
35713, V, 1, 1, 1, 1, 0, 700, 99
35714, V, 1, 1, 1, 1, 0, 700, 99
35715, V, 1, 1, 1, 1, 0, 700, 99
35716, V, 1, 1, 1, 1, 0, 700, 99
35717, V, 1, 1, 1, 1, 0, 700, 99
35718, V, 1, 1, 1, 1, 0, 700, 99
35719, V, 1, 1, 1, 1, 0, 700, 99
35720, V, 1, 1, 1, 1, 0, 700, 99
35721, V, 1, 1, 1, 1, 0, 700, 99
35722, V, 1, 1, 1, 1, 0, 700, 99
35723, V, 1, 1, 1, 1, 0, 700, 99
35724, V, 1, 1, 1, 1, 0, 700, 99
35725, V, 1, 1, 1, 1, 0, 700, 99
35726, V, 1, 1, 1, 1, 0, 700, 99
35727, V, 1, 1, 1, 1, 0, 700, 99
35728, V, 1, 1, 1, 1, 0, 700, 99
35729, V, 1, 1, 1, 1, 0, 700, 99
35730, V, 1, 1, 1, 1, 0, 700, 99
35731, V, 1, 1, 1, 1, 0, 700, 99
35732, V, 1, 1, 1, 1, 0, 700, 99
35733, V, 1, 1, 1, 1, 0, 700, 99
35734, V, 1, 1, 1, 1, 0, 700, 99
35735, V, 1, 1, 1, 1, 0, 700, 99
35736, V, 1, 1, 1, 1, 0, 700, 99
35737, V, 1, 1, 1, 1, 0, 700, 99
35738, V, 1, 1, 1, 1, 0, 700, 99
35739, V, 1, 1, 1, 1, 0, 700, 99
35740, V, 1, 1, 1, 1, 0, 700, 99
35741, V, 1, 1, 1, 1, 0, 700, 99
35742, V, 1, 1, 1, 1, 0, 700, 99
35743, V, 1, 1, 1, 1, 0, 700, 99
35744, V, 1, 1, 1, 1, 0, 700, 99
35745, V, 1, 1, 1, 1, 0, 700, 99
35746, V, 1, 1, 1, 1, 0, 700, 99
35747, V, 1, 1, 1, 1, 0, 700, 99
35748, V, 1, 1, 1, 1, 0, 700, 99
35749, V, 1, 1, 1, 1, 0, 700, 99
35750, V, 1, 1, 1, 1, 0, 700, 99
35751, V, 1, 1, 1, 1, 0, 700, 99
35752, V, 1, 1, 1, 1, 0, 700, 99
35753, V, 1, 1, 1, 1, 0, 700, 99
35755, V, 1, 1, 1, 1, 0, 700, 99
35756, V, 1, 1, 1, 1, 0, 700, 99
35757, V, 1, 1, 1, 1, 0, 700, 99
35758, V, 1, 1, 1, 1, 0, 700, 99
35759, V, 1, 1, 1, 1, 0, 700, 99
35760, V, 1, 1, 1, 1, 0, 700, 99
35761, V, 1, 1, 1, 1, 0, 700, 99
35762, V, 1, 1, 1, 1, 0, 700, 99
35763, V, 1, 1, 1, 1, 0, 700, 99
35764, V, 1, 1, 1, 1, 0, 700, 99
35765, V, 1, 1, 1, 1, 0, 700, 99
35766, V, 1, 1, 1, 1, 0, 700, 99
35767, V, 1, 1, 1, 1, 0, 700, 99
35768, V, 1, 1, 1, 1, 0, 700, 99
35769, V, 1, 1, 1, 1, 0, 700, 99
35770, V, 1, 1, 1, 1, 0, 700, 99
35771, V, 1, 1, 1, 1, 0, 700, 99
35772, V, 1, 1, 1, 1, 0, 700, 99
35773, V, 1, 1, 1, 1, 0, 700, 99
35774, V, 1, 1, 1, 1, 0, 700, 99
35775, V, 1, 1, 1, 1, 0, 700, 99
35776, V, 1, 1, 1, 1, 0, 700, 99
35777, V, 1, 1, 1, 1, 0, 700, 99
35778, V, 1, 1, 1, 1, 0, 700, 99
35779, V, 1, 1, 1, 1, 0, 700, 99
35780, V, 1, 1, 1, 1, 0, 700, 99
35781, V, 1, 1, 1, 1, 0, 700, 99
35782, V, 1, 1, 1, 1, 0, 700, 99
35783, V, 1, 1, 1, 1, 0, 700, 99
35784, V, 1, 1, 1, 1, 0, 700, 99
35785, V, 1, 1, 1, 1, 0, 700, 99
35786, V, 1, 1, 1, 1, 0, 700, 99
35787, V, 1, 1, 1, 1, 0, 700, 99
35788, V, 1, 1, 1, 1, 0, 700, 99
35789, V, 1, 1, 1, 1, 0, 700, 99
35790, V, 1, 1, 1, 1, 0, 700, 99
35791, V, 1, 1, 1, 1, 0, 700, 99
35792, V, 1, 1, 1, 1, 0, 700, 99
35793, V, 1, 1, 1, 1, 0, 700, 99
35794, V, 1, 1, 1, 1, 0, 700, 99
35795, V, 1, 1, 1, 1, 0, 700, 99
35796, V, 1, 1, 1, 1, 0, 700, 99
35798, V, 1, 1, 1, 1, 0, 700, 99
35799, V, 1, 1, 1, 1, 0, 700, 99
35800, V, 1, 1, 1, 1, 0, 700, 99
35801, V, 1, 1, 1, 1, 0, 700, 99
35802, V, 1, 1, 1, 1, 0, 700, 99
35803, V, 1, 1, 1, 1, 0, 700, 99
35804, V, 1, 1, 1, 1, 0, 700, 99
35805, V, 1, 1, 1, 1, 0, 700, 99
35806, V, 1, 1, 1, 1, 0, 700, 99
35807, V, 1, 1, 1, 1, 0, 700, 99
35808, V, 1, 1, 1, 1, 0, 700, 99
35809, V, 1, 1, 1, 1, 0, 700, 99
35810, V, 1, 1, 1, 1, 0, 700, 99
35811, V, 1, 1, 1, 1, 0, 700, 99
35812, V, 1, 1, 1, 1, 0, 700, 99
35813, V, 1, 1, 1, 1, 0, 700, 99
35814, V, 1, 1, 1, 1, 0, 700, 99
35815, V, 1, 1, 1, 1, 0, 700, 99
35816, V, 1, 1, 1, 1, 0, 700, 99
35817, V, 1, 1, 1, 1, 0, 700, 99
35818, V, 1, 1, 1, 1, 0, 700, 99
35819, V, 1, 1, 1, 1, 0, 700, 99
35820, V, 1, 1, 1, 1, 0, 700, 99
35821, V, 1, 1, 1, 1, 0, 700, 99
35822, V, 1, 1, 1, 1, 0, 700, 99
35823, V, 1, 1, 1, 1, 0, 700, 99
35824, V, 1, 1, 1, 1, 0, 700, 99
35825, V, 1, 1, 1, 1, 0, 700, 99
35826, V, 1, 1, 1, 1, 0, 700, 99
35827, V, 1, 1, 1, 1, 0, 700, 99
35828, V, 1, 1, 1, 1, 0, 700, 99
35829, V, 1, 1, 1, 1, 0, 700, 99
35830, V, 1, 1, 1, 1, 0, 700, 99
35831, V, 1, 1, 1, 1, 0, 700, 99
35832, V, 1, 1, 1, 1, 0, 700, 99
35833, V, 1, 1, 1, 1, 0, 700, 99
35834, V, 1, 1, 1, 1, 0, 700, 99
35835, V, 1, 1, 1, 1, 0, 700, 99
35836, V, 1, 1, 1, 1, 0, 700, 99
35837, V, 1, 1, 1, 1, 0, 700, 99
35838, V, 1, 1, 1, 1, 0, 700, 99
35840, V, 1, 1, 1, 1, 0, 700, 99
35841, V, 1, 1, 1, 1, 0, 700, 99
35842, V, 1, 1, 1, 1, 0, 700, 99
35843, V, 1, 1, 1, 1, 0, 700, 99
35844, V, 1, 1, 1, 1, 0, 700, 99
35845, V, 1, 1, 1, 1, 0, 700, 99
35846, V, 1, 1, 1, 1, 0, 700, 99
35847, V, 1, 1, 1, 1, 0, 700, 99
35848, V, 1, 1, 1, 1, 0, 700, 99
35849, V, 1, 1, 1, 1, 0, 700, 99
35850, V, 1, 1, 1, 1, 0, 700, 99
35851, V, 1, 1, 1, 1, 0, 700, 99
35852, V, 1, 1, 1, 1, 0, 700, 99
35853, V, 1, 1, 1, 1, 0, 700, 99
35854, V, 1, 1, 1, 1, 0, 700, 99
35855, V, 1, 1, 1, 1, 0, 700, 99
35856, V, 1, 1, 1, 1, 0, 700, 99
35857, V, 1, 1, 1, 1, 0, 700, 99
35858, V, 1, 1, 1, 1, 0, 700, 99
35859, V, 1, 1, 1, 1, 0, 700, 99
35860, V, 1, 1, 1, 1, 0, 700, 99
35861, V, 1, 1, 1, 1, 0, 700, 99
35862, V, 1, 1, 1, 1, 0, 700, 99
35863, V, 1, 1, 1, 1, 0, 700, 99
35864, V, 1, 1, 1, 1, 0, 700, 99
35865, V, 1, 1, 1, 1, 0, 700, 99
35866, V, 1, 1, 1, 1, 0, 700, 99
35867, V, 1, 1, 1, 1, 0, 700, 99
35868, V, 1, 1, 1, 1, 0, 700, 99
35869, V, 1, 1, 1, 1, 0, 700, 99
35870, V, 1, 1, 1, 1, 0, 700, 99
35871, V, 1, 1, 1, 1, 0, 700, 99
35872, V, 1, 1, 1, 1, 0, 700, 99
35873, V, 1, 1, 1, 1, 0, 700, 99
35874, V, 1, 1, 1, 1, 0, 700, 99
35875, V, 1, 1, 1, 1, 0, 700, 99
35876, V, 1, 1, 1, 1, 0, 700, 99
35877, V, 1, 1, 1, 1, 0, 700, 99
35878, V, 1, 1, 1, 1, 0, 700, 99
35879, V, 1, 1, 1, 1, 0, 700, 99
35880, V, 1, 1, 1, 1, 0, 700, 99
35881, V, 1, 1, 1, 1, 0, 700, 99
35883, V, 1, 1, 1, 1, 0, 700, 99
35884, V, 1, 1, 1, 1, 0, 700, 99
35885, V, 1, 1, 1, 1, 0, 700, 99
35886, V, 1, 1, 1, 1, 0, 700, 99
35887, V, 1, 1, 1, 1, 0, 700, 99
35888, V, 1, 1, 1, 1, 0, 700, 99
35889, V, 1, 1, 1, 1, 0, 700, 99
35890, V, 1, 1, 1, 1, 0, 700, 99
35891, V, 1, 1, 1, 1, 0, 700, 99
35892, V, 1, 1, 1, 1, 0, 700, 99
35893, V, 1, 1, 1, 1, 0, 700, 99
35894, V, 1, 1, 1, 1, 0, 700, 99
35895, V, 1, 1, 1, 1, 0, 700, 99
35896, V, 1, 1, 1, 1, 0, 700, 99
35897, V, 1, 1, 1, 1, 0, 700, 99
35898, V, 1, 1, 1, 1, 0, 700, 99
35899, V, 1, 1, 1, 1, 0, 700, 99
35900, V, 1, 1, 1, 1, 0, 700, 99
35901, V, 1, 1, 1, 1, 0, 700, 99
35902, V, 1, 1, 1, 1, 0, 700, 99
35903, V, 1, 1, 1, 1, 0, 700, 99
35904, V, 1, 1, 1, 1, 0, 700, 99
35905, V, 1, 1, 1, 1, 0, 700, 99
35906, V, 1, 1, 1, 1, 0, 700, 99
35907, V, 1, 1, 1, 1, 0, 700, 99
35908, V, 1, 1, 1, 1, 0, 700, 99
35909, V, 1, 1, 1, 1, 0, 700, 99
35910, V, 1, 1, 1, 1, 0, 700, 99
35911, V, 1, 1, 1, 1, 0, 700, 99
35912, V, 1, 1, 1, 1, 0, 700, 99
35913, V, 1, 1, 1, 1, 0, 700, 99
35914, V, 1, 1, 1, 1, 0, 700, 99
35915, V, 1, 1, 1, 1, 0, 700, 99
35916, V, 1, 1, 1, 1, 0, 700, 99
35917, V, 1, 1, 1, 1, 0, 700, 99
35918, V, 1, 1, 1, 1, 0, 700, 99
35919, V, 1, 1, 1, 1, 0, 700, 99
35920, V, 1, 1, 1, 1, 0, 700, 99
35921, V, 1, 1, 1, 1, 0, 700, 99
35922, V, 1, 1, 1, 1, 0, 700, 99
35923, V, 1, 1, 1, 1, 0, 700, 99
35924, V, 1, 1, 1, 1, 0, 700, 99
35926, V, 1, 1, 1, 1, 0, 700, 99
35927, V, 1, 1, 1, 1, 0, 700, 99
35928, V, 1, 1, 1, 1, 0, 700, 99
35929, V, 1, 1, 1, 1, 0, 700, 99
35930, V, 1, 1, 1, 1, 0, 700, 99
35931, V, 1, 1, 1, 1, 0, 700, 99
35932, V, 1, 1, 1, 1, 0, 700, 99
35933, V, 1, 1, 1, 1, 0, 700, 99
35934, V, 1, 1, 1, 1, 0, 700, 99
35935, V, 1, 1, 1, 1, 0, 700, 99
35936, V, 1, 1, 1, 1, 0, 700, 99
35937, V, 1, 1, 1, 1, 0, 700, 99
35938, V, 1, 1, 1, 1, 0, 700, 99
35939, V, 1, 1, 1, 1, 0, 700, 99
35940, V, 1, 1, 1, 1, 0, 700, 99
35941, V, 1, 1, 1, 1, 0, 700, 99
35942, V, 1, 1, 1, 1, 0, 700, 99
35943, V, 1, 1, 1, 1, 0, 700, 99
35944, V, 1, 1, 1, 1, 0, 700, 99
35945, V, 1, 1, 1, 1, 0, 700, 99
35946, V, 1, 1, 1, 1, 0, 700, 99
35947, V, 1, 1, 1, 1, 0, 700, 99
35948, V, 1, 1, 1, 1, 0, 700, 99
35949, V, 1, 1, 1, 1, 0, 700, 99
35950, V, 1, 1, 1, 1, 0, 700, 99
35951, V, 1, 1, 1, 1, 0, 700, 99
35952, V, 1, 1, 1, 1, 0, 700, 99
35953, V, 1, 1, 1, 1, 0, 700, 99
35954, V, 1, 1, 1, 1, 0, 700, 99
35955, V, 1, 1, 1, 1, 0, 700, 99
35956, V, 1, 1, 1, 1, 0, 700, 99
35957, V, 1, 1, 1, 1, 0, 700, 99
35958, V, 1, 1, 1, 1, 0, 700, 99
35959, V, 1, 1, 1, 1, 0, 700, 99
35960, V, 1, 1, 1, 1, 0, 700, 99
35961, V, 1, 1, 1, 1, 0, 700, 99
35962, V, 1, 1, 1, 1, 0, 700, 99
35963, V, 1, 1, 1, 1, 0, 700, 99
35964, V, 1, 1, 1, 1, 0, 700, 99
35965, V, 1, 1, 1, 1, 0, 700, 99
35966, V, 1, 1, 1, 1, 0, 700, 99
35968, V, 1, 1, 1, 1, 0, 700, 99
35969, V, 1, 1, 1, 1, 0, 700, 99
35970, V, 1, 1, 1, 1, 0, 700, 99
35971, V, 1, 1, 1, 1, 0, 700, 99
35972, V, 1, 1, 1, 1, 0, 700, 99
35973, V, 1, 1, 1, 1, 0, 700, 99
35974, V, 1, 1, 1, 1, 0, 700, 99
35975, V, 1, 1, 1, 1, 0, 700, 99
35976, V, 1, 1, 1, 1, 0, 700, 99
35977, V, 1, 1, 1, 1, 0, 700, 99
35978, V, 1, 1, 1, 1, 0, 700, 99
35979, V, 1, 1, 1, 1, 0, 700, 99
35980, V, 1, 1, 1, 1, 0, 700, 99
35981, V, 1, 1, 1, 1, 0, 700, 99
35982, V, 1, 1, 1, 1, 0, 700, 99
35983, V, 1, 1, 1, 1, 0, 700, 99
35984, V, 1, 1, 1, 1, 0, 700, 99
35985, V, 1, 1, 1, 1, 0, 700, 99
35986, V, 1, 1, 1, 1, 0, 700, 99
35987, V, 1, 1, 1, 1, 0, 700, 99
35988, V, 1, 1, 1, 1, 0, 700, 99
35989, V, 1, 1, 1, 1, 0, 700, 99
35990, V, 1, 1, 1, 1, 0, 700, 99
35991, V, 1, 1, 1, 1, 0, 700, 99
35992, V, 1, 1, 1, 1, 0, 700, 99
35993, V, 1, 1, 1, 1, 0, 700, 99
35994, V, 1, 1, 1, 1, 0, 700, 99
35995, V, 1, 1, 1, 1, 0, 700, 99
35996, V, 1, 1, 1, 1, 0, 700, 99
35997, V, 1, 1, 1, 1, 0, 700, 99
35998, V, 1, 1, 1, 1, 0, 700, 99
35999, V, 1, 1, 1, 1, 0, 700, 99
36000, V, 1, 1, 1, 1, 0, 700, 99
36001, V, 1, 1, 1, 1, 0, 700, 99
36002, V, 1, 1, 1, 1, 0, 700, 99
36003, V, 1, 1, 1, 1, 0, 700, 99
36004, V, 1, 1, 1, 1, 0, 700, 99
36005, V, 1, 1, 1, 1, 0, 700, 99
36006, V, 1, 1, 1, 1, 0, 700, 99
36007, V, 1, 1, 1, 1, 0, 700, 99
36008, V, 1, 1, 1, 1, 0, 700, 99
36009, V, 1, 1, 1, 1, 0, 700, 99
36011, V, 1, 1, 1, 1, 0, 700, 99
36012, V, 1, 1, 1, 1, 0, 700, 99
36013, V, 1, 1, 1, 1, 0, 700, 99
36014, V, 1, 1, 1, 1, 0, 700, 99
36015, V, 1, 1, 1, 1, 0, 700, 99
36016, V, 1, 1, 1, 1, 0, 700, 99
36017, V, 1, 1, 1, 1, 0, 700, 99
36018, V, 1, 1, 1, 1, 0, 700, 99
36019, V, 1, 1, 1, 1, 0, 700, 99
36020, V, 1, 1, 1, 1, 0, 700, 99
36021, V, 1, 1, 1, 1, 0, 700, 99
36022, V, 1, 1, 1, 1, 0, 700, 99
36023, V, 1, 1, 1, 1, 0, 700, 99
36024, V, 1, 1, 1, 1, 0, 700, 99
36025, V, 1, 1, 1, 1, 0, 700, 99
36026, V, 1, 1, 1, 1, 0, 700, 99
36027, V, 1, 1, 1, 1, 0, 700, 99
36028, V, 1, 1, 1, 1, 0, 700, 99
36029, V, 1, 1, 1, 1, 0, 700, 99
36030, V, 1, 1, 1, 1, 0, 700, 99
36031, V, 1, 1, 1, 1, 0, 700, 99
36032, V, 1, 1, 1, 1, 0, 700, 99
36033, V, 1, 1, 1, 1, 0, 700, 99
36034, V, 1, 1, 1, 1, 0, 700, 99
36035, V, 1, 1, 1, 1, 0, 700, 99
36036, V, 1, 1, 1, 1, 0, 700, 99
36037, V, 1, 1, 1, 1, 0, 700, 99
36038, V, 1, 1, 1, 1, 0, 700, 99
36039, V, 1, 1, 1, 1, 0, 700, 99
36040, V, 1, 1, 1, 1, 0, 700, 99
36041, V, 1, 1, 1, 1, 0, 700, 99
36042, V, 1, 1, 1, 1, 0, 700, 99
36043, V, 1, 1, 1, 1, 0, 700, 99
36044, V, 1, 1, 1, 1, 0, 700, 99
36045, V, 1, 1, 1, 1, 0, 700, 99
36046, V, 1, 1, 1, 1, 0, 700, 99
36047, V, 1, 1, 1, 1, 0, 700, 99
36048, V, 1, 1, 1, 1, 0, 700, 99
36049, V, 1, 1, 1, 1, 0, 700, 99
36050, V, 1, 1, 1, 1, 0, 700, 99
36051, V, 1, 1, 1, 1, 0, 700, 99
36052, V, 1, 1, 1, 1, 0, 700, 99
36054, V, 1, 1, 1, 1, 0, 700, 99
36055, V, 1, 1, 1, 1, 0, 700, 99
36056, V, 1, 1, 1, 1, 0, 700, 99
36057, V, 1, 1, 1, 1, 0, 700, 99
36058, V, 1, 1, 1, 1, 0, 700, 99
36059, V, 1, 1, 1, 1, 0, 700, 99
36060, V, 1, 1, 1, 1, 0, 700, 99
36061, V, 1, 1, 1, 1, 0, 700, 99
36062, V, 1, 1, 1, 1, 0, 700, 99
36063, V, 1, 1, 1, 1, 0, 700, 99
36064, V, 1, 1, 1, 1, 0, 700, 99
36065, V, 1, 1, 1, 1, 0, 700, 99
36066, V, 1, 1, 1, 1, 0, 700, 99
36067, V, 1, 1, 1, 1, 0, 700, 99
36068, V, 1, 1, 1, 1, 0, 700, 99
36069, V, 1, 1, 1, 1, 0, 700, 99
36070, V, 1, 1, 1, 1, 0, 700, 99
36071, V, 1, 1, 1, 1, 0, 700, 99
36072, V, 1, 1, 1, 1, 0, 700, 99
36073, V, 1, 1, 1, 1, 0, 700, 99
36074, V, 1, 1, 1, 1, 0, 700, 99
36075, V, 1, 1, 1, 1, 0, 700, 99
36076, V, 1, 1, 1, 1, 0, 700, 99
36077, V, 1, 1, 1, 1, 0, 700, 99
36078, V, 1, 1, 1, 1, 0, 700, 99
36079, V, 1, 1, 1, 1, 0, 700, 99
36080, V, 1, 1, 1, 1, 0, 700, 99
36081, V, 1, 1, 1, 1, 0, 700, 99
36082, V, 1, 1, 1, 1, 0, 700, 99
36083, V, 1, 1, 1, 1, 0, 700, 99
36084, V, 1, 1, 1, 1, 0, 700, 99
36085, V, 1, 1, 1, 1, 0, 700, 99
36086, V, 1, 1, 1, 1, 0, 700, 99
36087, V, 1, 1, 1, 1, 0, 700, 99
36088, V, 1, 1, 1, 1, 0, 700, 99
36089, V, 1, 1, 1, 1, 0, 700, 99
36090, V, 1, 1, 1, 1, 0, 700, 99
36091, V, 1, 1, 1, 1, 0, 700, 99
36092, V, 1, 1, 1, 1, 0, 700, 99
36093, V, 1, 1, 1, 1, 0, 700, 99
36094, V, 1, 1, 1, 1, 0, 700, 99
36096, V, 1, 1, 1, 1, 0, 700, 99
36097, V, 1, 1, 1, 1, 0, 700, 99
36098, V, 1, 1, 1, 1, 0, 700, 99
36099, V, 1, 1, 1, 1, 0, 700, 99
36100, V, 1, 1, 1, 1, 0, 700, 99
36101, V, 1, 1, 1, 1, 0, 700, 99
36102, V, 1, 1, 1, 1, 0, 700, 99
36103, V, 1, 1, 1, 1, 0, 700, 99
36104, V, 1, 1, 1, 1, 0, 700, 99
36105, V, 1, 1, 1, 1, 0, 700, 99
36106, V, 1, 1, 1, 1, 0, 700, 99
36107, V, 1, 1, 1, 1, 0, 700, 99
36108, V, 1, 1, 1, 1, 0, 700, 99
36109, V, 1, 1, 1, 1, 0, 700, 99
36110, V, 1, 1, 1, 1, 0, 700, 99
36111, V, 1, 1, 1, 1, 0, 700, 99
36112, V, 1, 1, 1, 1, 0, 700, 99
36113, V, 1, 1, 1, 1, 0, 700, 99
36114, V, 1, 1, 1, 1, 0, 700, 99
36115, V, 1, 1, 1, 1, 0, 700, 99
36116, V, 1, 1, 1, 1, 0, 700, 99
36117, V, 1, 1, 1, 1, 0, 700, 99
36118, V, 1, 1, 1, 1, 0, 700, 99
36119, V, 1, 1, 1, 1, 0, 700, 99
36120, V, 1, 1, 1, 1, 0, 700, 99
36121, V, 1, 1, 1, 1, 0, 700, 99
36122, V, 1, 1, 1, 1, 0, 700, 99
36123, V, 1, 1, 1, 1, 0, 700, 99
36124, V, 1, 1, 1, 1, 0, 700, 99
36125, V, 1, 1, 1, 1, 0, 700, 99
36126, V, 1, 1, 1, 1, 0, 700, 99
36127, V, 1, 1, 1, 1, 0, 700, 99
36128, V, 1, 1, 1, 1, 0, 700, 99
36129, V, 1, 1, 1, 1, 0, 700, 99
36130, V, 1, 1, 1, 1, 0, 700, 99
36131, V, 1, 1, 1, 1, 0, 700, 99
36132, V, 1, 1, 1, 1, 0, 700, 99
36133, V, 1, 1, 1, 1, 0, 700, 99
36134, V, 1, 1, 1, 1, 0, 700, 99
36135, V, 1, 1, 1, 1, 0, 700, 99
36136, V, 1, 1, 1, 1, 0, 700, 99
36137, V, 1, 1, 1, 1, 0, 700, 99
36139, V, 1, 1, 1, 1, 0, 700, 99
36140, V, 1, 1, 1, 1, 0, 700, 99
36141, V, 1, 1, 1, 1, 0, 700, 99
36142, V, 1, 1, 1, 1, 0, 700, 99
36143, V, 1, 1, 1, 1, 0, 700, 99
36144, V, 1, 1, 1, 1, 0, 700, 99
36145, V, 1, 1, 1, 1, 0, 700, 99
36146, V, 1, 1, 1, 1, 0, 700, 99
36147, V, 1, 1, 1, 1, 0, 700, 99
36148, V, 1, 1, 1, 1, 0, 700, 99
36149, V, 1, 1, 1, 1, 0, 700, 99
36150, V, 1, 1, 1, 1, 0, 700, 99
36151, V, 1, 1, 1, 1, 0, 700, 99
36152, V, 1, 1, 1, 1, 0, 700, 99
36153, V, 1, 1, 1, 1, 0, 700, 99
36154, V, 1, 1, 1, 1, 0, 700, 99
36155, V, 1, 1, 1, 1, 0, 700, 99
36156, V, 1, 1, 1, 1, 0, 700, 99
36157, V, 1, 1, 1, 1, 0, 700, 99
36158, V, 1, 1, 1, 1, 0, 700, 99
36159, V, 1, 1, 1, 1, 0, 700, 99
36160, V, 1, 1, 1, 1, 0, 700, 99
36161, V, 1, 1, 1, 1, 0, 700, 99
36162, V, 1, 1, 1, 1, 0, 700, 99
36163, V, 1, 1, 1, 1, 0, 700, 99
36164, V, 1, 1, 1, 1, 0, 700, 99
36165, V, 1, 1, 1, 1, 0, 700, 99
36166, V, 1, 1, 1, 1, 0, 700, 99
36167, V, 1, 1, 1, 1, 0, 700, 99
36168, V, 1, 1, 1, 1, 0, 700, 99
36169, V, 1, 1, 1, 1, 0, 700, 99
36170, V, 1, 1, 1, 1, 0, 700, 99
36171, V, 1, 1, 1, 1, 0, 700, 99
36172, V, 1, 1, 1, 1, 0, 700, 99
36173, V, 1, 1, 1, 1, 0, 700, 99
36174, V, 1, 1, 1, 1, 0, 700, 99
36175, V, 1, 1, 1, 1, 0, 700, 99
36176, V, 1, 1, 1, 1, 0, 700, 99
36177, V, 1, 1, 1, 1, 0, 700, 99
36178, V, 1, 1, 1, 1, 0, 700, 99
36179, V, 1, 1, 1, 1, 0, 700, 99
36180, V, 1, 1, 1, 1, 0, 700, 99
36182, V, 1, 1, 1, 1, 0, 700, 99
36183, V, 1, 1, 1, 1, 0, 700, 99
36184, V, 1, 1, 1, 1, 0, 700, 99
36185, V, 1, 1, 1, 1, 0, 700, 99
36186, V, 1, 1, 1, 1, 0, 700, 99
36187, V, 1, 1, 1, 1, 0, 700, 99
36188, V, 1, 1, 1, 1, 0, 700, 99
36189, V, 1, 1, 1, 1, 0, 700, 99
36190, V, 1, 1, 1, 1, 0, 700, 99
36191, V, 1, 1, 1, 1, 0, 700, 99
36192, V, 1, 1, 1, 1, 0, 700, 99
36193, V, 1, 1, 1, 1, 0, 700, 99
36194, V, 1, 1, 1, 1, 0, 700, 99
36195, V, 1, 1, 1, 1, 0, 700, 99
36196, V, 1, 1, 1, 1, 0, 700, 99
36197, V, 1, 1, 1, 1, 0, 700, 99
36198, V, 1, 1, 1, 1, 0, 700, 99
36199, V, 1, 1, 1, 1, 0, 700, 99
36200, V, 1, 1, 1, 1, 0, 700, 99
36201, V, 1, 1, 1, 1, 0, 700, 99
36202, V, 1, 1, 1, 1, 0, 700, 99
36203, V, 1, 1, 1, 1, 0, 700, 99
36204, V, 1, 1, 1, 1, 0, 700, 99
36205, V, 1, 1, 1, 1, 0, 700, 99
36206, V, 1, 1, 1, 1, 0, 700, 99
36207, V, 1, 1, 1, 1, 0, 700, 99
36208, V, 1, 1, 1, 1, 0, 700, 99
36209, V, 1, 1, 1, 1, 0, 700, 99
36210, V, 1, 1, 1, 1, 0, 700, 99
36211, V, 1, 1, 1, 1, 0, 700, 99
36212, V, 1, 1, 1, 1, 0, 700, 99
36213, V, 1, 1, 1, 1, 0, 700, 99
36214, V, 1, 1, 1, 1, 0, 700, 99
36215, V, 1, 1, 1, 1, 0, 700, 99
36216, V, 1, 1, 1, 1, 0, 700, 99
36217, V, 1, 1, 1, 1, 0, 700, 99
36218, V, 1, 1, 1, 1, 0, 700, 99
36219, V, 1, 1, 1, 1, 0, 700, 99
36220, V, 1, 1, 1, 1, 0, 700, 99
36221, V, 1, 1, 1, 1, 0, 700, 99
36222, V, 1, 1, 1, 1, 0, 700, 99
36224, V, 1, 1, 1, 1, 0, 700, 99
36225, V, 1, 1, 1, 1, 0, 700, 99
36226, V, 1, 1, 1, 1, 0, 700, 99
36227, V, 1, 1, 1, 1, 0, 700, 99
36228, V, 1, 1, 1, 1, 0, 700, 99
36229, V, 1, 1, 1, 1, 0, 700, 99
36230, V, 1, 1, 1, 1, 0, 700, 99
36231, V, 1, 1, 1, 1, 0, 700, 99
36232, V, 1, 1, 1, 1, 0, 700, 99
36233, V, 1, 1, 1, 1, 0, 700, 99
36234, V, 1, 1, 1, 1, 0, 700, 99
36235, V, 1, 1, 1, 1, 0, 700, 99
36236, V, 1, 1, 1, 1, 0, 700, 99
36237, V, 1, 1, 1, 1, 0, 700, 99
36238, V, 1, 1, 1, 1, 0, 700, 99
36239, V, 1, 1, 1, 1, 0, 700, 99
36240, V, 1, 1, 1, 1, 0, 700, 99
36241, V, 1, 1, 1, 1, 0, 700, 99
36242, V, 1, 1, 1, 1, 0, 700, 99
36243, V, 1, 1, 1, 1, 0, 700, 99
36244, V, 1, 1, 1, 1, 0, 700, 99
36245, V, 1, 1, 1, 1, 0, 700, 99
36246, V, 1, 1, 1, 1, 0, 700, 99
36247, V, 1, 1, 1, 1, 0, 700, 99
36248, V, 1, 1, 1, 1, 0, 700, 99
36249, V, 1, 1, 1, 1, 0, 700, 99
36250, V, 1, 1, 1, 1, 0, 700, 99
36251, V, 1, 1, 1, 1, 0, 700, 99
36252, V, 1, 1, 1, 1, 0, 700, 99
36253, V, 1, 1, 1, 1, 0, 700, 99
36254, V, 1, 1, 1, 1, 0, 700, 99
36255, V, 1, 1, 1, 1, 0, 700, 99
36256, V, 1, 1, 1, 1, 0, 700, 99
36257, V, 1, 1, 1, 1, 0, 700, 99
36258, V, 1, 1, 1, 1, 0, 700, 99
36259, V, 1, 1, 1, 1, 0, 700, 99
36260, V, 1, 1, 1, 1, 0, 700, 99
36261, V, 1, 1, 1, 1, 0, 700, 99
36262, V, 1, 1, 1, 1, 0, 700, 99
36263, V, 1, 1, 1, 1, 0, 700, 99
36264, V, 1, 1, 1, 1, 0, 700, 99
36265, V, 1, 1, 1, 1, 0, 700, 99
36267, V, 1, 1, 1, 1, 0, 700, 99
36268, V, 1, 1, 1, 1, 0, 700, 99
36269, V, 1, 1, 1, 1, 0, 700, 99
36270, V, 1, 1, 1, 1, 0, 700, 99
36271, V, 1, 1, 1, 1, 0, 700, 99
36272, V, 1, 1, 1, 1, 0, 700, 99
36273, V, 1, 1, 1, 1, 0, 700, 99
36274, V, 1, 1, 1, 1, 0, 700, 99
36275, V, 1, 1, 1, 1, 0, 700, 99
36276, V, 1, 1, 1, 1, 0, 700, 99
36277, V, 1, 1, 1, 1, 0, 700, 99
36278, V, 1, 1, 1, 1, 0, 700, 99
36279, V, 1, 1, 1, 1, 0, 700, 99
36280, V, 1, 1, 1, 1, 0, 700, 99
36281, V, 1, 1, 1, 1, 0, 700, 99
36282, V, 1, 1, 1, 1, 0, 700, 99
36283, V, 1, 1, 1, 1, 0, 700, 99
36284, V, 1, 1, 1, 1, 0, 700, 99
36285, V, 1, 1, 1, 1, 0, 700, 99
36286, V, 1, 1, 1, 1, 0, 700, 99
36287, V, 1, 1, 1, 1, 0, 700, 99
36288, V, 1, 1, 1, 1, 0, 700, 99
36289, V, 1, 1, 1, 1, 0, 700, 99
36290, V, 1, 1, 1, 1, 0, 700, 99
36291, V, 1, 1, 1, 1, 0, 700, 99
36292, V, 1, 1, 1, 1, 0, 700, 99
36293, V, 1, 1, 1, 1, 0, 700, 99
36294, V, 1, 1, 1, 1, 0, 700, 99
36295, V, 1, 1, 1, 1, 0, 700, 99
36296, V, 1, 1, 1, 1, 0, 700, 99
36297, V, 1, 1, 1, 1, 0, 700, 99
36298, V, 1, 1, 1, 1, 0, 700, 99
36299, V, 1, 1, 1, 1, 0, 700, 99
36300, V, 1, 1, 1, 1, 0, 700, 99
36301, V, 1, 1, 1, 1, 0, 700, 99
36302, V, 1, 1, 1, 1, 0, 700, 99
36303, V, 1, 1, 1, 1, 0, 700, 99
36304, V, 1, 1, 1, 1, 0, 700, 99
36305, V, 1, 1, 1, 1, 0, 700, 99
36306, V, 1, 1, 1, 1, 0, 700, 99
36307, V, 1, 1, 1, 1, 0, 700, 99
36308, V, 1, 1, 1, 1, 0, 700, 99
36310, V, 1, 1, 1, 1, 0, 700, 99
36311, V, 1, 1, 1, 1, 0, 700, 99
36312, V, 1, 1, 1, 1, 0, 700, 99
36313, V, 1, 1, 1, 1, 0, 700, 99
36314, V, 1, 1, 1, 1, 0, 700, 99
36315, V, 1, 1, 1, 1, 0, 700, 99
36316, V, 1, 1, 1, 1, 0, 700, 99
36317, V, 1, 1, 1, 1, 0, 700, 99
36318, V, 1, 1, 1, 1, 0, 700, 99
36319, V, 1, 1, 1, 1, 0, 700, 99
36320, V, 1, 1, 1, 1, 0, 700, 99
36321, V, 1, 1, 1, 1, 0, 700, 99
36322, V, 1, 1, 1, 1, 0, 700, 99
36323, V, 1, 1, 1, 1, 0, 700, 99
36324, V, 1, 1, 1, 1, 0, 700, 99
36325, V, 1, 1, 1, 1, 0, 700, 99
36326, V, 1, 1, 1, 1, 0, 700, 99
36327, V, 1, 1, 1, 1, 0, 700, 99
36328, V, 1, 1, 1, 1, 0, 700, 99
36329, V, 1, 1, 1, 1, 0, 700, 99
36330, V, 1, 1, 1, 1, 0, 700, 99
36331, V, 1, 1, 1, 1, 0, 700, 99
36332, V, 1, 1, 1, 1, 0, 700, 99
36333, V, 1, 1, 1, 1, 0, 700, 99
36334, V, 1, 1, 1, 1, 0, 700, 99
36335, V, 1, 1, 1, 1, 0, 700, 99
36336, V, 1, 1, 1, 1, 0, 700, 99
36337, V, 1, 1, 1, 1, 0, 700, 99
36338, V, 1, 1, 1, 1, 0, 700, 99
36339, V, 1, 1, 1, 1, 0, 700, 99
36340, V, 1, 1, 1, 1, 0, 700, 99
36341, V, 1, 1, 1, 1, 0, 700, 99
36342, V, 1, 1, 1, 1, 0, 700, 99
36343, V, 1, 1, 1, 1, 0, 700, 99
36344, V, 1, 1, 1, 1, 0, 700, 99
36345, V, 1, 1, 1, 1, 0, 700, 99
36346, V, 1, 1, 1, 1, 0, 700, 99
36347, V, 1, 1, 1, 1, 0, 700, 99
36348, V, 1, 1, 1, 1, 0, 700, 99
36349, V, 1, 1, 1, 1, 0, 700, 99
36350, V, 1, 1, 1, 1, 0, 700, 99
36352, V, 1, 1, 1, 1, 0, 700, 99
36353, V, 1, 1, 1, 1, 0, 700, 99
36354, V, 1, 1, 1, 1, 0, 700, 99
36355, V, 1, 1, 1, 1, 0, 700, 99
36356, V, 1, 1, 1, 1, 0, 700, 99
36357, V, 1, 1, 1, 1, 0, 700, 99
36358, V, 1, 1, 1, 1, 0, 700, 99
36359, V, 1, 1, 1, 1, 0, 700, 99
36360, V, 1, 1, 1, 1, 0, 700, 99
36361, V, 1, 1, 1, 1, 0, 700, 99
36362, V, 1, 1, 1, 1, 0, 700, 99
36363, V, 1, 1, 1, 1, 0, 700, 99
36364, V, 1, 1, 1, 1, 0, 700, 99
36365, V, 1, 1, 1, 1, 0, 700, 99
36366, V, 1, 1, 1, 1, 0, 700, 99
36367, V, 1, 1, 1, 1, 0, 700, 99
36368, V, 1, 1, 1, 1, 0, 700, 99
36369, V, 1, 1, 1, 1, 0, 700, 99
36370, V, 1, 1, 1, 1, 0, 700, 99
36371, V, 1, 1, 1, 1, 0, 700, 99
36372, V, 1, 1, 1, 1, 0, 700, 99
36373, V, 1, 1, 1, 1, 0, 700, 99
36374, V, 1, 1, 1, 1, 0, 700, 99
36375, V, 1, 1, 1, 1, 0, 700, 99
36376, V, 1, 1, 1, 1, 0, 700, 99
36377, V, 1, 1, 1, 1, 0, 700, 99
36378, V, 1, 1, 1, 1, 0, 700, 99
36379, V, 1, 1, 1, 1, 0, 700, 99
36380, V, 1, 1, 1, 1, 0, 700, 99
36381, V, 1, 1, 1, 1, 0, 700, 99
36382, V, 1, 1, 1, 1, 0, 700, 99
36383, V, 1, 1, 1, 1, 0, 700, 99
36384, V, 1, 1, 1, 1, 0, 700, 99
36385, V, 1, 1, 1, 1, 0, 700, 99
36386, V, 1, 1, 1, 1, 0, 700, 99
36387, V, 1, 1, 1, 1, 0, 700, 99
36388, V, 1, 1, 1, 1, 0, 700, 99
36389, V, 1, 1, 1, 1, 0, 700, 99
36390, V, 1, 1, 1, 1, 0, 700, 98
36391, V, 1, 1, 1, 1, 0, 700, 99
36392, V, 1, 1, 1, 1, 0, 700, 99
36393, V, 1, 1, 1, 1, 0, 700, 99
36395, V, 1, 1, 1, 1, 0, 700, 99
36396, V, 1, 1, 1, 1, 0, 700, 99
36397, V, 1, 1, 1, 1, 0, 700, 99
36398, V, 1, 1, 1, 1, 0, 700, 99
36399, V, 1, 1, 1, 1, 0, 700, 99
36400, V, 1, 1, 1, 1, 0, 700, 99
36401, V, 1, 1, 1, 1, 0, 700, 99
36402, V, 1, 1, 1, 1, 0, 700, 99
36403, V, 1, 1, 1, 1, 0, 700, 99
36404, V, 1, 1, 1, 1, 0, 700, 99
36405, V, 1, 1, 1, 1, 0, 700, 99
36406, V, 1, 1, 1, 1, 0, 700, 99
36407, V, 1, 1, 1, 1, 0, 700, 99
36408, V, 1, 1, 1, 1, 0, 700, 99
36409, V, 1, 1, 1, 1, 0, 700, 99
36410, V, 1, 1, 1, 1, 0, 700, 99
36411, V, 1, 1, 1, 1, 0, 700, 99
36412, V, 1, 1, 1, 1, 0, 700, 99
36413, V, 1, 1, 1, 1, 0, 700, 99
36414, V, 1, 1, 1, 1, 0, 700, 99
36415, V, 1, 1, 1, 1, 0, 700, 99
36416, V, 1, 1, 1, 1, 0, 700, 99
36417, V, 1, 1, 1, 1, 0, 700, 99
36418, V, 1, 1, 1, 1, 0, 700, 99
36419, V, 1, 1, 1, 1, 0, 700, 99
36420, V, 1, 1, 1, 1, 0, 700, 99
36421, V, 1, 1, 1, 1, 0, 700, 99
36422, V, 1, 1, 1, 1, 0, 700, 99
36423, V, 1, 1, 1, 1, 0, 700, 99
36424, V, 1, 1, 1, 1, 0, 700, 99
36425, V, 1, 1, 1, 1, 0, 700, 99
36426, V, 1, 1, 1, 1, 0, 700, 99
36427, V, 1, 1, 1, 1, 0, 700, 99
36428, V, 1, 1, 1, 1, 0, 700, 99
36429, V, 1, 1, 1, 1, 0, 700, 99
36430, V, 1, 1, 1, 1, 0, 700, 99
36431, V, 1, 1, 1, 1, 0, 700, 99
36432, V, 1, 1, 1, 1, 0, 700, 99
36433, V, 1, 1, 1, 1, 0, 700, 99
36434, V, 1, 1, 1, 1, 0, 700, 99
36435, V, 1, 1, 1, 1, 0, 700, 99
36436, V, 1, 1, 1, 1, 0, 700, 99
36438, V, 1, 1, 1, 1, 0, 700, 99
36439, V, 1, 1, 1, 1, 0, 700, 99
36440, V, 1, 1, 1, 1, 0, 700, 99
36441, V, 1, 1, 1, 1, 0, 700, 99
36442, V, 1, 1, 1, 1, 0, 700, 99
36443, V, 1, 1, 1, 1, 0, 700, 99
36444, V, 1, 1, 1, 1, 0, 700, 99
36445, V, 1, 1, 1, 1, 0, 700, 99
36446, V, 1, 1, 1, 1, 0, 700, 99
36447, V, 1, 1, 1, 1, 0, 700, 99
36448, V, 1, 1, 1, 1, 0, 700, 99
36449, V, 1, 1, 1, 1, 0, 700, 99
36450, V, 1, 1, 1, 1, 0, 700, 99
36451, V, 1, 1, 1, 1, 0, 700, 99
36452, V, 1, 1, 1, 1, 0, 700, 99
36453, V, 1, 1, 1, 1, 0, 700, 99
36454, V, 1, 1, 1, 1, 0, 700, 99
36455, V, 1, 1, 1, 1, 0, 700, 99
36456, V, 1, 1, 1, 1, 0, 700, 99
36457, V, 1, 1, 1, 1, 0, 700, 99
36458, V, 1, 1, 1, 1, 0, 700, 99
36459, V, 1, 1, 1, 1, 0, 700, 99
36460, V, 1, 1, 1, 1, 0, 700, 99
36461, V, 1, 1, 1, 1, 0, 700, 99
36462, V, 1, 1, 1, 1, 0, 700, 99
36463, V, 1, 1, 1, 1, 0, 700, 99
36464, V, 1, 1, 1, 1, 0, 700, 99
36465, V, 1, 1, 1, 1, 0, 700, 99
36466, V, 1, 1, 1, 1, 0, 700, 99
36467, V, 1, 1, 1, 1, 0, 700, 99
36468, V, 1, 1, 1, 1, 0, 700, 99
36469, V, 1, 1, 1, 1, 0, 700, 99
36470, V, 1, 1, 1, 1, 0, 700, 99
36471, V, 1, 1, 1, 1, 0, 700, 99
36472, V, 1, 1, 1, 1, 0, 700, 99
36473, V, 1, 1, 1, 1, 0, 700, 99
36474, V, 1, 1, 1, 1, 0, 700, 99
36475, V, 1, 1, 1, 1, 0, 700, 99
36476, V, 1, 1, 1, 1, 0, 700, 99
36477, V, 1, 1, 1, 1, 0, 700, 99
36478, V, 1, 1, 1, 1, 0, 700, 99
36480, V, 1, 1, 1, 1, 0, 700, 99
36481, V, 1, 1, 1, 1, 0, 700, 99
36482, V, 1, 1, 1, 1, 0, 700, 99
36483, V, 1, 1, 1, 1, 0, 700, 99
36484, V, 1, 1, 1, 1, 0, 700, 99
36485, V, 1, 1, 1, 1, 0, 700, 99
36486, V, 1, 1, 1, 1, 0, 700, 99
36487, V, 1, 1, 1, 1, 0, 700, 99
36488, V, 1, 1, 1, 1, 0, 700, 99
36489, V, 1, 1, 1, 1, 0, 700, 99
36490, V, 1, 1, 1, 1, 0, 700, 99
36491, V, 1, 1, 1, 1, 0, 700, 99
36492, V, 1, 1, 1, 1, 0, 700, 99
36493, V, 1, 1, 1, 1, 0, 700, 99
36494, V, 1, 1, 1, 1, 0, 700, 99
36495, V, 1, 1, 1, 1, 0, 700, 99
36496, V, 1, 1, 1, 1, 0, 700, 99
36497, V, 1, 1, 1, 1, 0, 700, 99
36498, V, 1, 1, 1, 1, 0, 700, 99
36499, V, 1, 1, 1, 1, 0, 700, 99
36500, V, 1, 1, 1, 1, 0, 700, 99
36501, V, 1, 1, 1, 1, 0, 700, 99
36502, V, 1, 1, 1, 1, 0, 700, 99
36503, V, 1, 1, 1, 1, 0, 700, 99
36504, V, 1, 1, 1, 1, 0, 700, 99
36505, V, 1, 1, 1, 1, 0, 700, 99
36506, V, 1, 1, 1, 1, 0, 700, 99
36507, V, 1, 1, 1, 1, 0, 700, 99
36508, V, 1, 1, 1, 1, 0, 700, 99
36509, V, 1, 1, 1, 1, 0, 700, 99
36510, V, 1, 1, 1, 1, 0, 700, 99
36511, V, 1, 1, 1, 1, 0, 700, 99
36512, V, 1, 1, 1, 1, 0, 700, 99
36513, V, 1, 1, 1, 1, 0, 700, 99
36514, V, 1, 1, 1, 1, 0, 700, 99
36515, V, 1, 1, 1, 1, 0, 700, 99
36516, V, 1, 1, 1, 1, 0, 700, 99
36517, V, 1, 1, 1, 1, 0, 700, 99
36518, V, 1, 1, 1, 1, 0, 700, 99
36519, V, 1, 1, 1, 1, 0, 700, 99
36520, V, 1, 1, 1, 1, 0, 700, 99
36521, V, 1, 1, 1, 1, 0, 700, 99
36523, V, 1, 1, 1, 1, 0, 700, 99
36524, V, 1, 1, 1, 1, 0, 700, 99
36525, V, 1, 1, 1, 1, 0, 700, 99
36526, V, 1, 1, 1, 1, 0, 700, 99
36527, V, 1, 1, 1, 1, 0, 700, 99
36528, V, 1, 1, 1, 1, 0, 700, 99
36529, V, 1, 1, 1, 1, 0, 700, 99
36530, V, 1, 1, 1, 1, 0, 700, 99
36531, V, 1, 1, 1, 1, 0, 700, 99
36532, V, 1, 1, 1, 1, 0, 700, 99
36533, V, 1, 1, 1, 1, 0, 700, 99
36534, V, 1, 1, 1, 1, 0, 700, 99
36535, V, 1, 1, 1, 1, 0, 700, 99
36536, V, 1, 1, 1, 1, 0, 700, 99
36537, V, 1, 1, 1, 1, 0, 700, 99
36538, V, 1, 1, 1, 1, 0, 700, 99
36539, V, 1, 1, 1, 1, 0, 700, 99
36540, V, 1, 1, 1, 1, 0, 700, 99
36541, V, 1, 1, 1, 1, 0, 700, 99
36542, V, 1, 1, 1, 1, 0, 700, 99
36543, V, 1, 1, 1, 1, 0, 700, 99
36544, V, 1, 1, 1, 1, 0, 700, 99
36545, V, 1, 1, 1, 1, 0, 700, 99
36546, V, 1, 1, 1, 1, 0, 700, 99
36547, V, 1, 1, 1, 1, 0, 700, 99
36548, V, 1, 1, 1, 1, 0, 700, 99
36549, V, 1, 1, 1, 1, 0, 700, 99
36550, V, 1, 1, 1, 1, 0, 700, 99
36551, V, 1, 1, 1, 1, 0, 700, 99
36552, V, 1, 1, 1, 1, 0, 700, 99
36553, V, 1, 1, 1, 1, 0, 700, 99
36554, V, 1, 1, 1, 1, 0, 700, 99
36555, V, 1, 1, 1, 1, 0, 700, 99
36556, V, 1, 1, 1, 1, 0, 700, 99
36557, V, 1, 1, 1, 1, 0, 700, 99
36558, V, 1, 1, 1, 1, 0, 700, 99
36559, V, 1, 1, 1, 1, 0, 700, 99
36560, V, 1, 1, 1, 1, 0, 700, 99
36561, V, 1, 1, 1, 1, 0, 700, 99
36562, V, 1, 1, 1, 1, 0, 700, 99
36563, V, 1, 1, 1, 1, 0, 700, 99
36564, V, 1, 1, 1, 1, 0, 700, 99
36566, V, 1, 1, 1, 1, 0, 700, 99
36567, V, 1, 1, 1, 1, 0, 700, 99
36568, V, 1, 1, 1, 1, 0, 700, 99
36569, V, 1, 1, 1, 1, 0, 700, 99
36570, V, 1, 1, 1, 1, 0, 700, 99
36571, V, 1, 1, 1, 1, 0, 700, 99
36572, V, 1, 1, 1, 1, 0, 700, 99
36573, V, 1, 1, 1, 1, 0, 700, 99
36574, V, 1, 1, 1, 1, 0, 700, 99
36575, V, 1, 1, 1, 1, 0, 700, 99
36576, V, 1, 1, 1, 1, 0, 700, 99
36577, V, 1, 1, 1, 1, 0, 700, 99
36578, V, 1, 1, 1, 1, 0, 700, 99
36579, V, 1, 1, 1, 1, 0, 700, 99
36580, V, 1, 1, 1, 1, 0, 700, 99
36581, V, 1, 1, 1, 1, 0, 700, 99
36582, V, 1, 1, 1, 1, 0, 700, 99
36583, V, 1, 1, 1, 1, 0, 700, 99
36584, V, 1, 1, 1, 1, 0, 700, 99
36585, V, 1, 1, 1, 1, 0, 700, 99
36586, V, 1, 1, 1, 1, 0, 700, 99
36587, V, 1, 1, 1, 1, 0, 700, 99
36588, V, 1, 1, 1, 1, 0, 700, 99
36589, V, 1, 1, 1, 1, 0, 700, 99
36590, V, 1, 1, 1, 1, 0, 700, 99
36591, V, 1, 1, 1, 1, 0, 700, 99
36592, V, 1, 1, 1, 1, 0, 700, 99
36593, V, 1, 1, 1, 1, 0, 700, 99
36594, V, 1, 1, 1, 1, 0, 700, 99
36595, V, 1, 1, 1, 1, 0, 700, 99
36596, V, 1, 1, 1, 1, 0, 700, 99
36597, V, 1, 1, 1, 1, 0, 700, 99
36598, V, 1, 1, 1, 1, 0, 700, 99
36599, V, 1, 1, 1, 1, 0, 700, 99
36600, V, 1, 1, 1, 1, 0, 700, 99
36601, V, 1, 1, 1, 1, 0, 700, 99
36602, V, 1, 1, 1, 1, 0, 700, 99
36603, V, 1, 1, 1, 1, 0, 700, 99
36604, V, 1, 1, 1, 1, 0, 700, 99
36605, V, 1, 1, 1, 1, 0, 700, 99
36606, V, 1, 1, 1, 1, 0, 700, 99
36608, V, 1, 1, 1, 1, 0, 700, 99
36609, V, 1, 1, 1, 1, 0, 700, 99
36610, V, 1, 1, 1, 1, 0, 700, 99
36611, V, 1, 1, 1, 1, 0, 700, 99
36612, V, 1, 1, 1, 1, 0, 700, 99
36613, V, 1, 1, 1, 1, 0, 700, 99
36614, V, 1, 1, 1, 1, 0, 700, 99
36615, V, 1, 1, 1, 1, 0, 700, 99
36616, V, 1, 1, 1, 1, 0, 700, 99
36617, V, 1, 1, 1, 1, 0, 700, 99
36618, V, 1, 1, 1, 1, 0, 700, 99
36619, V, 1, 1, 1, 1, 0, 700, 99
36620, V, 1, 1, 1, 1, 0, 700, 99
36621, V, 1, 1, 1, 1, 0, 700, 99
36622, V, 1, 1, 1, 1, 0, 700, 99
36623, V, 1, 1, 1, 1, 0, 700, 99
36624, V, 1, 1, 1, 1, 0, 700, 99
36625, V, 1, 1, 1, 1, 0, 700, 99
36626, V, 1, 1, 1, 1, 0, 700, 99
36627, V, 1, 1, 1, 1, 0, 700, 99
36628, V, 1, 1, 1, 1, 0, 700, 99
36629, V, 1, 1, 1, 1, 0, 700, 99
36630, V, 1, 1, 1, 1, 0, 700, 99
36631, V, 1, 1, 1, 1, 0, 700, 99
36632, V, 1, 1, 1, 1, 0, 700, 99
36633, V, 1, 1, 1, 1, 0, 700, 99
36634, V, 1, 1, 1, 1, 0, 700, 99
36635, V, 1, 1, 1, 1, 0, 700, 99
36636, V, 1, 1, 1, 1, 0, 700, 99
36637, V, 1, 1, 1, 1, 0, 700, 99
36638, V, 1, 1, 1, 1, 0, 700, 99
36639, V, 1, 1, 1, 1, 0, 700, 99
36640, V, 1, 1, 1, 1, 0, 700, 99
36641, V, 1, 1, 1, 1, 0, 700, 99
36642, V, 1, 1, 1, 1, 0, 700, 99
36643, V, 1, 1, 1, 1, 0, 700, 99
36644, V, 1, 1, 1, 1, 0, 700, 99
36645, V, 1, 1, 1, 1, 0, 700, 99
36646, V, 1, 1, 1, 1, 0, 700, 98
36647, V, 1, 1, 1, 1, 0, 700, 99
36648, V, 1, 1, 1, 1, 0, 700, 99
36649, V, 1, 1, 1, 1, 0, 700, 99
36651, V, 1, 1, 1, 1, 0, 700, 99
36652, V, 1, 1, 1, 1, 0, 700, 98
36653, V, 1, 1, 1, 1, 0, 700, 99
36654, V, 1, 1, 1, 1, 0, 700, 98
36655, V, 1, 1, 1, 1, 0, 700, 99
36656, V, 1, 1, 1, 1, 0, 700, 98
36657, V, 1, 1, 1, 1, 0, 700, 98
36658, V, 1, 1, 1, 1, 0, 700, 99
36659, V, 1, 1, 1, 1, 0, 700, 98
36660, V, 1, 1, 1, 1, 0, 700, 99
36661, V, 1, 1, 1, 1, 0, 700, 99
36662, V, 1, 1, 1, 1, 0, 700, 98
36663, V, 1, 1, 1, 1, 0, 700, 98
36664, V, 1, 1, 1, 1, 0, 700, 98
36665, V, 1, 1, 1, 1, 0, 700, 99
36666, V, 1, 1, 1, 1, 0, 700, 99
36667, V, 1, 1, 1, 1, 0, 700, 99
36668, V, 1, 1, 1, 1, 0, 700, 99
36669, V, 1, 1, 1, 1, 0, 700, 98
36670, V, 1, 1, 1, 1, 0, 700, 98
36671, V, 1, 1, 1, 1, 0, 700, 99
36672, V, 1, 1, 1, 1, 0, 700, 99
36673, V, 1, 1, 1, 1, 0, 700, 99
36674, V, 1, 1, 1, 1, 0, 700, 98
36675, V, 1, 1, 1, 1, 0, 700, 99
36676, V, 1, 1, 1, 1, 0, 700, 98
36677, V, 1, 1, 1, 1, 0, 700, 99
36678, V, 1, 1, 1, 1, 0, 700, 99
36679, V, 1, 1, 1, 1, 0, 700, 99
36680, V, 1, 1, 1, 1, 0, 700, 99
36681, V, 1, 1, 1, 1, 0, 700, 99
36682, V, 1, 1, 1, 1, 0, 700, 99
36683, V, 1, 1, 1, 1, 0, 700, 99
36684, V, 1, 1, 1, 1, 0, 700, 99
36685, V, 1, 1, 1, 1, 0, 700, 99
36686, V, 1, 1, 1, 1, 0, 700, 99
36687, V, 1, 1, 1, 1, 0, 700, 99
36688, V, 1, 1, 1, 1, 0, 700, 99
36689, V, 1, 1, 1, 1, 0, 700, 99
36690, V, 1, 1, 1, 1, 0, 700, 99
36691, V, 1, 1, 1, 1, 0, 700, 99
36692, V, 1, 1, 1, 1, 0, 700, 99
36694, V, 1, 1, 1, 1, 0, 700, 99
36695, V, 1, 1, 1, 1, 0, 700, 99
36696, V, 1, 1, 1, 1, 0, 700, 99
36697, V, 1, 1, 1, 1, 0, 700, 99
36698, V, 1, 1, 1, 1, 0, 700, 99
36699, V, 1, 1, 1, 1, 0, 700, 99
36700, V, 1, 1, 1, 1, 0, 700, 99
36701, V, 1, 1, 1, 1, 0, 700, 99
36702, V, 1, 1, 1, 1, 0, 700, 99
36703, V, 1, 1, 1, 1, 0, 700, 99
36704, V, 1, 1, 1, 1, 0, 700, 99
36705, V, 1, 1, 1, 1, 0, 700, 99
36706, V, 1, 1, 1, 1, 0, 700, 99
36707, V, 1, 1, 1, 1, 0, 700, 99
36708, V, 1, 1, 1, 1, 0, 700, 99
36709, V, 1, 1, 1, 1, 0, 700, 99
36710, V, 1, 1, 1, 1, 0, 700, 99
36711, V, 1, 1, 1, 1, 0, 700, 99
36712, V, 1, 1, 1, 1, 0, 700, 99
36713, V, 1, 1, 1, 1, 0, 700, 99
36714, V, 1, 1, 1, 1, 0, 700, 99
36715, V, 1, 1, 1, 1, 0, 700, 99
36716, V, 1, 1, 1, 1, 0, 700, 99
36717, V, 1, 1, 1, 1, 0, 700, 99
36718, V, 1, 1, 1, 1, 0, 700, 99
36719, V, 1, 1, 1, 1, 0, 700, 99
36720, V, 1, 1, 1, 1, 0, 700, 99
36721, V, 1, 1, 1, 1, 0, 700, 99
36722, V, 1, 1, 1, 1, 0, 700, 99
36723, V, 1, 1, 1, 1, 0, 700, 99
36724, V, 1, 1, 1, 1, 0, 700, 99
36725, V, 1, 1, 1, 1, 0, 700, 99
36726, V, 1, 1, 1, 1, 0, 700, 99
36727, V, 1, 1, 1, 1, 0, 700, 99
36728, V, 1, 1, 1, 1, 0, 700, 99
36729, V, 1, 1, 1, 1, 0, 700, 99
36730, V, 1, 1, 1, 1, 0, 700, 99
36731, V, 1, 1, 1, 1, 0, 700, 99
36732, V, 1, 1, 1, 1, 0, 700, 99
36733, V, 1, 1, 1, 1, 0, 700, 99
36734, V, 1, 1, 1, 1, 0, 700, 99
36736, V, 1, 1, 1, 1, 0, 700, 99
36737, V, 1, 1, 1, 1, 0, 700, 99
36738, V, 1, 1, 1, 1, 0, 700, 99
36739, V, 1, 1, 1, 1, 0, 700, 99
36740, V, 1, 1, 1, 1, 0, 700, 99
36741, V, 1, 1, 1, 1, 0, 700, 99
36742, V, 1, 1, 1, 1, 0, 700, 99
36743, V, 1, 1, 1, 1, 0, 700, 99
36744, V, 1, 1, 1, 1, 0, 700, 99
36745, V, 1, 1, 1, 1, 0, 700, 99
36746, V, 1, 1, 1, 1, 0, 700, 99
36747, V, 1, 1, 1, 1, 0, 700, 99
36748, V, 1, 1, 1, 1, 0, 700, 99
36749, V, 1, 1, 1, 1, 0, 700, 99
36750, V, 1, 1, 1, 1, 0, 700, 99
36751, V, 1, 1, 1, 1, 0, 700, 99
36752, V, 1, 1, 1, 1, 0, 700, 99
36753, V, 1, 1, 1, 1, 0, 700, 99
36754, V, 1, 1, 1, 1, 0, 700, 99
36755, V, 1, 1, 1, 1, 0, 700, 99
36756, V, 1, 1, 1, 1, 0, 700, 99
36757, V, 1, 1, 1, 1, 0, 700, 99
36758, V, 1, 1, 1, 1, 0, 700, 99
36759, V, 1, 1, 1, 1, 0, 700, 99
36760, V, 1, 1, 1, 1, 0, 700, 99
36761, V, 1, 1, 1, 1, 0, 700, 99
36762, V, 1, 1, 1, 1, 0, 700, 99
36763, V, 1, 1, 1, 1, 0, 700, 99
36764, V, 1, 1, 1, 1, 0, 700, 99
36765, V, 1, 1, 1, 1, 0, 700, 99
36766, V, 1, 1, 1, 1, 0, 700, 99
36767, V, 1, 1, 1, 1, 0, 700, 99
36768, V, 1, 1, 1, 1, 0, 700, 99
36769, V, 1, 1, 1, 1, 0, 700, 99
36770, V, 1, 1, 1, 1, 0, 700, 99
36771, V, 1, 1, 1, 1, 0, 700, 99
36772, V, 1, 1, 1, 1, 0, 700, 99
36773, V, 1, 1, 1, 1, 0, 700, 99
36774, V, 1, 1, 1, 1, 0, 700, 99
36775, V, 1, 1, 1, 1, 0, 700, 99
36776, V, 1, 1, 1, 1, 0, 700, 99
36777, V, 1, 1, 1, 1, 0, 700, 99
36779, V, 1, 1, 1, 1, 0, 700, 99
36780, V, 1, 1, 1, 1, 0, 700, 99
36781, V, 1, 1, 1, 1, 0, 700, 99
36782, V, 1, 1, 1, 1, 0, 700, 99
36783, V, 1, 1, 1, 1, 0, 700, 99
36784, V, 1, 1, 1, 1, 0, 700, 99
36785, V, 1, 1, 1, 1, 0, 700, 99
36786, V, 1, 1, 1, 1, 0, 700, 99
36787, V, 1, 1, 1, 1, 0, 700, 99
36788, V, 1, 1, 1, 1, 0, 700, 99
36789, V, 1, 1, 1, 1, 0, 700, 99
36790, V, 1, 1, 1, 1, 0, 700, 99
36791, V, 1, 1, 1, 1, 0, 700, 99
36792, V, 1, 1, 1, 1, 0, 700, 99
36793, V, 1, 1, 1, 1, 0, 700, 99
36794, V, 1, 1, 1, 1, 0, 700, 99
36795, V, 1, 1, 1, 1, 0, 700, 99
36796, V, 1, 1, 1, 1, 0, 700, 99
36797, V, 1, 1, 1, 1, 0, 700, 99
36798, V, 1, 1, 1, 1, 0, 700, 99
36799, V, 1, 1, 1, 1, 0, 700, 99
36800, V, 1, 1, 1, 1, 0, 700, 99
36801, V, 1, 1, 1, 1, 0, 700, 99
36802, V, 1, 1, 1, 1, 0, 700, 99
36803, V, 1, 1, 1, 1, 0, 700, 99
36804, V, 1, 1, 1, 1, 0, 700, 99
36805, V, 1, 1, 1, 1, 0, 700, 99
36806, V, 1, 1, 1, 1, 0, 700, 99
36807, V, 1, 1, 1, 1, 0, 700, 99
36808, V, 1, 1, 1, 1, 0, 700, 99
36809, V, 1, 1, 1, 1, 0, 700, 99
36810, V, 1, 1, 1, 1, 0, 700, 99
36811, V, 1, 1, 1, 1, 0, 700, 99
36812, V, 1, 1, 1, 1, 0, 700, 99
36813, V, 1, 1, 1, 1, 0, 700, 99
36814, V, 1, 1, 1, 1, 0, 700, 99
36815, V, 1, 1, 1, 1, 0, 700, 99
36816, V, 1, 1, 1, 1, 0, 700, 99
36817, V, 1, 1, 1, 1, 0, 700, 99
36818, V, 1, 1, 1, 1, 0, 700, 99
36819, V, 1, 1, 1, 1, 0, 700, 99
36820, V, 1, 1, 1, 1, 0, 700, 99
36822, V, 1, 1, 1, 1, 0, 700, 99
36823, V, 1, 1, 1, 1, 0, 700, 99
36824, V, 1, 1, 1, 1, 0, 700, 99
36825, V, 1, 1, 1, 1, 0, 700, 99
36826, V, 1, 1, 1, 1, 0, 700, 99
36827, V, 1, 1, 1, 1, 0, 700, 99
36828, V, 1, 1, 1, 1, 0, 700, 99
36829, V, 1, 1, 1, 1, 0, 700, 99
36830, V, 1, 1, 1, 1, 0, 700, 99
36831, V, 1, 1, 1, 1, 0, 700, 99
36832, V, 1, 1, 1, 1, 0, 700, 99
36833, V, 1, 1, 1, 1, 0, 700, 99
36834, V, 1, 1, 1, 1, 0, 700, 99
36835, V, 1, 1, 1, 1, 0, 700, 99
36836, V, 1, 1, 1, 1, 0, 700, 99
36837, V, 1, 1, 1, 1, 0, 700, 98
36838, V, 1, 1, 1, 1, 0, 700, 99
36839, V, 1, 1, 1, 1, 0, 700, 99
36840, V, 1, 1, 1, 1, 0, 700, 99
36841, V, 1, 1, 1, 1, 0, 700, 99
36842, V, 1, 1, 1, 1, 0, 700, 99
36843, V, 1, 1, 1, 1, 0, 700, 99
36844, V, 1, 1, 1, 1, 0, 700, 99
36845, V, 1, 1, 1, 1, 0, 700, 99
36846, V, 1, 1, 1, 1, 0, 700, 99
36847, V, 1, 1, 1, 1, 0, 700, 99
36848, V, 1, 1, 1, 1, 0, 700, 99
36849, V, 1, 1, 1, 1, 0, 700, 99
36850, V, 1, 1, 1, 1, 0, 700, 99
36851, V, 1, 1, 1, 1, 0, 700, 99
36852, V, 1, 1, 1, 1, 0, 700, 99
36853, V, 1, 1, 1, 1, 0, 700, 99
36854, V, 1, 1, 1, 1, 0, 700, 99
36855, V, 1, 1, 1, 1, 0, 700, 99
36856, V, 1, 1, 1, 1, 0, 700, 99
36857, V, 1, 1, 1, 1, 0, 700, 99
36858, V, 1, 1, 1, 1, 0, 700, 99
36859, V, 1, 1, 1, 1, 0, 700, 99
36860, V, 1, 1, 1, 1, 0, 700, 99
36861, V, 1, 1, 1, 1, 0, 700, 99
36862, V, 1, 1, 1, 1, 0, 700, 99
36864, V, 1, 1, 1, 1, 0, 700, 98
36865, V, 1, 1, 1, 1, 0, 700, 99
36866, V, 1, 1, 1, 1, 0, 700, 99
36867, V, 1, 1, 1, 1, 0, 700, 99
36868, V, 1, 1, 1, 1, 0, 700, 99
36869, V, 1, 1, 1, 1, 0, 700, 99
36870, V, 1, 1, 1, 1, 0, 700, 99
36871, V, 1, 1, 1, 1, 0, 700, 99
36872, V, 1, 1, 1, 1, 0, 700, 99
36873, V, 1, 1, 1, 1, 0, 700, 99
36874, V, 1, 1, 1, 1, 0, 700, 99
36875, V, 1, 1, 1, 1, 0, 700, 98
36876, V, 1, 1, 1, 1, 0, 700, 99
36877, V, 1, 1, 1, 1, 0, 700, 98
36878, V, 1, 1, 1, 1, 0, 700, 98
36879, V, 1, 1, 1, 1, 0, 700, 98
36880, V, 1, 1, 1, 1, 0, 700, 98
36881, V, 1, 1, 1, 1, 0, 700, 98
36882, V, 1, 1, 1, 1, 0, 700, 98
36883, V, 1, 1, 1, 1, 0, 700, 98
36884, V, 1, 1, 1, 1, 0, 700, 98
36885, V, 1, 1, 1, 1, 0, 700, 98
36886, V, 1, 1, 1, 1, 0, 700, 98
36887, V, 1, 1, 1, 1, 0, 700, 98
36888, V, 1, 1, 1, 1, 0, 700, 98
36889, V, 1, 1, 1, 1, 0, 700, 98
36890, V, 1, 1, 1, 1, 0, 700, 98
36891, V, 1, 1, 1, 1, 0, 700, 98
36892, V, 1, 1, 1, 1, 0, 700, 98
36893, V, 1, 1, 1, 1, 0, 700, 98
36894, V, 1, 1, 1, 1, 0, 700, 98
36895, V, 1, 1, 1, 1, 0, 700, 98
36896, V, 1, 1, 1, 1, 0, 700, 98
36897, V, 1, 1, 1, 1, 0, 700, 98
36898, V, 1, 1, 1, 1, 0, 700, 98
36899, V, 1, 1, 1, 1, 0, 700, 98
36900, V, 1, 1, 1, 1, 0, 700, 98
36901, V, 1, 1, 1, 1, 0, 700, 98
36902, V, 1, 1, 1, 1, 0, 700, 98
36903, V, 1, 1, 1, 1, 0, 700, 98
36904, V, 1, 1, 1, 1, 0, 700, 98
36905, V, 1, 1, 1, 1, 0, 700, 98
36907, V, 1, 1, 1, 1, 0, 700, 98
36908, V, 1, 1, 1, 1, 0, 700, 98
36909, V, 1, 1, 1, 1, 0, 700, 98
36910, V, 1, 1, 1, 1, 0, 700, 98
36911, V, 1, 1, 1, 1, 0, 700, 98
36912, V, 1, 1, 1, 1, 0, 700, 98
36913, V, 1, 1, 1, 1, 0, 700, 98
36914, V, 1, 1, 1, 1, 0, 700, 98
36915, V, 1, 1, 1, 1, 0, 700, 98
36916, V, 1, 1, 1, 1, 0, 700, 98
36917, V, 1, 1, 1, 1, 0, 700, 98
36918, V, 1, 1, 1, 1, 0, 700, 98
36919, V, 1, 1, 1, 1, 0, 700, 98
36920, V, 1, 1, 1, 1, 0, 700, 98
36921, V, 1, 1, 1, 1, 0, 700, 98
36922, V, 1, 1, 1, 1, 0, 700, 98
36923, V, 1, 1, 1, 1, 0, 700, 98
36924, V, 1, 1, 1, 1, 0, 700, 98
36925, V, 1, 1, 1, 1, 0, 700, 98
36926, V, 1, 1, 1, 1, 0, 700, 98
36927, V, 1, 1, 1, 1, 0, 700, 98
36928, V, 1, 1, 1, 1, 0, 700, 98
36929, V, 1, 1, 1, 1, 0, 700, 98
36930, V, 1, 1, 1, 1, 0, 700, 98
36931, V, 1, 1, 1, 1, 0, 700, 98
36932, V, 1, 1, 1, 1, 0, 700, 98
36933, V, 1, 1, 1, 1, 0, 700, 98
36934, V, 1, 1, 1, 1, 0, 700, 98
36935, V, 1, 1, 1, 1, 0, 700, 98
36936, V, 1, 1, 1, 1, 0, 700, 98
36937, V, 1, 1, 1, 1, 0, 700, 98
36938, V, 1, 1, 1, 1, 0, 700, 98
36939, V, 1, 1, 1, 1, 0, 700, 98
36940, V, 1, 1, 1, 1, 0, 700, 98
36941, V, 1, 1, 1, 1, 0, 700, 98
36942, V, 1, 1, 1, 1, 0, 700, 98
36943, V, 1, 1, 1, 1, 0, 700, 98
36944, V, 1, 1, 1, 1, 0, 700, 98
36945, V, 1, 1, 1, 1, 0, 700, 98
36946, V, 1, 1, 1, 1, 0, 700, 98
36947, V, 1, 1, 1, 1, 0, 700, 98
36948, V, 1, 1, 1, 1, 0, 700, 98
36950, V, 1, 1, 1, 1, 0, 700, 98
36951, V, 1, 1, 1, 1, 0, 700, 98
36952, V, 1, 1, 1, 1, 0, 700, 98
36953, V, 1, 1, 1, 1, 0, 700, 98
36954, V, 1, 1, 1, 1, 0, 700, 98
36955, V, 1, 1, 1, 1, 0, 700, 98
36956, V, 1, 1, 1, 1, 0, 700, 98
36957, V, 1, 1, 1, 1, 0, 700, 98
36958, V, 1, 1, 1, 1, 0, 700, 98
36959, V, 1, 1, 1, 1, 0, 700, 98
36960, V, 1, 1, 1, 1, 0, 700, 98
36961, V, 1, 1, 1, 1, 0, 700, 98
36962, V, 1, 1, 1, 1, 0, 700, 98
36963, V, 1, 1, 1, 1, 0, 700, 98
36964, V, 1, 1, 1, 1, 0, 700, 98
36965, V, 1, 1, 1, 1, 0, 700, 98
36966, V, 1, 1, 1, 1, 0, 700, 98
36967, V, 1, 1, 1, 1, 0, 700, 98
36968, V, 1, 1, 1, 1, 0, 700, 98
36969, V, 1, 1, 1, 1, 0, 700, 98
36970, V, 1, 1, 1, 1, 0, 700, 98
36971, V, 1, 1, 1, 1, 0, 700, 98
36972, V, 1, 1, 1, 1, 0, 700, 98
36973, V, 1, 1, 1, 1, 0, 700, 98
36974, V, 1, 1, 1, 1, 0, 700, 98
36975, V, 1, 1, 1, 1, 0, 700, 98
36976, V, 1, 1, 1, 1, 0, 700, 98
36977, V, 1, 1, 1, 1, 0, 700, 98
36978, V, 1, 1, 1, 1, 0, 700, 98
36979, V, 1, 1, 1, 1, 0, 700, 98
36980, V, 1, 1, 1, 1, 0, 700, 98
36981, V, 1, 1, 1, 1, 0, 700, 98
36982, V, 1, 1, 1, 1, 0, 700, 98
36983, V, 1, 1, 1, 1, 0, 700, 98
36984, V, 1, 1, 1, 1, 0, 700, 98
36985, V, 1, 1, 1, 1, 0, 700, 98
36986, V, 1, 1, 1, 1, 0, 700, 98
36987, V, 1, 1, 1, 1, 0, 700, 98
36988, V, 1, 1, 1, 1, 0, 700, 98
36989, V, 1, 1, 1, 1, 0, 700, 98
36990, V, 1, 1, 1, 1, 0, 700, 98
36992, V, 1, 1, 1, 1, 0, 700, 98
36993, V, 1, 1, 1, 1, 0, 700, 98
36994, V, 1, 1, 1, 1, 0, 700, 98
36995, V, 1, 1, 1, 1, 0, 700, 98
36996, V, 1, 1, 1, 1, 0, 700, 98
36997, V, 1, 1, 1, 1, 0, 700, 98
36998, V, 1, 1, 1, 1, 0, 700, 98
36999, V, 1, 1, 1, 1, 0, 700, 98
37000, V, 1, 1, 1, 1, 0, 700, 98
37001, V, 1, 1, 1, 1, 0, 700, 98
37002, V, 1, 1, 1, 1, 0, 700, 98
37003, V, 1, 1, 1, 1, 0, 700, 98
37004, V, 1, 1, 1, 1, 0, 700, 98
37005, V, 1, 1, 1, 1, 0, 700, 98
37006, V, 1, 1, 1, 1, 0, 700, 98
37007, V, 1, 1, 1, 1, 0, 700, 98
37008, V, 1, 1, 1, 1, 0, 700, 98
37009, V, 1, 1, 1, 1, 0, 700, 98
37010, V, 1, 1, 1, 1, 0, 700, 98
37011, V, 1, 1, 1, 1, 0, 700, 98
37012, V, 1, 1, 1, 1, 0, 700, 98
37013, V, 1, 1, 1, 1, 0, 700, 98
37014, V, 1, 1, 1, 1, 0, 700, 98
37015, V, 1, 1, 1, 1, 0, 700, 98
37016, V, 1, 1, 1, 1, 0, 700, 98
37017, V, 1, 1, 1, 1, 0, 700, 98
37018, V, 1, 1, 1, 1, 0, 700, 98
37019, V, 1, 1, 1, 1, 0, 700, 98
37020, V, 1, 1, 1, 1, 0, 700, 98
37021, V, 1, 1, 1, 1, 0, 700, 98
37022, V, 1, 1, 1, 1, 0, 700, 98
37023, V, 1, 1, 1, 1, 0, 700, 98
37024, V, 1, 1, 1, 1, 0, 700, 98
37025, V, 1, 1, 1, 1, 0, 700, 98
37026, V, 1, 1, 1, 1, 0, 700, 98
37027, V, 1, 1, 1, 1, 0, 700, 98
37028, V, 1, 1, 1, 1, 0, 700, 98
37029, V, 1, 1, 1, 1, 0, 700, 98
37030, V, 1, 1, 1, 1, 0, 700, 98
37031, V, 1, 1, 1, 1, 0, 700, 98
37032, V, 1, 1, 1, 1, 0, 700, 98
37033, V, 1, 1, 1, 1, 0, 700, 98
37035, V, 1, 1, 1, 1, 0, 700, 98
37036, V, 1, 1, 1, 1, 0, 700, 98
37037, V, 1, 1, 1, 1, 0, 700, 98
37038, V, 1, 1, 1, 1, 0, 700, 98
37039, V, 1, 1, 1, 1, 0, 700, 98
37040, V, 1, 1, 1, 1, 0, 700, 98
37041, V, 1, 1, 1, 1, 0, 700, 98
37042, V, 1, 1, 1, 1, 0, 700, 98
37043, V, 1, 1, 1, 1, 0, 700, 98
37044, V, 1, 1, 1, 1, 0, 700, 98
37045, V, 1, 1, 1, 1, 0, 700, 98
37046, V, 1, 1, 1, 1, 0, 700, 98
37047, V, 1, 1, 1, 1, 0, 700, 98
37048, V, 1, 1, 1, 1, 0, 700, 98
37049, V, 1, 1, 1, 1, 0, 700, 98
37050, V, 1, 1, 1, 1, 0, 700, 98
37051, V, 1, 1, 1, 1, 0, 700, 98
37052, V, 1, 1, 1, 1, 0, 700, 98
37053, V, 1, 1, 1, 1, 0, 700, 98
37054, V, 1, 1, 1, 1, 0, 700, 98
37055, V, 1, 1, 1, 1, 0, 700, 98
37056, V, 1, 1, 1, 1, 0, 700, 98
37057, V, 1, 1, 1, 1, 0, 700, 98
37058, V, 1, 1, 1, 1, 0, 700, 98
37059, V, 1, 1, 1, 1, 0, 700, 98
37060, V, 1, 1, 1, 1, 0, 700, 98
37061, V, 1, 1, 1, 1, 0, 700, 98
37062, V, 1, 1, 1, 1, 0, 700, 98
37063, V, 1, 1, 1, 1, 0, 700, 98
37064, V, 1, 1, 1, 1, 0, 700, 98
37065, V, 1, 1, 1, 1, 0, 700, 98
37066, V, 1, 1, 1, 1, 0, 700, 98
37067, V, 1, 1, 1, 1, 0, 700, 98
37068, V, 1, 1, 1, 1, 0, 700, 98
37069, V, 1, 1, 1, 1, 0, 700, 98
37070, V, 1, 1, 1, 1, 0, 700, 98
37071, V, 1, 1, 1, 1, 0, 700, 98
37072, V, 1, 1, 1, 1, 0, 700, 98
37073, V, 1, 1, 1, 1, 0, 700, 98
37074, V, 1, 1, 1, 1, 0, 700, 98
37075, V, 1, 1, 1, 1, 0, 700, 98
37076, V, 1, 1, 1, 1, 0, 700, 98
37078, V, 1, 1, 1, 1, 0, 700, 98
37079, V, 1, 1, 1, 1, 0, 700, 98
37080, V, 1, 1, 1, 1, 0, 700, 98
37081, V, 1, 1, 1, 1, 0, 700, 98
37082, V, 1, 1, 1, 1, 0, 700, 98
37083, V, 1, 1, 1, 1, 0, 700, 98
37084, V, 1, 1, 1, 1, 0, 700, 98
37085, V, 1, 1, 1, 1, 0, 700, 98
37086, V, 1, 1, 1, 1, 0, 700, 98
37087, V, 1, 1, 1, 1, 0, 700, 98
37088, V, 1, 1, 1, 1, 0, 700, 98
37089, V, 1, 1, 1, 1, 0, 700, 98
37090, V, 1, 1, 1, 1, 0, 700, 98
37091, V, 1, 1, 1, 1, 0, 700, 98
37092, V, 1, 1, 1, 1, 0, 700, 98
37093, V, 1, 1, 1, 1, 0, 700, 98
37094, V, 1, 1, 1, 1, 0, 700, 98
37095, V, 1, 1, 1, 1, 0, 700, 98
37096, V, 1, 1, 1, 1, 0, 700, 98
37097, V, 1, 1, 1, 1, 0, 700, 98
37098, V, 1, 1, 1, 1, 0, 700, 98
37099, V, 1, 1, 1, 1, 0, 700, 98
37100, V, 1, 1, 1, 1, 0, 700, 98
37101, V, 1, 1, 1, 1, 0, 700, 98
37102, V, 1, 1, 1, 1, 0, 700, 98
37103, V, 1, 1, 1, 1, 0, 700, 98
37104, V, 1, 1, 1, 1, 0, 700, 98
37105, V, 1, 1, 1, 1, 0, 700, 98
37106, V, 1, 1, 1, 1, 0, 700, 98
37107, V, 1, 1, 1, 1, 0, 700, 98
37108, V, 1, 1, 1, 1, 0, 700, 98
37109, V, 1, 1, 1, 1, 0, 700, 98
37110, V, 1, 1, 1, 1, 0, 700, 98
37111, V, 1, 1, 1, 1, 0, 700, 98
37112, V, 1, 1, 1, 1, 0, 700, 98
37113, V, 1, 1, 1, 1, 0, 700, 98
37114, V, 1, 1, 1, 1, 0, 700, 98
37115, V, 1, 1, 1, 1, 0, 700, 98
37116, V, 1, 1, 1, 1, 0, 700, 98
37117, V, 1, 1, 1, 1, 0, 700, 98
37118, V, 1, 1, 1, 1, 0, 700, 98
37120, V, 1, 1, 1, 1, 0, 700, 98
37121, V, 1, 1, 1, 1, 0, 700, 98
37122, V, 1, 1, 1, 1, 0, 700, 98
37123, V, 1, 1, 1, 1, 0, 700, 98
37124, V, 1, 1, 1, 1, 0, 700, 98
37125, V, 1, 1, 1, 1, 0, 700, 98
37126, V, 1, 1, 1, 1, 0, 700, 98
37127, V, 1, 1, 1, 1, 0, 700, 98
37128, V, 1, 1, 1, 1, 0, 700, 98
37129, V, 1, 1, 1, 1, 0, 700, 98
37130, V, 1, 1, 1, 1, 0, 700, 98
37131, V, 1, 1, 1, 1, 0, 700, 98
37132, V, 1, 1, 1, 1, 0, 700, 98
37133, V, 1, 1, 1, 1, 0, 700, 98
37134, V, 1, 1, 1, 1, 0, 700, 98
37135, V, 1, 1, 1, 1, 0, 700, 98
37136, V, 1, 1, 1, 1, 0, 700, 98
37137, V, 1, 1, 1, 1, 0, 700, 98
37138, V, 1, 1, 1, 1, 0, 700, 98
37139, V, 1, 1, 1, 1, 0, 700, 98
37140, V, 1, 1, 1, 1, 0, 700, 98
37141, V, 1, 1, 1, 1, 0, 700, 98
37142, V, 1, 1, 1, 1, 0, 700, 98
37143, V, 1, 1, 1, 1, 0, 700, 98
37144, V, 1, 1, 1, 1, 0, 700, 98
37145, V, 1, 1, 1, 1, 0, 700, 98
37146, V, 1, 1, 1, 1, 0, 700, 98
37147, V, 1, 1, 1, 1, 0, 700, 98
37148, V, 1, 1, 1, 1, 0, 700, 98
37149, V, 1, 1, 1, 1, 0, 700, 98
37150, V, 1, 1, 1, 1, 0, 700, 98
37151, V, 1, 1, 1, 1, 0, 700, 98
37152, V, 1, 1, 1, 1, 0, 700, 98
37153, V, 1, 1, 1, 1, 0, 700, 98
37154, V, 1, 1, 1, 1, 0, 700, 98
37155, V, 1, 1, 1, 1, 0, 700, 98
37156, V, 1, 1, 1, 1, 0, 700, 98
37157, V, 1, 1, 1, 1, 0, 700, 98
37158, V, 1, 1, 1, 1, 0, 700, 98
37159, V, 1, 1, 1, 1, 0, 700, 98
37160, V, 1, 1, 1, 1, 0, 700, 98
37161, V, 1, 1, 1, 1, 0, 700, 98
37163, V, 1, 1, 1, 1, 0, 700, 98
37164, V, 1, 1, 1, 1, 0, 700, 98
37165, V, 1, 1, 1, 1, 0, 700, 98
37166, V, 1, 1, 1, 1, 0, 700, 98
37167, V, 1, 1, 1, 1, 0, 700, 98
37168, V, 1, 1, 1, 1, 0, 700, 98
37169, V, 1, 1, 1, 1, 0, 700, 98
37170, V, 1, 1, 1, 1, 0, 700, 98
37171, V, 1, 1, 1, 1, 0, 700, 98
37172, V, 1, 1, 1, 1, 0, 700, 98
37173, V, 1, 1, 1, 1, 0, 700, 98
37174, V, 1, 1, 1, 1, 0, 700, 98
37175, V, 1, 1, 1, 1, 0, 700, 98
37176, V, 1, 1, 1, 1, 0, 700, 98
37177, V, 1, 1, 1, 1, 0, 700, 98
37178, V, 1, 1, 1, 1, 0, 700, 98
37179, V, 1, 1, 1, 1, 0, 700, 98
37180, V, 1, 1, 1, 1, 0, 700, 98
37181, V, 1, 1, 1, 1, 0, 700, 98
37182, V, 1, 1, 1, 1, 0, 700, 98
37183, V, 1, 1, 1, 1, 0, 700, 98
37184, V, 1, 1, 1, 1, 0, 700, 98
37185, V, 1, 1, 1, 1, 0, 700, 98
37186, V, 1, 1, 1, 1, 0, 700, 98
37187, V, 1, 1, 1, 1, 0, 700, 98
37188, V, 1, 1, 1, 1, 0, 700, 98
37189, V, 1, 1, 1, 1, 0, 700, 98
37190, V, 1, 1, 1, 1, 0, 700, 98
37191, V, 1, 1, 1, 1, 0, 700, 98
37192, V, 1, 1, 1, 1, 0, 700, 98
37193, V, 1, 1, 1, 1, 0, 700, 98
37194, V, 1, 1, 1, 1, 0, 700, 98
37195, V, 1, 1, 1, 1, 0, 700, 98
37196, V, 1, 1, 1, 1, 0, 700, 98
37197, V, 1, 1, 1, 1, 0, 700, 98
37198, V, 1, 1, 1, 1, 0, 700, 98
37199, V, 1, 1, 1, 1, 0, 700, 98
37200, V, 1, 1, 1, 1, 0, 700, 98
37201, V, 1, 1, 1, 1, 0, 700, 98
37202, V, 1, 1, 1, 1, 0, 700, 98
37203, V, 1, 1, 1, 1, 0, 700, 98
37204, V, 1, 1, 1, 1, 0, 700, 98
37206, V, 1, 1, 1, 1, 0, 700, 98
37207, V, 1, 1, 1, 1, 0, 700, 98
37208, V, 1, 1, 1, 1, 0, 700, 98
37209, V, 1, 1, 1, 1, 0, 700, 98
37210, V, 1, 1, 1, 1, 0, 700, 98
37211, V, 1, 1, 1, 1, 0, 700, 98
37212, V, 1, 1, 1, 1, 0, 700, 98
37213, V, 1, 1, 1, 1, 0, 700, 98
37214, V, 1, 1, 1, 1, 0, 700, 98
37215, V, 1, 1, 1, 1, 0, 700, 98
37216, V, 1, 1, 1, 1, 0, 700, 98
37217, V, 1, 1, 1, 1, 0, 700, 98
37218, V, 1, 1, 1, 1, 0, 700, 98
37219, V, 1, 1, 1, 1, 0, 700, 98
37220, V, 1, 1, 1, 1, 0, 700, 98
37221, V, 1, 1, 1, 1, 0, 700, 98
37222, V, 1, 1, 1, 1, 0, 700, 98
37223, V, 1, 1, 1, 1, 0, 700, 98
37224, V, 1, 1, 1, 1, 0, 700, 98
37225, V, 1, 1, 1, 1, 0, 700, 98
37226, V, 1, 1, 1, 1, 0, 700, 98
37227, V, 1, 1, 1, 1, 0, 700, 98
37228, V, 1, 1, 1, 1, 0, 700, 98
37229, V, 1, 1, 1, 1, 0, 700, 98
37230, V, 1, 1, 1, 1, 0, 700, 98
37231, V, 1, 1, 1, 1, 0, 700, 98
37232, V, 1, 1, 1, 1, 0, 700, 98
37233, V, 1, 1, 1, 1, 0, 700, 98
37234, V, 1, 1, 1, 1, 0, 700, 98
37235, V, 1, 1, 1, 1, 0, 700, 98
37236, V, 1, 1, 1, 1, 0, 700, 98
37237, V, 1, 1, 1, 1, 0, 700, 98
37238, V, 1, 1, 1, 1, 0, 700, 98
37239, V, 1, 1, 1, 1, 0, 700, 98
37240, V, 1, 1, 1, 1, 0, 700, 98
37241, V, 1, 1, 1, 1, 0, 700, 98
37242, V, 1, 1, 1, 1, 0, 700, 98
37243, V, 1, 1, 1, 1, 0, 700, 98
37244, V, 1, 1, 1, 1, 0, 700, 98
37245, V, 1, 1, 1, 1, 0, 700, 98
37246, V, 1, 1, 1, 1, 0, 700, 98
37248, V, 1, 1, 1, 1, 0, 700, 98
37249, V, 1, 1, 1, 1, 0, 700, 98
37250, V, 1, 1, 1, 1, 0, 700, 98
37251, V, 1, 1, 1, 1, 0, 700, 98
37252, V, 1, 1, 1, 1, 0, 700, 98
37253, V, 1, 1, 1, 1, 0, 700, 98
37254, V, 1, 1, 1, 1, 0, 700, 98
37255, V, 1, 1, 1, 1, 0, 700, 98
37256, V, 1, 1, 1, 1, 0, 700, 98
37257, V, 1, 1, 1, 1, 0, 700, 98
37258, V, 1, 1, 1, 1, 0, 700, 98
37259, V, 1, 1, 1, 1, 0, 700, 98
37260, V, 1, 1, 1, 1, 0, 700, 98
37261, V, 1, 1, 1, 1, 0, 700, 98
37262, V, 1, 1, 1, 1, 0, 700, 98
37263, V, 1, 1, 1, 1, 0, 700, 98
37264, V, 1, 1, 1, 1, 0, 700, 98
37265, V, 1, 1, 1, 1, 0, 700, 98
37266, V, 1, 1, 1, 1, 0, 700, 98
37267, V, 1, 1, 1, 1, 0, 700, 98
37268, V, 1, 1, 1, 1, 0, 700, 98
37269, V, 1, 1, 1, 1, 0, 700, 98
37270, V, 1, 1, 1, 1, 0, 700, 98
37271, V, 1, 1, 1, 1, 0, 700, 98
37272, V, 1, 1, 1, 1, 0, 700, 98
37273, V, 1, 1, 1, 1, 0, 700, 98
37274, V, 1, 1, 1, 1, 0, 700, 98
37275, V, 1, 1, 1, 1, 0, 700, 98
37276, V, 1, 1, 1, 1, 0, 700, 98
37277, V, 1, 1, 1, 1, 0, 700, 98
37278, V, 1, 1, 1, 1, 0, 700, 98
37279, V, 1, 1, 1, 1, 0, 700, 98
37280, V, 1, 1, 1, 1, 0, 700, 98
37281, V, 1, 1, 1, 1, 0, 700, 98
37282, V, 1, 1, 1, 1, 0, 700, 98
37283, V, 1, 1, 1, 1, 0, 700, 98
37284, V, 1, 1, 1, 1, 0, 700, 98
37285, V, 1, 1, 1, 1, 0, 700, 98
37286, V, 1, 1, 1, 1, 0, 700, 98
37287, V, 1, 1, 1, 1, 0, 700, 98
37288, V, 1, 1, 1, 1, 0, 700, 98
37289, V, 1, 1, 1, 1, 0, 700, 98
37291, V, 1, 1, 1, 1, 0, 700, 98
37292, V, 1, 1, 1, 1, 0, 700, 98
37293, V, 1, 1, 1, 1, 0, 700, 98
37294, V, 1, 1, 1, 1, 0, 700, 98
37295, V, 1, 1, 1, 1, 0, 700, 98
37296, V, 1, 1, 1, 1, 0, 700, 98
37297, V, 1, 1, 1, 1, 0, 700, 98
37298, V, 1, 1, 1, 1, 0, 700, 98
37299, V, 1, 1, 1, 1, 0, 700, 98
37300, V, 1, 1, 1, 1, 0, 700, 98
37301, V, 1, 1, 1, 1, 0, 700, 98
37302, V, 1, 1, 1, 1, 0, 700, 98
37303, V, 1, 1, 1, 1, 0, 700, 98
37304, V, 1, 1, 1, 1, 0, 700, 98
37305, V, 1, 1, 1, 1, 0, 700, 98
37306, V, 1, 1, 1, 1, 0, 700, 98
37307, V, 1, 1, 1, 1, 0, 700, 98
37308, V, 1, 1, 1, 1, 0, 700, 98
37309, V, 1, 1, 1, 1, 0, 700, 98
37310, V, 1, 1, 1, 1, 0, 700, 98
37311, V, 1, 1, 1, 1, 0, 700, 98
37312, V, 1, 1, 1, 1, 0, 700, 98
37313, V, 1, 1, 1, 1, 0, 700, 98
37314, V, 1, 1, 1, 1, 0, 700, 98
37315, V, 1, 1, 1, 1, 0, 700, 98
37316, V, 1, 1, 1, 1, 0, 700, 98
37317, V, 1, 1, 1, 1, 0, 700, 98
37318, V, 1, 1, 1, 1, 0, 700, 98
37319, V, 1, 1, 1, 1, 0, 700, 98
37320, V, 1, 1, 1, 1, 0, 700, 98
37321, V, 1, 1, 1, 1, 0, 700, 98
37322, V, 1, 1, 1, 1, 0, 700, 98
37323, V, 1, 1, 1, 1, 0, 700, 98
37324, V, 1, 1, 1, 1, 0, 700, 98
37325, V, 1, 1, 1, 1, 0, 700, 98
37326, V, 1, 1, 1, 1, 0, 700, 98
37327, V, 1, 1, 1, 1, 0, 700, 98
37328, V, 1, 1, 1, 1, 0, 700, 98
37329, V, 1, 1, 1, 1, 0, 700, 98
37330, V, 1, 1, 1, 1, 0, 700, 98
37331, V, 1, 1, 1, 1, 0, 700, 98
37332, V, 1, 1, 1, 1, 0, 700, 98
37334, V, 1, 1, 1, 1, 0, 700, 98
37335, V, 1, 1, 1, 1, 0, 700, 98
37336, V, 1, 1, 1, 1, 0, 700, 98
37337, V, 1, 1, 1, 1, 0, 700, 98
37338, V, 1, 1, 1, 1, 0, 700, 98
37339, V, 1, 1, 1, 1, 0, 700, 98
37340, V, 1, 1, 1, 1, 0, 700, 98
37341, V, 1, 1, 1, 1, 0, 700, 98
37342, V, 1, 1, 1, 1, 0, 700, 98
37343, V, 1, 1, 1, 1, 0, 700, 98
37344, V, 1, 1, 1, 1, 0, 700, 98
37345, V, 1, 1, 1, 1, 0, 700, 98
37346, V, 1, 1, 1, 1, 0, 700, 98
37347, V, 1, 1, 1, 1, 0, 700, 98
37348, V, 1, 1, 1, 1, 0, 700, 98
37349, V, 1, 1, 1, 1, 0, 700, 98
37350, V, 1, 1, 1, 1, 0, 700, 98
37351, V, 1, 1, 1, 1, 0, 700, 98
37352, V, 1, 1, 1, 1, 0, 700, 98
37353, V, 1, 1, 1, 1, 0, 700, 98
37354, V, 1, 1, 1, 1, 0, 700, 98
37355, V, 1, 1, 1, 1, 0, 700, 98
37356, V, 1, 1, 1, 1, 0, 700, 98
37357, V, 1, 1, 1, 1, 0, 700, 98
37358, V, 1, 1, 1, 1, 0, 700, 98
37359, V, 1, 1, 1, 1, 0, 700, 98
37360, V, 1, 1, 1, 1, 0, 700, 98
37361, V, 1, 1, 1, 1, 0, 700, 98
37362, V, 1, 1, 1, 1, 0, 700, 98
37363, V, 1, 1, 1, 1, 0, 700, 98
37364, V, 1, 1, 1, 1, 0, 700, 98
37365, V, 1, 1, 1, 1, 0, 700, 98
37366, V, 1, 1, 1, 1, 0, 700, 98
37367, V, 1, 1, 1, 1, 0, 700, 98
37368, V, 1, 1, 1, 1, 0, 700, 98
37369, V, 1, 1, 1, 1, 0, 700, 98
37370, V, 1, 1, 1, 1, 0, 700, 98
37371, V, 1, 1, 1, 1, 0, 700, 98
37372, V, 1, 1, 1, 1, 0, 700, 98
37373, V, 1, 1, 1, 1, 0, 700, 98
37374, V, 1, 1, 1, 1, 0, 700, 98
37376, V, 1, 1, 1, 1, 0, 700, 98
37377, V, 1, 1, 1, 1, 0, 700, 98
37378, V, 1, 1, 1, 1, 0, 700, 98
37379, V, 1, 1, 1, 1, 0, 700, 98
37380, V, 1, 1, 1, 1, 0, 700, 98
37381, V, 1, 1, 1, 1, 0, 700, 98
37382, V, 1, 1, 1, 1, 0, 700, 98
37383, V, 1, 1, 1, 1, 0, 700, 98
37384, V, 1, 1, 1, 1, 0, 700, 98
37385, V, 1, 1, 1, 1, 0, 700, 98
37386, V, 1, 1, 1, 1, 0, 700, 98
37387, V, 1, 1, 1, 1, 0, 700, 98
37388, V, 1, 1, 1, 1, 0, 700, 98
37389, V, 1, 1, 1, 1, 0, 700, 98
37390, V, 1, 1, 1, 1, 0, 700, 98
37391, V, 1, 1, 1, 1, 0, 700, 98
37392, V, 1, 1, 1, 1, 0, 700, 98
37393, V, 1, 1, 1, 1, 0, 700, 98
37394, V, 1, 1, 1, 1, 0, 700, 98
37395, V, 1, 1, 1, 1, 0, 700, 98
37396, V, 1, 1, 1, 1, 0, 700, 98
37397, V, 1, 1, 1, 1, 0, 700, 98
37398, V, 1, 1, 1, 1, 0, 700, 98
37399, V, 1, 1, 1, 1, 0, 700, 98
37400, V, 1, 1, 1, 1, 0, 700, 98
37401, V, 1, 1, 1, 1, 0, 700, 98
37402, V, 1, 1, 1, 1, 0, 700, 98
37403, V, 1, 1, 1, 1, 0, 700, 98
37404, V, 1, 1, 1, 1, 0, 700, 98
37405, V, 1, 1, 1, 1, 0, 700, 98
37406, V, 1, 1, 1, 1, 0, 700, 98
37407, V, 1, 1, 1, 1, 0, 700, 98
37408, V, 1, 1, 1, 1, 0, 700, 98
37409, V, 1, 1, 1, 1, 0, 700, 98
37410, V, 1, 1, 1, 1, 0, 700, 98
37411, V, 1, 1, 1, 1, 0, 700, 98
37412, V, 1, 1, 1, 1, 0, 700, 98
37413, V, 1, 1, 1, 1, 0, 700, 98
37414, V, 1, 1, 1, 1, 0, 700, 98
37415, V, 1, 1, 1, 1, 0, 700, 98
37416, V, 1, 1, 1, 1, 0, 700, 98
37417, V, 1, 1, 1, 1, 0, 700, 98
37419, V, 1, 1, 1, 1, 0, 700, 98
37420, V, 1, 1, 1, 1, 0, 700, 98
37421, V, 1, 1, 1, 1, 0, 700, 98
37422, V, 1, 1, 1, 1, 0, 700, 98
37423, V, 1, 1, 1, 1, 0, 700, 98
37424, V, 1, 1, 1, 1, 0, 700, 98
37425, V, 1, 1, 1, 1, 0, 700, 98
37426, V, 1, 1, 1, 1, 0, 700, 98
37427, V, 1, 1, 1, 1, 0, 700, 98
37428, V, 1, 1, 1, 1, 0, 700, 98
37429, V, 1, 1, 1, 1, 0, 700, 98
37430, V, 1, 1, 1, 1, 0, 700, 98
37431, V, 1, 1, 1, 1, 0, 700, 98
37432, V, 1, 1, 1, 1, 0, 700, 98
37433, V, 1, 1, 1, 1, 0, 700, 98
37434, V, 1, 1, 1, 1, 0, 700, 98
37435, V, 1, 1, 1, 1, 0, 700, 98
37436, V, 1, 1, 1, 1, 0, 700, 98
37437, V, 1, 1, 1, 1, 0, 700, 98
37438, V, 1, 1, 1, 1, 0, 700, 98
37439, V, 1, 1, 1, 1, 0, 700, 98
37440, V, 1, 1, 1, 1, 0, 700, 98
37441, V, 1, 1, 1, 1, 0, 700, 98
37442, V, 1, 1, 1, 1, 0, 700, 98
37443, V, 1, 1, 1, 1, 0, 700, 98
37444, V, 1, 1, 1, 1, 0, 700, 98
37445, V, 1, 1, 1, 1, 0, 700, 98
37446, V, 1, 1, 1, 1, 0, 700, 98
37447, V, 1, 1, 1, 1, 0, 700, 98
37448, V, 1, 1, 1, 1, 0, 700, 98
37449, V, 1, 1, 1, 1, 0, 700, 98
37450, V, 1, 1, 1, 1, 0, 700, 98
37451, V, 1, 1, 1, 1, 0, 700, 98
37452, V, 1, 1, 1, 1, 0, 700, 98
37453, V, 1, 1, 1, 1, 0, 700, 98
37454, V, 1, 1, 1, 1, 0, 700, 98
37455, V, 1, 1, 1, 1, 0, 700, 98
37456, V, 1, 1, 1, 1, 0, 700, 98
37457, V, 1, 1, 1, 1, 0, 700, 98
37458, V, 1, 1, 1, 1, 0, 700, 98
37459, V, 1, 1, 1, 1, 0, 700, 98
37460, V, 1, 1, 1, 1, 0, 700, 98
37462, V, 1, 1, 1, 1, 0, 700, 98
37463, V, 1, 1, 1, 1, 0, 700, 98
37464, V, 1, 1, 1, 1, 0, 700, 98
37465, V, 1, 1, 1, 1, 0, 700, 98
37466, V, 1, 1, 1, 1, 0, 700, 98
37467, V, 1, 1, 1, 1, 0, 700, 98
37468, V, 1, 1, 1, 1, 0, 700, 98
37469, V, 1, 1, 1, 1, 0, 700, 98
37470, V, 1, 1, 1, 1, 0, 700, 98
37471, V, 1, 1, 1, 1, 0, 700, 98
37472, V, 1, 1, 1, 1, 0, 700, 98
37473, V, 1, 1, 1, 1, 0, 700, 98
37474, V, 1, 1, 1, 1, 0, 700, 98
37475, V, 1, 1, 1, 1, 0, 700, 98
37476, V, 1, 1, 1, 1, 0, 700, 98
37477, V, 1, 1, 1, 1, 0, 700, 98
37478, V, 1, 1, 1, 1, 0, 700, 98
37479, V, 1, 1, 1, 1, 0, 700, 98
37480, V, 1, 1, 1, 1, 0, 700, 98
37481, V, 1, 1, 1, 1, 0, 700, 98
37482, V, 1, 1, 1, 1, 0, 700, 98
37483, V, 1, 1, 1, 1, 0, 700, 98
37484, V, 1, 1, 1, 1, 0, 700, 98
37485, V, 1, 1, 1, 1, 0, 700, 98
37486, V, 1, 1, 1, 1, 0, 700, 98
37487, V, 1, 1, 1, 1, 0, 700, 98
37488, V, 1, 1, 1, 1, 0, 700, 98
37489, V, 1, 1, 1, 1, 0, 700, 98
37490, V, 1, 1, 1, 1, 0, 700, 98
37491, V, 1, 1, 1, 1, 0, 700, 98
37492, V, 1, 1, 1, 1, 0, 700, 98
37493, V, 1, 1, 1, 1, 0, 700, 98
37494, V, 1, 1, 1, 1, 0, 700, 98
37495, V, 1, 1, 1, 1, 0, 700, 98
37496, V, 1, 1, 1, 1, 0, 700, 98
37497, V, 1, 1, 1, 1, 0, 700, 98
37498, V, 1, 1, 1, 1, 0, 700, 98
37499, V, 1, 1, 1, 1, 0, 700, 98
37500, V, 1, 1, 1, 1, 0, 700, 98
37501, V, 1, 1, 1, 1, 0, 700, 98
37502, V, 1, 1, 1, 1, 0, 700, 98
37504, V, 1, 1, 1, 1, 0, 700, 98
37505, V, 1, 1, 1, 1, 0, 700, 98
37506, V, 1, 1, 1, 1, 0, 700, 98
37507, V, 1, 1, 1, 1, 0, 700, 98
37508, V, 1, 1, 1, 1, 0, 700, 98
37509, V, 1, 1, 1, 1, 0, 700, 98
37510, V, 1, 1, 1, 1, 0, 700, 98
37511, V, 1, 1, 1, 1, 0, 700, 98
37512, V, 1, 1, 1, 1, 0, 700, 98
37513, V, 1, 1, 1, 1, 0, 700, 98
37514, V, 1, 1, 1, 1, 0, 700, 98
37515, V, 1, 1, 1, 1, 0, 700, 98
37516, V, 1, 1, 1, 1, 0, 700, 98
37517, V, 1, 1, 1, 1, 0, 700, 98
37518, V, 1, 1, 1, 1, 0, 700, 98
37519, V, 1, 1, 1, 1, 0, 700, 98
37520, V, 1, 1, 1, 1, 0, 700, 98
37521, V, 1, 1, 1, 1, 0, 700, 98
37522, V, 1, 1, 1, 1, 0, 700, 98
37523, V, 1, 1, 1, 1, 0, 700, 98
37524, V, 1, 1, 1, 1, 0, 700, 98
37525, V, 1, 1, 1, 1, 0, 700, 98
37526, V, 1, 1, 1, 1, 0, 700, 98
37527, V, 1, 1, 1, 1, 0, 700, 98
37528, V, 1, 1, 1, 1, 0, 700, 98
37529, V, 1, 1, 1, 1, 0, 700, 98
37530, V, 1, 1, 1, 1, 0, 700, 98
37531, V, 1, 1, 1, 1, 0, 700, 98
37532, V, 1, 1, 1, 1, 0, 700, 98
37533, V, 1, 1, 1, 1, 0, 700, 98
37534, V, 1, 1, 1, 1, 0, 700, 98
37535, V, 1, 1, 1, 1, 0, 700, 98
37536, V, 1, 1, 1, 1, 0, 700, 98
37537, V, 1, 1, 1, 1, 0, 700, 98
37538, V, 1, 1, 1, 1, 0, 700, 98
37539, V, 1, 1, 1, 1, 0, 700, 98
37540, V, 1, 1, 1, 1, 0, 700, 98
37541, V, 1, 1, 1, 1, 0, 700, 98
37542, V, 1, 1, 1, 1, 0, 700, 98
37543, V, 1, 1, 1, 1, 0, 700, 98
37544, V, 1, 1, 1, 1, 0, 700, 98
37545, V, 1, 1, 1, 1, 0, 700, 98
37547, V, 1, 1, 1, 1, 0, 700, 98
37548, V, 1, 1, 1, 1, 0, 700, 98
37549, V, 1, 1, 1, 1, 0, 700, 98
37550, V, 1, 1, 1, 1, 0, 700, 98
37551, V, 1, 1, 1, 1, 0, 700, 98
37552, V, 1, 1, 1, 1, 0, 700, 98
37553, V, 1, 1, 1, 1, 0, 700, 98
37554, V, 1, 1, 1, 1, 0, 700, 98
37555, V, 1, 1, 1, 1, 0, 700, 98
37556, V, 1, 1, 1, 1, 0, 700, 98
37557, V, 1, 1, 1, 1, 0, 700, 98
37558, V, 1, 1, 1, 1, 0, 700, 98
37559, V, 1, 1, 1, 1, 0, 700, 98
37560, V, 1, 1, 1, 1, 0, 700, 98
37561, V, 1, 1, 1, 1, 0, 700, 98
37562, V, 1, 1, 1, 1, 0, 700, 98
37563, V, 1, 1, 1, 1, 0, 700, 98
37564, V, 1, 1, 1, 1, 0, 700, 98
37565, V, 1, 1, 1, 1, 0, 700, 98
37566, V, 1, 1, 1, 1, 0, 700, 98
37567, V, 1, 1, 1, 1, 0, 700, 98
37568, V, 1, 1, 1, 1, 0, 700, 98
37569, V, 1, 1, 1, 1, 0, 700, 98
37570, V, 1, 1, 1, 1, 0, 700, 98
37571, V, 1, 1, 1, 1, 0, 700, 98
37572, V, 1, 1, 1, 1, 0, 700, 98
37573, V, 1, 1, 1, 1, 0, 700, 98
37574, V, 1, 1, 1, 1, 0, 700, 98
37575, V, 1, 1, 1, 1, 0, 700, 98
37576, V, 1, 1, 1, 1, 0, 700, 98
37577, V, 1, 1, 1, 1, 0, 700, 98
37578, V, 1, 1, 1, 1, 0, 700, 98
37579, V, 1, 1, 1, 1, 0, 700, 98
37580, V, 1, 1, 1, 1, 0, 700, 98
37581, V, 1, 1, 1, 1, 0, 700, 98
37582, V, 1, 1, 1, 1, 0, 700, 98
37583, V, 1, 1, 1, 1, 0, 700, 98
37584, V, 1, 1, 1, 1, 0, 700, 98
37585, V, 1, 1, 1, 1, 0, 700, 98
37586, V, 1, 1, 1, 1, 0, 700, 98
37587, V, 1, 1, 1, 1, 0, 700, 98
37588, V, 1, 1, 1, 1, 0, 700, 98
37590, V, 1, 1, 1, 1, 0, 700, 98
37591, V, 1, 1, 1, 1, 0, 700, 98
37592, V, 1, 1, 1, 1, 0, 700, 98
37593, V, 1, 1, 1, 1, 0, 700, 98
37594, V, 1, 1, 1, 1, 0, 700, 98
37595, V, 1, 1, 1, 1, 0, 700, 98
37596, V, 1, 1, 1, 1, 0, 700, 98
37597, V, 1, 1, 1, 1, 0, 700, 98
37598, V, 1, 1, 1, 1, 0, 700, 98
37599, V, 1, 1, 1, 1, 0, 700, 98
37600, V, 1, 1, 1, 1, 0, 700, 98
37601, V, 1, 1, 1, 1, 0, 700, 98
37602, V, 1, 1, 1, 1, 0, 700, 98
37603, V, 1, 1, 1, 1, 0, 700, 98
37604, V, 1, 1, 1, 1, 0, 700, 98
37605, V, 1, 1, 1, 1, 0, 700, 98
37606, V, 1, 1, 1, 1, 0, 700, 98
37607, V, 1, 1, 1, 1, 0, 700, 98
37608, V, 1, 1, 1, 1, 0, 700, 98
37609, V, 1, 1, 1, 1, 0, 700, 98
37610, V, 1, 1, 1, 1, 0, 700, 98
37611, V, 1, 1, 1, 1, 0, 700, 98
37612, V, 1, 1, 1, 1, 0, 700, 98
37613, V, 1, 1, 1, 1, 0, 700, 98
37614, V, 1, 1, 1, 1, 0, 700, 98
37615, V, 1, 1, 1, 1, 0, 700, 98
37616, V, 1, 1, 1, 1, 0, 700, 98
37617, V, 1, 1, 1, 1, 0, 700, 98
37618, V, 1, 1, 1, 1, 0, 700, 98
37619, V, 1, 1, 1, 1, 0, 700, 98
37620, V, 1, 1, 1, 1, 0, 700, 98
37621, V, 1, 1, 1, 1, 0, 700, 98
37622, V, 1, 1, 1, 1, 0, 700, 98
37623, V, 1, 1, 1, 1, 0, 700, 98
37624, V, 1, 1, 1, 1, 0, 700, 98
37625, V, 1, 1, 1, 1, 0, 700, 98
37626, V, 1, 1, 1, 1, 0, 700, 98
37627, V, 1, 1, 1, 1, 0, 700, 98
37628, V, 1, 1, 1, 1, 0, 700, 98
37629, V, 1, 1, 1, 1, 0, 700, 98
37630, V, 1, 1, 1, 1, 0, 700, 98
37632, V, 1, 1, 1, 1, 0, 700, 98
37633, V, 1, 1, 1, 1, 0, 700, 98
37634, V, 1, 1, 1, 1, 0, 700, 98
37635, V, 1, 1, 1, 1, 0, 700, 98
37636, V, 1, 1, 1, 1, 0, 700, 98
37637, V, 1, 1, 1, 1, 0, 700, 98
37638, V, 1, 1, 1, 1, 0, 700, 98
37639, V, 1, 1, 1, 1, 0, 700, 98
37640, V, 1, 1, 1, 1, 0, 700, 98
37641, V, 1, 1, 1, 1, 0, 700, 98
37642, V, 1, 1, 1, 1, 0, 700, 98
37643, V, 1, 1, 1, 1, 0, 700, 98
37644, V, 1, 1, 1, 1, 0, 700, 98
37645, V, 1, 1, 1, 1, 0, 700, 98
37646, V, 1, 1, 1, 1, 0, 700, 98
37647, V, 1, 1, 1, 1, 0, 700, 98
37648, V, 1, 1, 1, 1, 0, 700, 98
37649, V, 1, 1, 1, 1, 0, 700, 98
37650, V, 1, 1, 1, 1, 0, 700, 98
37651, V, 1, 1, 1, 1, 0, 700, 98
37652, V, 1, 1, 1, 1, 0, 700, 98
37653, V, 1, 1, 1, 1, 0, 700, 98
37654, V, 1, 1, 1, 1, 0, 700, 98
37655, V, 1, 1, 1, 1, 0, 700, 98
37656, V, 1, 1, 1, 1, 0, 700, 98
37657, V, 1, 1, 1, 1, 0, 700, 98
37658, V, 1, 1, 1, 1, 0, 700, 98
37659, V, 1, 1, 1, 1, 0, 700, 98
37660, V, 1, 1, 1, 1, 0, 700, 98
37661, V, 1, 1, 1, 1, 0, 700, 98
37662, V, 1, 1, 1, 1, 0, 700, 98
37663, V, 1, 1, 1, 1, 0, 700, 98
37664, V, 1, 1, 1, 1, 0, 700, 98
37665, V, 1, 1, 1, 1, 0, 700, 98
37666, V, 1, 1, 1, 1, 0, 700, 98
37667, V, 1, 1, 1, 1, 0, 700, 98
37668, V, 1, 1, 1, 1, 0, 700, 98
37669, V, 1, 1, 1, 1, 0, 700, 98
37670, V, 1, 1, 1, 1, 0, 700, 98
37671, V, 1, 1, 1, 1, 0, 700, 98
37672, V, 1, 1, 1, 1, 0, 700, 98
37673, V, 1, 1, 1, 1, 0, 700, 98
37675, V, 1, 1, 1, 1, 0, 700, 98
37676, V, 1, 1, 1, 1, 0, 700, 98
37677, V, 1, 1, 1, 1, 0, 700, 98
37678, V, 1, 1, 1, 1, 0, 700, 98
37679, V, 1, 1, 1, 1, 0, 700, 98
37680, V, 1, 1, 1, 1, 0, 700, 98
37681, V, 1, 1, 1, 1, 0, 700, 98
37682, V, 1, 1, 1, 1, 0, 700, 98
37683, V, 1, 1, 1, 1, 0, 700, 98
37684, V, 1, 1, 1, 1, 0, 700, 98
37685, V, 1, 1, 1, 1, 0, 700, 98
37686, V, 1, 1, 1, 1, 0, 700, 98
37687, V, 1, 1, 1, 1, 0, 700, 98
37688, V, 1, 1, 1, 1, 0, 700, 98
37689, V, 1, 1, 1, 1, 0, 700, 98
37690, V, 1, 1, 1, 1, 0, 700, 98
37691, V, 1, 1, 1, 1, 0, 700, 98
37692, V, 1, 1, 1, 1, 0, 700, 98
37693, V, 1, 1, 1, 1, 0, 700, 98
37694, V, 1, 1, 1, 1, 0, 700, 98
37695, V, 1, 1, 1, 1, 0, 700, 98
37696, V, 1, 1, 1, 1, 0, 700, 98
37697, V, 1, 1, 1, 1, 0, 700, 98
37698, V, 1, 1, 1, 1, 0, 700, 98
37699, V, 1, 1, 1, 1, 0, 700, 98
37700, V, 1, 1, 1, 1, 0, 700, 98
37701, V, 1, 1, 1, 1, 0, 700, 98
37702, V, 1, 1, 1, 1, 0, 700, 98
37703, V, 1, 1, 1, 1, 0, 700, 98
37704, V, 1, 1, 1, 1, 0, 700, 98
37705, V, 1, 1, 1, 1, 0, 700, 98
37706, V, 1, 1, 1, 1, 0, 700, 98
37707, V, 1, 1, 1, 1, 0, 700, 98
37708, V, 1, 1, 1, 1, 0, 700, 98
37709, V, 1, 1, 1, 1, 0, 700, 98
37710, V, 1, 1, 1, 1, 0, 700, 98
37711, V, 1, 1, 1, 1, 0, 700, 98
37712, V, 1, 1, 1, 1, 0, 700, 98
37713, V, 1, 1, 1, 1, 0, 700, 98
37714, V, 1, 1, 1, 1, 0, 700, 98
37715, V, 1, 1, 1, 1, 0, 700, 98
37716, V, 1, 1, 1, 1, 0, 700, 98
37718, V, 1, 1, 1, 1, 0, 700, 98
37719, V, 1, 1, 1, 1, 0, 700, 98
37720, V, 1, 1, 1, 1, 0, 700, 98
37721, V, 1, 1, 1, 1, 0, 700, 98
37722, V, 1, 1, 1, 1, 0, 700, 98
37723, V, 1, 1, 1, 1, 0, 700, 98
37724, V, 1, 1, 1, 1, 0, 700, 98
37725, V, 1, 1, 1, 1, 0, 700, 98
37726, V, 1, 1, 1, 1, 0, 700, 98
37727, V, 1, 1, 1, 1, 0, 700, 98
37728, V, 1, 1, 1, 1, 0, 700, 98
37729, V, 1, 1, 1, 1, 0, 700, 98
37730, V, 1, 1, 1, 1, 0, 700, 98
37731, V, 1, 1, 1, 1, 0, 700, 98
37732, V, 1, 1, 1, 1, 0, 700, 98
37733, V, 1, 1, 1, 1, 0, 700, 98
37734, V, 1, 1, 1, 1, 0, 700, 98
37735, V, 1, 1, 1, 1, 0, 700, 98
37736, V, 1, 1, 1, 1, 0, 700, 98
37737, V, 1, 1, 1, 1, 0, 700, 98
37738, V, 1, 1, 1, 1, 0, 700, 98
37739, V, 1, 1, 1, 1, 0, 700, 98
37740, V, 1, 1, 1, 1, 0, 700, 98
37741, V, 1, 1, 1, 1, 0, 700, 98
37742, V, 1, 1, 1, 1, 0, 700, 98
37743, V, 1, 1, 1, 1, 0, 700, 98
37744, V, 1, 1, 1, 1, 0, 700, 98
37745, V, 1, 1, 1, 1, 0, 700, 98
37746, V, 1, 1, 1, 1, 0, 700, 98
37747, V, 1, 1, 1, 1, 0, 700, 98
37748, V, 1, 1, 1, 1, 0, 700, 98
37749, V, 1, 1, 1, 1, 0, 700, 98
37750, V, 1, 1, 1, 1, 0, 700, 98
37751, V, 1, 1, 1, 1, 0, 700, 98
37752, V, 1, 1, 1, 1, 0, 700, 98
37753, V, 1, 1, 1, 1, 0, 700, 98
37754, V, 1, 1, 1, 1, 0, 700, 98
37755, V, 1, 1, 1, 1, 0, 700, 98
37756, V, 1, 1, 1, 1, 0, 700, 98
37757, V, 1, 1, 1, 1, 0, 700, 98
37758, V, 1, 1, 1, 1, 0, 700, 98
37760, V, 1, 1, 1, 1, 0, 700, 98
37761, V, 1, 1, 1, 1, 0, 700, 98
37762, V, 1, 1, 1, 1, 0, 700, 98
37763, V, 1, 1, 1, 1, 0, 700, 98
37764, V, 1, 1, 1, 1, 0, 700, 98
37765, V, 1, 1, 1, 1, 0, 700, 98
37766, V, 1, 1, 1, 1, 0, 700, 98
37767, V, 1, 1, 1, 1, 0, 700, 98
37768, V, 1, 1, 1, 1, 0, 700, 98
37769, V, 1, 1, 1, 1, 0, 700, 98
37770, V, 1, 1, 1, 1, 0, 700, 98
37771, V, 1, 1, 1, 1, 0, 700, 98
37772, V, 1, 1, 1, 1, 0, 700, 98
37773, V, 1, 1, 1, 1, 0, 700, 98
37774, V, 1, 1, 1, 1, 0, 700, 98
37775, V, 1, 1, 1, 1, 0, 700, 98
37776, V, 1, 1, 1, 1, 0, 700, 98
37777, V, 1, 1, 1, 1, 0, 700, 98
37778, V, 1, 1, 1, 1, 0, 700, 98
37779, V, 1, 1, 1, 1, 0, 700, 98
37780, V, 1, 1, 1, 1, 0, 700, 98
37781, V, 1, 1, 1, 1, 0, 700, 98
37782, V, 1, 1, 1, 1, 0, 700, 98
37783, V, 1, 1, 1, 1, 0, 700, 98
37784, V, 1, 1, 1, 1, 0, 700, 98
37785, V, 1, 1, 1, 1, 0, 700, 98
37786, V, 1, 1, 1, 1, 0, 700, 98
37787, V, 1, 1, 1, 1, 0, 700, 98
37788, V, 1, 1, 1, 1, 0, 700, 98
37789, V, 1, 1, 1, 1, 0, 700, 98
37790, V, 1, 1, 1, 1, 0, 700, 98
37791, V, 1, 1, 1, 1, 0, 700, 98
37792, V, 1, 1, 1, 1, 0, 700, 98
37793, V, 1, 1, 1, 1, 0, 700, 98
37794, V, 1, 1, 1, 1, 0, 700, 98
37795, V, 1, 1, 1, 1, 0, 700, 98
37796, V, 1, 1, 1, 1, 0, 700, 98
37797, V, 1, 0, 0, 1, 0, 700, 98
37797, V, 1, 0, 0, 0, 0, 700, 98
37798, V, 1, 1, 0, 0, 0, 700, 98
37798, V, 1, 1, 0, 0, 0, 700, 98
37799, V, 1, 1, 1, 1, 0, 700, 98
37800, V, 1, 1, 1, 1, 0, 700, 98
37801, V, 1, 1, 1, 1, 0, 700, 98
37803, V, 1, 1, 1, 1, 0, 700, 98
37804, V, 1, 1, 1, 1, 0, 700, 98
37805, V, 1, 1, 1, 1, 0, 700, 98
37806, V, 1, 1, 1, 1, 0, 700, 98
37807, V, 1, 1, 1, 1, 0, 700, 98
37808, V, 1, 1, 1, 1, 0, 700, 98
37809, V, 1, 1, 1, 1, 0, 700, 98
37810, V, 1, 1, 1, 1, 0, 700, 98
37811, V, 1, 1, 1, 1, 0, 700, 98
37812, V, 1, 1, 1, 1, 0, 700, 98
37813, V, 1, 1, 1, 1, 0, 700, 98
37814, V, 1, 1, 1, 1, 0, 700, 98
37815, V, 1, 1, 1, 1, 0, 700, 98
37816, V, 1, 1, 1, 1, 0, 700, 98
37817, V, 1, 1, 1, 1, 0, 700, 98
37818, V, 1, 1, 1, 1, 0, 700, 98
37819, V, 1, 1, 1, 1, 0, 700, 98
37820, V, 1, 1, 1, 1, 0, 700, 98
37821, V, 1, 1, 1, 1, 0, 700, 98
37822, V, 1, 1, 1, 1, 0, 700, 98
37823, V, 1, 1, 1, 1, 0, 700, 98
37824, V, 1, 1, 1, 1, 0, 700, 98
37825, V, 1, 1, 1, 1, 0, 700, 98
37826, V, 1, 1, 1, 1, 0, 700, 98
37827, V, 1, 1, 1, 1, 0, 700, 98
37828, V, 1, 1, 1, 1, 0, 700, 98
37829, V, 1, 1, 1, 1, 0, 700, 98
37830, V, 1, 1, 1, 1, 0, 700, 98
37831, V, 1, 1, 1, 1, 0, 700, 98
37832, V, 1, 1, 1, 1, 0, 700, 98
37833, V, 1, 1, 1, 1, 0, 700, 98
37834, V, 1, 1, 1, 1, 0, 700, 98
37835, V, 1, 1, 1, 1, 0, 700, 98
37836, V, 1, 1, 1, 1, 0, 700, 98
37837, V, 1, 1, 1, 1, 0, 700, 98
37838, V, 1, 1, 1, 1, 0, 700, 98
37839, V, 1, 1, 1, 1, 0, 700, 98
37840, V, 1, 1, 1, 1, 0, 700, 98
37841, V, 1, 1, 1, 1, 0, 700, 98
37842, V, 1, 1, 1, 1, 0, 700, 98
37843, V, 1, 1, 1, 1, 0, 700, 98
37844, V, 1, 1, 1, 1, 0, 700, 98
37846, V, 1, 1, 1, 1, 0, 700, 98
37847, V, 1, 1, 1, 1, 0, 700, 98
37848, V, 1, 1, 1, 1, 0, 700, 98
37849, V, 1, 1, 1, 1, 0, 700, 98
37850, V, 1, 1, 1, 1, 0, 700, 98
37851, V, 1, 1, 1, 1, 0, 700, 98
37852, V, 1, 1, 1, 1, 0, 700, 98
37853, V, 1, 1, 1, 1, 0, 700, 98
37854, V, 1, 1, 1, 1, 0, 700, 98
37855, V, 1, 1, 1, 1, 0, 700, 98
37856, V, 1, 1, 1, 1, 0, 700, 98
37857, V, 1, 1, 1, 1, 0, 700, 98
37858, V, 1, 1, 1, 1, 0, 700, 98
37859, V, 1, 1, 1, 1, 0, 700, 98
37860, V, 1, 1, 1, 1, 0, 700, 98
37861, V, 1, 1, 1, 1, 0, 700, 98
37862, V, 1, 1, 1, 1, 0, 700, 98
37863, V, 1, 1, 1, 1, 0, 700, 98
37864, V, 1, 1, 1, 1, 0, 700, 98
37865, V, 1, 1, 1, 1, 0, 700, 98
37866, V, 1, 1, 1, 1, 0, 700, 98
37867, V, 1, 1, 1, 1, 0, 700, 98
37868, V, 1, 1, 1, 1, 0, 700, 98
37869, V, 1, 1, 1, 1, 0, 700, 98
37870, V, 1, 1, 1, 1, 0, 700, 98
37871, V, 1, 1, 1, 1, 0, 700, 98
37872, V, 1, 1, 1, 1, 0, 700, 98
37873, V, 1, 1, 1, 1, 0, 700, 98
37874, V, 1, 1, 1, 1, 0, 700, 98
37875, V, 1, 1, 1, 1, 0, 700, 98
37876, V, 1, 1, 1, 1, 0, 700, 98
37877, V, 1, 1, 1, 1, 0, 700, 98
37878, V, 1, 1, 1, 1, 0, 700, 98
37879, V, 1, 1, 1, 1, 0, 700, 98
37880, V, 1, 1, 1, 1, 0, 700, 98
37881, V, 1, 1, 1, 1, 0, 700, 98
37882, V, 1, 1, 1, 1, 0, 700, 98
37883, V, 1, 1, 1, 1, 0, 700, 98
37884, V, 1, 1, 1, 1, 0, 700, 98
37885, V, 1, 1, 1, 1, 0, 700, 98
37886, V, 1, 1, 1, 1, 0, 700, 98
37888, V, 1, 1, 1, 1, 0, 700, 98
37889, V, 1, 1, 1, 1, 0, 700, 98
37890, V, 1, 1, 1, 1, 0, 700, 98
37891, V, 1, 1, 1, 1, 0, 700, 98
37892, V, 1, 1, 1, 1, 0, 700, 98
37893, V, 1, 1, 1, 1, 0, 700, 98
37894, V, 1, 1, 1, 1, 0, 700, 98
37895, V, 1, 1, 1, 1, 0, 700, 98
37896, V, 1, 1, 1, 1, 0, 700, 98
37897, V, 1, 1, 1, 1, 0, 700, 98
37898, V, 1, 1, 1, 1, 0, 700, 98
37899, V, 1, 1, 1, 1, 0, 700, 98
37900, V, 1, 1, 1, 1, 0, 700, 98
37901, V, 1, 1, 1, 1, 0, 700, 98
37902, V, 1, 1, 1, 1, 0, 700, 98
37903, V, 1, 1, 1, 1, 0, 700, 98
37904, V, 1, 1, 1, 1, 0, 700, 98
37905, V, 1, 1, 1, 1, 0, 700, 98
37906, V, 1, 1, 1, 1, 0, 700, 98
37907, V, 1, 1, 1, 1, 0, 700, 98
37908, V, 1, 1, 1, 1, 0, 700, 98
37909, V, 1, 1, 1, 1, 0, 700, 98
37910, V, 1, 1, 1, 1, 0, 700, 98
37911, V, 1, 1, 1, 1, 0, 700, 98
37912, V, 1, 1, 1, 1, 0, 700, 98
37913, V, 1, 1, 1, 1, 0, 700, 98
37914, V, 1, 1, 1, 1, 0, 700, 98
37915, V, 1, 1, 1, 1, 0, 700, 98
37916, V, 1, 1, 1, 1, 0, 700, 98
37917, V, 1, 1, 1, 1, 0, 700, 98
37918, V, 1, 1, 1, 1, 0, 700, 98
37919, V, 1, 1, 1, 1, 0, 700, 98
37920, V, 1, 1, 1, 1, 0, 700, 98
37921, V, 1, 1, 1, 1, 0, 700, 98
37922, V, 1, 1, 1, 1, 0, 700, 98
37923, V, 1, 1, 1, 1, 0, 700, 98
37924, V, 1, 1, 1, 1, 0, 700, 98
37925, V, 1, 1, 1, 1, 0, 700, 98
37926, V, 1, 1, 1, 1, 0, 700, 98
37927, V, 1, 1, 1, 1, 0, 700, 98
37928, V, 1, 1, 1, 1, 0, 700, 98
37929, V, 1, 1, 1, 1, 0, 700, 98
37931, V, 1, 1, 1, 1, 0, 700, 98
37932, V, 1, 1, 1, 1, 0, 700, 98
37933, V, 1, 1, 1, 1, 0, 700, 98
37934, V, 1, 1, 1, 1, 0, 700, 98
37935, V, 1, 1, 1, 1, 0, 700, 98
37936, V, 1, 1, 1, 1, 0, 700, 98
37937, V, 1, 1, 1, 1, 0, 700, 98
37938, V, 1, 1, 1, 1, 0, 700, 98
37939, V, 1, 1, 1, 1, 0, 700, 98
37940, V, 1, 1, 1, 1, 0, 700, 98
37941, V, 1, 1, 1, 1, 0, 700, 98
37942, V, 1, 1, 1, 1, 0, 700, 98
37943, V, 1, 1, 1, 1, 0, 700, 98
37944, V, 1, 1, 1, 1, 0, 700, 98
37945, V, 1, 1, 1, 1, 0, 700, 98
37946, V, 1, 1, 1, 1, 0, 700, 98
37947, V, 1, 1, 1, 1, 0, 700, 98
37948, V, 1, 1, 1, 1, 0, 700, 98
37949, V, 1, 1, 1, 1, 0, 700, 98
37950, V, 1, 1, 1, 1, 0, 700, 98
37951, V, 1, 1, 1, 1, 0, 700, 98
37952, V, 1, 1, 1, 1, 0, 700, 98
37953, V, 1, 1, 1, 1, 0, 700, 98
37954, V, 1, 1, 1, 1, 0, 700, 98
37955, V, 1, 1, 1, 1, 0, 700, 98
37956, V, 1, 1, 1, 1, 0, 700, 98
37957, V, 1, 1, 1, 1, 0, 700, 98
37958, V, 1, 1, 1, 1, 0, 700, 98
37959, V, 1, 1, 1, 1, 0, 700, 98
37960, V, 1, 1, 1, 1, 0, 700, 98
37961, V, 1, 1, 1, 1, 0, 700, 98
37962, V, 1, 1, 1, 1, 0, 700, 98
37963, V, 1, 1, 1, 1, 0, 700, 98
37964, V, 1, 1, 1, 1, 0, 700, 98
37965, V, 1, 1, 1, 1, 0, 700, 98
37966, V, 1, 1, 1, 1, 0, 700, 98
37967, V, 1, 1, 1, 1, 0, 700, 98
37968, V, 1, 1, 1, 1, 0, 700, 98
37969, V, 1, 1, 1, 1, 0, 700, 98
37970, V, 1, 1, 1, 1, 0, 700, 98
37971, V, 1, 1, 1, 1, 0, 700, 98
37972, V, 1, 1, 1, 1, 0, 700, 98
37974, V, 1, 1, 1, 1, 0, 700, 98
37975, V, 1, 1, 1, 1, 0, 700, 98
37976, V, 1, 1, 1, 1, 0, 700, 98
37977, V, 1, 1, 1, 1, 0, 700, 98
37978, V, 1, 1, 1, 1, 0, 700, 98
37979, V, 1, 1, 1, 1, 0, 700, 98
37980, V, 1, 1, 1, 1, 0, 700, 98
37981, V, 1, 1, 1, 1, 0, 700, 98
37982, V, 1, 1, 1, 1, 0, 700, 98
37983, V, 1, 1, 1, 1, 0, 700, 98
37984, V, 1, 1, 1, 1, 0, 700, 98
37985, V, 1, 1, 1, 1, 0, 700, 98
37986, V, 1, 1, 1, 1, 0, 700, 98
37987, V, 1, 1, 1, 1, 0, 700, 98
37988, V, 1, 1, 1, 1, 0, 700, 98
37989, V, 1, 1, 1, 1, 0, 700, 98
37990, V, 1, 1, 1, 1, 0, 700, 98
37991, V, 1, 1, 1, 1, 0, 700, 98
37992, V, 1, 1, 1, 1, 0, 700, 98
37993, V, 1, 1, 1, 1, 0, 700, 98
37994, V, 1, 1, 1, 1, 0, 700, 98
37995, V, 1, 1, 1, 1, 0, 700, 98
37996, V, 1, 1, 1, 1, 0, 700, 98
37997, V, 1, 1, 1, 1, 0, 700, 98
37998, V, 1, 1, 1, 1, 0, 700, 98
37999, V, 1, 1, 1, 1, 0, 700, 98
38000, V, 1, 1, 1, 1, 0, 700, 98
38001, V, 1, 1, 1, 1, 0, 700, 98
38002, V, 1, 1, 1, 1, 0, 700, 98
38003, V, 1, 1, 1, 1, 0, 700, 98
38004, V, 1, 1, 1, 1, 0, 700, 98
38005, V, 1, 1, 1, 1, 0, 700, 98
38006, V, 1, 1, 1, 1, 0, 700, 98
38007, V, 1, 1, 1, 1, 0, 700, 98
38008, V, 1, 1, 1, 1, 0, 700, 98
38009, V, 1, 1, 1, 1, 0, 700, 98
38010, V, 1, 1, 1, 1, 0, 700, 98
38011, V, 1, 1, 1, 1, 0, 700, 98
38012, V, 1, 1, 1, 1, 0, 700, 98
38013, V, 1, 1, 1, 1, 0, 700, 98
38014, V, 1, 1, 1, 1, 0, 700, 98
38016, V, 1, 1, 1, 1, 0, 700, 98
38017, V, 1, 1, 1, 1, 0, 700, 98
38018, V, 1, 1, 1, 1, 0, 700, 98
38019, V, 1, 1, 1, 1, 0, 700, 98
38020, V, 1, 1, 1, 1, 0, 700, 98
38021, V, 1, 1, 1, 1, 0, 700, 98
38022, V, 1, 1, 1, 1, 0, 700, 98
38023, V, 1, 1, 1, 1, 0, 700, 98
38024, V, 1, 1, 1, 1, 0, 700, 98
38025, V, 1, 1, 1, 1, 0, 700, 98
38026, V, 1, 1, 1, 1, 0, 700, 98
38027, V, 1, 1, 1, 1, 0, 700, 98
38028, V, 1, 1, 1, 1, 0, 700, 98
38029, V, 1, 1, 1, 1, 0, 700, 98
38030, V, 1, 1, 1, 1, 0, 700, 98
38031, V, 1, 1, 1, 1, 0, 700, 98
38032, V, 1, 1, 1, 1, 0, 700, 98
38033, V, 1, 1, 1, 1, 0, 700, 98
38034, V, 1, 1, 1, 1, 0, 700, 98
38035, V, 1, 1, 1, 1, 0, 700, 98
38036, V, 1, 1, 1, 1, 0, 700, 98
38037, V, 1, 1, 1, 1, 0, 700, 98
38038, V, 1, 1, 1, 1, 0, 700, 98
38039, V, 1, 1, 1, 1, 0, 700, 98
38040, V, 1, 1, 1, 1, 0, 700, 98
38041, V, 1, 1, 1, 1, 0, 700, 98
38042, V, 1, 1, 1, 1, 0, 700, 98
38043, V, 1, 1, 1, 1, 0, 700, 98
38044, V, 1, 1, 1, 1, 0, 700, 98
38045, V, 1, 1, 1, 1, 0, 700, 98
38046, V, 1, 1, 1, 1, 0, 700, 98
38047, V, 1, 1, 1, 1, 0, 700, 98
38048, V, 1, 1, 1, 1, 0, 700, 98
38049, V, 1, 1, 1, 1, 0, 700, 98
38050, V, 1, 1, 1, 1, 0, 700, 98
38051, V, 1, 1, 1, 1, 0, 700, 98
38052, V, 1, 1, 1, 1, 0, 700, 98
38053, V, 1, 1, 1, 1, 0, 700, 98
38054, V, 1, 1, 1, 1, 0, 700, 98
38055, V, 1, 1, 1, 1, 0, 700, 98
38056, V, 1, 1, 1, 1, 0, 700, 98
38057, V, 1, 1, 1, 1, 0, 700, 98
38059, V, 1, 1, 1, 1, 0, 700, 98
38060, V, 1, 1, 1, 1, 0, 700, 98
38061, V, 1, 1, 1, 1, 0, 700, 98
38062, V, 1, 1, 1, 1, 0, 700, 98
38063, V, 1, 1, 1, 1, 0, 700, 98
38064, V, 1, 1, 1, 1, 0, 700, 98
38065, V, 1, 1, 1, 1, 0, 700, 98
38066, V, 1, 1, 1, 1, 0, 700, 98
38067, V, 1, 1, 1, 1, 0, 700, 98
38068, V, 1, 1, 1, 1, 0, 700, 98
38069, V, 1, 1, 1, 1, 0, 700, 98
38070, V, 1, 1, 1, 1, 0, 700, 98
38071, V, 1, 1, 1, 1, 0, 700, 98
38072, V, 1, 1, 1, 1, 0, 700, 98
38073, V, 1, 1, 1, 1, 0, 700, 98
38074, V, 1, 1, 1, 1, 0, 700, 98
38075, V, 1, 1, 1, 1, 0, 700, 98
38076, V, 1, 1, 1, 1, 0, 700, 98
38077, V, 1, 1, 1, 1, 0, 700, 98
38078, V, 1, 1, 1, 1, 0, 700, 98
38079, V, 1, 1, 1, 1, 0, 700, 98
38080, V, 1, 1, 1, 1, 0, 700, 98
38081, V, 1, 1, 1, 1, 0, 700, 98
38082, V, 1, 1, 1, 1, 0, 700, 98
38083, V, 1, 1, 1, 1, 0, 700, 98
38084, V, 1, 1, 1, 1, 0, 700, 98
38085, V, 1, 1, 1, 1, 0, 700, 98
38086, V, 1, 1, 1, 1, 0, 700, 98
38087, V, 1, 1, 1, 1, 0, 700, 98
38088, V, 1, 1, 1, 1, 0, 700, 98
38089, V, 1, 1, 1, 1, 0, 700, 98
38090, V, 1, 1, 1, 1, 0, 700, 98
38091, V, 1, 1, 1, 1, 0, 700, 98
38092, V, 1, 1, 1, 1, 0, 700, 98
38093, V, 1, 1, 1, 1, 0, 700, 98
38094, V, 1, 1, 1, 1, 0, 700, 98
38095, V, 1, 1, 1, 1, 0, 700, 98
38096, V, 1, 1, 1, 1, 0, 700, 98
38097, V, 1, 1, 1, 1, 0, 700, 98
38098, V, 1, 1, 1, 1, 0, 700, 98
38099, V, 1, 1, 1, 1, 0, 700, 98
38100, V, 1, 1, 1, 1, 0, 700, 98
38102, V, 1, 1, 1, 1, 0, 700, 98
38103, V, 1, 1, 1, 1, 0, 700, 98
38104, V, 1, 1, 1, 1, 0, 700, 98
38105, V, 1, 1, 1, 1, 0, 700, 98
38106, V, 1, 1, 1, 1, 0, 700, 98
38107, V, 1, 1, 1, 1, 0, 700, 98
38108, V, 1, 1, 1, 1, 0, 700, 98
38109, V, 1, 1, 1, 1, 0, 700, 98
38110, V, 1, 1, 1, 1, 0, 700, 98
38111, V, 1, 1, 1, 1, 0, 700, 98
38112, V, 1, 1, 1, 1, 0, 700, 98
38113, V, 1, 1, 1, 1, 0, 700, 98
38114, V, 1, 1, 1, 1, 0, 700, 98
38115, V, 1, 1, 1, 1, 0, 700, 98
38116, V, 1, 1, 1, 1, 0, 700, 98
38117, V, 1, 1, 1, 1, 0, 700, 98
38118, V, 1, 1, 1, 1, 0, 700, 98
38119, V, 1, 1, 1, 1, 0, 700, 98
38120, V, 1, 1, 1, 1, 0, 700, 98
38121, V, 1, 1, 1, 1, 0, 700, 98
38122, V, 1, 1, 1, 1, 0, 700, 98
38123, V, 1, 1, 1, 1, 0, 700, 98
38124, V, 1, 1, 1, 1, 0, 700, 98
38125, V, 1, 1, 1, 1, 0, 700, 98
38126, V, 1, 1, 1, 1, 0, 700, 98
38127, V, 1, 1, 1, 1, 0, 700, 98
38128, V, 1, 1, 1, 1, 0, 700, 98
38129, V, 1, 1, 1, 1, 0, 700, 98
38130, V, 1, 1, 1, 1, 0, 700, 98
38131, V, 1, 1, 1, 1, 0, 700, 98
38132, V, 1, 1, 1, 1, 0, 700, 98
38133, V, 1, 1, 1, 1, 0, 700, 98
38134, V, 1, 1, 1, 1, 0, 700, 98
38135, V, 1, 1, 1, 1, 0, 700, 98
38136, V, 1, 1, 1, 1, 0, 700, 98
38137, V, 1, 1, 1, 1, 0, 700, 98
38138, V, 1, 1, 1, 1, 0, 700, 98
38139, V, 1, 1, 1, 1, 0, 700, 98
38140, V, 1, 1, 1, 1, 0, 700, 98
38141, V, 1, 1, 1, 1, 0, 700, 98
38142, V, 1, 1, 1, 1, 0, 700, 98
38144, V, 1, 1, 1, 1, 0, 700, 98
38145, V, 1, 1, 1, 1, 0, 700, 98
38146, V, 1, 1, 1, 1, 0, 700, 98
38147, V, 1, 1, 1, 1, 0, 700, 98
38148, V, 1, 1, 1, 1, 0, 700, 98
38149, V, 1, 1, 1, 1, 0, 700, 98
38150, V, 1, 1, 1, 1, 0, 700, 98
38151, V, 1, 1, 1, 1, 0, 700, 98
38152, V, 1, 1, 1, 1, 0, 700, 98
38153, V, 1, 1, 1, 1, 0, 700, 98
38154, V, 1, 1, 1, 1, 0, 700, 98
38155, V, 1, 1, 1, 1, 0, 700, 98
38156, V, 1, 1, 1, 1, 0, 700, 98
38157, V, 1, 1, 1, 1, 0, 700, 98
38158, V, 1, 1, 1, 1, 0, 700, 98
38159, V, 1, 1, 1, 1, 0, 700, 98
38160, V, 1, 1, 1, 1, 0, 700, 98
38161, V, 1, 1, 1, 1, 0, 700, 98
38162, V, 1, 1, 1, 1, 0, 700, 98
38163, V, 1, 1, 1, 1, 0, 700, 98
38164, V, 1, 1, 1, 1, 0, 700, 98
38165, V, 1, 1, 1, 1, 0, 700, 98
38166, V, 1, 1, 1, 1, 0, 700, 98
38167, V, 1, 1, 1, 1, 0, 700, 98
38168, V, 1, 1, 1, 1, 0, 700, 98
38169, V, 1, 1, 1, 1, 0, 700, 98
38170, V, 1, 1, 1, 1, 0, 700, 98
38171, V, 1, 1, 1, 1, 0, 700, 98
38172, V, 1, 1, 1, 1, 0, 700, 98
38173, V, 1, 1, 1, 1, 0, 700, 98
38174, V, 1, 1, 1, 1, 0, 700, 98
38175, V, 1, 1, 1, 1, 0, 700, 98
38176, V, 1, 1, 1, 1, 0, 700, 98
38177, V, 1, 1, 1, 1, 0, 700, 98
38178, V, 1, 1, 1, 1, 0, 700, 98
38179, V, 1, 1, 1, 1, 0, 700, 98
38180, V, 1, 1, 1, 1, 0, 700, 98
38181, V, 1, 1, 1, 1, 0, 700, 98
38182, V, 1, 1, 1, 1, 0, 700, 98
38183, V, 1, 1, 1, 1, 0, 700, 98
38184, V, 1, 1, 1, 1, 0, 700, 98
38185, V, 1, 1, 1, 1, 0, 700, 98
38187, V, 1, 1, 1, 1, 0, 700, 98
38188, V, 1, 1, 1, 1, 0, 700, 98
38189, V, 1, 1, 1, 1, 0, 700, 98
38190, V, 1, 1, 1, 1, 0, 700, 98
38191, V, 1, 1, 1, 1, 0, 700, 98
38192, V, 1, 1, 1, 1, 0, 700, 98
38193, V, 1, 1, 1, 1, 0, 700, 98
38194, V, 1, 1, 1, 1, 0, 700, 98
38195, V, 1, 1, 1, 1, 0, 700, 98
38196, V, 1, 1, 1, 1, 0, 700, 98
38197, V, 1, 1, 1, 1, 0, 700, 98
38198, V, 1, 1, 1, 1, 0, 700, 98
38199, V, 1, 1, 1, 1, 0, 700, 98
38200, V, 1, 1, 1, 1, 0, 700, 98
38201, V, 1, 1, 1, 1, 0, 700, 98
38202, V, 1, 1, 1, 1, 0, 700, 98
38203, V, 1, 1, 1, 1, 0, 700, 98
38204, V, 1, 1, 1, 1, 0, 700, 98
38205, V, 1, 1, 1, 1, 0, 700, 98
38206, V, 1, 1, 1, 1, 0, 700, 98
38207, V, 1, 1, 1, 1, 0, 700, 98
38208, V, 1, 1, 1, 1, 0, 700, 98
38209, V, 1, 1, 1, 1, 0, 700, 98
38210, V, 1, 0, 0, 1, 0, 700, 98
38210, V, 1, 0, 0, 0, 0, 700, 98
38211, V, 1, 1, 0, 0, 0, 700, 98
38211, V, 1, 1, 0, 0, 0, 700, 98
38212, V, 1, 1, 1, 1, 0, 700, 98
38213, V, 1, 1, 1, 1, 0, 700, 98
38214, V, 1, 1, 1, 1, 0, 700, 98
38215, V, 1, 1, 1, 1, 0, 700, 98
38216, V, 1, 1, 1, 1, 0, 700, 98
38217, V, 1, 1, 1, 1, 0, 700, 98
38218, V, 1, 1, 1, 1, 0, 700, 98
38219, V, 1, 1, 1, 1, 0, 700, 98
38220, V, 1, 1, 1, 1, 0, 700, 98
38221, V, 1, 1, 1, 1, 0, 700, 98
38222, V, 1, 1, 1, 1, 0, 700, 98
38223, V, 1, 1, 1, 1, 0, 700, 98
38224, V, 1, 1, 1, 1, 0, 700, 98
38225, V, 1, 1, 1, 1, 0, 700, 98
38226, V, 1, 1, 1, 1, 0, 700, 98
38227, V, 1, 1, 1, 1, 0, 700, 98
38228, V, 1, 1, 1, 1, 0, 700, 98
38230, V, 1, 1, 1, 1, 0, 700, 98
38231, V, 1, 1, 1, 1, 0, 700, 98
38232, V, 1, 1, 1, 1, 0, 700, 98
38233, V, 1, 1, 1, 1, 0, 700, 98
38234, V, 1, 1, 1, 1, 0, 700, 98
38235, V, 1, 1, 1, 1, 0, 700, 98
38236, V, 1, 1, 1, 1, 0, 700, 98
38237, V, 1, 1, 1, 1, 0, 700, 98
38238, V, 1, 1, 1, 1, 0, 700, 98
38239, V, 1, 1, 1, 1, 0, 700, 98
38240, V, 1, 1, 1, 1, 0, 700, 98
38241, V, 1, 1, 1, 1, 0, 700, 98
38242, V, 1, 1, 1, 1, 0, 700, 98
38243, V, 1, 1, 1, 1, 0, 700, 98
38244, V, 1, 1, 1, 1, 0, 700, 98
38245, V, 1, 1, 1, 1, 0, 700, 98
38246, V, 1, 1, 1, 1, 0, 700, 98
38247, V, 1, 1, 1, 1, 0, 700, 98
38248, V, 1, 1, 1, 1, 0, 700, 98
38249, V, 1, 1, 1, 1, 0, 700, 98
38250, V, 1, 1, 1, 1, 0, 700, 98
38251, V, 1, 1, 1, 1, 0, 700, 98
38252, V, 1, 1, 1, 1, 0, 700, 98
38253, V, 1, 1, 1, 1, 0, 700, 98
38254, V, 1, 1, 1, 1, 0, 700, 98
38255, V, 1, 1, 1, 1, 0, 700, 98
38256, V, 1, 1, 1, 1, 0, 700, 98
38257, V, 1, 1, 1, 1, 0, 700, 98
38258, V, 1, 1, 1, 1, 0, 700, 98
38259, V, 1, 1, 1, 1, 0, 700, 98
38260, V, 1, 1, 1, 1, 0, 700, 98
38261, V, 1, 1, 1, 1, 0, 700, 98
38262, V, 1, 1, 1, 1, 0, 700, 98
38263, V, 1, 1, 1, 1, 0, 700, 98
38264, V, 1, 1, 1, 1, 0, 700, 98
38265, V, 1, 1, 1, 1, 0, 700, 98
38266, V, 1, 1, 1, 1, 0, 700, 98
38267, V, 1, 1, 1, 1, 0, 700, 98
38268, V, 1, 1, 1, 1, 0, 700, 98
38269, V, 1, 1, 1, 1, 0, 700, 98
38270, V, 1, 1, 1, 1, 0, 700, 98
38272, V, 1, 1, 1, 1, 0, 700, 98
38273, V, 1, 1, 1, 1, 0, 700, 98
38274, V, 1, 1, 1, 1, 0, 700, 98
38275, V, 1, 1, 1, 1, 0, 700, 98
38276, V, 1, 1, 1, 1, 0, 700, 98
38277, V, 1, 1, 1, 1, 0, 700, 98
38278, V, 1, 1, 1, 1, 0, 700, 98
38279, V, 1, 1, 1, 1, 0, 700, 98
38280, V, 1, 1, 1, 1, 0, 700, 98
38281, V, 1, 1, 1, 1, 0, 700, 98
38282, V, 1, 1, 1, 1, 0, 700, 98
38283, V, 1, 1, 1, 1, 0, 700, 98
38284, V, 1, 1, 1, 1, 0, 700, 98
38285, V, 1, 1, 1, 1, 0, 700, 98
38286, V, 1, 1, 1, 1, 0, 700, 98
38287, V, 1, 1, 1, 1, 0, 700, 98
38288, V, 1, 1, 1, 1, 0, 700, 98
38289, V, 1, 1, 1, 1, 0, 700, 98
38290, V, 1, 1, 1, 1, 0, 700, 98
38291, V, 1, 1, 1, 1, 0, 700, 98
38292, V, 1, 1, 1, 1, 0, 700, 98
38293, V, 1, 1, 1, 1, 0, 700, 98
38294, V, 1, 1, 1, 1, 0, 700, 98
38295, V, 1, 1, 1, 1, 0, 700, 98
38296, V, 1, 1, 1, 1, 0, 700, 98
38297, V, 1, 1, 1, 1, 0, 700, 98
38298, V, 1, 1, 1, 1, 0, 700, 98
38299, V, 1, 1, 1, 1, 0, 700, 98
38300, V, 1, 1, 1, 1, 0, 700, 98
38301, V, 1, 1, 1, 1, 0, 700, 98
38302, V, 1, 1, 1, 1, 0, 700, 98
38303, V, 1, 1, 1, 1, 0, 700, 98
38304, V, 1, 1, 1, 1, 0, 700, 98
38305, V, 1, 1, 1, 1, 0, 700, 98
38306, V, 1, 1, 1, 1, 0, 700, 98
38307, V, 1, 1, 1, 1, 0, 700, 98
38308, V, 1, 1, 1, 1, 0, 700, 98
38309, V, 1, 1, 1, 1, 0, 700, 98
38310, V, 1, 1, 1, 1, 0, 700, 98
38311, V, 1, 1, 1, 1, 0, 700, 98
38312, V, 1, 1, 1, 1, 0, 700, 98
38313, V, 1, 1, 1, 1, 0, 700, 98
38315, V, 1, 1, 1, 1, 0, 700, 98
38316, V, 1, 1, 1, 1, 0, 700, 98
38317, V, 1, 1, 1, 1, 0, 700, 98
38318, V, 1, 1, 1, 1, 0, 700, 98
38319, V, 1, 1, 1, 1, 0, 700, 98
38320, V, 1, 1, 1, 1, 0, 700, 98
38321, V, 1, 1, 1, 1, 0, 700, 98
38322, V, 1, 1, 1, 1, 0, 700, 98
38323, V, 1, 1, 1, 1, 0, 700, 98
38324, V, 1, 1, 1, 1, 0, 700, 98
38325, V, 1, 1, 1, 1, 0, 700, 98
38326, V, 1, 1, 1, 1, 0, 700, 98
38327, V, 1, 1, 1, 1, 0, 700, 98
38328, V, 1, 1, 1, 1, 0, 700, 98
38329, V, 1, 1, 1, 1, 0, 700, 98
38330, V, 1, 1, 1, 1, 0, 700, 98
38331, V, 1, 1, 1, 1, 0, 700, 98
38332, V, 1, 1, 1, 1, 0, 700, 98
38333, V, 1, 1, 1, 1, 0, 700, 98
38334, V, 1, 1, 1, 1, 0, 700, 98
38335, V, 1, 1, 1, 1, 0, 700, 98
38336, V, 1, 1, 1, 1, 0, 700, 98
38337, V, 1, 1, 1, 1, 0, 700, 98
38338, V, 1, 1, 1, 1, 0, 700, 98
38339, V, 1, 1, 1, 1, 0, 700, 98
38340, V, 1, 1, 1, 1, 0, 700, 98
38341, V, 1, 1, 1, 1, 0, 700, 98
38342, V, 1, 1, 1, 1, 0, 700, 98
38343, V, 1, 1, 1, 1, 0, 700, 98
38344, V, 1, 1, 1, 1, 0, 700, 98
38345, V, 1, 1, 1, 1, 0, 700, 98
38346, V, 1, 1, 1, 1, 0, 700, 98
38347, V, 1, 0, 0, 1, 0, 700, 98
38347, V, 1, 0, 0, 0, 0, 700, 98
38348, V, 1, 1, 0, 0, 0, 700, 98
38348, V, 1, 1, 0, 0, 0, 700, 98
38349, V, 1, 1, 1, 1, 0, 700, 98
38350, V, 1, 1, 1, 1, 0, 700, 98
38351, V, 1, 1, 1, 1, 0, 700, 98
38352, V, 1, 1, 1, 1, 0, 700, 98
38353, V, 1, 1, 1, 1, 0, 700, 98
38354, V, 1, 1, 1, 1, 0, 700, 98
38355, V, 1, 1, 1, 1, 0, 700, 98
38356, V, 1, 1, 1, 1, 0, 700, 97
38358, V, 1, 1, 1, 1, 0, 700, 97
38359, V, 1, 1, 1, 1, 0, 700, 97
38360, V, 1, 1, 1, 1, 0, 700, 97
38361, V, 1, 1, 1, 1, 0, 700, 97
38362, V, 1, 1, 1, 1, 0, 700, 97
38363, V, 1, 1, 1, 1, 0, 700, 98
38364, V, 1, 1, 1, 1, 0, 700, 98
38365, V, 1, 1, 1, 1, 0, 700, 98
38366, V, 1, 1, 1, 1, 0, 700, 98
38367, V, 1, 1, 1, 1, 0, 700, 98
38368, V, 1, 1, 1, 1, 0, 700, 98
38369, V, 1, 1, 1, 1, 0, 700, 98
38370, V, 1, 1, 1, 1, 0, 700, 98
38371, V, 1, 1, 1, 1, 0, 700, 98
38372, V, 1, 1, 1, 1, 0, 700, 98
38373, V, 1, 1, 1, 1, 0, 700, 98
38374, V, 1, 1, 1, 1, 0, 700, 98
38375, V, 1, 1, 1, 1, 0, 700, 98
38376, V, 1, 1, 1, 1, 0, 700, 98
38377, V, 1, 1, 1, 1, 0, 700, 98
38378, V, 1, 1, 1, 1, 0, 700, 98
38379, V, 1, 1, 1, 1, 0, 700, 98
38380, V, 1, 1, 1, 1, 0, 700, 98
38381, V, 1, 1, 1, 1, 0, 700, 98
38382, V, 1, 1, 1, 1, 0, 700, 98
38383, V, 1, 1, 1, 1, 0, 700, 98
38384, V, 1, 1, 1, 1, 0, 700, 98
38385, V, 1, 1, 1, 1, 0, 700, 98
38386, V, 1, 1, 1, 1, 0, 700, 98
38387, V, 1, 1, 1, 1, 0, 700, 98
38388, V, 1, 1, 1, 1, 0, 700, 98
38389, V, 1, 1, 1, 1, 0, 700, 98
38390, V, 1, 1, 1, 1, 0, 700, 98
38391, V, 1, 1, 1, 1, 0, 700, 98
38392, V, 1, 1, 1, 1, 0, 700, 98
38393, V, 1, 1, 1, 1, 0, 700, 98
38394, V, 1, 1, 1, 1, 0, 700, 98
38395, V, 1, 1, 1, 1, 0, 700, 98
38396, V, 1, 1, 1, 1, 0, 700, 98
38397, V, 1, 1, 1, 1, 0, 700, 98
38398, V, 1, 1, 1, 1, 0, 700, 98
38400, V, 1, 1, 1, 1, 0, 700, 98
38401, V, 1, 1, 1, 1, 0, 700, 98
38402, V, 1, 1, 1, 1, 0, 700, 98
38403, V, 1, 1, 1, 1, 0, 700, 98
38404, V, 1, 1, 1, 1, 0, 700, 98
38405, V, 1, 1, 1, 1, 0, 700, 98
38406, V, 1, 1, 1, 1, 0, 700, 98
38407, V, 1, 1, 1, 1, 0, 700, 98
38408, V, 1, 1, 1, 1, 0, 700, 98
38409, V, 1, 1, 1, 1, 0, 700, 98
38410, V, 1, 1, 1, 1, 0, 700, 98
38411, V, 1, 1, 1, 1, 0, 700, 98
38412, V, 1, 1, 1, 1, 0, 700, 98
38413, V, 1, 1, 1, 1, 0, 700, 98
38414, V, 1, 1, 1, 1, 0, 700, 98
38415, V, 1, 1, 1, 1, 0, 700, 98
38416, V, 1, 1, 1, 1, 0, 700, 98
38417, V, 1, 1, 1, 1, 0, 700, 98
38418, V, 1, 1, 1, 1, 0, 700, 98
38419, V, 1, 1, 1, 1, 0, 700, 98
38420, V, 1, 1, 1, 1, 0, 700, 98
38421, V, 1, 1, 1, 1, 0, 700, 98
38422, V, 1, 1, 1, 1, 0, 700, 98
38423, V, 1, 1, 1, 1, 0, 700, 98
38424, V, 1, 1, 1, 1, 0, 700, 98
38425, V, 1, 1, 1, 1, 0, 700, 98
38426, V, 1, 1, 1, 1, 0, 700, 98
38427, V, 1, 1, 1, 1, 0, 700, 98
38428, V, 1, 1, 1, 1, 0, 700, 98
38429, V, 1, 1, 1, 1, 0, 700, 98
38430, V, 1, 1, 1, 1, 0, 700, 98
38431, V, 1, 1, 1, 1, 0, 700, 98
38432, V, 1, 1, 1, 1, 0, 700, 98
38433, V, 1, 1, 1, 1, 0, 700, 98
38434, V, 1, 1, 1, 1, 0, 700, 98
38435, V, 1, 1, 1, 1, 0, 700, 98
38436, V, 1, 1, 1, 1, 0, 700, 98
38437, V, 1, 1, 1, 1, 0, 700, 98
38438, V, 1, 1, 1, 1, 0, 700, 98
38439, V, 1, 1, 1, 1, 0, 700, 98
38440, V, 1, 1, 1, 1, 0, 700, 98
38441, V, 1, 1, 1, 1, 0, 700, 98
38443, V, 1, 1, 1, 1, 0, 700, 98
38444, V, 1, 1, 1, 1, 0, 700, 98
38445, V, 1, 1, 1, 1, 0, 700, 98
38446, V, 1, 1, 1, 1, 0, 700, 98
38447, V, 1, 1, 1, 1, 0, 700, 98
38448, V, 1, 1, 1, 1, 0, 700, 98
38449, V, 1, 1, 1, 1, 0, 700, 98
38450, V, 1, 1, 1, 1, 0, 700, 98
38451, V, 1, 1, 1, 1, 0, 700, 98
38452, V, 1, 1, 1, 1, 0, 700, 98
38453, V, 1, 1, 1, 1, 0, 700, 98
38454, V, 1, 1, 1, 1, 0, 700, 98
38455, V, 1, 1, 1, 1, 0, 700, 98
38456, V, 1, 1, 1, 1, 0, 700, 98
38457, V, 1, 1, 1, 1, 0, 700, 98
38458, V, 1, 1, 1, 1, 0, 700, 98
38459, V, 1, 1, 1, 1, 0, 700, 98
38460, V, 1, 1, 1, 1, 0, 700, 98
38461, V, 1, 1, 1, 1, 0, 700, 98
38462, V, 1, 1, 1, 1, 0, 700, 98
38463, V, 1, 1, 1, 1, 0, 700, 98
38464, V, 1, 1, 1, 1, 0, 700, 98
38465, V, 1, 1, 1, 1, 0, 700, 98
38466, V, 1, 1, 1, 1, 0, 700, 98
38467, V, 1, 1, 1, 1, 0, 700, 98
38468, V, 1, 1, 1, 1, 0, 700, 98
38469, V, 1, 1, 1, 1, 0, 700, 98
38470, V, 1, 1, 1, 1, 0, 700, 98
38471, V, 1, 1, 1, 1, 0, 700, 98
38472, V, 1, 1, 1, 1, 0, 700, 98
38473, V, 1, 1, 1, 1, 0, 700, 98
38474, V, 1, 1, 1, 1, 0, 700, 98
38475, V, 1, 1, 1, 1, 0, 700, 98
38476, V, 1, 1, 1, 1, 0, 700, 98
38477, V, 1, 1, 1, 1, 0, 700, 98
38478, V, 1, 1, 1, 1, 0, 700, 98
38479, V, 1, 1, 1, 1, 0, 700, 98
38480, V, 1, 1, 1, 1, 0, 700, 98
38481, V, 1, 1, 1, 1, 0, 700, 98
38482, V, 1, 1, 1, 1, 0, 700, 98
38483, V, 1, 1, 1, 1, 0, 700, 98
38484, V, 1, 1, 1, 1, 0, 700, 98
38486, V, 1, 1, 1, 1, 0, 700, 98
38487, V, 1, 1, 1, 1, 0, 700, 98
38488, V, 1, 1, 1, 1, 0, 700, 98
38489, V, 1, 1, 1, 1, 0, 700, 98
38490, V, 1, 1, 1, 1, 0, 700, 98
38491, V, 1, 1, 1, 1, 0, 700, 98
38492, V, 1, 1, 1, 1, 0, 700, 98
38493, V, 1, 1, 1, 1, 0, 700, 98
38494, V, 1, 1, 1, 1, 0, 700, 98
38495, V, 1, 1, 1, 1, 0, 700, 98
38496, V, 1, 1, 1, 1, 0, 700, 98
38497, V, 1, 1, 1, 1, 0, 700, 98
38498, V, 1, 1, 1, 1, 0, 700, 98
38499, V, 1, 1, 1, 1, 0, 700, 98
38500, V, 1, 1, 1, 1, 0, 700, 98
38501, V, 1, 1, 1, 1, 0, 700, 98
38502, V, 1, 1, 1, 1, 0, 700, 98
38503, V, 1, 1, 1, 1, 0, 700, 98
38504, V, 1, 1, 1, 1, 0, 700, 98
38505, V, 1, 1, 1, 1, 0, 700, 98
38506, V, 1, 1, 1, 1, 0, 700, 98
38507, V, 1, 1, 1, 1, 0, 700, 98
38508, V, 1, 1, 1, 1, 0, 700, 98
38509, V, 1, 1, 1, 1, 0, 700, 98
38510, V, 1, 1, 1, 1, 0, 700, 98
38511, V, 1, 1, 1, 1, 0, 700, 98
38512, V, 1, 1, 1, 1, 0, 700, 98
38513, V, 1, 1, 1, 1, 0, 700, 98
38514, V, 1, 1, 1, 1, 0, 700, 98
38515, V, 1, 1, 1, 1, 0, 700, 98
38516, V, 1, 1, 1, 1, 0, 700, 98
38517, V, 1, 1, 1, 1, 0, 700, 98
38518, V, 1, 1, 1, 1, 0, 700, 98
38519, V, 1, 1, 1, 1, 0, 700, 98
38520, V, 1, 1, 1, 1, 0, 700, 98
38521, V, 1, 1, 1, 1, 0, 700, 98
38522, V, 1, 1, 1, 1, 0, 700, 98
38523, V, 1, 1, 1, 1, 0, 700, 98
38524, V, 1, 1, 1, 1, 0, 700, 98
38525, V, 1, 1, 1, 1, 0, 700, 98
38526, V, 1, 1, 1, 1, 0, 700, 98
38528, V, 1, 1, 1, 1, 0, 700, 98
38529, V, 1, 1, 1, 1, 0, 700, 98
38530, V, 1, 1, 1, 1, 0, 700, 98
38531, V, 1, 1, 1, 1, 0, 700, 98
38532, V, 1, 1, 1, 1, 0, 700, 98
38533, V, 1, 1, 1, 1, 0, 700, 98
38534, V, 1, 1, 1, 1, 0, 700, 98
38535, V, 1, 1, 1, 1, 0, 700, 98
38536, V, 1, 1, 1, 1, 0, 700, 98
38537, V, 1, 1, 1, 1, 0, 700, 98
38538, V, 1, 1, 1, 1, 0, 700, 98
38539, V, 1, 1, 1, 1, 0, 700, 98
38540, V, 1, 1, 1, 1, 0, 700, 98
38541, V, 1, 1, 1, 1, 0, 700, 98
38542, V, 1, 1, 1, 1, 0, 700, 98
38543, V, 1, 1, 1, 1, 0, 700, 98
38544, V, 1, 1, 1, 1, 0, 700, 98
38545, V, 1, 1, 1, 1, 0, 700, 98
38546, V, 1, 1, 1, 1, 0, 700, 98
38547, V, 1, 1, 1, 1, 0, 700, 98
38548, V, 1, 1, 1, 1, 0, 700, 98
38549, V, 1, 1, 1, 1, 0, 700, 98
38550, V, 1, 1, 1, 1, 0, 700, 98
38551, V, 1, 1, 1, 1, 0, 700, 98
38552, V, 1, 1, 1, 1, 0, 700, 98
38553, V, 1, 1, 1, 1, 0, 700, 98
38554, V, 1, 1, 1, 1, 0, 700, 98
38555, V, 1, 1, 1, 1, 0, 700, 98
38556, V, 1, 1, 1, 1, 0, 700, 98
38557, V, 1, 1, 1, 1, 0, 700, 98
38558, V, 1, 1, 1, 1, 0, 700, 98
38559, V, 1, 1, 1, 1, 0, 700, 98
38560, V, 1, 1, 1, 1, 0, 700, 98
38561, V, 1, 1, 1, 1, 0, 700, 98
38562, V, 1, 1, 1, 1, 0, 700, 98
38563, V, 1, 1, 1, 1, 0, 700, 98
38564, V, 1, 1, 1, 1, 0, 700, 98
38565, V, 1, 1, 1, 1, 0, 700, 98
38566, V, 1, 1, 1, 1, 0, 700, 98
38567, V, 1, 1, 1, 1, 0, 700, 98
38568, V, 1, 1, 1, 1, 0, 700, 98
38569, V, 1, 1, 1, 1, 0, 700, 98
38571, V, 1, 1, 1, 1, 0, 700, 98
38572, V, 1, 1, 1, 1, 0, 700, 98
38573, V, 1, 1, 1, 1, 0, 700, 98
38574, V, 1, 1, 1, 1, 0, 700, 98
38575, V, 1, 1, 1, 1, 0, 700, 98
38576, V, 1, 1, 1, 1, 0, 700, 98
38577, V, 1, 1, 1, 1, 0, 700, 98
38578, V, 1, 1, 1, 1, 0, 700, 98
38579, V, 1, 1, 1, 1, 0, 700, 98
38580, V, 1, 1, 1, 1, 0, 700, 98
38581, V, 1, 1, 1, 1, 0, 700, 98
38582, V, 1, 1, 1, 1, 0, 700, 98
38583, V, 1, 1, 1, 1, 0, 700, 98
38584, V, 1, 1, 1, 1, 0, 700, 98
38585, V, 1, 1, 1, 1, 0, 700, 98
38586, V, 1, 1, 1, 1, 0, 700, 98
38587, V, 1, 1, 1, 1, 0, 700, 98
38588, V, 1, 1, 1, 1, 0, 700, 98
38589, V, 1, 1, 1, 1, 0, 700, 98
38590, V, 1, 1, 1, 1, 0, 700, 98
38591, V, 1, 1, 1, 1, 0, 700, 98
38592, V, 1, 1, 1, 1, 0, 700, 98
38593, V, 1, 1, 1, 1, 0, 700, 98
38594, V, 1, 1, 1, 1, 0, 700, 98
38595, V, 1, 1, 1, 1, 0, 700, 98
38596, V, 1, 1, 1, 1, 0, 700, 98
38597, V, 1, 1, 1, 1, 0, 700, 98
38598, V, 1, 1, 1, 1, 0, 700, 98
38599, V, 1, 1, 1, 1, 0, 700, 98
38600, V, 1, 1, 1, 1, 0, 700, 98
38601, V, 1, 1, 1, 1, 0, 700, 98
38602, V, 1, 1, 1, 1, 0, 700, 98
38603, V, 1, 1, 1, 1, 0, 700, 98
38604, V, 1, 1, 1, 1, 0, 700, 98
38605, V, 1, 1, 1, 1, 0, 700, 98
38606, V, 1, 1, 1, 1, 0, 700, 98
38607, V, 1, 1, 1, 1, 0, 700, 98
38608, V, 1, 1, 1, 1, 0, 700, 98
38609, V, 1, 1, 1, 1, 0, 700, 98
38610, V, 1, 1, 1, 1, 0, 700, 98
38611, V, 1, 1, 1, 1, 0, 700, 98
38612, V, 1, 1, 1, 1, 0, 700, 98
38614, V, 1, 1, 1, 1, 0, 700, 98
38615, V, 1, 1, 1, 1, 0, 700, 98
38616, V, 1, 1, 1, 1, 0, 700, 98
38617, V, 1, 1, 1, 1, 0, 700, 98
38618, V, 1, 1, 1, 1, 0, 700, 98
38619, V, 1, 1, 1, 1, 0, 700, 98
38620, V, 1, 1, 1, 1, 0, 700, 98
38621, V, 1, 1, 1, 1, 0, 700, 98
38622, V, 1, 1, 1, 1, 0, 700, 98
38623, V, 1, 1, 1, 1, 0, 700, 98
38624, V, 1, 1, 1, 1, 0, 700, 98
38625, V, 1, 1, 1, 1, 0, 700, 98
38626, V, 1, 1, 1, 1, 0, 700, 98
38627, V, 1, 1, 1, 1, 0, 700, 98
38628, V, 1, 1, 1, 1, 0, 700, 98
38629, V, 1, 1, 1, 1, 0, 700, 98
38630, V, 1, 1, 1, 1, 0, 700, 98
38631, V, 1, 1, 1, 1, 0, 700, 98
38632, V, 1, 1, 1, 1, 0, 700, 98
38633, V, 1, 1, 1, 1, 0, 700, 98
38634, V, 1, 1, 1, 1, 0, 700, 98
38635, V, 1, 1, 1, 1, 0, 700, 98
38636, V, 1, 1, 1, 1, 0, 700, 98
38637, V, 1, 1, 1, 1, 0, 700, 98
38638, V, 1, 1, 1, 1, 0, 700, 98
38639, V, 1, 1, 1, 1, 0, 700, 98
38640, V, 1, 1, 1, 1, 0, 700, 98
38641, V, 1, 1, 1, 1, 0, 700, 98
38642, V, 1, 1, 1, 1, 0, 700, 98
38643, V, 1, 1, 1, 1, 0, 700, 98
38644, V, 1, 1, 1, 1, 0, 700, 98
38645, V, 1, 1, 1, 1, 0, 700, 98
38646, V, 1, 1, 1, 1, 0, 700, 98
38647, V, 1, 1, 1, 1, 0, 700, 98
38648, V, 1, 1, 1, 1, 0, 700, 98
38649, V, 1, 1, 1, 1, 0, 700, 98
38650, V, 1, 1, 1, 1, 0, 700, 98
38651, V, 1, 1, 1, 1, 0, 700, 98
38652, V, 1, 1, 1, 1, 0, 700, 98
38653, V, 1, 1, 1, 1, 0, 700, 98
38654, V, 1, 1, 1, 1, 0, 700, 98
38656, V, 1, 1, 1, 1, 0, 700, 98
38657, V, 1, 1, 1, 1, 0, 700, 98
38658, V, 1, 1, 1, 1, 0, 700, 98
38659, V, 1, 1, 1, 1, 0, 700, 98
38660, V, 1, 1, 1, 1, 0, 700, 98
38661, V, 1, 1, 1, 1, 0, 700, 98
38662, V, 1, 1, 1, 1, 0, 700, 98
38663, V, 1, 1, 1, 1, 0, 700, 98
38664, V, 1, 1, 1, 1, 0, 700, 98
38665, V, 1, 1, 1, 1, 0, 700, 98
38666, V, 1, 1, 1, 1, 0, 700, 98
38667, V, 1, 1, 1, 1, 0, 700, 98
38668, V, 1, 1, 1, 1, 0, 700, 98
38669, V, 1, 1, 1, 1, 0, 700, 98
38670, V, 1, 1, 1, 1, 0, 700, 98
38671, V, 1, 1, 1, 1, 0, 700, 98
38672, V, 1, 1, 1, 1, 0, 700, 98
38673, V, 1, 1, 1, 1, 0, 700, 98
38674, V, 1, 1, 1, 1, 0, 700, 98
38675, V, 1, 1, 1, 1, 0, 700, 98
38676, V, 1, 1, 1, 1, 0, 700, 98
38677, V, 1, 1, 1, 1, 0, 700, 98
38678, V, 1, 1, 1, 1, 0, 700, 98
38679, V, 1, 1, 1, 1, 0, 700, 98
38680, V, 1, 1, 1, 1, 0, 700, 98
38681, V, 1, 1, 1, 1, 0, 700, 98
38682, V, 1, 1, 1, 1, 0, 700, 98
38683, V, 1, 1, 1, 1, 0, 700, 98
38684, V, 1, 1, 1, 1, 0, 700, 98
38685, V, 1, 1, 1, 1, 0, 700, 98
38686, V, 1, 1, 1, 1, 0, 700, 98
38687, V, 1, 1, 1, 1, 0, 700, 98
38688, V, 1, 1, 1, 1, 0, 700, 98
38689, V, 1, 1, 1, 1, 0, 700, 98
38690, V, 1, 1, 1, 1, 0, 700, 98
38691, V, 1, 1, 1, 1, 0, 700, 98
38692, V, 1, 1, 1, 1, 0, 700, 98
38693, V, 1, 1, 1, 1, 0, 700, 98
38694, V, 1, 1, 1, 1, 0, 700, 98
38695, V, 1, 1, 1, 1, 0, 700, 98
38696, V, 1, 1, 1, 1, 0, 700, 98
38697, V, 1, 1, 1, 1, 0, 700, 98
38699, V, 1, 1, 1, 1, 0, 700, 98
38700, V, 1, 1, 1, 1, 0, 700, 98
38701, V, 1, 1, 1, 1, 0, 700, 98
38702, V, 1, 1, 1, 1, 0, 700, 98
38703, V, 1, 1, 1, 1, 0, 700, 98
38704, V, 1, 1, 1, 1, 0, 700, 98
38705, V, 1, 1, 1, 1, 0, 700, 98
38706, V, 1, 1, 1, 1, 0, 700, 98
38707, V, 1, 1, 1, 1, 0, 700, 98
38708, V, 1, 1, 1, 1, 0, 700, 98
38709, V, 1, 1, 1, 1, 0, 700, 98
38710, V, 1, 1, 1, 1, 0, 700, 98
38711, V, 1, 1, 1, 1, 0, 700, 98
38712, V, 1, 1, 1, 1, 0, 700, 98
38713, V, 1, 1, 1, 1, 0, 700, 98
38714, V, 1, 1, 1, 1, 0, 700, 98
38715, V, 1, 1, 1, 1, 0, 700, 98
38716, V, 1, 1, 1, 1, 0, 700, 98
38717, V, 1, 1, 1, 1, 0, 700, 98
38718, V, 1, 1, 1, 1, 0, 700, 98
38719, V, 1, 1, 1, 1, 0, 700, 98
38720, V, 1, 1, 1, 1, 0, 700, 98
38721, V, 1, 1, 1, 1, 0, 700, 98
38722, V, 1, 1, 1, 1, 0, 700, 98
38723, V, 1, 1, 1, 1, 0, 700, 98
38724, V, 1, 1, 1, 1, 0, 700, 98
38725, V, 1, 1, 1, 1, 0, 700, 98
38726, V, 1, 1, 1, 1, 0, 700, 98
38727, V, 1, 1, 1, 1, 0, 700, 98
38728, V, 1, 1, 1, 1, 0, 700, 98
38729, V, 1, 1, 1, 1, 0, 700, 98
38730, V, 1, 1, 1, 1, 0, 700, 98
38731, V, 1, 1, 1, 1, 0, 700, 98
38732, V, 1, 1, 1, 1, 0, 700, 98
38733, V, 1, 1, 1, 1, 0, 700, 98
38734, V, 1, 1, 1, 1, 0, 700, 98
38735, V, 1, 1, 1, 1, 0, 700, 98
38736, V, 1, 1, 1, 1, 0, 700, 98
38737, V, 1, 1, 1, 1, 0, 700, 98
38738, V, 1, 1, 1, 1, 0, 700, 98
38739, V, 1, 1, 1, 1, 0, 700, 98
38740, V, 1, 1, 1, 1, 0, 700, 98
38742, V, 1, 1, 1, 1, 0, 700, 98
38743, V, 1, 1, 1, 1, 0, 700, 98
38744, V, 1, 1, 1, 1, 0, 700, 98
38745, V, 1, 1, 1, 1, 0, 700, 98
38746, V, 1, 1, 1, 1, 0, 700, 98
38747, V, 1, 1, 1, 1, 0, 700, 98
38748, V, 1, 1, 1, 1, 0, 700, 98
38749, V, 1, 1, 1, 1, 0, 700, 98
38750, V, 1, 1, 1, 1, 0, 700, 98
38751, V, 1, 1, 1, 1, 0, 700, 98
38752, V, 1, 1, 1, 1, 0, 700, 98
38753, V, 1, 1, 1, 1, 0, 700, 98
38754, V, 1, 1, 1, 1, 0, 700, 98
38755, V, 1, 1, 1, 1, 0, 700, 98
38756, V, 1, 1, 1, 1, 0, 700, 98
38757, V, 1, 1, 1, 1, 0, 700, 98
38758, V, 1, 1, 1, 1, 0, 700, 98
38759, V, 1, 1, 1, 1, 0, 700, 98
38760, V, 1, 1, 1, 1, 0, 700, 98
38761, V, 1, 1, 1, 1, 0, 700, 98
38762, V, 1, 1, 1, 1, 0, 700, 98
38763, V, 1, 1, 1, 1, 0, 700, 98
38764, V, 1, 1, 1, 1, 0, 700, 98
38765, V, 1, 1, 1, 1, 0, 700, 98
38766, V, 1, 1, 1, 1, 0, 700, 98
38767, V, 1, 1, 1, 1, 0, 700, 98
38768, V, 1, 1, 1, 1, 0, 700, 98
38769, V, 1, 1, 1, 1, 0, 700, 98
38770, V, 1, 1, 1, 1, 0, 700, 98
38771, V, 1, 1, 1, 1, 0, 700, 98
38772, V, 1, 1, 1, 1, 0, 700, 98
38773, V, 1, 1, 1, 1, 0, 700, 98
38774, V, 1, 1, 1, 1, 0, 700, 98
38775, V, 1, 1, 1, 1, 0, 700, 98
38776, V, 1, 1, 1, 1, 0, 700, 98
38777, V, 1, 1, 1, 1, 0, 700, 98
38778, V, 1, 1, 1, 1, 0, 700, 98
38779, V, 1, 1, 1, 1, 0, 700, 98
38780, V, 1, 1, 1, 1, 0, 700, 98
38781, V, 1, 1, 1, 1, 0, 700, 98
38782, V, 1, 1, 1, 1, 0, 700, 98
38784, V, 1, 1, 1, 1, 0, 700, 98
38785, V, 1, 1, 1, 1, 0, 700, 98
38786, V, 1, 1, 1, 1, 0, 700, 98
38787, V, 1, 1, 1, 1, 0, 700, 98
38788, V, 1, 1, 1, 1, 0, 700, 98
38789, V, 1, 1, 1, 1, 0, 700, 98
38790, V, 1, 1, 1, 1, 0, 700, 98
38791, V, 1, 1, 1, 1, 0, 700, 98
38792, V, 1, 1, 1, 1, 0, 700, 98
38793, V, 1, 1, 1, 1, 0, 700, 98
38794, V, 1, 1, 1, 1, 0, 700, 98
38795, V, 1, 1, 1, 1, 0, 700, 98
38796, V, 1, 1, 1, 1, 0, 700, 98
38797, V, 1, 1, 1, 1, 0, 700, 98
38798, V, 1, 1, 1, 1, 0, 700, 98
38799, V, 1, 1, 1, 1, 0, 700, 98
38800, V, 1, 1, 1, 1, 0, 700, 98
38801, V, 1, 1, 1, 1, 0, 700, 98
38802, V, 1, 1, 1, 1, 0, 700, 98
38803, V, 1, 1, 1, 1, 0, 700, 98
38804, V, 1, 1, 1, 1, 0, 700, 98
38805, V, 1, 1, 1, 1, 0, 700, 98
38806, V, 1, 1, 1, 1, 0, 700, 98
38807, V, 1, 1, 1, 1, 0, 700, 98
38808, V, 1, 1, 1, 1, 0, 700, 98
38809, V, 1, 1, 1, 1, 0, 700, 98
38810, V, 1, 1, 1, 1, 0, 700, 98
38811, V, 1, 1, 1, 1, 0, 700, 98
38812, V, 1, 1, 1, 1, 0, 700, 98
38813, V, 1, 1, 1, 1, 0, 700, 98
38814, V, 1, 1, 1, 1, 0, 700, 98
38815, V, 1, 1, 1, 1, 0, 700, 98
38816, V, 1, 1, 1, 1, 0, 700, 98
38817, V, 1, 1, 1, 1, 0, 700, 98
38818, V, 1, 1, 1, 1, 0, 700, 98
38819, V, 1, 1, 1, 1, 0, 700, 98
38820, V, 1, 1, 1, 1, 0, 700, 98
38821, V, 1, 1, 1, 1, 0, 700, 98
38822, V, 1, 1, 1, 1, 0, 700, 98
38823, V, 1, 1, 1, 1, 0, 700, 98
38824, V, 1, 1, 1, 1, 0, 700, 98
38825, V, 1, 1, 1, 1, 0, 700, 98
38827, V, 1, 1, 1, 1, 0, 700, 98
38828, V, 1, 1, 1, 1, 0, 700, 98
38829, V, 1, 1, 1, 1, 0, 700, 98
38830, V, 1, 1, 1, 1, 0, 700, 98
38831, V, 1, 1, 1, 1, 0, 700, 98
38832, V, 1, 1, 1, 1, 0, 700, 98
38833, V, 1, 1, 1, 1, 0, 700, 98
38834, V, 1, 1, 1, 1, 0, 700, 98
38835, V, 1, 1, 1, 1, 0, 700, 98
38836, V, 1, 1, 1, 1, 0, 700, 98
38837, V, 1, 1, 1, 1, 0, 700, 98
38838, V, 1, 1, 1, 1, 0, 700, 98
38839, V, 1, 1, 1, 1, 0, 700, 98
38840, V, 1, 1, 1, 1, 0, 700, 98
38841, V, 1, 1, 1, 1, 0, 700, 98
38842, V, 1, 1, 1, 1, 0, 700, 98
38843, V, 1, 1, 1, 1, 0, 700, 98
38844, V, 1, 1, 1, 1, 0, 700, 98
38845, V, 1, 1, 1, 1, 0, 700, 98
38846, V, 1, 1, 1, 1, 0, 700, 98
38847, V, 1, 1, 1, 1, 0, 700, 98
38848, V, 1, 1, 1, 1, 0, 700, 98
38849, V, 1, 1, 1, 1, 0, 700, 98
38850, V, 1, 1, 1, 1, 0, 700, 98
38851, V, 1, 1, 1, 1, 0, 700, 98
38852, V, 1, 1, 1, 1, 0, 700, 98
38853, V, 1, 1, 1, 1, 0, 700, 98
38854, V, 1, 1, 1, 1, 0, 700, 98
38855, V, 1, 1, 1, 1, 0, 700, 98
38856, V, 1, 1, 1, 1, 0, 700, 98
38857, V, 1, 1, 1, 1, 0, 700, 98
38858, V, 1, 1, 1, 1, 0, 700, 98
38859, V, 1, 1, 1, 1, 0, 700, 98
38860, V, 1, 1, 1, 1, 0, 700, 98
38861, V, 1, 1, 1, 1, 0, 700, 98
38862, V, 1, 1, 1, 1, 0, 700, 98
38863, V, 1, 1, 1, 1, 0, 700, 98
38864, V, 1, 1, 1, 1, 0, 700, 98
38865, V, 1, 1, 1, 1, 0, 700, 98
38866, V, 1, 1, 1, 1, 0, 700, 98
38867, V, 1, 1, 1, 1, 0, 700, 98
38868, V, 1, 1, 1, 1, 0, 700, 98
38870, V, 1, 1, 1, 1, 0, 700, 98
38871, V, 1, 1, 1, 1, 0, 700, 98
38872, V, 1, 1, 1, 1, 0, 700, 98
38873, V, 1, 1, 1, 1, 0, 700, 98
38874, V, 1, 1, 1, 1, 0, 700, 98
38875, V, 1, 1, 1, 1, 0, 700, 98
38876, V, 1, 1, 1, 1, 0, 700, 98
38877, V, 1, 1, 1, 1, 0, 700, 98
38878, V, 1, 1, 1, 1, 0, 700, 98
38879, V, 1, 1, 1, 1, 0, 700, 98
38880, V, 1, 1, 1, 1, 0, 700, 98
38881, V, 1, 1, 1, 1, 0, 700, 98
38882, V, 1, 1, 1, 1, 0, 700, 98
38883, V, 1, 1, 1, 1, 0, 700, 98
38884, V, 1, 1, 1, 1, 0, 700, 98
38885, V, 1, 1, 1, 1, 0, 700, 98
38886, V, 1, 1, 1, 1, 0, 700, 98
38887, V, 1, 1, 1, 1, 0, 700, 98
38888, V, 1, 1, 1, 1, 0, 700, 98
38889, V, 1, 1, 1, 1, 0, 700, 98
38890, V, 1, 1, 1, 1, 0, 700, 98
38891, V, 1, 1, 1, 1, 0, 700, 98
38892, V, 1, 1, 1, 1, 0, 700, 98
38893, V, 1, 1, 1, 1, 0, 700, 98
38894, V, 1, 1, 1, 1, 0, 700, 98
38895, V, 1, 1, 1, 1, 0, 700, 98
38896, V, 1, 1, 1, 1, 0, 700, 98
38897, V, 1, 1, 1, 1, 0, 700, 98
38898, V, 1, 1, 1, 1, 0, 700, 98
38899, V, 1, 1, 1, 1, 0, 700, 98
38900, V, 1, 1, 1, 1, 0, 700, 98
38901, V, 1, 1, 1, 1, 0, 700, 98
38902, V, 1, 1, 1, 1, 0, 700, 98
38903, V, 1, 1, 1, 1, 0, 700, 98
38904, V, 1, 1, 1, 1, 0, 700, 98
38905, V, 1, 1, 1, 1, 0, 700, 98
38906, V, 1, 1, 1, 1, 0, 700, 98
38907, V, 1, 1, 1, 1, 0, 700, 98
38908, V, 1, 1, 1, 1, 0, 700, 98
38909, V, 1, 1, 1, 1, 0, 700, 98
38910, V, 1, 1, 1, 1, 0, 700, 98
38912, V, 1, 1, 1, 1, 0, 700, 98
38913, V, 1, 1, 1, 1, 0, 700, 98
38914, V, 1, 1, 1, 1, 0, 700, 98
38915, V, 1, 1, 1, 1, 0, 700, 98
38916, V, 1, 1, 1, 1, 0, 700, 98
38917, V, 1, 1, 1, 1, 0, 700, 98
38918, V, 1, 1, 1, 1, 0, 700, 98
38919, V, 1, 1, 1, 1, 0, 700, 98
38920, V, 1, 1, 1, 1, 0, 700, 98
38921, V, 1, 1, 1, 1, 0, 700, 98
38922, V, 1, 1, 1, 1, 0, 700, 98
38923, V, 1, 1, 1, 1, 0, 700, 98
38924, V, 1, 1, 1, 1, 0, 700, 98
38925, V, 1, 1, 1, 1, 0, 700, 98
38926, V, 1, 1, 1, 1, 0, 700, 98
38927, V, 1, 1, 1, 1, 0, 700, 98
38928, V, 1, 1, 1, 1, 0, 700, 98
38929, V, 1, 1, 1, 1, 0, 700, 98
38930, V, 1, 1, 1, 1, 0, 700, 98
38931, V, 1, 1, 1, 1, 0, 700, 98
38932, V, 1, 1, 1, 1, 0, 700, 98
38933, V, 1, 1, 1, 1, 0, 700, 98
38934, V, 1, 1, 1, 1, 0, 700, 98
38935, V, 1, 1, 1, 1, 0, 700, 98
38936, V, 1, 1, 1, 1, 0, 700, 98
38937, V, 1, 1, 1, 1, 0, 700, 98
38938, V, 1, 1, 1, 1, 0, 700, 98
38939, V, 1, 1, 1, 1, 0, 700, 98
38940, V, 1, 1, 1, 1, 0, 700, 98
38941, V, 1, 1, 1, 1, 0, 700, 98
38942, V, 1, 1, 1, 1, 0, 700, 98
38943, V, 1, 1, 1, 1, 0, 700, 98
38944, V, 1, 1, 1, 1, 0, 700, 98
38945, V, 1, 1, 1, 1, 0, 700, 98
38946, V, 1, 1, 1, 1, 0, 700, 98
38947, V, 1, 1, 1, 1, 0, 700, 98
38948, V, 1, 1, 1, 1, 0, 700, 98
38949, V, 1, 1, 1, 1, 0, 700, 98
38950, V, 1, 1, 1, 1, 0, 700, 98
38951, V, 1, 1, 1, 1, 0, 700, 98
38952, V, 1, 1, 1, 1, 0, 700, 98
38953, V, 1, 1, 1, 1, 0, 700, 98
38955, V, 1, 1, 1, 1, 0, 700, 98
38956, V, 1, 1, 1, 1, 0, 700, 98
38957, V, 1, 1, 1, 1, 0, 700, 98
38958, V, 1, 1, 1, 1, 0, 700, 98
38959, V, 1, 1, 1, 1, 0, 700, 98
38960, V, 1, 1, 1, 1, 0, 700, 98
38961, V, 1, 1, 1, 1, 0, 700, 98
38962, V, 1, 1, 1, 1, 0, 700, 98
38963, V, 1, 1, 1, 1, 0, 700, 98
38964, V, 1, 1, 1, 1, 0, 700, 98
38965, V, 1, 1, 1, 1, 0, 700, 98
38966, V, 1, 1, 1, 1, 0, 700, 98
38967, V, 1, 1, 1, 1, 0, 700, 98
38968, V, 1, 1, 1, 1, 0, 700, 98
38969, V, 1, 1, 1, 1, 0, 700, 98
38970, V, 1, 1, 1, 1, 0, 700, 98
38971, V, 1, 1, 1, 1, 0, 700, 98
38972, V, 1, 1, 1, 1, 0, 700, 98
38973, V, 1, 1, 1, 1, 0, 700, 98
38974, V, 1, 1, 1, 1, 0, 700, 98
38975, V, 1, 1, 1, 1, 0, 700, 98
38976, V, 1, 1, 1, 1, 0, 700, 98
38977, V, 1, 1, 1, 1, 0, 700, 98
38978, V, 1, 1, 1, 1, 0, 700, 98
38979, V, 1, 1, 1, 1, 0, 700, 98
38980, V, 1, 1, 1, 1, 0, 700, 98
38981, V, 1, 1, 1, 1, 0, 700, 98
38982, V, 1, 1, 1, 1, 0, 700, 98
38983, V, 1, 1, 1, 1, 0, 700, 98
38984, V, 1, 1, 1, 1, 0, 700, 98
38985, V, 1, 1, 1, 1, 0, 700, 98
38986, V, 1, 1, 1, 1, 0, 700, 98
38987, V, 1, 1, 1, 1, 0, 700, 98
38988, V, 1, 1, 1, 1, 0, 700, 98
38989, V, 1, 1, 1, 1, 0, 700, 98
38990, V, 1, 1, 1, 1, 0, 700, 98
38991, V, 1, 1, 1, 1, 0, 700, 98
38992, V, 1, 1, 1, 1, 0, 700, 98
38993, V, 1, 1, 1, 1, 0, 700, 98
38994, V, 1, 1, 1, 1, 0, 700, 98
38995, V, 1, 1, 1, 1, 0, 700, 98
38996, V, 1, 1, 1, 1, 0, 700, 98
38998, V, 1, 1, 1, 1, 0, 700, 98
38999, V, 1, 1, 1, 1, 0, 700, 98
39000, V, 1, 1, 1, 1, 0, 700, 98
39001, V, 1, 1, 1, 1, 0, 700, 98
39002, V, 1, 1, 1, 1, 0, 700, 98
39003, V, 1, 1, 1, 1, 0, 700, 98
39004, V, 1, 1, 1, 1, 0, 700, 98
39005, V, 1, 1, 1, 1, 0, 700, 98
39006, V, 1, 1, 1, 1, 0, 700, 98
39007, V, 1, 1, 1, 1, 0, 700, 98
39008, V, 1, 1, 1, 1, 0, 700, 98
39009, V, 1, 1, 1, 1, 0, 700, 98
39010, V, 1, 1, 1, 1, 0, 700, 98
39011, V, 1, 1, 1, 1, 0, 700, 98
39012, V, 1, 1, 1, 1, 0, 700, 98
39013, V, 1, 1, 1, 1, 0, 700, 98
39014, V, 1, 1, 1, 1, 0, 700, 98
39015, V, 1, 1, 1, 1, 0, 700, 98
39016, V, 1, 1, 1, 1, 0, 700, 98
39017, V, 1, 1, 1, 1, 0, 700, 98
39018, V, 1, 1, 1, 1, 0, 700, 98
39019, V, 1, 1, 1, 1, 0, 700, 98
39020, V, 1, 1, 1, 1, 0, 700, 98
39021, V, 1, 1, 1, 1, 0, 700, 98
39022, V, 1, 1, 1, 1, 0, 700, 98
39023, V, 1, 1, 1, 1, 0, 700, 98
39024, V, 1, 1, 1, 1, 0, 700, 98
39025, V, 1, 1, 1, 1, 0, 700, 98
39026, V, 1, 1, 1, 1, 0, 700, 98
39027, V, 1, 1, 1, 1, 0, 700, 98
39028, V, 1, 1, 1, 1, 0, 700, 98
39029, V, 1, 1, 1, 1, 0, 700, 98
39030, V, 1, 1, 1, 1, 0, 700, 98
39031, V, 1, 1, 1, 1, 0, 700, 98
39032, V, 1, 1, 1, 1, 0, 700, 98
39033, V, 1, 1, 1, 1, 0, 700, 98
39034, V, 1, 1, 1, 1, 0, 700, 98
39035, V, 1, 1, 1, 1, 0, 700, 98
39036, V, 1, 1, 1, 1, 0, 700, 98
39037, V, 1, 1, 1, 1, 0, 700, 98
39038, V, 1, 1, 1, 1, 0, 700, 98
39040, V, 1, 1, 1, 1, 0, 700, 98
39041, V, 1, 1, 1, 1, 0, 700, 98
39042, V, 1, 1, 1, 1, 0, 700, 98
39043, V, 1, 1, 1, 1, 0, 700, 98
39044, V, 1, 1, 1, 1, 0, 700, 98
39045, V, 1, 1, 1, 1, 0, 700, 98
39046, V, 1, 1, 1, 1, 0, 700, 98
39047, V, 1, 1, 1, 1, 0, 700, 98
39048, V, 1, 1, 1, 1, 0, 700, 98
39049, V, 1, 1, 1, 1, 0, 700, 98
39050, V, 1, 1, 1, 1, 0, 700, 98
39051, V, 1, 1, 1, 1, 0, 700, 98
39052, V, 1, 1, 1, 1, 0, 700, 98
39053, V, 1, 1, 1, 1, 0, 700, 98
39054, V, 1, 1, 1, 1, 0, 700, 98
39055, V, 1, 1, 1, 1, 0, 700, 98
39056, V, 1, 1, 1, 1, 0, 700, 98
39057, V, 1, 1, 1, 1, 0, 700, 98
39058, V, 1, 1, 1, 1, 0, 700, 98
39059, V, 1, 1, 1, 1, 0, 700, 98
39060, V, 1, 1, 1, 1, 0, 700, 98
39061, V, 1, 1, 1, 1, 0, 700, 98
39062, V, 1, 1, 1, 1, 0, 700, 98
39063, V, 1, 1, 1, 1, 0, 700, 98
39064, V, 1, 1, 1, 1, 0, 700, 98
39065, V, 1, 1, 1, 1, 0, 700, 98
39066, V, 1, 1, 1, 1, 0, 700, 98
39067, V, 1, 1, 1, 1, 0, 700, 98
39068, V, 1, 1, 1, 1, 0, 700, 98
39069, V, 1, 1, 1, 1, 0, 700, 98
39070, V, 1, 1, 1, 1, 0, 700, 98
39071, V, 1, 1, 1, 1, 0, 700, 98
39072, V, 1, 1, 1, 1, 0, 700, 98
39073, V, 1, 1, 1, 1, 0, 700, 98
39074, V, 1, 1, 1, 1, 0, 700, 98
39075, V, 1, 1, 1, 1, 0, 700, 98
39076, V, 1, 1, 1, 1, 0, 700, 98
39077, V, 1, 1, 1, 1, 0, 700, 98
39078, V, 1, 1, 1, 1, 0, 700, 98
39079, V, 1, 1, 1, 1, 0, 700, 98
39080, V, 1, 1, 1, 1, 0, 700, 98
39081, V, 1, 1, 1, 1, 0, 700, 98
39083, V, 1, 1, 1, 1, 0, 700, 98
39084, V, 1, 1, 1, 1, 0, 700, 98
39085, V, 1, 1, 1, 1, 0, 700, 98
39086, V, 1, 1, 1, 1, 0, 700, 98
39087, V, 1, 1, 1, 1, 0, 700, 98
39088, V, 1, 1, 1, 1, 0, 700, 98
39089, V, 1, 1, 1, 1, 0, 700, 98
39090, V, 1, 1, 1, 1, 0, 700, 98
39091, V, 1, 1, 1, 1, 0, 700, 98
39092, V, 1, 1, 1, 1, 0, 700, 98
39093, V, 1, 1, 1, 1, 0, 700, 98
39094, V, 1, 1, 1, 1, 0, 700, 98
39095, V, 1, 1, 1, 1, 0, 700, 98
39096, V, 1, 1, 1, 1, 0, 700, 98
39097, V, 1, 1, 1, 1, 0, 700, 98
39098, V, 1, 1, 1, 1, 0, 700, 98
39099, V, 1, 1, 1, 1, 0, 700, 98
39100, V, 1, 1, 1, 1, 0, 700, 98
39101, V, 1, 1, 1, 1, 0, 700, 98
39102, V, 1, 1, 1, 1, 0, 700, 98
39103, V, 1, 1, 1, 1, 0, 700, 98
39104, V, 1, 1, 1, 1, 0, 700, 98
39105, V, 1, 1, 1, 1, 0, 700, 98
39106, V, 1, 1, 1, 1, 0, 700, 98
39107, V, 1, 1, 1, 1, 0, 700, 98
39108, V, 1, 1, 1, 1, 0, 700, 98
39109, V, 1, 1, 1, 1, 0, 700, 98
39110, V, 1, 1, 1, 1, 0, 700, 98
39111, V, 1, 1, 1, 1, 0, 700, 98
39112, V, 1, 1, 1, 1, 0, 700, 98
39113, V, 1, 1, 1, 1, 0, 700, 98
39114, V, 1, 1, 1, 1, 0, 700, 98
39115, V, 1, 1, 1, 1, 0, 700, 98
39116, V, 1, 1, 1, 1, 0, 700, 98
39117, V, 1, 1, 1, 1, 0, 700, 98
39118, V, 1, 1, 1, 1, 0, 700, 98
39119, V, 1, 1, 1, 1, 0, 700, 98
39120, V, 1, 1, 1, 1, 0, 700, 98
39121, V, 1, 1, 1, 1, 0, 700, 98
39122, V, 1, 1, 1, 1, 0, 700, 98
39123, V, 1, 1, 1, 1, 0, 700, 98
39124, V, 1, 1, 1, 1, 0, 700, 98
39126, V, 1, 1, 1, 1, 0, 700, 98
39127, V, 1, 1, 1, 1, 0, 700, 98
39128, V, 1, 1, 1, 1, 0, 700, 98
39129, V, 1, 1, 1, 1, 0, 700, 98
39130, V, 1, 1, 1, 1, 0, 700, 98
39131, V, 1, 1, 1, 1, 0, 700, 98
39132, V, 1, 1, 1, 1, 0, 700, 98
39133, V, 1, 1, 1, 1, 0, 700, 98
39134, V, 1, 1, 1, 1, 0, 700, 98
39135, V, 1, 1, 1, 1, 0, 700, 98
39136, V, 1, 1, 1, 1, 0, 700, 98
39137, V, 1, 1, 1, 1, 0, 700, 98
39138, V, 1, 1, 1, 1, 0, 700, 98
39139, V, 1, 1, 1, 1, 0, 700, 98
39140, V, 1, 1, 1, 1, 0, 700, 98
39141, V, 1, 1, 1, 1, 0, 700, 98
39142, V, 1, 1, 1, 1, 0, 700, 98
39143, V, 1, 1, 1, 1, 0, 700, 98
39144, V, 1, 1, 1, 1, 0, 700, 98
39145, V, 1, 1, 1, 1, 0, 700, 98
39146, V, 1, 1, 1, 1, 0, 700, 98
39147, V, 1, 1, 1, 1, 0, 700, 98
39148, V, 1, 1, 1, 1, 0, 700, 98
39149, V, 1, 1, 1, 1, 0, 700, 98
39150, V, 1, 1, 1, 1, 0, 700, 98
39151, V, 1, 1, 1, 1, 0, 700, 98
39152, V, 1, 1, 1, 1, 0, 700, 98
39153, V, 1, 1, 1, 1, 0, 700, 98
39154, V, 1, 1, 1, 1, 0, 700, 98
39155, V, 1, 1, 1, 1, 0, 700, 98
39156, V, 1, 1, 1, 1, 0, 700, 98
39157, V, 1, 1, 1, 1, 0, 700, 98
39158, V, 1, 1, 1, 1, 0, 700, 98
39159, V, 1, 1, 1, 1, 0, 700, 98
39160, V, 1, 1, 1, 1, 0, 700, 98
39161, V, 1, 1, 1, 1, 0, 700, 98
39162, V, 1, 1, 1, 1, 0, 700, 98
39163, V, 1, 1, 1, 1, 0, 700, 98
39164, V, 1, 1, 1, 1, 0, 700, 98
39165, V, 1, 1, 1, 1, 0, 700, 98
39166, V, 1, 1, 1, 1, 0, 700, 98
39168, V, 1, 1, 1, 1, 0, 700, 98
39169, V, 1, 1, 1, 1, 0, 700, 98
39170, V, 1, 1, 1, 1, 0, 700, 98
39171, V, 1, 1, 1, 1, 0, 700, 98
39172, V, 1, 1, 1, 1, 0, 700, 98
39173, V, 1, 1, 1, 1, 0, 700, 98
39174, V, 1, 1, 1, 1, 0, 700, 98
39175, V, 1, 1, 1, 1, 0, 700, 98
39176, V, 1, 1, 1, 1, 0, 700, 98
39177, V, 1, 1, 1, 1, 0, 700, 98
39178, V, 1, 1, 1, 1, 0, 700, 98
39179, V, 1, 1, 1, 1, 0, 700, 98
39180, V, 1, 1, 1, 1, 0, 700, 98
39181, V, 1, 1, 1, 1, 0, 700, 98
39182, V, 1, 1, 1, 1, 0, 700, 98
39183, V, 1, 1, 1, 1, 0, 700, 98
39184, V, 1, 1, 1, 1, 0, 700, 98
39185, V, 1, 1, 1, 1, 0, 700, 98
39186, V, 1, 1, 1, 1, 0, 700, 98
39187, V, 1, 1, 1, 1, 0, 700, 98
39188, V, 1, 1, 1, 1, 0, 700, 98
39189, V, 1, 1, 1, 1, 0, 700, 98
39190, V, 1, 1, 1, 1, 0, 700, 98
39191, V, 1, 1, 1, 1, 0, 700, 98
39192, V, 1, 1, 1, 1, 0, 700, 98
39193, V, 1, 1, 1, 1, 0, 700, 98
39194, V, 1, 1, 1, 1, 0, 700, 98
39195, V, 1, 1, 1, 1, 0, 700, 98
39196, V, 1, 1, 1, 1, 0, 700, 98
39197, V, 1, 1, 1, 1, 0, 700, 98
39198, V, 1, 1, 1, 1, 0, 700, 98
39199, V, 1, 1, 1, 1, 0, 700, 98
39200, V, 1, 1, 1, 1, 0, 700, 98
39201, V, 1, 1, 1, 1, 0, 700, 98
39202, V, 1, 1, 1, 1, 0, 700, 98
39203, V, 1, 1, 1, 1, 0, 700, 98
39204, V, 1, 1, 1, 1, 0, 700, 98
39205, V, 1, 1, 1, 1, 0, 700, 98
39206, V, 1, 1, 1, 1, 0, 700, 98
39207, V, 1, 1, 1, 1, 0, 700, 98
39208, V, 1, 1, 1, 1, 0, 700, 98
39209, V, 1, 1, 1, 1, 0, 700, 98
39211, V, 1, 1, 1, 1, 0, 700, 98
39212, V, 1, 1, 1, 1, 0, 700, 98
39213, V, 1, 1, 1, 1, 0, 700, 98
39214, V, 1, 1, 1, 1, 0, 700, 98
39215, V, 1, 1, 1, 1, 0, 700, 98
39216, V, 1, 1, 1, 1, 0, 700, 98
39217, V, 1, 1, 1, 1, 0, 700, 98
39218, V, 1, 1, 1, 1, 0, 700, 98
39219, V, 1, 1, 1, 1, 0, 700, 98
39220, V, 1, 1, 1, 1, 0, 700, 98
39221, V, 1, 1, 1, 1, 0, 700, 98
39222, V, 1, 1, 1, 1, 0, 700, 98
39223, V, 1, 1, 1, 1, 0, 700, 98
39224, V, 1, 1, 1, 1, 0, 700, 98
39225, V, 1, 1, 1, 1, 0, 700, 98
39226, V, 1, 1, 1, 1, 0, 700, 98
39227, V, 1, 1, 1, 1, 0, 700, 98
39228, V, 1, 1, 1, 1, 0, 700, 98
39229, V, 1, 1, 1, 1, 0, 700, 98
39230, V, 1, 1, 1, 1, 0, 700, 98
39231, V, 1, 1, 1, 1, 0, 700, 98
39232, V, 1, 1, 1, 1, 0, 700, 98
39233, V, 1, 1, 1, 1, 0, 700, 98
39234, V, 1, 1, 1, 1, 0, 700, 98
39235, V, 1, 1, 1, 1, 0, 700, 98
39236, V, 1, 1, 1, 1, 0, 700, 98
39237, V, 1, 1, 1, 1, 0, 700, 98
39238, V, 1, 1, 1, 1, 0, 700, 98
39239, V, 1, 1, 1, 1, 0, 700, 98
39240, V, 1, 1, 1, 1, 0, 700, 98
39241, V, 1, 1, 1, 1, 0, 700, 98
39242, V, 1, 1, 1, 1, 0, 700, 98
39243, V, 1, 1, 1, 1, 0, 700, 98
39244, V, 1, 1, 1, 1, 0, 700, 98
39245, V, 1, 1, 1, 1, 0, 700, 98
39246, V, 1, 1, 1, 1, 0, 700, 98
39247, V, 1, 1, 1, 1, 0, 700, 98
39248, V, 1, 1, 1, 1, 0, 700, 98
39249, V, 1, 1, 1, 1, 0, 700, 98
39250, V, 1, 1, 1, 1, 0, 700, 98
39251, V, 1, 1, 1, 1, 0, 700, 98
39252, V, 1, 1, 1, 1, 0, 700, 98
39254, V, 1, 1, 1, 1, 0, 700, 98
39255, V, 1, 1, 1, 1, 0, 700, 98
39256, V, 1, 1, 1, 1, 0, 700, 98
39257, V, 1, 1, 1, 1, 0, 700, 98
39258, V, 1, 1, 1, 1, 0, 700, 98
39259, V, 1, 1, 1, 1, 0, 700, 98
39260, V, 1, 1, 1, 1, 0, 700, 98
39261, V, 1, 1, 1, 1, 0, 700, 98
39262, V, 1, 1, 1, 1, 0, 700, 98
39263, V, 1, 1, 1, 1, 0, 700, 98
39264, V, 1, 1, 1, 1, 0, 700, 98
39265, V, 1, 1, 1, 1, 0, 700, 98
39266, V, 1, 1, 1, 1, 0, 700, 98
39267, V, 1, 1, 1, 1, 0, 700, 98
39268, V, 1, 1, 1, 1, 0, 700, 98
39269, V, 1, 1, 1, 1, 0, 700, 98
39270, V, 1, 1, 1, 1, 0, 700, 98
39271, V, 1, 1, 1, 1, 0, 700, 98
39272, V, 1, 1, 1, 1, 0, 700, 98
39273, V, 1, 1, 1, 1, 0, 700, 98
39274, V, 1, 1, 1, 1, 0, 700, 98
39275, V, 1, 1, 1, 1, 0, 700, 98
39276, V, 1, 1, 1, 1, 0, 700, 98
39277, V, 1, 1, 1, 1, 0, 700, 98
39278, V, 1, 1, 1, 1, 0, 700, 98
39279, V, 1, 1, 1, 1, 0, 700, 98
39280, V, 1, 1, 1, 1, 0, 700, 98
39281, V, 1, 1, 1, 1, 0, 700, 98
39282, V, 1, 1, 1, 1, 0, 700, 98
39283, V, 1, 1, 1, 1, 0, 700, 98
39284, V, 1, 1, 1, 1, 0, 700, 98
39285, V, 1, 1, 1, 1, 0, 700, 98
39286, V, 1, 1, 1, 1, 0, 700, 98
39287, V, 1, 1, 1, 1, 0, 700, 98
39288, V, 1, 1, 1, 1, 0, 700, 98
39289, V, 1, 1, 1, 1, 0, 700, 98
39290, V, 1, 1, 1, 1, 0, 700, 98
39291, V, 1, 1, 1, 1, 0, 700, 98
39292, V, 1, 1, 1, 1, 0, 700, 98
39293, V, 1, 1, 1, 1, 0, 700, 98
39294, V, 1, 1, 1, 1, 0, 700, 98
39296, V, 1, 1, 1, 1, 0, 700, 98
39297, V, 1, 1, 1, 1, 0, 700, 98
39298, V, 1, 1, 1, 1, 0, 700, 98
39299, V, 1, 1, 1, 1, 0, 700, 98
39300, V, 1, 1, 1, 1, 0, 700, 98
39301, V, 1, 1, 1, 1, 0, 700, 98
39302, V, 1, 1, 1, 1, 0, 700, 98
39303, V, 1, 1, 1, 1, 0, 700, 98
39304, V, 1, 1, 1, 1, 0, 700, 98
39305, V, 1, 1, 1, 1, 0, 700, 98
39306, V, 1, 1, 1, 1, 0, 700, 98
39307, V, 1, 1, 1, 1, 0, 700, 98
39308, V, 1, 1, 1, 1, 0, 700, 98
39309, V, 1, 1, 1, 1, 0, 700, 98
39310, V, 1, 1, 1, 1, 0, 700, 98
39311, V, 1, 1, 1, 1, 0, 700, 98
39312, V, 1, 1, 1, 1, 0, 700, 98
39313, V, 1, 1, 1, 1, 0, 700, 98
39314, V, 1, 1, 1, 1, 0, 700, 98
39315, V, 1, 1, 1, 1, 0, 700, 98
39316, V, 1, 1, 1, 1, 0, 700, 98
39317, V, 1, 1, 1, 1, 0, 700, 98
39318, V, 1, 1, 1, 1, 0, 700, 98
39319, V, 1, 1, 1, 1, 0, 700, 98
39320, V, 1, 1, 1, 1, 0, 700, 98
39321, V, 1, 1, 1, 1, 0, 700, 98
39322, V, 1, 1, 1, 1, 0, 700, 98
39323, V, 1, 1, 1, 1, 0, 700, 98
39324, V, 1, 1, 1, 1, 0, 700, 98
39325, V, 1, 1, 1, 1, 0, 700, 98
39326, V, 1, 1, 1, 1, 0, 700, 98
39327, V, 1, 1, 1, 1, 0, 700, 98
39328, V, 1, 1, 1, 1, 0, 700, 98
39329, V, 1, 1, 1, 1, 0, 700, 98
39330, V, 1, 1, 1, 1, 0, 700, 98
39331, V, 1, 1, 1, 1, 0, 700, 98
39332, V, 1, 1, 1, 1, 0, 700, 98
39333, V, 1, 1, 1, 1, 0, 700, 98
39334, V, 1, 1, 1, 1, 0, 700, 98
39335, V, 1, 1, 1, 1, 0, 700, 98
39336, V, 1, 1, 1, 1, 0, 700, 98
39337, V, 1, 1, 1, 1, 0, 700, 98
39339, V, 1, 1, 1, 1, 0, 700, 98
39340, V, 1, 1, 1, 1, 0, 700, 98
39341, V, 1, 1, 1, 1, 0, 700, 98
39342, V, 1, 1, 1, 1, 0, 700, 98
39343, V, 1, 1, 1, 1, 0, 700, 98
39344, V, 1, 1, 1, 1, 0, 700, 98
39345, V, 1, 1, 1, 1, 0, 700, 98
39346, V, 1, 1, 1, 1, 0, 700, 98
39347, V, 1, 1, 1, 1, 0, 700, 98
39348, V, 1, 1, 1, 1, 0, 700, 98
39349, V, 1, 1, 1, 1, 0, 700, 98
39350, V, 1, 1, 1, 1, 0, 700, 98
39351, V, 1, 1, 1, 1, 0, 700, 98
39352, V, 1, 1, 1, 1, 0, 700, 98
39353, V, 1, 1, 1, 1, 0, 700, 98
39354, V, 1, 1, 1, 1, 0, 700, 98
39355, V, 1, 1, 1, 1, 0, 700, 98
39356, V, 1, 1, 1, 1, 0, 700, 98
39357, V, 1, 1, 1, 1, 0, 700, 98
39358, V, 1, 1, 1, 1, 0, 700, 98
39359, V, 1, 1, 1, 1, 0, 700, 98
39360, V, 1, 1, 1, 1, 0, 700, 98
39361, V, 1, 1, 1, 1, 0, 700, 98
39362, V, 1, 1, 1, 1, 0, 700, 98
39363, V, 1, 1, 1, 1, 0, 700, 98
39364, V, 1, 1, 1, 1, 0, 700, 98
39365, V, 1, 1, 1, 1, 0, 700, 98
39366, V, 1, 1, 1, 1, 0, 700, 98
39367, V, 1, 1, 1, 1, 0, 700, 98
39368, V, 1, 1, 1, 1, 0, 700, 98
39369, V, 1, 1, 1, 1, 0, 700, 98
39370, V, 1, 1, 1, 1, 0, 700, 98
39371, V, 1, 1, 1, 1, 0, 700, 98
39372, V, 1, 1, 1, 1, 0, 700, 98
39373, V, 1, 1, 1, 1, 0, 700, 98
39374, V, 1, 1, 1, 1, 0, 700, 98
39375, V, 1, 1, 1, 1, 0, 700, 98
39376, V, 1, 1, 1, 1, 0, 700, 98
39377, V, 1, 1, 1, 1, 0, 700, 98
39378, V, 1, 1, 1, 1, 0, 700, 98
39379, V, 1, 1, 1, 1, 0, 700, 98
39380, V, 1, 1, 1, 1, 0, 700, 98
39382, V, 1, 1, 1, 1, 0, 700, 98
39383, V, 1, 1, 1, 1, 0, 700, 98
39384, V, 1, 1, 1, 1, 0, 700, 98
39385, V, 1, 1, 1, 1, 0, 700, 98
39386, V, 1, 1, 1, 1, 0, 700, 98
39387, V, 1, 1, 1, 1, 0, 700, 98
39388, V, 1, 1, 1, 1, 0, 700, 98
39389, V, 1, 1, 1, 1, 0, 700, 98
39390, V, 1, 1, 1, 1, 0, 700, 98
39391, V, 1, 1, 1, 1, 0, 700, 98
39392, V, 1, 1, 1, 1, 0, 700, 98
39393, V, 1, 1, 1, 1, 0, 700, 98
39394, V, 1, 1, 1, 1, 0, 700, 98
39395, V, 1, 1, 1, 1, 0, 700, 98
39396, V, 1, 1, 1, 1, 0, 700, 98
39397, V, 1, 1, 1, 1, 0, 700, 98
39398, V, 1, 1, 1, 1, 0, 700, 98
39399, V, 1, 1, 1, 1, 0, 700, 98
39400, V, 1, 1, 1, 1, 0, 700, 98
39401, V, 1, 1, 1, 1, 0, 700, 98
39402, V, 1, 1, 1, 1, 0, 700, 98
39403, V, 1, 1, 1, 1, 0, 700, 98
39404, V, 1, 1, 1, 1, 0, 700, 98
39405, V, 1, 1, 1, 1, 0, 700, 98
39406, V, 1, 1, 1, 1, 0, 700, 98
39407, V, 1, 1, 1, 1, 0, 700, 98
39408, V, 1, 1, 1, 1, 0, 700, 98
39409, V, 1, 1, 1, 1, 0, 700, 98
39410, V, 1, 1, 1, 1, 0, 700, 98
39411, V, 1, 1, 1, 1, 0, 700, 98
39412, V, 1, 1, 1, 1, 0, 700, 98
39413, V, 1, 1, 1, 1, 0, 700, 98
39414, V, 1, 1, 1, 1, 0, 700, 98
39415, V, 1, 1, 1, 1, 0, 700, 98
39416, V, 1, 1, 1, 1, 0, 700, 98
39417, V, 1, 1, 1, 1, 0, 700, 98
39418, V, 1, 1, 1, 1, 0, 700, 98
39419, V, 1, 1, 1, 1, 0, 700, 98
39420, V, 1, 1, 1, 1, 0, 700, 98
39421, V, 1, 1, 1, 1, 0, 700, 98
39422, V, 1, 1, 1, 1, 0, 700, 98
39424, V, 1, 1, 1, 1, 0, 700, 98
39425, V, 1, 1, 1, 1, 0, 700, 98
39426, V, 1, 1, 1, 1, 0, 700, 98
39427, V, 1, 1, 1, 1, 0, 700, 98
39428, V, 1, 1, 1, 1, 0, 700, 98
39429, V, 1, 1, 1, 1, 0, 700, 98
39430, V, 1, 1, 1, 1, 0, 700, 98
39431, V, 1, 1, 1, 1, 0, 700, 98
39432, V, 1, 1, 1, 1, 0, 700, 98
39433, V, 1, 1, 1, 1, 0, 700, 98
39434, V, 1, 1, 1, 1, 0, 700, 98
39435, V, 1, 1, 1, 1, 0, 700, 98
39436, V, 1, 1, 1, 1, 0, 700, 98
39437, V, 1, 1, 1, 1, 0, 700, 98
39438, V, 1, 1, 1, 1, 0, 700, 98
39439, V, 1, 1, 1, 1, 0, 700, 98
39440, V, 1, 1, 1, 1, 0, 700, 98
39441, V, 1, 1, 1, 1, 0, 700, 98
39442, V, 1, 1, 1, 1, 0, 700, 98
39443, V, 1, 1, 1, 1, 0, 700, 98
39444, V, 1, 1, 1, 1, 0, 700, 98
39445, V, 1, 1, 1, 1, 0, 700, 98
39446, V, 1, 1, 1, 1, 0, 700, 98
39447, V, 1, 1, 1, 1, 0, 700, 98
39448, V, 1, 1, 1, 1, 0, 700, 98
39449, V, 1, 1, 1, 1, 0, 700, 98
39450, V, 1, 1, 1, 1, 0, 700, 98
39451, V, 1, 1, 1, 1, 0, 700, 98
39452, V, 1, 1, 1, 1, 0, 700, 98
39453, V, 1, 1, 1, 1, 0, 700, 98
39454, V, 1, 1, 1, 1, 0, 700, 98
39455, V, 1, 1, 1, 1, 0, 700, 98
39456, V, 1, 1, 1, 1, 0, 700, 98
39457, V, 1, 1, 1, 1, 0, 700, 98
39458, V, 1, 1, 1, 1, 0, 700, 98
39459, V, 1, 1, 1, 1, 0, 700, 98
39460, V, 1, 1, 1, 1, 0, 700, 98
39461, V, 1, 1, 1, 1, 0, 700, 98
39462, V, 1, 1, 1, 1, 0, 700, 98
39463, V, 1, 1, 1, 1, 0, 700, 98
39464, V, 1, 1, 1, 1, 0, 700, 98
39465, V, 1, 1, 1, 1, 0, 700, 98
39467, V, 1, 1, 1, 1, 0, 700, 98
39468, V, 1, 1, 1, 1, 0, 700, 98
39469, V, 1, 1, 1, 1, 0, 700, 98
39470, V, 1, 1, 1, 1, 0, 700, 98
39471, V, 1, 1, 1, 1, 0, 700, 98
39472, V, 1, 1, 1, 1, 0, 700, 98
39473, V, 1, 1, 1, 1, 0, 700, 98
39474, V, 1, 1, 1, 1, 0, 700, 98
39475, V, 1, 1, 1, 1, 0, 700, 98
39476, V, 1, 1, 1, 1, 0, 700, 98
39477, V, 1, 1, 1, 1, 0, 700, 98
39478, V, 1, 1, 1, 1, 0, 700, 98
39479, V, 1, 1, 1, 1, 0, 700, 98
39480, V, 1, 1, 1, 1, 0, 700, 98
39481, V, 1, 1, 1, 1, 0, 700, 98
39482, V, 1, 1, 1, 1, 0, 700, 98
39483, V, 1, 1, 1, 1, 0, 700, 98
39484, V, 1, 1, 1, 1, 0, 700, 98
39485, V, 1, 1, 1, 1, 0, 700, 98
39486, V, 1, 1, 1, 1, 0, 700, 98
39487, V, 1, 1, 1, 1, 0, 700, 98
39488, V, 1, 1, 1, 1, 0, 700, 98
39489, V, 1, 1, 1, 1, 0, 700, 98
39490, V, 1, 1, 1, 1, 0, 700, 98
39491, V, 1, 1, 1, 1, 0, 700, 98
39492, V, 1, 1, 1, 1, 0, 700, 98
39493, V, 1, 1, 1, 1, 0, 700, 98
39494, V, 1, 1, 1, 1, 0, 700, 98
39495, V, 1, 1, 1, 1, 0, 700, 98
39496, V, 1, 1, 1, 1, 0, 700, 98
39497, V, 1, 1, 1, 1, 0, 700, 98
39498, V, 1, 1, 1, 1, 0, 700, 98
39499, V, 1, 1, 1, 1, 0, 700, 98
39500, V, 1, 1, 1, 1, 0, 700, 98
39501, V, 1, 1, 1, 1, 0, 700, 98
39502, V, 1, 1, 1, 1, 0, 700, 98
39503, V, 1, 1, 1, 1, 0, 700, 98
39504, V, 1, 1, 1, 1, 0, 700, 98
39505, V, 1, 1, 1, 1, 0, 700, 98
39506, V, 1, 1, 1, 1, 0, 700, 98
39507, V, 1, 1, 1, 1, 0, 700, 98
39508, V, 1, 1, 1, 1, 0, 700, 98
39510, V, 1, 1, 1, 1, 0, 700, 98
39511, V, 1, 1, 1, 1, 0, 700, 98
39512, V, 1, 1, 1, 1, 0, 700, 98
39513, V, 1, 1, 1, 1, 0, 700, 98
39514, V, 1, 1, 1, 1, 0, 700, 98
39515, V, 1, 1, 1, 1, 0, 700, 98
39516, V, 1, 1, 1, 1, 0, 700, 98
39517, V, 1, 1, 1, 1, 0, 700, 98
39518, V, 1, 1, 1, 1, 0, 700, 98
39519, V, 1, 1, 1, 1, 0, 700, 98
39520, V, 1, 1, 1, 1, 0, 700, 98
39521, V, 1, 1, 1, 1, 0, 700, 98
39522, V, 1, 1, 1, 1, 0, 700, 98
39523, V, 1, 1, 1, 1, 0, 700, 98
39524, V, 1, 1, 1, 1, 0, 700, 98
39525, V, 1, 1, 1, 1, 0, 700, 98
39526, V, 1, 1, 1, 1, 0, 700, 98
39527, V, 1, 1, 1, 1, 0, 700, 98
39528, V, 1, 1, 1, 1, 0, 700, 98
39529, V, 1, 1, 1, 1, 0, 700, 98
39530, V, 1, 1, 1, 1, 0, 700, 98
39531, V, 1, 1, 1, 1, 0, 700, 98
39532, V, 1, 1, 1, 1, 0, 700, 98
39533, V, 1, 1, 1, 1, 0, 700, 98
39534, V, 1, 1, 1, 1, 0, 700, 98
39535, V, 1, 1, 1, 1, 0, 700, 98
39536, V, 1, 1, 1, 1, 0, 700, 98
39537, V, 1, 1, 1, 1, 0, 700, 98
39538, V, 1, 1, 1, 1, 0, 700, 98
39539, V, 1, 1, 1, 1, 0, 700, 98
39540, V, 1, 1, 1, 1, 0, 700, 98
39541, V, 1, 1, 1, 1, 0, 700, 98
39542, V, 1, 1, 1, 1, 0, 700, 98
39543, V, 1, 1, 1, 1, 0, 700, 98
39544, V, 1, 1, 1, 1, 0, 700, 98
39545, V, 1, 1, 1, 1, 0, 700, 98
39546, V, 1, 1, 1, 1, 0, 700, 98
39547, V, 1, 1, 1, 1, 0, 700, 98
39548, V, 1, 1, 1, 1, 0, 700, 98
39549, V, 1, 1, 1, 1, 0, 700, 98
39550, V, 1, 1, 1, 1, 0, 700, 98
39552, V, 1, 1, 1, 1, 0, 700, 98
39553, V, 1, 1, 1, 1, 0, 700, 98
39554, V, 1, 1, 1, 1, 0, 700, 98
39555, V, 1, 1, 1, 1, 0, 700, 98
39556, V, 1, 1, 1, 1, 0, 700, 98
39557, V, 1, 1, 1, 1, 0, 700, 98
39558, V, 1, 1, 1, 1, 0, 700, 98
39559, V, 1, 1, 1, 1, 0, 700, 98
39560, V, 1, 1, 1, 1, 0, 700, 98
39561, V, 1, 1, 1, 1, 0, 700, 98
39562, V, 1, 1, 1, 1, 0, 700, 98
39563, V, 1, 1, 1, 1, 0, 700, 98
39564, V, 1, 1, 1, 1, 0, 700, 98
39565, V, 1, 1, 1, 1, 0, 700, 98
39566, V, 1, 1, 1, 1, 0, 700, 98
39567, V, 1, 1, 1, 1, 0, 700, 98
39568, V, 1, 1, 1, 1, 0, 700, 98
39569, V, 1, 1, 1, 1, 0, 700, 98
39570, V, 1, 1, 1, 1, 0, 700, 98
39571, V, 1, 1, 1, 1, 0, 700, 98
39572, V, 1, 1, 1, 1, 0, 700, 98
39573, V, 1, 1, 1, 1, 0, 700, 98
39574, V, 1, 1, 1, 1, 0, 700, 98
39575, V, 1, 1, 1, 1, 0, 700, 98
39576, V, 1, 1, 1, 1, 0, 700, 98
39577, V, 1, 1, 1, 1, 0, 700, 98
39578, V, 1, 1, 1, 1, 0, 700, 98
39579, V, 1, 1, 1, 1, 0, 700, 98
39580, V, 1, 1, 1, 1, 0, 700, 98
39581, V, 1, 1, 1, 1, 0, 700, 98
39582, V, 1, 1, 1, 1, 0, 700, 98
39583, V, 1, 1, 1, 1, 0, 700, 98
39584, V, 1, 1, 1, 1, 0, 700, 98
39585, V, 1, 1, 1, 1, 0, 700, 98
39586, V, 1, 1, 1, 1, 0, 700, 98
39587, V, 1, 1, 1, 1, 0, 700, 98
39588, V, 1, 1, 1, 1, 0, 700, 98
39589, V, 1, 1, 1, 1, 0, 700, 98
39590, V, 1, 1, 1, 1, 0, 700, 98
39591, V, 1, 1, 1, 1, 0, 700, 98
39592, V, 1, 1, 1, 1, 0, 700, 98
39593, V, 1, 1, 1, 1, 0, 700, 98
39595, V, 1, 1, 1, 1, 0, 700, 98
39596, V, 1, 1, 1, 1, 0, 700, 98
39597, V, 1, 1, 1, 1, 0, 700, 98
39598, V, 1, 1, 1, 1, 0, 700, 98
39599, V, 1, 1, 1, 1, 0, 700, 98
39600, V, 1, 1, 1, 1, 0, 700, 98
39601, V, 1, 1, 1, 1, 0, 700, 98
39602, V, 1, 1, 1, 1, 0, 700, 98
39603, V, 1, 1, 1, 1, 0, 700, 98
39604, V, 1, 1, 1, 1, 0, 700, 98
39605, V, 1, 1, 1, 1, 0, 700, 98
39606, V, 1, 1, 1, 1, 0, 700, 98
39607, V, 1, 1, 1, 1, 0, 700, 98
39608, V, 1, 1, 1, 1, 0, 700, 98
39609, V, 1, 1, 1, 1, 0, 700, 98
39610, V, 1, 1, 1, 1, 0, 700, 98
39611, V, 1, 1, 1, 1, 0, 700, 98
39612, V, 1, 1, 1, 1, 0, 700, 98
39613, V, 1, 1, 1, 1, 0, 700, 98
39614, V, 1, 1, 1, 1, 0, 700, 98
39615, V, 1, 1, 1, 1, 0, 700, 98
39616, V, 1, 1, 1, 1, 0, 700, 98
39617, V, 1, 1, 1, 1, 0, 700, 98
39618, V, 1, 1, 1, 1, 0, 700, 98
39619, V, 1, 1, 1, 1, 0, 700, 98
39620, V, 1, 1, 1, 1, 0, 700, 98
39621, V, 1, 1, 1, 1, 0, 700, 98
39622, V, 1, 1, 1, 1, 0, 700, 98
39623, V, 1, 1, 1, 1, 0, 700, 98
39624, V, 1, 1, 1, 1, 0, 700, 98
39625, V, 1, 1, 1, 1, 0, 700, 98
39626, V, 1, 1, 1, 1, 0, 700, 98
39627, V, 1, 1, 1, 1, 0, 700, 98
39628, V, 1, 1, 1, 1, 0, 700, 98
39629, V, 1, 1, 1, 1, 0, 700, 98
39630, V, 1, 1, 1, 1, 0, 700, 98
39631, V, 1, 1, 1, 1, 0, 700, 98
39632, V, 1, 1, 1, 1, 0, 700, 98
39633, V, 1, 1, 1, 1, 0, 700, 98
39634, V, 1, 1, 1, 1, 0, 700, 98
39635, V, 1, 1, 1, 1, 0, 700, 98
39636, V, 1, 1, 1, 1, 0, 700, 98
39638, V, 1, 1, 1, 1, 0, 700, 98
39639, V, 1, 1, 1, 1, 0, 700, 98
39640, V, 1, 1, 1, 1, 0, 700, 98
39641, V, 1, 1, 1, 1, 0, 700, 98
39642, V, 1, 1, 1, 1, 0, 700, 98
39643, V, 1, 1, 1, 1, 0, 700, 98
39644, V, 1, 1, 1, 1, 0, 700, 98
39645, V, 1, 1, 1, 1, 0, 700, 98
39646, V, 1, 1, 1, 1, 0, 700, 98
39647, V, 1, 1, 1, 1, 0, 700, 98
39648, V, 1, 1, 1, 1, 0, 700, 98
39649, V, 1, 1, 1, 1, 0, 700, 98
39650, V, 1, 1, 1, 1, 0, 700, 98
39651, V, 1, 1, 1, 1, 0, 700, 98
39652, V, 1, 1, 1, 1, 0, 700, 98
39653, V, 1, 1, 1, 1, 0, 700, 98
39654, V, 1, 1, 1, 1, 0, 700, 98
39655, V, 1, 1, 1, 1, 0, 700, 98
39656, V, 1, 1, 1, 1, 0, 700, 98
39657, V, 1, 1, 1, 1, 0, 700, 98
39658, V, 1, 1, 1, 1, 0, 700, 98
39659, V, 1, 1, 1, 1, 0, 700, 98
39660, V, 1, 1, 1, 1, 0, 700, 98
39661, V, 1, 1, 1, 1, 0, 700, 98
39662, V, 1, 1, 1, 1, 0, 700, 98
39663, V, 1, 1, 1, 1, 0, 700, 98
39664, V, 1, 1, 1, 1, 0, 700, 98
39665, V, 1, 1, 1, 1, 0, 700, 98
39666, V, 1, 1, 1, 1, 0, 700, 98
39667, V, 1, 1, 1, 1, 0, 700, 98
39668, V, 1, 1, 1, 1, 0, 700, 98
39669, V, 1, 1, 1, 1, 0, 700, 98
39670, V, 1, 1, 1, 1, 0, 700, 98
39671, V, 1, 1, 1, 1, 0, 700, 98
39672, V, 1, 1, 1, 1, 0, 700, 98
39673, V, 1, 1, 1, 1, 0, 700, 98
39674, V, 1, 1, 1, 1, 0, 700, 98
39675, V, 1, 1, 1, 1, 0, 700, 98
39676, V, 1, 1, 1, 1, 0, 700, 98
39677, V, 1, 1, 1, 1, 0, 700, 98
39678, V, 1, 1, 1, 1, 0, 700, 98
39680, V, 1, 1, 1, 1, 0, 700, 98
39681, V, 1, 1, 1, 1, 0, 700, 98
39682, V, 1, 1, 1, 1, 0, 700, 98
39683, V, 1, 1, 1, 1, 0, 700, 98
39684, V, 1, 1, 1, 1, 0, 700, 98
39685, V, 1, 1, 1, 1, 0, 700, 98
39686, V, 1, 1, 1, 1, 0, 700, 98
39687, V, 1, 1, 1, 1, 0, 700, 98
39688, V, 1, 1, 1, 1, 0, 700, 98
39689, V, 1, 1, 1, 1, 0, 700, 98
39690, V, 1, 1, 1, 1, 0, 700, 98
39691, V, 1, 1, 1, 1, 0, 700, 98
39692, V, 1, 1, 1, 1, 0, 700, 98
39693, V, 1, 1, 1, 1, 0, 700, 98
39694, V, 1, 1, 1, 1, 0, 700, 98
39695, V, 1, 1, 1, 1, 0, 700, 98
39696, V, 1, 1, 1, 1, 0, 700, 98
39697, V, 1, 1, 1, 1, 0, 700, 98
39698, V, 1, 1, 1, 1, 0, 700, 98
39699, V, 1, 1, 1, 1, 0, 700, 98
39700, V, 1, 1, 1, 1, 0, 700, 98
39701, V, 1, 1, 1, 1, 0, 700, 98
39702, V, 1, 1, 1, 1, 0, 700, 98
39703, V, 1, 1, 1, 1, 0, 700, 98
39704, V, 1, 1, 1, 1, 0, 700, 98
39705, V, 1, 1, 1, 1, 0, 700, 98
39706, V, 1, 1, 1, 1, 0, 700, 98
39707, V, 1, 1, 1, 1, 0, 700, 98
39708, V, 1, 1, 1, 1, 0, 700, 98
39709, V, 1, 1, 1, 1, 0, 700, 98
39710, V, 1, 1, 1, 1, 0, 700, 98
39711, V, 1, 1, 1, 1, 0, 700, 98
39712, V, 1, 1, 1, 1, 0, 700, 98
39713, V, 1, 1, 1, 1, 0, 700, 98
39714, V, 1, 1, 1, 1, 0, 700, 98
39715, V, 1, 1, 1, 1, 0, 700, 98
39716, V, 1, 1, 1, 1, 0, 700, 98
39717, V, 1, 1, 1, 1, 0, 700, 98
39718, V, 1, 1, 1, 1, 0, 700, 98
39719, V, 1, 1, 1, 1, 0, 700, 98
39720, V, 1, 1, 1, 1, 0, 700, 98
39721, V, 1, 1, 1, 1, 0, 700, 98
39723, V, 1, 1, 1, 1, 0, 700, 98
39724, V, 1, 1, 1, 1, 0, 700, 98
39725, V, 1, 1, 1, 1, 0, 700, 98
39726, V, 1, 1, 1, 1, 0, 700, 98
39727, V, 1, 1, 1, 1, 0, 700, 98
39728, V, 1, 1, 1, 1, 0, 700, 98
39729, V, 1, 1, 1, 1, 0, 700, 98
39730, V, 1, 1, 1, 1, 0, 700, 98
39731, V, 1, 1, 1, 1, 0, 700, 98
39732, V, 1, 1, 1, 1, 0, 700, 98
39733, V, 1, 1, 1, 1, 0, 700, 98
39734, V, 1, 1, 1, 1, 0, 700, 98
39735, V, 1, 1, 1, 1, 0, 700, 98
39736, V, 1, 1, 1, 1, 0, 700, 98
39737, V, 1, 1, 1, 1, 0, 700, 98
39738, V, 1, 1, 1, 1, 0, 700, 98
39739, V, 1, 1, 1, 1, 0, 700, 98
39740, V, 1, 1, 1, 1, 0, 700, 98
39741, V, 1, 1, 1, 1, 0, 700, 98
39742, V, 1, 1, 1, 1, 0, 700, 98
39743, V, 1, 1, 1, 1, 0, 700, 98
39744, V, 1, 1, 1, 1, 0, 700, 98
39745, V, 1, 1, 1, 1, 0, 700, 98
39746, V, 1, 1, 1, 1, 0, 700, 98
39747, V, 1, 1, 1, 1, 0, 700, 98
39748, V, 1, 1, 1, 1, 0, 700, 98
39749, V, 1, 1, 1, 1, 0, 700, 98
39750, V, 1, 1, 1, 1, 0, 700, 98
39751, V, 1, 1, 1, 1, 0, 700, 98
39752, V, 1, 1, 1, 1, 0, 700, 98
39753, V, 1, 1, 1, 1, 0, 700, 98
39754, V, 1, 1, 1, 1, 0, 700, 98
39755, V, 1, 1, 1, 1, 0, 700, 98
39756, V, 1, 1, 1, 1, 0, 700, 98
39757, V, 1, 1, 1, 1, 0, 700, 98
39758, V, 1, 1, 1, 1, 0, 700, 98
39759, V, 1, 1, 1, 1, 0, 700, 98
39760, V, 1, 1, 1, 1, 0, 700, 98
39761, V, 1, 1, 1, 1, 0, 700, 98
39762, V, 1, 1, 1, 1, 0, 700, 98
39763, V, 1, 1, 1, 1, 0, 700, 98
39764, V, 1, 1, 1, 1, 0, 700, 98
39766, V, 1, 1, 1, 1, 0, 700, 98
39767, V, 1, 1, 1, 1, 0, 700, 98
39768, V, 1, 1, 1, 1, 0, 700, 98
39769, V, 1, 1, 1, 1, 0, 700, 98
39770, V, 1, 1, 1, 1, 0, 700, 98
39771, V, 1, 1, 1, 1, 0, 700, 98
39772, V, 1, 1, 1, 1, 0, 700, 98
39773, V, 1, 1, 1, 1, 0, 700, 98
39774, V, 1, 1, 1, 1, 0, 700, 98
39775, V, 1, 1, 1, 1, 0, 700, 98
39776, V, 1, 1, 1, 1, 0, 700, 98
39777, V, 1, 1, 1, 1, 0, 700, 98
39778, V, 1, 1, 1, 1, 0, 700, 98
39779, V, 1, 1, 1, 1, 0, 700, 98
39780, V, 1, 1, 1, 1, 0, 700, 98
39781, V, 1, 1, 1, 1, 0, 700, 98
39782, V, 1, 1, 1, 1, 0, 700, 98
39783, V, 1, 1, 1, 1, 0, 700, 98
39784, V, 1, 1, 1, 1, 0, 700, 98
39785, V, 1, 1, 1, 1, 0, 700, 98
39786, V, 1, 1, 1, 1, 0, 700, 98
39787, V, 1, 1, 1, 1, 0, 700, 98
39788, V, 1, 1, 1, 1, 0, 700, 98
39789, V, 1, 1, 1, 1, 0, 700, 98
39790, V, 1, 1, 1, 1, 0, 700, 98
39791, V, 1, 1, 1, 1, 0, 700, 98
39792, V, 1, 1, 1, 1, 0, 700, 98
39793, V, 1, 1, 1, 1, 0, 700, 98
39794, V, 1, 1, 1, 1, 0, 700, 98
39795, V, 1, 1, 1, 1, 0, 700, 98
39796, V, 1, 1, 1, 1, 0, 700, 98
39797, V, 1, 1, 1, 1, 0, 700, 98
39798, V, 1, 1, 1, 1, 0, 700, 98
39799, V, 1, 1, 1, 1, 0, 700, 98
39800, V, 1, 1, 1, 1, 0, 700, 98
39801, V, 1, 1, 1, 1, 0, 700, 98
39802, V, 1, 1, 1, 1, 0, 700, 98
39803, V, 1, 1, 1, 1, 0, 700, 98
39804, V, 1, 1, 1, 1, 0, 700, 98
39805, V, 1, 1, 1, 1, 0, 700, 98
39806, V, 1, 1, 1, 1, 0, 700, 98
39808, V, 1, 1, 1, 1, 0, 700, 98
39809, V, 1, 1, 1, 1, 0, 700, 98
39810, V, 1, 1, 1, 1, 0, 700, 98
39811, V, 1, 1, 1, 1, 0, 700, 98
39812, V, 1, 1, 1, 1, 0, 700, 98
39813, V, 1, 1, 1, 1, 0, 700, 98
39814, V, 1, 1, 1, 1, 0, 700, 98
39815, V, 1, 1, 1, 1, 0, 700, 98
39816, V, 1, 1, 1, 1, 0, 700, 98
39817, V, 1, 1, 1, 1, 0, 700, 98
39818, V, 1, 1, 1, 1, 0, 700, 98
39819, V, 1, 1, 1, 1, 0, 700, 98
39820, V, 1, 1, 1, 1, 0, 700, 98
39821, V, 1, 1, 1, 1, 0, 700, 98
39822, V, 1, 1, 1, 1, 0, 700, 98
39823, V, 1, 1, 1, 1, 0, 700, 98
39824, V, 1, 1, 1, 1, 0, 700, 98
39825, V, 1, 1, 1, 1, 0, 700, 98
39826, V, 1, 1, 1, 1, 0, 700, 98
39827, V, 1, 1, 1, 1, 0, 700, 98
39828, V, 1, 1, 1, 1, 0, 700, 98
39829, V, 1, 1, 1, 1, 0, 700, 98
39830, V, 1, 1, 1, 1, 0, 700, 98
39831, V, 1, 1, 1, 1, 0, 700, 98
39832, V, 1, 1, 1, 1, 0, 700, 98
39833, V, 1, 1, 1, 1, 0, 700, 98
39834, V, 1, 1, 1, 1, 0, 700, 98
39835, V, 1, 1, 1, 1, 0, 700, 98
39836, V, 1, 1, 1, 1, 0, 700, 98
39837, V, 1, 1, 1, 1, 0, 700, 98
39838, V, 1, 1, 1, 1, 0, 700, 98
39839, V, 1, 1, 1, 1, 0, 700, 98
39840, V, 1, 1, 1, 1, 0, 700, 98
39841, V, 1, 1, 1, 1, 0, 700, 98
39842, V, 1, 1, 1, 1, 0, 700, 98
39843, V, 1, 1, 1, 1, 0, 700, 98
39844, V, 1, 1, 1, 1, 0, 700, 98
39845, V, 1, 1, 1, 1, 0, 700, 98
39846, V, 1, 1, 1, 1, 0, 700, 98
39847, V, 1, 1, 1, 1, 0, 700, 98
39848, V, 1, 1, 1, 1, 0, 700, 98
39849, V, 1, 1, 1, 1, 0, 700, 98
39851, V, 1, 1, 1, 1, 0, 700, 98
39852, V, 1, 1, 1, 1, 0, 700, 98
39853, V, 1, 1, 1, 1, 0, 700, 98
39854, V, 1, 1, 1, 1, 0, 700, 98
39855, V, 1, 1, 1, 1, 0, 700, 98
39856, V, 1, 1, 1, 1, 0, 700, 98
39857, V, 1, 1, 1, 1, 0, 700, 98
39858, V, 1, 1, 1, 1, 0, 700, 98
39859, V, 1, 1, 1, 1, 0, 700, 98
39860, V, 1, 1, 1, 1, 0, 700, 98
39861, V, 1, 1, 1, 1, 0, 700, 98
39862, V, 1, 1, 1, 1, 0, 700, 98
39863, V, 1, 1, 1, 1, 0, 700, 98
39864, V, 1, 1, 1, 1, 0, 700, 98
39865, V, 1, 1, 1, 1, 0, 700, 98
39866, V, 1, 1, 1, 1, 0, 700, 98
39867, V, 1, 1, 1, 1, 0, 700, 98
39868, V, 1, 1, 1, 1, 0, 700, 98
39869, V, 1, 1, 1, 1, 0, 700, 98
39870, V, 1, 1, 1, 1, 0, 700, 98
39871, V, 1, 1, 1, 1, 0, 700, 98
39872, V, 1, 1, 1, 1, 0, 700, 98
39873, V, 1, 1, 1, 1, 0, 700, 98
39874, V, 1, 1, 1, 1, 0, 700, 98
39875, V, 1, 1, 1, 1, 0, 700, 98
39876, V, 1, 1, 1, 1, 0, 700, 98
39877, V, 1, 1, 1, 1, 0, 700, 98
39878, V, 1, 1, 1, 1, 0, 700, 98
39879, V, 1, 1, 1, 1, 0, 700, 98
39880, V, 1, 1, 1, 1, 0, 700, 98
39881, V, 1, 1, 1, 1, 0, 700, 98
39882, V, 1, 1, 1, 1, 0, 700, 98
39883, V, 1, 1, 1, 1, 0, 700, 98
39884, V, 1, 1, 1, 1, 0, 700, 98
39885, V, 1, 1, 1, 1, 0, 700, 98
39886, V, 1, 1, 1, 1, 0, 700, 98
39887, V, 1, 1, 1, 1, 0, 700, 98
39888, V, 1, 1, 1, 1, 0, 700, 98
39889, V, 1, 1, 1, 1, 0, 700, 98
39890, V, 1, 1, 1, 1, 0, 700, 98
39891, V, 1, 1, 1, 1, 0, 700, 98
39892, V, 1, 1, 1, 1, 0, 700, 98
39894, V, 1, 1, 1, 1, 0, 700, 98
39895, V, 1, 1, 1, 1, 0, 700, 98
39896, V, 1, 1, 1, 1, 0, 700, 98
39897, V, 1, 1, 1, 1, 0, 700, 98
39898, V, 1, 1, 1, 1, 0, 700, 98
39899, V, 1, 1, 1, 1, 0, 700, 98
39900, V, 1, 1, 1, 1, 0, 700, 98
39901, V, 1, 1, 1, 1, 0, 700, 98
39902, V, 1, 1, 1, 1, 0, 700, 98
39903, V, 1, 1, 1, 1, 0, 700, 98
39904, V, 1, 1, 1, 1, 0, 700, 98
39905, V, 1, 1, 1, 1, 0, 700, 98
39906, V, 1, 1, 1, 1, 0, 700, 98
39907, V, 1, 1, 1, 1, 0, 700, 98
39908, V, 1, 1, 1, 1, 0, 700, 98
39909, V, 1, 1, 1, 1, 0, 700, 98
39910, V, 1, 1, 1, 1, 0, 700, 98
39911, V, 1, 1, 1, 1, 0, 700, 98
39912, V, 1, 1, 1, 1, 0, 700, 98
39913, V, 1, 1, 1, 1, 0, 700, 98
39914, V, 1, 1, 1, 1, 0, 700, 98
39915, V, 1, 1, 1, 1, 0, 700, 98
39916, V, 1, 1, 1, 1, 0, 700, 98
39917, V, 1, 1, 1, 1, 0, 700, 98
39918, V, 1, 1, 1, 1, 0, 700, 98
39919, V, 1, 1, 1, 1, 0, 700, 98
39920, V, 1, 1, 1, 1, 0, 700, 98
39921, V, 1, 1, 1, 1, 0, 700, 98
39922, V, 1, 1, 1, 1, 0, 700, 98
39923, V, 1, 1, 1, 1, 0, 700, 98
39924, V, 1, 1, 1, 1, 0, 700, 98
39925, V, 1, 1, 1, 1, 0, 700, 98
39926, V, 1, 1, 1, 1, 0, 700, 98
39927, V, 1, 1, 1, 1, 0, 700, 98
39928, V, 1, 1, 1, 1, 0, 700, 98
39929, V, 1, 1, 1, 1, 0, 700, 98
39930, V, 1, 1, 1, 1, 0, 700, 98
39931, V, 1, 1, 1, 1, 0, 700, 98
39932, V, 1, 1, 1, 1, 0, 700, 98
39933, V, 1, 1, 1, 1, 0, 700, 98
39934, V, 1, 1, 1, 1, 0, 700, 98
39936, V, 1, 1, 1, 1, 0, 700, 98
39937, V, 1, 1, 1, 1, 0, 700, 98
39938, V, 1, 1, 1, 1, 0, 700, 98
39939, V, 1, 1, 1, 1, 0, 700, 98
39940, V, 1, 1, 1, 1, 0, 700, 98
39941, V, 1, 1, 1, 1, 0, 700, 98
39942, V, 1, 1, 1, 1, 0, 700, 98
39943, V, 1, 1, 1, 1, 0, 700, 98
39944, V, 1, 1, 1, 1, 0, 700, 98
39945, V, 1, 1, 1, 1, 0, 700, 98
39946, V, 1, 1, 1, 1, 0, 700, 98
39947, V, 1, 1, 1, 1, 0, 700, 98
39948, V, 1, 1, 1, 1, 0, 700, 98
39949, V, 1, 1, 1, 1, 0, 700, 98
39950, V, 1, 1, 1, 1, 0, 700, 98
39951, V, 1, 1, 1, 1, 0, 700, 98
39952, V, 1, 1, 1, 1, 0, 700, 98
39953, V, 1, 1, 1, 1, 0, 700, 98
39954, V, 1, 1, 1, 1, 0, 700, 98
39955, V, 1, 1, 1, 1, 0, 700, 98
39956, V, 1, 1, 1, 1, 0, 700, 98
39957, V, 1, 1, 1, 1, 0, 700, 98
39958, V, 1, 1, 1, 1, 0, 700, 98
39959, V, 1, 1, 1, 1, 0, 700, 98
39960, V, 1, 1, 1, 1, 0, 700, 98
39961, V, 1, 1, 1, 1, 0, 700, 98
39962, V, 1, 1, 1, 1, 0, 700, 98
39963, V, 1, 1, 1, 1, 0, 700, 98
39964, V, 1, 1, 1, 1, 0, 700, 98
39965, V, 1, 1, 1, 1, 0, 700, 98
39966, V, 1, 1, 1, 1, 0, 700, 98
39967, V, 1, 1, 1, 1, 0, 700, 98
39968, V, 1, 1, 1, 1, 0, 700, 98
39969, V, 1, 1, 1, 1, 0, 700, 98
39970, V, 1, 1, 1, 1, 0, 700, 98
39971, V, 1, 1, 1, 1, 0, 700, 98
39972, V, 1, 1, 1, 1, 0, 700, 98
39973, V, 1, 1, 1, 1, 0, 700, 98
39974, V, 1, 1, 1, 1, 0, 700, 98
39975, V, 1, 1, 1, 1, 0, 700, 98
39976, V, 1, 1, 1, 1, 0, 700, 98
39977, V, 1, 1, 1, 1, 0, 700, 98
39979, V, 1, 1, 1, 1, 0, 700, 98
39980, V, 1, 1, 1, 1, 0, 700, 98
39981, V, 1, 1, 1, 1, 0, 700, 98
39982, V, 1, 1, 1, 1, 0, 700, 98
39983, V, 1, 1, 1, 1, 0, 700, 98
39984, V, 1, 1, 1, 1, 0, 700, 98
39985, V, 1, 1, 1, 1, 0, 700, 98
39986, V, 1, 1, 1, 1, 0, 700, 98
39987, V, 1, 1, 1, 1, 0, 700, 98
39988, V, 1, 1, 1, 1, 0, 700, 98
39989, V, 1, 1, 1, 1, 0, 700, 98
39990, V, 1, 1, 1, 1, 0, 700, 98
39991, V, 1, 1, 1, 1, 0, 700, 98
39992, V, 1, 1, 1, 1, 0, 700, 98
39993, V, 1, 1, 1, 1, 0, 700, 98
39994, V, 1, 1, 1, 1, 0, 700, 98
39995, V, 1, 1, 1, 1, 0, 700, 98
39996, V, 1, 1, 1, 1, 0, 700, 98
39997, V, 1, 1, 1, 1, 0, 700, 98
39998, V, 1, 1, 1, 1, 0, 700, 98
39999, V, 1, 1, 1, 1, 0, 700, 98
40000, V, 1, 1, 1, 1, 0, 700, 98
40001, V, 1, 1, 1, 1, 0, 700, 98
40002, V, 1, 1, 1, 1, 0, 700, 98
40003, V, 1, 1, 1, 1, 0, 700, 98
40004, V, 1, 1, 1, 1, 0, 700, 98
40005, V, 1, 1, 1, 1, 0, 700, 98
40006, V, 1, 1, 1, 1, 0, 700, 98
40007, V, 1, 1, 1, 1, 0, 700, 98
40008, V, 1, 1, 1, 1, 0, 700, 98
40009, V, 1, 1, 1, 1, 0, 700, 98
40010, V, 1, 1, 1, 1, 0, 700, 98
40011, V, 1, 1, 1, 1, 0, 700, 98
40012, V, 1, 1, 1, 1, 0, 700, 98
40013, V, 1, 1, 1, 1, 0, 700, 98
40014, V, 1, 1, 1, 1, 0, 700, 98
40015, V, 1, 1, 1, 1, 0, 700, 98
40016, V, 1, 1, 1, 1, 0, 700, 98
40017, V, 1, 1, 1, 1, 0, 700, 98
40018, V, 1, 1, 1, 1, 0, 700, 98
40019, V, 1, 1, 1, 1, 0, 700, 98
40020, V, 1, 1, 1, 1, 0, 700, 98
40022, V, 1, 1, 1, 1, 0, 700, 98
40023, V, 1, 1, 1, 1, 0, 700, 98
40024, V, 1, 1, 1, 1, 0, 700, 98
40025, V, 1, 1, 1, 1, 0, 700, 98
40026, V, 1, 1, 1, 1, 0, 700, 98
40027, V, 1, 1, 1, 1, 0, 700, 98
40028, V, 1, 1, 1, 1, 0, 700, 98
40029, V, 1, 1, 1, 1, 0, 700, 98
40030, V, 1, 1, 1, 1, 0, 700, 98
40031, V, 1, 1, 1, 1, 0, 700, 98
40032, V, 1, 1, 1, 1, 0, 700, 98
40033, V, 1, 1, 1, 1, 0, 700, 98
40034, V, 1, 1, 1, 1, 0, 700, 98
40035, V, 1, 1, 1, 1, 0, 700, 98
40036, V, 1, 1, 1, 1, 0, 700, 98
40037, V, 1, 1, 1, 1, 0, 700, 98
40038, V, 1, 1, 1, 1, 0, 700, 98
40039, V, 1, 1, 1, 1, 0, 700, 98
40040, V, 1, 1, 1, 1, 0, 700, 98
40041, V, 1, 1, 1, 1, 0, 700, 98
40042, V, 1, 1, 1, 1, 0, 700, 98
40043, V, 1, 1, 1, 1, 0, 700, 98
40044, V, 1, 1, 1, 1, 0, 700, 98
40045, V, 1, 1, 1, 1, 0, 700, 98
40046, V, 1, 1, 1, 1, 0, 700, 98
40047, V, 1, 1, 1, 1, 0, 700, 98
40048, V, 1, 1, 1, 1, 0, 700, 98
40049, V, 1, 1, 1, 1, 0, 700, 98
40050, V, 1, 1, 1, 1, 0, 700, 98
40051, V, 1, 1, 1, 1, 0, 700, 98
40052, V, 1, 1, 1, 1, 0, 700, 98
40053, V, 1, 1, 1, 1, 0, 700, 98
40054, V, 1, 1, 1, 1, 0, 700, 98
40055, V, 1, 1, 1, 1, 0, 700, 98
40056, V, 1, 1, 1, 1, 0, 700, 98
40057, V, 1, 1, 1, 1, 0, 700, 98
40058, V, 1, 1, 1, 1, 0, 700, 98
40059, V, 1, 1, 1, 1, 0, 700, 98
40060, V, 1, 1, 1, 1, 0, 700, 98
40061, V, 1, 1, 1, 1, 0, 700, 98
40062, V, 1, 1, 1, 1, 0, 700, 98
40064, V, 1, 1, 1, 1, 0, 700, 98
40065, V, 1, 1, 1, 1, 0, 700, 98
40066, V, 1, 1, 1, 1, 0, 700, 98
40067, V, 1, 1, 1, 1, 0, 700, 98
40068, V, 1, 1, 1, 1, 0, 700, 98
40069, V, 1, 1, 1, 1, 0, 700, 98
40070, V, 1, 1, 1, 1, 0, 700, 98
40071, V, 1, 1, 1, 1, 0, 700, 98
40072, V, 1, 1, 1, 1, 0, 700, 98
40073, V, 1, 1, 1, 1, 0, 700, 98
40074, V, 1, 1, 1, 1, 0, 700, 98
40075, V, 1, 1, 1, 1, 0, 700, 98
40076, V, 1, 1, 1, 1, 0, 700, 98
40077, V, 1, 1, 1, 1, 0, 700, 98
40078, V, 1, 1, 1, 1, 0, 700, 98
40079, V, 1, 1, 1, 1, 0, 700, 98
40080, V, 1, 1, 1, 1, 0, 700, 98
40081, V, 1, 1, 1, 1, 0, 700, 98
40082, V, 1, 1, 1, 1, 0, 700, 98
40083, V, 1, 1, 1, 1, 0, 700, 98
40084, V, 1, 1, 1, 1, 0, 700, 98
40085, V, 1, 1, 1, 1, 0, 700, 98
40086, V, 1, 1, 1, 1, 0, 700, 98
40087, V, 1, 1, 1, 1, 0, 700, 98
40088, V, 1, 1, 1, 1, 0, 700, 98
40089, V, 1, 1, 1, 1, 0, 700, 98
40090, V, 1, 1, 1, 1, 0, 700, 98
40091, V, 1, 1, 1, 1, 0, 700, 98
40092, V, 1, 1, 1, 1, 0, 700, 98
40093, V, 1, 1, 1, 1, 0, 700, 98
40094, V, 1, 1, 1, 1, 0, 700, 98
40095, V, 1, 1, 1, 1, 0, 700, 98
40096, V, 1, 1, 1, 1, 0, 700, 98
40097, V, 1, 1, 1, 1, 0, 700, 98
40098, V, 1, 1, 1, 1, 0, 700, 98
40099, V, 1, 1, 1, 1, 0, 700, 98
40100, V, 1, 1, 1, 1, 0, 700, 98
40101, V, 1, 1, 1, 1, 0, 700, 98
40102, V, 1, 1, 1, 1, 0, 700, 98
40103, V, 1, 1, 1, 1, 0, 700, 98
40104, V, 1, 1, 1, 1, 0, 700, 98
40105, V, 1, 1, 1, 1, 0, 700, 98
40107, V, 1, 1, 1, 1, 0, 700, 98
40108, V, 1, 1, 1, 1, 0, 700, 98
40109, V, 1, 1, 1, 1, 0, 700, 98
40110, V, 1, 1, 1, 1, 0, 700, 98
40111, V, 1, 1, 1, 1, 0, 700, 98
40112, V, 1, 1, 1, 1, 0, 700, 98
40113, V, 1, 1, 1, 1, 0, 700, 98
40114, V, 1, 1, 1, 1, 0, 700, 98
40115, V, 1, 1, 1, 1, 0, 700, 98
40116, V, 1, 1, 1, 1, 0, 700, 98
40117, V, 1, 1, 1, 1, 0, 700, 98
40118, V, 1, 1, 1, 1, 0, 700, 98
40119, V, 1, 1, 1, 1, 0, 700, 98
40120, V, 1, 1, 1, 1, 0, 700, 98
40121, V, 1, 1, 1, 1, 0, 700, 98
40122, V, 1, 1, 1, 1, 0, 700, 98
40123, V, 1, 1, 1, 1, 0, 700, 98
40124, V, 1, 1, 1, 1, 0, 700, 98
40125, V, 1, 1, 1, 1, 0, 700, 98
40126, V, 1, 1, 1, 1, 0, 700, 98
40127, V, 1, 1, 1, 1, 0, 700, 98
40128, V, 1, 1, 1, 1, 0, 700, 98
40129, V, 1, 1, 1, 1, 0, 700, 98
40130, V, 1, 1, 1, 1, 0, 700, 98
40131, V, 1, 1, 1, 1, 0, 700, 98
40132, V, 1, 1, 1, 1, 0, 700, 98
40133, V, 1, 1, 1, 1, 0, 700, 98
40134, V, 1, 1, 1, 1, 0, 700, 98
40135, V, 1, 1, 1, 1, 0, 700, 98
40136, V, 1, 1, 1, 1, 0, 700, 98
40137, V, 1, 1, 1, 1, 0, 700, 98
40138, V, 1, 1, 1, 1, 0, 700, 98
40139, V, 1, 1, 1, 1, 0, 700, 98
40140, V, 1, 1, 1, 1, 0, 700, 98
40141, V, 1, 1, 1, 1, 0, 700, 98
40142, V, 1, 1, 1, 1, 0, 700, 98
40143, V, 1, 1, 1, 1, 0, 700, 98
40144, V, 1, 1, 1, 1, 0, 700, 98
40145, V, 1, 1, 1, 1, 0, 700, 98
40146, V, 1, 1, 1, 1, 0, 700, 98
40147, V, 1, 1, 1, 1, 0, 700, 98
40148, V, 1, 1, 1, 1, 0, 700, 98
40150, V, 1, 1, 1, 1, 0, 700, 98
40151, V, 1, 1, 1, 1, 0, 700, 98
40152, V, 1, 1, 1, 1, 0, 700, 98
40153, V, 1, 1, 1, 1, 0, 700, 98
40154, V, 1, 1, 1, 1, 0, 700, 98
40155, V, 1, 1, 1, 1, 0, 700, 98
40156, V, 1, 1, 1, 1, 0, 700, 98
40157, V, 1, 1, 1, 1, 0, 700, 98
40158, V, 1, 1, 1, 1, 0, 700, 98
40159, V, 1, 1, 1, 1, 0, 700, 98
40160, V, 1, 1, 1, 1, 0, 700, 98
40161, V, 1, 1, 1, 1, 0, 700, 98
40162, V, 1, 1, 1, 1, 0, 700, 98
40163, V, 1, 1, 1, 1, 0, 700, 98
40164, V, 1, 1, 1, 1, 0, 700, 98
40165, V, 1, 1, 1, 1, 0, 700, 98
40166, V, 1, 1, 1, 1, 0, 700, 98
40167, V, 1, 1, 1, 1, 0, 700, 98
40168, V, 1, 1, 1, 1, 0, 700, 98
40169, V, 1, 1, 1, 1, 0, 700, 98
40170, V, 1, 1, 1, 1, 0, 700, 98
40171, V, 1, 1, 1, 1, 0, 700, 98
40172, V, 1, 1, 1, 1, 0, 700, 98
40173, V, 1, 1, 1, 1, 0, 700, 98
40174, V, 1, 1, 1, 1, 0, 700, 98
40175, V, 1, 1, 1, 1, 0, 700, 98
40176, V, 1, 1, 1, 1, 0, 700, 98
40177, V, 1, 1, 1, 1, 0, 700, 98
40178, V, 1, 1, 1, 1, 0, 700, 98
40179, V, 1, 1, 1, 1, 0, 700, 98
40180, V, 1, 1, 1, 1, 0, 700, 98
40181, V, 1, 1, 1, 1, 0, 700, 98
40182, V, 1, 1, 1, 1, 0, 700, 98
40183, V, 1, 1, 1, 1, 0, 700, 98
40184, V, 1, 1, 1, 1, 0, 700, 98
40185, V, 1, 1, 1, 1, 0, 700, 98
40186, V, 1, 1, 1, 1, 0, 700, 98
40187, V, 1, 1, 1, 1, 0, 700, 98
40188, V, 1, 1, 1, 1, 0, 700, 98
40189, V, 1, 1, 1, 1, 0, 700, 98
40190, V, 1, 1, 1, 1, 0, 700, 98
40192, V, 1, 1, 1, 1, 0, 700, 98
40193, V, 1, 1, 1, 1, 0, 700, 98
40194, V, 1, 1, 1, 1, 0, 700, 98
40195, V, 1, 1, 1, 1, 0, 700, 98
40196, V, 1, 1, 1, 1, 0, 700, 98
40197, V, 1, 1, 1, 1, 0, 700, 98
40198, V, 1, 1, 1, 1, 0, 700, 98
40199, V, 1, 1, 1, 1, 0, 700, 98
40200, V, 1, 1, 1, 1, 0, 700, 98
40201, V, 1, 1, 1, 1, 0, 700, 98
40202, V, 1, 1, 1, 1, 0, 700, 98
40203, V, 1, 1, 1, 1, 0, 700, 98
40204, V, 1, 1, 1, 1, 0, 700, 98
40205, V, 1, 1, 1, 1, 0, 700, 98
40206, V, 1, 1, 1, 1, 0, 700, 98
40207, V, 1, 1, 1, 1, 0, 700, 98
40208, V, 1, 1, 1, 1, 0, 700, 98
40209, V, 1, 1, 1, 1, 0, 700, 98
40210, V, 1, 1, 1, 1, 0, 700, 98
40211, V, 1, 1, 1, 1, 0, 700, 98
40212, V, 1, 1, 1, 1, 0, 700, 98
40213, V, 1, 1, 1, 1, 0, 700, 98
40214, V, 1, 1, 1, 1, 0, 700, 98
40215, V, 1, 1, 1, 1, 0, 700, 98
40216, V, 1, 1, 1, 1, 0, 700, 98
40217, V, 1, 1, 1, 1, 0, 700, 98
40218, V, 1, 1, 1, 1, 0, 700, 98
40219, V, 1, 1, 1, 1, 0, 700, 98
40220, V, 1, 1, 1, 1, 0, 700, 98
40221, V, 1, 1, 1, 1, 0, 700, 98
40222, V, 1, 1, 1, 1, 0, 700, 98
40223, V, 1, 1, 1, 1, 0, 700, 98
40224, V, 1, 1, 1, 1, 0, 700, 98
40225, V, 1, 1, 1, 1, 0, 700, 98
40226, V, 1, 1, 1, 1, 0, 700, 98
40227, V, 1, 1, 1, 1, 0, 700, 98
40228, V, 1, 1, 1, 1, 0, 700, 98
40229, V, 1, 1, 1, 1, 0, 700, 98
40230, V, 1, 1, 1, 1, 0, 700, 98
40231, V, 1, 1, 1, 1, 0, 700, 98
40232, V, 1, 1, 1, 1, 0, 700, 98
40233, V, 1, 1, 1, 1, 0, 700, 98
40235, V, 1, 1, 1, 1, 0, 700, 98
40236, V, 1, 1, 1, 1, 0, 700, 98
40237, V, 1, 1, 1, 1, 0, 700, 98
40238, V, 1, 1, 1, 1, 0, 700, 98
40239, V, 1, 1, 1, 1, 0, 700, 98
40240, V, 1, 1, 1, 1, 0, 700, 98
40241, V, 1, 1, 1, 1, 0, 700, 98
40242, V, 1, 1, 1, 1, 0, 700, 98
40243, V, 1, 1, 1, 1, 0, 700, 98
40244, V, 1, 1, 1, 1, 0, 700, 98
40245, V, 1, 1, 1, 1, 0, 700, 98
40246, V, 1, 1, 1, 1, 0, 700, 98
40247, V, 1, 1, 1, 1, 0, 700, 98
40248, V, 1, 1, 1, 1, 0, 700, 98
40249, V, 1, 1, 1, 1, 0, 700, 98
40250, V, 1, 1, 1, 1, 0, 700, 98
40251, V, 1, 1, 1, 1, 0, 700, 98
40252, V, 1, 1, 1, 1, 0, 700, 98
40253, V, 1, 1, 1, 1, 0, 700, 98
40254, V, 1, 1, 1, 1, 0, 700, 98
40255, V, 1, 1, 1, 1, 0, 700, 98
40256, V, 1, 1, 1, 1, 0, 700, 98
40257, V, 1, 1, 1, 1, 0, 700, 98
40258, V, 1, 1, 1, 1, 0, 700, 98
40259, V, 1, 1, 1, 1, 0, 700, 98
40260, V, 1, 1, 1, 1, 0, 700, 98
40261, V, 1, 1, 1, 1, 0, 700, 98
40262, V, 1, 1, 1, 1, 0, 700, 98
40263, V, 1, 1, 1, 1, 0, 700, 98
40264, V, 1, 1, 1, 1, 0, 700, 98
40265, V, 1, 1, 1, 1, 0, 700, 98
40266, V, 1, 1, 1, 1, 0, 700, 98
40267, V, 1, 1, 1, 1, 0, 700, 98
40268, V, 1, 1, 1, 1, 0, 700, 98
40269, V, 1, 1, 1, 1, 0, 700, 98
40270, V, 1, 1, 1, 1, 0, 700, 98
40271, V, 1, 1, 1, 1, 0, 700, 98
40272, V, 1, 1, 1, 1, 0, 700, 98
40273, V, 1, 1, 1, 1, 0, 700, 98
40274, V, 1, 1, 1, 1, 0, 700, 98
40275, V, 1, 1, 1, 1, 0, 700, 98
40276, V, 1, 1, 1, 1, 0, 700, 98
40278, V, 1, 1, 1, 1, 0, 700, 98
40279, V, 1, 1, 1, 1, 0, 700, 98
40280, V, 1, 1, 1, 1, 0, 700, 98
40281, V, 1, 1, 1, 1, 0, 700, 98
40282, V, 1, 1, 1, 1, 0, 700, 98
40283, V, 1, 1, 1, 1, 0, 700, 98
40284, V, 1, 1, 1, 1, 0, 700, 98
40285, V, 1, 1, 1, 1, 0, 700, 98
40286, V, 1, 1, 1, 1, 0, 700, 98
40287, V, 1, 1, 1, 1, 0, 700, 98
40288, V, 1, 1, 1, 1, 0, 700, 98
40289, V, 1, 1, 1, 1, 0, 700, 98
40290, V, 1, 1, 1, 1, 0, 700, 98
40291, V, 1, 1, 1, 1, 0, 700, 98
40292, V, 1, 1, 1, 1, 0, 700, 98
40293, V, 1, 1, 1, 1, 0, 700, 98
40294, V, 1, 1, 1, 1, 0, 700, 98
40295, V, 1, 1, 1, 1, 0, 700, 98
40296, V, 1, 1, 1, 1, 0, 700, 98
40297, V, 1, 1, 1, 1, 0, 700, 98
40298, V, 1, 1, 1, 1, 0, 700, 98
40299, V, 1, 1, 1, 1, 0, 700, 98
40300, V, 1, 1, 1, 1, 0, 700, 98
40301, V, 1, 1, 1, 1, 0, 700, 98
40302, V, 1, 1, 1, 1, 0, 700, 98
40303, V, 1, 1, 1, 1, 0, 700, 98
40304, V, 1, 1, 1, 1, 0, 700, 98
40305, V, 1, 1, 1, 1, 0, 700, 98
40306, V, 1, 1, 1, 1, 0, 700, 98
40307, V, 1, 1, 1, 1, 0, 700, 98
40308, V, 1, 1, 1, 1, 0, 700, 98
40309, V, 1, 1, 1, 1, 0, 700, 98
40310, V, 1, 1, 1, 1, 0, 700, 98
40311, V, 1, 1, 1, 1, 0, 700, 98
40312, V, 1, 1, 1, 1, 0, 700, 98
40313, V, 1, 1, 1, 1, 0, 700, 98
40314, V, 1, 1, 1, 1, 0, 700, 98
40315, V, 1, 1, 1, 1, 0, 700, 98
40316, V, 1, 1, 1, 1, 0, 700, 98
40317, V, 1, 1, 1, 1, 0, 700, 98
40318, V, 1, 1, 1, 1, 0, 700, 98
40320, V, 1, 1, 1, 1, 0, 700, 98
40321, V, 1, 1, 1, 1, 0, 700, 98
40322, V, 1, 1, 1, 1, 0, 700, 98
40323, V, 1, 1, 1, 1, 0, 700, 98
40324, V, 1, 1, 1, 1, 0, 700, 98
40325, V, 1, 1, 1, 1, 0, 700, 98
40326, V, 1, 1, 1, 1, 0, 700, 98
40327, V, 1, 1, 1, 1, 0, 700, 98
40328, V, 1, 1, 1, 1, 0, 700, 98
40329, V, 1, 1, 1, 1, 0, 700, 98
40330, V, 1, 1, 1, 1, 0, 700, 98
40331, V, 1, 1, 1, 1, 0, 700, 98
40332, V, 1, 1, 1, 1, 0, 700, 98
40333, V, 1, 1, 1, 1, 0, 700, 98
40334, V, 1, 1, 1, 1, 0, 700, 98
40335, V, 1, 1, 1, 1, 0, 700, 98
40336, V, 1, 1, 1, 1, 0, 700, 98
40337, V, 1, 1, 1, 1, 0, 700, 98
40338, V, 1, 1, 1, 1, 0, 700, 98
40339, V, 1, 1, 1, 1, 0, 700, 98
40340, V, 1, 1, 1, 1, 0, 700, 98
40341, V, 1, 1, 1, 1, 0, 700, 98
40342, V, 1, 1, 1, 1, 0, 700, 98
40343, V, 1, 1, 1, 1, 0, 700, 98
40344, V, 1, 1, 1, 1, 0, 700, 98
40345, V, 1, 1, 1, 1, 0, 700, 98
40346, V, 1, 1, 1, 1, 0, 700, 98
40347, V, 1, 1, 1, 1, 0, 700, 98
40348, V, 1, 1, 1, 1, 0, 700, 98
40349, V, 1, 1, 1, 1, 0, 700, 98
40350, V, 1, 1, 1, 1, 0, 700, 98
40351, V, 1, 1, 1, 1, 0, 700, 98
40352, V, 1, 1, 1, 1, 0, 700, 98
40353, V, 1, 1, 1, 1, 0, 700, 98
40354, V, 1, 1, 1, 1, 0, 700, 98
40355, V, 1, 1, 1, 1, 0, 700, 98
40356, V, 1, 1, 1, 1, 0, 700, 98
40357, V, 1, 1, 1, 1, 0, 700, 98
40358, V, 1, 1, 1, 1, 0, 700, 98
40359, V, 1, 1, 1, 1, 0, 700, 98
40360, V, 1, 1, 1, 1, 0, 700, 98
40361, V, 1, 1, 1, 1, 0, 700, 98
40363, V, 1, 1, 1, 1, 0, 700, 98
40364, V, 1, 1, 1, 1, 0, 700, 98
40365, V, 1, 1, 1, 1, 0, 700, 98
40366, V, 1, 1, 1, 1, 0, 700, 98
40367, V, 1, 1, 1, 1, 0, 700, 98
40368, V, 1, 1, 1, 1, 0, 700, 98
40369, V, 1, 1, 1, 1, 0, 700, 98
40370, V, 1, 1, 1, 1, 0, 700, 98
40371, V, 1, 1, 1, 1, 0, 700, 98
40372, V, 1, 1, 1, 1, 0, 700, 98
40373, V, 1, 1, 1, 1, 0, 700, 98
40374, V, 1, 1, 1, 1, 0, 700, 98
40375, V, 1, 1, 1, 1, 0, 700, 98
40376, V, 1, 1, 1, 1, 0, 700, 98
40377, V, 1, 1, 1, 1, 0, 700, 98
40378, V, 1, 1, 1, 1, 0, 700, 98
40379, V, 1, 1, 1, 1, 0, 700, 98
40380, V, 1, 1, 1, 1, 0, 700, 98
40381, V, 1, 1, 1, 1, 0, 700, 98
40382, V, 1, 1, 1, 1, 0, 700, 98
40383, V, 1, 1, 1, 1, 0, 700, 98
40384, V, 1, 1, 1, 1, 0, 700, 98
40385, V, 1, 1, 1, 1, 0, 700, 98
40386, V, 1, 1, 1, 1, 0, 700, 98
40387, V, 1, 1, 1, 1, 0, 700, 98
40388, V, 1, 1, 1, 1, 0, 700, 98
40389, V, 1, 1, 1, 1, 0, 700, 98
40390, V, 1, 1, 1, 1, 0, 700, 98
40391, V, 1, 1, 1, 1, 0, 700, 98
40392, V, 1, 1, 1, 1, 0, 700, 98
40393, V, 1, 1, 1, 1, 0, 700, 98
40394, V, 1, 1, 1, 1, 0, 700, 98
40395, V, 1, 1, 1, 1, 0, 700, 98
40396, V, 1, 1, 1, 1, 0, 700, 98
40397, V, 1, 1, 1, 1, 0, 700, 98
40398, V, 1, 1, 1, 1, 0, 700, 98
40399, V, 1, 1, 1, 1, 0, 700, 98
40400, V, 1, 1, 1, 1, 0, 700, 98
40401, V, 1, 1, 1, 1, 0, 700, 98
40402, V, 1, 1, 1, 1, 0, 700, 98
40403, V, 1, 1, 1, 1, 0, 700, 98
40404, V, 1, 1, 1, 1, 0, 700, 98
40406, V, 1, 1, 1, 1, 0, 700, 98
40407, V, 1, 1, 1, 1, 0, 700, 98
40408, V, 1, 1, 1, 1, 0, 700, 98
40409, V, 1, 1, 1, 1, 0, 700, 98
40410, V, 1, 1, 1, 1, 0, 700, 98
40411, V, 1, 1, 1, 1, 0, 700, 98
40412, V, 1, 1, 1, 1, 0, 700, 98
40413, V, 1, 1, 1, 1, 0, 700, 98
40414, V, 1, 1, 1, 1, 0, 700, 98
40415, V, 1, 1, 1, 1, 0, 700, 98
40416, V, 1, 1, 1, 1, 0, 700, 98
40417, V, 1, 1, 1, 1, 0, 700, 98
40418, V, 1, 1, 1, 1, 0, 700, 98
40419, V, 1, 1, 1, 1, 0, 700, 98
40420, V, 1, 1, 1, 1, 0, 700, 98
40421, V, 1, 1, 1, 1, 0, 700, 98
40422, V, 1, 1, 1, 1, 0, 700, 98
40423, V, 1, 1, 1, 1, 0, 700, 98
40424, V, 1, 1, 1, 1, 0, 700, 98
40425, V, 1, 1, 1, 1, 0, 700, 98
40426, V, 1, 1, 1, 1, 0, 700, 98
40427, V, 1, 1, 1, 1, 0, 700, 98
40428, V, 1, 1, 1, 1, 0, 700, 98
40429, V, 1, 1, 1, 1, 0, 700, 98
40430, V, 1, 1, 1, 1, 0, 700, 98
40431, V, 1, 1, 1, 1, 0, 700, 98
40432, V, 1, 1, 1, 1, 0, 700, 98
40433, V, 1, 1, 1, 1, 0, 700, 98
40434, V, 1, 1, 1, 1, 0, 700, 98
40435, V, 1, 1, 1, 1, 0, 700, 98
40436, V, 1, 1, 1, 1, 0, 700, 98
40437, V, 1, 1, 1, 1, 0, 700, 98
40438, V, 1, 1, 1, 1, 0, 700, 98
40439, V, 1, 1, 1, 1, 0, 700, 98
40440, V, 1, 1, 1, 1, 0, 700, 98
40441, V, 1, 1, 1, 1, 0, 700, 98
40442, V, 1, 1, 1, 1, 0, 700, 98
40443, V, 1, 1, 1, 1, 0, 700, 98
40444, V, 1, 1, 1, 1, 0, 700, 98
40445, V, 1, 1, 1, 1, 0, 700, 98
40446, V, 1, 1, 1, 1, 0, 700, 98
40448, V, 1, 1, 1, 1, 0, 700, 98
40449, V, 1, 1, 1, 1, 0, 700, 98
40450, V, 1, 1, 1, 1, 0, 700, 98
40451, V, 1, 1, 1, 1, 0, 700, 98
40452, V, 1, 1, 1, 1, 0, 700, 98
40453, V, 1, 1, 1, 1, 0, 700, 98
40454, V, 1, 1, 1, 1, 0, 700, 98
40455, V, 1, 1, 1, 1, 0, 700, 98
40456, V, 1, 1, 1, 1, 0, 700, 98
40457, V, 1, 1, 1, 1, 0, 700, 98
40458, V, 1, 1, 1, 1, 0, 700, 98
40459, V, 1, 1, 1, 1, 0, 700, 98
40460, V, 1, 1, 1, 1, 0, 700, 98
40461, V, 1, 1, 1, 1, 0, 700, 98
40462, V, 1, 1, 1, 1, 0, 700, 98
40463, V, 1, 1, 1, 1, 0, 700, 98
40464, V, 1, 1, 1, 1, 0, 700, 98
40465, V, 1, 1, 1, 1, 0, 700, 98
40466, V, 1, 1, 1, 1, 0, 700, 98
40467, V, 1, 1, 1, 1, 0, 700, 98
40468, V, 1, 1, 1, 1, 0, 700, 98
40469, V, 1, 1, 1, 1, 0, 700, 98
40470, V, 1, 1, 1, 1, 0, 700, 98
40471, V, 1, 1, 1, 1, 0, 700, 98
40472, V, 1, 1, 1, 1, 0, 700, 98
40473, V, 1, 1, 1, 1, 0, 700, 98
40474, V, 1, 1, 1, 1, 0, 700, 98
40475, V, 1, 1, 1, 1, 0, 700, 98
40476, V, 1, 1, 1, 1, 0, 700, 98
40477, V, 1, 1, 1, 1, 0, 700, 98
40478, V, 1, 1, 1, 1, 0, 700, 98
40479, V, 1, 1, 1, 1, 0, 700, 98
40480, V, 1, 1, 1, 1, 0, 700, 98
40481, V, 1, 1, 1, 1, 0, 700, 98
40482, V, 1, 1, 1, 1, 0, 700, 98
40483, V, 1, 1, 1, 1, 0, 700, 98
40484, V, 1, 1, 1, 1, 0, 700, 98
40485, V, 1, 1, 1, 1, 0, 700, 98
40486, V, 1, 1, 1, 1, 0, 700, 98
40487, V, 1, 1, 1, 1, 0, 700, 98
40488, V, 1, 1, 1, 1, 0, 700, 98
40489, V, 1, 1, 1, 1, 0, 700, 98
40491, V, 1, 1, 1, 1, 0, 700, 98
40492, V, 1, 1, 1, 1, 0, 700, 98
40493, V, 1, 1, 1, 1, 0, 700, 98
40494, V, 1, 1, 1, 1, 0, 700, 98
40495, V, 1, 1, 1, 1, 0, 700, 98
40496, V, 1, 1, 1, 1, 0, 700, 98
40497, V, 1, 1, 1, 1, 0, 700, 98
40498, V, 1, 1, 1, 1, 0, 700, 98
40499, V, 1, 1, 1, 1, 0, 700, 98
40500, V, 1, 1, 1, 1, 0, 700, 98
40501, V, 1, 1, 1, 1, 0, 700, 98
40502, V, 1, 1, 1, 1, 0, 700, 98
40503, V, 1, 1, 1, 1, 0, 700, 98
40504, V, 1, 1, 1, 1, 0, 700, 98
40505, V, 1, 1, 1, 1, 0, 700, 98
40506, V, 1, 1, 1, 1, 0, 700, 98
40507, V, 1, 1, 1, 1, 0, 700, 98
40508, V, 1, 1, 1, 1, 0, 700, 98
40509, V, 1, 1, 1, 1, 0, 700, 98
40510, V, 1, 1, 1, 1, 0, 700, 98
40511, V, 1, 1, 1, 1, 0, 700, 98
40512, V, 1, 1, 1, 1, 0, 700, 98
40513, V, 1, 1, 1, 1, 0, 700, 98
40514, V, 1, 1, 1, 1, 0, 700, 98
40515, V, 1, 1, 1, 1, 0, 700, 98
40516, V, 1, 1, 1, 1, 0, 700, 98
40517, V, 1, 1, 1, 1, 0, 700, 98
40518, V, 1, 1, 1, 1, 0, 700, 98
40519, V, 1, 1, 1, 1, 0, 700, 98
40520, V, 1, 1, 1, 1, 0, 700, 98
40521, V, 1, 1, 1, 1, 0, 700, 98
40522, V, 1, 1, 1, 1, 0, 700, 98
40523, V, 1, 1, 1, 1, 0, 700, 98
40524, V, 1, 1, 1, 1, 0, 700, 98
40525, V, 1, 1, 1, 1, 0, 700, 98
40526, V, 1, 1, 1, 1, 0, 700, 98
40527, V, 1, 1, 1, 1, 0, 700, 98
40528, V, 1, 1, 1, 1, 0, 700, 98
40529, V, 1, 1, 1, 1, 0, 700, 98
40530, V, 1, 1, 1, 1, 0, 700, 98
40531, V, 1, 1, 1, 1, 0, 700, 98
40532, V, 1, 1, 1, 1, 0, 700, 98
40534, V, 1, 1, 1, 1, 0, 700, 98
40535, V, 1, 1, 1, 1, 0, 700, 98
40536, V, 1, 1, 1, 1, 0, 700, 98
40537, V, 1, 1, 1, 1, 0, 700, 98
40538, V, 1, 1, 1, 1, 0, 700, 98
40539, V, 1, 1, 1, 1, 0, 700, 98
40540, V, 1, 1, 1, 1, 0, 700, 98
40541, V, 1, 1, 1, 1, 0, 700, 98
40542, V, 1, 1, 1, 1, 0, 700, 98
40543, V, 1, 1, 1, 1, 0, 700, 98
40544, V, 1, 1, 1, 1, 0, 700, 98
40545, V, 1, 1, 1, 1, 0, 700, 98
40546, V, 1, 1, 1, 1, 0, 700, 98
40547, V, 1, 1, 1, 1, 0, 700, 98
40548, V, 1, 1, 1, 1, 0, 700, 98
40549, V, 1, 1, 1, 1, 0, 700, 98
40550, V, 1, 1, 1, 1, 0, 700, 98
40551, V, 1, 1, 1, 1, 0, 700, 98
40552, V, 1, 1, 1, 1, 0, 700, 98
40553, V, 1, 1, 1, 1, 0, 700, 98
40554, V, 1, 1, 1, 1, 0, 700, 98
40555, V, 1, 1, 1, 1, 0, 700, 98
40556, V, 1, 1, 1, 1, 0, 700, 98
40557, V, 1, 1, 1, 1, 0, 700, 98
40558, V, 1, 1, 1, 1, 0, 700, 98
40559, V, 1, 1, 1, 1, 0, 700, 98
40560, V, 1, 1, 1, 1, 0, 700, 98
40561, V, 1, 1, 1, 1, 0, 700, 98
40562, V, 1, 1, 1, 1, 0, 700, 98
40563, V, 1, 1, 1, 1, 0, 700, 98
40564, V, 1, 1, 1, 1, 0, 700, 98
40565, V, 1, 1, 1, 1, 0, 700, 98
40566, V, 1, 1, 1, 1, 0, 700, 98
40567, V, 1, 1, 1, 1, 0, 700, 98
40568, V, 1, 1, 1, 1, 0, 700, 98
40569, V, 1, 1, 1, 1, 0, 700, 98
40570, V, 1, 1, 1, 1, 0, 700, 98
40571, V, 1, 1, 1, 1, 0, 700, 98
40572, V, 1, 1, 1, 1, 0, 700, 98
40573, V, 1, 1, 1, 1, 0, 700, 98
40574, V, 1, 1, 1, 1, 0, 700, 98
40576, V, 1, 1, 1, 1, 0, 700, 98
40577, V, 1, 1, 1, 1, 0, 700, 98
40578, V, 1, 1, 1, 1, 0, 700, 98
40579, V, 1, 1, 1, 1, 0, 700, 98
40580, V, 1, 1, 1, 1, 0, 700, 98
40581, V, 1, 1, 1, 1, 0, 700, 98
40582, V, 1, 1, 1, 1, 0, 700, 98
40583, V, 1, 1, 1, 1, 0, 700, 98
40584, V, 1, 1, 1, 1, 0, 700, 98
40585, V, 1, 1, 1, 1, 0, 700, 98
40586, V, 1, 1, 1, 1, 0, 700, 98
40587, V, 1, 1, 1, 1, 0, 700, 98
40588, V, 1, 1, 1, 1, 0, 700, 98
40589, V, 1, 1, 1, 1, 0, 700, 98
40590, V, 1, 1, 1, 1, 0, 700, 98
40591, V, 1, 1, 1, 1, 0, 700, 98
40592, V, 1, 1, 1, 1, 0, 700, 98
40593, V, 1, 1, 1, 1, 0, 700, 98
40594, V, 1, 1, 1, 1, 0, 700, 98
40595, V, 1, 1, 1, 1, 0, 700, 98
40596, V, 1, 1, 1, 1, 0, 700, 98
40597, V, 1, 1, 1, 1, 0, 700, 98
40598, V, 1, 1, 1, 1, 0, 700, 98
40599, V, 1, 1, 1, 1, 0, 700, 98
40600, V, 1, 1, 1, 1, 0, 700, 98
40601, V, 1, 1, 1, 1, 0, 700, 98
40602, V, 1, 1, 1, 1, 0, 700, 98
40603, V, 1, 1, 1, 1, 0, 700, 98
40604, V, 1, 1, 1, 1, 0, 700, 98
40605, V, 1, 1, 1, 1, 0, 700, 98
40606, V, 1, 1, 1, 1, 0, 700, 98
40607, V, 1, 1, 1, 1, 0, 700, 98
40608, V, 1, 1, 1, 1, 0, 700, 98
40609, V, 1, 1, 1, 1, 0, 700, 98
40610, V, 1, 1, 1, 1, 0, 700, 98
40611, V, 1, 1, 1, 1, 0, 700, 98
40612, V, 1, 1, 1, 1, 0, 700, 98
40613, V, 1, 1, 1, 1, 0, 700, 98
40614, V, 1, 1, 1, 1, 0, 700, 98
40615, V, 1, 1, 1, 1, 0, 700, 98
40616, V, 1, 1, 1, 1, 0, 700, 98
40617, V, 1, 1, 1, 1, 0, 700, 98
40619, V, 1, 1, 1, 1, 0, 700, 98
40620, V, 1, 1, 1, 1, 0, 700, 98
40621, V, 1, 1, 1, 1, 0, 700, 98
40622, V, 1, 1, 1, 1, 0, 700, 98
40623, V, 1, 1, 1, 1, 0, 700, 98
40624, V, 1, 1, 1, 1, 0, 700, 98
40625, V, 1, 1, 1, 1, 0, 700, 98
40626, V, 1, 1, 1, 1, 0, 700, 98
40627, V, 1, 1, 1, 1, 0, 700, 98
40628, V, 1, 1, 1, 1, 0, 700, 98
40629, V, 1, 1, 1, 1, 0, 700, 98
40630, V, 1, 1, 1, 1, 0, 700, 98
40631, V, 1, 1, 1, 1, 0, 700, 98
40632, V, 1, 1, 1, 1, 0, 700, 98
40633, V, 1, 1, 1, 1, 0, 700, 98
40634, V, 1, 1, 1, 1, 0, 700, 98
40635, V, 1, 1, 1, 1, 0, 700, 98
40636, V, 1, 1, 1, 1, 0, 700, 98
40637, V, 1, 1, 1, 1, 0, 700, 98
40638, V, 1, 1, 1, 1, 0, 700, 98
40639, V, 1, 1, 1, 1, 0, 700, 98
40640, V, 1, 1, 1, 1, 0, 700, 98
40641, V, 1, 1, 1, 1, 0, 700, 98
40642, V, 1, 1, 1, 1, 0, 700, 98
40643, V, 1, 1, 1, 1, 0, 700, 98
40644, V, 1, 1, 1, 1, 0, 700, 98
40645, V, 1, 1, 1, 1, 0, 700, 98
40646, V, 1, 1, 1, 1, 0, 700, 98
40647, V, 1, 1, 1, 1, 0, 700, 98
40648, V, 1, 1, 1, 1, 0, 700, 98
40649, V, 1, 1, 1, 1, 0, 700, 98
40650, V, 1, 1, 1, 1, 0, 700, 98
40651, V, 1, 1, 1, 1, 0, 700, 98
40652, V, 1, 1, 1, 1, 0, 700, 98
40653, V, 1, 1, 1, 1, 0, 700, 98
40654, V, 1, 1, 1, 1, 0, 700, 98
40655, V, 1, 1, 1, 1, 0, 700, 98
40656, V, 1, 1, 1, 1, 0, 700, 98
40657, V, 1, 1, 1, 1, 0, 700, 98
40658, V, 1, 1, 1, 1, 0, 700, 98
40659, V, 1, 1, 1, 1, 0, 700, 98
40660, V, 1, 1, 1, 1, 0, 700, 98
40662, V, 1, 1, 1, 1, 0, 700, 98
40663, V, 1, 1, 1, 1, 0, 700, 98
40664, V, 1, 1, 1, 1, 0, 700, 98
40665, V, 1, 1, 1, 1, 0, 700, 98
40666, V, 1, 1, 1, 1, 0, 700, 98
40667, V, 1, 1, 1, 1, 0, 700, 98
40668, V, 1, 1, 1, 1, 0, 700, 98
40669, V, 1, 1, 1, 1, 0, 700, 98
40670, V, 1, 1, 1, 1, 0, 700, 98
40671, V, 1, 1, 1, 1, 0, 700, 98
40672, V, 1, 1, 1, 1, 0, 700, 98
40673, V, 1, 1, 1, 1, 0, 700, 98
40674, V, 1, 1, 1, 1, 0, 700, 98
40675, V, 1, 1, 1, 1, 0, 700, 98
40676, V, 1, 1, 1, 1, 0, 700, 98
40677, V, 1, 1, 1, 1, 0, 700, 98
40678, V, 1, 1, 1, 1, 0, 700, 98
40679, V, 1, 1, 1, 1, 0, 700, 98
40680, V, 1, 1, 1, 1, 0, 700, 98
40681, V, 1, 1, 1, 1, 0, 700, 98
40682, V, 1, 1, 1, 1, 0, 700, 98
40683, V, 1, 1, 1, 1, 0, 700, 98
40684, V, 1, 1, 1, 1, 0, 700, 98
40685, V, 1, 1, 1, 1, 0, 700, 98
40686, V, 1, 1, 1, 1, 0, 700, 98
40687, V, 1, 1, 1, 1, 0, 700, 98
40688, V, 1, 1, 1, 1, 0, 700, 98
40689, V, 1, 1, 1, 1, 0, 700, 98
40690, V, 1, 1, 1, 1, 0, 700, 98
40691, V, 1, 1, 1, 1, 0, 700, 98
40692, V, 1, 1, 1, 1, 0, 700, 98
40693, V, 1, 1, 1, 1, 0, 700, 98
40694, V, 1, 1, 1, 1, 0, 700, 98
40695, V, 1, 1, 1, 1, 0, 700, 98
40696, V, 1, 1, 1, 1, 0, 700, 98
40697, V, 1, 1, 1, 1, 0, 700, 98
40698, V, 1, 1, 1, 1, 0, 700, 98
40699, V, 1, 1, 1, 1, 0, 700, 98
40700, V, 1, 1, 1, 1, 0, 700, 98
40701, V, 1, 1, 1, 1, 0, 700, 98
40702, V, 1, 1, 1, 1, 0, 700, 98
40704, V, 1, 1, 1, 1, 0, 700, 98
40705, V, 1, 1, 1, 1, 0, 700, 98
40706, V, 1, 1, 1, 1, 0, 700, 98
40707, V, 1, 1, 1, 1, 0, 700, 98
40708, V, 1, 1, 1, 1, 0, 700, 98
40709, V, 1, 1, 1, 1, 0, 700, 98
40710, V, 1, 1, 1, 1, 0, 700, 98
40711, V, 1, 1, 1, 1, 0, 700, 98
40712, V, 1, 1, 1, 1, 0, 700, 98
40713, V, 1, 1, 1, 1, 0, 700, 98
40714, V, 1, 1, 1, 1, 0, 700, 98
40715, V, 1, 1, 1, 1, 0, 700, 98
40716, V, 1, 1, 1, 1, 0, 700, 98
40717, V, 1, 1, 1, 1, 0, 700, 98
40718, V, 1, 1, 1, 1, 0, 700, 98
40719, V, 1, 1, 1, 1, 0, 700, 98
40720, V, 1, 1, 1, 1, 0, 700, 98
40721, V, 1, 1, 1, 1, 0, 700, 98
40722, V, 1, 1, 1, 1, 0, 700, 98
40723, V, 1, 1, 1, 1, 0, 700, 98
40724, V, 1, 1, 1, 1, 0, 700, 98
40725, V, 1, 1, 1, 1, 0, 700, 98
40726, V, 1, 1, 1, 1, 0, 700, 98
40727, V, 1, 1, 1, 1, 0, 700, 98
40728, V, 1, 1, 1, 1, 0, 700, 98
40729, V, 1, 1, 1, 1, 0, 700, 98
40730, V, 1, 1, 1, 1, 0, 700, 98
40731, V, 1, 1, 1, 1, 0, 700, 98
40732, V, 1, 1, 1, 1, 0, 700, 98
40733, V, 1, 1, 1, 1, 0, 700, 98
40734, V, 1, 1, 1, 1, 0, 700, 98
40735, V, 1, 1, 1, 1, 0, 700, 98
40736, V, 1, 1, 1, 1, 0, 700, 98
40737, V, 1, 1, 1, 1, 0, 700, 98
40738, V, 1, 1, 1, 1, 0, 700, 98
40739, V, 1, 1, 1, 1, 0, 700, 98
40740, V, 1, 1, 1, 1, 0, 700, 98
40741, V, 1, 1, 1, 1, 0, 700, 98
40742, V, 1, 1, 1, 1, 0, 700, 98
40743, V, 1, 1, 1, 1, 0, 700, 98
40744, V, 1, 1, 1, 1, 0, 700, 98
40745, V, 1, 1, 1, 1, 0, 700, 98
40747, V, 1, 1, 1, 1, 0, 700, 98
40748, V, 1, 1, 1, 1, 0, 700, 98
40749, V, 1, 1, 1, 1, 0, 700, 98
40750, V, 1, 1, 1, 1, 0, 700, 98
40751, V, 1, 1, 1, 1, 0, 700, 98
40752, V, 1, 1, 1, 1, 0, 700, 98
40753, V, 1, 1, 1, 1, 0, 700, 98
40754, V, 1, 1, 1, 1, 0, 700, 98
40755, V, 1, 1, 1, 1, 0, 700, 98
40756, V, 1, 1, 1, 1, 0, 700, 98
40757, V, 1, 1, 1, 1, 0, 700, 98
40758, V, 1, 1, 1, 1, 0, 700, 98
40759, V, 1, 1, 1, 1, 0, 700, 98
40760, V, 1, 1, 1, 1, 0, 700, 98
40761, V, 1, 1, 1, 1, 0, 700, 98
40762, V, 1, 1, 1, 1, 0, 700, 98
40763, V, 1, 1, 1, 1, 0, 700, 98
40764, V, 1, 1, 1, 1, 0, 700, 98
40765, V, 1, 1, 1, 1, 0, 700, 98
40766, V, 1, 1, 1, 1, 0, 700, 98
40767, V, 1, 1, 1, 1, 0, 700, 98
40768, V, 1, 1, 1, 1, 0, 700, 98
40769, V, 1, 1, 1, 1, 0, 700, 98
40770, V, 1, 1, 1, 1, 0, 700, 98
40771, V, 1, 1, 1, 1, 0, 700, 98
40772, V, 1, 1, 1, 1, 0, 700, 98
40773, V, 1, 1, 1, 1, 0, 700, 98
40774, V, 1, 1, 1, 1, 0, 700, 98
40775, V, 1, 1, 1, 1, 0, 700, 98
40776, V, 1, 1, 1, 1, 0, 700, 98
40777, V, 1, 1, 1, 1, 0, 700, 98
40778, V, 1, 1, 1, 1, 0, 700, 98
40779, V, 1, 1, 1, 1, 0, 700, 98
40780, V, 1, 1, 1, 1, 0, 700, 98
40781, V, 1, 1, 1, 1, 0, 700, 98
40782, V, 1, 1, 1, 1, 0, 700, 98
40783, V, 1, 1, 1, 1, 0, 700, 98
40784, V, 1, 1, 1, 1, 0, 700, 98
40785, V, 1, 1, 1, 1, 0, 700, 98
40786, V, 1, 1, 1, 1, 0, 700, 98
40787, V, 1, 1, 1, 1, 0, 700, 98
40788, V, 1, 1, 1, 1, 0, 700, 98
40790, V, 1, 1, 1, 1, 0, 700, 98
40791, V, 1, 1, 1, 1, 0, 700, 98
40792, V, 1, 1, 1, 1, 0, 700, 98
40793, V, 1, 1, 1, 1, 0, 700, 98
40794, V, 1, 1, 1, 1, 0, 700, 98
40795, V, 1, 1, 1, 1, 0, 700, 98
40796, V, 1, 1, 1, 1, 0, 700, 98
40797, V, 1, 1, 1, 1, 0, 700, 98
40798, V, 1, 1, 1, 1, 0, 700, 98
40799, V, 1, 1, 1, 1, 0, 700, 98
40800, V, 1, 1, 1, 1, 0, 700, 98
40801, V, 1, 1, 1, 1, 0, 700, 98
40802, V, 1, 1, 1, 1, 0, 700, 98
40803, V, 1, 1, 1, 1, 0, 700, 98
40804, V, 1, 1, 1, 1, 0, 700, 98
40805, V, 1, 1, 1, 1, 0, 700, 98
40806, V, 1, 1, 1, 1, 0, 700, 98
40807, V, 1, 1, 1, 1, 0, 700, 98
40808, V, 1, 1, 1, 1, 0, 700, 98
40809, V, 1, 1, 1, 1, 0, 700, 98
40810, V, 1, 1, 1, 1, 0, 700, 98
40811, V, 1, 1, 1, 1, 0, 700, 98
40812, V, 1, 1, 1, 1, 0, 700, 98
40813, V, 1, 1, 1, 1, 0, 700, 98
40814, V, 1, 1, 1, 1, 0, 700, 98
40815, V, 1, 1, 1, 1, 0, 700, 98
40816, V, 1, 1, 1, 1, 0, 700, 98
40817, V, 1, 1, 1, 1, 0, 700, 98
40818, V, 1, 1, 1, 1, 0, 700, 98
40819, V, 1, 1, 1, 1, 0, 700, 98
40820, V, 1, 1, 1, 1, 0, 700, 98
40821, V, 1, 1, 1, 1, 0, 700, 98
40822, V, 1, 1, 1, 1, 0, 700, 98
40823, V, 1, 1, 1, 1, 0, 700, 98
40824, V, 1, 1, 1, 1, 0, 700, 98
40825, V, 1, 1, 1, 1, 0, 700, 98
40826, V, 1, 1, 1, 1, 0, 700, 98
40827, V, 1, 1, 1, 1, 0, 700, 98
40828, V, 1, 1, 1, 1, 0, 700, 98
40829, V, 1, 1, 1, 1, 0, 700, 98
40830, V, 1, 1, 1, 1, 0, 700, 98
40832, V, 1, 1, 1, 1, 0, 700, 98
40833, V, 1, 1, 1, 1, 0, 700, 98
40834, V, 1, 1, 1, 1, 0, 700, 98
40835, V, 1, 1, 1, 1, 0, 700, 98
40836, V, 1, 1, 1, 1, 0, 700, 98
40837, V, 1, 1, 1, 1, 0, 700, 98
40838, V, 1, 1, 1, 1, 0, 700, 98
40839, V, 1, 1, 1, 1, 0, 700, 98
40840, V, 1, 1, 1, 1, 0, 700, 98
40841, V, 1, 1, 1, 1, 0, 700, 98
40842, V, 1, 1, 1, 1, 0, 700, 98
40843, V, 1, 1, 1, 1, 0, 700, 98
40844, V, 1, 1, 1, 1, 0, 700, 98
40845, V, 1, 1, 1, 1, 0, 700, 98
40846, V, 1, 1, 1, 1, 0, 700, 98
40847, V, 1, 1, 1, 1, 0, 700, 98
40848, V, 1, 1, 1, 1, 0, 700, 98
40849, V, 1, 1, 1, 1, 0, 700, 98
40850, V, 1, 1, 1, 1, 0, 700, 98
40851, V, 1, 1, 1, 1, 0, 700, 98
40852, V, 1, 1, 1, 1, 0, 700, 98
40853, V, 1, 1, 1, 1, 0, 700, 98
40854, V, 1, 1, 1, 1, 0, 700, 98
40855, V, 1, 1, 1, 1, 0, 700, 98
40856, V, 1, 1, 1, 1, 0, 700, 98
40857, V, 1, 1, 1, 1, 0, 700, 98
40858, V, 1, 1, 1, 1, 0, 700, 98
40859, V, 1, 1, 1, 1, 0, 700, 98
40860, V, 1, 1, 1, 1, 0, 700, 98
40861, V, 1, 1, 1, 1, 0, 700, 98
40862, V, 1, 1, 1, 1, 0, 700, 98
40863, V, 1, 1, 1, 1, 0, 700, 98
40864, V, 1, 1, 1, 1, 0, 700, 98
40865, V, 1, 1, 1, 1, 0, 700, 98
40866, V, 1, 1, 1, 1, 0, 700, 98
40867, V, 1, 1, 1, 1, 0, 700, 98
40868, V, 1, 1, 1, 1, 0, 700, 97
40869, V, 1, 1, 1, 1, 0, 700, 98
40870, V, 1, 1, 1, 1, 0, 700, 98
40871, V, 1, 1, 1, 1, 0, 700, 97
40872, V, 1, 1, 1, 1, 0, 700, 98
40873, V, 1, 1, 1, 1, 0, 700, 97
40875, V, 1, 1, 1, 1, 0, 700, 98
40876, V, 1, 1, 1, 1, 0, 700, 97
40877, V, 1, 1, 1, 1, 0, 700, 97
40878, V, 1, 1, 1, 1, 0, 700, 98
40879, V, 1, 1, 1, 1, 0, 700, 98
40880, V, 1, 1, 1, 1, 0, 700, 98
40881, V, 1, 1, 1, 1, 0, 700, 98
40882, V, 1, 1, 1, 1, 0, 700, 98
40883, V, 1, 1, 1, 1, 0, 700, 98
40884, V, 1, 1, 1, 1, 0, 700, 97
40885, V, 1, 1, 1, 1, 0, 700, 98
40886, V, 1, 1, 1, 1, 0, 700, 98
40887, V, 1, 1, 1, 1, 0, 700, 98
40888, V, 1, 1, 1, 1, 0, 700, 98
40889, V, 1, 1, 1, 1, 0, 700, 98
40890, V, 1, 1, 1, 1, 0, 700, 98
40891, V, 1, 1, 1, 1, 0, 700, 98
40892, V, 1, 1, 1, 1, 0, 700, 98
40893, V, 1, 1, 1, 1, 0, 700, 98
40894, V, 1, 1, 1, 1, 0, 700, 98
40895, V, 1, 1, 1, 1, 0, 700, 98
40896, V, 1, 1, 1, 1, 0, 700, 98
40897, V, 1, 1, 1, 1, 0, 700, 98
40898, V, 1, 1, 1, 1, 0, 700, 98
40899, V, 1, 1, 1, 1, 0, 700, 98
40900, V, 1, 1, 1, 1, 0, 700, 98
40901, V, 1, 1, 1, 1, 0, 700, 98
40902, V, 1, 1, 1, 1, 0, 700, 98
40903, V, 1, 1, 1, 1, 0, 700, 98
40904, V, 1, 1, 1, 1, 0, 700, 98
40905, V, 1, 1, 1, 1, 0, 700, 98
40906, V, 1, 1, 1, 1, 0, 700, 98
40907, V, 1, 1, 1, 1, 0, 700, 98
40908, V, 1, 1, 1, 1, 0, 700, 98
40909, V, 1, 1, 1, 1, 0, 700, 98
40910, V, 1, 1, 1, 1, 0, 700, 98
40911, V, 1, 1, 1, 1, 0, 700, 98
40912, V, 1, 1, 1, 1, 0, 700, 98
40913, V, 1, 1, 1, 1, 0, 700, 98
40914, V, 1, 1, 1, 1, 0, 700, 98
40915, V, 1, 1, 1, 1, 0, 700, 98
40916, V, 1, 1, 1, 1, 0, 700, 98
40918, V, 1, 1, 1, 1, 0, 700, 98
40919, V, 1, 1, 1, 1, 0, 700, 98
40920, V, 1, 1, 1, 1, 0, 700, 98
40921, V, 1, 1, 1, 1, 0, 700, 98
40922, V, 1, 1, 1, 1, 0, 700, 98
40923, V, 1, 1, 1, 1, 0, 700, 98
40924, V, 1, 1, 1, 1, 0, 700, 98
40925, V, 1, 1, 1, 1, 0, 700, 98
40926, V, 1, 1, 1, 1, 0, 700, 98
40927, V, 1, 1, 1, 1, 0, 700, 98
40928, V, 1, 1, 1, 1, 0, 700, 98
40929, V, 1, 1, 1, 1, 0, 700, 98
40930, V, 1, 1, 1, 1, 0, 700, 98
40931, V, 1, 1, 1, 1, 0, 700, 98
40932, V, 1, 1, 1, 1, 0, 700, 98
40933, V, 1, 1, 1, 1, 0, 700, 98
40934, V, 1, 1, 1, 1, 0, 700, 98
40935, V, 1, 1, 1, 1, 0, 700, 98
40936, V, 1, 1, 1, 1, 0, 700, 98
40937, V, 1, 1, 1, 1, 0, 700, 98
40938, V, 1, 1, 1, 1, 0, 700, 98
40939, V, 1, 1, 1, 1, 0, 700, 98
40940, V, 1, 1, 1, 1, 0, 700, 97
40941, V, 1, 1, 1, 1, 0, 700, 98
40942, V, 1, 1, 1, 1, 0, 700, 97
40943, V, 1, 1, 1, 1, 0, 700, 98
40944, V, 1, 1, 1, 1, 0, 700, 98
40945, V, 1, 1, 1, 1, 0, 700, 98
40946, V, 1, 1, 1, 1, 0, 700, 97
40947, V, 1, 1, 1, 1, 0, 700, 98
40948, V, 1, 1, 1, 1, 0, 700, 98
40949, V, 1, 1, 1, 1, 0, 700, 98
40950, V, 1, 1, 1, 1, 0, 700, 98
40951, V, 1, 1, 1, 1, 0, 700, 98
40952, V, 1, 1, 1, 1, 0, 700, 98
40953, V, 1, 1, 1, 1, 0, 700, 98
40954, V, 1, 1, 1, 1, 0, 700, 98
40955, V, 1, 1, 1, 1, 0, 700, 98
40956, V, 1, 1, 1, 1, 0, 700, 98
40957, V, 1, 1, 1, 1, 0, 700, 98
40958, V, 1, 1, 1, 1, 0, 700, 98
40960, V, 1, 1, 1, 1, 0, 700, 98
40961, V, 1, 1, 1, 1, 0, 700, 98
40962, V, 1, 1, 1, 1, 0, 700, 98
40963, V, 1, 1, 1, 1, 0, 700, 98
40964, V, 1, 1, 1, 1, 0, 700, 98
40965, V, 1, 1, 1, 1, 0, 700, 98
40966, V, 1, 1, 1, 1, 0, 700, 98
40967, V, 1, 1, 1, 1, 0, 700, 98
40968, V, 1, 1, 1, 1, 0, 700, 98
40969, V, 1, 1, 1, 1, 0, 700, 98
40970, V, 1, 1, 1, 1, 0, 700, 98
40971, V, 1, 1, 1, 1, 0, 700, 98
40972, V, 1, 1, 1, 1, 0, 700, 98
40973, V, 1, 1, 1, 1, 0, 700, 98
40974, V, 1, 1, 1, 1, 0, 700, 98
40975, V, 1, 1, 1, 1, 0, 700, 98
40976, V, 1, 1, 1, 1, 0, 700, 98
40977, V, 1, 1, 1, 1, 0, 700, 98
40978, V, 1, 1, 1, 1, 0, 700, 98
40979, V, 1, 1, 1, 1, 0, 700, 98
40980, V, 1, 1, 1, 1, 0, 700, 98
40981, V, 1, 1, 1, 1, 0, 700, 98
40982, V, 1, 1, 1, 1, 0, 700, 98
40983, V, 1, 1, 1, 1, 0, 700, 98
40984, V, 1, 1, 1, 1, 0, 700, 98
40985, V, 1, 1, 1, 1, 0, 700, 98
40986, V, 1, 1, 1, 1, 0, 700, 98
40987, V, 1, 1, 1, 1, 0, 700, 98
40988, V, 1, 1, 1, 1, 0, 700, 98
40989, V, 1, 1, 1, 1, 0, 700, 98
40990, V, 1, 1, 1, 1, 0, 700, 98
40991, V, 1, 1, 1, 1, 0, 700, 98
40992, V, 1, 1, 1, 1, 0, 700, 98
40993, V, 1, 1, 1, 1, 0, 700, 98
40994, V, 1, 1, 1, 1, 0, 700, 98
40995, V, 1, 1, 1, 1, 0, 700, 98
40996, V, 1, 1, 1, 1, 0, 700, 98
40997, V, 1, 1, 1, 1, 0, 700, 98
40998, V, 1, 1, 1, 1, 0, 700, 98
40999, V, 1, 1, 1, 1, 0, 700, 98
41000, V, 1, 1, 1, 1, 0, 700, 98
41001, V, 1, 1, 1, 1, 0, 700, 98
41003, V, 1, 1, 1, 1, 0, 700, 97
41004, V, 1, 1, 1, 1, 0, 700, 98
41005, V, 1, 1, 1, 1, 0, 700, 98
41006, V, 1, 1, 1, 1, 0, 700, 98
41007, V, 1, 1, 1, 1, 0, 700, 98
41008, V, 1, 1, 1, 1, 0, 700, 98
41009, V, 1, 1, 1, 1, 0, 700, 98
41010, V, 1, 1, 1, 1, 0, 700, 98
41011, V, 1, 1, 1, 1, 0, 700, 98
41012, V, 1, 1, 1, 1, 0, 700, 98
41013, V, 1, 1, 1, 1, 0, 700, 98
41014, V, 1, 1, 1, 1, 0, 700, 98
41015, V, 1, 1, 1, 1, 0, 700, 98
41016, V, 1, 1, 1, 1, 0, 700, 97
41017, V, 1, 1, 1, 1, 0, 700, 97
41018, V, 1, 1, 1, 1, 0, 700, 97
41019, V, 1, 1, 1, 1, 0, 700, 98
41020, V, 1, 1, 1, 1, 0, 700, 97
41021, V, 1, 1, 1, 1, 0, 700, 97
41022, V, 1, 1, 1, 1, 0, 700, 98
41023, V, 1, 1, 1, 1, 0, 700, 97
41024, V, 1, 1, 1, 1, 0, 700, 97
41025, V, 1, 1, 1, 1, 0, 700, 97
41026, V, 1, 1, 1, 1, 0, 700, 97
41027, V, 1, 1, 1, 1, 0, 700, 97
41028, V, 1, 1, 1, 1, 0, 700, 97
41029, V, 1, 1, 1, 1, 0, 700, 98
41030, V, 1, 1, 1, 1, 0, 700, 97
41031, V, 1, 1, 1, 1, 0, 700, 98
41032, V, 1, 1, 1, 1, 0, 700, 98
41033, V, 1, 1, 1, 1, 0, 700, 97
41034, V, 1, 1, 1, 1, 0, 700, 98
41035, V, 1, 1, 1, 1, 0, 700, 97
41036, V, 1, 1, 1, 1, 0, 700, 97
41037, V, 1, 1, 1, 1, 0, 700, 97
41038, V, 1, 1, 1, 1, 0, 700, 97
41039, V, 1, 1, 1, 1, 0, 700, 98
41040, V, 1, 1, 1, 1, 0, 700, 97
41041, V, 1, 1, 1, 1, 0, 700, 98
41042, V, 1, 1, 1, 1, 0, 700, 98
41043, V, 1, 1, 1, 1, 0, 700, 97
41044, V, 1, 1, 1, 1, 0, 700, 98
41046, V, 1, 1, 1, 1, 0, 700, 98
41047, V, 1, 1, 1, 1, 0, 700, 98
41048, V, 1, 1, 1, 1, 0, 700, 98
41049, V, 1, 1, 1, 1, 0, 700, 98
41050, V, 1, 1, 1, 1, 0, 700, 98
41051, V, 1, 1, 1, 1, 0, 700, 98
41052, V, 1, 1, 1, 1, 0, 700, 98
41053, V, 1, 1, 1, 1, 0, 700, 98
41054, V, 1, 1, 1, 1, 0, 700, 98
41055, V, 1, 1, 1, 1, 0, 700, 98
41056, V, 1, 1, 1, 1, 0, 700, 98
41057, V, 1, 1, 1, 1, 0, 700, 98
41058, V, 1, 1, 1, 1, 0, 700, 98
41059, V, 1, 1, 1, 1, 0, 700, 98
41060, V, 1, 1, 1, 1, 0, 700, 98
41061, V, 1, 1, 1, 1, 0, 700, 98
41062, V, 1, 1, 1, 1, 0, 700, 98
41063, V, 1, 1, 1, 1, 0, 700, 98
41064, V, 1, 1, 1, 1, 0, 700, 98
41065, V, 1, 1, 1, 1, 0, 700, 98
41066, V, 1, 1, 1, 1, 0, 700, 98
41067, V, 1, 1, 1, 1, 0, 700, 98
41068, V, 1, 1, 1, 1, 0, 700, 98
41069, V, 1, 1, 1, 1, 0, 700, 98
41070, V, 1, 1, 1, 1, 0, 700, 98
41071, V, 1, 1, 1, 1, 0, 700, 98
41072, V, 1, 1, 1, 1, 0, 700, 98
41073, V, 1, 1, 1, 1, 0, 700, 98
41074, V, 1, 1, 1, 1, 0, 700, 98
41075, V, 1, 1, 1, 1, 0, 700, 98
41076, V, 1, 1, 1, 1, 0, 700, 98
41077, V, 1, 1, 1, 1, 0, 700, 98
41078, V, 1, 1, 1, 1, 0, 700, 98
41079, V, 1, 1, 1, 1, 0, 700, 98
41080, V, 1, 1, 1, 1, 0, 700, 98
41081, V, 1, 1, 1, 1, 0, 700, 98
41082, V, 1, 1, 1, 1, 0, 700, 98
41083, V, 1, 1, 1, 1, 0, 700, 98
41084, V, 1, 1, 1, 1, 0, 700, 98
41085, V, 1, 1, 1, 1, 0, 700, 98
41086, V, 1, 1, 1, 1, 0, 700, 98
41088, V, 1, 1, 1, 1, 0, 700, 98
41089, V, 1, 1, 1, 1, 0, 700, 98
41090, V, 1, 1, 1, 1, 0, 700, 98
41091, V, 1, 1, 1, 1, 0, 700, 98
41092, V, 1, 1, 1, 1, 0, 700, 98
41093, V, 1, 1, 1, 1, 0, 700, 97
41094, V, 1, 1, 1, 1, 0, 700, 97
41095, V, 1, 1, 1, 1, 0, 700, 98
41096, V, 1, 1, 1, 1, 0, 700, 97
41097, V, 1, 1, 1, 1, 0, 700, 97
41098, V, 1, 1, 1, 1, 0, 700, 98
41099, V, 1, 1, 1, 1, 0, 700, 97
41100, V, 1, 1, 1, 1, 0, 700, 97
41101, V, 1, 1, 1, 1, 0, 700, 97
41102, V, 1, 1, 1, 1, 0, 700, 97
41103, V, 1, 1, 1, 1, 0, 700, 98
41104, V, 1, 1, 1, 1, 0, 700, 97
41105, V, 1, 1, 1, 1, 0, 700, 98
41106, V, 1, 1, 1, 1, 0, 700, 97
41107, V, 1, 1, 1, 1, 0, 700, 98
41108, V, 1, 1, 1, 1, 0, 700, 98
41109, V, 1, 1, 1, 1, 0, 700, 98
41110, V, 1, 1, 1, 1, 0, 700, 98
41111, V, 1, 1, 1, 1, 0, 700, 98
41112, V, 1, 1, 1, 1, 0, 700, 98
41113, V, 1, 1, 1, 1, 0, 700, 98
41114, V, 1, 1, 1, 1, 0, 700, 98
41115, V, 1, 1, 1, 1, 0, 700, 97
41116, V, 1, 1, 1, 1, 0, 700, 97
41117, V, 1, 1, 1, 1, 0, 700, 98
41118, V, 1, 1, 1, 1, 0, 700, 98
41119, V, 1, 1, 1, 1, 0, 700, 98
41120, V, 1, 1, 1, 1, 0, 700, 98
41121, V, 1, 1, 1, 1, 0, 700, 98
41122, V, 1, 1, 1, 1, 0, 700, 98
41123, V, 1, 1, 1, 1, 0, 700, 98
41124, V, 1, 1, 1, 1, 0, 700, 98
41125, V, 1, 1, 1, 1, 0, 700, 98
41126, V, 1, 1, 1, 1, 0, 700, 98
41127, V, 1, 1, 1, 1, 0, 700, 98
41128, V, 1, 1, 1, 1, 0, 700, 98
41129, V, 1, 1, 1, 1, 0, 700, 98
41131, V, 1, 1, 1, 1, 0, 700, 98
41132, V, 1, 1, 1, 1, 0, 700, 98
41133, V, 1, 1, 1, 1, 0, 700, 98
41134, V, 1, 1, 1, 1, 0, 700, 98
41135, V, 1, 1, 1, 1, 0, 700, 98
41136, V, 1, 1, 1, 1, 0, 700, 98
41137, V, 1, 1, 1, 1, 0, 700, 98
41138, V, 1, 1, 1, 1, 0, 700, 98
41139, V, 1, 1, 1, 1, 0, 700, 98
41140, V, 1, 1, 1, 1, 0, 700, 98
41141, V, 1, 1, 1, 1, 0, 700, 98
41142, V, 1, 1, 1, 1, 0, 700, 98
41143, V, 1, 1, 1, 1, 0, 700, 98
41144, V, 1, 1, 1, 1, 0, 700, 98
41145, V, 1, 1, 1, 1, 0, 700, 98
41146, V, 1, 1, 1, 1, 0, 700, 98
41147, V, 1, 1, 1, 1, 0, 700, 98
41148, V, 1, 1, 1, 1, 0, 700, 98
41149, V, 1, 1, 1, 1, 0, 700, 98
41150, V, 1, 1, 1, 1, 0, 700, 98
41151, V, 1, 1, 1, 1, 0, 700, 98
41152, V, 1, 1, 1, 1, 0, 700, 98
41153, V, 1, 1, 1, 1, 0, 700, 98
41154, V, 1, 1, 1, 1, 0, 700, 98
41155, V, 1, 1, 1, 1, 0, 700, 98
41156, V, 1, 1, 1, 1, 0, 700, 98
41157, V, 1, 1, 1, 1, 0, 700, 98
41158, V, 1, 1, 1, 1, 0, 700, 98
41159, V, 1, 1, 1, 1, 0, 700, 98
41160, V, 1, 1, 1, 1, 0, 700, 98
41161, V, 1, 1, 1, 1, 0, 700, 97
41162, V, 1, 1, 1, 1, 0, 700, 98
41163, V, 1, 1, 1, 1, 0, 700, 98
41164, V, 1, 1, 1, 1, 0, 700, 98
41165, V, 1, 1, 1, 1, 0, 700, 97
41166, V, 1, 1, 1, 1, 0, 700, 97
41167, V, 1, 1, 1, 1, 0, 700, 98
41168, V, 1, 1, 1, 1, 0, 700, 97
41169, V, 1, 1, 1, 1, 0, 700, 97
41170, V, 1, 1, 1, 1, 0, 700, 97
41171, V, 1, 1, 1, 1, 0, 700, 97
41172, V, 1, 1, 1, 1, 0, 700, 97
41174, V, 1, 1, 1, 1, 0, 700, 97
41175, V, 1, 1, 1, 1, 0, 700, 97
41176, V, 1, 1, 1, 1, 0, 700, 97
41177, V, 1, 1, 1, 1, 0, 700, 97
41178, V, 1, 1, 1, 1, 0, 700, 97
41179, V, 1, 1, 1, 1, 0, 700, 97
41180, V, 1, 1, 1, 1, 0, 700, 97
41181, V, 1, 1, 1, 1, 0, 700, 97
41182, V, 1, 1, 1, 1, 0, 700, 97
41183, V, 1, 1, 1, 1, 0, 700, 97
41184, V, 1, 1, 1, 1, 0, 700, 97
41185, V, 1, 1, 1, 1, 0, 700, 97
41186, V, 1, 1, 1, 1, 0, 700, 98
41187, V, 1, 1, 1, 1, 0, 700, 97
41188, V, 1, 1, 1, 1, 0, 700, 97
41189, V, 1, 1, 1, 1, 0, 700, 97
41190, V, 1, 1, 1, 1, 0, 700, 97
41191, V, 1, 1, 1, 1, 0, 700, 97
41192, V, 1, 1, 1, 1, 0, 700, 97
41193, V, 1, 1, 1, 1, 0, 700, 97
41194, V, 1, 1, 1, 1, 0, 700, 98
41195, V, 1, 1, 1, 1, 0, 700, 98
41196, V, 1, 1, 1, 1, 0, 700, 98
41197, V, 1, 1, 1, 1, 0, 700, 98
41198, V, 1, 1, 1, 1, 0, 700, 98
41199, V, 1, 1, 1, 1, 0, 700, 98
41200, V, 1, 1, 1, 1, 0, 700, 97
41201, V, 1, 1, 1, 1, 0, 700, 98
41202, V, 1, 1, 1, 1, 0, 700, 98
41203, V, 1, 1, 1, 1, 0, 700, 98
41204, V, 1, 1, 1, 1, 0, 700, 98
41205, V, 1, 1, 1, 1, 0, 700, 98
41206, V, 1, 1, 1, 1, 0, 700, 98
41207, V, 1, 1, 1, 1, 0, 700, 98
41208, V, 1, 1, 1, 1, 0, 700, 98
41209, V, 1, 1, 1, 1, 0, 700, 98
41210, V, 1, 1, 1, 1, 0, 700, 98
41211, V, 1, 1, 1, 1, 0, 700, 98
41212, V, 1, 1, 1, 1, 0, 700, 98
41213, V, 1, 1, 1, 1, 0, 700, 98
41214, V, 1, 1, 1, 1, 0, 700, 97
41216, V, 1, 1, 1, 1, 0, 700, 98
41217, V, 1, 1, 1, 1, 0, 700, 98
41218, V, 1, 1, 1, 1, 0, 700, 97
41219, V, 1, 1, 1, 1, 0, 700, 98
41220, V, 1, 1, 1, 1, 0, 700, 97
41221, V, 1, 1, 1, 1, 0, 700, 98
41222, V, 1, 1, 1, 1, 0, 700, 98
41223, V, 1, 1, 1, 1, 0, 700, 97
41224, V, 1, 1, 1, 1, 0, 700, 98
41225, V, 1, 1, 1, 1, 0, 700, 98
41226, V, 1, 1, 1, 1, 0, 700, 98
41227, V, 1, 1, 1, 1, 0, 700, 98
41228, V, 1, 1, 1, 1, 0, 700, 98
41229, V, 1, 1, 1, 1, 0, 700, 98
41230, V, 1, 1, 1, 1, 0, 700, 98
41231, V, 1, 1, 1, 1, 0, 700, 98
41232, V, 1, 1, 1, 1, 0, 700, 98
41233, V, 1, 1, 1, 1, 0, 700, 98
41234, V, 1, 1, 1, 1, 0, 700, 98
41235, V, 1, 1, 1, 1, 0, 700, 97
41236, V, 1, 1, 1, 1, 0, 700, 97
41237, V, 1, 1, 1, 1, 0, 700, 97
41238, V, 1, 1, 1, 1, 0, 700, 97
41239, V, 1, 1, 1, 1, 0, 700, 98
41240, V, 1, 1, 1, 1, 0, 700, 97
41241, V, 1, 1, 1, 1, 0, 700, 97
41242, V, 1, 1, 1, 1, 0, 700, 97
41243, V, 1, 1, 1, 1, 0, 700, 97
41244, V, 1, 1, 1, 1, 0, 700, 98
41245, V, 1, 1, 1, 1, 0, 700, 97
41246, V, 1, 1, 1, 1, 0, 700, 98
41247, V, 1, 1, 1, 1, 0, 700, 98
41248, V, 1, 1, 1, 1, 0, 700, 97
41249, V, 1, 1, 1, 1, 0, 700, 97
41250, V, 1, 1, 1, 1, 0, 700, 98
41251, V, 1, 1, 1, 1, 0, 700, 97
41252, V, 1, 1, 1, 1, 0, 700, 98
41253, V, 1, 1, 1, 1, 0, 700, 98
41254, V, 1, 1, 1, 1, 0, 700, 98
41255, V, 1, 1, 1, 1, 0, 700, 98
41256, V, 1, 1, 1, 1, 0, 700, 97
41257, V, 1, 1, 1, 1, 0, 700, 98
41259, V, 1, 1, 1, 1, 0, 700, 98
41260, V, 1, 1, 1, 1, 0, 700, 98
41261, V, 1, 1, 1, 1, 0, 700, 98
41262, V, 1, 1, 1, 1, 0, 700, 98
41263, V, 1, 1, 1, 1, 0, 700, 98
41264, V, 1, 1, 1, 1, 0, 700, 98
41265, V, 1, 1, 1, 1, 0, 700, 98
41266, V, 1, 1, 1, 1, 0, 700, 98
41267, V, 1, 1, 1, 1, 0, 700, 98
41268, V, 1, 1, 1, 1, 0, 700, 98
41269, V, 1, 1, 1, 1, 0, 700, 98
41270, V, 1, 1, 1, 1, 0, 700, 98
41271, V, 1, 1, 1, 1, 0, 700, 98
41272, V, 1, 1, 1, 1, 0, 700, 98
41273, V, 1, 1, 1, 1, 0, 700, 98
41274, V, 1, 1, 1, 1, 0, 700, 98
41275, V, 1, 1, 1, 1, 0, 700, 98
41276, V, 1, 1, 1, 1, 0, 700, 98
41277, V, 1, 1, 1, 1, 0, 700, 98
41278, V, 1, 1, 1, 1, 0, 700, 98
41279, V, 1, 1, 1, 1, 0, 700, 98
41280, V, 1, 1, 1, 1, 0, 700, 98
41281, V, 1, 1, 1, 1, 0, 700, 98
41282, V, 1, 1, 1, 1, 0, 700, 98
41283, V, 1, 1, 1, 1, 0, 700, 98
41284, V, 1, 1, 1, 1, 0, 700, 98
41285, V, 1, 1, 1, 1, 0, 700, 98
41286, V, 1, 1, 1, 1, 0, 700, 98
41287, V, 1, 1, 1, 1, 0, 700, 98
41288, V, 1, 1, 1, 1, 0, 700, 98
41289, V, 1, 1, 1, 1, 0, 700, 98
41290, V, 1, 1, 1, 1, 0, 700, 98
41291, V, 1, 1, 1, 1, 0, 700, 98
41292, V, 1, 1, 1, 1, 0, 700, 98
41293, V, 1, 1, 1, 1, 0, 700, 98
41294, V, 1, 1, 1, 1, 0, 700, 98
41295, V, 1, 1, 1, 1, 0, 700, 98
41296, V, 1, 1, 1, 1, 0, 700, 98
41297, V, 1, 1, 1, 1, 0, 700, 98
41298, V, 1, 1, 1, 1, 0, 700, 98
41299, V, 1, 1, 1, 1, 0, 700, 98
41300, V, 1, 1, 1, 1, 0, 700, 98
41302, V, 1, 1, 1, 1, 0, 700, 98
41303, V, 1, 1, 1, 1, 0, 700, 98
41304, V, 1, 1, 1, 1, 0, 700, 98
41305, V, 1, 1, 1, 1, 0, 700, 98
41306, V, 1, 1, 1, 1, 0, 700, 98
41307, V, 1, 1, 1, 1, 0, 700, 98
41308, V, 1, 1, 1, 1, 0, 700, 98
41309, V, 1, 1, 1, 1, 0, 700, 98
41310, V, 1, 1, 1, 1, 0, 700, 98
41311, V, 1, 1, 1, 1, 0, 700, 98
41312, V, 1, 1, 1, 1, 0, 700, 98
41313, V, 1, 1, 1, 1, 0, 700, 98
41314, V, 1, 1, 1, 1, 0, 700, 98
41315, V, 1, 1, 1, 1, 0, 700, 97
41316, V, 1, 1, 1, 1, 0, 700, 98
41317, V, 1, 1, 1, 1, 0, 700, 97
41318, V, 1, 1, 1, 1, 0, 700, 97
41319, V, 1, 1, 1, 1, 0, 700, 97
41320, V, 1, 1, 1, 1, 0, 700, 97
41321, V, 1, 1, 1, 1, 0, 700, 97
41322, V, 1, 1, 1, 1, 0, 700, 97
41323, V, 1, 1, 1, 1, 0, 700, 97
41324, V, 1, 1, 1, 1, 0, 700, 97
41325, V, 1, 1, 1, 1, 0, 700, 97
41326, V, 1, 1, 1, 1, 0, 700, 97
41327, V, 1, 1, 1, 1, 0, 700, 97
41328, V, 1, 1, 1, 1, 0, 700, 97
41329, V, 1, 1, 1, 1, 0, 700, 97
41330, V, 1, 1, 1, 1, 0, 700, 97
41331, V, 1, 1, 1, 1, 0, 700, 97
41332, V, 1, 1, 1, 1, 0, 700, 97
41333, V, 1, 1, 1, 1, 0, 700, 97
41334, V, 1, 1, 1, 1, 0, 700, 97
41335, V, 1, 1, 1, 1, 0, 700, 97
41336, V, 1, 1, 1, 1, 0, 700, 97
41337, V, 1, 1, 1, 1, 0, 700, 97
41338, V, 1, 1, 1, 1, 0, 700, 97
41339, V, 1, 1, 1, 1, 0, 700, 97
41340, V, 1, 1, 1, 1, 0, 700, 97
41341, V, 1, 1, 1, 1, 0, 700, 97
41342, V, 1, 1, 1, 1, 0, 700, 97
41344, V, 1, 1, 1, 1, 0, 700, 97
41345, V, 1, 1, 1, 1, 0, 700, 97
41346, V, 1, 1, 1, 1, 0, 700, 97
41347, V, 1, 1, 1, 1, 0, 700, 97
41348, V, 1, 1, 1, 1, 0, 700, 97
41349, V, 1, 1, 1, 1, 0, 700, 97
41350, V, 1, 1, 1, 1, 0, 700, 97
41351, V, 1, 1, 1, 1, 0, 700, 98
41352, V, 1, 1, 1, 1, 0, 700, 97
41353, V, 1, 1, 1, 1, 0, 700, 97
41354, V, 1, 1, 1, 1, 0, 700, 97
41355, V, 1, 1, 1, 1, 0, 700, 98
41356, V, 1, 1, 1, 1, 0, 700, 98
41357, V, 1, 1, 1, 1, 0, 700, 97
41358, V, 1, 1, 1, 1, 0, 700, 98
41359, V, 1, 1, 1, 1, 0, 700, 98
41360, V, 1, 1, 1, 1, 0, 700, 98
41361, V, 1, 1, 1, 1, 0, 700, 97
41362, V, 1, 1, 1, 1, 0, 700, 98
41363, V, 1, 1, 1, 1, 0, 700, 98
41364, V, 1, 1, 1, 1, 0, 700, 97
41365, V, 1, 1, 1, 1, 0, 700, 98
41366, V, 1, 1, 1, 1, 0, 700, 98
41367, V, 1, 1, 1, 1, 0, 700, 98
41368, V, 1, 1, 1, 1, 0, 700, 98
41369, V, 1, 1, 1, 1, 0, 700, 98
41370, V, 1, 1, 1, 1, 0, 700, 97
41371, V, 1, 1, 1, 1, 0, 700, 98
41372, V, 1, 1, 1, 1, 0, 700, 98
41373, V, 1, 1, 1, 1, 0, 700, 97
41374, V, 1, 1, 1, 1, 0, 700, 98
41375, V, 1, 1, 1, 1, 0, 700, 98
41376, V, 1, 1, 1, 1, 0, 700, 98
41377, V, 1, 1, 1, 1, 0, 700, 98
41378, V, 1, 1, 1, 1, 0, 700, 98
41379, V, 1, 1, 1, 1, 0, 700, 98
41380, V, 1, 1, 1, 1, 0, 700, 98
41381, V, 1, 1, 1, 1, 0, 700, 98
41382, V, 1, 1, 1, 1, 0, 700, 97
41383, V, 1, 1, 1, 1, 0, 700, 98
41384, V, 1, 1, 1, 1, 0, 700, 98
41385, V, 1, 1, 1, 1, 0, 700, 98
41387, V, 1, 1, 1, 1, 0, 700, 98
41388, V, 1, 1, 1, 1, 0, 700, 98
41389, V, 1, 1, 1, 1, 0, 700, 97
41390, V, 1, 1, 1, 1, 0, 700, 98
41391, V, 1, 1, 1, 1, 0, 700, 97
41392, V, 1, 1, 1, 1, 0, 700, 97
41393, V, 1, 1, 1, 1, 0, 700, 97
41394, V, 1, 1, 1, 1, 0, 700, 97
41395, V, 1, 1, 1, 1, 0, 700, 97
41396, V, 1, 1, 1, 1, 0, 700, 97
41397, V, 1, 1, 1, 1, 0, 700, 97
41398, V, 1, 1, 1, 1, 0, 700, 97
41399, V, 1, 1, 1, 1, 0, 700, 97
41400, V, 1, 1, 1, 1, 0, 700, 97
41401, V, 1, 1, 1, 1, 0, 700, 97
41402, V, 1, 1, 1, 1, 0, 700, 97
41403, V, 1, 1, 1, 1, 0, 700, 97
41404, V, 1, 1, 1, 1, 0, 700, 97
41405, V, 1, 1, 1, 1, 0, 700, 97
41406, V, 1, 1, 1, 1, 0, 700, 97
41407, V, 1, 1, 1, 1, 0, 700, 97
41408, V, 1, 1, 1, 1, 0, 700, 97
41409, V, 1, 1, 1, 1, 0, 700, 97
41410, V, 1, 1, 1, 1, 0, 700, 97
41411, V, 1, 1, 1, 1, 0, 700, 97
41412, V, 1, 1, 1, 1, 0, 700, 97
41413, V, 1, 1, 1, 1, 0, 700, 97
41414, V, 1, 1, 1, 1, 0, 700, 97
41415, V, 1, 1, 1, 1, 0, 700, 97
41416, V, 1, 1, 1, 1, 0, 700, 97
41417, V, 1, 1, 1, 1, 0, 700, 97
41418, V, 1, 1, 1, 1, 0, 700, 97
41419, V, 1, 1, 1, 1, 0, 700, 97
41420, V, 1, 1, 1, 1, 0, 700, 97
41421, V, 1, 1, 1, 1, 0, 700, 97
41422, V, 1, 1, 1, 1, 0, 700, 97
41423, V, 1, 1, 1, 1, 0, 700, 98
41424, V, 1, 1, 1, 1, 0, 700, 98
41425, V, 1, 1, 1, 1, 0, 700, 97
41426, V, 1, 1, 1, 1, 0, 700, 98
41427, V, 1, 1, 1, 1, 0, 700, 97
41428, V, 1, 1, 1, 1, 0, 700, 98
41430, V, 1, 1, 1, 1, 0, 700, 98
41431, V, 1, 1, 1, 1, 0, 700, 98
41432, V, 1, 1, 1, 1, 0, 700, 98
41433, V, 1, 1, 1, 1, 0, 700, 97
41434, V, 1, 1, 1, 1, 0, 700, 98
41435, V, 1, 1, 1, 1, 0, 700, 98
41436, V, 1, 1, 1, 1, 0, 700, 98
41437, V, 1, 1, 1, 1, 0, 700, 98
41438, V, 1, 1, 1, 1, 0, 700, 98
41439, V, 1, 1, 1, 1, 0, 700, 98
41440, V, 1, 1, 1, 1, 0, 700, 98
41441, V, 1, 1, 1, 1, 0, 700, 98
41442, V, 1, 1, 1, 1, 0, 700, 98
41443, V, 1, 1, 1, 1, 0, 700, 98
41444, V, 1, 1, 1, 1, 0, 700, 98
41445, V, 1, 1, 1, 1, 0, 700, 98
41446, V, 1, 1, 1, 1, 0, 700, 98
41447, V, 1, 1, 1, 1, 0, 700, 98
41448, V, 1, 1, 1, 1, 0, 700, 98
41449, V, 1, 1, 1, 1, 0, 700, 98
41450, V, 1, 1, 1, 1, 0, 700, 98
41451, V, 1, 1, 1, 1, 0, 700, 98
41452, V, 1, 1, 1, 1, 0, 700, 98
41453, V, 1, 1, 1, 1, 0, 700, 98
41454, V, 1, 1, 1, 1, 0, 700, 98
41455, V, 1, 1, 1, 1, 0, 700, 98
41456, V, 1, 1, 1, 1, 0, 700, 97
41457, V, 1, 1, 1, 1, 0, 700, 97
41458, V, 1, 1, 1, 1, 0, 700, 98
41459, V, 1, 1, 1, 1, 0, 700, 98
41460, V, 1, 1, 1, 1, 0, 700, 98
41461, V, 1, 1, 1, 1, 0, 700, 98
41462, V, 1, 1, 1, 1, 0, 700, 98
41463, V, 1, 1, 1, 1, 0, 700, 98
41464, V, 1, 1, 1, 1, 0, 700, 98
41465, V, 1, 1, 1, 1, 0, 700, 98
41466, V, 1, 1, 1, 1, 0, 700, 97
41467, V, 1, 1, 1, 1, 0, 700, 98
41468, V, 1, 1, 1, 1, 0, 700, 98
41469, V, 1, 1, 1, 1, 0, 700, 98
41470, V, 1, 1, 1, 1, 0, 700, 97
41472, V, 1, 1, 1, 1, 0, 700, 98
41473, V, 1, 1, 1, 1, 0, 700, 97
41474, V, 1, 1, 1, 1, 0, 700, 97
41475, V, 1, 1, 1, 1, 0, 700, 97
41476, V, 1, 1, 1, 1, 0, 700, 97
41477, V, 1, 1, 1, 1, 0, 700, 97
41478, V, 1, 1, 1, 1, 0, 700, 97
41479, V, 1, 1, 1, 1, 0, 700, 97
41480, V, 1, 1, 1, 1, 0, 700, 97
41481, V, 1, 1, 1, 1, 0, 700, 97
41482, V, 1, 1, 1, 1, 0, 700, 97
41483, V, 1, 1, 1, 1, 0, 700, 97
41484, V, 1, 1, 1, 1, 0, 700, 97
41485, V, 1, 1, 1, 1, 0, 700, 97
41486, V, 1, 1, 1, 1, 0, 700, 97
41487, V, 1, 1, 1, 1, 0, 700, 97
41488, V, 1, 1, 1, 1, 0, 700, 97
41489, V, 1, 1, 1, 1, 0, 700, 97
41490, V, 1, 1, 1, 1, 0, 700, 97
41491, V, 1, 1, 1, 1, 0, 700, 97
41492, V, 1, 1, 1, 1, 0, 700, 97
41493, V, 1, 1, 1, 1, 0, 700, 97
41494, V, 1, 1, 1, 1, 0, 700, 97
41495, V, 1, 1, 1, 1, 0, 700, 97
41496, V, 1, 1, 1, 1, 0, 700, 97
41497, V, 1, 1, 1, 1, 0, 700, 97
41498, V, 1, 1, 1, 1, 0, 700, 97
41499, V, 1, 1, 1, 1, 0, 700, 97
41500, V, 1, 1, 1, 1, 0, 700, 98
41501, V, 1, 1, 1, 1, 0, 700, 97
41502, V, 1, 1, 1, 1, 0, 700, 97
41503, V, 1, 1, 1, 1, 0, 700, 97
41504, V, 1, 1, 1, 1, 0, 700, 97
41505, V, 1, 1, 1, 1, 0, 700, 97
41506, V, 1, 1, 1, 1, 0, 700, 97
41507, V, 1, 1, 1, 1, 0, 700, 97
41508, V, 1, 1, 1, 1, 0, 700, 98
41509, V, 1, 1, 1, 1, 0, 700, 98
41510, V, 1, 1, 1, 1, 0, 700, 98
41511, V, 1, 1, 1, 1, 0, 700, 98
41512, V, 1, 1, 1, 1, 0, 700, 97
41513, V, 1, 1, 1, 1, 0, 700, 98
41515, V, 1, 1, 1, 1, 0, 700, 98
41516, V, 1, 1, 1, 1, 0, 700, 97
41517, V, 1, 1, 1, 1, 0, 700, 98
41518, V, 1, 1, 1, 1, 0, 700, 97
41519, V, 1, 1, 1, 1, 0, 700, 97
41520, V, 1, 1, 1, 1, 0, 700, 97
41521, V, 1, 1, 1, 1, 0, 700, 98
41522, V, 1, 1, 1, 1, 0, 700, 97
41523, V, 1, 1, 1, 1, 0, 700, 97
41524, V, 1, 1, 1, 1, 0, 700, 97
41525, V, 1, 1, 1, 1, 0, 700, 97
41526, V, 1, 1, 1, 1, 0, 700, 98
41527, V, 1, 1, 1, 1, 0, 700, 98
41528, V, 1, 1, 1, 1, 0, 700, 98
41529, V, 1, 1, 1, 1, 0, 700, 97
41530, V, 1, 1, 1, 1, 0, 700, 98
41531, V, 1, 1, 1, 1, 0, 700, 98
41532, V, 1, 1, 1, 1, 0, 700, 97
41533, V, 1, 1, 1, 1, 0, 700, 98
41534, V, 1, 1, 1, 1, 0, 700, 98
41535, V, 1, 1, 1, 1, 0, 700, 98
41536, V, 1, 1, 1, 1, 0, 700, 97
41537, V, 1, 1, 1, 1, 0, 700, 97
41538, V, 1, 1, 1, 1, 0, 700, 97
41539, V, 1, 1, 1, 1, 0, 700, 97
41540, V, 1, 1, 1, 1, 0, 700, 98
41541, V, 1, 1, 1, 1, 0, 700, 98
41542, V, 1, 1, 1, 1, 0, 700, 97
41543, V, 1, 1, 1, 1, 0, 700, 97
41544, V, 1, 1, 1, 1, 0, 700, 98
41545, V, 1, 1, 1, 1, 0, 700, 98
41546, V, 1, 1, 1, 1, 0, 700, 97
41547, V, 1, 1, 1, 1, 0, 700, 97
41548, V, 1, 1, 1, 1, 0, 700, 97
41549, V, 1, 1, 1, 1, 0, 700, 97
41550, V, 1, 1, 1, 1, 0, 700, 97
41551, V, 1, 1, 1, 1, 0, 700, 98
41552, V, 1, 1, 1, 1, 0, 700, 97
41553, V, 1, 1, 1, 1, 0, 700, 97
41554, V, 1, 1, 1, 1, 0, 700, 97
41555, V, 1, 1, 1, 1, 0, 700, 97
41556, V, 1, 1, 1, 1, 0, 700, 97
41558, V, 1, 1, 1, 1, 0, 700, 97
41559, V, 1, 1, 1, 1, 0, 700, 97
41560, V, 1, 1, 1, 1, 0, 700, 97
41561, V, 1, 1, 1, 1, 0, 700, 97
41562, V, 1, 1, 1, 1, 0, 700, 97
41563, V, 1, 1, 1, 1, 0, 700, 97
41564, V, 1, 1, 1, 1, 0, 700, 97
41565, V, 1, 1, 1, 1, 0, 700, 97
41566, V, 1, 1, 1, 1, 0, 700, 97
41567, V, 1, 1, 1, 1, 0, 700, 97
41568, V, 1, 1, 1, 1, 0, 700, 97
41569, V, 1, 1, 1, 1, 0, 700, 97
41570, V, 1, 1, 1, 1, 0, 700, 97
41571, V, 1, 1, 1, 1, 0, 700, 97
41572, V, 1, 1, 1, 1, 0, 700, 97
41573, V, 1, 1, 1, 1, 0, 700, 98
41574, V, 1, 1, 1, 1, 0, 700, 97
41575, V, 1, 1, 1, 1, 0, 700, 97
41576, V, 1, 1, 1, 1, 0, 700, 97
41577, V, 1, 1, 1, 1, 0, 700, 97
41578, V, 1, 1, 1, 1, 0, 700, 97
41579, V, 1, 1, 1, 1, 0, 700, 97
41580, V, 1, 1, 1, 1, 0, 700, 98
41581, V, 1, 1, 1, 1, 0, 700, 98
41582, V, 1, 1, 1, 1, 0, 700, 98
41583, V, 1, 1, 1, 1, 0, 700, 98
41584, V, 1, 1, 1, 1, 0, 700, 98
41585, V, 1, 1, 1, 1, 0, 700, 97
41586, V, 1, 1, 1, 1, 0, 700, 98
41587, V, 1, 1, 1, 1, 0, 700, 98
41588, V, 1, 1, 1, 1, 0, 700, 98
41589, V, 1, 1, 1, 1, 0, 700, 98
41590, V, 1, 1, 1, 1, 0, 700, 98
41591, V, 1, 1, 1, 1, 0, 700, 98
41592, V, 1, 1, 1, 1, 0, 700, 98
41593, V, 1, 1, 1, 1, 0, 700, 98
41594, V, 1, 1, 1, 1, 0, 700, 97
41595, V, 1, 1, 1, 1, 0, 700, 97
41596, V, 1, 1, 1, 1, 0, 700, 98
41597, V, 1, 1, 1, 1, 0, 700, 98
41598, V, 1, 1, 1, 1, 0, 700, 97
41600, V, 1, 1, 1, 1, 0, 700, 97
41601, V, 1, 1, 1, 1, 0, 700, 98
41602, V, 1, 1, 1, 1, 0, 700, 98
41603, V, 1, 1, 1, 1, 0, 700, 98
41604, V, 1, 1, 1, 1, 0, 700, 98
41605, V, 1, 1, 1, 1, 0, 700, 98
41606, V, 1, 1, 1, 1, 0, 700, 98
41607, V, 1, 1, 1, 1, 0, 700, 98
41608, V, 1, 1, 1, 1, 0, 700, 98
41609, V, 1, 1, 1, 1, 0, 700, 98
41610, V, 1, 1, 1, 1, 0, 700, 98
41611, V, 1, 1, 1, 1, 0, 700, 98
41612, V, 1, 1, 1, 1, 0, 700, 97
41613, V, 1, 1, 1, 1, 0, 700, 97
41614, V, 1, 1, 1, 1, 0, 700, 98
41615, V, 1, 1, 1, 1, 0, 700, 97
41616, V, 1, 1, 1, 1, 0, 700, 97
41617, V, 1, 1, 1, 1, 0, 700, 97
41618, V, 1, 1, 1, 1, 0, 700, 97
41619, V, 1, 1, 1, 1, 0, 700, 97
41620, V, 1, 1, 1, 1, 0, 700, 97
41621, V, 1, 1, 1, 1, 0, 700, 97
41622, V, 1, 1, 1, 1, 0, 700, 97
41623, V, 1, 1, 1, 1, 0, 700, 97
41624, V, 1, 1, 1, 1, 0, 700, 97
41625, V, 1, 1, 1, 1, 0, 700, 97
41626, V, 1, 1, 1, 1, 0, 700, 97
41627, V, 1, 1, 1, 1, 0, 700, 97
41628, V, 1, 1, 1, 1, 0, 700, 97
41629, V, 1, 1, 1, 1, 0, 700, 97
41630, V, 1, 1, 1, 1, 0, 700, 97
41631, V, 1, 1, 1, 1, 0, 700, 97
41632, V, 1, 1, 1, 1, 0, 700, 97
41633, V, 1, 1, 1, 1, 0, 700, 97
41634, V, 1, 1, 1, 1, 0, 700, 97
41635, V, 1, 1, 1, 1, 0, 700, 97
41636, V, 1, 1, 1, 1, 0, 700, 97
41637, V, 1, 1, 1, 1, 0, 700, 97
41638, V, 1, 1, 1, 1, 0, 700, 97
41639, V, 1, 1, 1, 1, 0, 700, 97
41640, V, 1, 1, 1, 1, 0, 700, 97
41641, V, 1, 1, 1, 1, 0, 700, 97
41643, V, 1, 1, 1, 1, 0, 700, 97
41644, V, 1, 1, 1, 1, 0, 700, 97
41645, V, 1, 1, 1, 1, 0, 700, 97
41646, V, 1, 1, 1, 1, 0, 700, 97
41647, V, 1, 1, 1, 1, 0, 700, 97
41648, V, 1, 1, 1, 1, 0, 700, 97
41649, V, 1, 1, 1, 1, 0, 700, 97
41650, V, 1, 1, 1, 1, 0, 700, 97
41651, V, 1, 1, 1, 1, 0, 700, 97
41652, V, 1, 1, 1, 1, 0, 700, 97
41653, V, 1, 1, 1, 1, 0, 700, 97
41654, V, 1, 1, 1, 1, 0, 700, 97
41655, V, 1, 1, 1, 1, 0, 700, 97
41656, V, 1, 1, 1, 1, 0, 700, 97
41657, V, 1, 1, 1, 1, 0, 700, 97
41658, V, 1, 1, 1, 1, 0, 700, 97
41659, V, 1, 1, 1, 1, 0, 700, 97
41660, V, 1, 1, 1, 1, 0, 700, 97
41661, V, 1, 1, 1, 1, 0, 700, 97
41662, V, 1, 1, 1, 1, 0, 700, 98
41663, V, 1, 1, 1, 1, 0, 700, 97
41664, V, 1, 1, 1, 1, 0, 700, 97
41665, V, 1, 1, 1, 1, 0, 700, 98
41666, V, 1, 1, 1, 1, 0, 700, 98
41667, V, 1, 1, 1, 1, 0, 700, 98
41668, V, 1, 1, 1, 1, 0, 700, 98
41669, V, 1, 1, 1, 1, 0, 700, 98
41670, V, 1, 1, 1, 1, 0, 700, 97
41671, V, 1, 1, 1, 1, 0, 700, 98
41672, V, 1, 1, 1, 1, 0, 700, 97
41673, V, 1, 1, 1, 1, 0, 700, 97
41674, V, 1, 1, 1, 1, 0, 700, 97
41675, V, 1, 1, 1, 1, 0, 700, 97
41676, V, 1, 1, 1, 1, 0, 700, 97
41677, V, 1, 1, 1, 1, 0, 700, 97
41678, V, 1, 1, 1, 1, 0, 700, 98
41679, V, 1, 1, 1, 1, 0, 700, 98
41680, V, 1, 1, 1, 1, 0, 700, 97
41681, V, 1, 1, 1, 1, 0, 700, 97
41682, V, 1, 1, 1, 1, 0, 700, 97
41683, V, 1, 1, 1, 1, 0, 700, 97
41684, V, 1, 1, 1, 1, 0, 700, 97
41686, V, 1, 1, 1, 1, 0, 700, 97
41687, V, 1, 1, 1, 1, 0, 700, 97
41688, V, 1, 1, 1, 1, 0, 700, 98
41689, V, 1, 1, 1, 1, 0, 700, 97
41690, V, 1, 1, 1, 1, 0, 700, 97
41691, V, 1, 1, 1, 1, 0, 700, 97
41692, V, 1, 1, 1, 1, 0, 700, 98
41693, V, 1, 1, 1, 1, 0, 700, 97
41694, V, 1, 1, 1, 1, 0, 700, 97
41695, V, 1, 1, 1, 1, 0, 700, 97
41696, V, 1, 1, 1, 1, 0, 700, 97
41697, V, 1, 1, 1, 1, 0, 700, 97
41698, V, 1, 1, 1, 1, 0, 700, 97
41699, V, 1, 1, 1, 1, 0, 700, 97
41700, V, 1, 1, 1, 1, 0, 700, 97
41701, V, 1, 1, 1, 1, 0, 700, 97
41702, V, 1, 1, 1, 1, 0, 700, 97
41703, V, 1, 1, 1, 1, 0, 700, 97
41704, V, 1, 1, 1, 1, 0, 700, 97
41705, V, 1, 1, 1, 1, 0, 700, 97
41706, V, 1, 1, 1, 1, 0, 700, 97
41707, V, 1, 1, 1, 1, 0, 700, 97
41708, V, 1, 1, 1, 1, 0, 700, 97
41709, V, 1, 1, 1, 1, 0, 700, 97
41710, V, 1, 1, 1, 1, 0, 700, 97
41711, V, 1, 1, 1, 1, 0, 700, 97
41712, V, 1, 1, 1, 1, 0, 700, 97
41713, V, 1, 1, 1, 1, 0, 700, 97
41714, V, 1, 1, 1, 1, 0, 700, 97
41715, V, 1, 1, 1, 1, 0, 700, 97
41716, V, 1, 1, 1, 1, 0, 700, 97
41717, V, 1, 1, 1, 1, 0, 700, 97
41718, V, 1, 1, 1, 1, 0, 700, 97
41719, V, 1, 1, 1, 1, 0, 700, 97
41720, V, 1, 1, 1, 1, 0, 700, 97
41721, V, 1, 1, 1, 1, 0, 700, 97
41722, V, 1, 1, 1, 1, 0, 700, 97
41723, V, 1, 1, 1, 1, 0, 700, 97
41724, V, 1, 1, 1, 1, 0, 700, 97
41725, V, 1, 1, 1, 1, 0, 700, 97
41726, V, 1, 1, 1, 1, 0, 700, 97
41728, V, 1, 1, 1, 1, 0, 700, 97
41729, V, 1, 1, 1, 1, 0, 700, 97
41730, V, 1, 1, 1, 1, 0, 700, 97
41731, V, 1, 1, 1, 1, 0, 700, 97
41732, V, 1, 1, 1, 1, 0, 700, 97
41733, V, 1, 1, 1, 1, 0, 700, 97
41734, V, 1, 1, 1, 1, 0, 700, 97
41735, V, 1, 1, 1, 1, 0, 700, 97
41736, V, 1, 1, 1, 1, 0, 700, 97
41737, V, 1, 1, 1, 1, 0, 700, 97
41738, V, 1, 1, 1, 1, 0, 700, 97
41739, V, 1, 1, 1, 1, 0, 700, 97
41740, V, 1, 1, 1, 1, 0, 700, 98
41741, V, 1, 1, 1, 1, 0, 700, 97
41742, V, 1, 1, 1, 1, 0, 700, 97
41743, V, 1, 1, 1, 1, 0, 700, 97
41744, V, 1, 1, 1, 1, 0, 700, 97
41745, V, 1, 1, 1, 1, 0, 700, 97
41746, V, 1, 1, 1, 1, 0, 700, 97
41747, V, 1, 1, 1, 1, 0, 700, 97
41748, V, 1, 1, 1, 1, 0, 700, 97
41749, V, 1, 1, 1, 1, 0, 700, 97
41750, V, 1, 1, 1, 1, 0, 700, 97
41751, V, 1, 1, 1, 1, 0, 700, 97
41752, V, 1, 1, 1, 1, 0, 700, 97
41753, V, 1, 1, 1, 1, 0, 700, 97
41754, V, 1, 1, 1, 1, 0, 700, 97
41755, V, 1, 1, 1, 1, 0, 700, 97
41756, V, 1, 1, 1, 1, 0, 700, 97
41757, V, 1, 1, 1, 1, 0, 700, 97
41758, V, 1, 1, 1, 1, 0, 700, 97
41759, V, 1, 1, 1, 1, 0, 700, 97
41760, V, 1, 1, 1, 1, 0, 700, 97
41761, V, 1, 1, 1, 1, 0, 700, 97
41762, V, 1, 1, 1, 1, 0, 700, 97
41763, V, 1, 1, 1, 1, 0, 700, 97
41764, V, 1, 1, 1, 1, 0, 700, 97
41765, V, 1, 1, 1, 1, 0, 700, 97
41766, V, 1, 1, 1, 1, 0, 700, 97
41767, V, 1, 1, 1, 1, 0, 700, 97
41768, V, 1, 1, 1, 1, 0, 700, 97
41769, V, 1, 1, 1, 1, 0, 700, 97
41771, V, 1, 1, 1, 1, 0, 700, 97
41772, V, 1, 1, 1, 1, 0, 700, 97
41773, V, 1, 1, 1, 1, 0, 700, 97
41774, V, 1, 1, 1, 1, 0, 700, 97
41775, V, 1, 1, 1, 1, 0, 700, 97
41776, V, 1, 1, 1, 1, 0, 700, 97
41777, V, 1, 1, 1, 1, 0, 700, 97
41778, V, 1, 1, 1, 1, 0, 700, 97
41779, V, 1, 1, 1, 1, 0, 700, 97
41780, V, 1, 1, 1, 1, 0, 700, 97
41781, V, 1, 1, 1, 1, 0, 700, 97
41782, V, 1, 1, 1, 1, 0, 700, 97
41783, V, 1, 1, 1, 1, 0, 700, 97
41784, V, 1, 1, 1, 1, 0, 700, 97
41785, V, 1, 1, 1, 1, 0, 700, 97
41786, V, 1, 1, 1, 1, 0, 700, 97
41787, V, 1, 1, 1, 1, 0, 700, 97
41788, V, 1, 1, 1, 1, 0, 700, 97
41789, V, 1, 1, 1, 1, 0, 700, 97
41790, V, 1, 1, 1, 1, 0, 700, 97
41791, V, 1, 1, 1, 1, 0, 700, 97
41792, V, 1, 1, 1, 1, 0, 700, 97
41793, V, 1, 1, 1, 1, 0, 700, 97
41794, V, 1, 1, 1, 1, 0, 700, 97
41795, V, 1, 1, 1, 1, 0, 700, 97
41796, V, 1, 1, 1, 1, 0, 700, 97
41797, V, 1, 1, 1, 1, 0, 700, 97
41798, V, 1, 1, 1, 1, 0, 700, 97
41799, V, 1, 1, 1, 1, 0, 700, 97
41800, V, 1, 1, 1, 1, 0, 700, 97
41801, V, 1, 1, 1, 1, 0, 700, 97
41802, V, 1, 1, 1, 1, 0, 700, 97
41803, V, 1, 1, 1, 1, 0, 700, 97
41804, V, 1, 1, 1, 1, 0, 700, 97
41805, V, 1, 1, 1, 1, 0, 700, 97
41806, V, 1, 1, 1, 1, 0, 700, 97
41807, V, 1, 1, 1, 1, 0, 700, 97
41808, V, 1, 1, 1, 1, 0, 700, 97
41809, V, 1, 1, 1, 1, 0, 700, 97
41810, V, 1, 1, 1, 1, 0, 700, 97
41811, V, 1, 1, 1, 1, 0, 700, 97
41812, V, 1, 1, 1, 1, 0, 700, 97
41814, V, 1, 1, 1, 1, 0, 700, 97
41815, V, 1, 1, 1, 1, 0, 700, 97
41816, V, 1, 1, 1, 1, 0, 700, 97
41817, V, 1, 1, 1, 1, 0, 700, 97
41818, V, 1, 1, 1, 1, 0, 700, 97
41819, V, 1, 1, 1, 1, 0, 700, 97
41820, V, 1, 1, 1, 1, 0, 700, 97
41821, V, 1, 1, 1, 1, 0, 700, 97
41822, V, 1, 1, 1, 1, 0, 700, 97
41823, V, 1, 1, 1, 1, 0, 700, 97
41824, V, 1, 1, 1, 1, 0, 700, 97
41825, V, 1, 1, 1, 1, 0, 700, 97
41826, V, 1, 1, 1, 1, 0, 700, 97
41827, V, 1, 1, 1, 1, 0, 700, 97
41828, V, 1, 1, 1, 1, 0, 700, 97
41829, V, 1, 1, 1, 1, 0, 700, 97
41830, V, 1, 1, 1, 1, 0, 700, 97
41831, V, 1, 1, 1, 1, 0, 700, 97
41832, V, 1, 1, 1, 1, 0, 700, 97
41833, V, 1, 1, 1, 1, 0, 700, 97
41834, V, 1, 1, 1, 1, 0, 700, 97
41835, V, 1, 1, 1, 1, 0, 700, 97
41836, V, 1, 1, 1, 1, 0, 700, 97
41837, V, 1, 1, 1, 1, 0, 700, 97
41838, V, 1, 1, 1, 1, 0, 700, 97
41839, V, 1, 1, 1, 1, 0, 700, 97
41840, V, 1, 1, 1, 1, 0, 700, 97
41841, V, 1, 1, 1, 1, 0, 700, 97
41842, V, 1, 1, 1, 1, 0, 700, 97
41843, V, 1, 1, 1, 1, 0, 700, 97
41844, V, 1, 1, 1, 1, 0, 700, 97
41845, V, 1, 1, 1, 1, 0, 700, 97
41846, V, 1, 1, 1, 1, 0, 700, 97
41847, V, 1, 1, 1, 1, 0, 700, 97
41848, V, 1, 1, 1, 1, 0, 700, 97
41849, V, 1, 1, 1, 1, 0, 700, 97
41850, V, 1, 1, 1, 1, 0, 700, 97
41851, V, 1, 1, 1, 1, 0, 700, 97
41852, V, 1, 1, 1, 1, 0, 700, 97
41853, V, 1, 1, 1, 1, 0, 700, 97
41854, V, 1, 1, 1, 1, 0, 700, 97
41856, V, 1, 1, 1, 1, 0, 700, 97
41857, V, 1, 1, 1, 1, 0, 700, 97
41858, V, 1, 1, 1, 1, 0, 700, 97
41859, V, 1, 1, 1, 1, 0, 700, 97
41860, V, 1, 1, 1, 1, 0, 700, 97
41861, V, 1, 1, 1, 1, 0, 700, 97
41862, V, 1, 1, 1, 1, 0, 700, 97
41863, V, 1, 1, 1, 1, 0, 700, 97
41864, V, 1, 1, 1, 1, 0, 700, 97
41865, V, 1, 1, 1, 1, 0, 700, 97
41866, V, 1, 1, 1, 1, 0, 700, 97
41867, V, 1, 1, 1, 1, 0, 700, 97
41868, V, 1, 1, 1, 1, 0, 700, 97
41869, V, 1, 1, 1, 1, 0, 700, 97
41870, V, 1, 1, 1, 1, 0, 700, 97
41871, V, 1, 1, 1, 1, 0, 700, 97
41872, V, 1, 1, 1, 1, 0, 700, 97
41873, V, 1, 1, 1, 1, 0, 700, 97
41874, V, 1, 1, 1, 1, 0, 700, 97
41875, V, 1, 1, 1, 1, 0, 700, 97
41876, V, 1, 1, 1, 1, 0, 700, 97
41877, V, 1, 1, 1, 1, 0, 700, 97
41878, V, 1, 1, 1, 1, 0, 700, 97
41879, V, 1, 1, 1, 1, 0, 700, 97
41880, V, 1, 1, 1, 1, 0, 700, 97
41881, V, 1, 1, 1, 1, 0, 700, 97
41882, V, 1, 1, 1, 1, 0, 700, 97
41883, V, 1, 1, 1, 1, 0, 700, 97
41884, V, 1, 1, 1, 1, 0, 700, 97
41885, V, 1, 1, 1, 1, 0, 700, 97
41886, V, 1, 1, 1, 1, 0, 700, 97
41887, V, 1, 1, 1, 1, 0, 700, 97
41888, V, 1, 1, 1, 1, 0, 700, 97
41889, V, 1, 1, 1, 1, 0, 700, 97
41890, V, 1, 1, 1, 1, 0, 700, 97
41891, V, 1, 1, 1, 1, 0, 700, 97
41892, V, 1, 1, 1, 1, 0, 700, 97
41893, V, 1, 1, 1, 1, 0, 700, 97
41894, V, 1, 1, 1, 1, 0, 700, 97
41895, V, 1, 1, 1, 1, 0, 700, 97
41896, V, 1, 1, 1, 1, 0, 700, 97
41897, V, 1, 1, 1, 1, 0, 700, 97
41899, V, 1, 1, 1, 1, 0, 700, 97
41900, V, 1, 1, 1, 1, 0, 700, 97
41901, V, 1, 1, 1, 1, 0, 700, 97
41902, V, 1, 1, 1, 1, 0, 700, 97
41903, V, 1, 1, 1, 1, 0, 700, 97
41904, V, 1, 1, 1, 1, 0, 700, 97
41905, V, 1, 1, 1, 1, 0, 700, 97
41906, V, 1, 1, 1, 1, 0, 700, 97
41907, V, 1, 1, 1, 1, 0, 700, 97
41908, V, 1, 1, 1, 1, 0, 700, 97
41909, V, 1, 1, 1, 1, 0, 700, 97
41910, V, 1, 1, 1, 1, 0, 700, 97
41911, V, 1, 1, 1, 1, 0, 700, 97
41912, V, 1, 1, 1, 1, 0, 700, 97
41913, V, 1, 1, 1, 1, 0, 700, 97
41914, V, 1, 1, 1, 1, 0, 700, 97
41915, V, 1, 1, 1, 1, 0, 700, 97
41916, V, 1, 1, 1, 1, 0, 700, 97
41917, V, 1, 1, 1, 1, 0, 700, 97
41918, V, 1, 1, 1, 1, 0, 700, 97
41919, V, 1, 1, 1, 1, 0, 700, 97
41920, V, 1, 1, 1, 1, 0, 700, 97
41921, V, 1, 1, 1, 1, 0, 700, 97
41922, V, 1, 1, 1, 1, 0, 700, 97
41923, V, 1, 1, 1, 1, 0, 700, 97
41924, V, 1, 1, 1, 1, 0, 700, 97
41925, V, 1, 1, 1, 1, 0, 700, 97
41926, V, 1, 1, 1, 1, 0, 700, 97
41927, V, 1, 1, 1, 1, 0, 700, 97
41928, V, 1, 1, 1, 1, 0, 700, 97
41929, V, 1, 1, 1, 1, 0, 700, 97
41930, V, 1, 1, 1, 1, 0, 700, 97
41931, V, 1, 1, 1, 1, 0, 700, 97
41932, V, 1, 1, 1, 1, 0, 700, 97
41933, V, 1, 1, 1, 1, 0, 700, 97
41934, V, 1, 1, 1, 1, 0, 700, 97
41935, V, 1, 1, 1, 1, 0, 700, 97
41936, V, 1, 1, 1, 1, 0, 700, 97
41937, V, 1, 1, 1, 1, 0, 700, 97
41938, V, 1, 1, 1, 1, 0, 700, 97
41939, V, 1, 1, 1, 1, 0, 700, 97
41940, V, 1, 1, 1, 1, 0, 700, 97
41942, V, 1, 1, 1, 1, 0, 700, 97
41943, V, 1, 1, 1, 1, 0, 700, 97
41944, V, 1, 1, 1, 1, 0, 700, 97
41945, V, 1, 1, 1, 1, 0, 700, 97
41946, V, 1, 1, 1, 1, 0, 700, 97
41947, V, 1, 1, 1, 1, 0, 700, 97
41948, V, 1, 1, 1, 1, 0, 700, 97
41949, V, 1, 1, 1, 1, 0, 700, 97
41950, V, 1, 1, 1, 1, 0, 700, 97
41951, V, 1, 1, 1, 1, 0, 700, 97
41952, V, 1, 1, 1, 1, 0, 700, 97
41953, V, 1, 1, 1, 1, 0, 700, 97
41954, V, 1, 1, 1, 1, 0, 700, 97
41955, V, 1, 1, 1, 1, 0, 700, 97
41956, V, 1, 1, 1, 1, 0, 700, 97
41957, V, 1, 1, 1, 1, 0, 700, 97
41958, V, 1, 1, 1, 1, 0, 700, 97
41959, V, 1, 1, 1, 1, 0, 700, 97
41960, V, 1, 1, 1, 1, 0, 700, 97
41961, V, 1, 1, 1, 1, 0, 700, 97
41962, V, 1, 1, 1, 1, 0, 700, 97
41963, V, 1, 1, 1, 1, 0, 700, 97
41964, V, 1, 1, 1, 1, 0, 700, 97
41965, V, 1, 1, 1, 1, 0, 700, 97
41966, V, 1, 1, 1, 1, 0, 700, 97
41967, V, 1, 1, 1, 1, 0, 700, 97
41968, V, 1, 1, 1, 1, 0, 700, 97
41969, V, 1, 1, 1, 1, 0, 700, 97
41970, V, 1, 1, 1, 1, 0, 700, 97
41971, V, 1, 1, 1, 1, 0, 700, 97
41972, V, 1, 1, 1, 1, 0, 700, 97
41973, V, 1, 1, 1, 1, 0, 700, 97
41974, V, 1, 1, 1, 1, 0, 700, 97
41975, V, 1, 1, 1, 1, 0, 700, 97
41976, V, 1, 1, 1, 1, 0, 700, 97
41977, V, 1, 1, 1, 1, 0, 700, 97
41978, V, 1, 1, 1, 1, 0, 700, 97
41979, V, 1, 1, 1, 1, 0, 700, 97
41980, V, 1, 1, 1, 1, 0, 700, 97
41981, V, 1, 1, 1, 1, 0, 700, 97
41982, V, 1, 1, 1, 1, 0, 700, 97
41984, V, 1, 1, 1, 1, 0, 700, 97
41985, V, 1, 1, 1, 1, 0, 700, 97
41986, V, 1, 1, 1, 1, 0, 700, 97
41987, V, 1, 1, 1, 1, 0, 700, 97
41988, V, 1, 1, 1, 1, 0, 700, 97
41989, V, 1, 1, 1, 1, 0, 700, 97
41990, V, 1, 1, 1, 1, 0, 700, 97
41991, V, 1, 1, 1, 1, 0, 700, 97
41992, V, 1, 1, 1, 1, 0, 700, 97
41993, V, 1, 1, 1, 1, 0, 700, 97
41994, V, 1, 1, 1, 1, 0, 700, 97
41995, V, 1, 1, 1, 1, 0, 700, 97
41996, V, 1, 1, 1, 1, 0, 700, 97
41997, V, 1, 1, 1, 1, 0, 700, 97
41998, V, 1, 1, 1, 1, 0, 700, 97
41999, V, 1, 1, 1, 1, 0, 700, 97
42000, V, 1, 1, 1, 1, 0, 700, 97
42001, V, 1, 1, 1, 1, 0, 700, 97
42002, V, 1, 1, 1, 1, 0, 700, 97
42003, V, 1, 1, 1, 1, 0, 700, 97
42004, V, 1, 1, 1, 1, 0, 700, 97
42005, V, 1, 1, 1, 1, 0, 700, 97
42006, V, 1, 1, 1, 1, 0, 700, 97
42007, V, 1, 1, 1, 1, 0, 700, 97
42008, V, 1, 1, 1, 1, 0, 700, 97
42009, V, 1, 1, 1, 1, 0, 700, 97
42010, V, 1, 1, 1, 1, 0, 700, 97
42011, V, 1, 1, 1, 1, 0, 700, 97
42012, V, 1, 1, 1, 1, 0, 700, 97
42013, V, 1, 1, 1, 1, 0, 700, 97
42014, V, 1, 1, 1, 1, 0, 700, 97
42015, V, 1, 1, 1, 1, 0, 700, 97
42016, V, 1, 1, 1, 1, 0, 700, 97
42017, V, 1, 1, 1, 1, 0, 700, 97
42018, V, 1, 1, 1, 1, 0, 700, 97
42019, V, 1, 1, 1, 1, 0, 700, 97
42020, V, 1, 1, 1, 1, 0, 700, 97
42021, V, 1, 1, 1, 1, 0, 700, 97
42022, V, 1, 1, 1, 1, 0, 700, 97
42023, V, 1, 1, 1, 1, 0, 700, 97
42024, V, 1, 1, 1, 1, 0, 700, 97
42025, V, 1, 1, 1, 1, 0, 700, 97
42027, V, 1, 1, 1, 1, 0, 700, 97
42028, V, 1, 1, 1, 1, 0, 700, 97
42029, V, 1, 1, 1, 1, 0, 700, 97
42030, V, 1, 1, 1, 1, 0, 700, 97
42031, V, 1, 1, 1, 1, 0, 700, 97
42032, V, 1, 1, 1, 1, 0, 700, 97
42033, V, 1, 1, 1, 1, 0, 700, 97
42034, V, 1, 1, 1, 1, 0, 700, 97
42035, V, 1, 1, 1, 1, 0, 700, 97
42036, V, 1, 1, 1, 1, 0, 700, 97
42037, V, 1, 1, 1, 1, 0, 700, 97
42038, V, 1, 1, 1, 1, 0, 700, 97
42039, V, 1, 1, 1, 1, 0, 700, 97
42040, V, 1, 1, 1, 1, 0, 700, 97
42041, V, 1, 1, 1, 1, 0, 700, 97
42042, V, 1, 1, 1, 1, 0, 700, 97
42043, V, 1, 1, 1, 1, 0, 700, 97
42044, V, 1, 1, 1, 1, 0, 700, 97
42045, V, 1, 1, 1, 1, 0, 700, 97
42046, V, 1, 1, 1, 1, 0, 700, 97
42047, V, 1, 1, 1, 1, 0, 700, 97
42048, V, 1, 1, 1, 1, 0, 700, 97
42049, V, 1, 1, 1, 1, 0, 700, 97
42050, V, 1, 1, 1, 1, 0, 700, 97
42051, V, 1, 1, 1, 1, 0, 700, 97
42052, V, 1, 1, 1, 1, 0, 700, 97
42053, V, 1, 1, 1, 1, 0, 700, 97
42054, V, 1, 1, 1, 1, 0, 700, 97
42055, V, 1, 1, 1, 1, 0, 700, 97
42056, V, 1, 1, 1, 1, 0, 700, 97
42057, V, 1, 1, 1, 1, 0, 700, 97
42058, V, 1, 1, 1, 1, 0, 700, 97
42059, V, 1, 1, 1, 1, 0, 700, 97
42060, V, 1, 1, 1, 1, 0, 700, 97
42061, V, 1, 1, 1, 1, 0, 700, 97
42062, V, 1, 1, 1, 1, 0, 700, 97
42063, V, 1, 1, 1, 1, 0, 700, 97
42064, V, 1, 1, 1, 1, 0, 700, 97
42065, V, 1, 1, 1, 1, 0, 700, 97
42066, V, 1, 1, 1, 1, 0, 700, 97
42067, V, 1, 1, 1, 1, 0, 700, 97
42068, V, 1, 1, 1, 1, 0, 700, 97
42070, V, 1, 1, 1, 1, 0, 700, 97
42071, V, 1, 1, 1, 1, 0, 700, 97
42072, V, 1, 1, 1, 1, 0, 700, 97
42073, V, 1, 1, 1, 1, 0, 700, 97
42074, V, 1, 1, 1, 1, 0, 700, 97
42075, V, 1, 1, 1, 1, 0, 700, 97
42076, V, 1, 1, 1, 1, 0, 700, 97
42077, V, 1, 1, 1, 1, 0, 700, 97
42078, V, 1, 1, 1, 1, 0, 700, 97
42079, V, 1, 1, 1, 1, 0, 700, 97
42080, V, 1, 1, 1, 1, 0, 700, 97
42081, V, 1, 1, 1, 1, 0, 700, 97
42082, V, 1, 1, 1, 1, 0, 700, 97
42083, V, 1, 1, 1, 1, 0, 700, 97
42084, V, 1, 1, 1, 1, 0, 700, 97
42085, V, 1, 1, 1, 1, 0, 700, 97
42086, V, 1, 1, 1, 1, 0, 700, 97
42087, V, 1, 1, 1, 1, 0, 700, 97
42088, V, 1, 1, 1, 1, 0, 700, 97
42089, V, 1, 1, 1, 1, 0, 700, 97
42090, V, 1, 1, 1, 1, 0, 700, 97
42091, V, 1, 1, 1, 1, 0, 700, 97
42092, V, 1, 1, 1, 1, 0, 700, 97
42093, V, 1, 1, 1, 1, 0, 700, 97
42094, V, 1, 1, 1, 1, 0, 700, 97
42095, V, 1, 1, 1, 1, 0, 700, 97
42096, V, 1, 1, 1, 1, 0, 700, 97
42097, V, 1, 1, 1, 1, 0, 700, 97
42098, V, 1, 1, 1, 1, 0, 700, 97
42099, V, 1, 1, 1, 1, 0, 700, 97
42100, V, 1, 1, 1, 1, 0, 700, 97
42101, V, 1, 1, 1, 1, 0, 700, 97
42102, V, 1, 1, 1, 1, 0, 700, 97
42103, V, 1, 1, 1, 1, 0, 700, 97
42104, V, 1, 1, 1, 1, 0, 700, 97
42105, V, 1, 1, 1, 1, 0, 700, 97
42106, V, 1, 1, 1, 1, 0, 700, 97
42107, V, 1, 1, 1, 1, 0, 700, 97
42108, V, 1, 1, 1, 1, 0, 700, 97
42109, V, 1, 1, 1, 1, 0, 700, 97
42110, V, 1, 1, 1, 1, 0, 700, 97
42112, V, 1, 1, 1, 1, 0, 700, 97
42113, V, 1, 1, 1, 1, 0, 700, 97
42114, V, 1, 1, 1, 1, 0, 700, 97
42115, V, 1, 1, 1, 1, 0, 700, 97
42116, V, 1, 1, 1, 1, 0, 700, 97
42117, V, 1, 1, 1, 1, 0, 700, 97
42118, V, 1, 1, 1, 1, 0, 700, 97
42119, V, 1, 1, 1, 1, 0, 700, 97
42120, V, 1, 1, 1, 1, 0, 700, 97
42121, V, 1, 1, 1, 1, 0, 700, 97
42122, V, 1, 1, 1, 1, 0, 700, 97
42123, V, 1, 1, 1, 1, 0, 700, 97
42124, V, 1, 1, 1, 1, 0, 700, 97
42125, V, 1, 1, 1, 1, 0, 700, 97
42126, V, 1, 1, 1, 1, 0, 700, 97
42127, V, 1, 1, 1, 1, 0, 700, 97
42128, V, 1, 1, 1, 1, 0, 700, 97
42129, V, 1, 1, 1, 1, 0, 700, 97
42130, V, 1, 1, 1, 1, 0, 700, 97
42131, V, 1, 1, 1, 1, 0, 700, 97
42132, V, 1, 1, 1, 1, 0, 700, 97
42133, V, 1, 1, 1, 1, 0, 700, 97
42134, V, 1, 1, 1, 1, 0, 700, 97
42135, V, 1, 1, 1, 1, 0, 700, 97
42136, V, 1, 1, 1, 1, 0, 700, 97
42137, V, 1, 1, 1, 1, 0, 700, 97
42138, V, 1, 1, 1, 1, 0, 700, 97
42139, V, 1, 1, 1, 1, 0, 700, 97
42140, V, 1, 1, 1, 1, 0, 700, 97
42141, V, 1, 1, 1, 1, 0, 700, 97
42142, V, 1, 1, 1, 1, 0, 700, 97
42143, V, 1, 1, 1, 1, 0, 700, 97
42144, V, 1, 1, 1, 1, 0, 700, 97
42145, V, 1, 1, 1, 1, 0, 700, 97
42146, V, 1, 1, 1, 1, 0, 700, 97
42147, V, 1, 1, 1, 1, 0, 700, 97
42148, V, 1, 1, 1, 1, 0, 700, 97
42149, V, 1, 1, 1, 1, 0, 700, 97
42150, V, 1, 1, 1, 1, 0, 700, 97
42151, V, 1, 1, 1, 1, 0, 700, 97
42152, V, 1, 1, 1, 1, 0, 700, 97
42153, V, 1, 1, 1, 1, 0, 700, 97
42155, V, 1, 1, 1, 1, 0, 700, 97
42156, V, 1, 1, 1, 1, 0, 700, 97
42157, V, 1, 1, 1, 1, 0, 700, 97
42158, V, 1, 1, 1, 1, 0, 700, 97
42159, V, 1, 1, 1, 1, 0, 700, 97
42160, V, 1, 1, 1, 1, 0, 700, 97
42161, V, 1, 1, 1, 1, 0, 700, 97
42162, V, 1, 1, 1, 1, 0, 700, 97
42163, V, 1, 1, 1, 1, 0, 700, 97
42164, V, 1, 1, 1, 1, 0, 700, 97
42165, V, 1, 1, 1, 1, 0, 700, 97
42166, V, 1, 1, 1, 1, 0, 700, 97
42167, V, 1, 1, 1, 1, 0, 700, 97
42168, V, 1, 1, 1, 1, 0, 700, 97
42169, V, 1, 1, 1, 1, 0, 700, 97
42170, V, 1, 1, 1, 1, 0, 700, 97
42171, V, 1, 1, 1, 1, 0, 700, 97
42172, V, 1, 1, 1, 1, 0, 700, 97
42173, V, 1, 1, 1, 1, 0, 700, 97
42174, V, 1, 1, 1, 1, 0, 700, 97
42175, V, 1, 1, 1, 1, 0, 700, 97
42176, V, 1, 1, 1, 1, 0, 700, 97
42177, V, 1, 1, 1, 1, 0, 700, 97
42178, V, 1, 1, 1, 1, 0, 700, 97
42179, V, 1, 1, 1, 1, 0, 700, 97
42180, V, 1, 1, 1, 1, 0, 700, 97
42181, V, 1, 1, 1, 1, 0, 700, 97
42182, V, 1, 1, 1, 1, 0, 700, 97
42183, V, 1, 1, 1, 1, 0, 700, 97
42184, V, 1, 1, 1, 1, 0, 700, 97
42185, V, 1, 1, 1, 1, 0, 700, 97
42186, V, 1, 1, 1, 1, 0, 700, 97
42187, V, 1, 1, 1, 1, 0, 700, 97
42188, V, 1, 1, 1, 1, 0, 700, 97
42189, V, 1, 1, 1, 1, 0, 700, 97
42190, V, 1, 1, 1, 1, 0, 700, 97
42191, V, 1, 1, 1, 1, 0, 700, 97
42192, V, 1, 1, 1, 1, 0, 700, 97
42193, V, 1, 1, 1, 1, 0, 700, 97
42194, V, 1, 1, 1, 1, 0, 700, 97
42195, V, 1, 1, 1, 1, 0, 700, 97
42196, V, 1, 1, 1, 1, 0, 700, 97
42198, V, 1, 1, 1, 1, 0, 700, 97
42199, V, 1, 1, 1, 1, 0, 700, 97
42200, V, 1, 1, 1, 1, 0, 700, 97
42201, V, 1, 1, 1, 1, 0, 700, 97
42202, V, 1, 1, 1, 1, 0, 700, 97
42203, V, 1, 1, 1, 1, 0, 700, 97
42204, V, 1, 1, 1, 1, 0, 700, 97
42205, V, 1, 1, 1, 1, 0, 700, 97
42206, V, 1, 1, 1, 1, 0, 700, 97
42207, V, 1, 1, 1, 1, 0, 700, 97
42208, V, 1, 1, 1, 1, 0, 700, 97
42209, V, 1, 1, 1, 1, 0, 700, 97
42210, V, 1, 1, 1, 1, 0, 700, 97
42211, V, 1, 1, 1, 1, 0, 700, 97
42212, V, 1, 1, 1, 1, 0, 700, 97
42213, V, 1, 1, 1, 1, 0, 700, 97
42214, V, 1, 1, 1, 1, 0, 700, 97
42215, V, 1, 1, 1, 1, 0, 700, 97
42216, V, 1, 1, 1, 1, 0, 700, 97
42217, V, 1, 1, 1, 1, 0, 700, 97
42218, V, 1, 1, 1, 1, 0, 700, 97
42219, V, 1, 1, 1, 1, 0, 700, 97
42220, V, 1, 1, 1, 1, 0, 700, 97
42221, V, 1, 1, 1, 1, 0, 700, 97
42222, V, 1, 1, 1, 1, 0, 700, 97
42223, V, 1, 1, 1, 1, 0, 700, 97
42224, V, 1, 1, 1, 1, 0, 700, 97
42225, V, 1, 1, 1, 1, 0, 700, 97
42226, V, 1, 1, 1, 1, 0, 700, 97
42227, V, 1, 1, 1, 1, 0, 700, 97
42228, V, 1, 1, 1, 1, 0, 700, 97
42229, V, 1, 1, 1, 1, 0, 700, 97
42230, V, 1, 1, 1, 1, 0, 700, 97
42231, V, 1, 1, 1, 1, 0, 700, 97
42232, V, 1, 1, 1, 1, 0, 700, 97
42233, V, 1, 1, 1, 1, 0, 700, 97
42234, V, 1, 1, 1, 1, 0, 700, 97
42235, V, 1, 1, 1, 1, 0, 700, 97
42236, V, 1, 1, 1, 1, 0, 700, 97
42237, V, 1, 1, 1, 1, 0, 700, 97
42238, V, 1, 1, 1, 1, 0, 700, 97
42240, V, 1, 1, 1, 1, 0, 700, 97
42241, V, 1, 1, 1, 1, 0, 700, 97
42242, V, 1, 1, 1, 1, 0, 700, 97
42243, V, 1, 1, 1, 1, 0, 700, 97
42244, V, 1, 1, 1, 1, 0, 700, 97
42245, V, 1, 1, 1, 1, 0, 700, 97
42246, V, 1, 1, 1, 1, 0, 700, 97
42247, V, 1, 1, 1, 1, 0, 700, 97
42248, V, 1, 1, 1, 1, 0, 700, 97
42249, V, 1, 1, 1, 1, 0, 700, 97
42250, V, 1, 1, 1, 1, 0, 700, 97
42251, V, 1, 1, 1, 1, 0, 700, 97
42252, V, 1, 1, 1, 1, 0, 700, 97
42253, V, 1, 1, 1, 1, 0, 700, 97
42254, V, 1, 1, 1, 1, 0, 700, 97
42255, V, 1, 1, 1, 1, 0, 700, 97
42256, V, 1, 1, 1, 1, 0, 700, 97
42257, V, 1, 1, 1, 1, 0, 700, 97
42258, V, 1, 1, 1, 1, 0, 700, 97
42259, V, 1, 1, 1, 1, 0, 700, 97
42260, V, 1, 1, 1, 1, 0, 700, 97
42261, V, 1, 1, 1, 1, 0, 700, 97
42262, V, 1, 1, 1, 1, 0, 700, 97
42263, V, 1, 1, 1, 1, 0, 700, 97
42264, V, 1, 1, 1, 1, 0, 700, 97
42265, V, 1, 1, 1, 1, 0, 700, 97
42266, V, 1, 1, 1, 1, 0, 700, 97
42267, V, 1, 1, 1, 1, 0, 700, 97
42268, V, 1, 1, 1, 1, 0, 700, 97
42269, V, 1, 1, 1, 1, 0, 700, 97
42270, V, 1, 1, 1, 1, 0, 700, 97
42271, V, 1, 1, 1, 1, 0, 700, 97
42272, V, 1, 1, 1, 1, 0, 700, 97
42273, V, 1, 1, 1, 1, 0, 700, 97
42274, V, 1, 1, 1, 1, 0, 700, 97
42275, V, 1, 1, 1, 1, 0, 700, 97
42276, V, 1, 1, 1, 1, 0, 700, 97
42277, V, 1, 1, 1, 1, 0, 700, 97
42278, V, 1, 1, 1, 1, 0, 700, 97
42279, V, 1, 1, 1, 1, 0, 700, 97
42280, V, 1, 1, 1, 1, 0, 700, 97
42281, V, 1, 1, 1, 1, 0, 700, 97
42283, V, 1, 1, 1, 1, 0, 700, 97
42284, V, 1, 1, 1, 1, 0, 700, 97
42285, V, 1, 1, 1, 1, 0, 700, 97
42286, V, 1, 1, 1, 1, 0, 700, 97
42287, V, 1, 1, 1, 1, 0, 700, 97
42288, V, 1, 1, 1, 1, 0, 700, 97
42289, V, 1, 1, 1, 1, 0, 700, 97
42290, V, 1, 1, 1, 1, 0, 700, 97
42291, V, 1, 1, 1, 1, 0, 700, 97
42292, V, 1, 1, 1, 1, 0, 700, 97
42293, V, 1, 1, 1, 1, 0, 700, 97
42294, V, 1, 1, 1, 1, 0, 700, 97
42295, V, 1, 1, 1, 1, 0, 700, 97
42296, V, 1, 1, 1, 1, 0, 700, 97
42297, V, 1, 1, 1, 1, 0, 700, 97
42298, V, 1, 1, 1, 1, 0, 700, 97
42299, V, 1, 1, 1, 1, 0, 700, 97
42300, V, 1, 1, 1, 1, 0, 700, 97
42301, V, 1, 1, 1, 1, 0, 700, 97
42302, V, 1, 1, 1, 1, 0, 700, 97
42303, V, 1, 1, 1, 1, 0, 700, 97
42304, V, 1, 1, 1, 1, 0, 700, 97
42305, V, 1, 1, 1, 1, 0, 700, 97
42306, V, 1, 1, 1, 1, 0, 700, 97
42307, V, 1, 1, 1, 1, 0, 700, 97
42308, V, 1, 1, 1, 1, 0, 700, 97
42309, V, 1, 1, 1, 1, 0, 700, 97
42310, V, 1, 1, 1, 1, 0, 700, 97
42311, V, 1, 1, 1, 1, 0, 700, 97
42312, V, 1, 1, 1, 1, 0, 700, 97
42313, V, 1, 1, 1, 1, 0, 700, 97
42314, V, 1, 1, 1, 1, 0, 700, 97
42315, V, 1, 1, 1, 1, 0, 700, 97
42316, V, 1, 1, 1, 1, 0, 700, 97
42317, V, 1, 1, 1, 1, 0, 700, 97
42318, V, 1, 1, 1, 1, 0, 700, 97
42319, V, 1, 1, 1, 1, 0, 700, 97
42320, V, 1, 1, 1, 1, 0, 700, 97
42321, V, 1, 1, 1, 1, 0, 700, 97
42322, V, 1, 1, 1, 1, 0, 700, 97
42323, V, 1, 1, 1, 1, 0, 700, 97
42324, V, 1, 1, 1, 1, 0, 700, 97
42326, V, 1, 1, 1, 1, 0, 700, 97
42327, V, 1, 1, 1, 1, 0, 700, 97
42328, V, 1, 1, 1, 1, 0, 700, 97
42329, V, 1, 1, 1, 1, 0, 700, 97
42330, V, 1, 1, 1, 1, 0, 700, 97
42331, V, 1, 1, 1, 1, 0, 700, 97
42332, V, 1, 1, 1, 1, 0, 700, 97
42333, V, 1, 1, 1, 1, 0, 700, 97
42334, V, 1, 1, 1, 1, 0, 700, 97
42335, V, 1, 1, 1, 1, 0, 700, 97
42336, V, 1, 1, 1, 1, 0, 700, 97
42337, V, 1, 1, 1, 1, 0, 700, 97
42338, V, 1, 1, 1, 1, 0, 700, 97
42339, V, 1, 1, 1, 1, 0, 700, 97
42340, V, 1, 1, 1, 1, 0, 700, 97
42341, V, 1, 1, 1, 1, 0, 700, 97
42342, V, 1, 1, 1, 1, 0, 700, 97
42343, V, 1, 1, 1, 1, 0, 700, 97
42344, V, 1, 1, 1, 1, 0, 700, 97
42345, V, 1, 1, 1, 1, 0, 700, 97
42346, V, 1, 1, 1, 1, 0, 700, 97
42347, V, 1, 1, 1, 1, 0, 700, 97
42348, V, 1, 1, 1, 1, 0, 700, 97
42349, V, 1, 1, 1, 1, 0, 700, 97
42350, V, 1, 1, 1, 1, 0, 700, 97
42351, V, 1, 1, 1, 1, 0, 700, 97
42352, V, 1, 1, 1, 1, 0, 700, 97
42353, V, 1, 1, 1, 1, 0, 700, 97
42354, V, 1, 1, 1, 1, 0, 700, 97
42355, V, 1, 1, 1, 1, 0, 700, 97
42356, V, 1, 1, 1, 1, 0, 700, 97
42357, V, 1, 1, 1, 1, 0, 700, 97
42358, V, 1, 1, 1, 1, 0, 700, 97
42359, V, 1, 1, 1, 1, 0, 700, 97
42360, V, 1, 1, 1, 1, 0, 700, 97
42361, V, 1, 1, 1, 1, 0, 700, 97
42362, V, 1, 1, 1, 1, 0, 700, 97
42363, V, 1, 1, 1, 1, 0, 700, 97
42364, V, 1, 1, 1, 1, 0, 700, 97
42365, V, 1, 1, 1, 1, 0, 700, 97
42366, V, 1, 1, 1, 1, 0, 700, 97
42368, V, 1, 1, 1, 1, 0, 700, 97
42369, V, 1, 1, 1, 1, 0, 700, 97
42370, V, 1, 1, 1, 1, 0, 700, 97
42371, V, 1, 1, 1, 1, 0, 700, 97
42372, V, 1, 1, 1, 1, 0, 700, 97
42373, V, 1, 1, 1, 1, 0, 700, 97
42374, V, 1, 1, 1, 1, 0, 700, 97
42375, V, 1, 1, 1, 1, 0, 700, 97
42376, V, 1, 1, 1, 1, 0, 700, 97
42377, V, 1, 1, 1, 1, 0, 700, 97
42378, V, 1, 1, 1, 1, 0, 700, 97
42379, V, 1, 1, 1, 1, 0, 700, 97
42380, V, 1, 1, 1, 1, 0, 700, 97
42381, V, 1, 1, 1, 1, 0, 700, 97
42382, V, 1, 1, 1, 1, 0, 700, 97
42383, V, 1, 1, 1, 1, 0, 700, 97
42384, V, 1, 1, 1, 1, 0, 700, 97
42385, V, 1, 1, 1, 1, 0, 700, 97
42386, V, 1, 1, 1, 1, 0, 700, 97
42387, V, 1, 1, 1, 1, 0, 700, 97
42388, V, 1, 1, 1, 1, 0, 700, 97
42389, V, 1, 1, 1, 1, 0, 700, 97
42390, V, 1, 1, 1, 1, 0, 700, 97
42391, V, 1, 1, 1, 1, 0, 700, 97
42392, V, 1, 1, 1, 1, 0, 700, 97
42393, V, 1, 1, 1, 1, 0, 700, 97
42394, V, 1, 1, 1, 1, 0, 700, 97
42395, V, 1, 1, 1, 1, 0, 700, 97
42396, V, 1, 1, 1, 1, 0, 700, 97
42397, V, 1, 1, 1, 1, 0, 700, 97
42398, V, 1, 1, 1, 1, 0, 700, 97
42399, V, 1, 1, 1, 1, 0, 700, 97
42400, V, 1, 1, 1, 1, 0, 700, 97
42401, V, 1, 1, 1, 1, 0, 700, 97
42402, V, 1, 1, 1, 1, 0, 700, 97
42403, V, 1, 1, 1, 1, 0, 700, 97
42404, V, 1, 1, 1, 1, 0, 700, 97
42405, V, 1, 1, 1, 1, 0, 700, 97
42406, V, 1, 1, 1, 1, 0, 700, 97
42407, V, 1, 1, 1, 1, 0, 700, 97
42408, V, 1, 1, 1, 1, 0, 700, 97
42409, V, 1, 1, 1, 1, 0, 700, 97
42411, V, 1, 1, 1, 1, 0, 700, 97
42412, V, 1, 1, 1, 1, 0, 700, 97
42413, V, 1, 1, 1, 1, 0, 700, 97
42414, V, 1, 1, 1, 1, 0, 700, 97
42415, V, 1, 1, 1, 1, 0, 700, 97
42416, V, 1, 1, 1, 1, 0, 700, 97
42417, V, 1, 1, 1, 1, 0, 700, 97
42418, V, 1, 1, 1, 1, 0, 700, 97
42419, V, 1, 1, 1, 1, 0, 700, 97
42420, V, 1, 1, 1, 1, 0, 700, 97
42421, V, 1, 1, 1, 1, 0, 700, 97
42422, V, 1, 1, 1, 1, 0, 700, 97
42423, V, 1, 1, 1, 1, 0, 700, 97
42424, V, 1, 1, 1, 1, 0, 700, 97
42425, V, 1, 1, 1, 1, 0, 700, 97
42426, V, 1, 1, 1, 1, 0, 700, 97
42427, V, 1, 1, 1, 1, 0, 700, 97
42428, V, 1, 1, 1, 1, 0, 700, 97
42429, V, 1, 1, 1, 1, 0, 700, 97
42430, V, 1, 1, 1, 1, 0, 700, 97
42431, V, 1, 1, 1, 1, 0, 700, 97
42432, V, 1, 1, 1, 1, 0, 700, 97
42433, V, 1, 1, 1, 1, 0, 700, 97
42434, V, 1, 1, 1, 1, 0, 700, 97
42435, V, 1, 1, 1, 1, 0, 700, 97
42436, V, 1, 1, 1, 1, 0, 700, 97
42437, V, 1, 1, 1, 1, 0, 700, 97
42438, V, 1, 0, 0, 1, 0, 700, 97
42438, V, 1, 0, 0, 0, 0, 700, 97
42439, V, 1, 1, 0, 0, 0, 700, 97
42439, V, 1, 1, 0, 0, 0, 700, 97
42440, V, 1, 1, 1, 1, 0, 700, 97
42441, V, 1, 1, 1, 1, 0, 700, 97
42442, V, 1, 1, 1, 1, 0, 700, 97
42443, V, 1, 1, 1, 1, 0, 700, 97
42444, V, 1, 1, 1, 1, 0, 700, 97
42445, V, 1, 1, 1, 1, 0, 700, 97
42446, V, 1, 1, 1, 1, 0, 700, 97
42447, V, 1, 1, 1, 1, 0, 700, 96
42448, V, 1, 1, 1, 1, 0, 700, 96
42449, V, 1, 1, 1, 1, 0, 700, 96
42450, V, 1, 1, 1, 1, 0, 700, 96
42451, V, 1, 1, 1, 1, 0, 700, 97
42452, V, 1, 1, 1, 1, 0, 700, 96
42454, V, 1, 1, 1, 1, 0, 700, 97
42455, V, 1, 1, 1, 1, 0, 700, 97
42456, V, 1, 1, 1, 1, 0, 700, 97
42457, V, 1, 1, 1, 1, 0, 700, 97
42458, V, 1, 1, 1, 1, 0, 700, 97
42459, V, 1, 1, 1, 1, 0, 700, 97
42460, V, 1, 1, 1, 1, 0, 700, 97
42461, V, 1, 1, 1, 1, 0, 700, 97
42462, V, 1, 1, 1, 1, 0, 700, 97
42463, V, 1, 1, 1, 1, 0, 700, 97
42464, V, 1, 1, 1, 1, 0, 700, 97
42465, V, 1, 1, 1, 1, 0, 700, 97
42466, V, 1, 1, 1, 1, 0, 700, 97
42467, V, 1, 1, 1, 1, 0, 700, 97
42468, V, 1, 1, 1, 1, 0, 700, 97
42469, V, 1, 0, 0, 1, 0, 700, 97
42469, V, 1, 0, 0, 0, 0, 700, 97
42470, V, 1, 1, 0, 0, 0, 700, 97
42470, V, 1, 1, 0, 0, 0, 700, 97
42471, V, 1, 1, 1, 1, 0, 700, 97
42472, V, 1, 1, 1, 1, 0, 700, 97
42473, V, 1, 1, 1, 1, 0, 700, 97
42474, V, 1, 1, 1, 1, 0, 700, 96
42475, V, 1, 1, 1, 1, 0, 700, 96
42476, V, 1, 1, 1, 1, 0, 700, 96
42477, V, 1, 1, 1, 1, 0, 700, 96
42478, V, 1, 1, 1, 1, 0, 700, 96
42479, V, 1, 1, 1, 1, 0, 700, 96
42480, V, 1, 1, 1, 1, 0, 700, 96
42481, V, 1, 1, 1, 1, 0, 700, 96
42482, V, 1, 1, 1, 1, 0, 700, 96
42483, V, 1, 1, 1, 1, 0, 700, 96
42484, V, 1, 1, 1, 1, 0, 700, 96
42485, V, 1, 1, 1, 1, 0, 700, 96
42486, V, 1, 1, 1, 1, 0, 700, 96
42487, V, 1, 1, 1, 1, 0, 700, 96
42488, V, 1, 1, 1, 1, 0, 700, 96
42489, V, 1, 1, 1, 1, 0, 700, 96
42490, V, 1, 1, 1, 1, 0, 700, 96
42491, V, 1, 1, 1, 1, 0, 700, 96
42492, V, 1, 1, 1, 1, 0, 700, 96
42493, V, 1, 1, 1, 1, 0, 700, 96
42494, V, 1, 1, 1, 1, 0, 700, 96
42496, V, 1, 1, 1, 1, 0, 700, 96
42497, V, 1, 1, 1, 1, 0, 700, 97
42498, V, 1, 1, 1, 1, 0, 700, 97
42499, V, 1, 1, 1, 1, 0, 700, 97
42500, V, 1, 1, 1, 1, 0, 700, 97
42501, V, 1, 1, 1, 1, 0, 700, 97
42502, V, 1, 1, 1, 1, 0, 700, 97
42503, V, 1, 1, 1, 1, 0, 700, 97
42504, V, 1, 1, 1, 1, 0, 700, 97
42505, V, 1, 1, 1, 1, 0, 700, 97
42506, V, 1, 1, 1, 1, 0, 700, 97
42507, V, 1, 1, 1, 1, 0, 700, 97
42508, V, 1, 1, 1, 1, 0, 700, 97
42509, V, 1, 1, 1, 1, 0, 700, 97
42510, V, 1, 1, 1, 1, 0, 700, 97
42511, V, 1, 1, 1, 1, 0, 700, 97
42512, V, 1, 1, 1, 1, 0, 700, 97
42513, V, 1, 1, 1, 1, 0, 700, 97
42514, V, 1, 1, 1, 1, 0, 700, 97
42515, V, 1, 1, 1, 1, 0, 700, 97
42516, V, 1, 1, 1, 1, 0, 700, 97
42517, V, 1, 1, 1, 1, 0, 700, 97
42518, V, 1, 1, 1, 1, 0, 700, 97
42519, V, 1, 1, 1, 1, 0, 700, 97
42520, V, 1, 1, 1, 1, 0, 700, 97
42521, V, 1, 1, 1, 1, 0, 700, 97
42522, V, 1, 1, 1, 1, 0, 700, 97
42523, V, 1, 1, 1, 1, 0, 700, 97
42524, V, 1, 1, 1, 1, 0, 700, 97
42525, V, 1, 1, 1, 1, 0, 700, 97
42526, V, 1, 1, 1, 1, 0, 700, 97
42527, V, 1, 1, 1, 1, 0, 700, 97
42528, V, 1, 1, 1, 1, 0, 700, 97
42529, V, 1, 1, 1, 1, 0, 700, 97
42530, V, 1, 1, 1, 1, 0, 700, 97
42531, V, 1, 1, 1, 1, 0, 700, 97
42532, V, 1, 1, 1, 1, 0, 700, 97
42533, V, 1, 1, 1, 1, 0, 700, 97
42534, V, 1, 1, 1, 1, 0, 700, 97
42535, V, 1, 1, 1, 1, 0, 700, 97
42536, V, 1, 1, 1, 1, 0, 700, 97
42537, V, 1, 1, 1, 1, 0, 700, 97
42539, V, 1, 1, 1, 1, 0, 700, 97
42540, V, 1, 1, 1, 1, 0, 700, 97
42541, V, 1, 1, 1, 1, 0, 700, 97
42542, V, 1, 1, 1, 1, 0, 700, 97
42543, V, 1, 1, 1, 1, 0, 700, 97
42544, V, 1, 1, 1, 1, 0, 700, 97
42545, V, 1, 1, 1, 1, 0, 700, 97
42546, V, 1, 1, 1, 1, 0, 700, 97
42547, V, 1, 1, 1, 1, 0, 700, 97
42548, V, 1, 1, 1, 1, 0, 700, 97
42549, V, 1, 1, 1, 1, 0, 700, 97
42550, V, 1, 1, 1, 1, 0, 700, 97
42551, V, 1, 1, 1, 1, 0, 700, 97
42552, V, 1, 1, 1, 1, 0, 700, 97
42553, V, 1, 1, 1, 1, 0, 700, 97
42554, V, 1, 1, 1, 1, 0, 700, 97
42555, V, 1, 1, 1, 1, 0, 700, 97
42556, V, 1, 1, 1, 1, 0, 700, 97
42557, V, 1, 1, 1, 1, 0, 700, 97
42558, V, 1, 1, 1, 1, 0, 700, 97
42559, V, 1, 1, 1, 1, 0, 700, 97
42560, V, 1, 1, 1, 1, 0, 700, 97
42561, V, 1, 1, 1, 1, 0, 700, 97
42562, V, 1, 1, 1, 1, 0, 700, 97
42563, V, 1, 1, 1, 1, 0, 700, 97
42564, V, 1, 1, 1, 1, 0, 700, 97
42565, V, 1, 1, 1, 1, 0, 700, 97
42566, V, 1, 1, 1, 1, 0, 700, 97
42567, V, 1, 1, 1, 1, 0, 700, 97
42568, V, 1, 1, 1, 1, 0, 700, 97
42569, V, 1, 1, 1, 1, 0, 700, 97
42570, V, 1, 1, 1, 1, 0, 700, 97
42571, V, 1, 1, 1, 1, 0, 700, 97
42572, V, 1, 1, 1, 1, 0, 700, 97
42573, V, 1, 1, 1, 1, 0, 700, 97
42574, V, 1, 1, 1, 1, 0, 700, 97
42575, V, 1, 1, 1, 1, 0, 700, 97
42576, V, 1, 1, 1, 1, 0, 700, 97
42577, V, 1, 1, 1, 1, 0, 700, 97
42578, V, 1, 1, 1, 1, 0, 700, 97
42579, V, 1, 1, 1, 1, 0, 700, 97
42580, V, 1, 1, 1, 1, 0, 700, 97
42582, V, 1, 1, 1, 1, 0, 700, 97
42583, V, 1, 1, 1, 1, 0, 700, 97
42584, V, 1, 1, 1, 1, 0, 700, 97
42585, V, 1, 1, 1, 1, 0, 700, 97
42586, V, 1, 1, 1, 1, 0, 700, 97
42587, V, 1, 1, 1, 1, 0, 700, 97
42588, V, 1, 1, 1, 1, 0, 700, 97
42589, V, 1, 1, 1, 1, 0, 700, 97
42590, V, 1, 1, 1, 1, 0, 700, 97
42591, V, 1, 1, 1, 1, 0, 700, 97
42592, V, 1, 1, 1, 1, 0, 700, 97
42593, V, 1, 1, 1, 1, 0, 700, 97
42594, V, 1, 1, 1, 1, 0, 700, 97
42595, V, 1, 1, 1, 1, 0, 700, 97
42596, V, 1, 1, 1, 1, 0, 700, 97
42597, V, 1, 1, 1, 1, 0, 700, 97
42598, V, 1, 1, 1, 1, 0, 700, 97
42599, V, 1, 1, 1, 1, 0, 700, 97
42600, V, 1, 1, 1, 1, 0, 700, 97
42601, V, 1, 1, 1, 1, 0, 700, 97
42602, V, 1, 1, 1, 1, 0, 700, 97
42603, V, 1, 1, 1, 1, 0, 700, 97
42604, V, 1, 1, 1, 1, 0, 700, 97
42605, V, 1, 1, 1, 1, 0, 700, 97
42606, V, 1, 1, 1, 1, 0, 700, 97
42607, V, 1, 1, 1, 1, 0, 700, 97
42608, V, 1, 1, 1, 1, 0, 700, 97
42609, V, 1, 1, 1, 1, 0, 700, 97
42610, V, 1, 1, 1, 1, 0, 700, 97
42611, V, 1, 1, 1, 1, 0, 700, 97
42612, V, 1, 1, 1, 1, 0, 700, 97
42613, V, 1, 1, 1, 1, 0, 700, 97
42614, V, 1, 1, 1, 1, 0, 700, 97
42615, V, 1, 1, 1, 1, 0, 700, 97
42616, V, 1, 1, 1, 1, 0, 700, 97
42617, V, 1, 1, 1, 1, 0, 700, 97
42618, V, 1, 1, 1, 1, 0, 700, 97
42619, V, 1, 1, 1, 1, 0, 700, 97
42620, V, 1, 1, 1, 1, 0, 700, 97
42621, V, 1, 1, 1, 1, 0, 700, 97
42622, V, 1, 1, 1, 1, 0, 700, 97
42624, V, 1, 1, 1, 1, 0, 700, 97
42625, V, 1, 1, 1, 1, 0, 700, 97
42626, V, 1, 1, 1, 1, 0, 700, 97
42627, V, 1, 1, 1, 1, 0, 700, 97
42628, V, 1, 1, 1, 1, 0, 700, 97
42629, V, 1, 1, 1, 1, 0, 700, 97
42630, V, 1, 1, 1, 1, 0, 700, 97
42631, V, 1, 1, 1, 1, 0, 700, 97
42632, V, 1, 1, 1, 1, 0, 700, 97
42633, V, 1, 1, 1, 1, 0, 700, 97
42634, V, 1, 1, 1, 1, 0, 700, 97
42635, V, 1, 1, 1, 1, 0, 700, 97
42636, V, 1, 1, 1, 1, 0, 700, 97
42637, V, 1, 1, 1, 1, 0, 700, 97
42638, V, 1, 1, 1, 1, 0, 700, 97
42639, V, 1, 1, 1, 1, 0, 700, 97
42640, V, 1, 1, 1, 1, 0, 700, 97
42641, V, 1, 1, 1, 1, 0, 700, 97
42642, V, 1, 1, 1, 1, 0, 700, 97
42643, V, 1, 1, 1, 1, 0, 700, 97
42644, V, 1, 1, 1, 1, 0, 700, 97
42645, V, 1, 1, 1, 1, 0, 700, 97
42646, V, 1, 1, 1, 1, 0, 700, 97
42647, V, 1, 1, 1, 1, 0, 700, 97
42648, V, 1, 1, 1, 1, 0, 700, 97
42649, V, 1, 1, 1, 1, 0, 700, 97
42650, V, 1, 1, 1, 1, 0, 700, 97
42651, V, 1, 1, 1, 1, 0, 700, 97
42652, V, 1, 1, 1, 1, 0, 700, 97
42653, V, 1, 1, 1, 1, 0, 700, 97
42654, V, 1, 1, 1, 1, 0, 700, 97
42655, V, 1, 1, 1, 1, 0, 700, 97
42656, V, 1, 1, 1, 1, 0, 700, 97
42657, V, 1, 1, 1, 1, 0, 700, 97
42658, V, 1, 1, 1, 1, 0, 700, 97
42659, V, 1, 1, 1, 1, 0, 700, 97
42660, V, 1, 1, 1, 1, 0, 700, 97
42661, V, 1, 1, 1, 1, 0, 700, 97
42662, V, 1, 1, 1, 1, 0, 700, 97
42663, V, 1, 1, 1, 1, 0, 700, 97
42664, V, 1, 1, 1, 1, 0, 700, 97
42665, V, 1, 1, 1, 1, 0, 700, 97
42667, V, 1, 1, 1, 1, 0, 700, 97
42668, V, 1, 1, 1, 1, 0, 700, 97
42669, V, 1, 1, 1, 1, 0, 700, 97
42670, V, 1, 1, 1, 1, 0, 700, 97
42671, V, 1, 1, 1, 1, 0, 700, 97
42672, V, 1, 1, 1, 1, 0, 700, 97
42673, V, 1, 1, 1, 1, 0, 700, 97
42674, V, 1, 1, 1, 1, 0, 700, 97
42675, V, 1, 1, 1, 1, 0, 700, 97
42676, V, 1, 1, 1, 1, 0, 700, 97
42677, V, 1, 1, 1, 1, 0, 700, 97
42678, V, 1, 1, 1, 1, 0, 700, 97
42679, V, 1, 1, 1, 1, 0, 700, 97
42680, V, 1, 1, 1, 1, 0, 700, 97
42681, V, 1, 1, 1, 1, 0, 700, 97
42682, V, 1, 1, 1, 1, 0, 700, 97
42683, V, 1, 1, 1, 1, 0, 700, 97
42684, V, 1, 1, 1, 1, 0, 700, 97
42685, V, 1, 1, 1, 1, 0, 700, 97
42686, V, 1, 1, 1, 1, 0, 700, 97
42687, V, 1, 1, 1, 1, 0, 700, 97
42688, V, 1, 1, 1, 1, 0, 700, 97
42689, V, 1, 1, 1, 1, 0, 700, 97
42690, V, 1, 1, 1, 1, 0, 700, 97
42691, V, 1, 1, 1, 1, 0, 700, 97
42692, V, 1, 1, 1, 1, 0, 700, 97
42693, V, 1, 1, 1, 1, 0, 700, 97
42694, V, 1, 1, 1, 1, 0, 700, 97
42695, V, 1, 1, 1, 1, 0, 700, 97
42696, V, 1, 1, 1, 1, 0, 700, 97
42697, V, 1, 1, 1, 1, 0, 700, 97
42698, V, 1, 1, 1, 1, 0, 700, 97
42699, V, 1, 1, 1, 1, 0, 700, 97
42700, V, 1, 1, 1, 1, 0, 700, 97
42701, V, 1, 1, 1, 1, 0, 700, 97
42702, V, 1, 1, 1, 1, 0, 700, 97
42703, V, 1, 1, 1, 1, 0, 700, 97
42704, V, 1, 1, 1, 1, 0, 700, 97
42705, V, 1, 1, 1, 1, 0, 700, 97
42706, V, 1, 1, 1, 1, 0, 700, 97
42707, V, 1, 1, 1, 1, 0, 700, 97
42708, V, 1, 1, 1, 1, 0, 700, 97
42710, V, 1, 1, 1, 1, 0, 700, 97
42711, V, 1, 1, 1, 1, 0, 700, 97
42712, V, 1, 1, 1, 1, 0, 700, 97
42713, V, 1, 1, 1, 1, 0, 700, 97
42714, V, 1, 1, 1, 1, 0, 700, 97
42715, V, 1, 1, 1, 1, 0, 700, 97
42716, V, 1, 1, 1, 1, 0, 700, 97
42717, V, 1, 1, 1, 1, 0, 700, 97
42718, V, 1, 1, 1, 1, 0, 700, 97
42719, V, 1, 1, 1, 1, 0, 700, 97
42720, V, 1, 1, 1, 1, 0, 700, 97
42721, V, 1, 1, 1, 1, 0, 700, 97
42722, V, 1, 1, 1, 1, 0, 700, 97
42723, V, 1, 1, 1, 1, 0, 700, 97
42724, V, 1, 1, 1, 1, 0, 700, 97
42725, V, 1, 1, 1, 1, 0, 700, 97
42726, V, 1, 1, 1, 1, 0, 700, 97
42727, V, 1, 1, 1, 1, 0, 700, 97
42728, V, 1, 1, 1, 1, 0, 700, 97
42729, V, 1, 1, 1, 1, 0, 700, 97
42730, V, 1, 1, 1, 1, 0, 700, 97
42731, V, 1, 1, 1, 1, 0, 700, 97
42732, V, 1, 1, 1, 1, 0, 700, 97
42733, V, 1, 1, 1, 1, 0, 700, 97
42734, V, 1, 1, 1, 1, 0, 700, 97
42735, V, 1, 1, 1, 1, 0, 700, 97
42736, V, 1, 1, 1, 1, 0, 700, 97
42737, V, 1, 1, 1, 1, 0, 700, 97
42738, V, 1, 1, 1, 1, 0, 700, 97
42739, V, 1, 1, 1, 1, 0, 700, 97
42740, V, 1, 1, 1, 1, 0, 700, 97
42741, V, 1, 1, 1, 1, 0, 700, 97
42742, V, 1, 1, 1, 1, 0, 700, 97
42743, V, 1, 1, 1, 1, 0, 700, 97
42744, V, 1, 1, 1, 1, 0, 700, 97
42745, V, 1, 1, 1, 1, 0, 700, 97
42746, V, 1, 1, 1, 1, 0, 700, 97
42747, V, 1, 1, 1, 1, 0, 700, 97
42748, V, 1, 1, 1, 1, 0, 700, 97
42749, V, 1, 1, 1, 1, 0, 700, 97
42750, V, 1, 1, 1, 1, 0, 700, 97
42752, V, 1, 1, 1, 1, 0, 700, 97
42753, V, 1, 1, 1, 1, 0, 700, 97
42754, V, 1, 1, 1, 1, 0, 700, 97
42755, V, 1, 1, 1, 1, 0, 700, 97
42756, V, 1, 1, 1, 1, 0, 700, 97
42757, V, 1, 1, 1, 1, 0, 700, 97
42758, V, 1, 1, 1, 1, 0, 700, 97
42759, V, 1, 1, 1, 1, 0, 700, 97
42760, V, 1, 1, 1, 1, 0, 700, 97
42761, V, 1, 1, 1, 1, 0, 700, 97
42762, V, 1, 1, 1, 1, 0, 700, 97
42763, V, 1, 1, 1, 1, 0, 700, 97
42764, V, 1, 1, 1, 1, 0, 700, 97
42765, V, 1, 1, 1, 1, 0, 700, 97
42766, V, 1, 1, 1, 1, 0, 700, 97
42767, V, 1, 1, 1, 1, 0, 700, 97
42768, V, 1, 1, 1, 1, 0, 700, 97
42769, V, 1, 1, 1, 1, 0, 700, 97
42770, V, 1, 1, 1, 1, 0, 700, 97
42771, V, 1, 1, 1, 1, 0, 700, 97
42772, V, 1, 1, 1, 1, 0, 700, 97
42773, V, 1, 1, 1, 1, 0, 700, 97
42774, V, 1, 1, 1, 1, 0, 700, 97
42775, V, 1, 1, 1, 1, 0, 700, 97
42776, V, 1, 1, 1, 1, 0, 700, 97
42777, V, 1, 1, 1, 1, 0, 700, 97
42778, V, 1, 1, 1, 1, 0, 700, 97
42779, V, 1, 1, 1, 1, 0, 700, 97
42780, V, 1, 1, 1, 1, 0, 700, 97
42781, V, 1, 1, 1, 1, 0, 700, 97
42782, V, 1, 1, 1, 1, 0, 700, 97
42783, V, 1, 1, 1, 1, 0, 700, 97
42784, V, 1, 1, 1, 1, 0, 700, 97
42785, V, 1, 1, 1, 1, 0, 700, 97
42786, V, 1, 1, 1, 1, 0, 700, 97
42787, V, 1, 1, 1, 1, 0, 700, 97
42788, V, 1, 1, 1, 1, 0, 700, 97
42789, V, 1, 1, 1, 1, 0, 700, 97
42790, V, 1, 1, 1, 1, 0, 700, 97
42791, V, 1, 1, 1, 1, 0, 700, 97
42792, V, 1, 1, 1, 1, 0, 700, 97
42793, V, 1, 1, 1, 1, 0, 700, 97
42795, V, 1, 1, 1, 1, 0, 700, 97
42796, V, 1, 1, 1, 1, 0, 700, 97
42797, V, 1, 1, 1, 1, 0, 700, 97
42798, V, 1, 1, 1, 1, 0, 700, 97
42799, V, 1, 1, 1, 1, 0, 700, 97
42800, V, 1, 1, 1, 1, 0, 700, 97
42801, V, 1, 1, 1, 1, 0, 700, 97
42802, V, 1, 1, 1, 1, 0, 700, 97
42803, V, 1, 1, 1, 1, 0, 700, 97
42804, V, 1, 1, 1, 1, 0, 700, 97
42805, V, 1, 1, 1, 1, 0, 700, 97
42806, V, 1, 1, 1, 1, 0, 700, 97
42807, V, 1, 1, 1, 1, 0, 700, 97
42808, V, 1, 1, 1, 1, 0, 700, 97
42809, V, 1, 1, 1, 1, 0, 700, 97
42810, V, 1, 1, 1, 1, 0, 700, 97
42811, V, 1, 1, 1, 1, 0, 700, 97
42812, V, 1, 1, 1, 1, 0, 700, 97
42813, V, 1, 1, 1, 1, 0, 700, 97
42814, V, 1, 1, 1, 1, 0, 700, 97
42815, V, 1, 1, 1, 1, 0, 700, 97
42816, V, 1, 1, 1, 1, 0, 700, 97
42817, V, 1, 1, 1, 1, 0, 700, 97
42818, V, 1, 1, 1, 1, 0, 700, 97
42819, V, 1, 1, 1, 1, 0, 700, 97
42820, V, 1, 1, 1, 1, 0, 700, 97
42821, V, 1, 1, 1, 1, 0, 700, 97
42822, V, 1, 1, 1, 1, 0, 700, 97
42823, V, 1, 1, 1, 1, 0, 700, 97
42824, V, 1, 1, 1, 1, 0, 700, 97
42825, V, 1, 1, 1, 1, 0, 700, 97
42826, V, 1, 1, 1, 1, 0, 700, 97
42827, V, 1, 1, 1, 1, 0, 700, 97
42828, V, 1, 1, 1, 1, 0, 700, 97
42829, V, 1, 1, 1, 1, 0, 700, 97
42830, V, 1, 1, 1, 1, 0, 700, 97
42831, V, 1, 1, 1, 1, 0, 700, 97
42832, V, 1, 1, 1, 1, 0, 700, 97
42833, V, 1, 1, 1, 1, 0, 700, 97
42834, V, 1, 1, 1, 1, 0, 700, 97
42835, V, 1, 1, 1, 1, 0, 700, 97
42836, V, 1, 1, 1, 1, 0, 700, 97
42838, V, 1, 1, 1, 1, 0, 700, 97
42839, V, 1, 1, 1, 1, 0, 700, 97
42840, V, 1, 1, 1, 1, 0, 700, 97
42841, V, 1, 1, 1, 1, 0, 700, 97
42842, V, 1, 1, 1, 1, 0, 700, 97
42843, V, 1, 1, 1, 1, 0, 700, 97
42844, V, 1, 1, 1, 1, 0, 700, 97
42845, V, 1, 1, 1, 1, 0, 700, 97
42846, V, 1, 1, 1, 1, 0, 700, 97
42847, V, 1, 1, 1, 1, 0, 700, 97
42848, V, 1, 1, 1, 1, 0, 700, 97
42849, V, 1, 1, 1, 1, 0, 700, 97
42850, V, 1, 1, 1, 1, 0, 700, 97
42851, V, 1, 1, 1, 1, 0, 700, 97
42852, V, 1, 1, 1, 1, 0, 700, 97
42853, V, 1, 1, 1, 1, 0, 700, 97
42854, V, 1, 1, 1, 1, 0, 700, 97
42855, V, 1, 1, 1, 1, 0, 700, 97
42856, V, 1, 1, 1, 1, 0, 700, 97
42857, V, 1, 1, 1, 1, 0, 700, 97
42858, V, 1, 1, 1, 1, 0, 700, 97
42859, V, 1, 1, 1, 1, 0, 700, 97
42860, V, 1, 1, 1, 1, 0, 700, 97
42861, V, 1, 1, 1, 1, 0, 700, 97
42862, V, 1, 1, 1, 1, 0, 700, 97
42863, V, 1, 1, 1, 1, 0, 700, 97
42864, V, 1, 1, 1, 1, 0, 700, 97
42865, V, 1, 1, 1, 1, 0, 700, 97
42866, V, 1, 1, 1, 1, 0, 700, 97
42867, V, 1, 1, 1, 1, 0, 700, 97
42868, V, 1, 1, 1, 1, 0, 700, 97
42869, V, 1, 1, 1, 1, 0, 700, 97
42870, V, 1, 1, 1, 1, 0, 700, 97
42871, V, 1, 1, 1, 1, 0, 700, 97
42872, V, 1, 1, 1, 1, 0, 700, 97
42873, V, 1, 1, 1, 1, 0, 700, 97
42874, V, 1, 1, 1, 1, 0, 700, 97
42875, V, 1, 1, 1, 1, 0, 700, 97
42876, V, 1, 1, 1, 1, 0, 700, 97
42877, V, 1, 1, 1, 1, 0, 700, 97
42878, V, 1, 1, 1, 1, 0, 700, 97
42880, V, 1, 1, 1, 1, 0, 700, 97
42881, V, 1, 1, 1, 1, 0, 700, 97
42882, V, 1, 1, 1, 1, 0, 700, 97
42883, V, 1, 1, 1, 1, 0, 700, 97
42884, V, 1, 1, 1, 1, 0, 700, 97
42885, V, 1, 1, 1, 1, 0, 700, 97
42886, V, 1, 1, 1, 1, 0, 700, 97
42887, V, 1, 1, 1, 1, 0, 700, 97
42888, V, 1, 1, 1, 1, 0, 700, 97
42889, V, 1, 1, 1, 1, 0, 700, 97
42890, V, 1, 1, 1, 1, 0, 700, 97
42891, V, 1, 1, 1, 1, 0, 700, 97
42892, V, 1, 1, 1, 1, 0, 700, 97
42893, V, 1, 1, 1, 1, 0, 700, 97
42894, V, 1, 1, 1, 1, 0, 700, 97
42895, V, 1, 1, 1, 1, 0, 700, 97
42896, V, 1, 1, 1, 1, 0, 700, 97
42897, V, 1, 1, 1, 1, 0, 700, 97
42898, V, 1, 1, 1, 1, 0, 700, 97
42899, V, 1, 1, 1, 1, 0, 700, 97
42900, V, 1, 1, 1, 1, 0, 700, 97
42901, V, 1, 1, 1, 1, 0, 700, 97
42902, V, 1, 1, 1, 1, 0, 700, 97
42903, V, 1, 1, 1, 1, 0, 700, 97
42904, V, 1, 1, 1, 1, 0, 700, 97
42905, V, 1, 1, 1, 1, 0, 700, 97
42906, V, 1, 1, 1, 1, 0, 700, 97
42907, V, 1, 1, 1, 1, 0, 700, 97
42908, V, 1, 1, 1, 1, 0, 700, 97
42909, V, 1, 1, 1, 1, 0, 700, 97
42910, V, 1, 1, 1, 1, 0, 700, 97
42911, V, 1, 1, 1, 1, 0, 700, 97
42912, V, 1, 1, 1, 1, 0, 700, 97
42913, V, 1, 1, 1, 1, 0, 700, 97
42914, V, 1, 1, 1, 1, 0, 700, 97
42915, V, 1, 1, 1, 1, 0, 700, 97
42916, V, 1, 1, 1, 1, 0, 700, 97
42917, V, 1, 1, 1, 1, 0, 700, 97
42918, V, 1, 1, 1, 1, 0, 700, 97
42919, V, 1, 1, 1, 1, 0, 700, 97
42920, V, 1, 1, 1, 1, 0, 700, 97
42921, V, 1, 1, 1, 1, 0, 700, 97
42923, V, 1, 1, 1, 1, 0, 700, 97
42924, V, 1, 1, 1, 1, 0, 700, 97
42925, V, 1, 1, 1, 1, 0, 700, 97
42926, V, 1, 1, 1, 1, 0, 700, 97
42927, V, 1, 1, 1, 1, 0, 700, 97
42928, V, 1, 1, 1, 1, 0, 700, 97
42929, V, 1, 1, 1, 1, 0, 700, 97
42930, V, 1, 1, 1, 1, 0, 700, 97
42931, V, 1, 1, 1, 1, 0, 700, 97
42932, V, 1, 1, 1, 1, 0, 700, 97
42933, V, 1, 1, 1, 1, 0, 700, 97
42934, V, 1, 1, 1, 1, 0, 700, 97
42935, V, 1, 1, 1, 1, 0, 700, 97
42936, V, 1, 1, 1, 1, 0, 700, 97
42937, V, 1, 1, 1, 1, 0, 700, 97
42938, V, 1, 1, 1, 1, 0, 700, 97
42939, V, 1, 1, 1, 1, 0, 700, 97
42940, V, 1, 1, 1, 1, 0, 700, 97
42941, V, 1, 1, 1, 1, 0, 700, 97
42942, V, 1, 1, 1, 1, 0, 700, 97
42943, V, 1, 1, 1, 1, 0, 700, 97
42944, V, 1, 1, 1, 1, 0, 700, 97
42945, V, 1, 1, 1, 1, 0, 700, 97
42946, V, 1, 1, 1, 1, 0, 700, 97
42947, V, 1, 1, 1, 1, 0, 700, 97
42948, V, 1, 1, 1, 1, 0, 700, 97
42949, V, 1, 1, 1, 1, 0, 700, 97
42950, V, 1, 1, 1, 1, 0, 700, 97
42951, V, 1, 1, 1, 1, 0, 700, 97
42952, V, 1, 1, 1, 1, 0, 700, 97
42953, V, 1, 1, 1, 1, 0, 700, 97
42954, V, 1, 1, 1, 1, 0, 700, 97
42955, V, 1, 1, 1, 1, 0, 700, 97
42956, V, 1, 1, 1, 1, 0, 700, 97
42957, V, 1, 1, 1, 1, 0, 700, 97
42958, V, 1, 1, 1, 1, 0, 700, 97
42959, V, 1, 1, 1, 1, 0, 700, 97
42960, V, 1, 1, 1, 1, 0, 700, 97
42961, V, 1, 1, 1, 1, 0, 700, 97
42962, V, 1, 1, 1, 1, 0, 700, 97
42963, V, 1, 1, 1, 1, 0, 700, 97
42964, V, 1, 1, 1, 1, 0, 700, 97
42966, V, 1, 1, 1, 1, 0, 700, 97
42967, V, 1, 1, 1, 1, 0, 700, 97
42968, V, 1, 1, 1, 1, 0, 700, 97
42969, V, 1, 1, 1, 1, 0, 700, 97
42970, V, 1, 1, 1, 1, 0, 700, 97
42971, V, 1, 1, 1, 1, 0, 700, 97
42972, V, 1, 1, 1, 1, 0, 700, 97
42973, V, 1, 1, 1, 1, 0, 700, 97
42974, V, 1, 1, 1, 1, 0, 700, 97
42975, V, 1, 1, 1, 1, 0, 700, 97
42976, V, 1, 1, 1, 1, 0, 700, 97
42977, V, 1, 1, 1, 1, 0, 700, 97
42978, V, 1, 1, 1, 1, 0, 700, 97
42979, V, 1, 1, 1, 1, 0, 700, 97
42980, V, 1, 1, 1, 1, 0, 700, 97
42981, V, 1, 1, 1, 1, 0, 700, 97
42982, V, 1, 1, 1, 1, 0, 700, 97
42983, V, 1, 1, 1, 1, 0, 700, 97
42984, V, 1, 1, 1, 1, 0, 700, 97
42985, V, 1, 1, 1, 1, 0, 700, 97
42986, V, 1, 1, 1, 1, 0, 700, 97
42987, V, 1, 1, 1, 1, 0, 700, 97
42988, V, 1, 1, 1, 1, 0, 700, 97
42989, V, 1, 1, 1, 1, 0, 700, 97
42990, V, 1, 1, 1, 1, 0, 700, 97
42991, V, 1, 1, 1, 1, 0, 700, 97
42992, V, 1, 1, 1, 1, 0, 700, 97
42993, V, 1, 1, 1, 1, 0, 700, 97
42994, V, 1, 1, 1, 1, 0, 700, 97
42995, V, 1, 1, 1, 1, 0, 700, 97
42996, V, 1, 1, 1, 1, 0, 700, 97
42997, V, 1, 1, 1, 1, 0, 700, 97
42998, V, 1, 1, 1, 1, 0, 700, 97
42999, V, 1, 1, 1, 1, 0, 700, 97
43000, V, 1, 1, 1, 1, 0, 700, 97
43001, V, 1, 1, 1, 1, 0, 700, 97
43002, V, 1, 1, 1, 1, 0, 700, 97
43003, V, 1, 1, 1, 1, 0, 700, 97
43004, V, 1, 1, 1, 1, 0, 700, 97
43005, V, 1, 1, 1, 1, 0, 700, 97
43006, V, 1, 1, 1, 1, 0, 700, 97
43008, V, 1, 1, 1, 1, 0, 700, 97
43009, V, 1, 1, 1, 1, 0, 700, 97
43010, V, 1, 1, 1, 1, 0, 700, 97
43011, V, 1, 1, 1, 1, 0, 700, 97
43012, V, 1, 1, 1, 1, 0, 700, 97
43013, V, 1, 1, 1, 1, 0, 700, 97
43014, V, 1, 1, 1, 1, 0, 700, 97
43015, V, 1, 1, 1, 1, 0, 700, 97
43016, V, 1, 1, 1, 1, 0, 700, 97
43017, V, 1, 1, 1, 1, 0, 700, 97
43018, V, 1, 1, 1, 1, 0, 700, 97
43019, V, 1, 1, 1, 1, 0, 700, 97
43020, V, 1, 1, 1, 1, 0, 700, 97
43021, V, 1, 1, 1, 1, 0, 700, 97
43022, V, 1, 1, 1, 1, 0, 700, 97
43023, V, 1, 1, 1, 1, 0, 700, 97
43024, V, 1, 1, 1, 1, 0, 700, 97
43025, V, 1, 1, 1, 1, 0, 700, 97
43026, V, 1, 1, 1, 1, 0, 700, 97
43027, V, 1, 1, 1, 1, 0, 700, 97
43028, V, 1, 1, 1, 1, 0, 700, 97
43029, V, 1, 1, 1, 1, 0, 700, 97
43030, V, 1, 1, 1, 1, 0, 700, 97
43031, V, 1, 1, 1, 1, 0, 700, 97
43032, V, 1, 1, 1, 1, 0, 700, 97
43033, V, 1, 1, 1, 1, 0, 700, 97
43034, V, 1, 1, 1, 1, 0, 700, 97
43035, V, 1, 1, 1, 1, 0, 700, 97
43036, V, 1, 1, 1, 1, 0, 700, 97
43037, V, 1, 1, 1, 1, 0, 700, 97
43038, V, 1, 1, 1, 1, 0, 700, 97
43039, V, 1, 1, 1, 1, 0, 700, 97
43040, V, 1, 1, 1, 1, 0, 700, 97
43041, V, 1, 1, 1, 1, 0, 700, 97
43042, V, 1, 1, 1, 1, 0, 700, 97
43043, V, 1, 1, 1, 1, 0, 700, 97
43044, V, 1, 1, 1, 1, 0, 700, 97
43045, V, 1, 1, 1, 1, 0, 700, 97
43046, V, 1, 1, 1, 1, 0, 700, 97
43047, V, 1, 1, 1, 1, 0, 700, 97
43048, V, 1, 1, 1, 1, 0, 700, 97
43049, V, 1, 1, 1, 1, 0, 700, 97
43051, V, 1, 1, 1, 1, 0, 700, 97
43052, V, 1, 1, 1, 1, 0, 700, 97
43053, V, 1, 1, 1, 1, 0, 700, 97
43054, V, 1, 1, 1, 1, 0, 700, 97
43055, V, 1, 1, 1, 1, 0, 700, 97
43056, V, 1, 1, 1, 1, 0, 700, 97
43057, V, 1, 1, 1, 1, 0, 700, 97
43058, V, 1, 1, 1, 1, 0, 700, 97
43059, V, 1, 1, 1, 1, 0, 700, 97
43060, V, 1, 1, 1, 1, 0, 700, 97
43061, V, 1, 1, 1, 1, 0, 700, 97
43062, V, 1, 1, 1, 1, 0, 700, 97
43063, V, 1, 1, 1, 1, 0, 700, 97
43064, V, 1, 1, 1, 1, 0, 700, 97
43065, V, 1, 1, 1, 1, 0, 700, 97
43066, V, 1, 1, 1, 1, 0, 700, 97
43067, V, 1, 1, 1, 1, 0, 700, 97
43068, V, 1, 1, 1, 1, 0, 700, 97
43069, V, 1, 1, 1, 1, 0, 700, 97
43070, V, 1, 1, 1, 1, 0, 700, 97
43071, V, 1, 1, 1, 1, 0, 700, 97
43072, V, 1, 1, 1, 1, 0, 700, 97
43073, V, 1, 1, 1, 1, 0, 700, 97
43074, V, 1, 1, 1, 1, 0, 700, 97
43075, V, 1, 1, 1, 1, 0, 700, 97
43076, V, 1, 1, 1, 1, 0, 700, 97
43077, V, 1, 1, 1, 1, 0, 700, 97
43078, V, 1, 1, 1, 1, 0, 700, 97
43079, V, 1, 1, 1, 1, 0, 700, 97
43080, V, 1, 1, 1, 1, 0, 700, 97
43081, V, 1, 1, 1, 1, 0, 700, 97
43082, V, 1, 1, 1, 1, 0, 700, 97
43083, V, 1, 1, 1, 1, 0, 700, 97
43084, V, 1, 1, 1, 1, 0, 700, 97
43085, V, 1, 1, 1, 1, 0, 700, 97
43086, V, 1, 1, 1, 1, 0, 700, 97
43087, V, 1, 1, 1, 1, 0, 700, 97
43088, V, 1, 1, 1, 1, 0, 700, 97
43089, V, 1, 1, 1, 1, 0, 700, 97
43090, V, 1, 1, 1, 1, 0, 700, 97
43091, V, 1, 1, 1, 1, 0, 700, 97
43092, V, 1, 1, 1, 1, 0, 700, 97
43094, V, 1, 1, 1, 1, 0, 700, 97
43095, V, 1, 1, 1, 1, 0, 700, 97
43096, V, 1, 1, 1, 1, 0, 700, 97
43097, V, 1, 1, 1, 1, 0, 700, 97
43098, V, 1, 1, 1, 1, 0, 700, 97
43099, V, 1, 1, 1, 1, 0, 700, 97
43100, V, 1, 1, 1, 1, 0, 700, 97
43101, V, 1, 1, 1, 1, 0, 700, 97
43102, V, 1, 1, 1, 1, 0, 700, 97
43103, V, 1, 1, 1, 1, 0, 700, 97
43104, V, 1, 1, 1, 1, 0, 700, 97
43105, V, 1, 1, 1, 1, 0, 700, 97
43106, V, 1, 1, 1, 1, 0, 700, 97
43107, V, 1, 1, 1, 1, 0, 700, 97
43108, V, 1, 1, 1, 1, 0, 700, 97
43109, V, 1, 1, 1, 1, 0, 700, 97
43110, V, 1, 1, 1, 1, 0, 700, 97
43111, V, 1, 1, 1, 1, 0, 700, 97
43112, V, 1, 1, 1, 1, 0, 700, 97
43113, V, 1, 1, 1, 1, 0, 700, 97
43114, V, 1, 1, 1, 1, 0, 700, 97
43115, V, 1, 1, 1, 1, 0, 700, 97
43116, V, 1, 1, 1, 1, 0, 700, 97
43117, V, 1, 1, 1, 1, 0, 700, 97
43118, V, 1, 1, 1, 1, 0, 700, 97
43119, V, 1, 1, 1, 1, 0, 700, 97
43120, V, 1, 1, 1, 1, 0, 700, 97
43121, V, 1, 1, 1, 1, 0, 700, 97
43122, V, 1, 1, 1, 1, 0, 700, 97
43123, V, 1, 1, 1, 1, 0, 700, 97
43124, V, 1, 1, 1, 1, 0, 700, 97
43125, V, 1, 1, 1, 1, 0, 700, 97
43126, V, 1, 1, 1, 1, 0, 700, 97
43127, V, 1, 1, 1, 1, 0, 700, 97
43128, V, 1, 1, 1, 1, 0, 700, 97
43129, V, 1, 1, 1, 1, 0, 700, 97
43130, V, 1, 1, 1, 1, 0, 700, 97
43131, V, 1, 1, 1, 1, 0, 700, 97
43132, V, 1, 1, 1, 1, 0, 700, 97
43133, V, 1, 1, 1, 1, 0, 700, 97
43134, V, 1, 1, 1, 1, 0, 700, 97
43136, V, 1, 1, 1, 1, 0, 700, 97
43137, V, 1, 1, 1, 1, 0, 700, 97
43138, V, 1, 1, 1, 1, 0, 700, 97
43139, V, 1, 1, 1, 1, 0, 700, 97
43140, V, 1, 1, 1, 1, 0, 700, 97
43141, V, 1, 1, 1, 1, 0, 700, 97
43142, V, 1, 1, 1, 1, 0, 700, 97
43143, V, 1, 1, 1, 1, 0, 700, 97
43144, V, 1, 1, 1, 1, 0, 700, 97
43145, V, 1, 1, 1, 1, 0, 700, 97
43146, V, 1, 1, 1, 1, 0, 700, 97
43147, V, 1, 1, 1, 1, 0, 700, 97
43148, V, 1, 1, 1, 1, 0, 700, 97
43149, V, 1, 1, 1, 1, 0, 700, 97
43150, V, 1, 1, 1, 1, 0, 700, 97
43151, V, 1, 1, 1, 1, 0, 700, 97
43152, V, 1, 1, 1, 1, 0, 700, 97
43153, V, 1, 1, 1, 1, 0, 700, 97
43154, V, 1, 1, 1, 1, 0, 700, 97
43155, V, 1, 1, 1, 1, 0, 700, 97
43156, V, 1, 1, 1, 1, 0, 700, 97
43157, V, 1, 1, 1, 1, 0, 700, 97
43158, V, 1, 1, 1, 1, 0, 700, 97
43159, V, 1, 1, 1, 1, 0, 700, 97
43160, V, 1, 1, 1, 1, 0, 700, 97
43161, V, 1, 1, 1, 1, 0, 700, 97
43162, V, 1, 1, 1, 1, 0, 700, 97
43163, V, 1, 1, 1, 1, 0, 700, 97
43164, V, 1, 1, 1, 1, 0, 700, 97
43165, V, 1, 1, 1, 1, 0, 700, 97
43166, V, 1, 1, 1, 1, 0, 700, 97
43167, V, 1, 1, 1, 1, 0, 700, 97
43168, V, 1, 1, 1, 1, 0, 700, 97
43169, V, 1, 1, 1, 1, 0, 700, 97
43170, V, 1, 1, 1, 1, 0, 700, 97
43171, V, 1, 1, 1, 1, 0, 700, 97
43172, V, 1, 1, 1, 1, 0, 700, 97
43173, V, 1, 1, 1, 1, 0, 700, 97
43174, V, 1, 1, 1, 1, 0, 700, 97
43175, V, 1, 1, 1, 1, 0, 700, 97
43176, V, 1, 1, 1, 1, 0, 700, 97
43177, V, 1, 1, 1, 1, 0, 700, 97
43179, V, 1, 1, 1, 1, 0, 700, 97
43180, V, 1, 1, 1, 1, 0, 700, 97
43181, V, 1, 1, 1, 1, 0, 700, 97
43182, V, 1, 1, 1, 1, 0, 700, 97
43183, V, 1, 1, 1, 1, 0, 700, 97
43184, V, 1, 1, 1, 1, 0, 700, 97
43185, V, 1, 1, 1, 1, 0, 700, 97
43186, V, 1, 1, 1, 1, 0, 700, 97
43187, V, 1, 1, 1, 1, 0, 700, 97
43188, V, 1, 1, 1, 1, 0, 700, 97
43189, V, 1, 1, 1, 1, 0, 700, 97
43190, V, 1, 1, 1, 1, 0, 700, 97
43191, V, 1, 1, 1, 1, 0, 700, 97
43192, V, 1, 1, 1, 1, 0, 700, 97
43193, V, 1, 1, 1, 1, 0, 700, 97
43194, V, 1, 1, 1, 1, 0, 700, 97
43195, V, 1, 1, 1, 1, 0, 700, 97
43196, V, 1, 1, 1, 1, 0, 700, 97
43197, V, 1, 1, 1, 1, 0, 700, 97
43198, V, 1, 1, 1, 1, 0, 700, 97
43199, V, 1, 1, 1, 1, 0, 700, 97
43200, V, 1, 1, 1, 1, 0, 700, 97
43201, V, 1, 1, 1, 1, 0, 700, 97
43202, V, 1, 1, 1, 1, 0, 700, 97
43203, V, 1, 1, 1, 1, 0, 700, 97
43204, V, 1, 1, 1, 1, 0, 700, 97
43205, V, 1, 1, 1, 1, 0, 700, 97
43206, V, 1, 1, 1, 1, 0, 700, 97
43207, V, 1, 1, 1, 1, 0, 700, 97
43208, V, 1, 1, 1, 1, 0, 700, 97
43209, V, 1, 1, 1, 1, 0, 700, 97
43210, V, 1, 1, 1, 1, 0, 700, 97
43211, V, 1, 1, 1, 1, 0, 700, 97
43212, V, 1, 1, 1, 1, 0, 700, 97
43213, V, 1, 1, 1, 1, 0, 700, 97
43214, V, 1, 1, 1, 1, 0, 700, 97
43215, V, 1, 1, 1, 1, 0, 700, 97
43216, V, 1, 1, 1, 1, 0, 700, 97
43217, V, 1, 1, 1, 1, 0, 700, 97
43218, V, 1, 1, 1, 1, 0, 700, 97
43219, V, 1, 1, 1, 1, 0, 700, 97
43220, V, 1, 1, 1, 1, 0, 700, 97
43222, V, 1, 1, 1, 1, 0, 700, 97
43223, V, 1, 1, 1, 1, 0, 700, 97
43224, V, 1, 1, 1, 1, 0, 700, 97
43225, V, 1, 1, 1, 1, 0, 700, 97
43226, V, 1, 1, 1, 1, 0, 700, 97
43227, V, 1, 1, 1, 1, 0, 700, 97
43228, V, 1, 1, 1, 1, 0, 700, 97
43229, V, 1, 1, 1, 1, 0, 700, 97
43230, V, 1, 1, 1, 1, 0, 700, 97
43231, V, 1, 1, 1, 1, 0, 700, 97
43232, V, 1, 1, 1, 1, 0, 700, 97
43233, V, 1, 1, 1, 1, 0, 700, 97
43234, V, 1, 1, 1, 1, 0, 700, 97
43235, V, 1, 1, 1, 1, 0, 700, 97
43236, V, 1, 1, 1, 1, 0, 700, 97
43237, V, 1, 1, 1, 1, 0, 700, 97
43238, V, 1, 1, 1, 1, 0, 700, 97
43239, V, 1, 1, 1, 1, 0, 700, 97
43240, V, 1, 1, 1, 1, 0, 700, 97
43241, V, 1, 1, 1, 1, 0, 700, 97
43242, V, 1, 1, 1, 1, 0, 700, 97
43243, V, 1, 1, 1, 1, 0, 700, 97
43244, V, 1, 1, 1, 1, 0, 700, 97
43245, V, 0, 1, 0, 0, 0, 700, 97
43270, V, 0, 0, 0, 0, 0, 700, 93
43441, V, 0, 0, 0, 0, 0, 700, 51
43441, V, 0, 0, 0, 0, 0, 700, 51
43698, V, 0, 0, 0, 0, 0, 700, 51
43698, V, 0, 0, 0, 0, 0, 700, 51
43955, V, 0, 0, 0, 0, 0, 700, 51
43955, V, 0, 0, 0, 0, 0, 700, 51
44212, V, 0, 0, 0, 0, 0, 700, 51
44212, V, 0, 0, 0, 0, 0, 700, 51
44469, V, 0, 0, 0, 0, 0, 700, 51
44469, V, 0, 0, 0, 0, 0, 700, 51
44726, V, 0, 0, 0, 0, 0, 700, 52
44726, V, 0, 0, 0, 0, 0, 700, 52
44983, V, 0, 0, 0, 0, 0, 700, 52
44983, V, 0, 0, 0, 0, 0, 700, 52
45240, V, 0, 0, 0, 0, 0, 700, 52
45240, V, 0, 0, 0, 0, 0, 700, 52
45497, V, 0, 0, 0, 0, 0, 700, 52
45497, V, 0, 0, 0, 0, 0, 700, 52
45754, V, 0, 0, 0, 0, 0, 700, 52
45754, V, 0, 0, 0, 0, 0, 700, 52
46011, V, 0, 0, 0, 0, 0, 700, 52
46011, V, 0, 0, 0, 0, 0, 700, 52
46268, V, 0, 0, 0, 0, 0, 700, 52
46268, V, 0, 0, 0, 0, 0, 700, 52
46525, V, 0, 0, 0, 0, 0, 700, 52
46525, V, 0, 0, 0, 0, 0, 700, 52
46782, V, 0, 0, 0, 0, 0, 700, 52
46782, V, 0, 0, 0, 0, 0, 700, 52
47039, V, 0, 0, 0, 0, 0, 700, 52
47039, V, 0, 0, 0, 0, 0, 700, 52
47296, V, 0, 0, 0, 0, 0, 700, 52
47296, V, 0, 0, 0, 0, 0, 700, 52
47553, V, 0, 0, 0, 0, 0, 700, 52
47553, V, 0, 0, 0, 0, 0, 700, 52
47810, V, 0, 0, 0, 0, 0, 700, 52
47810, V, 0, 0, 0, 0, 0, 700, 52
48067, V, 0, 0, 0, 0, 0, 700, 52
48067, V, 0, 0, 0, 0, 0, 700, 52
48324, V, 0, 0, 0, 0, 0, 700, 52
48324, V, 0, 0, 0, 0, 0, 700, 52
48581, V, 0, 0, 0, 0, 0, 700, 52
48581, V, 0, 0, 0, 0, 0, 700, 52
48838, V, 0, 0, 0, 0, 0, 700, 52
48838, V, 0, 0, 0, 0, 0, 700, 52
49095, V, 0, 0, 0, 0, 0, 700, 52
49095, V, 0, 0, 0, 0, 0, 700, 52
49352, V, 0, 0, 0, 0, 0, 700, 52
49352, V, 0, 0, 0, 0, 0, 700, 52
49609, V, 0, 0, 0, 0, 0, 700, 52
49609, V, 0, 0, 0, 0, 0, 700, 52
49866, V, 0, 0, 0, 0, 0, 700, 52
49866, V, 0, 0, 0, 0, 0, 700, 52
50123, V, 0, 0, 0, 0, 0, 700, 52
50123, V, 0, 0, 0, 0, 0, 700, 52
50380, V, 0, 0, 0, 0, 0, 700, 52
50380, V, 0, 0, 0, 0, 0, 700, 52
50637, V, 0, 0, 0, 0, 0, 700, 52
50637, V, 0, 0, 0, 0, 0, 700, 52
50894, V, 0, 0, 0, 0, 0, 700, 52
50894, V, 0, 0, 0, 0, 0, 700, 52
51151, V, 0, 0, 0, 0, 0, 700, 52
51151, V, 0, 0, 0, 0, 0, 700, 52
51408, V, 0, 0, 0, 0, 0, 700, 52
51408, V, 0, 0, 0, 0, 0, 700, 52
51665, V, 0, 0, 0, 0, 0, 700, 52
51665, V, 0, 0, 0, 0, 0, 700, 52
51922, V, 0, 0, 0, 0, 0, 700, 52
51922, V, 0, 0, 0, 0, 0, 700, 52
52179, V, 0, 0, 0, 0, 0, 700, 52
52179, V, 0, 0, 0, 0, 0, 700, 52
52436, V, 0, 0, 0, 0, 0, 700, 52
52436, V, 0, 0, 0, 0, 0, 700, 52
52694, V, 0, 0, 0, 0, 0, 700, 52
52694, V, 0, 0, 0, 0, 0, 700, 52
52951, V, 0, 0, 0, 0, 0, 700, 52
52951, V, 0, 0, 0, 0, 0, 700, 52
53208, V, 0, 0, 0, 0, 0, 700, 52
53208, V, 0, 0, 0, 0, 0, 700, 52
53465, V, 0, 0, 0, 0, 0, 700, 52
53465, V, 0, 0, 0, 0, 0, 700, 52
53722, V, 0, 0, 0, 0, 0, 700, 52
53722, V, 0, 0, 0, 0, 0, 700, 52
53979, V, 0, 0, 0, 0, 0, 700, 52
53979, V, 0, 0, 0, 0, 0, 700, 52
54236, V, 0, 0, 0, 0, 0, 700, 52
54236, V, 0, 0, 0, 0, 0, 700, 52
54493, V, 0, 0, 0, 0, 0, 700, 52
54493, V, 0, 0, 0, 0, 0, 700, 52
54750, V, 0, 0, 0, 0, 0, 700, 52
54750, V, 0, 0, 0, 0, 0, 700, 52
55007, V, 0, 0, 0, 0, 0, 700, 52
55007, V, 0, 0, 0, 0, 0, 700, 52
55264, V, 0, 0, 0, 0, 0, 700, 52
55264, V, 0, 0, 0, 0, 0, 700, 52
55521, V, 0, 0, 0, 0, 0, 700, 52
55521, V, 0, 0, 0, 0, 0, 700, 52
55778, V, 0, 0, 0, 0, 0, 700, 52
55778, V, 0, 0, 0, 0, 0, 700, 52
56035, V, 0, 0, 0, 0, 0, 700, 52
56035, V, 0, 0, 0, 0, 0, 700, 52
56292, V, 0, 0, 0, 0, 0, 700, 52
56292, V, 0, 0, 0, 0, 0, 700, 52
56549, V, 0, 0, 0, 0, 0, 700, 52
56549, V, 0, 0, 0, 0, 0, 700, 52
56806, V, 0, 0, 0, 0, 0, 700, 52
56806, V, 0, 0, 0, 0, 0, 700, 52
57063, V, 0, 0, 0, 0, 0, 700, 52
57063, V, 0, 0, 0, 0, 0, 700, 52
57320, V, 0, 0, 0, 0, 0, 700, 52
57320, V, 0, 0, 0, 0, 0, 700, 52
57577, V, 0, 0, 0, 0, 0, 700, 52
57577, V, 0, 0, 0, 0, 0, 700, 52
57834, V, 0, 0, 0, 0, 0, 700, 52
57834, V, 0, 0, 0, 0, 0, 700, 52
58091, V, 0, 0, 0, 0, 0, 700, 52
58091, V, 0, 0, 0, 0, 0, 700, 52
58348, V, 0, 0, 0, 0, 0, 700, 52
58348, V, 0, 0, 0, 0, 0, 700, 52
58605, V, 0, 0, 0, 0, 0, 700, 52
58605, V, 0, 0, 0, 0, 0, 700, 52
58862, V, 0, 0, 0, 0, 0, 700, 52
58862, V, 0, 0, 0, 0, 0, 700, 52
59119, V, 0, 0, 0, 0, 0, 700, 52
59119, V, 0, 0, 0, 0, 0, 700, 52
59376, V, 0, 0, 0, 0, 0, 700, 52
59376, V, 0, 0, 0, 0, 0, 700, 52
59633, V, 0, 0, 0, 0, 0, 700, 52
59633, V, 0, 0, 0, 0, 0, 700, 52
59890, V, 0, 0, 0, 0, 0, 700, 52
59890, V, 0, 0, 0, 0, 0, 700, 52
60147, V, 0, 0, 0, 0, 0, 700, 52
60147, V, 0, 0, 0, 0, 0, 700, 52
60404, V, 0, 0, 0, 0, 0, 700, 52
60404, V, 0, 0, 0, 0, 0, 700, 52
60661, V, 0, 0, 0, 0, 0, 700, 52
60661, V, 0, 0, 0, 0, 0, 700, 52
60918, V, 0, 0, 0, 0, 0, 700, 52
60918, V, 0, 0, 0, 0, 0, 700, 52
61175, V, 0, 0, 0, 0, 0, 700, 52
61175, V, 0, 0, 0, 0, 0, 700, 52
61432, V, 0, 0, 0, 0, 0, 700, 52
61432, V, 0, 0, 0, 0, 0, 700, 52
61689, V, 0, 0, 0, 0, 0, 700, 52
61689, V, 0, 0, 0, 0, 0, 700, 52
61946, V, 0, 0, 0, 0, 0, 700, 52
61946, V, 0, 0, 0, 0, 0, 700, 52
62203, V, 0, 0, 0, 0, 0, 700, 52
62203, V, 0, 0, 0, 0, 0, 700, 52
62460, V, 0, 0, 0, 0, 0, 700, 52
62460, V, 0, 0, 0, 0, 0, 700, 52
62717, V, 0, 0, 0, 0, 0, 700, 52
62717, V, 0, 0, 0, 0, 0, 700, 52
62974, V, 0, 0, 0, 0, 0, 700, 52
62974, V, 0, 0, 0, 0, 0, 700, 52
63232, V, 0, 0, 0, 0, 0, 700, 52
63232, V, 0, 0, 0, 0, 0, 700, 52
63489, V, 0, 0, 0, 0, 0, 700, 52
63489, V, 0, 0, 0, 0, 0, 700, 52
63746, V, 0, 0, 0, 0, 0, 700, 52
63746, V, 0, 0, 0, 0, 0, 700, 52
64003, V, 0, 0, 0, 0, 0, 700, 52
64003, V, 0, 0, 0, 0, 0, 700, 52
64260, V, 0, 0, 0, 0, 0, 700, 52
64260, V, 0, 0, 0, 0, 0, 700, 52
64517, V, 0, 0, 0, 0, 0, 700, 52
64517, V, 0, 0, 0, 0, 0, 700, 52
64774, V, 0, 0, 0, 0, 0, 700, 52
64774, V, 0, 0, 0, 0, 0, 700, 52
65031, V, 0, 0, 0, 0, 0, 700, 52
65031, V, 0, 0, 0, 0, 0, 700, 52
65288, V, 0, 0, 0, 0, 0, 700, 52
65288, V, 0, 0, 0, 0, 0, 700, 52
9, V, 0, 0, 0, 0, 0, 700, 52
9, V, 0, 0, 0, 0, 0, 700, 52
266, V, 0, 0, 0, 0, 0, 700, 52
266, V, 0, 0, 0, 0, 0, 700, 52
523, V, 0, 0, 0, 0, 0, 700, 52
523, V, 0, 0, 0, 0, 0, 700, 52
780, V, 0, 0, 0, 0, 0, 700, 52
780, V, 0, 0, 0, 0, 0, 700, 52
1037, V, 0, 0, 0, 0, 0, 700, 52
1037, V, 0, 0, 0, 0, 0, 700, 52
1294, V, 0, 0, 0, 0, 0, 700, 52
1294, V, 0, 0, 0, 0, 0, 700, 52
1551, V, 0, 0, 0, 0, 0, 700, 52
1551, V, 0, 0, 0, 0, 0, 700, 52
1808, V, 0, 0, 0, 0, 0, 700, 52
1808, V, 0, 0, 0, 0, 0, 700, 52
2065, V, 0, 0, 0, 0, 0, 700, 52
2065, V, 0, 0, 0, 0, 0, 700, 52
2322, V, 0, 0, 0, 0, 0, 700, 52
2322, V, 0, 0, 0, 0, 0, 700, 52
2579, V, 0, 0, 0, 0, 0, 700, 52
2579, V, 0, 0, 0, 0, 0, 700, 52
2836, V, 0, 0, 0, 0, 0, 700, 52
2836, V, 0, 0, 0, 0, 0, 700, 52
3093, V, 0, 0, 0, 0, 0, 700, 52
3093, V, 0, 0, 0, 0, 0, 700, 52
3350, V, 0, 0, 0, 0, 0, 700, 52
3350, V, 0, 0, 0, 0, 0, 700, 52
3607, V, 0, 0, 0, 0, 0, 700, 52
3607, V, 0, 0, 0, 0, 0, 700, 52
3864, V, 0, 0, 0, 0, 0, 700, 52
3864, V, 0, 0, 0, 0, 0, 700, 52
4121, V, 0, 0, 0, 0, 0, 700, 52
4121, V, 0, 0, 0, 0, 0, 700, 52
4378, V, 0, 0, 0, 0, 0, 700, 52
4378, V, 0, 0, 0, 0, 0, 700, 52
4635, V, 0, 0, 0, 0, 0, 700, 52
4635, V, 0, 0, 0, 0, 0, 700, 52
4892, V, 0, 0, 0, 0, 0, 700, 52
4892, V, 0, 0, 0, 0, 0, 700, 52
5149, V, 0, 0, 0, 0, 0, 700, 52
5149, V, 0, 0, 0, 0, 0, 700, 52
5406, V, 0, 0, 0, 0, 0, 700, 52
5406, V, 0, 0, 0, 0, 0, 700, 52
5663, V, 0, 0, 0, 0, 0, 700, 52
5663, V, 0, 0, 0, 0, 0, 700, 52
5920, V, 0, 0, 0, 0, 0, 700, 52
5920, V, 0, 0, 0, 0, 0, 700, 52
6177, V, 0, 0, 0, 0, 0, 700, 52
6177, V, 0, 0, 0, 0, 0, 700, 52
6434, V, 0, 0, 0, 0, 0, 700, 52
6434, V, 0, 0, 0, 0, 0, 700, 52
6691, V, 0, 0, 0, 0, 0, 700, 52
6691, V, 0, 0, 0, 0, 0, 700, 52
6948, V, 0, 0, 0, 0, 0, 700, 52
6948, V, 0, 0, 0, 0, 0, 700, 52
7205, V, 0, 0, 0, 0, 0, 700, 52
7205, V, 0, 0, 0, 0, 0, 700, 52
7462, V, 0, 0, 0, 0, 0, 700, 52
7462, V, 0, 0, 0, 0, 0, 700, 52
7766, V, 0, 0, 0, 0, 0, 700, 52
7766, V, 0, 0, 0, 0, 0, 700, 52
8023, V, 0, 0, 0, 0, 0, 700, 52
8023, V, 0, 0, 0, 0, 0, 700, 52
8280, V, 0, 0, 0, 0, 0, 700, 52
8280, V, 0, 0, 0, 0, 0, 700, 52
8537, V, 0, 0, 0, 0, 0, 700, 52
8537, V, 0, 0, 0, 0, 0, 700, 52
8794, V, 0, 0, 0, 0, 0, 700, 52
8794, V, 0, 0, 0, 0, 0, 700, 52
9051, V, 0, 0, 0, 0, 0, 700, 52
9051, V, 0, 0, 0, 0, 0, 700, 52
9308, V, 0, 0, 0, 0, 0, 700, 52
9308, V, 0, 0, 0, 0, 0, 700, 52
9565, V, 0, 0, 0, 0, 0, 700, 52
9565, V, 0, 0, 0, 0, 0, 700, 52
9822, V, 0, 0, 0, 0, 0, 700, 52
9822, V, 0, 0, 0, 0, 0, 700, 52
10079, V, 0, 0, 0, 0, 0, 700, 52
10079, V, 0, 0, 0, 0, 0, 700, 52
10336, V, 0, 0, 0, 0, 0, 700, 52
10336, V, 0, 0, 0, 0, 0, 700, 52
10593, V, 0, 0, 0, 0, 0, 700, 52
10593, V, 0, 0, 0, 0, 0, 700, 52
10850, V, 0, 0, 0, 0, 0, 700, 52
10850, V, 0, 0, 0, 0, 0, 700, 52
11107, V, 0, 0, 0, 0, 0, 700, 52
11107, V, 0, 0, 0, 0, 0, 700, 52
11364, V, 0, 0, 0, 0, 0, 700, 52
11364, V, 0, 0, 0, 0, 0, 700, 52
11621, V, 0, 0, 0, 0, 0, 700, 52
11621, V, 0, 0, 0, 0, 0, 700, 52
11878, V, 0, 0, 0, 0, 0, 700, 52
11878, V, 0, 0, 0, 0, 0, 700, 52
12135, V, 0, 0, 0, 0, 0, 700, 52
12135, V, 0, 0, 0, 0, 0, 700, 52
12392, V, 0, 0, 0, 0, 0, 700, 52
12392, V, 0, 0, 0, 0, 0, 700, 52
12649, V, 0, 0, 0, 0, 0, 700, 52
12649, V, 0, 0, 0, 0, 0, 700, 52
12906, V, 0, 0, 0, 0, 0, 700, 52
12906, V, 0, 0, 0, 0, 0, 700, 52
13163, V, 0, 0, 0, 0, 0, 700, 52
13163, V, 0, 0, 0, 0, 0, 700, 52
13420, V, 0, 0, 0, 0, 0, 700, 52
13420, V, 0, 0, 0, 0, 0, 700, 52
13677, V, 0, 0, 0, 0, 0, 700, 52
13677, V, 0, 0, 0, 0, 0, 700, 52
13934, V, 0, 0, 0, 0, 0, 700, 52
13934, V, 0, 0, 0, 0, 0, 700, 52
14191, V, 0, 0, 0, 0, 0, 700, 52
14191, V, 0, 0, 0, 0, 0, 700, 52
14448, V, 0, 0, 0, 0, 0, 700, 52
14448, V, 0, 0, 0, 0, 0, 700, 52
14705, V, 0, 0, 0, 0, 0, 700, 52
14705, V, 0, 0, 0, 0, 0, 700, 52
14962, V, 0, 0, 0, 0, 0, 700, 52
14962, V, 0, 0, 0, 0, 0, 700, 52
15219, V, 0, 0, 0, 0, 0, 700, 52
15219, V, 0, 0, 0, 0, 0, 700, 52
15476, V, 0, 0, 0, 0, 0, 700, 52
15476, V, 0, 0, 0, 0, 0, 700, 52
15733, V, 0, 0, 0, 0, 0, 700, 52
15733, V, 0, 0, 0, 0, 0, 700, 52
15990, V, 0, 0, 0, 0, 0, 700, 52
15990, V, 0, 0, 0, 0, 0, 700, 52
16247, V, 0, 0, 0, 0, 0, 700, 52
16247, V, 0, 0, 0, 0, 0, 700, 52
16504, V, 0, 0, 0, 0, 0, 700, 52
16504, V, 0, 0, 0, 0, 0, 700, 52
16761, V, 0, 0, 0, 0, 0, 700, 52
16761, V, 0, 0, 0, 0, 0, 700, 52
17018, V, 0, 0, 0, 0, 0, 700, 52
17018, V, 0, 0, 0, 0, 0, 700, 52
17275, V, 0, 0, 0, 0, 0, 700, 52
17275, V, 0, 0, 0, 0, 0, 700, 52
17532, V, 0, 0, 0, 0, 0, 700, 52
17532, V, 0, 0, 0, 0, 0, 700, 52
17789, V, 0, 0, 0, 0, 0, 700, 52
17789, V, 0, 0, 0, 0, 0, 700, 52
18046, V, 0, 0, 0, 0, 0, 700, 52
18046, V, 0, 0, 0, 0, 0, 700, 52
18304, V, 0, 0, 0, 0, 0, 700, 52
18304, V, 0, 0, 0, 0, 0, 700, 52
18561, V, 0, 0, 0, 0, 0, 700, 52
18561, V, 0, 0, 0, 0, 0, 700, 52
18818, V, 0, 0, 0, 0, 0, 700, 52
18818, V, 0, 0, 0, 0, 0, 700, 52
19075, V, 0, 0, 0, 0, 0, 700, 52
19075, V, 0, 0, 0, 0, 0, 700, 52
19332, V, 0, 0, 0, 0, 0, 700, 52
19332, V, 0, 0, 0, 0, 0, 700, 52
19589, V, 0, 0, 0, 0, 0, 700, 52
19589, V, 0, 0, 0, 0, 0, 700, 52
19846, V, 0, 0, 0, 0, 0, 700, 52
19846, V, 0, 0, 0, 0, 0, 700, 52
20103, V, 0, 0, 0, 0, 0, 700, 52
20103, V, 0, 0, 0, 0, 0, 700, 52
20360, V, 0, 0, 0, 0, 0, 700, 52
20360, V, 0, 0, 0, 0, 0, 700, 52
20617, V, 0, 0, 0, 0, 0, 700, 52
20617, V, 0, 0, 0, 0, 0, 700, 52
20874, V, 0, 0, 0, 0, 0, 700, 52
20874, V, 0, 0, 0, 0, 0, 700, 52
21131, V, 0, 0, 0, 0, 0, 700, 52
21131, V, 0, 0, 0, 0, 0, 700, 52
21388, V, 0, 0, 0, 0, 0, 700, 52
21388, V, 0, 0, 0, 0, 0, 700, 52
21645, V, 0, 0, 0, 0, 0, 700, 52
21645, V, 0, 0, 0, 0, 0, 700, 52
21902, V, 0, 0, 0, 0, 0, 700, 52
21902, V, 0, 0, 0, 0, 0, 700, 52
22159, V, 0, 0, 0, 0, 0, 700, 52
22159, V, 0, 0, 0, 0, 0, 700, 52
22416, V, 0, 0, 0, 0, 0, 700, 52
22416, V, 0, 0, 0, 0, 0, 700, 52
22673, V, 0, 0, 0, 0, 0, 700, 52
22673, V, 0, 0, 0, 0, 0, 700, 52
22930, V, 0, 0, 0, 0, 0, 700, 52
22930, V, 0, 0, 0, 0, 0, 700, 52
23187, V, 0, 0, 0, 0, 0, 700, 52
23187, V, 0, 0, 0, 0, 0, 700, 52
23444, V, 0, 0, 0, 0, 0, 700, 52
23444, V, 0, 0, 0, 0, 0, 700, 52
23701, V, 0, 0, 0, 0, 0, 700, 52
23701, V, 0, 0, 0, 0, 0, 700, 52
23958, V, 0, 0, 0, 0, 0, 700, 52
23958, V, 0, 0, 0, 0, 0, 700, 52
24215, V, 0, 0, 0, 0, 0, 700, 52
24215, V, 0, 0, 0, 0, 0, 700, 52
24472, V, 0, 0, 0, 0, 0, 700, 52
24472, V, 0, 0, 0, 0, 0, 700, 52
24729, V, 0, 0, 0, 0, 0, 700, 52
24729, V, 0, 0, 0, 0, 0, 700, 52
24986, V, 0, 0, 0, 0, 0, 700, 52
24986, V, 0, 0, 0, 0, 0, 700, 52
25243, V, 0, 0, 0, 0, 0, 700, 52
25243, V, 0, 0, 0, 0, 0, 700, 52
25500, V, 0, 0, 0, 0, 0, 700, 52
25500, V, 0, 0, 0, 0, 0, 700, 52
25757, V, 0, 0, 0, 0, 0, 700, 52
25757, V, 0, 0, 0, 0, 0, 700, 52
26014, V, 0, 0, 0, 0, 0, 700, 52
26014, V, 0, 0, 0, 0, 0, 700, 52
26271, V, 0, 0, 0, 0, 0, 700, 52
26271, V, 0, 0, 0, 0, 0, 700, 52
26528, V, 0, 0, 0, 0, 0, 700, 52
26528, V, 0, 0, 0, 0, 0, 700, 52
26785, V, 0, 0, 0, 0, 0, 700, 52
26785, V, 0, 0, 0, 0, 0, 700, 52
27042, V, 0, 0, 0, 0, 0, 700, 52
27042, V, 0, 0, 0, 0, 0, 700, 52
27299, V, 0, 0, 0, 0, 0, 700, 52
27299, V, 0, 0, 0, 0, 0, 700, 52
27556, V, 0, 0, 0, 0, 0, 700, 52
27556, V, 0, 0, 0, 0, 0, 700, 52
27813, V, 0, 0, 0, 0, 0, 700, 52
27813, V, 0, 0, 0, 0, 0, 700, 52
28070, V, 0, 0, 0, 0, 0, 700, 52
28070, V, 0, 0, 0, 0, 0, 700, 52
28327, V, 0, 0, 0, 0, 0, 700, 52
28327, V, 0, 0, 0, 0, 0, 700, 52
28584, V, 0, 0, 0, 0, 0, 700, 52
28584, V, 0, 0, 0, 0, 0, 700, 52
28841, V, 0, 0, 0, 0, 0, 700, 52
28841, V, 0, 0, 0, 0, 0, 700, 52
29099, V, 0, 0, 0, 0, 0, 700, 52
29099, V, 0, 0, 0, 0, 0, 700, 52
29356, V, 0, 0, 0, 0, 0, 700, 52
29356, V, 0, 0, 0, 0, 0, 700, 52
29613, V, 0, 0, 0, 0, 0, 700, 52
29613, V, 0, 0, 0, 0, 0, 700, 52
29870, V, 0, 0, 0, 0, 0, 700, 52
29870, V, 0, 0, 0, 0, 0, 700, 52
30127, V, 0, 0, 0, 0, 0, 700, 52
30127, V, 0, 0, 0, 0, 0, 700, 52
30384, V, 0, 0, 0, 0, 0, 700, 52
30384, V, 0, 0, 0, 0, 0, 700, 52
30641, V, 0, 0, 0, 0, 0, 700, 52
30641, V, 0, 0, 0, 0, 0, 700, 52
30898, V, 0, 0, 0, 0, 0, 700, 52
30898, V, 0, 0, 0, 0, 0, 700, 52
31155, V, 0, 0, 0, 0, 0, 700, 52
31155, V, 0, 0, 0, 0, 0, 700, 52
31412, V, 0, 0, 0, 0, 0, 700, 52
31412, V, 0, 0, 0, 0, 0, 700, 52
31669, V, 0, 0, 0, 0, 0, 700, 52
31669, V, 0, 0, 0, 0, 0, 700, 52
31926, V, 0, 0, 0, 0, 0, 700, 52
31926, V, 0, 0, 0, 0, 0, 700, 52
32183, V, 0, 0, 0, 0, 0, 700, 52
32183, V, 0, 0, 0, 0, 0, 700, 52
32440, V, 0, 0, 0, 0, 0, 700, 52
32440, V, 0, 0, 0, 0, 0, 700, 52
32697, V, 0, 0, 0, 0, 0, 700, 52
32697, V, 0, 0, 0, 0, 0, 700, 52
32954, V, 0, 0, 0, 0, 0, 700, 52
32954, V, 0, 0, 0, 0, 0, 700, 52
33211, V, 0, 0, 0, 0, 0, 700, 52
33211, V, 0, 0, 0, 0, 0, 700, 52
33468, V, 0, 0, 0, 0, 0, 700, 52
33468, V, 0, 0, 0, 0, 0, 700, 52
33725, V, 0, 0, 0, 0, 0, 700, 52
33725, V, 0, 0, 0, 0, 0, 700, 52
33982, V, 0, 0, 0, 0, 0, 700, 52
33982, V, 0, 0, 0, 0, 0, 700, 52
34239, V, 0, 0, 0, 0, 0, 700, 52
34239, V, 0, 0, 0, 0, 0, 700, 52
34496, V, 0, 0, 0, 0, 0, 700, 52
34496, V, 0, 0, 0, 0, 0, 700, 52
34753, V, 0, 0, 0, 0, 0, 700, 52
34753, V, 0, 0, 0, 0, 0, 700, 52
35010, V, 0, 0, 0, 0, 0, 700, 52
35010, V, 0, 0, 0, 0, 0, 700, 52
35267, V, 0, 0, 0, 0, 0, 700, 52
35267, V, 0, 0, 0, 0, 0, 700, 52
35524, V, 0, 0, 0, 0, 0, 700, 52
35524, V, 0, 0, 0, 0, 0, 700, 52
35781, V, 0, 0, 0, 0, 0, 700, 52
35781, V, 0, 0, 0, 0, 0, 700, 52
36038, V, 0, 0, 0, 0, 0, 700, 52
36038, V, 0, 0, 0, 0, 0, 700, 52
36295, V, 0, 0, 0, 0, 0, 700, 52
36295, V, 0, 0, 0, 0, 0, 700, 52
36552, V, 0, 0, 0, 0, 0, 700, 52
36552, V, 0, 0, 0, 0, 0, 700, 52
36809, V, 0, 0, 0, 0, 0, 700, 52
36809, V, 0, 0, 0, 0, 0, 700, 52
37066, V, 0, 0, 0, 0, 0, 700, 52
37066, V, 0, 0, 0, 0, 0, 700, 52
37323, V, 0, 0, 0, 0, 0, 700, 52
37323, V, 0, 0, 0, 0, 0, 700, 52
37580, V, 0, 0, 0, 0, 0, 700, 52
37580, V, 0, 0, 0, 0, 0, 700, 52
37837, V, 0, 0, 0, 0, 0, 700, 52
37837, V, 0, 0, 0, 0, 0, 700, 52
38094, V, 0, 0, 0, 0, 0, 700, 52
38094, V, 0, 0, 0, 0, 0, 700, 52
38351, V, 0, 0, 0, 0, 0, 700, 52
38351, V, 0, 0, 0, 0, 0, 700, 52
38608, V, 0, 0, 0, 0, 0, 700, 52
38608, V, 0, 0, 0, 0, 0, 700, 52
38865, V, 0, 0, 0, 0, 0, 700, 52
38865, V, 0, 0, 0, 0, 0, 700, 52